Preparation of zinc oxide / mesoporous silver molybdate nanobelt material, and product and application thereof
By combining zinc oxide with mesoporous silver molybdate nanoribbons, the zinc oxide/mesoporous silver molybdate nanoribbons were prepared by chemical solution method and electrospinning technology, the existing problem of insufficient catalytic performance of silver molybdate was solved. , achieving high-efficiency photocatalytic performance in the visible light zone, especially in treating organic pollutants in water.
Patent Information
- Application Number
- CN202411100466.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-12
- Publication Date
- 2024-11-22
AI Technical Summary
The catalytic performance of existing silver molybdate photocatalytic materials is not high enough to effectively treat organic pollutants in water, especially in the visible light zone.
By combining zinc oxide with mesoporous silver molybdate nanoribbons, zinc oxide/mesoporous silver molybdate nanoribbons are prepared by chemical solution method and electrospinning technology, which improves its spectral absorption range and separation and transport of photogenerated charges. ability.
The photocatalytic properties of the material are significantly improved, and the adsorption of methyl orange in the dark can be achieved with a 99.7% tetracycline degradation effect under ultraviolet light conditions.
Smart Images

Figure FT_1
Abstract
Description
Technical Field
[0001] The invention relates to a nano photocatalytic material and preparation and application thereof, in particular to a preparation method, product and application of a zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material. Background Art
[0002] With the development of the chemical industry, environmental pollution is becoming increasingly serious. The discharge of printing and dyeing wastewater is one of the important causes of water pollution. Every year, a large amount of commercial dyes are discharged. These dyes have stable chemical properties and cause great harm to the ecological environment. By utilizing the characteristics of semiconductor oxide materials that can be activated under sunlight, organic matter can be effectively oxidized and degraded into small molecules such as carbon dioxide and water. Compared with traditional purification methods, semiconductor photocatalytic technology has the advantages of mild reaction conditions, no secondary pollution, simple operation and obvious degradation effect. Common traditional photocatalysts are materials such as titanium dioxide and zinc oxide with large bandgap width, which also have good photocatalytic properties. Of course, these materials have better catalytic properties in the ultraviolet light region, and there are certain limitations in real life.
[0003] In addition to its bactericidal effect, silver molybdate material can also be used as a new type of photocatalytic material. Under light conditions, it can not only sterilize sewage, but also treat organic pollutants in the water phase through photocatalytic technology.
[0004] In order to improve the catalytic efficiency of silver molybdate as a photocatalyst, people have used a variety of methods to modify the material. Among them, the composite of zinc oxide and silver molybdate and the control of the morphology of mesoporous nanobelts not only significantly improve its spectral absorption range, but also promote the effective separation and transmission of photogenerated charges, thereby improving the photocatalytic performance of the material.
[0005] The present invention provides a method for preparing a zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material. The present invention prepares the zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material by combining a chemical solution method with an electrostatic spinning technology. The composite of zinc oxide and silver molybdate and the control of the morphology of the mesoporous nanobelt not only significantly improve the spectral absorption range, but also promote the effective separation and transmission of photogenerated charges, thereby improving the photocatalytic performance of the material. The preparation process is relatively simple and easy to operate. Summary of the invention
[0006] In order to overcome the shortcoming that the existing silver molybdate photocatalytic performance is not high enough, the purpose of the present invention is to provide a method for preparing a zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material.
[0007] Another object of the present invention is to provide a zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material product obtained by the above method.
[0008] Another object of the present invention is to provide an application of the above product.
[0009] The object of the present invention is achieved by the following scheme: a method for preparing a zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material, wherein the zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material is prepared by combining a chemical solution method with an electrostatic spinning technology, and the specific steps of the method are: 1) Dissolve PVP in a mixed solution of ethanol and N,N-dimethylformamide in a mass ratio of 1:2:1, and stir magnetically for 1-2 h until the mixture is uniform, marked as solution A; 2) Add soluble molybdate and silver salt to the above solution A, wherein the stoichiometric ratio of molybdate to silver salt is 1:2, and stir magnetically for 1-2 h until uniform, so that the mass ratio of molybdate, silver salt, PVP, ethanol and N,N-dimethylformamide is 2:4:1:2:1, marked as solution B; 3) Add the foaming agent to solution B, stir magnetically until uniform, then electrospin at a potential of 18 kV, and then dry in an oven at a constant temperature of 60-80 °C; 4) The dried precursor is calcined at 500-600 °C for 30-60 min to obtain silver molybdate mesoporous nanobelts.
