Enhanced anti-penetration composite boron carbide ceramic plate
By adding a spherical diamond layer between the boron carbide ceramic plate and the foam aluminum plate, the problem of cracking during high-speed impact is solved, and the penetration resistance and impact resistance are improved, meeting the high protection needs.
Patent Information
- Application Number
- CN202411293261.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-14
- Publication Date
- 2024-11-19
AI Technical Summary
Traditional boron carbide ceramic plates are prone to cracking during high-speed impact, resulting in a degradation of anti-penetration performance and difficult to meet the high protection needs of national defense and aerospace fields.
Add a diamond layer composed of multiple spherical diamonds between the boron carbide ceramic plate and the foam aluminum plate. The overall strength and impact resistance of the material are improved through the high-density structure of the spherical diamond and the adhesive filling, and utilize the lightweight of the foam aluminum plate. and toughness absorbs impact energy.
It effectively improves the anti-penetration ability of composite boron carbide ceramic plates, enhances the overall strength and rigidity of the material, reduces the risk of local damage, improves bulletproof performance, and extends the service life.
Smart Images

Figure CN118980289A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of boron carbide ceramics, and in particular relates to an enhanced anti-penetration composite boron carbide ceramic plate. Background Art
[0002] With the development of modern society, the demand for protective materials is increasing, especially in high-risk fields such as military, police and special operations. Boron carbide ceramic plates, as a material with unique physical, chemical and mechanical properties, have shown great application potential in these fields due to their high hardness, high melting point, excellent wear resistance, corrosion resistance and good thermal stability.
[0003] Although boron carbide ceramic plates have many advantages, their brittle properties can easily cause the material to crack when facing high-speed impact, thus affecting its anti-penetration performance. Especially in the fields of national defense and aerospace, the anti-penetration performance of protective materials is extremely high, and traditional boron carbide ceramic plates are difficult to meet these requirements. Therefore, composite boron carbide ceramic plates are often used in these fields to improve the bulletproof, anti-penetration and impact absorption capabilities of boron carbide ceramic plates. For example, the Chinese invention patent with application number 2020106646304 provides "a lightweight composite armor and its manufacturing method", which includes an inner layer, a transition layer and an outer layer from the inside to the outside. The outer layer is a modified boron carbide ceramic plate, and the inner layer is a composite of carbon fiber and epoxy resin. The transition layer includes a corrugated ceramic plate and an ultra-high molecular weight polyethylene fiber cloth coated on the outside of the ceramic plate. Hollow rubber microspheres are arranged in the gap between the ceramic plate and the ultra-high molecular weight polyethylene fiber cloth. The ultra-high molecular weight polyethylene fiber cloth is used to prevent the broken ceramic plate from flying and collapsing, and the rubber microspheres can play a strong buffering role.
[0004] However, when subjected to strong impact from high-speed / high-energy projectiles, the hollow rubber microspheres may break or deform, which is likely to reduce the overall structural stability and integrity of the composite armor, and the anti-penetration capability will also be greatly reduced. Summary of the invention
[0005] The present invention proposes an enhanced anti-penetration composite boron carbide ceramic plate, by adding a diamond layer composed of multiple spherical diamonds between the boron carbide ceramic plate and the foam aluminum plate, so that objects penetrating into the ceramic plate at high speed can be deflected or even broken, thereby effectively improving the anti-penetration ability of the composite boron carbide ceramic plate.
[0006] In order to solve the above technical problems, the technical solution of the present invention is:
[0007] A reinforced anti-penetration composite boron carbide ceramic plate comprises a boron carbide ceramic plate and a foam aluminum plate, a diamond layer is further arranged between the boron carbide ceramic plate and the foam aluminum plate, two sides of the diamond layer are respectively fixedly connected to the boron carbide ceramic plate and the foam aluminum plate, the diamond layer comprises spherical diamonds and a first adhesive for bonding the spherical diamonds to each other, adjacent spherical diamonds are bonded to each other, and the first adhesive is filled in the gaps between the spherical diamonds.
