Machining tool
By using a combination of annular grinding and abrasive tools under specific conditions, the problem of low productivity in the removal of wafer chamfers was solved, achieving a highly efficient and smooth chamfer removal effect.
Patent Information
- Application Number
- CN202410567638.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-17
- Filing Date
- 2024-05-09
- Publication Date
- 2024-11-22
AI Technical Summary
Existing technologies suffer from low productivity when removing chamfered edges from wafers, especially due to the long time spent in the rough removal and finishing processes, resulting in low efficiency.
By employing machining tools, combining annular grinding wheels and abrasive wheels, and meeting specific conditions (H+h>L, L/3>h>L/100), the chamfered portion of the wafer is efficiently removed. The selection of the grinding wheel width H and the abrasive wheel width h is based on the wafer material characteristics to ensure efficient removal and finishing.
This technology enables efficient removal of the chamfered edges of wafers, improving productivity and ensuring the smoothness of the removed area and overall processing efficiency.
Smart Images

Figure CN118990181A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a processing tool for removing a chamfered portion of a wafer. The wafer has a central region and a peripheral remaining region surrounding the central region on a front surface, and the chamfered portion is formed on the periphery of the peripheral remaining region. Background Art
[0002] Regarding a wafer having a plurality of devices such as ICs and LSIs formed on the front side thereof divided by a plurality of intersecting predetermined dividing lines, after the back side of the wafer is ground to a prescribed thickness by a grinding device, it is divided into individual device chips by a cutting device. The divided device chips are used in electronic devices such as mobile phones and personal computers.
[0003] The grinding device is composed of: a chuck table that holds a wafer; a grinding unit that has a rotatable grinding wheel, the grinding wheel being provided with a grinding tool in a ring shape for grinding the wafer held by the chuck table; a feeding mechanism that feeds the grinding unit for grinding; and a thickness gauge that measures the thickness of the wafer. The grinding device can grind the back side of the wafer to process the wafer to a desired thickness.
[0004] However, since a chamfer is formed on the periphery of the wafer, there is a problem as follows: when the back side of the wafer is ground and thinned, the chamfer at the peripheral end of the wafer becomes a sharp blade, cracks are generated from the periphery and spread toward the device area, thus causing damage to the device and possibly injuring the operator.
[0005] Therefore, the present applicant has proposed a technique of removing the chamfered portion formed at the outer peripheral end of the outer peripheral excess area before grinding the back surface of the wafer (see, for example, Patent Document 1).
[0006] In addition, when the chamfered portion is cut using a cutting tool, defects will occur on the periphery of the chip, resulting in a decrease in quality. Therefore, the applicant has also proposed the following technology: after roughly removing the chamfered portion using a coarse grinding tool, the defects are removed using a fine grinding tool, thereby improving the quality before grinding the back side of the chip (see patent document 2).
[0007] Patent Document 1: Japanese Patent Application Publication No. 2010-225976
[0008] Patent Document 2: Japanese Patent No. 2014-003198
[0009] However, in the process of roughly removing the chamfered portion using the coarse-mesh die surface and then performing finish machining using the fine-mesh die surface, it takes time to remove the chamfered portion, which leads to poor productivity and a troublesome problem. Summary of the invention
[0010] Therefore, an object of the present invention is to provide a processing tool capable of efficiently removing a chamfered portion of a wafer.
[0011] According to one aspect of the present invention, there is provided a processing tool for removing a chamfered portion of a wafer, the wafer having a central region and a peripheral residual region surrounding the central region on a front surface, the chamfered portion being formed on the periphery of the peripheral residual region, wherein the processing tool comprises: an annular grinding tool having an opening at the center for inserting a spindle, the grinding tool having a first side surface and a second side surface; and a grinding tool formed on at least one of the first side surface or the second side surface, wherein when the length of the chamfered portion to be removed in the radial direction from the peripheral end is set to L, the width of the grinding tool is set to H, and the width of the grinding tool is set to h, the processing tool is formed to satisfy the following two conditions (1) and (2):
[0012] H+h>L…(1)
[0013] L / 3>h>L / 100…(2).