[0010] 5) Zinc sheets (1 × 1 cm, 0.1 cm thick) were then −1 HCl, ethanol, and acetone were thoroughly cleaned under ultrasonic conditions for 20–30 min; 6) Place the prepared zinc sheet and the silver molybdate mesoporous nanobelts obtained in step 4) in ammonium persulfate (0.13 mol L −1 ) and strong base (2.5 mol L −1 ) in 20 mL of deionized water at room temperature for 20-30 min, the obtained product was rinsed with distilled water and ethanol, and the washed material was dried at 60-80 ° C overnight to obtain C; 7) C is placed in a muffle furnace and calcined at 200-260 °C for 2-3 h to obtain the final product, zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material.
[0011] The invention combines a chemical solution method with an electrostatic spinning technology to prepare copper-loaded oxygen-deficient mesoporous silver molybdate nanobelts. The preparation method is simple, the process conditions are easy to achieve, the energy consumption is low, and the preparation is pollution-free.
[0012] Preferably, in the step 2), the molybdate is one or a combination of ammonium molybdate, potassium molybdate or sodium molybdate.
[0013] Preferably, in the step 2), the silver salt is one of silver nitrate and silver chlorate or a combination thereof.
[0014] Preferably, in step 3), the foaming agent is tea saponin or sodium bicarbonate or a combination thereof.
[0015] Preferably, in step 6), the strong base is sodium hydroxide, potassium hydroxide or a combination thereof.
[0016] The invention provides a zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material, which is prepared according to any of the above methods.
[0017] The invention provides an application of a zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material to the degradation of methyl orange in wastewater treatment.
[0018] Beneficial effects: The present invention provides a method for preparing a zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material. The present invention prepares the zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material by combining a chemical solution method with an electrostatic spinning technology. The composite of zinc oxide and silver molybdate and the control of the morphology of the mesoporous nanobelt not only significantly improve the spectral absorption range, but also promote the effective separation and transmission of photogenerated charges, thereby improving the photocatalytic performance of the material. The preparation process is relatively simple and easy to operate. The zinc oxide / mesoporous silver molybdate nanobelt first reaches equilibrium in the adsorption of methyl orange in the dark, and then, under ultraviolet light catalytic conditions, after 60 minutes, the degradation of tetracycline reaches 99.7%. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 This is a diagram of the ultraviolet light catalytic degradation of the zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material of Example 1. DETAILED DESCRIPTION
[0020] The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0021] Embodiment 1 A zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material is prepared by combining a chemical solution method with an electrostatic spinning technique, and is prepared according to the following steps: A method for preparing a zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material, characterized in that the zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material is prepared by combining a chemical solution method and an electrostatic spinning technology, comprising the following steps: 1) PVP was dissolved in a mixed solution of ethanol and N,N-dimethylformamide in a mass ratio of 1:2:1, and magnetically stirred for 1 h until the mixture was uniform, which was marked as solution A; 2) Add soluble ammonium molybdate and silver nitrate to the above solution A, wherein the molar ratio of ammonium molybdate to silver nitrate is 1:2, and stir magnetically for 1 h until uniform, so that the mass ratio of ammonium molybdate, silver nitrate, PVP, ethanol and N,N-dimethylformamide is 2:4:1:2:1, marked as solution B; 3) Add the foaming agent tea saponin to solution B, stir magnetically until uniform, then electrospin at a potential of 18 kV, and then dry in an oven at a constant temperature of 60 °C; 4) calcining the dried precursor at 500°C for 60 min to obtain silver molybdate mesoporous nanobelts; 5) Take a zinc sheet (1 cm long × 1 cm wide × 0.1 cm thick) and use 1.0 mol L −1 HCl, ethanol, and acetone were thoroughly cleaned under ultrasonic conditions for 20–30 min; 6) Place the prepared zinc sheet and the silver molybdate mesoporous nanobelt obtained in step 4) in 0.13 mol L −1 Ammonium persulfate and 2.5 mol L −1 The product was immersed in 20 mL of deionized water solution of sodium hydroxide at room temperature for 20 min, and then rinsed with distilled water and ethanol. The washed material was dried at 60 °C overnight to obtain C; 7) C was placed in a muffle furnace and calcined at 200°C for 3 h to obtain the final product, zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material.
