Intermittent supplied high-temperature metallurgical slag continuous conveying device and conveying method
By designing the intermittent high-temperature metallurgical slag continuous conveying device of the cured crushing bed and the material pushing mechanism, the problem of uncontrollable slurry transportation is solved, the continuous conveying and stable feeding of slurry is realized, and the metallurgical slag is promoted. Efficient resource utilization.
Patent Information
- Application Number
- CN202411098624.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-12
- Publication Date
- 2024-11-22
AI Technical Summary
The existing technology cannot realize the continuous transport of smelting slag, resulting in uncontrollable transport rate of smelting slag, and cannot provide stable material feeding process parameters for continuous metal extraction and waste heat recovery, limiting the efficient resource utilization of metallurgical slag. .
A continuous conveying device for intermittent incoming materials is designed, including a curing crushing bed, a curing crusher and a material pushing mechanism. The high-temperature smelting slag is crushed into smelting slag blocks through the solidification crushing bed, and the material pushing mechanism is used to cure it. The transfer device between the crushing bed and the conveyor realizes the continuous transport of smelting slag blocks.
The continuous transportation of high-temperature smelting slag is realized, stable feeding conditions are provided, metal extraction and waste heat recovery are continuously carried out, and efficient resource utilization of metallurgical slag is promoted.
Smart Images

Figure CN118992513A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of steel slag processing, and in particular to a continuous conveying device and a conveying method for intermittently fed high-temperature metallurgical slag. Background Art
[0002] The slag tapping temperature of smelting slag often exceeds 1300℃. After tapping, the slag often needs to be cooled and crushed before the next processing can be carried out, providing good material conditions for the resource utilization of smelting slag.
[0003] Metal smelting production often uses special smelting furnaces. For example, steel and copper smelting uses converters and other equipment. The slag removal process basically uses slag pots for slag collection and transportation. Because each furnace smelting often takes a certain amount of time, the slag collection and transportation process is also divided into slag pots and transported in batches. Therefore, smelting slags such as steel slag and copper slag are mostly intermittent feeding characteristics. This feeding method leads to the processing process also being processed in batches. There is a lack of continuous transportation and conveying process equipment and methods, which is not conducive to subsequent continuous processing, waste heat recovery and other resource processing and utilization.
[0004] At present, the treatment of typical bulk smelting slag such as steel slag and copper slag still mainly uses slag pots for material transfer. Taking the steel slag hot stuffing treatment process as an example, after the slag is discharged from the converter, it is transported to the steel slag crushing area using a hot slag pot. After the high-temperature steel slag is pumped with water, cooled, and crushed, it is taken up by a solid slag pot for the next step of hot stuffing treatment. The material transfer is entirely dependent on the slag pot, which is still an intermittent material transportation method, and it is impossible to achieve continuous material transfer. The intermittent material transportation method results in an uncontrollable conveying rate of the smelting slag, and it is impossible to provide stable material feeding process parameter conditions for continuous metal extraction, waste heat recovery and other treatments, which is not conducive to the efficient resource utilization of metallurgical slag. Therefore, it is urgent to develop a continuous conveying device and method for intermittent incoming high-temperature metallurgical slag. Summary of the invention
[0005] Technical purpose: In view of the above-mentioned shortcomings of the existing high-temperature steel slag transportation, the present invention discloses a continuous transportation device and transportation method for intermittent high-temperature metallurgical slag that can ensure a stable transportation rate.
[0006] Technical solution: To achieve the above technical objectives, the present invention adopts the following technical solution: A device for continuously conveying intermittent high-temperature metallurgical slag comprises a solidification crushing bed for receiving intermittent high-temperature smelting slag, a solidification crusher for crushing the high-temperature smelting slag into smelting slag blocks, and a conveyor for continuously conveying the smelting slag blocks to a processing step. A transfer device for transferring the smelting slag blocks is arranged between the solidification crushing bed and the conveyor, and the transfer device can transfer the smelting slag blocks from the solidification crushing bed to the conveyor in a quantitative manner within a fixed time interval.
[0007] Preferably, the transfer device of the present invention includes a slag pushing bed, both ends of which are connected to the solidification crushing bed and the conveyor, and a plurality of slag pushing troughs are arranged side by side on the slag pushing bed, with the ends of the slag pushing troughs facing the direction of the conveyor, and a pushing mechanism is arranged in each slag pushing trough for pushing the smelting slag blocks in the slag pushing trough to the conveyor.
[0008] Preferably, the pushing mechanism of the present invention comprises a slag pushing plate and a linear power source, the plate surface of the slag pushing plate is vertically arranged to the slag pushing groove, and the driving end of the linear power source is fixedly connected to the slag pushing plate to push the slag pushing plate to move back and forth in the slag pushing groove.
