Method for producing cooling device
Through multi-stage sintering molding and heat treatment technology, the problem of waste of cooling power and resources of cooling equipment is solved, and efficient cooling and mechanical strength are achieved, and the overall performance of cooling equipment is improved.
Patent Information
- Application Number
- CN202410636357.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-22
- Filing Date
- 2024-05-22
- Publication Date
- 2024-11-22
AI Technical Summary
While the existing cooling equipment increases the cooling power, the problems of waste of resources and mechanical strength limitations during the manufacturing process make it difficult to reduce the size of structural components, affecting the cooling efficiency.
The cooling structure is manufactured through multi-stage molding using sintered powder, the surface area of the cooling element is increased in multiple molding steps using a molding mold, and the height and density of the cooling element are adjusted by heat treatment and calibration mold to ensure material strength and cooling efficiency.
It realizes the improvement of the cooling power of the cooling equipment under the condition of saving resources, reduces waste and processing time during the manufacturing process, improves productivity and cooling efficiency, and ensures the mechanical strength and corrosion performance of the cooling elements.
Smart Images

Figure CN118989327A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for manufacturing a cooling device, the method comprising the steps of providing a material and constructing a cooling structure from the material.
[0002] The invention further relates to a cooling device for cooling a component, comprising a base element having a first surface and a cooling structure having a cooling element, which is arranged on the base element so as to protrude beyond the first surface. Background Art
[0003] So-called power electronic components, such as power semiconductors, are well known from the prior art. Such components are frequently used, for example also in motor vehicles. It is also known that during operation these components generate a large amount of heat which usually has to be dissipated with the aid of a cooling medium. For this purpose, a wide variety of coolers are known from the prior art.
[0004] Thus, for example, DE112007000829B4 describes an assembly consisting of a frequency converter and a cooler for cooling the frequency converter, the cooler comprising the following components: a substrate having one surface on which an inverter is provided; a heat dissipation member fixed to another opposite surface of the substrate, the heat dissipation member surrounding an area opposite to an area on one of the surfaces of the substrate on which the inverter is provided; a main pipe remote from another surface of the substrate, the main pipe defining a space between the main pipe and the substrate, and the space being thus constructed such that a coolant can be guided to the space and the space enables the coolant to come into contact with the heat dissipation member; and a secondary pipe extending from the main pipe toward the substrate, the secondary pipe being opposite to an area of the substrate on which the frequency converter is provided, thereby allowing the secondary pipe to meet the coolant supplied to the main pipe on the other surface of the substrate in an area opposite to the area on which the frequency converter is provided, the coolant supplied to the main pipe being separated from the coolant supplied to the space until it is discharged from the secondary pipe.
[0005] So-called pin-fin cooling bodies are also described in the prior art, which are surrounded and flushed by a cooling medium and thus transfer heat from the pins to the cooling medium. For example, DE 10 2019 108 106 A1 describes a cooler for power semiconductors in an inverter, which is designed in two parts and includes a base plate as a first part, which can be attached to the power semiconductor in a heat-conducting manner; a cooling body as a second part, which is arranged on the base plate and has at least one corrugated recess, which is constructed continuously from the side of the cooling body facing away from the base plate to the side facing the cooling body; the first part and the second part are connected to each other and are coated with a layer that protects the two parts from electrochemical reduction.
[0006] DE102018216859A1 discloses a device for cooling a component, which comprises: a first base body and a second base body; cylindrical and / or conical first cooling ribs constructed in the first base body, through which a coolant can flow; and cylindrical and / or conical second cooling ribs constructed in the second base body, through which a coolant can flow, the second base body being joined to the first base body in such a way that the second cooling ribs are located between the first cooling ribs without contacting the first base body.
[0007] Cooling devices for power electronics usually have a structure consisting of structural elements on their surface. In order to increase the cooling performance, it is advantageous to have the largest possible surface of the structural elements around which the cooling fluid can flow. However, this surface is limited by the mechanical strength of the structural elements, since the structural elements can only be reduced to a minimum size. By reducing the structural elements, more structural elements can be arranged per unit area, so that the cooling performance can be improved due to the larger surface thus provided. Summary of the invention
[0008] The object of the present invention is to improve the cooling capacity of a cooling device for a component, which cooling device is to be manufactured in a resource-saving manner.