[0008] Although the boron carbide ceramic plate has a high hardness, it is easy to crack and lose its blocking effect when impacted by high-speed flying objects such as projectiles, and high-speed flying objects have a high probability of penetrating through the boron carbide ceramic plate and continuing to penetrate. Therefore, in the solution of the present invention, a diamond layer is compounded into the boron carbide ceramic plate to further prevent objects from penetrating.
[0009] Diamond is the hardest substance in nature, which can effectively resist the penetration of high-speed impact objects. Diamond has low density and excellent thermal conductivity, which makes it light in weight and can quickly dissipate the heat generated during the impact. The diamond layer in the present invention is composed of spherical diamonds, and the surface of the spherical diamonds is arc-shaped and has extremely high hardness. When the projectile hits, it can effectively change its motion trajectory, causing the projectile to deflect or break, thereby reducing the penetration of the projectile; wherein, the spherical diamonds are bonded to each other, thereby forming a high-density structure, which increases the overall strength and rigidity of the material. The gaps between the spherical diamonds are filled with the first adhesive, which further improves the integrity and impact resistance of the material.
[0010] In addition, it is worth mentioning that after the outer anti-penetration material is damaged, it is easy to cause further damage to the internal anti-impact material, so it is necessary to add a material layer that can provide a certain structural strength and absorb impact force to provide additional support and preliminary impact force absorption function for the composite ceramic plate as a whole. Usually, the material layer with this performance will use solid metal plate or polyethylene foam or foam aluminum plate, but the solid metal plate is heavy and does not meet the lightweight design requirements of anti-penetration ceramics. Although polyethylene foam is light and has certain energy absorption performance, its impact strength is poor and it is easy to break when subjected to strong impact. Therefore, it is more appropriate to use foam aluminum plate with light weight and good impact resistance. Therefore, in the present invention, a foam aluminum plate is arranged behind the diamond layer; firstly, the density of the foam aluminum plate is low, so its weight is light; secondly, as an aluminum material, the foam aluminum plate has a certain toughness, which enables it to deform and not break easily when impacted, thereby helping to maintain the structural integrity of the foam aluminum plate to provide additional support; importantly, when impacted, the holes in the foam aluminum will collapse, which effectively converts the impact energy into the energy of material deformation, realizing the function of the foam aluminum plate to absorb a large amount of impact energy, thereby reducing the impact force transmitted to the inside and improving the overall energy absorption capacity of the ceramic plate.
[0011] Preferably, the diamond layer is provided with at least two layers, and the spherical diamonds of each layer are stuck in the gap between two spherical diamonds of the adjacent layer, so that a stable triangular structure is formed between the adjacent spherical diamonds. In this way, by forming a stable triangular structure, the structural stability and overall strength of the diamond layer can be significantly improved, and the stress can be effectively dispersed to reduce the risk of local damage; the mutual contact between multiple spherical diamonds can not only play a role of mutual support, but also better absorb and disperse the impact energy, thereby reducing the impact on a single diamond and improving the ballistic performance of the entire composite material.
[0012] Preferably, a first groove is provided on the inner wall of the boron carbide ceramic plate, the inner wall and the first groove of the boron carbide ceramic plate are both sandblasted, the spherical diamond can be embedded in the first groove, and the spherical diamond is fixedly connected to the first groove through a first adhesive. Even if the spherical diamond cracks after being impacted, the integrity of the composite ceramic plate will not be affected due to the supporting bonding effect of the groove sidewall and the adhesive and the mutual support of the surrounding spherical diamonds. It is worth mentioning that sandblasting can increase the surface roughness of the inner wall of the boron carbide ceramic plate and the first groove, thereby improving the adhesion of the first adhesive, and making the connection between the spherical diamond and the first groove more secure. In this way, when subjected to a high-speed impact of an object, the spherical diamond is not easily deflected, and can better play its role, change the direction of movement of the impactor, and thus reduce the risk of penetration.
[0013] The depth of the first groove is the same as the radius of the spherical diamond, which can ensure that the spherical diamond is firmly connected to the boron carbide ceramic plate, reduce the risk of the spherical diamond falling off or shifting when impacted, and avoid affecting the overall thickness of the boron carbide ceramic plate.
