Production control method and device for Ti-Br composite photocatalytic assembly
By optimizing the temperature control of the TiO2-eosin solution and the drying of the components, the problem of continuous and efficient production of photocatalytic components was solved, improving production efficiency and quality.
Patent Information
- Application Number
- CN202411271974.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-11
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-09-11
AI Technical Summary
Existing technologies make it difficult to achieve continuous and efficient production of photocatalytic components under light-protected conditions.
By controlling the temperature and time of the TiO2-eosin solution in the immersion tank, and combining this with a first-in-first-out drying method for the components, the conveying and cleaning processes of the processing unit are optimized, enabling continuous production of Ti-Br composite photocatalytic components.
This improved the production efficiency of Ti-Br composite photocatalytic modules, avoided the waste of TiO2 and eosin, and ensured the stability and quality of the production process.
Smart Images

Figure CN118988204A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of production control technology, and more specifically, to a production control method and device for a Ti-Br composite photocatalytic component. Background Art
[0002] The reaction mechanism of photocatalytic technology is that the photocatalyst itself absorbs light energy while adsorbing the catalytic target, and uses the photogenerated electrons and holes generated by light excitation to react with the target pollutants in a photochemical reaction. Photocatalytic technology can almost completely mineralize organic substances and some inorganic substances that are harmful to the human body and the environment into simple inorganic substances such as CO2 and H2O without selectivity within a sufficient reaction time. At present, there are no photocatalytic products for air purification in open environments such as tunnels, highways, landfills and chemical plants. For example, pollutants in urban roads include organic and inorganic particles in automobile exhaust, a mixture of rainfall and ground sediment, etc. These pollutants accumulate in the isolation belts, service areas and living areas on both sides of the road for many years, affecting the appearance of the road and the air quality around the road. Existing literature reports only photocatalytic research and development materials with tunnels as the application situation, and construction methods for adding photocatalytic additives to road construction materials. Existing technologies and research and development samples have not yet solved the convenience and universality of on-site construction.
[0003] Patent application CN115845828A (application number: CN202211657170.8) provides a photocatalytic component, which includes an attached matrix, and a Ti-Br composite photocatalytic material is attached to the surface of the attached matrix. The Ti-Br composite photocatalytic material is prepared by compounding a visible light photosensitive material and nano-scale TiO2 powder. The visible light photosensitive material is eosin, and the mass ratio of TiO2 powder to eosin is (1-50):1. The particle size of the TiO2 powder is 10-40nm. The attached matrix is an iron-based mesh, an aluminum-based mesh or a stainless steel-based mesh, and a frame is fixed to the periphery of the attached matrix. The photocatalytic component in patent application CN115845828A is difficult to produce continuously and efficiently during production. Summary of the invention
[0004] The purpose of this application is to provide a production control method and device for a Ti-Br composite photocatalytic component, which solves the technical problem of difficulty in ensuring continuous and efficient production of photocatalytic components under light-proof conditions, and achieves the technical effect of ensuring continuous and efficient production of photocatalytic components under light-proof conditions.
[0005] An embodiment of the present application provides a production control method for a Ti-Br composite photocatalytic component, the method comprising: controlling the TiO2-eosin solution in an immersion and attachment tank in which a treatment unit is immersed to heat up to a preset temperature within a first time period and keeping stirring the TiO2-eosin solution within the first time period, continuing to immerse the treatment unit with the heated TiO2-eosin solution, and obtaining the immersion and attachment time for continuing to immerse the treatment unit with the heated TiO2-eosin solution; wherein each treatment unit comprises a bracket carrying an aluminum-based mesh; when the first immersion and attachment time is greater than an immersion and attachment time threshold, controlling the first treatment unit in the first immersion and attachment tank corresponding to the first immersion and attachment time to be transported to a cleaning component, and controlling the cleaning component to clean the bracket of the first treatment unit; controlling the first treatment unit after cleaning by the cleaning component to be transported to a drying component for drying for a preset time, and controlling the drying component to discharge multiple treatment units in the drying component in a first-in-first-out manner.
[0006] In one possible implementation, the method also includes: obtaining the number of processing units of all processing units in the drying component, and when the number of processing units is less than the first number of processing units, reducing the soaking attachment time threshold by the first soaking attachment time threshold, and reducing the first time period by the second time period; when the number of processing units is greater than the second number of processing units, increasing the soaking attachment time threshold by the second soaking attachment time threshold, and increasing the first time period by the second time period; wherein the first number of processing units is less than the second number of processing units.
[0007] In another possible implementation, the method also includes: obtaining the amount of time processing units entering the drying component in sequence; wherein the amount of time processing unit entry includes multiple moment values and the amount of processing unit entry corresponding to each moment value; through the drying component temperature prediction model, according to the amount of time processing unit entry and the current drying temperature in the drying component, determine the time drying temperature of the drying component in the future time period; wherein the time drying temperature includes multiple moment values and the drying temperature corresponding to each moment value; when the first drying temperature corresponding to the first moment value in the future time period is less than the preset drying temperature, the drying temperature is adjusted to the preset drying temperature in the third time period before the first moment value.
[0008] In another possible implementation, the method also includes: when the first time value is reached, obtaining the first actual drying temperature and the first actual processing unit entry amount corresponding to the first time value, when the first actual processing unit entry amount and the first processing unit entry amount in the timing processing unit entry amount do not match, and when the first actual drying temperature is lower than the preset drying temperature, adjusting the drying temperature to the preset drying temperature.
[0009] In another possible implementation, when the first actual drying temperature is lower than the preset drying temperature, the drying temperature is adjusted to the preset drying temperature, including: determining the drying temperature difference between the first actual drying temperature and the preset drying temperature, taking the product of the drying temperature difference and the drying temperature adjustment coefficient as the temperature adjustment time, and uniformly adjusting the drying temperature to the preset drying temperature within the temperature adjustment time.
[0010] In another possible implementation, the drying temperature adjustment coefficient is determined by the following method: obtaining the remaining drying time of each processing unit being dried in the drying component, determining the ratio of the remaining drying time of each processing unit to the total drying time, and using the sum of the ratios of the remaining drying time of all processing units to the total drying time as the drying temperature adjustment coefficient.