[0009] The object of the present invention is achieved by means of the method mentioned at the outset, according to which it is provided that: a sintering powder is used as material, a green body is produced from the sintering powder by pressing; the green body is sintered into a molded body, and the cooling structure in the form of a cooling element is produced from the molded body by molding, for which purpose a part of the molded body is pressed by a molding die, so that the molding is carried out in multiple molding steps.
[0010] Furthermore, the object of the invention is achieved with a cooling device of the type mentioned at the outset, in which the base element and the cooling element consist of a sintered material and in which the cooling element is produced from the material of the base element by multi-stage forming.
[0011] The advantage here is that by shaping the basic element into a cooling element, no waste material is generated for its production, as is the case, for example, during machining. In addition, all cooling elements of the cooling device can be produced simultaneously, thereby achieving a corresponding increase in productivity. For shaping, the advantage here is that although the preform already has a corresponding strength due to sintering, the preform can still be shaped more easily than solid material due to the porosity. By means of a multi-stage shaping process, cooling elements with a larger surface can be provided, thereby improving the cooling power of the cooling device. For example, by means of multi-stage shaping, cooling elements that are undercut or generally change in cross section can be provided.
[0012] According to a preferred embodiment variant of the invention, it can be provided that the height of the cooling element above the base element of the cooling structure is increased by at least two of the plurality of shaping steps, thereby increasing the surface available for cooling. In this case, a cooling structure with relatively thin cooling elements is achieved by means of a multi-stage performance, without subjecting the cooling elements to a significantly increased risk of damage (e.g. due to cracks etc.) during shaping. Thus, a large number / the same number of cooling elements per unit area can be achieved as before, but the cooling elements are or can be constructed higher.
[0013] According to another embodiment variant of the present invention, it can be provided that the same or identical forming tool is used for at least two of the plurality of forming steps. With this embodiment variant, the forming can be performed more economically or the motion sequence of the forming can be simplified.
[0014] According to another embodiment of the present invention, the cooling device can be subjected to a heat treatment between at least two of the plurality of forming steps, thereby making it possible to carry out the subsequent forming steps in a more mold-saving manner.
[0015] According to one embodiment variant of the invention, it can be provided that the preform is recompacted and the cooling structure is partially formed during the recompacting. By combining these steps into a single method step, a corresponding reduction in the production time of the cooling device can be achieved. It is advantageous here that by not recompacting the preform beforehand, the first forming step of forming the preform into the cooling structure can be carried out more simply due to the higher porosity ratio.
[0016] According to another embodiment variant of the invention, it can be provided that the cooling structure is produced in the form of a pin-shaped cooling element by using a perforated plate as a forming tool or a plurality of perforated plates as forming tools. The one forming tool or the plurality of forming tools can thus be designed relatively simply. In addition, the forming tools can be easily adapted to cooling elements of different shapes. Surprisingly, despite the large contact surface, demoulding the cooling element by removing the perforated plate does not cause problems such as material damage.
[0017] According to another embodiment variant of the invention, it can be provided that the cooling device is calibrated after the shaping step for producing the cooling element. Thus, the tolerances of the cooling element can be reduced using a method that is easy to implement.
[0018] According to another embodiment variant of the invention, it can be provided that the height of the cooling element is adjusted by pressing material from the head region of the cooling element into the region next to or below the head region of the cooling element. Here again, the use of sintered material is advantageous, since the material in the head region of the cooling element can be pressed relatively easily due to the remaining pores. Thus, the height of the cooling element can be adjusted easily and quickly without reworking by cutting, in particular to a height of the cooling element that is the same except for tolerances.
[0019] According to another embodiment of the invention, the density of the base element and the cooling element can be at least 98% of the solid density of the material used, so that despite powder metallurgical production, the cooling device can have improved corrosion properties without further post-processing. This is particularly advantageous for cooling elements that are circulated by a coolant during operation.
[0020] According to another embodiment of the invention, it can be provided that the height of the cooling element above the first surface of the base element can be between 4 mm and 40 mm. These heights of the cooling element have proven to be advantageous in terms of formability, since the material flow can be formed relatively uniformly over the entire height of the cooling element even in multi-stage forming.
[0021] According to an embodiment variant of the invention, it can be provided that the back side of the basic element is designed as a flat surface, thereby improving the contact of the basic element with the punch during forming and with the component to be cooled during operation of the cooling device.