[0014] Preferably, the first adhesive comprises epoxy resin and anhydride curing agent. The first adhesive comprising epoxy resin and anhydride curing agent is filled between the spherical diamonds and between the spherical diamonds and the boron carbide plate, so that these are firmly bonded to each other. The reason for selecting epoxy resin and adding anhydride curing agent is that epoxy resin itself has a very high bonding strength and is very suitable for such materials that are subject to strong impact; moreover, epoxy resin is a polymer composed of epoxy groups, which can react with anhydride curing agent to form a cross-linked network structure; the bonding layer formed by epoxy resin can disperse the impact force of the bullet, because the cross-linked network structure can absorb the impact energy and disperse the energy into a larger area, thereby reducing stress concentration; at the same time, during the curing process, epoxy resin will form some tiny protrusions or grooves in the three-dimensional cross-linked network due to chemical reactions between molecules or volume shrinkage of the material. These protrusions or grooves constitute tiny mechanical interlocking points, which enhance the connection between the spherical diamond and the matrix material.
[0015] It is worth noting that for curing agents mixed with epoxy resin, although amine curing agents are also an option, anhydride curing agents provide higher thermal stability, chemical stability and mechanical properties than amine curing agents; epoxy groups react with carboxyl groups in anhydride to form ester bonds, while amine groups react with epoxy groups to form ether bonds. In comparison, ester bonds have better thermal stability and chemical stability; and, among all types of curing agents, anhydride curing agents have longer carbon chains and lower activity, which helps to form a more uniform and delicate cross-linked network during the curing process, which can better disperse stress and thus improve the overall strength and impact resistance of the material. In contrast, amine curing agents are more likely to form a more uneven and rough cross-linked network during the curing process due to their higher activity. Since high temperatures may be generated when impacted by high-speed objects, forming an epoxy resin bonding layer that is resistant to high temperatures and has good impact resistance is more beneficial to improving the overall firmness and protective performance of the composite ceramic plate. Therefore, it is more appropriate to use anhydride curing agents.
[0016] The first binder further comprises reinforcing fibers, which include one or more of carbon fibers and glass fibers. The addition of reinforcing fibers can significantly improve the mechanical properties of the first binder, enhance its strength and toughness, and help improve the impact resistance of the entire composite material; it can also effectively improve the crack resistance of the first binder, prevent cracks from occurring when impacted, and thus maintain the overall structural integrity of the composite material.
[0017] Preferably, a second adhesive is also included, a second groove is provided on the inner wall of the foam aluminum plate, the spherical diamond can be embedded in the second groove, the spherical diamond is fixedly connected to the second groove through the second adhesive, and the second adhesive is silicone rubber. The hole structure of the foam aluminum provides a large surface area, which increases the contact area between the spherical diamond and the foam aluminum, and helps to improve the bonding strength. Silicone rubber is used to bond the spherical diamond to the foam aluminum plate, because silicone rubber has good flexibility compared to other adhesives, can adapt to the structure of the holes of the foam aluminum plate, and provide a buffering effect, and the elastic modulus of silicone rubber is low, which helps to absorb impact energy.
[0018] Preferably, an elastic layer is further included, the elastic layer being fixedly connected to the side of the foam aluminum plate facing away from the diamond layer, and the elastic layer being made of rubber or polyurea elastomer. In this way, the elastic layer made of rubber or polyurea elastomer can effectively absorb and disperse the residual impact energy, minimize the impact on people or objects, and further improve the anti-penetration ability of the composite ceramic plate.
[0019] Preferably, aramid fibers are also included, and the aramid fibers are coated on the surface and side of the boron carbide ceramic plate and the elastic layer. Aramid fibers have excellent strength and toughness, can initially block high-speed flying objects, and reduce the damage to the inner layer structure caused by impact force; and aramid fibers have high wear resistance, can protect the surface of the internal composite material from wear and tear, and extend its service life. It is worth noting that the aramid fibers coated on the outer layer can prevent the internal material from scattering after being broken, ensuring that the composite ceramic plate can still maintain a certain structural integrity after being damaged.