[0011] The embodiment of the present application also provides a production device for a Ti-Br composite photocatalytic component. The production device for the Ti-Br composite photocatalytic component adopts the method described in any of the above items when working, including a drying component, a cleaning component, multiple immersion and attachment tanks, a conveying component and a control component; the drying component is used to dry multiple processing units, each processing unit includes a bracket carrying an aluminum-based mesh, and the drying component is provided with a drying heating component and a drying temperature measuring component; the cleaning component is used to clean the bracket of the processing unit; the immersion and attachment tank is used to hold the TiO2-eosin solution and immerse the processing unit, and the immersion and attachment tank is provided with a solution heating component, a solution temperature measuring component and a stirring component, the solution heating component is used to heat the TiO2-eosin solution, the solution temperature measuring component is used to measure the temperature of the TiO2-eosin solution, and the stirring component is used to stir the TiO2-eosin solution; the conveying component is used to convey the processing unit through the immersion and attachment tank, the cleaning component and the drying component in sequence; the drying heating component, the drying temperature measuring component, the cleaning component, the solution heating component, the solution temperature measuring component, the stirring component and the conveying component are electrically connected to the control component respectively.
[0012] In another possible implementation, the drying component is linear, with a feed end and a discharge end respectively provided at both ends of the drying component, multiple immersion and attachment pools are arranged along the length direction of the drying component, and the cleaning component is arranged near the feed end of the drying component. The drying component uses a first-in-first-out method to discharge multiple processing units in the drying component.
[0013] In another possible implementation, it also includes a TiO2-eosin recovery component, which includes a conveying and collecting tank and a cleaning and collecting tank. The conveying track of the conveying component to the processing unit is located on one side of the multiple immersion and attachment pools, the conveying and collecting tank is arranged below the conveying track of the conveying component to the processing unit, and the cleaning and collecting tank is arranged at the bottom of the cleaning component. The solutions collected by the conveying and collecting tank and the cleaning and collecting tank are mixed and formulated into a TiO2-eosin solution with a preset concentration value, and the TiO2-eosin solution with the preset concentration value is conveyed to the multiple immersion and attachment pools through a pipeline.
[0014] In another possible implementation, a concentration detection component for detecting the concentration of the recovered TiO2-eosin solution is provided in the cleaning collection tank. The concentration detection component and the control component are electrically connected. When the concentration of the recovered TiO2-eosin solution detected by the concentration detection component is higher than a preset concentration value, the control component issues a prompt message to inspect the cleaning component.
[0015] Compared with the prior art, the embodiments of the present invention have the following beneficial effects:
[0016] An embodiment of the present application provides a production control method for a Ti-Br composite photocatalytic component, the method comprising: controlling the TiO2-eosin solution in an immersion and attachment tank in which a treatment unit is immersed to heat up to a preset temperature within a first time period and maintaining stirring of the TiO2-eosin solution within the first time period, continuing to immerse the treatment unit with the heated TiO2-eosin solution, and obtaining the immersion and attachment time for continuing to immerse the treatment unit with the heated TiO2-eosin solution; wherein each treatment unit comprises a bracket carrying an aluminum-based mesh; when the first immersion and attachment time is greater than an immersion and attachment time threshold, controlling the first treatment unit in the first immersion and attachment tank corresponding to the first immersion and attachment time to be transported to a cleaning component, and controlling the cleaning component to clean the bracket of the first treatment unit; controlling the first treatment unit after cleaning by the cleaning component to be transported to a drying component for drying for a preset time, and controlling the drying component to discharge multiple treatment units in the drying component in a first-in-first-out manner. During the production of the Ti-Br composite photocatalytic component in the embodiment of the present application, the processing unit is immersed and attached through multiple immersion and attachment pools, which can reasonably control and schedule the production process of multiple Ti-Br composite photocatalytic components, thereby improving the production efficiency of the Ti-Br composite photocatalytic component. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0018] Figure 1 A schematic flow chart of a production control method of a Ti-Br composite photocatalytic component provided in an embodiment of the present application;
[0019] Figure 2 A schematic diagram of the structure of a production device for a Ti-Br composite photocatalytic component provided in an embodiment of the present application;
[0020] Figure 3 A schematic diagram of the structure of a processing unit provided in an embodiment of the present application;
[0021] Figure 4 A schematic diagram of a control structure of a production device for a Ti-Br composite photocatalytic component provided in an embodiment of the present application;
[0022] In the figure, 1. drying component; 11. processing unit; 111. aluminum-based mesh; 112. bracket; 12. drying and heating component; 13. drying and temperature measuring component; 2. cleaning component; 3. immersion and attachment tank; 31. solution heating component; 32. solution temperature measuring component; 33. stirring component; 4. control component; 5. TiO2-eosin recovery component; 51. conveying and collecting tank; 52. cleaning and collecting tank. DETAILED DESCRIPTION
[0023] It should be understood that when used in the present specification and the appended claims, the term "comprising" indicates the presence of described features, wholes, steps, operations, elements and / or components, but does not exclude the presence or addition of one or more other features, wholes, steps, operations, elements, components and / or combinations thereof.
[0024] It should also be understood that the term “and / or” used in the specification and appended claims refers to any and all possible combinations of one or more of the associated listed items, and includes these combinations.
[0025] As used in the specification and appended claims of this application, the term "if" can be interpreted as "when" or "uponce" or "in response to determining" or "in response to detecting", depending on the context. Similarly, the phrase "if it is determined" or "if [described condition or event] is detected" can be interpreted as meaning "uponce it is determined" or "in response to determining" or "uponce [described condition or event] is detected" or "in response to detecting [described condition or event]", depending on the context.
[0026] In addition, in the description of the present application specification and the appended claims, the terms "first", "second", "third", etc. are only used to distinguish the descriptions and cannot be understood as indicating or implying relative importance.
[0027] References to "one embodiment" or "some embodiments" etc. described in the specification of this application mean that one or more embodiments of the present application include specific features, structures or characteristics described in conjunction with the embodiment. Therefore, the statements "in one embodiment", "in some embodiments", "in some other embodiments", "in some other embodiments", etc. that appear in different places in this specification do not necessarily refer to the same embodiment, but mean "one or more but not all embodiments", unless otherwise specifically emphasized in other ways. The terms "including", "comprising", "having" and their variations all mean "including but not limited to", unless otherwise specifically emphasized in other ways.
[0028] It is difficult to carry out continuous and efficient production of photocatalytic components in the prior art during production.
