Preparation method and application of low-resistivity composite current collector
By using DC magnetron sputtering and high-power pulse magnetron sputtering technology in the composite fluid collection, a low resistivity composite fluid collection is formed, which solves the problem of poor density of the composite fluid collection and significantly improves the performance of the battery.
Patent Information
- Application Number
- CN202411228195.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-03
- Publication Date
- 2024-11-22
AI Technical Summary
Poor density of composite liquid collectors during magnetron control leads to an increase in battery resistivity, affecting cycle life, energy density and safety performance.
The copper metallization treatment is performed using DC magnetron sputtering technology, and then the tungsten target is irradiated by high-power pulse magnetron sputtering technology to form a composite fluid with low resistivity.
It improves the density of the composite liquid collector, significantly reduces the resistivity, and improves the cycle life, energy density and safety performance of the battery.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of current collectors, and in particular to a preparation method and application of a low-resistivity composite current collector. Background Art
[0002] With the rapid development of new energy and electronic technology, improving battery cycle life, energy density, safety and other performance has become a top priority in battery development. As a very important part of the battery, the current collector is used to collect the current generated by the active material of the battery to form a larger current output. Its performance will directly affect the battery's cycle life, energy density, safety and other performance.
[0003] At present, the positive and negative electrodes in lithium batteries and sodium batteries mostly use copper foil and aluminum foil as current collectors. This type of current collector is expensive and heavier, which is not conducive to controlling battery costs and improving energy density. In this regard, compared with traditional foil current collectors, composite current collectors have obvious advantages. Composite current collectors are usually a "sandwich" structure, with a polymer high molecular layer as the inner layer and metal conductive layers on both sides; because the metal layer on its surface is thinner and the internal polymer layer is lighter, it can well reduce the overall weight of the current collector, thereby increasing the energy density of lithium-ion batteries; at the same time, the thinner metal layer on the surface of the composite current collector is easier to disconnect than the traditional foil current collector when the lithium-ion battery has thermal runaway, thereby isolating the connection between the active material and the current collector, preventing the lithium-ion battery from continuing to have thermal runaway, which can improve the safety performance of the battery.
[0004] Although the composite current collector has the advantages of low cost and light weight, the high-speed deposition during the magnetron process can easily lead to more defects in the composite current collector film, resulting in poor density, which in turn increases the resistivity of the battery, ultimately reducing the battery's cycle life, energy density and safety performance.
[0005] Based on this, the present invention will provide a method for preparing a low-resistivity composite current collector, which is of great significance. Summary of the invention
[0006] The purpose of the present invention is to provide a preparation method and application of a low-resistivity composite current collector to solve the problems raised in the above background technology.
[0007] In order to solve the above technical problems, the present invention provides the following technical solutions: A method for preparing a low resistivity composite current collector comprises the following steps: S1: DC magnetron sputtering technology is used, copper is used as a target material, and a base film is used as a substrate, and the base film is metallized to obtain a metallized film; S2: High-power pulsed magnetron sputtering technology is used, with tungsten as the target material and the metallized film as the substrate. The metallized film is irradiated and finally cooled to obtain a low-resistivity composite current collector.
[0008] Furthermore, the preparation method of the low resistivity composite current collector is specifically as follows: S1: Surface treatment of copper, tungsten and substrate film to ensure that the surface is smooth and free of impurities for standby use; S2: Using DC magnetron sputtering technology, with copper as the target material and the base film as the substrate, the base film is metallized, and a copper layer is sputtered and deposited on its surface to obtain a metallized film; S3: After the DC magnetron sputtering is completed, the metallized film is irradiated by high-power pulsed magnetron sputtering technology within 3 to 5 seconds. Tungsten is used as the target material and the metallized film is used as the substrate. A tungsten layer is sputtered and deposited on the copper layer of the metallized film. Finally, after cooling, a low-resistivity composite current collector is obtained.
[0009] Furthermore, the base film is a PP film with a thickness of 5-10 μm.
[0010] Furthermore, the metallization treatment is specifically: sputtering and depositing a copper layer with a thickness of 30-50 nm on both surfaces of the base film.