[0022] According to another embodiment variant of the invention, it can be provided that at least one further structural element is arranged on the first surface of the base element, the at least one further structural element protruding in the height direction beyond the cooling element and being produced with a net shape or near net shape quality. Here again, powder metallurgical production of the cooling device is advantageous, since other surfaces on the cooling device can be produced without complex machining reprocessing, by already taking them into account in the original shaping for producing the preform.
[0023] According to another embodiment variant of the invention, it can be provided that at least some of the cooling elements have a higher density in the head region than the remaining cooling elements and / or that at least some of the cooling elements have a different shape in the head region than the remaining cooling elements. Thus, cooling elements can be used that are better adapted to the respective field of application. Here again, multi-stage molding is advantageous, since all cooling elements of the cooling device can be manufactured using simpler molds. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] In order to better understand the present invention, the present invention is explained in detail with reference to the following drawings.
[0025] In the simplified schematic diagram:
[0026] Figure 1 A side view of a cooling device with a component to be cooled is shown;
[0027] Figure 2 An oblique view showing a cooling device;
[0028] Figure 3 An embodiment variant of the preform is shown;
[0029] Figure 4 An embodiment variant of a mold for manufacturing a cooling device is shown;
[0030] Figure 5 An embodiment variant of the sequence of method steps for producing a cooling device with multi-stage forming is shown;
[0031] Figure 6 A detail in a mold is shown for adjusting the height of the cooling element. DETAILED DESCRIPTION
[0032] First of all, it should be pointed out that in the different described embodiments, the same parts are provided with the same reference numerals or the same component names, and the disclosure contained in the entire description can be transferred to the same parts with the same reference numerals or the same component names. The selected positional descriptions in the description, such as top, bottom, sideways, etc., also refer to the directly described and shown figures and these positional descriptions are transferred to the new positions in the case of a change in position.
[0033] exist Figure 1 A side view of the cooling device 1 is shown in FIG.
[0034] The cooling device 1 is used to cool a component 2 or a plurality of components 2 or an assembly. To this end, the cooling device 1 is placed with its rear side 3, in particular directly against at least one component 2, and is therefore preferably in direct contact with the component 2 for heat exchange.
[0035] The component 2 is preferably an electronic component, in particular a so-called power electronic component or a high-power electronic component or a power semiconductor or a high-power semiconductor, but it can also be implemented differently. Such a component 2 or an assembly composed of / having these components can be particularly configured for power ranging from a few kilowatts to a megawatt. Such a component 2 is used, for example, to convert electrical energy using switching electronic components. Typical applications are converters or frequency converters in the field of electrical drive technology, solar inverters for regenerative energy grids or switching power supplies (usually converting AC voltage into DC voltage through a rectifier and converting DC voltage into AC voltage through an inverter), converters for wind power equipment, control systems in drive technology for electric drive systems of electric vehicles or hybrid vehicles, battery management systems, etc. For example, power electronic components can be semiconductors, in particular so-called power semiconductors, such as IGBTs.
[0036] Since such a component 2 is known per se from the relevant prior art, reference is made to this prior art in order to avoid a repetition of details.
[0037] The cooling device 1 comprises a base element 4, which also forms the back side 3 of the cooling device 1, and which has a cooling structure on a first surface 5, or the cooling device is composed of the base element 4 and the cooling structure. The cooling structure is composed of a cooling element 6, which is arranged on the base element 4 protruding from the first surface 5 and is connected to it in one piece, as can also be seen from Figure 2 In other words, in a preferred embodiment variant, the cooling device consists of only one component. Regardless of this unity, within the scope of the invention, there is the possibility that, for each component 2 or an assembly consisting of / having at least one such component 2, a plurality of cooling devices 1 can be combined with one another to form a cooling device group according to the invention. Thus, a plurality of cooling devices 1 can also be assembled in a modular manner to form a cooling device group.
[0038] The base element 4 and the cooling element 6 are made of a sintered material or consist of a sintered material. Furthermore, the cooling element 6 is produced from the base element 4 by forming.
[0039] In a preferred embodiment variant, the density of the base element 4 and the cooling element 8 is at least 98%, in particular at least 98.5%, preferably at least 99%, of the solid density of the material used.