[0029] Based on the above reasons, an embodiment of the present application provides a production control method for a Ti-Br composite photocatalytic component, the method comprising: controlling the TiO2-eosin solution in the immersion and attachment tank in which the treatment unit is immersed to heat up to a preset temperature within a first time period and keeping stirring the TiO2-eosin solution within the first time period, continuing to immerse the treatment unit with the heated TiO2-eosin solution, and obtaining the immersion and attachment time for continuing to immerse the treatment unit with the heated TiO2-eosin solution; wherein each treatment unit comprises a bracket carrying an aluminum-based mesh; when the first immersion and attachment time is greater than the immersion and attachment time threshold, controlling the first treatment unit in the first immersion and attachment tank corresponding to the first immersion and attachment time to be transported to the cleaning component, and controlling the cleaning component to clean the bracket of the first treatment unit; controlling the first treatment unit after cleaning by the cleaning component to be transported to the drying component for drying for a preset time, and controlling the drying component to discharge the multiple treatment units in the drying component in a first-in-first-out manner. During the production of the Ti-Br composite photocatalytic component in the embodiment of the present application, the processing unit is immersed and attached through multiple immersion and attachment pools, which can reasonably control and schedule the production process of multiple Ti-Br composite photocatalytic components, thereby improving the production efficiency of the Ti-Br composite photocatalytic component.
[0030] In some scenarios, a production control method of a Ti-Br composite photocatalytic component of an embodiment of the present application can be applied to the production of Ti-Br composite photocatalytic components attached by immersion in TiO2-eosin solution, which can improve the production efficiency of the Ti-Br composite photocatalytic components.
[0031] The following is a detailed description of a production control method for a Ti-Br composite photocatalytic component provided in an embodiment of the present application with reference to specific examples.
[0032] Figure 1 A schematic diagram of a production control method of a Ti-Br composite photocatalytic component provided in an embodiment of the present application is shown in FIG. Figure 1 As shown, the method includes S110 to S130, and S110 to S130 are described in detail below.
[0033] S110, controlling the TiO2-eosin solution in the soaking and attachment pool 3 in which the processing unit 11 is soaked to heat up to a preset temperature within a first time period and maintaining stirring of the TiO2-eosin solution within the first time period, continuing to soak the processing unit 11 with the heated TiO2-eosin solution, and obtaining the soaking and attachment time for continuing to soak the processing unit 11 with the heated TiO2-eosin solution. Each processing unit 11 includes a bracket 112 carrying an aluminum-based mesh 111.
[0034] Figure 2A schematic diagram of the structure of a production device for a Ti-Br composite photocatalytic component provided in an embodiment of the present application, Figure 3 A schematic diagram of the structure of a processing unit provided in an embodiment of the present application is shown in FIG. Figure 2 and Figure 3 As shown, a production control method of a Ti-Br composite photocatalytic component provided in an embodiment of the present application is applied to control Figure 2 The production device of the Ti-Br composite photocatalytic component shown, when working, the method in the embodiment of the present application aims to improve the production efficiency of the immersion attachment and drying process of multiple processing units 11 by controlling the immersion attachment and drying process of multiple processing units 11.
[0035] During production, the general production process of the Ti-Br composite photocatalytic component is as follows: first weigh eosin and put it into pure water, stir it in the dark until it is uniform, and prepare an eosin solution with a concentration of 0.25 to 10 g / L; add 1 to 50 times the mass of TiO2 powder to the eosin solution to form a TiO2-eosin solution, take the aluminum-based mesh and immerse it in the formed TiO2-eosin solution, place it in a 30°C light-proof water bath, stir and heat it to 80°C, then keep the temperature attached for 1.5 hours, and then take out the aluminum-based mesh attached with TiO2 and eosin. The stirring and heating process is: stirring at a speed of 200r / min for 10 minutes, and the heating rate is 5°C / min. The drying process is: placing the aluminum-based mesh attached with TiO2 and eosin in a dark and dry environment for 1 hour, and the drying temperature is 100°C.
[0036] When the embodiment of the present application is working, in order to improve the production efficiency of the Ti-Br composite photocatalytic component, the TiO2-eosin solution in the immersion and attachment tank 3 in which the treatment unit 11 is immersed can be first controlled to heat up to a preset temperature within a first time period and the TiO2-eosin solution can be kept stirred within the first time period to complete the initial attachment of the TiO2-eosin solution, and then the treatment unit 11 can be continuously immersed in the heated TiO2-eosin solution to continuously attach the aluminum-based mesh.
[0037] In an embodiment of the present application, when the processing unit 11 continues to be immersed in the heated TiO2-eosin solution, the immersion and adhesion time of the processing unit 11 continued to be immersed in the heated TiO2-eosin solution is obtained, thereby realizing the control of the immersion and adhesion process of the TiO2-eosin solution.
[0038] For example, when the heated TiO2-eosin solution is reused, the heated TiO2-eosin solution can be cooled down by cooling water so as to reuse the heated TiO2-eosin solution for the production of Ti-Br composite photocatalytic components.
[0039] like Figure 3 As shown, each processing unit 11 includes a bracket 112 carrying an aluminum-based mesh 111 . In the embodiment of the present application, the bracket 112 is used to carry a plurality of aluminum-based meshes 111 to improve the efficiency of immersion and attachment of the plurality of aluminum-based meshes 111 .
[0040] Exemplarily, the first time period may be 5 minutes to 15 minutes.
[0041] Exemplarily, the soaking and attachment time may be 1 hour to 2 hours.
[0042] Illustratively, the conveying component for conveying the processing unit 11 in the embodiment of the present application may be a guide rail conveying system installed on the roof of a factory building, and the conveying component can be used to convey and transport multiple processing units 11 in an orderly manner.
[0043] Exemplarily, the conveying assembly is further configured with a lifting assembly, and the conveying assembly can control the lifting process of the processing unit 11 through the lifting assembly to achieve the lifting of the processing unit 11 in the immersion and adhesion tank 3.
[0044] S120, when the first immersion attachment time is greater than the immersion attachment time threshold, control the first processing unit in the first immersion attachment pool corresponding to the first immersion attachment time to be transported to the cleaning component 2, and control the cleaning component 2 to clean the bracket 112 of the first processing unit.