[0014] The particle size of the diamond abrasive grains constituting the grinding tool is preferably selected according to the material of the wafer, and the particle size of the diamond abrasive grains constituting the grinding tool is selected within the range of 1.5 to 5 times the particle size of the diamond abrasive grains constituting the grinding tool. The bonding material constituting the grinding tool and the grinding tool is preferably selected from any bonding material of a resin bonding agent, a ceramic bonding agent, and a metal bonding agent. The wafer is preferably a semiconductor wafer having a device region in which a plurality of devices are divided by a plurality of intersecting predetermined division lines in the central region.
[0015] According to the processing tool of the present invention, the area of the wafer with a length L in the radial direction from the outer peripheral end to be removed can be roughly removed efficiently using a grinding tool, and the outer peripheral surface of the removed area formed in the chamfered portion can be smoothly finished to improve productivity. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 It is an overall perspective view of a cutting device to which a processing tool according to the present embodiment is mounted.
[0017] Figure 2 (a) is Figure 1 A partially enlarged stereoscopic view of a cutting unit of the cutting device shown in FIG. Figure 2 (b) is Figure 2 (a) is an exploded perspective view of the cutting unit shown.
[0018] Figure 3It is a perspective view showing a state of a wafer holding process of holding a wafer.
[0019] Figure 4 It is a perspective view showing a state of detecting a position to be processed of a chamfered portion.
[0020] Figure 5 It is shown in Figure 4 A side view of a wafer undergoing chamfer inspection.
[0021] Figure 6 This is a perspective view showing a state where a grinding unit is positioned on a wafer when performing a chamfer removal step.
[0022] Figure 7 This is a perspective view showing how the chamfered portion is removed in the chamfered portion removing step.
[0023] Figure 8 (a) is a partial enlarged side view showing the situation where the grinding tool cuts into the chamfered portion of the wafer, Figure 8 (b) is a partially enlarged side view showing a state where a part of the chamfered portion is removed by the chamfered portion removing step.
[0024] Description of symbols
[0025] 1: cutting device; 2: housing; 3: loading and unloading mechanism; 4: box; 5: temporary table; 6: conveying mechanism; 7: chuck table; 71: suction chuck; 72: frame; 8: cutting unit; 81: grinding tool cover; 82: spindle housing; 83: spindle; 83a: front end; 86: fixing flange; 86a: hub; 86b: external thread; 87: mounting and disassembling flange; 88: nut; 9: grinding tool; 91: grinding tool; 91a: first side Surface; 91b: second side surface; 92: grinding tool; 10: alignment unit; 11: height detector; 12: cleaning device; 13: cleaning and unloading mechanism; 14: display unit; 20: wafer; 20a: front surface; 20b: back surface; 20c: peripheral surface; 22: device; 24: predetermined dividing line; 25: notch; 26a: central area; 26b: peripheral remaining area; 26c: chamfered portion; 26d: removal area; 28: dividing line. DETAILED DESCRIPTION
[0026] Hereinafter, a processing tool according to an embodiment of the present invention will be described in detail with reference to the drawings.
[0027] exist Figure 12 shows a cutting device 1 having a cutting unit 8 , and a grinding wheel 9 , which is a processing tool of the present embodiment, is mounted on the cutting unit 8 . The cutting device 1 has a shell 2 of a substantially rectangular parallelepiped shape, and the cutting device comprises: a box 4 (shown by a double-dotted line), which is placed on a box table 4a of the shell 2; a carry-in and carry-out mechanism 3, which carries a wafer 20 out of the box 4 to a temporary table 5; a conveying mechanism 6, which has a rotating arm for conveying the wafer 20 carried out to the temporary table 5 to a chuck table 7; a cutting unit 8, which is equipped with a grinding tool 9 of the present embodiment for processing the wafer 20 held by the chuck table 7 and the grinding tool 6 is rotatable, and the cutting unit 8 includes a grinding tool cover 81 and a spindle housing 82; an alignment unit 10, which is used to photograph the processing area of the wafer 20 held on the above-mentioned chuck table 7 and detect the area to be processed by the cutting unit 8; a height detector 11, which is arranged adjacent to the alignment unit 10 in the Y-axis direction and is used to detect the thickness of the wafer 20 held by the chuck table 7; a cleaning and carrying-out mechanism 13, which is installed from the chuck table 7 at Figure 1 The wafer 20 is transported to the cleaning device 12 at the loading and unloading position positioned in the middle; and the display unit 14 is arranged on the upper part of the housing 2.