[0020] Preferably, the surface of the boron carbide ceramic plate is coated with an anti-corrosion coating, and the anti-corrosion coating is a boron nitride coating. The anti-corrosion coating can prevent the boron carbide ceramic plate from being corroded and oxidized, reduce surface wear, and extend the service life of the boron carbide ceramic plate. It is worth noting that the reason for selecting the boron nitride coating is that the thermal expansion coefficients of boron nitride and boron carbide are similar, which helps to reduce the stress caused by thermal expansion and contraction, thereby improving the thermal stability of the overall structure, and boron nitride has good thermal conductivity, which can effectively transfer heat from the surface of the boron carbide plate, reduce the thermal stress caused by heat accumulation, and avoid the accumulation of thermal stress causing the boron carbide ceramic plate to crack.
[0021] In summary, such an enhanced anti-penetration composite boron carbide ceramic plate adds a diamond layer composed of multiple spherical diamonds between the boron carbide ceramic plate and the foam aluminum plate to deflect or even break objects that penetrate into the ceramic plate at high speed, thereby effectively improving the anti-penetration ability of the composite boron carbide ceramic plate. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0023] Figure 1 This is a schematic diagram of the structure of the enhanced anti-penetration composite boron carbide ceramic plate of the present invention;
[0024] Figure 2 for Figure 1 A partial enlarged view of the part marked in the middle.
[0025] In the figure, 1-boron carbide ceramic plate; 11-first groove; 2-foam aluminum plate; 21-second groove; 3-diamond layer; 31-spherical diamond; 32-first adhesive; 4-second adhesive; 5-elastic layer; 6-aramid fiber; 7-anti-corrosion coating. DETAILED DESCRIPTION
[0026] The specific embodiments of the present invention are further described below in conjunction with the accompanying drawings. It should be noted that the description of these embodiments is used to help understand the present invention, but does not constitute a limitation of the present invention. In addition, the technical features involved in the various embodiments of the present invention described below can be combined with each other as long as they do not conflict with each other.
[0027] Reference Figure 1 and Figure 2 As shown, an enhanced anti-penetration composite boron carbide ceramic plate comprises a boron carbide ceramic plate 1 and a foam aluminum plate 2, a diamond layer 3 is further arranged between the boron carbide ceramic plate 1 and the foam aluminum plate 2, the two sides of the diamond layer 3 are respectively fixedly connected to the boron carbide ceramic plate 1 and the foam aluminum plate 2, the diamond layer 3 comprises spherical diamonds 31 and a first adhesive 32 for bonding the spherical diamonds 31 to each other, the adjacent spherical diamonds 31 are bonded to each other, and the first adhesive 32 is filled in the gaps between the spherical diamonds 31.
[0028] Although the boron carbide ceramic plate 1 has a high hardness, it is easy to crack and lose its blocking effect when impacted by high-speed flying objects such as projectiles, and high-speed flying objects have a high probability of penetrating through the boron carbide ceramic plate 1 and continuing to penetrate. Therefore, in the solution of the present invention, the diamond layer 3 is compounded into the boron carbide ceramic plate 1 to further prevent objects from penetrating.
[0029] Diamond is the hardest substance in nature, which can effectively resist the penetration of high-speed impact objects. Diamond has low density and excellent thermal conductivity, which makes it light in weight and can quickly dissipate the heat generated during the impact. The diamond layer 3 in the present invention is composed of spherical diamonds 31, and the surface of the spherical diamonds 31 is arc-shaped and has extremely high hardness. When the projectile hits, it can effectively change its motion trajectory, causing the projectile to deflect or break, thereby reducing the penetration of the projectile; wherein, the spherical diamonds 31 are bonded to each other, thereby forming a high-density structure, which increases the overall strength and rigidity of the material. The gaps between the spherical diamonds 31 are filled with the first adhesive 32, which further improves the integrity and impact resistance of the material.