[0045] During operation, when the first immersion attachment time is greater than the immersion attachment time threshold, it means that the immersion attachment time of the aluminum-based mesh in the first immersion attachment pool has reached the time requirement of the immersion attachment time threshold, and the first processing unit in the first immersion attachment pool corresponding to the first immersion attachment time can be controlled to be transported to the cleaning component 2. The cleaning component 2 is used to clean the bracket 112 of the processing unit to avoid drying after the TiO2 and eosin are attached to the bracket 112, thereby avoiding waste of TiO2 and eosin.
[0046] When the first processing unit in the first immersion and attachment tank is transported, the cleaning component 2 can be controlled to clean the bracket 112 of the first processing unit, so as to clean the TiO 2 and eosin on the bracket 112 .
[0047] like Figure 2 As shown, a plurality of aluminum-based meshes 111 are provided on the main structure of the bracket 112. By cleaning the bracket 112, the TiO2 and eosin on the main structure of the bracket 112 can be cleaned and recovered, thereby realizing the recycling of TiO2 and eosin.
[0048] S130, controlling the first processing unit 11 cleaned by the cleaning component 2 to be transported to the drying component 1 for drying for a preset time, and controlling the drying component 1 to discharge the multiple processing units 11 in the drying component 1 in a first-in-first-out manner.
[0049] During drying, the first processing unit after being cleaned by the cleaning component 2 can be controlled to be transported to the drying component 1 for drying for a preset time, so as to achieve drying and drying of TiO2 and eosin attached to the aluminum-based net.
[0050] When the drying component 1 is working, the drying component 1 can be controlled to discharge the multiple processing units 11 in the drying component 1 in a first-in-first-out manner, so that the processing unit 11 with a long drying time is discharged first, and the processing unit 11 with a short drying time can continue drying, thereby improving the control effect of the drying process.
[0051] Exemplarily, the preset drying time of the drying component 1 may be 0.8h to 1.5h.
[0052] To sum up, since the demand for Ti-Br composite photocatalytic assemblies is large when they are used on the road, and the production efficiency of the Ti-Br composite photocatalytic assemblies is required to be high, in the production process of the Ti-Br composite photocatalytic assemblies, the processing units are immersed and attached through multiple immersion and attachment pools, so that the production processes of multiple Ti-Br composite photocatalytic assemblies can be reasonably controlled and scheduled, thereby improving the production efficiency of the Ti-Br composite photocatalytic assemblies.
[0053] At the same time, the bracket of the processing unit is cleaned to avoid drying after the TiO2 and eosin are attached to the bracket, thereby avoiding waste of TiO2 and eosin.
[0054] At the same time, the brackets of multiple processing units can be cleaned by one cleaning component, which improves the utilization rate of the cleaning component and improves the utilization efficiency of the cleaning component during the production of the Ti-Br composite photocatalytic component.
[0055] In some implementations, the above method further includes: obtaining the number of processing units of all processing units 11 in the drying component 1, and when the number of processing units is less than the first number of processing units, reducing the soaking and attachment time threshold by the first soaking and attachment time threshold, and reducing the first time period by the second time period. When the number of processing units is greater than the second number of processing units, increasing the soaking and attachment time threshold by the second soaking and attachment time threshold, and increasing the first time period by the second time period. The first number of processing units is less than the second number of processing units.
[0056] When controlling the drying process, the processing unit number of all processing units 11 in the drying component 1 can be obtained, and the processing unit number represents the number of processing units that are drying in the drying component 1 .
[0057] After obtaining the number of processing units, when the number of processing units is less than the first number of processing units, it means that the number of processing units is small, the temperature and humidity in the drying component may increase, which may have an adverse effect on the drying quality of the drying process, and because the drying time is long, the immersion attachment time threshold can be reduced by the first immersion attachment time threshold to increase the number of processing units entering the drying component in a short time. At the same time, the first time period can be reduced by the second time period to increase the speed of the immersion process, so as to increase the number of processing units in the drying component and ensure the stability of the drying environment in the drying component.
[0058] Exemplarily, the first soaking attachment time threshold may be 10% to 20% of the soaking attachment time threshold.
[0059] Exemplarily, the second time period may be 20% to 30% of the first time period.
[0060] When the drying environment is unstable, the TiO2 and eosin adhesion layers on the surface of the Ti-Br composite photocatalytic component may crack, resulting in poor production quality of the TiO2 and eosin adhesion layers and affecting the production effect of TiO2 and eosin.
[0061] After obtaining the number of processing units, when the number of processing units is greater than the second number of processing units, and the first number of processing units is less than the second number of processing units, it means that the number of processing units in the drying component is large. In order to avoid excessive humidity and low temperature in the drying component, the immersion attachment time threshold can be increased by the second immersion attachment time threshold to reduce the number of processing units entering the drying component, and the first time period can be increased by the second time period to reduce the heating rate in the immersion attachment pool, which can slow down the speed at which the processing units enter the drying component to ensure the stability of the environment in the drying component and avoid affecting the drying quality.
[0062] Exemplarily, the number of the first processing units may be 80% of the rated drying number of the drying component, and the number of the second processing units may be 120% of the rated drying number of the drying component.
[0063] To sum up, when the number of processing units is small, in order to ensure the drying quality, and because the drying time is long, the immersion attachment time threshold can be reduced by the first immersion attachment time threshold, and the first time period can be reduced by the second time period to increase the speed of the immersion process, so as to increase the number of processing units in the drying component and improve the drying environment stability and drying quality in the drying component.
[0064] At the same time, when the number of processing units in the drying component is large, the immersion attachment time threshold is increased by the second immersion attachment time threshold, and the first time period is increased by the second time period, which can ensure the stability of the environment in the drying component and avoid affecting the drying quality.
[0065] At the same time, when the number of processing units in the drying component is large, increasing the first time period by the second time period can reduce the heating rate in the immersion attachment pool, thereby improving the uniformity of TiO2 and eosin attached to the aluminum base mesh and improving the production quality of the Ti-Br composite photocatalytic component.
[0066] When the cleaning component 2 cleans the processing unit 11, the temperature of the processing unit 11 drops significantly. Therefore, when the processing unit 11 enters the drying component 1, it may have a significant impact on the temperature inside the drying component 1. The temperature inside the drying component 1 needs to be controlled and adjusted in time.
[0067] In some implementations, the above method further includes S210 to S220, and S210 to S220 are described in detail below.
[0068] S210, obtaining the entry amount of the sequential processing units that sequentially enter the drying component 1. The entry amount of the sequential processing units includes a plurality of time values and the entry amount of the processing units corresponding to each time value.