[0028] The chuck table 7 is composed of an adsorption chuck 71 and a frame 72. The adsorption chuck 71 is formed of an air-permeable porous member and constitutes a holding surface. The frame 72 surrounds the adsorption chuck 71. The chuck table 7 is connected to a suction unit (not shown) via the frame 72. By operating the suction unit, negative pressure can be generated on the upper surface of the adsorption chuck 71 to suck and hold the workpiece.
[0029] The shell 2 includes: an X-axis feed mechanism that feeds the chuck table 7 for processing in the X-axis direction; a Y-axis feed mechanism that indexes and feeds the cutting unit 8 in the Y-axis direction perpendicular to the X-axis direction; a Z-axis feed mechanism that moves in the Z-axis direction (up and down direction) perpendicular to the X-axis direction and the Y-axis direction for cutting-in feeding; and a rotation drive mechanism that rotates the chuck table 7. In addition, a controller (not shown) that controls the various action parts of the cutting device 1 is provided inside the shell 2.
[0030] exist Figure 2 (a) shows that the Figure 1 The main part of the cutting unit 8 of the cutting device 1 is enlarged in a three-dimensional view. Figure 2 (b) shows that Figure 2 (a) is a three-dimensional diagram of the decomposed state of the structure. Figure 2In the figure, for the sake of convenience, the mold cover 81 covering the above-mentioned mold 9 is omitted. The cutting unit 8 has: a spindle housing 82; a spindle 83, which is rotatably held in the spindle housing 82; and a mold 9, which is mounted on the front end 83a of the spindle 83 and is selected in a manner that satisfies the conditions described in detail below. A rotation drive source such as an electric motor (not shown) is accommodated on the other end side of the spindle housing 82, and the rotation drive source rotates the spindle 83 to rotate the mold 9 at a high speed.
[0031] Further details of the cutting unit 8, according to Figure 2 As can be seen from (b), the cutting unit 8 includes: a fixing flange 86 formed on the front end 83a side of the spindle 83; a hub portion 86a protruding axially from the center of the fixing flange 86; a mounting flange 87 engaged with the hub portion 86a and cooperating with the fixing flange 86 to clamp the grinding tool 9; and a nut 88 screwed with an external thread 86b formed on the side of the hub portion 86a to tighten the mounting flange 87. The opening 9a of the grinding tool 9 is formed corresponding to the diameter of the hub portion 86a, the hub portion 86a is inserted into the opening 9a of the grinding tool 9, and the mounting flange 87 is mounted on the hub portion 86a, and the nut 88 is screwed and tightened with the external thread 86b, thereby clamping the grinding tool 9 with the fixing flange 86 and the mounting flange 87 and firmly fixing it.
[0032] like Figure 2 As shown in (b), the grinding tool 9 has an annular grinding tool 91 and an annular polishing tool 92 formed integrally with the grinding tool 91. Figure 2 As shown in the enlarged cross-sectional view of a part in the upper left of (b), the grinding tool 91 is a flat-plate-shaped grinding tool having a first side 91a and a second side 91b, and the grinding tool 92 is formed on at least one of the first side 91a or the second side 91b, and is formed on the first side 91a side in the present embodiment. In addition, the grinding tool 9 constituting the processing tool of the present invention is not limited to forming the grinding tool 92 only on the side of any one side of the grinding tool 91 as described above, and the grinding tool 92 may be formed on both the first side 91a and the second side 91b. The abrasive grains constituting the grinding tool 92 and the grinding tool 91 are, for example, diamond abrasive grains, and the preferred bonding material is, for example, any bonding material selected from a resin bonding agent, a ceramic bonding agent, and a metal bonding agent. The grinding tool 92 is a fine-mesh grinding tool for smoothly finishing the surface in contact with the workpiece, and the average particle size (hereinafter referred to as "particle size") of the diamond abrasive grains constituting the grinding tool 92 is appropriately selected according to the material of the workpiece, and is set in a manner smaller than the particle size of the diamond abrasive grains constituting the grinding tool 91. The width (thickness) of the grinding tool 91 and the width (thickness) of the grinding tool 92 in the present invention are required to meet the prescribed conditions, which will be described in detail below.