[0040] Solid density refers to the density of a cooling device produced by melt metallurgy from the same material, ie a component consisting of solid material. Solid material refers to a metallic material which, apart from defects, has no pores, as is usually the case in sintered components.
[0041] The cooling element 6 is provided for a cooling fluid, for example water, to flow around it, so that the heat absorbed by the cooling device 1 is transported away via the cooling fluid. The cooling device 1 is preferably a so-called pin-fin cooler.
[0042] The cooling element 6 of the embodiment variant shown is cylindrical. However, the cooling element can also have a different shape, for example a truncated cone or generally have a cross section that tapers toward the cooling element head 7, for example a truncated pyramid. According to one embodiment variant, several or all cooling elements 6 can be mushroom-shaped in the head region, as in this Figure 6 Indicated by dotted line.
[0043] The cross section of the cooling element 6 may be circular, oval, diamond-shaped, square, etc.
[0044] Furthermore, all cooling elements 6 can be designed identically. However, cooling elements 6 of different shapes can also be arranged or combined on the base element 4 .
[0045] The height 8 of the cooling element 6 above the first surface 5 of the base element 4 can preferably be between 4 millimeters and 40 millimeters.
[0046] In the simplest embodiment of the cooling device 1 , all cooling elements 6 of the cooling device 1 have the same height 8 within tolerances. However, within the scope of the invention, some cooling elements 6 can have a smaller height than the remaining cooling elements 6 .
[0047] Furthermore, it can be provided that between 300 and 1300, in particular between 300 and 1000, for example between 300 and 750 cooling elements 6 are arranged or formed per square dm of the first surface. This number has been found to be advantageous in particular with regard to the production of the cooling device 1, i.e. with regard to the forming of the base element 4 into the cooling element 6, since damage to the cooling element 6 or incompletely formed cooling elements 6 can thereby be avoided or reduced.
[0048] In particular, from Figure 1 As can be seen in FIG. 1 , according to one embodiment variant of the cooling device 1, the back side 3 of the base element 4 can be designed as a flat surface. However, there is also the possibility that the back side 3 is also designed with one or more recesses 9, in which the component 2 is at least partially accommodated. This allows for better attachment of the component 2 to the cooling device 1. The component 2 can usually be glued or screwed or welded or sintered to the cooling device 1, for example.
[0049] At least one recess 9 can be produced simultaneously with the cooling element 6 during the production of the cooling element 6 . By means of the at least one recess 9 , it is also possible to produce a cooling element 6 having a height 8 that is greater than the height of the remaining cooling element 6 .
[0050] If available from Figure 2 As can be seen, the cooling device 1 can have at least one further structural element 10 on the first surface 5 of the base element 4. The structural element 10 is a cylinder in the shape shown, but can also have a different cross section, for example a rhombus cross section. With the structural element 10, a further surface 11 can be provided on the cooling device 1 above the plane of the cooling element 6. Therefore, the height of the structural element 10 can be greater than the cooling element 6. However, it is also possible that the height of at least one structural element 10 is less than or equal to the cooling element 6. In addition, more than one structural element 10 can be provided, and a plurality of structural elements 10 can be designed, for example, in the same or different manner in terms of shape and / or height.
[0051] The structural element 10 can be provided, for example, for screw connection, as a reinforcement, as a spacer or as a stop.
[0052] The structural element 10 is preferably not subjected to mechanical post-processing, but is pressed or powder-metallurgically produced in net or near net shape quality during the pressing of the preform for producing the cooling device 1. The structural element 10 or the structural elements 10 are therefore preferably designed in one piece with the base element 4 and the cooling element 6.
[0053] Sintered powders or powders used in powder metallurgy, in particular metals, are used to produce the cooling device 1. Sintered powders with correspondingly good thermal conductivity are preferably used. In particular, sintered powders based on aluminum or aluminum alloys or based on copper or copper alloys or MMC powders (metal matrix composites) are used.
[0054] The cooling device is manufactured in a powder metallurgical manner according to the powder metallurgy method, so that the cooling device 1 is preferably a sintered component. For this purpose, a green body is produced in a corresponding die (die) from a sintering powder that can be produced from individual (metal) powders by mixing, and the powder can be used pre-alloyed if necessary. The density of the green body is preferably at least 80% of the solid density of the material, in particular between 80% and 96%.