[0069] During drying, in order to stably control the drying environment in the drying component, the entry amount of the timing processing unit that enters the drying component 1 in sequence can be obtained. The entry amount of the timing processing unit includes multiple moment values and the entry amount of the processing unit corresponding to each moment value. The working environment of the drying component can be stably controlled through the entry amount of the timing processing unit.
[0070] Exemplarily, the time sequence processing unit entry quantity may include multiple time values within 1 hour and the processing unit entry quantity corresponding to each time value. The time sequence processing unit can reflect the number of processing units entering the drying component at different times.
[0071] S220, using the drying component temperature prediction model, determine the sequential drying temperature of the drying component 1 in the future time period according to the sequential processing unit input amount and the current drying temperature in the drying component 1. The sequential drying temperature includes multiple time values and the drying temperature corresponding to each time value.
[0072] When controlling the drying environment, the drying component temperature prediction model can be used to determine the time-series drying temperature of the drying component 1 in the future time period according to the input amount of the timing processing unit and the current drying temperature in the drying component 1. The time-series drying temperature includes multiple moment values and the drying temperature corresponding to each moment value, thereby realizing the prediction of the drying temperature in the drying component 1 in the future time period.
[0073] Exemplarily, the drying component temperature prediction model may be a LSTM-based time series temperature prediction model.
[0074] Exemplarily, when the timing processing unit entry volume is multiple moment values within 1 hour and each moment value corresponds to the processing unit entry volume, when the current drying temperature in the drying component 1 is 110°C, the timing drying temperature of the drying component 1 in the future time period can be the timing drying temperature in the drying component 1 in the next 1 hour.
[0075] S230: When the first drying temperature corresponding to the first time value in the future time period is lower than the preset drying temperature, the drying temperature is adjusted to the preset drying temperature in a third time period before the first time value.
[0076] After obtaining the sequential drying temperature of the drying component 1 in the future time period, when the first drying temperature corresponding to the first moment value in the future time period is less than the preset drying temperature, it means that the drying temperature of the first moment value may be too low. At this time, the drying temperature can be adjusted to the preset drying temperature in the third time period before the first moment value to achieve stable adjustment of the drying temperature and avoid affecting the drying quality.
[0077] Exemplarily, when the drying temperature is adjusted to the preset drying temperature within the third time period before the first time value, the drying temperature can be adjusted to the preset drying temperature within the third time period before the first time value by the heating component, and the third time period can be 5 minutes to 10 minutes.
[0078] To summarize, through the drying component temperature prediction model, the sequential drying temperature of the drying component in the future time period is predicted according to the input amount of the sequential processing unit and the current drying temperature in the drying component. When the drying temperature in the future time period is too low, the drying temperature is adjusted in advance, thereby ensuring the control effect on the stability of the drying effect of the processing unit, and being able to improve the drying stability of the drying component in the future time period.
[0079] In some implementations, the above method also includes: when the first time value is reached, obtaining the first actual drying temperature and the first actual processing unit entry amount corresponding to the first time value, when the first actual processing unit entry amount and the first processing unit entry amount in the timing processing unit entry amount do not match, and when the first actual drying temperature is lower than the preset drying temperature, adjusting the drying temperature to the preset drying temperature.
[0080] When adjustment is performed using the method in S130 described above, when the first moment value is actually reached, the first actual drying temperature and the first actual processing unit entry amount corresponding to the first moment value can be obtained, and then the drying temperature can be controlled in real time according to the first actual drying temperature and the first actual processing unit entry amount corresponding to the first moment value, thereby improving the control effect of the drying temperature.
[0081] During drying, when the first actual processing unit input quantity and the first processing unit input quantity in the timing processing unit input quantity do not match, it means that the first actual processing unit input quantity in actual production and the expected first processing unit input quantity do not match, and the drying temperature may deviate from the expected drying temperature, and the drying temperature needs to be re-monitored.
[0082] When the drying temperature is monitored, when the first actual drying temperature is lower than the preset drying temperature, it indicates that the first actual drying temperature in the drying component is too low. The drying temperature can be adjusted to the preset drying temperature to achieve dynamic adjustment of the drying temperature.
[0083] Exemplarily, the preset drying temperature may be 100°C.
[0084] To sum up, when the first time value is actually reached, when the first actual processing unit entry amount and the first processing unit entry amount in the timing processing unit entry amount do not match, and when the first actual drying temperature is lower than the preset drying temperature, dynamically adjusting the drying temperature can improve the control effect of the stability of the drying temperature.
[0085] In some implementations, in the above method, when the first actual drying temperature is lower than the preset drying temperature, the drying temperature is adjusted to the preset drying temperature, including: determining the drying temperature difference between the first actual drying temperature and the preset drying temperature, taking the product of the drying temperature difference and the drying temperature adjustment coefficient as the temperature adjustment time, and uniformly adjusting the drying temperature to the preset drying temperature within the temperature adjustment time.
[0086] When adjusting the drying temperature, since the drying temperature adjustment speed in the drying component is slow, in order to ensure the drying quality, the drying temperature difference between the first actual drying temperature and the preset drying temperature can be determined, and the drying temperature difference represents the amplitude of the drying temperature that needs to be adjusted.
[0087] Exemplarily, the drying temperature difference may be 10°C to 30°C.
[0088] After determining the drying temperature difference, the product of the drying temperature difference and the drying temperature adjustment coefficient can be used as the temperature adjustment time. The temperature adjustment time is the time corresponding to the planned temperature adjustment process. The drying temperature is uniformly adjusted to the preset drying temperature within the temperature adjustment time.
[0089] To sum up, when the drying temperature adjustment coefficient remains unchanged, the greater the drying temperature difference, the longer the temperature adjustment time, which can ensure that the temperature fluctuation amplitude in the drying component is reduced, avoiding the large temperature fluctuation amplitude of the processing unit in the drying component, which may cause the TiO2 and eosin adhesion layers attached to the aluminum base mesh to crack, thereby improving the quality of the TiO2 and eosin adhesion layers.
[0090] In some implementations, the drying temperature adjustment coefficient is determined by the following method: obtaining the remaining drying time of each processing unit being dried in the drying component, determining the ratio of the remaining drying time of each processing unit to the total drying time, and using the sum of the ratios of the remaining drying time of all processing units to the total drying time as the drying temperature adjustment coefficient.