[0009] Preferably, the solidifying crushing bed and slag pushing bed of the present invention are composed of two parts: a liner and a cushion layer. The liner is located below the cushion layer, wherein the liner adopts steel plate as an impact-resistant liner with a thickness of ≥20mm, and the cushion layer adopts cold smelting slag particles with a thickness of ≥100mm.
[0010] Preferably, the solidification crushing bed, slag pushing bed and conveyor of the present invention are arranged in a stepped manner in the height direction, with one end of the slag pushing bed located below the discharge end of the solidification crushing bed and the other end located above the conveyor.
[0011] The present invention discloses a method for continuously conveying intermittent high-temperature metallurgical slag, using the above-mentioned conveying device, comprising the steps of: S01, pouring the high-temperature smelting slag from the slag pot onto the solidification crushing bed, using a solidification crusher to walk and stir on the solidification crushing bed, stirring and crushing the high-temperature smelting slag for a certain period of time, until the high-temperature smelting slag is crushed into smelting slag blocks of a certain particle size; S02, push the smelting slag block as a whole onto the slag pushing bed, and the pushing mechanism on the slag pushing bed operates in sequence to push the smelting slag block in the slag pushing trough onto the conveyor, and the smelting slag block is sent out to the metal extraction and waste heat recovery process for processing through the conveyor.
[0012] Preferably, the temperature of the high-temperature smelting slag of the present invention is 500°C~1800°C, the solidification crusher stirs and crushes the high-temperature smelting slag on the solidification crushing bed for 8 minutes~50 minutes, and after the stirring and crushing treatment, 80% of the particle size of the smelting slag blocks does not exceed 200 mm.
[0013] Preferably, the overall time of pushing slag by the pushing mechanism on the slag pushing bed of the present invention is consistent with the total process time of the high-temperature smelting slag being fed, discharged, crushed by the solidification crushing bed and pushed to the top of the slag pushing bed.
[0014] Beneficial effect: The present invention provides an intermittently fed high-temperature metallurgical slag continuous conveying device and conveying method, which adopts a solidifying crusher to achieve stirring and crushing of the high-temperature smelting slag, and processes the incoming high-temperature steel slag from irregular high-temperature metallurgical slag into smelting slag blocks with relatively uniform particle size, and piles them up above the slag pusher bed, and then adopts a pushing mechanism to evenly push the smelting slag blocks piled on the slag pusher bed to the conveyor, so that the continuous conveying of high-temperature smelting slag is realized on the device, which provides stable and reliable feeding conditions for the subsequent metal extraction and waste heat recovery of the high-temperature smelting slag, ensures that the treatment process can be carried out continuously, and is conducive to the efficient resource utilization of metallurgical slag. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art are briefly introduced below.
[0016] Figure 1 It is the overall structure diagram of the conveying device of the present invention; Figure 2 A top view of the conveying device of the present invention; Among them, 1-solidification crushing bed, 2-high temperature smelting slag, 3-smelting slag block, 4-solidification crusher, 5-conveyor, 6-slag pushing bed, 7-slag pushing trough, 8-slag pushing plate, 9-linear power source. DETAILED DESCRIPTION
[0017] Reference will now be made in detail to embodiments of the present disclosure, one or more examples of which are set forth herein below. Each embodiment and example is provided by explaining the apparatus, composition and materials of the present disclosure, rather than limiting. On the contrary, the following description provides a convenient illustration of an exemplary embodiment for implementing the present disclosure. In fact, it will be clear to those skilled in the art that various modifications and variations can be made in the teachings of the present disclosure without departing from the scope or spirit of the present disclosure. For example, a feature shown or described as a part of an embodiment can be used in conjunction with another embodiment to produce yet another embodiment. It is expected that the present disclosure covers such modifications and variations within the scope of the appended claims and their equivalents. Other objects, features and aspects of the present disclosure are disclosed in or clear from the following detailed description. It will be understood by those of ordinary skill in the art that this discussion is only a description of exemplary embodiments and is not intended to limit the wider aspects of the present disclosure.
[0018] like Figure 1 and Figure 2As shown, the present invention discloses a continuous conveying device for intermittent high-temperature metallurgical slag, comprising a solidification crushing bed 1 for receiving intermittent high-temperature smelting slag, a solidification crusher 4 for crushing the high-temperature smelting slag 2 into smelting slag blocks 3, and a conveyor 5 for continuously conveying the smelting slag blocks 3 to a processing step, and a transfer device for transferring the smelting slag blocks 3 is arranged between the solidification crushing bed 1 and the conveyor 5, and the transfer device can transfer the smelting slag blocks 3 from the solidification crushing bed 1 to the conveyor 5 in a quantitative manner within a fixed time interval.
