Bamboo wood pretreatment process and method for preparing bamboo source cellulose

Through mechanical collection, cooking, enzymatic decomposition and the use of biodegradable solvents, the problem of environmental pollution in the existing bamboo cellulose extraction process has been solved, pollution-free process flow and high-performance products have been achieved, and resource sustainability has been promoted. use.

CN118996883AInactive Publication Date: 2024-11-22COMMUNIST YOUTH BRANCH OF CHINA ACAD OF TEXTILE SCI
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411298642.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-18
Publication Date
2024-11-22
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The solvents and chemicals used in the existing bamboo cellulose extraction process cause pollution to the environment and lead to water, atmosphere and soil pollution. A pollution-free extraction process is needed.

Method used

Use mechanical or manual methods to collect bamboo, and use biodegradable solvents and environmentally friendly processes to reduce the environment through cooking, grinding, enzymatic degradation, centrifugation, heating and mixing with biodegradable solvents, membrane separation, washing, drying and chemical modification. pollute.

Benefits of technology

The pollution-free bamboo cellulose extraction is achieved, which reduces the risk to the environment and the health threat of operators, improves the performance and market competitiveness of the final product, and promotes the sustainable use of resources.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention relates to the technical field of extraction processes and preparation methods thereof, in particular to a bamboo pretreatment process and method for preparing bamboo cellulose. The technical problem is that in the use process of an extraction process and a preparation method thereof, solvents or chemicals such as a chlorinating agent, an organic solvent, an alkaline substance or a surfactant which are harmful to the environment are partially used, and the substances possibly pollute water sources, atmosphere and soil in the extraction process and cause negative effects on the environment. According to the technical scheme, the bamboo wood pretreatment process and method for preparing the bamboo source cellulose comprise the following steps of 1, raw material preparation, 2, pretreatment, 3, grinding, 4, enzymolysis, 5, extraction, 6, separation, 7, purification and the like. According to the extraction process, in the process of extracting the bamboo source cellulose, a biodegradable solvent is used, so that the influence on the environment can be reduced, meanwhile, the health risk on operators can be reduced, and the possibility of safety accidents can be reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of extraction technology and preparation method thereof, and in particular to a bamboo material pretreatment technology and method for preparing bamboo-derived cellulose. Background Art

[0002] The extraction processes used for bamboo cellulose on the market are relatively simple, and some of them use solvents or chemicals that are harmful to the environment, such as chlorinating agents, organic solvents, alkaline substances or surfactants. These substances may pollute water sources, atmosphere and soil during the extraction process, causing negative impacts on the environment. Therefore, it is urgent to set up a process and preparation method for pollution-free extraction of bamboo cellulose, which will help protect natural resources, reduce long-term impacts on the environment, and reduce the risks of water pollution, air pollution and soil pollution. Summary of the invention

[0003] In order to overcome the problem that in the process of extraction technology and its preparation method, some solvents or chemicals harmful to the environment will be used, such as chlorinating agents, organic solvents, alkaline substances or surfactants, etc. These substances may pollute water sources, atmosphere and soil during the extraction process, causing negative impacts on the environment.

[0004] The technical solution of the present invention is: a bamboo material pretreatment process and method for preparing bamboo-derived cellulose, characterized in that the steps are as follows:

[0005] Step 1: Raw material preparation

[0006] Collect bamboo from bamboo forests mechanically or manually, using harvesters to cut the bamboo into appropriate lengths and widths;

[0007] Step 2: Preprocessing

[0008] Pre-cook the bamboo in step 1 using a steamer or autoclave to soften the bamboo. The pre-cooking time ranges from 15 minutes to 1 hour.

[0009] Step 3: Grinding

[0010] Use a grinder to grind the pre-cooked bamboo from step 2 into pulp;

[0011] Step 4: Enzymatic hydrolysis

[0012] Put the pulp in step 3 into the enzymolysis tank, mix the cellulase with the bamboo pulp, and perform enzymolysis reaction. At the same time, use a stirring device to decompose the cellulose into soluble sugars. The optimum temperature of the cellulase is between 40°C and 50°C, and the pH value is between 4.5 and 5.5. When the enzymolysis reaction reaches the expected effect, hot water or chemical reagents such as NaOH can be used to terminate the reaction and stop the activity of the enzyme.