[0091] When determining the drying temperature adjustment coefficient, the remaining drying time of each processing unit being dried in the drying component can be obtained, the ratio of the remaining drying time of each processing unit to the total drying time can be determined, and the sum of the ratios of the remaining drying time of all processing units to the total drying time can be used as the drying temperature adjustment coefficient.
[0092] Exemplarily, the remaining drying time of the first processing unit in the drying component can be 0.2h, the total drying time can be 1h, the ratio of the remaining drying time to the total drying time of the first processing unit can be 0.2, and the sum of the ratios of the remaining drying time to the total drying time of all processing units in the drying component can be 2.
[0093] Exemplarily, when the product of the drying temperature difference and the drying temperature adjustment coefficient is taken as the temperature adjustment time, when the sum of the ratios of the remaining drying time and the total drying time of all processing units in the drying component is 2, and the drying temperature difference is 10°C, the calculated temperature adjustment time is 20 (in min), and the drying temperature can be uniformly adjusted to the preset drying temperature within 20 minutes.
[0094] To summarize, the sum of the ratios of the remaining drying time of all processing units to the total drying time is taken as the drying temperature adjustment coefficient. The longer the remaining drying time is, the more moisture needs to be removed during drying. The more moisture there is, the slower the drying speed needs to be, so as to avoid cracking of the TiO2 and eosin oxide adhesion layers attached to the aluminum base mesh, thereby further improving the quality of the TiO2 and eosin oxide adhesion layers.
[0095] The present application also provides a production device for a Ti-Br composite photocatalytic component. The production device for the Ti-Br composite photocatalytic component adopts any of the above methods when working. Figure 2 As shown, the production device of the Ti-Br composite photocatalytic component includes a drying component 1, a cleaning component 2, a plurality of immersion and attachment pools 3, a conveying component and a control component 4. The control component 4 controls the drying component 1, the cleaning component 2, a plurality of immersion and attachment pools 3, and the conveying component to cooperate with each other to complete the production process of the Ti-Br composite photocatalytic component.
[0096] like Figure 2 and Figure 3As shown, the drying assembly 1 is used to dry a plurality of processing units 11 , each processing unit 11 includes a bracket 112 carrying an aluminum-based mesh 111 , and the bracket 112 is used to carry and fix the aluminum-based mesh 111 .
[0097] like Figure 2 As shown, the TiO 2 and eosin attached to the aluminum-based mesh 111 can be dried by the drying component 1, thereby achieving the drying of the TiO 2 and eosin on the aluminum-based mesh 111.
[0098] Structurally, a drying component 1 is provided with a drying heating component 12 and a drying temperature measuring component 13. The drying heating component 12 is used to heat the air in the drying component 1, and the drying temperature measuring component 13 is used to measure the temperature in the drying component 1. The drying component 1 can be a long strip of factory building to construct a light-proof environment for drying the processing unit 11. During production, the interior of the factory building can be a low-light environment to ensure a light-proof environment for the production of the Ti-Br composite photocatalytic component.
[0099] When in operation, the cleaning component 2 is used to clean the bracket 112 of the processing unit 11 to recover TiO 2 and eosin on the bracket 112 .
[0100] Exemplarily, the cleaning component 2 can clean the bracket 112 vertically by using a cleaning head that can move up and down, thereby recovering TiO 2 and eosin on the outer wall of the bracket 112 .
[0101] like Figure 2 As shown, the immersion attachment pool 3 is used to contain the TiO2-eosin solution and soak the processing unit 11. The immersion attachment pool 3 is provided with a solution heating component 31, a solution temperature measuring component 32 and a stirring component 33. The solution heating component 31 is used to heat the TiO2-eosin solution, the solution temperature measuring component 32 is used to measure the temperature of the TiO2-eosin solution, and the stirring component 33 is used to stir the TiO2-eosin solution.
[0102] During operation, the immersion and attachment tank 3 is used to contain the TiO 2 -eosin solution and immerse the treatment unit 11 , so that the treatment unit 11 can be circulated through the immersion and attachment tank 3 .
[0103] Structurally, the immersion and attachment pool 3 is provided with a solution heating component 31, a solution temperature measuring component 32 and a stirring component 33. The solution heating component 31 is used to heat the TiO2-eosin solution so that the TiO2-eosin solution gradually heats up to immerse and attach the processing unit. The solution temperature measuring component 32 is used to measure the temperature of the TiO2-eosin solution, thereby being able to control the temperature of the TiO2-eosin solution. The stirring component 33 is used to stir the TiO2-eosin solution to achieve stable immersion and attachment of the TiO2-eosin solution on the processing unit.
[0104] When working, the conveying component is used to convey the processing unit 11 through the immersion and attachment tank 3, the cleaning component 2 and the drying component 1 in sequence, so as to control the working process of the processing unit 11.
[0105] In terms of structure, Figure 4 As shown, the drying and heating component 12, the drying and temperature measuring component 13, the cleaning component 2, the solution heating component 31, the solution temperature measuring component 32, the stirring component 33, and the conveying component are electrically connected to the control component 4, respectively, and then the control component 4 can centrally control the drying and heating component 12, the drying and temperature measuring component 13, the cleaning component 2, the solution heating component 31, the solution temperature measuring component 32, the stirring component 33, and the conveying component.
[0106] In summary, the control component can centrally control the drying and heating component, the drying and temperature measuring component, the cleaning component, the solution heating component, the solution temperature measuring component, the stirring component and the conveying component, and can centrally control the production process of the Ti-Br composite photocatalytic component, thereby improving the production efficiency of the production process of the Ti-Br composite photocatalytic component.
[0107] In some implementations, the drying component 1 is linear, with a feed end and a discharge end respectively provided at both ends of the drying component 1, multiple immersion attachment pools 3 are arranged along the length direction of the drying component 1, and the cleaning component 2 is arranged close to the feed end of the drying component 1. The drying component 1 adopts a first-in-first-out method to discharge the multiple processing units 11 in the drying component 1.
[0108] like Figure 2 As shown, the drying component 1 is linear in structure, and a feed end and a discharge end are respectively provided at both ends of the drying component 1, so that the drying component 1 can feed from the feed end and discharge from the discharge end, and can realize continuous drying of multiple processing units 11.