[0033] Below, refer to Figure 3 to Figure 8 A processing method for removing the chamfered portion of a wafer using the grinding wheel 9 of the processing tool according to the present embodiment and conditions of the grinding wheel 91 and the polishing wheel 92 constituting the grinding wheel 9 will be described.
[0034] In use Figure 1 The cutting device 1 shown implements Figure 3 When the chamfered portion 26c of the wafer 20 shown is removed, a grinding tool preparation step is performed. The wafer 20 to be processed in this embodiment is a semiconductor (e.g., silicon) wafer on which a plurality of devices 22 are formed by being divided on the front side 20a by a plurality of intersecting predetermined dividing lines 24, and has: a central area 26a on which the devices 22 are formed; a peripheral remaining area 26b surrounding the central area 26a; and a chamfered portion 26c on which chamfering is performed at the peripheral end of the peripheral remaining area 26b. Figure 3 , a circular dividing line 28 (indicated by a dotted line) is described that divides the central area 26a and the peripheral remaining area 26b, but the dividing line 28 is marked for convenience of explanation and is not actually formed on the front surface 20a of the wafer 20. Here, for example, the wafer 20 is pre-set to have a thickness of 700 μm and a length L in the radial direction from the outer peripheral end to be removed in the chamfered portion 26c (see Figure 5 ) is 3.0 mm. Furthermore, when the width of the grinding tool 91 is set to H and the width of the polishing tool 92 is set to h, based on the length L (= 3.0 mm) in the radial direction from the outer peripheral end to be removed, the following conditions (1) and (2) are satisfied:
[0035] H+h>L…(1)
[0036] L / 3>h>L / 100…(2)
[0037] Both grinding wheels 9. In the present embodiment, the length L in the radial direction from the outer peripheral end to be removed in the chamfered portion 26c is 3.0 mm, and a grinding wheel 9 with a diameter of 58 mm is prepared, with a width H of 3.0 mm for the grinding wheel 91 and a width h of 0.3 mm for the polishing wheel 92, so that the total width is 3.3 mm.
[0038] Regarding condition (2) of the grinding tool 9 prepared by the above-mentioned grinding tool preparation step, it is more preferable to set it within the range of the size that the width h of the grinding tool 92 is less than L / 20 and greater than L / 60. In addition, the particle size of the diamond abrasive grains constituting the grinding tool 92 is selected corresponding to the physical properties of the silicon constituting the wafer 20, but it is preferable to select the particle size of the diamond abrasive grains constituting the grinding tool 91 within the range of 1.5 times to 5 times the particle size of the diamond abrasive grains constituting the grinding tool 92. More specifically, in the case where 3μm to 10μm is selected as the particle size of the diamond abrasive grains constituting the grinding tool 92, the particle size of the diamond abrasive grains constituting the grinding tool 91 is set within the range of 15μm to 50μm which is 1.5 times to 5 times thereof. If the grinding tool 9 satisfying the above-mentioned condition is prepared in the grinding tool preparation step, then based on Figure 2 The grinding wheel 9 is mounted on the cutting unit 8 as described in (b). In the present embodiment, the grinding wheel 92 is disposed on the front end portion 83a side of the spindle 83 and the grinding wheel 91 is disposed on the spindle housing 82 side.