[0055] The green body can then be dewaxed at room temperature and subjected to one-stage, two-stage or multi-stage sintering and then preferably cooled to room temperature. The sintering can be carried out at a temperature between 500°C and 1300°C, for example.
[0056] Since these method sequences and the method parameters used therein are likewise known from the prior art, in order to avoid repetitions, reference is made to the relevant prior art in this regard.
[0057] By sintering, a preform 11 is formed from the green body, as is exemplified in Figure 3The preform 11 can be designed as a flat plate or in a plate-shaped manner, so that the rear side 3 and at least a section of the first surface 5 can extend parallel to one another.
[0058] According to an embodiment variant of the method, it can be provided that the first surface 5 of the preform 11 provided with the cooling structure is produced in a curved manner at least in some sections. In general, the preform 11 can be produced with different thicknesses 12 at least in some sections. In particular, the preform 11 can be produced thinner in at least one edge section 13 or in a plurality of edge sections 13 than in the central section 14, such as in this Figure 3 The central section 14 is the region of the preform 11 with the greatest thickness 12. The thinner edge sections 13 can be formed, for example, around the central section 14, i.e. along the entire periphery of the central section 14. The reduction in thickness 12 can be formed abruptly and / or ramp-like starting from the central section 14, as is also the case in Figure 3 Other shapes are also possible.
[0059] The reduced thickness 12 in at least one edge section 13 may also be present on the finished cooling device 1, such as from Figure 2 See.
[0060] In view of the improved formability of the preform 11, other shapes of the first surface of the preform 11 are possible. Thus, first pin-fin additions or cooling element additions (round, egg-shaped, oval, etc.) with a height between 0.1 mm and 2.0 mm can already be preformed. Additionally, structures (waves, ribs, etc.) can be deliberately introduced into the surface 5 of the preform in order to increase the turbulence of the cooling fluid if necessary.
[0061] The preform 11 can then be recompacted. However, the recompacting preferably takes place simultaneously with the shaping of the preform 11 into the cooling element 6.
[0062] The preform 11 is formed in a forming die 15. For this purpose, the preform 11 is placed in the forming die 15 or is placed against it. In the simplest case, the forming die 15 is formed by a perforated plate 16. The perforated plate 16 has a recess 17, in particular a penetration, into which a part of the material of the preform 11 is pressed or through which a part of the material of the preform 11 is pressed, thereby forming the cooling element 6. The rest of the material of the preform 11 that is not pressed into the forming die 15 or through the forming die 15 forms the base element 4.
[0063] The recess 17 , ie its cross section, is adapted accordingly to the cross section of the cooling element 6 to be produced.
[0064] The shaping tool 15 can also have a different appearance, ie it does not necessarily have to be a simple perforated plate 16. The shaping tool 15 can be designed in particular as a "pot-shaped" die.
[0065] In the event that at least one further structural element 10 is present, it can be taken into account by a corresponding recess or a corresponding penetration in the forming tool 15 .
[0066] For forming, the punch 18 can be placed against the back side 3 of the preform 11 and pressed against the preform 11 with a predeterminable pressure, the back side also forming the back side 3 of the base element 4. The material of the preform 11 is pressed into the recess 17 or the penetration of the forming die 15 by the pressure applied to the preform 11. The forming can be carried out, for example, at a pressure between 700 MPa and 1600 MPa. In addition, the forming can be carried out during a time of up to 10 seconds, in particular between 0.1 seconds and 10 seconds. In addition, the forming is preferably carried out at room temperature (20° C.), that is, cold forming, or the forming can also be carried out after the preform 11 is preheated to a temperature between 50° C. and 300° C., for example, between 50° C. and 150° C. and / or in or with the forming die 15 heated to a temperature between 50° C. and 300° C., for example, between 50° C. and 150° C.
[0067] It can be provided that the shaping of the preform 11 into the cooling structure or the cooling device 1 is carried out in multiple stages, that is, in two or more steps, such as Figure 5 The schematic illustration is based on a forming method with two forming steps. However, it should be mentioned that the method for producing the cooling device 1 can also have more than two forming steps, for example three or four or five, etc., with which the cooling element 6 is formed.
[0068] It should be mentioned here that the multi-stage shaping refers to the shaping of the preform 11 into the cooling element 6 and not to further shaping which may also be carried out, such as, for example, calibration of the cooling element 6 , as will be described below.