[0109] like Figure 2 As shown, the plurality of immersion and attachment pools 3 are arranged along the length direction of the drying component 1 , so that the plurality of immersion and attachment pools 3 can be immersed and attached in the length direction of the drying component 1 .
[0110] like Figure 2 As shown, the cleaning component 2 is arranged near the feed end of the drying component 1, so that after soaking the multiple processing units 11, the multiple immersion attachment pools 3 can enter the drying component 1 through the feed end of the drying component 1 for drying. The drying component 1 adopts a first-in-first-out method to discharge the multiple processing units 11 in the drying component 1, thereby realizing centralized drying of the drying component 1.
[0111] To summarize, multiple immersion attachment pools are arranged along the length direction of the drying component, the processing units in the multiple immersion attachment pools are convenient for transporting to the cleaning component, and the multiple immersion attachment pools share one cleaning component, which improves the utilization efficiency of the cleaning component. The drying component adopts a first-in-first-out method to discharge the multiple processing units in the drying component, thereby realizing continuous and centralized drying of the drying component and improving the production efficiency of the Ti-Br composite photocatalytic component.
[0112] In some implementations, the production device also includes a TiO2-eosin recovery component 5, which includes a conveying and collecting tank 51 and a cleaning and collecting tank 52. The conveying track of the conveying component to the processing unit 11 is located on one side of the multiple immersion and attachment pools 3. The conveying and collecting tank 51 is arranged below the conveying track of the conveying component to the processing unit 11. The cleaning and collecting tank 52 is arranged at the bottom of the cleaning component 2. The solutions collected by the conveying and collecting tank 51 and the cleaning and collecting tank 52 are mixed and formulated into a TiO2-eosin solution with a preset concentration value, and the TiO2-eosin solution with the preset concentration value is conveyed to the multiple immersion and attachment pools 3 through a pipeline.
[0113] like Figure 2 As shown, the TiO2-eosin recovery component 5 includes a conveying and collecting tank 51 and a cleaning and collecting tank 52, and the conveying and collecting tank 51 and the cleaning and collecting tank 52 are used to cooperate with each other to recover TiO2 and eosin.
[0114] like Figure 2 As shown, the conveying track of the conveying component to the processing unit 11 is located on one side of the multiple immersion attachment pools 3, and the conveying collection trough 51 is arranged below the conveying track of the conveying component to the processing unit 11, so that the conveying collection trough 51 can collect the TiO2-eosin solution dripping when the conveying component transports the processing unit 11, thereby realizing the centralized collection of the TiO2-eosin solution and avoiding the waste of TiO2 and eosin.
[0115] like Figure 2 As shown, the cleaning collection tank 52 is arranged at the bottom of the cleaning component 2, so as to realize the collection of the TiO2-eosin solution in the cleaning component 2. Since the liquid collected by the cleaning collection tank 52 is mainly the solution formed after the bracket 112 is cleaned, the concentration of TiO2 and eosin in the cleaning collection tank 52 is lower than the concentration of TiO2 and eosin collected by the conveying collection tank 51. The solutions collected by the conveying collection tank 51 and the cleaning collection tank 52 can be mixed and formulated into a TiO2-eosin solution with a preset concentration value, and the TiO2-eosin solution with the preset concentration value can be transported to the multiple immersion attachment pools 3 through pipelines, so as to realize the timely replenishment of the TiO2-eosin solution in the multiple immersion attachment pools 3.
[0116] In summary, the concentrations of TiO2 and eosin in the cleaning collection tank are lower than those collected in the transporting collection tank. The solutions collected in the transporting collection tank and the cleaning collection tank are mixed by the TiO2-eosin recovery component and then formulated into a TiO2-eosin solution with a preset concentration value. This achieves precise control of the concentration of the TiO2-eosin solution when replenishing the immersion attachment tank, thereby improving the collection and utilization effect of the TiO2-eosin solution.
[0117] In some implementations, a concentration detection component for detecting the concentration of the recovered TiO2-eosin solution is provided in the cleaning collection tank 52. The concentration detection component is electrically connected to the control component 4. When the concentration of the recovered TiO2-eosin solution detected by the concentration detection component is higher than a preset concentration value, the control component 4 issues a prompt message to prompt the cleaning component 2 to perform maintenance.
[0118] Structurally, a concentration detection component for detecting the concentration of the recovered TiO2-eosin solution is provided in the cleaning collection tank 52. The concentration detection component is electrically connected to the control component 4 so that the concentration detection component can detect the concentration of the TiO2-eosin solution to determine the working status of the cleaning component 2.
[0119] During operation, when the concentration of the recovered TiO2-eosin solution detected by the concentration detection component is higher than the preset concentration value, it means that when the cleaning component 2 cleans the treatment unit, the TiO2 and eosin on the aluminum-based mesh 111 on the treatment unit 11 may be washed away, which may cause the TiO2 and eosin on the aluminum-based mesh 111 to be insufficient and affect the working effect of the photocatalytic component. Therefore, a prompt message for repairing the cleaning component 2 can be issued through the control component 4 to prompt the cleaning component 2 to be repaired.
[0120] Exemplarily, when detecting the concentration of the TiO2-eosin solution, the turbidity of the TiO2-eosin solution is used as the concentration of the TiO2-eosin solution, and the concentration of the TiO2-eosin solution can be detected by a turbidity detection method.
[0121] In summary, by detecting the flushing amount of TiO2 and eosin on the aluminum-based mesh through the concentration detection component of the cleaning collection tank, the adhesion amount of TiO2 and eosin on the aluminum-based mesh can be detected, thereby improving the production quality monitoring effect of the catalytic component.
[0122] In the above embodiments, the description of each embodiment has its own emphasis. For parts that are not described or recorded in detail in a certain embodiment, reference can be made to the relevant descriptions of other embodiments.
[0123] The embodiments described above are only used to illustrate the technical solutions of the present application, rather than to limit them. Although the present application has been described in detail with reference to the aforementioned embodiments, a person skilled in the art should understand that the technical solutions described in the aforementioned embodiments may still be modified, or some of the technical features may be replaced by equivalents. Such modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present application, and should all be included in the protection scope of the present application.