[0030] In addition, it is worth noting that after the outer anti-penetration material is damaged, it is easy to cause further damage to the internal anti-impact material, so it is necessary to add a material layer that can provide a certain structural strength and absorb impact force to provide additional support and preliminary impact force absorption function to the composite ceramic plate as a whole. Usually, the material layer with this performance will use solid metal plate or polyethylene foam or foam aluminum plate 2, but the weight of solid metal plate is large, which does not meet the lightweight design requirements of bulletproof ceramics. Although polyethylene foam is light and has certain energy absorption performance, its impact strength is poor and it is easy to break when subjected to strong impact. Therefore, it is more appropriate to use a foam aluminum plate 2 that is light in weight and has good impact resistance. Therefore, in the present invention, a foam aluminum plate 2 is arranged behind the diamond layer 3; firstly, the density of the foam aluminum plate 2 is relatively low, so its weight is relatively light; secondly, as an aluminum material, the foam aluminum plate 2 has a certain toughness, which enables it to deform and not break easily when impacted, thereby helping to maintain the structural integrity of the foam aluminum plate 2 to provide additional support; importantly, when impacted, the holes in the foam aluminum will collapse, which effectively converts the impact energy into the energy of material deformation, realizing the function of the foam aluminum plate 2 to absorb a large amount of impact energy, thereby reducing the impact force transmitted to the inside and improving the overall energy absorption capacity of the ceramic plate.
[0031] Furthermore, the diamond layer 3 is provided with at least two layers, and the spherical diamonds 31 of each layer are stuck in the gap between two spherical diamonds 31 of the adjacent layer, so that a stable triangular structure is formed between the adjacent spherical diamonds 31. In this way, by forming a stable triangular structure, the structural stability and overall strength of the diamond layer 3 can be significantly improved, and the stress can be effectively dispersed to reduce the risk of local damage; the mutual contact between the multiple spherical diamonds 31 can not only play a role of mutual support, but also better absorb and disperse the impact energy, thereby reducing the impact on a single diamond and improving the ballistic performance of the entire composite material.
[0032] Reference Figure 2As shown, further, a first groove 11 is provided on the inner wall of the boron carbide ceramic plate 1, the inner wall of the boron carbide ceramic plate 1 and the first groove 11 are both sandblasted, the spherical diamond 31 can be embedded in the first groove 11, and the spherical diamond 31 is fixedly connected to the first groove 11 through a first adhesive 32. Even if the spherical diamond 31 cracks after being impacted, the integrity of the composite ceramic plate will not be affected due to the supporting bonding effect of the groove sidewall and the adhesive and the mutual support of the surrounding spherical diamonds 31.
[0033] It is worth mentioning that the sandblasting process can increase the surface roughness of the inner wall of the boron carbide ceramic plate 1 and the first groove 11, thereby improving the adhesion of the first adhesive 32, and making the connection between the spherical diamond 31 and the first groove 11 more firmly. In this way, when subjected to a high-speed impact by an object, the spherical diamond 31 is not easily deflected, and can better play its role, change the movement direction of the impacting object, and thus reduce the risk of penetration.
[0034] Furthermore, the depth of the first groove 11 is the same as the radius of the spherical diamond 31. In this way, the spherical diamond 31 can be firmly connected to the boron carbide ceramic plate 1, reducing the risk of the spherical diamond 31 falling off or shifting when impacted, while avoiding affecting the overall thickness of the boron carbide ceramic plate 1.
[0035] Furthermore, the first adhesive 32 includes epoxy resin and anhydride curing agent. The first adhesive 32 containing epoxy resin and anhydride curing agent is filled between the spherical diamonds 31 and between the spherical diamonds 31 and the boron carbide plate, so that these are firmly bonded to each other. The reason for selecting epoxy resin and adding anhydride curing agent is that epoxy resin itself has a very high bonding strength and is very suitable for such materials that are subject to strong impact; moreover, epoxy resin is a polymer composed of epoxy groups (-O-CH-CH-O-), and these epoxy groups can react with anhydride curing agent to form a cross-linked network structure; the bonding layer formed by epoxy resin can disperse the impact force of the bullet, because the cross-linked network structure can absorb the impact energy and disperse the energy into a larger area, thereby reducing stress concentration; at the same time, during the curing process, epoxy resin will form some tiny protrusions or grooves in the three-dimensional cross-linked network due to chemical reactions between molecules or volume shrinkage of the material. These protrusions or grooves constitute tiny mechanical interlocking points, which enhance the connection between the spherical diamonds 31 and the matrix material.