[0019] The transfer device of the present invention includes a slag pushing bed 6, both ends of which are connected to the solidification crushing bed 1 and the conveyor 5. A plurality of slag pushing troughs 7 are arranged side by side on the slag pushing bed 6, and the ends of the slag pushing troughs 7 are facing the direction of the conveyor 5. A pushing mechanism is arranged in each slag pushing trough 7 for pushing the smelting slag blocks 3 in the slag pushing trough 7 to the conveyor.
[0020] The solidification crushing bed 1, the slag pushing bed 6 and the conveyor 5 are arranged in a stepped manner in the height direction. One end of the slag pushing bed 6 is located below the discharge end of the solidification crushing bed 1. The height of the slag pushing bed 6 is 0.4m~1.6m lower than that of the solidification crushing bed 1. The other end is located above the conveyor 5, so that the smelting slag 3 can be transferred and transported step by step. The conveyor 5 is a chain plate conveyor. The inner groove width of the chain plate used is 0.6m~2.4m, which can meet the unloading and transportation needs of the smelting slag 3; the chain plate is made of steel structure material to meet the high-temperature transportation requirements of the smelting slag 3 materials.
[0021] Among them, the solidification crushing bed 1 and the slag pushing bed 6 of the present invention are both composed of two parts: a lining plate and a cushion layer. The lining plate is located below the cushion layer, wherein the lining plate adopts a steel plate as an impact-resistant lining plate with a thickness of ≥20mm, and the cushion layer adopts cold smelting slag particles with a thickness of ≥100mm. The solidification crusher 4 is a steel structure roller tooth crushing equipment, which moves above the solidification crushing bed 1 and is used for the solidification and crushing of high-temperature smelting slag 2. According to the different amounts of incoming smelting slag, the width of the solidification crushing bed 1 is 2m~8m, the width of the solidification crusher 4, the slag pushing bed 6 and the solidification crushing bed 1 are consistent, the length of the solidification crushing bed 1 is 6m~30m, and the length of the slag pushing bed 6 is 2m~6m.
[0022] The pushing mechanism of the present invention includes a slag pushing plate 8 and a linear power source 9. The plate surface of the slag pushing plate 9 is vertically arranged to the slag pushing groove 7. The driving end of the linear power source 9 is fixedly connected to the slag pushing plate 8, pushing the slag pushing plate 8 to move back and forth in the slag pushing groove 7. The moving stroke of the slag pushing plate 8 can cover the corresponding length of the slag pushing groove 7, thereby realizing the complete unloading of the smelting slag blocks 4 on the slag pushing bed 5; the number of slag pushing grooves 7 is set according to the amount of smelting slag blocks 3 that need to be processed at a single time, and the width of the slag pushing groove 7 is controlled to be 0.5-2.5m.
[0023] The present invention also discloses a method for continuously conveying intermittent high-temperature metallurgical slag, using the above-mentioned conveying device, comprising the steps of: S01, pouring the high-temperature smelting slag 2 from the slag pot onto the solidification crushing bed 1, using the solidification crusher 4 to travel and stir on the solidification crushing bed 1, stirring and crushing the high-temperature smelting slag 2 for a certain period of time, until the high-temperature smelting slag 2 is crushed into smelting slag blocks 3 of a certain particle size; The temperature of the high-temperature smelting slag 2 is 500℃~1800℃, and the solidification crusher 43 stirs and crushes the high-temperature smelting slag 2 on the solidification crushing bed 1 for 8 minutes~50 minutes. After the stirring and crushing treatment, 80% of the particles of the smelting slag blocks do not exceed 200mm in size; when the high-temperature smelting slag 2 is liquid, the high-temperature smelting slag 2 can be cooled by water or air blowing while the solidification crusher 4 is stirring and crushing to promote the rapid transformation of the high-temperature smelting slag 2 into a solid state, thereby controlling the process time to remain stable.
[0024] S02, push the smelting slag block 3 as a whole onto the slag pushing bed 6, and the pushing mechanism on the slag pushing bed 6 operates in sequence to push the smelting slag block 3 in the slag pushing trough 7 onto the conveyor 5, and the smelting slag block 3 is sent to the metal extraction and waste heat recovery process by the conveyor 5 for processing.