[0011] Furthermore, the process parameters of the irradiation treatment are: pulse width of 30~100μs, pulse frequency of 150~200Hz, average power of 10~15kW, pulse peak power of 1~1.5MW, and Ar gas pressure of 0.5~0.6Pa.
[0012] Furthermore, the irradiation treatment is specifically as follows: sputtering and depositing a tungsten layer with a thickness of 5-10 nm on the copper layer of the metallized film.
[0013] Furthermore, the distance between the target and the substrate during the irradiation process is 10-13 cm.
[0014] Furthermore, during the metallization and irradiation processes, the cooling temperature of the substrate is controlled to be between -20 and -10°C.
[0015] Furthermore, the cooling temperature of the low resistivity composite current collector is 0-20°C.
[0016] Too high process parameters such as pulse characteristics, pulse peak power, gas pressure, temperature, and too low target-substrate distance will lead to excessive irradiation energy, which will cause excessive temperature rise on the surface of the metallized film and damage the substrate; while too low process parameters such as pulse characteristics, pulse peak power, gas pressure, temperature, and too high target-substrate distance will lead to insufficient irradiation energy, which will lead to insufficient atomic migration energy, making it impossible for the sputtered film to achieve a dense effect, affecting the performance of the finished product, so the process parameters need to be strictly limited.
[0017] Furthermore, the low-resistivity composite current collector is used in a battery.
[0018] Compared with the prior art, the beneficial effects achieved by the present invention are: (1) The present invention uses high-power pulsed magnetron sputtering technology to irradiate tungsten, successfully solving the problem of insufficient mobility of thermally driven adsorbed atoms in conventional composite current collectors, so that the atomic mobility can be improved at a lower substrate temperature (below 130°C), thereby successfully obtaining a composite current collector with better metal layer density; (2) The composite current collector has a lower resistivity. Using it to make batteries can significantly improve the battery's cycle life, energy density, safety and other performance. DETAILED DESCRIPTION
[0019] The following is a preferred implementation of the embodiment of the present invention. Obviously, the described embodiment is only a part of the embodiment of the present invention, not all of the embodiments. For ordinary technicians in this technical field, all other embodiments obtained by ordinary technicians in this field without creative work without departing from the principle of the embodiment of the present invention are within the scope of protection of the present invention.
[0020] Example 1: A method for preparing a low resistivity composite current collector: S1: Surface treatment is performed on the copper target, tungsten target and substrate film to make their surfaces smooth and free of impurities for standby use; S2: Using DC magnetron sputtering technology, with copper as the target material and the base film as the substrate, a 40 μm thick copper layer was sputtered and deposited on both surfaces of a 6 μm thick PP film, during which the cooling temperature of the PP film was controlled to be -10°C, to obtain a metallized film; S3: After the DC magnetron sputtering technology is completed, the metallized film is irradiated by high-power pulsed magnetron sputtering technology within 3 to 5 seconds, and the process parameters of the irradiation treatment are set as follows: pulse width of 100μs, pulse frequency of 200Hz, average power of 10kW, pulse peak power of 1MW, Ar gas pressure of 0.5Pa; tungsten is used as the target material and the metallized film is used as the substrate, and a 5nm thick tungsten layer is sputtered and deposited on the copper layer of the metallized film. During this period, the cooling temperature of the metallized film is controlled to be -10℃, and the target-substrate distance is 10cm; after the irradiation is completed, it is cooled at 20℃ to obtain a low resistivity composite current collector.