[0069] The multi-stage forming can be carried out with an at least approximately constant degree of forming in the individual forming steps. The cooling element 6 can, for example, undergo at least approximately the same height change in each of the forming steps. However, it is also possible that the degrees of forming in the individual forming steps also differ from one another. The height change of the cooling element 6 can, for example, be greater in the first forming step than in the subsequent forming steps, or conversely, the height change of the cooling element can be smaller in the first forming step than in the subsequent forming steps.
[0070] In each molding step, the parameters for molding can be the same or different. The pressure applied to the parison 11 can be greater in the first molding step than in the subsequent molding steps, for example. The parameters for molding in each molding step can be selected from the above range.
[0071] For Figure 5 In the two-stage forming method for forming the cooling element 6, which is exemplarily shown in FIG. 1 , in the first forming step of forming the preform 11 by means of a forming die 15 (for example, the perforated plate 16 mentioned above), the cooling element 6 is formed with a first sub-height 19. The first sub-height 19 is smaller than the height 8 of the cooling element 6 after the second forming step, as can be seen from Figure 5 It can be seen that the sub-height 19 can be in the range between 20% and 80% of the height 8, for example.
[0072] Thus, the height 8 of the cooling element 6 above the base element 4 of the cooling structure can be increased by means of a method having at least two molding steps out of a plurality of molding steps. To this end, the method can have exactly two molding steps or more than two such molding steps for constructing the height using a molding die 15, for example a perforated plate 16. That is, in the molding "having at least two molding steps out of the plurality of molding steps", the term "plurality" can also mean just "two".
[0073] For the second shaping step or generally for at least two of the plurality of shaping steps, the same shaping tool, i.e. the shaping tool 15, for example the perforated plate 16, can be used, so that after the first shaping step, the partially constructed cooling element 6 is pressed through the shaping tool 15 of the previous shaping stage or pressed into the shaping tool of the previous shaping stage. However, it is also possible to use two or more identical shaping tools 15, for example the perforated plate 16. On the other hand, it is also possible to carry out the shaping with different shaping tools 15, for example with shaping tools 15 with different diameters of the recesses 17. In order to form undercuts or protrusions in or on the cooling element 6 of the cooling device 1 or at least individual cooling elements of the plurality of cooling elements 6, different shaping tools 15 can also be used in the individual shaping steps.
[0074] In accordance with Figure 5 In the illustration of an embodiment variant of the method sequence according to the invention, a forming tool 15 which is designed identically to the forming tool 15 of the first forming step is shown in the second step. The dashed line indicates that the forming tool 15 in the second forming stage can also have a greater layer thickness, in particular a layer thickness which is at least approximately the same as the height 8 of the cooling element 6 at the end of this forming step, in order to thus provide a support possibility for the already formed section of the cooling element 6 in the second or further forming step.
[0075] The two forming steps or at least two of the multiple forming steps can be implemented in separate forming molds 15. However, a method implementation variant is also possible, in which the two forming steps or at least two of the multiple forming steps are implemented in one forming mold 15. The cross section of the recess 17 of this forming mold 15 can be reduced in the direction of the material flow during forming. The reduction can be constructed continuously or in a jumpy manner. If necessary, a mold stage with a widened cross section can be constructed between two jump-changed cross-sectional dimensions to achieve pressure relief of the material formed in the previous forming stage. The individual stages of the multi-stage forming mold 15 can have the same or different heights from each other. With this structure of the forming mold 15, a staged cooling element 6 can be manufactured. If necessary, the stages can be further formed when necessary using other forming molds 15 in other forming steps, so as to produce a cooling element 6 that has no cross-sectional changes in height, that is, for example, a cylindrical structure.
[0076] according to Figure 5 A further embodiment variant of the invention is shown in the method flow. It can be provided that a heat treatment of the cooling device is carried out between two forming steps or between at least two of the plurality of forming steps or between all forming steps. The heat treatment can be carried out in a furnace 20, for example in a continuous process. Other heat sources can also be used. The heat treatment can be carried out inductively, for example. With induction heat treatment, only limited areas can also be heat treated, in particular in the area of the cooling element 6 which was partially formed in the previous forming.