Claims
1. A production control method for a Ti-Br composite photocatalytic component, characterized in that: The method comprises: The TiO2-eosin solution in the soaking and attachment pool (3) in which the processing unit (11) is soaked is controlled to be heated to a preset temperature within a first time period and the TiO2-eosin solution is kept stirred within the first time period, the processing unit (11) is continuously soaked with the heated TiO2-eosin solution, and the soaking and attachment time for the processing unit (11) to be continuously soaked with the heated TiO2-eosin solution is obtained; wherein each processing unit (11) comprises a bracket (112) carrying an aluminum-based mesh (111); When the first soaking and attachment time is greater than a soaking and attachment time threshold, controlling the first processing unit in the first soaking and attachment pool corresponding to the first soaking and attachment time to be transported to the cleaning component (2), and controlling the cleaning component (2) to clean the bracket (112) of the first processing unit; The first processing unit cleaned by the cleaning component (2) is controlled to be transported to the drying component (1) for drying for a preset time, and the drying component (1) is controlled to discharge the multiple processing units (11) in the drying component (1) in a first-in-first-out manner.
2. The method according to claim 1, characterized in that The method further comprises: The number of processing units of all processing units (11) in the drying component (1) is obtained; when the number of processing units is less than the first number of processing units, the soaking and adhesion time threshold is reduced by the first soaking and adhesion time threshold, and the first time period is reduced by the second time period; when the number of processing units is greater than the second number of processing units, the soaking and adhesion time threshold is increased by the second soaking and adhesion time threshold, and the first time period is increased by the second time period; wherein the first number of processing units is less than the second number of processing units.
3. The method according to claim 2, characterized in that The method further comprises: Acquiring the amount of time sequence processing units entering the drying component (1) in time sequence; wherein the amount of time sequence processing units entering includes a plurality of time values and the amount of processing units entering corresponding to each time value; By using a drying component temperature prediction model, the sequential drying temperature of the drying component (1) in a future time period is determined according to the amount of time processing unit input and the current drying temperature in the drying component (1); wherein the sequential drying temperature includes a plurality of time values and a drying temperature corresponding to each time value; When the first drying temperature corresponding to the first time value in the future time period is lower than the preset drying temperature, the drying temperature is adjusted to the preset drying temperature in a third time period before the first time value.
4. The method according to claim 3, characterized in that The method further comprises: When the first time value is reached, the first actual drying temperature and the first actual processing unit entry amount corresponding to the first time value are obtained. When the first actual processing unit entry amount and the first processing unit entry amount in the timing processing unit entry amount do not match, and when the first actual drying temperature is lower than the preset drying temperature, the drying temperature is adjusted to the preset drying temperature.
5. The method according to claim 4, characterized in that When the first actual drying temperature is lower than the preset drying temperature, adjusting the drying temperature to the preset drying temperature includes: The drying temperature difference between the first actual drying temperature and the preset drying temperature is determined, the product of the drying temperature difference and the drying temperature adjustment coefficient is used as the temperature adjustment time, and the drying temperature is uniformly adjusted to the preset drying temperature within the temperature adjustment time.
6. The method according to claim 5, characterized in that Determine the drying temperature adjustment factor by the following method: The remaining drying time of each processing unit being dried in the drying component is obtained, the ratio of the remaining drying time of each processing unit to the total drying time is determined, and the sum of the ratios of the remaining drying time of all processing units to the total drying time is used as the drying temperature adjustment coefficient.
7. A production device for a Ti-Br composite photocatalytic component, characterized in that: The method according to any one of claims 1 to 6 comprises a drying component (1), a cleaning component (2), a plurality of immersion and attachment tanks (3), a conveying component and a control component (4); The drying component (1) is used to dry a plurality of processing units (11), each processing unit (11) comprising a bracket (112) carrying an aluminum-based mesh (111), and a drying heating component (12) and a drying temperature measuring component (13) are provided in the drying component (1); The cleaning component (2) is used to clean the bracket (112) of the processing unit (11); The soaking and attachment pool (3) is used to contain a TiO2-eosin solution and soak the processing unit (111). The soaking and attachment pool (3) is provided with a solution heating component (31), a solution temperature measuring component (32) and a stirring component (33). The solution heating component (31) is used to heat the TiO2-eosin solution, the solution temperature measuring component (32) is used to measure the temperature of the TiO2-eosin solution, and the stirring component (33) is used to stir the TiO2-eosin solution. The conveying component is used to convey the processing unit (11) through the soaking and attachment tank (3), the cleaning component (2) and the drying component (1) in sequence; The drying and heating component (12), the drying and temperature measuring component (13), the cleaning component (2), the solution heating component (31), the solution temperature measuring component (32), the stirring component (33), and the conveying component are electrically connected to the control component (4) respectively.
8. The production device according to claim 7, characterized in that: The drying component (1) is in a straight line shape, and a feed end and a discharge end are respectively provided at two ends of the drying component (1). A plurality of soaking and adhering pools (3) are arranged along the length direction of the drying component (1), and a cleaning component (2) is arranged near the feed end of the drying component (1). The drying component (1) discharges the plurality of processing units (11) in the drying component (1) in a first-in-first-out manner.
9. The production device according to claim 8, characterized in that It also includes a TiO2-eosin recovery component (5), which includes a conveying collection trough (51) and a cleaning collection trough (52). The conveying track of the conveying component to the processing unit (11) is located on one side of the multiple immersion attachment pools (3). The conveying collection trough (51) is arranged below the conveying track of the conveying component to the processing unit (11). The cleaning collection trough (52) is arranged at the bottom of the cleaning component (2). The solutions collected by the conveying collection trough (51) and the cleaning collection trough (52) are mixed and then prepared into a TiO2-eosin solution with a preset concentration value, and the TiO2-eosin solution with the preset concentration value is conveyed to the multiple immersion attachment pools (3) through a pipeline.
10. The production device according to claim 9, characterized in that A concentration detection component for detecting the concentration of the recovered TiO2-eosin solution is provided in the cleaning collection tank (52). The concentration detection component is electrically connected to the control component (4). When the concentration of the recovered TiO2-eosin solution detected by the concentration detection component is higher than a preset concentration value, the control component (4) issues a prompt message for prompting the cleaning component (2) to be repaired.
Citation Information
Patent Citations
Preparation method of photocatalysis materials of biomorphic fine hiberarchy
CN101664675A
Preparation method of catalyst for light-reducing water to produce hydrogen
CN102600901A
Organic-salt-doped Ir-loaded g-C3N4 / TiO2 composite photocatalytic semiconductor material
CN110404590A
Ti-Br composite photocatalytic material, photocatalytic component, preparation method and application