[0039] After the mold preparation process is performed, the mold is loaded and unloaded by the loading and unloading mechanism 3. Figure 1 The wafer 20 is taken out of the cassette 4 of the cutting device 1 described above and temporarily placed on the temporary placement table 5, and the transfer mechanism 6 is operated to suck the wafer 20 from the temporary placement table 5 and transfer it to the chuck table 7. Figure 3 As shown, the wafer 20 is placed on the chuck table 7 with the back surface 20 b facing downward, and a suction unit (not shown) is operated to generate negative pressure on the suction chuck 71 to hold the wafer by suction.
[0040] After the wafer holding process is performed as described above, the X-axis feed mechanism is operated to position the wafer 20 together with the chuck table 7 directly below the alignment unit 10 and to photograph the wafer 20, and to detect the position of the center of the wafer 20 and the position of the area of the chamfered portion 26c to be removed in the peripheral remaining area 26b with a length L (3.0 mm) in the radial direction from the peripheral end. Figure 4 As shown, the thickness of the area of the chamfered portion 26c to be removed is detected by using the height detector 11. More specifically, as shown in FIG. Figure 5 As shown, the height Z0 of the surface of the chuck worktable 7 and the height Z1 of the front surface 20a at the chamfered portion 26c of the chip 20 are detected, and the difference (Z0-Z1) between the two is calculated as the thickness of the chip 20, and the detected information related to the processing area is stored in a controller omitted from the figure.
[0041] Next, based on the information of the processing area to be removed in the chamfered portion 26c detected by the processing position detection step and stored in the controller, the X-axis feed mechanism and the Y-axis feed mechanism of the cutting device 1 are operated, such as Figure 6 As shown, the chamfered portion 26c of the wafer 20 is positioned directly below the grinder 9 installed on the cutting unit 8. At this time, the grinding grinder 92 of the grinder 9 is positioned above a position that is consistent with the length L in the radial direction from the outer peripheral end to be removed. Then, the grinder 9 is rotated in the direction indicated by the arrow R1 at a specified rotation speed (for example, 30,000 rpm), and the above-mentioned Z-axis feed mechanism is activated to lower the cutting unit 8 in the direction indicated by the arrow R2, so that the grinder 9 cuts into the chamfered portion 26c of the wafer 20. At the same time, as Figure 7 As shown in FIG. 1 , the chuck table 7 is rotated at least once in the direction indicated by the arrow R3 at a predetermined rotation speed (e.g., 0.8 rpm to 3 rpm). Figure 8 As shown in (a), the grinding tool 9 is cut and fed to a position where an area of length L in the radial direction from the outer peripheral end is removed and a predetermined cutting depth DZ (30 μm in this embodiment) is reached. By the above, the chamfered portion 26c of the outer peripheral end of the wafer 20 forming the outer peripheral residual area 26b is removed in an annular shape according to the predetermined cutting depth DZ with a width of length L in the radial direction from the outer peripheral end, as shown in FIG. Figure 8 As shown in (b), the chamfer removal process is completed. In addition, the above-mentioned cutting depth DZ is set according to the thickness of the wafer 20 that is finished by grinding from the back surface 20b side through the back grinding process (detailed description omitted) implemented in the process after the processing method of this embodiment is implemented. In this embodiment, the back surface 20b of the wafer 20 is ground and finished to a thickness of 250μm through the back grinding process implemented later, so the cutting depth DZ in the chamfer removal process is sufficient to be 300μm.
[0042] In the present embodiment, the width H of the grinding tool 91 + the width h of the grinding tool 92 is formed to be larger than the length L in the radial direction from the outer peripheral end to be removed in the chamfered portion 26c of the outer peripheral end portion forming the outer peripheral surplus area 26b (condition (1)), and the width h of the grinding tool 92 is formed to be smaller than L / 3 and larger than L / 100 (condition (2)). Thus, as described above, the grinding tool 92 is positioned on the center side of the wafer 20 and the grinding tool 91 is positioned on the outside, and the wafer 20 is rotated while being rotated at least once at a predetermined cutting depth, thereby, as shown in FIG. Figure 8 As shown in (b), the chamfered portion 26 can be roughly removed by the length L in the radial direction from the outer peripheral end to be removed. At the same time, the outer peripheral surface 20c of the removed area 26d formed in the chamfered portion 26c can be finely processed, thereby improving productivity.