[0013] Step 5: Extraction

[0014] The centrifuge centrifuges the mixture after enzymatic hydrolysis to separate the cellulose solution and the solid residue, collects the cellulose solution in a stirring tank, adds a biodegradable solvent to the cellulose solution, and heats and stirs it at the same time to improve the mixing and dissolving efficiency;

[0015] Step 6: Separation

[0016] Use membrane separation equipment to preliminarily purify the cellulose solution, and select microfiltration membrane, nanofiltration membrane or ultrafiltration membrane to meet the purification requirements of the cellulose solution;

[0017] Step 7: Purification

[0018] The separated cellulose solution is washed using a washing device to remove impurities;

[0019] Step 8: Drying

[0020] Drying the cellulose solution into cellulose powder using a fluidized bed dryer or a drum dryer;

[0021] Step 9: Modification

[0022] The cellulose is chemically modified using a reactor and corresponding chemical reagents to improve its specific physical and chemical properties. For etherification modification, strong acids such as sulfuric acid or phosphoric acid are used as catalysts to react cellulose with chloroacetic acid derivatives such as 2-chloroacetic acid or 3-chloro-2-hydroxypropionic acid to introduce hydroxyethyl or hydroxypropyl functional groups to improve the hydrophilicity and swelling properties of cellulose. For esterification modification, acid catalysts such as sulfuric acid or hydrochloric acid are used to react cellulose with formic acid, acetic acid or chloroacetic acid (etc.) to react with cellulose.

[0023] Introducing methoxy, acetate or chloroacetate groups to improve the solubility and biodegradability of cellulose;

[0024] If acylation modification is used, an acid catalyst such as sulfuric acid or phosphoric acid is used to react cellulose with an acylating agent such as benzoyl chloride or p-toluenesulfonyl chloride to introduce benzoyl or p-toluenesulfonyl groups to improve the solubility and thermal stability of cellulose. If graft copolymerization modification is used, a free radical initiator such as benzoyl peroxide BPO, azobisisobutyronitrile AIBN, etc. is used to graft copolymerize cellulose with vinyl monomers such as acrylic acid and acrylonitrile to introduce polymer chains to improve the mechanical properties and functionality of cellulose.

[0025] If oxidative modification is used, cellulose is oxidized using oxidants such as potassium persulfate and potassium permanganate.

[0026] Introducing functional groups such as aldehyde and carboxyl to improve the hydrophilicity and chemical activity of cellulose;

[0027] Step 10: Forming and packaging

[0028] The modified cellulose powder is made into a granular product by a granulator, and then the cellulose particles are made into the desired molded products by an extruder, a calender or other molding equipment, and the crushed cellulose particles are packaged by an automatic packaging machine.

[0029] Preferably, in step 2, the precooking temperature is between 100° C. and 150° C., the precooking pressure is between 0.1 MPa and 2 MPa, and the pH value is between 8 and 12.

[0030] Preferably, the refining time in step three is between 8 minutes and 30 minutes.

[0031] Preferably, the biodegradable solvent in step five can be ethanol or propanol, which is highly efficient and environmentally friendly and can reduce the impact on the environment.

[0032] Preferably, if ethanol is used as the biodegradable solvent in the stirred tank, the heating temperature is between 40°C and 60°C; if propanol is used, the heating temperature is between 50°C and 70°C.

[0033] Preferably, the heating rate of the stirred tank should be increased slowly to avoid damage to the cellulose structure.

[0034] Preferably, in step seven, an alkaline or neutral washing liquid may be used to wash the cellulose solution, and the washing time is between 10 minutes and 50 minutes.