[0036] It is worth noting that for curing agents mixed with epoxy resin, although amine curing agents are also an option, anhydride curing agents provide higher thermal stability, chemical stability and mechanical properties than amine curing agents; epoxy groups react with carboxyl groups in anhydride to form ester bonds, while amine groups react with epoxy groups to form ether bonds. In comparison, ester bonds have better thermal stability and chemical stability; and, among all types of curing agents, anhydride curing agents have longer carbon chains and lower activity, which helps to form a more uniform and delicate cross-linked network during the curing process, which can better disperse stress and thus improve the overall strength and impact resistance of the material. In contrast, amine curing agents are more likely to form a more uneven and rough cross-linked network during the curing process due to their higher activity. Since high temperatures may be generated when impacted by high-speed objects, forming an epoxy resin bonding layer that is resistant to high temperatures and has good impact resistance is more beneficial to improving the overall firmness and protective performance of the composite ceramic plate. Therefore, it is more appropriate to use anhydride curing agents.
[0037] The first binder 32 further includes reinforcing fibers, which include one or more of carbon fibers and glass fibers. The addition of reinforcing fibers can significantly improve the mechanical properties of the first binder 32, enhance its strength and toughness, and help improve the impact resistance of the entire composite material; it can also effectively improve the crack resistance of the first binder 32, prevent cracks from occurring when impacted, and thus maintain the overall structural integrity of the composite material.
[0038] Furthermore, a second adhesive 4 is also included. A second groove 21 is provided on the inner wall of the foam aluminum plate 2. The spherical diamond 31 can be embedded in the second groove 21. The spherical diamond 31 is fixedly connected to the second groove 21 through the second adhesive 4. The second adhesive 4 is silicone rubber. The pore structure of the foam aluminum provides a large surface area, which increases the contact area between the spherical diamond 31 and the foam aluminum, and helps to improve the bonding strength. Silicone rubber is used to bond the spherical diamond 31 to the foam aluminum plate 2, because silicone rubber has good flexibility compared to other adhesives, can adapt to the structure of the pores of the foam aluminum plate 2, and provide a buffering effect. In addition, the elastic modulus of silicone rubber is low, which helps to absorb impact energy.
[0039] Furthermore, it also includes an elastic layer 5, which is fixedly connected to the side of the foam aluminum plate 2 facing away from the diamond layer 3, and the elastic layer 5 is rubber or polyurea elastomer. In this way, the elastic layer 5 made of rubber or polyurea elastomer can effectively absorb and disperse the residual impact energy, reduce the impact on people or objects as much as possible, and further improve the anti-penetration ability of the composite ceramic plate. It should be noted that the elastic layer 5 and the foam aluminum plate 2 can be fixedly connected to each other by epoxy resin or polyurethane adhesive.
[0040] Furthermore, it also includes aramid fiber 6, which is coated on the surface and side of the boron carbide ceramic plate 1 and the elastic layer 5. The aramid fiber 6 has excellent strength and toughness, can initially block high-speed flying objects, and reduce the damage of the impact force to the inner layer structure; and the aramid fiber 6 has high wear resistance, can protect the surface of the internal composite material from wear and tear, and prolong its service life.
[0041] It is worth noting that the aramid fiber 6 coated on the outer layer can prevent the internal material from scattering after being broken, ensuring that the composite ceramic plate can still maintain a certain structural integrity after being damaged.
[0042] Furthermore, the surface of the boron carbide ceramic plate 1 is coated with an anti-corrosion coating 7, which is a boron nitride coating. The anti-corrosion coating 7 can prevent the boron carbide ceramic plate 1 from being corroded and oxidized, reduce surface wear, and extend the service life of the boron carbide ceramic plate 1.
[0043] It is worth noting that the reason for choosing boron nitride coating is that the thermal expansion coefficients of boron nitride and boron carbide are similar, which helps to reduce the stress caused by thermal expansion and contraction, thereby improving the thermal stability of the overall structure. In addition, boron nitride has good thermal conductivity and can effectively transfer heat from the surface of the boron carbide plate, reducing the thermal stress caused by heat accumulation and avoiding the cracking of the boron carbide ceramic plate 1 caused by the accumulation of thermal stress.