[0022] Figure 1 The figure is the UV photocatalytic degradation diagram of the obtained zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material. The zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material first reaches equilibrium in the adsorption of methyl orange in the dark, and then under UV photocatalytic conditions, after 60 minutes, the degradation of methyl orange reaches 99.7%.
[0023] Example 2 A zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material is prepared similarly to Example 1 by the following steps: 1) PVP was dissolved in a mixed solution of ethanol and N,N-dimethylformamide in a mass ratio of 1:2:1, and magnetically stirred for 2 h until the mixture was uniformly mixed, which was marked as solution A; 2) Add soluble sodium molybdate and silver chlorate to the above solution A, wherein the molar ratio of sodium molybdate to silver chlorate is 1:2, and stir magnetically for 2 h until uniform, so that the mass ratio of sodium molybdate, silver chlorate, PVP, ethanol and N,N-dimethylformamide is 2:4:1:2:1, marked as solution B; 3) Adding the foaming agent sodium bicarbonate to solution B, stirring magnetically until uniform, then electrospinning at a potential of 18 kV, and then drying in an oven at a constant temperature of 80 °C; 4) calcining the dried precursor at 550 °C for 45 min to obtain silver molybdate mesoporous nanobelts; 5) A zinc sheet with a size of 1 cm long × 1 cm wide × 0.1 cm thick was treated with 1.0 mol L −1 HCl, ethanol, and acetone were thoroughly cleaned under ultrasonic conditions for 30 min; 6) Place the prepared zinc sheet and the silver molybdate mesoporous nanobelt obtained in step 4) in 0.13 mol L −1 Ammonium persulfate and 2.5 mol L −1 The product was immersed in 20 mL of deionized water solution of potassium hydroxide at room temperature for 30 min, and then rinsed with distilled water and ethanol. The washed material was dried at 80 °C overnight to obtain C; 7) C was placed in a muffle furnace and calcined at 230°C for 2 h to obtain the final product, zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material.
[0024] Example 3 A zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material is prepared similarly to Example 1 by the following steps: 1) PVP was dissolved in a mixed solution of ethanol and N,N-dimethylformamide in a mass ratio of 1:2:1, and magnetically stirred for 2 h until the mixture was uniformly mixed, which was marked as solution A; 2) Add soluble molybdate and silver salt to the above solution A, wherein the molar ratio of molybdate to silver salt is 1:2, and stir magnetically for 2 h until uniform, so that the mass ratio of potassium molybdate, silver nitrate, PVP, ethanol and N,N-dimethylformamide is 2:4:1:2:1, marked as solution B; 3) Add the foaming agent tea saponin to solution B, stir magnetically until uniform, then electrospin at a potential of 18 kV, and then dry in an oven at a constant temperature of 80 °C; 4) The dried precursor was calcined at 600 °C for 30 min to obtain silver molybdate mesoporous nanobelts; 5) The zinc sheet was cut into 1 × 1 cm pieces with a thickness of 0.1 cm, and then 1.0 mol L −1 HCl, ethanol, and acetone were thoroughly cleaned under ultrasonic conditions for 30 min; 6) Place the prepared zinc sheet and the silver molybdate mesoporous nanobelt obtained in step 4) in 0.13 mol L −1 Ammonium persulfate and 2.5 mol L −1 The product was immersed in 20 mL of deionized water solution of sodium hydroxide at room temperature for 30 min, and then rinsed with distilled water and ethanol. The washed material was dried at 80 °C overnight to obtain C; 7) C was placed in a muffle furnace and calcined at 260 °C for 2 h to obtain the final product, zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material.