[0077] The heat treatment can be carried out at a temperature between 100° C. and 500° C., depending on the sintering material used and its melting point. The heat treatment can also be carried out as an intermediate sintering, ie, re-sintering, of the already partially formed preform 11 .
[0078] The heat treatment makes it possible to make the region of the cooling element 6 which was formed in the preceding forming step softer again, so that the forming step which follows the heat treatment can be carried out more easily.
[0079] After the preform 11 has been shaped, ie formed, the cooling device 1 can be completed. However, there is also the possibility of further processing the cooling device 1.
[0080] After the preform 11 has been shaped, i.e. formed, the cooling device 1 can be calibrated. By means of the calibration, the dimensional accuracy of the cooling device 1 is increased at least in some sections or locally. Furthermore, by means of the calibration, pores in the region of the calibrated surface can be closed, thereby making it possible to achieve a denser structure. During the calibration, the cooling structure, in particular at least individual cooling elements of the cooling elements 6, are subjected to pressure against the corresponding surface.
[0081] According to a preferred embodiment variant, the height of the cooling element 6 can be calibrated, as in Figure 6 . Here, a calibration die 22, which can be designed, for example, in the form of a plate or a die, can be pressed from above onto the cooling element head 7. During this process, the cooling device 1 can be held in a holding element, for example a die. The height deviation after a number of forming steps can be reduced, for example, in the direction of the central section 14 of the cooling device 1 (see Figure 3 ) until the height difference of the cooling element 6 or the tolerable tolerance range of the height 8 is reached. Unless part of this height difference has already been taken into account by the shape of the preform 11 (for example, by forming areas with different thicknesses 12, for example according to a curve), the calibration can be carried out accordingly. With a preform 11, in which the height deviations of the sintered and formed green body are already at least partially taken into account, the calibration work, i.e. the calibration effort, can be reduced.
[0082] The calibration mold 22 can also have a mold cavity in which the cooling element 6 is at least partially accommodated during calibration.
[0083] The calibration can be carried out in one stage or in several stages, if necessary with an intermediate depressurization of the cooling device 1 between the calibration steps.
[0084] According to one embodiment variant, it can also be provided that the height 8 of the cooling element 6 is adjusted by pressing material from the head region of the cooling element 6 (cooling element head 7) into the region 23 next to or below the head region of the cooling element 6. Figure 6 For the extrusion, a simple plate-shaped die, in particular the aforementioned calibration die 22 , can be used which is pressed onto the cooling element 6 .
[0085] It may be advantageous for the calibration or the extruded material that the height difference of the cooling element 6 after the forming is between a maximum of 0.2 mm and a maximum of 0.4 mm, i.e., it is produced with relatively small height differences. This can be achieved, for example, by taking into account the shape of the preform 11 as described above. The final height tolerance can be achieved relatively easily in a subsequent work process by means of height calibration.
[0086] The calibration can avoid machining of the cooling element 6 in order to reduce the height tolerance of the cooling element 6. By reducing the height tolerance, a partially mushroom-shaped or (slightly) convex cooling element 6 can be produced, which can also be advantageous with regard to the flow of the cooling fluid flowing around the cooling element 6 and thus the cooling capacity of the cooling device 1. Furthermore, reducing the height tolerance can also reduce or eliminate residual porosity at the upper end of the cooling element 6.
[0087] As already mentioned above, the cooling elements 6 of the cooling device 1 can also have different heights 8. In order to be able to carry out a height calibration or calibration in this case as well, the calibration mold can be designed, for example in stages, according to the desired height profile of the cooling elements 6.
[0088] A correspondingly designed calibration mold 22 can also be used to form a certain shape of the cooling element 6. For this purpose, the calibration mold 22 can have a matching contour, for example, in order to shape the head of the cooling element 6 accordingly, i.e. to provide a contour or surface design such as, for example, a rounding, a chamfer, etc. or to provide a recess, a surface roughness greater than the roughness after sintering, etc.
[0089] For the case of a configuration with cooling elements 6 of different heights, a staged calibration mold 22 can also be used.
[0090] The method according to the invention can be used to manufacture a cooling device 1 for cooling a component 2, which provides a base element 4 having a first surface 5 and a cooling structure having cooling elements 6, which are arranged on the base element 4 protruding from the first surface 5. At least individual cooling elements of the cooling elements 6 can have a higher density in the head region than the remaining cooling elements 6, and / or at least individual cooling elements of the cooling elements 6 can have a different shape in the head region than the remaining cooling elements 6.