[0044] In summary, such an enhanced anti-penetration composite boron carbide ceramic plate, by adding a diamond layer 3 composed of multiple spherical diamonds 31 between the boron carbide ceramic plate 1 and the foam aluminum plate 2, can deflect or even break objects that penetrate into the ceramic plate at high speed, thereby effectively improving the anti-penetration ability of the composite boron carbide ceramic plate 1.
[0045] The embodiments of the present invention are described in detail above with reference to the accompanying drawings, but the present invention is not limited to the described embodiments. For those skilled in the art, various changes, modifications, substitutions and variations of these embodiments are made without departing from the principles and spirit of the present invention, and still fall within the scope of protection of the present invention.
Claims
1. An enhanced anti-penetration composite boron carbide ceramic plate, comprising a boron carbide ceramic plate (1) and a foamed aluminum plate (2), characterized in that: A diamond layer (3) is further provided between the boron carbide ceramic plate (1) and the foamed aluminum plate (2); two surfaces of the diamond layer (3) are respectively fixedly connected to the boron carbide ceramic plate (1) and the foamed aluminum plate (2); the diamond layer (3) comprises spherical diamonds (31) and a first adhesive (32) for bonding the spherical diamonds (31) to each other; adjacent spherical diamonds (31) are bonded to each other, and the first adhesive (32) is filled in the gaps between the spherical diamonds (31).
2. The enhanced anti-penetration composite boron carbide ceramic plate according to claim 1 is characterized in that: The diamond layer (3) is provided with at least two layers, and the spherical diamonds (31) of each layer are stuck in the gap between two spherical diamonds (31) of the adjacent layer, so that a stable triangular structure is formed between adjacent spherical diamonds.
3. The enhanced anti-penetration composite boron carbide ceramic plate according to claim 2 is characterized in that: A first groove (11) is provided on the inner wall of the boron carbide ceramic plate (1); the inner wall of the boron carbide ceramic plate (1) and the first groove (11) are both sandblasted; the spherical diamond (31) can be embedded in the first groove (11); and the spherical diamond (31) is fixedly connected to the first groove (11) via a first adhesive (32).
4. The enhanced anti-penetration composite boron carbide ceramic plate according to claim 3 is characterized in that: The depth of the first groove (11) is the same as the radius of the spherical diamond (31).
5. The enhanced anti-penetration composite boron carbide ceramic plate according to claim 1 is characterized in that: The first adhesive (32) includes epoxy resin and anhydride curing agent.
6. The enhanced anti-penetration composite boron carbide ceramic plate according to claim 5, characterized in that: The first binder (32) further comprises reinforcing fibers, wherein the reinforcing fibers comprise one or more of carbon fibers and glass fibers.
7. The enhanced anti-penetration composite boron carbide ceramic plate according to claim 1 is characterized in that: The invention also comprises a second adhesive (4), a second groove (21) is arranged on the inner wall of the foam aluminum plate (2), the spherical diamond (31) can be embedded in the second groove (21), the spherical diamond (31) is fixedly connected to the second groove (21) via the second adhesive (4), and the second adhesive (4) is silicone rubber.
8. The enhanced anti-penetration composite boron carbide ceramic plate according to claim 3 is characterized in that: It also comprises an elastic layer (5), wherein the elastic layer (5) is fixedly connected to the side of the foam aluminum plate (2) facing away from the diamond layer (3), and the elastic layer (5) is rubber or polyurea elastomer.
9. The enhanced anti-penetration composite boron carbide ceramic plate according to claim 8, characterized in that: It also comprises aramid fibers (6), wherein the aramid fibers (6) are coated on the surface and side surfaces of the boron carbide ceramic plate (1) and the elastic layer (5).
10. The enhanced anti-penetration composite boron carbide ceramic plate according to claim 9, characterized in that: The surface of the boron carbide ceramic plate (1) is coated with an anti-corrosion coating (7), and the anti-corrosion coating (7) is a boron nitride coating.
Citation Information
Patent Citations
Lightweight composite armor and manufacturing method thereof
CN111811324A