[0025] The slag pushing rate of the pushing mechanism on the slag pushing bed 6 remains stable, so that the overall slag pushing time can be controlled. The overall slag pushing time of the pushing mechanism on the slag pushing bed 6 of the present invention is consistent with the total process time of the high-temperature smelting slag 2 being fed and discharged and pushed to the top of the slag pushing bed 6 after being crushed by the solidification crushing bed, thereby ensuring the continuity of the slag pushing bed 6 unloading to the conveyor 5. The conveyor 5 can maintain a stable conveying rate to transport the smelting slag blocks 3, providing stable and reliable feeding conditions for the subsequent metal extraction and waste heat recovery of the high-temperature smelting slag, thereby realizing efficient resource utilization of the smelting slag.
Claims
1. A continuous conveying device for intermittent high-temperature metallurgical slag, characterized in that: The invention comprises a solidification crushing bed (1) for receiving intermittent high-temperature smelting slag, a solidification crusher (4) for crushing the high-temperature smelting slag (2) into smelting slag blocks (3), and a conveyor (5) for continuously conveying the smelting slag blocks (3) to a processing step. A transfer device for transferring the smelting slag blocks (3) is arranged between the solidification crushing bed (1) and the conveyor (5). The transfer device can transfer the smelting slag blocks (3) from the solidification crushing bed (1) to the conveyor (5) in a quantitative manner within a fixed time interval.
2. The intermittent high-temperature metallurgical slag continuous conveying device according to claim 1 is characterized in that: The transfer device comprises a slag pushing bed (6), the two ends of which are connected to the solidification crushing bed (1) and the conveyor (5), a plurality of slag pushing grooves (7) are arranged side by side on the slag pushing bed (6), the ends of the slag pushing grooves (7) are oriented in the direction of the conveyor (5), and a pushing mechanism for pushing the smelting slag block (3) in the slag pushing groove (7) to the conveyor is arranged in each slag pushing groove (7).
3. The intermittent high-temperature metallurgical slag continuous conveying device according to claim 2 is characterized in that: The material pushing mechanism comprises a slag pushing plate (8) and a linear power source (9); the plate surface of the slag pushing plate (9) is arranged perpendicular to the slag pushing groove (7); the driving end of the linear power source (9) is fixedly connected to the slag pushing plate (8) to push the slag pushing plate (8) to move back and forth in the slag pushing groove (7).
4. The intermittent high-temperature metallurgical slag continuous conveying device according to claim 2 is characterized in that: The solidification crushing bed (1) and the slag pushing bed (6) are both composed of a liner and a cushion layer. The liner is located below the cushion layer, wherein the liner is made of steel plate as an impact-resistant liner with a thickness of ≥20 mm, and the cushion layer is made of cold smelting slag particles with a thickness of ≥100 mm.
5. The device for continuously conveying intermittent high-temperature metallurgical slag according to claim 2, characterized in that: The solidification crushing bed (1), the slag pushing bed (6) and the conveyor (5) are arranged in a stepped manner in the height direction; one end of the slag pushing bed (6) is located below the discharge end of the solidification crushing bed (1), and the other end is located above the conveyor (5).
6. A method for continuously conveying intermittent high-temperature metallurgical slag, using the conveying device according to any one of claims 1 to 5, characterized in that: Includes steps: S01, pouring the high-temperature smelting slag (2) from the slag pot onto the solidification crushing bed (1), using the solidification crusher (4) to move and stir on the solidification crushing bed (1), stirring and crushing the high-temperature smelting slag (2) for a certain period of time, until the high-temperature smelting slag (2) is crushed into smelting slag blocks (3) of a certain particle size; S02, pushing the smelting slag block (3) as a whole onto the slag pushing bed (6), and the pushing mechanism on the slag pushing bed (6) operates in sequence to push the smelting slag block (3) in the slag pushing trough (7) onto the conveyor (5), and the smelting slag block (3) is transported to the metal extraction and waste heat recovery process for processing via the conveyor (5).
7. The method for continuous conveying of intermittent high-temperature metallurgical slag according to claim 6, characterized in that: The temperature of the high-temperature smelting slag (2) is 500° C. to 1800° C. The solidification crusher (43) stirs and crushes the high-temperature smelting slag (2) on the solidification crushing bed (1) for 8 minutes to 50 minutes. After the stirring and crushing process, 80% of the particles of the smelting slag block (4) have a particle size of no more than 200 mm.
8. The method for continuous conveying of intermittent high-temperature metallurgical slag according to claim 6, characterized in that: The overall time for the pushing mechanism on the slag pushing bed (6) to push the slag is consistent with the total process time of the high-temperature smelting slag (2) being fed, discharged, crushed by the solidification crushing bed, and pushed to the top of the slag pushing bed (6).
Citation Information
Patent Citations
Plastic granulator with screening function
CN112917734A
High-temperature steel slag crushing and flattening method and device
CN115608468A
Fully-closed blast cooling and waste heat recovery method and device for sintered ore
CN115615184A