Claims
1. A method for preparing a zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material, characterized in that: The method combines a chemical solution method with an electrospinning technique to prepare a zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material, comprising the following steps: 1) Dissolve PVP in a mixed solution of ethanol and N,N-dimethylformamide in a mass ratio of 1:2:1, and stir magnetically for 1-2 h until the mixture is uniform, marked as solution A; 2) Add soluble molybdate and silver salt to the above solution A, wherein the stoichiometric ratio of molybdate to silver salt is 1:2, and stir magnetically for 1-2 h until uniform, so that the mass ratio of molybdate, silver salt, PVP, ethanol and N,N-dimethylformamide is 2:4:1:2:1, marked as solution B; 3) Add the foaming agent to solution B, stir magnetically until uniform, then electrospin at a potential of 18 kV, and then dry in an oven at a constant temperature of 60-80 °C; 4) calcining the dried precursor at 500-600 °C for 30-60 min to obtain silver molybdate mesoporous nanobelts; 5) Zinc sheets (1 × 1 cm, 0.1 cm thick) were then −1 HCl, ethanol, and acetone were thoroughly cleaned under ultrasonic conditions for 20–30 min; 6) Place the prepared zinc sheet and the silver molybdate mesoporous nanobelts obtained in step 4) in ammonium persulfate (0.13 mol L −1 ) and strong base (2.5 mol L −1 ) in 20 mL of deionized water at room temperature for 20-30 min, the obtained product was rinsed with distilled water and ethanol, and the washed material was dried at 60-80 ° C overnight to obtain C; 7) C is placed in a muffle furnace and calcined at 200-260 °C for 2-3 h to obtain the final product, zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material.
2. The method for preparing a zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material according to claim 1, characterized in that The molybdate is one of ammonium molybdate, potassium molybdate and sodium molybdate or a combination thereof.
3. The method for preparing a zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material according to claim 1, characterized in that The silver salt is one of silver nitrate and silver chlorate or a combination thereof.
4. The method for preparing the zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material according to claim 1, characterized in that: The foaming agent is tea saponin or sodium bicarbonate or a combination thereof.
5. The method for preparing the zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material according to claim 1, characterized in that: The strong base is one of sodium hydroxide and potassium hydroxide or a combination thereof.
6. The method for preparing a zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material according to any one of claims 1 to 5, characterized in that: Prepare as follows: 1) PVP was dissolved in a mixed solution of ethanol and N,N-dimethylformamide in a mass ratio of 1:2:1, and magnetically stirred for 1 h until the mixture was uniform, which was marked as solution A; 2) Add soluble ammonium molybdate and silver nitrate to the above solution A, wherein the molar ratio of ammonium molybdate to silver nitrate is 1:2, and stir magnetically for 1 h until uniform, so that the mass ratio of ammonium molybdate, silver nitrate, PVP, ethanol and N,N-dimethylformamide is 2:4:1:2:1, marked as solution B; 3) Add the foaming agent tea saponin to solution B, stir magnetically until uniform, then electrospin at a potential of 18 kV, and then dry in an oven at a constant temperature of 60 °C; 4) calcining the dried precursor at 500°C for 60 min to obtain silver molybdate mesoporous nanobelts; 5) Take a zinc sheet (1 cm long × 1 cm wide × 0.1 cm thick) and use 1.0 mol L −1 HCl, ethanol, and acetone were thoroughly cleaned under ultrasonic conditions for 20–30 min; 6) Place the prepared zinc sheet and the silver molybdate mesoporous nanobelt obtained in step 4) in 0.13 mol L −1 Ammonium persulfate and 2.5 mol L −1 The product was immersed in 20 mL of deionized water solution of sodium hydroxide at room temperature for 20 min, and then rinsed with distilled water and ethanol. The washed material was dried at 60 °C overnight to obtain C; 7) C was placed in a muffle furnace and calcined at 200°C for 3 h to obtain the final product, zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material.