[0043] Regarding the above condition (2), it is more preferable to set the width h of the grinding tool 92 to a size smaller than L / 20 and larger than L / 60. For example, when the length L in the radial direction from the outer peripheral end to be removed is 3.00 mm (3000 μm), it is preferable to set the width h of the grinding tool 92 to 50 μm to 150 μm, adjust the width H of the grinding tool 91 within the range of 2950 μm to 3050 μm, and set the total width (H+h) of the grinding tool 9 to 3100 μm. By setting the width H of the grinding tool 91 and the width h of the grinding tool 92 within such a range, the region of the length L in the radial direction from the outer peripheral end to be removed in the wafer 20 can be roughly removed by the grinding tool 91, and at the same time, the outer peripheral surface 20c of the removed region 26d formed in the chamfered portion 26c can be more efficiently finished.
[0044] In addition, it is preferable that the particle size of the diamond abrasive grains constituting the grinding tool 91 is formed within a range of 1.5 to 5 times the particle size of the diamond abrasive grains constituting the grinding tool 92. More specifically, when the particle size of the diamond abrasive grains constituting the grinding tool 92 is 3 μm to 10 μm in consideration of the material of the wafer 20, the particle size of the diamond abrasive grains constituting the grinding tool 91 can be set within a range of 15 μm to 50 μm. Thus, the affinity when the grinding tool 91 and the grinding tool 92 are formed integrally can be ensured, and the grinding tool 9 can be firmly formed to improve durability, and the area of the length L in the radial direction from the outer peripheral end to be removed in the wafer 20 can be roughly removed efficiently, and the outer peripheral surface 20c of the removed area 26d formed in the chamfered portion 26c can be smoothly finished.
[0045] In the above-mentioned embodiment, when the grinding tool 9 is mounted on the spindle 83 of the grinding unit 8, the grinding tool 92 is mounted on the front end portion 83a side of the spindle 82 and the grinding tool 91 is mounted on the spindle housing 82 side. However, the present invention is not limited to this. The grinding tool 92 side can also be mounted on the grinding unit 8 on the spindle housing 82 side and the grinding tool 91 is mounted on the front end portion 83a side of the spindle 82 to implement the chamfering portion removal process of the above-mentioned processing method. In this case, when implementing the chamfering portion removal process, the grinding tool 92 side is located on the center side of the wafer 20 in the radial direction. More specifically, for example, across Figure 7 The wafer 20 shown in the figure is positioned at the lower left side ( Figure 7 The chamfered portion removal step can be performed by rotating the chuck table 7 (the area where the notch 25 of the wafer 20 shown in the figure is positioned).
Claims
1. A processing tool for removing a chamfered portion of a wafer, wherein the wafer has a central region and a peripheral remaining region surrounding the central region on a front surface, the chamfered portion being formed on the periphery of the peripheral remaining region. in, The processing tool has: an annular grinding tool having an opening at the center for inserting the spindle, and the grinding tool having a first side surface and a second side surface; and A grinding tool formed on at least one of the first side surface or the second side surface, When the length of the chamfered portion to be removed in the radial direction from the outer peripheral end is L, the width of the grinding tool is H, and the width of the polishing tool is h, the processing tool is formed to satisfy the following two conditions (1) and (2): H+h>L…(1) L / 3>h>L / 100…(2).
2. The processing tool according to claim 1, wherein The particle size of the diamond abrasive grains constituting the grinding tool is selected according to the material of the wafer, and the particle size of the diamond abrasive grains constituting the grinding tool is selected within a range of 1.5 to 5 times the particle size of the diamond abrasive grains constituting the grinding tool.
3. The processing tool according to claim 2, wherein: The bonding material constituting the grinding tool and the abrasive tool is selected from any bonding material of a resin bond, a ceramic bond and a metal bond.
4. The processing tool according to claim 1, wherein This wafer is a semiconductor wafer having a device region in which a plurality of devices are divided by a plurality of intersecting division planned lines in the central region.
Citation Information
Patent Citations
Method of dividing laminated wafer
JP2010225976A
JP特许2014-003198