[0021] Based on Example 1, Examples 2 to 7 and Comparative Examples 1 to 2 are provided: Embodiment 2: Compared with Embodiment 1, the difference is that: the pulse width in the process parameters of the irradiation treatment is 80 μs; Embodiment 3: Compared with Embodiment 1, the difference is that: the pulse frequency in the process parameters of the irradiation treatment is 180 Hz; Embodiment 4: Compared with Embodiment 1, the difference is that: the average power in the process parameters of the irradiation treatment is 15 kW; Example 5: Compared with Example 1, the difference is that the target-substrate distance in the process parameters of the irradiation treatment is 12 cm; Embodiment 6: Compared with Embodiment 1, the difference is that: the Ar gas pressure in the process parameters of the irradiation treatment is 0.6 Pa; Embodiment 7: Compared with Embodiment 1, the difference is that: the pulse peak power in the process parameters of the irradiation treatment is 1.5 MW; Embodiment 8: Compared with Embodiment 1, the difference is that: a tungsten layer with a thickness of 10 nm is sputter-deposited on the copper layer of the metallized film; Comparative Example 1: Compared with Example 1, the difference is that: high-power pulsed magnetron sputtering irradiation treatment is not performed; Comparative Example 2: Compared with Example 1, the difference is that the pulse peak power in the process parameters of the irradiation treatment is 0.5 MW.
[0022] Performance test: The resistivity of the low resistivity composite current collectors prepared in Examples 1 to 8 and the composite current collectors prepared in Comparative Examples 1 to 2 was tested using a RM3545 resistance meter. The specific test results are shown in Table 1 below: Table 1
[0023] Result analysis: By comparing the data of Example 1 and Comparative Example 1 in Table 1 above, it can be seen that the present invention successfully prepared a low-resistivity composite current collector by using high-power pulsed magnetron sputtering technology for tungsten irradiation, and the lowest resistivity reached 3.0×10-8 Ω·m; in addition, by comparing Examples 1 to 8 with Comparative Example 2, it can be seen that the process parameters of high-power pulsed magnetron sputtering have a great influence on the resistivity of the low-resistance composite current collector, that is, the quality of the irradiation treatment has an important influence on the film density of the low-resistivity composite current collector.
[0024] Finally, it should be noted that the above is only a preferred embodiment of the present invention, but the protection scope of this application is not limited thereto. Any changes or substitutions that can be easily thought of by any technician familiar with the technical field within the spirit and principle of the present invention and within the technical scope disclosed in this application should be included in the protection scope of this application; in the absence of conflict, the embodiments of this application and the features in the embodiments can be combined with each other. Therefore, the protection scope of this application shall be based on the protection scope of the claims.
Claims
1. A method for preparing a low resistivity composite current collector, characterized in that: The following steps are involved: S1: DC magnetron sputtering technology is used, copper is used as a target material, and a base film is used as a substrate, and the base film is metallized to obtain a metallized film; S2: Using high-power pulsed magnetron sputtering technology, with tungsten as the target material and metallized film as the substrate, the metallized film is irradiated and cooled to obtain a low-resistivity composite current collector.
2. The method for preparing a low resistivity composite current collector according to claim 1, characterized in that: In S1, the metallization treatment specifically includes: sputtering and depositing a copper layer with a thickness of 30-50 nm on both surfaces of the base film.
3. The method for preparing a low resistivity composite current collector according to claim 1, characterized in that: In S2, the process parameters of the irradiation treatment are: pulse width of 30~100μs, pulse frequency of 150~200Hz, average power of 10~15kW, pulse peak power of 1~1.5MW, and Ar gas pressure of 0.5~0.6Pa.
4. The method for preparing a low resistivity composite current collector according to claim 1, characterized in that: In S2, the irradiation treatment specifically includes: sputtering and depositing a tungsten layer with a thickness of 5-10 nm on the copper layer of the metallized film.
5. The method for preparing a low resistivity composite current collector according to claim 1, characterized in that: In S2, the distance between the target and the substrate during the irradiation process is 10-13 cm.
6. The method for preparing a low resistivity composite current collector according to claim 1, characterized in that: During the metallization and irradiation processes, the cooling temperature of the substrate is controlled at -20~-10°C.
7. The method for preparing a low resistivity composite current collector according to claim 1, characterized in that: In S2, the cooling temperature of the low resistivity composite current collector is 0-20°C.
8. A low-resistivity composite current collector prepared by the method for preparing a low-resistivity composite current collector according to any one of claims 1 to 7.
9. Use of the low-resistivity composite current collector according to claim 8 in a battery.