[0091] The exemplary embodiments show possible embodiment variants, at which point it should be noted that combinations of the individual embodiment variants with one another are also possible.
[0092] Finally, it should be pointed out that, in order to provide a better understanding of the structure of the cooling device 1 or of the forming tool 12 , these are not necessarily shown to scale.
[0093] Reference numerals list
[0094] 1 Cooling equipment
[0095] 2 Components
[0096] 3 Dorsal
[0097] 4 Basic components
[0098] 5 Surface
[0099] 6 Cooling element
[0100] 7 Cooling element head
[0101] 8 Height
[0102] 9 recess
[0103] 10 Structural elements
[0104] 11. Parison
[0105] 12 Thickness
[0106] 13 Edge Segment
[0107] 14 Central section
[0108] 15. Forming mold
[0109] 16-well plate
[0110] 17 Gap
[0111] 18 Punch
[0112] 19 Sub-height
[0113] 20 furnaces
[0114] 21. Calibrate the mold
[0115] 22 Mold wall
[0116] 23 regions.
Claims
1. A method for manufacturing a cooling device (1), said method comprising the steps of providing a material and constructing a cooling structure from said material, characterized in that Sintering powder is used as material, and a green body is manufactured from the sintering powder by pressing; the green body is sintered to form a blank (11), and the cooling structure in the form of a cooling element (6) is manufactured from the blank (11) by molding, for which a part of the blank (11) is pressed by a molding die (22), so that the molding is carried out in multiple molding steps.
2. The method according to claim 1, characterized in that At least two of the plurality of forming steps are used to increase the height (8) of the cooling element (6) above the base element (4) of the cooling structure.
3. The method according to claim 1 or 2, characterized in that: The same or identical molding die (22) is used for at least two molding steps among the plurality of molding steps.
4. The method according to any one of claims 1 to 3, characterized in that The cooling device (1) is subjected to heat treatment between at least two of the plurality of forming steps.
5. The method according to any one of claims 1 to 4, characterized in that The preform (11) is recompacted and the cooling structure is partially constructed during the recompacting.
6. The method according to claims 1 to 5, characterized in that The cooling structure is produced in the form of a pin-shaped cooling element (6) by using a perforated plate (16) as a forming tool (12) or a plurality of perforated plates (16) as forming tools (15).
7. The method according to any one of claims 1 to 6, characterized in that After the shaping step for producing the cooling element (6), the cooling device (1) is calibrated.
8. The method according to claim 7, characterized in that The height (8) of at least individual cooling elements (6) is adjusted by pressing material in the head region of the cooling element (6) into a region (23) next to or below the head region of the cooling element (6).
9. A cooling device (1) for cooling a component (2), comprising a base element (4) having a first surface (5) and a cooling structure having a cooling element (6), the cooling structure being arranged on the base element (4) so as to protrude beyond the first surface (5), characterized in that: The base element (3) and the cooling element (6) are composed of sintered material, and the cooling element (61) is produced from the material of the base element (3) by multi-stage forming.
10. The cooling device (1) according to claim 9, characterized in that The density of the base element (4) and the cooling element (6) is at least 98% of the solid density of the material used.
11. The cooling device (1) according to claim 9 or 10, characterized in that The height (8) of the cooling element (6) above the first surface (5) of the base element (4) is between 4 mm and 40 mm.
12. The cooling device (1) according to any one of claims 9 to 11, characterized in that The rear side (3) of the base element (4) is designed as a flat surface.
13. The cooling device (1) according to any one of claims 9 to 12, characterized in that At least one further structural element (10) is arranged on the first surface (5) of the base element (4), the at least one further structural element protruding beyond the cooling element (6) in the direction of the height (8) and the at least one further structural element is manufactured with a net shape or near net shape quality.
14. The cooling device (1) according to any one of claims 9 to 13, characterized in that At least some of the cooling elements (6) have a higher density in the head region than the remaining cooling elements (6), and / or at least some of the cooling elements (6) have a different shape in the head region than the remaining cooling elements (6).
Citation Information
Patent Citations
Cooling with cooling fins
DE102018216859A1
Cooler for a power semiconductor in an inverter
DE102019108106A1
Inverter and cooler arrangement and its use
DE112007000829B4