7. The method for preparing a zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material according to any one of claims 1 to 5, characterized in that: Prepare as follows: 1) PVP was dissolved in a mixed solution of ethanol and N,N-dimethylformamide in a mass ratio of 1:2:1, and magnetically stirred for 2 h until the mixture was uniformly mixed, which was marked as solution A; 2) Add soluble sodium molybdate and silver chlorate to the above solution A, wherein the molar ratio of sodium molybdate to silver chlorate is 1:2, and stir magnetically for 2 h until uniform, so that the mass ratio of sodium molybdate, silver chlorate, PVP, ethanol and N,N-dimethylformamide is 2:4:1:2:1, marked as solution B; 3) Adding the foaming agent sodium bicarbonate to solution B, stirring magnetically until uniform, then electrospinning at a potential of 18 kV, and then drying in an oven at a constant temperature of 80 °C; 4) calcining the dried precursor at 550 °C for 45 min to obtain silver molybdate mesoporous nanobelts; 5) A zinc sheet with a size of 1 cm long × 1 cm wide × 0.1 cm thick was treated with 1.0 mol L −1 HCl, ethanol, and acetone were thoroughly cleaned under ultrasonic conditions for 30 min; 6) Place the prepared zinc sheet and the silver molybdate mesoporous nanobelt obtained in step 4) in 0.13 mol L −1 Ammonium persulfate and 2.5 mol L −1 The product was immersed in 20 mL of deionized water solution of potassium hydroxide at room temperature for 30 min, and then rinsed with distilled water and ethanol. The washed material was dried at 80 °C overnight to obtain C; 7) C was placed in a muffle furnace and calcined at 230°C for 2 h to obtain the final product, zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material.
8. The method for preparing a zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material according to any one of claims 1 to 5, characterized in that: Prepare as follows: 1) PVP was dissolved in a mixed solution of ethanol and N,N-dimethylformamide in a mass ratio of 1:2:1, and magnetically stirred for 2 h until the mixture was uniformly mixed, which was marked as solution A; 2) Add soluble molybdate and silver salt to the above solution A, wherein the molar ratio of molybdate to silver salt is 1:2, and stir magnetically for 2 h until uniform, so that the mass ratio of potassium molybdate, silver nitrate, PVP, ethanol and N,N-dimethylformamide is 2:4:1:2:1, marked as solution B; 3) Add the foaming agent tea saponin to solution B, stir magnetically until uniform, then electrospin at a potential of 18 kV, and then dry in an oven at a constant temperature of 80 °C; 4) The dried precursor was calcined at 600 °C for 30 min to obtain silver molybdate mesoporous nanobelts; 5) The zinc sheet was cut into 1 × 1 cm pieces with a thickness of 0.1 cm, and then 1.0 mol L −1 HCl, ethanol, and acetone were thoroughly cleaned under ultrasonic conditions for 30 min; 6) Place the prepared zinc sheet and the silver molybdate mesoporous nanobelt obtained in step 4) in 0.13 mol L −1 Ammonium persulfate and 2.5 mol L −1 The product was immersed in 20 mL of deionized water solution of sodium hydroxide at room temperature for 30 min, and then rinsed with distilled water and ethanol. The washed material was dried at 80 °C overnight to obtain C. 7) C was placed in a muffle furnace and calcined at 260 °C for 2 h to obtain the final product, zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material.
9. A zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material, characterized in that: Prepared according to any one of claims 1 to 8.
10. Use of the zinc oxide / mesoporous silver molybdate nanobelt photocatalytic material according to claim 9 for degrading methyl orange in wastewater treatment.
Citation Information
Patent Citations
Preparation method of high-weather-resistance low-yellowing colored polycarbonate color master batch
CN113185826A
Photocatalytic material for catalytically degrading tetracycline and preparation method thereof
CN114950494A
Preparation method of magnesium titanate and superoxide magnesium titanate battery material as well as product and application of magnesium titanate and superoxide magnesium titanate battery material
CN115367789A
Preparation method of zinc sulfide / zinc oxide nano composite material, product and application
CN116282131A
Preparation of copper-loaded oxygen-deficient mesoporous silver molybdate photocatalytic material, and product and application thereof
CN116371406A