[0035] Beneficial effects of the present invention:

[0036] 1. This extraction process uses biodegradable solvents in the process of extracting bamboo cellulose, which can reduce the impact on the environment. These solvents can be decomposed by microorganisms in the natural environment, reducing pollution to the environment. At the same time, it can reduce the risk to the health of operators and the possibility of safety accidents. The pollution-free extraction process is conducive to the sustainable use of resources, helps to protect natural resources, reduces the long-term impact on the environment, further improves the performance and market competitiveness of the final product, and facilitates long-term sustainable development preparation and use. DETAILED DESCRIPTION

[0037] Example 1

[0038] A bamboo material pretreatment process and method for preparing bamboo-derived cellulose, characterized in that the steps are as follows:

[0039] Step 1: Raw material preparation

[0040] Collect bamboo from bamboo forests mechanically or manually, using harvesters to cut the bamboo into appropriate lengths and widths;

[0041] Step 2: Preprocessing

[0042] Use a cooking pot or an autoclave to precook the bamboo in step 1 to soften the bamboo, the precooking time is 15 minutes, the precooking temperature is 100° C., the precooking pressure value is 0.1 MPa, and the pH value is 8;

[0043] Step 3: Grinding

[0044] Use a grinder to grind the pre-cooked bamboo from step 2 into pulp for 8 minutes;

[0045] Step 4: Enzymatic hydrolysis

[0046] Put the pulp in step 3 into the enzymolysis tank, mix the cellulase with the bamboo pulp, and perform enzymolysis reaction. At the same time, use a stirring device to decompose the cellulose into soluble sugars. The optimum temperature of the cellulase is 40°C and the pH value is 4.5. When the enzymolysis reaction reaches the expected effect, hot water or chemical reagents such as NaOH can be used to terminate the reaction and stop the activity of the enzyme.

[0047] Step 5: Extraction

[0048] The centrifuge centrifuges the mixture after enzymatic hydrolysis to separate the cellulose solution and the solid residue. The cellulose solution is collected in a stirring tank, and a biodegradable solvent is added to the cellulose solution, and heating and stirring are performed at the same time to improve the mixing and dissolution efficiency. The biodegradable solvent can be ethanol or propanol, which is efficient and environmentally friendly and can reduce the impact on the environment. If ethanol is used as the biodegradable solvent in the stirring tank, the heating temperature is 40°C, and if propanol is used, the heating temperature is 50°C. The heating speed of the stirring tank should be increased slowly to avoid damage to the cellulose structure.

[0049] Step 6: Separation

[0050] Use membrane separation equipment to preliminarily purify the cellulose solution, and select microfiltration membrane, nanofiltration membrane or ultrafiltration membrane to meet the purification requirements of the cellulose solution;

[0051] Step 7: Purification

[0052] The separated cellulose solution is washed with a washing device to remove impurities. The cellulose solution can be washed with an alkaline or neutral washing liquid for 10 minutes;

[0053] Step 8: Drying

[0054] Drying the cellulose solution into cellulose powder using a fluidized bed dryer or a drum dryer;

[0055] Step 9: Modification

[0056] The cellulose is chemically modified using a reactor and corresponding chemical reagents to improve its specific physical and chemical properties; if etherification modification is used, strong acids such as sulfuric acid or phosphoric acid are used as catalysts to etherify cellulose with chloroacetic acid derivatives such as 2-chloroacetic acid or 3-chloro-2-hydroxypropionic acid to introduce hydroxyethyl or hydroxypropyl functional groups to improve the hydrophilicity and swelling properties of cellulose; if esterification modification is used, acid catalysts such as sulfuric acid or hydrochloric acid are used to esterify cellulose with formic acid, acetic acid or chloroacetic acid (etc.) to introduce methoxyl, acetate or chloroacetate groups to improve the solubility and biodegradability of cellulose; if acylation modification is used, sulfuric acid or phosphoric acid is used as a catalyst to esterify cellulose with formic acid, acetic acid or chloroacetic acid (etc.) to introduce methoxyl, acetate or chloroacetate groups to improve the solubility and biodegradability of cellulose. Using acid catalysts such as benzoyl chloride and p-toluenesulfonyl chloride to react cellulose with acylating agents such as benzoyl chloride and p-toluenesulfonyl chloride to introduce benzoyl or p-toluenesulfonyl groups, thereby improving the solubility and thermal stability of cellulose. For graft copolymerization modification, using free radical initiators such as benzoyl peroxide BPO and azobisisobutyronitrile AIBN to graft copolymerize cellulose with vinyl monomers such as acrylic acid and acrylonitrile to introduce polymer chains and improve the mechanical properties and functionality of cellulose. For oxidative modification, using oxidants such as potassium persulfate and potassium permanganate to oxidize cellulose, introduce functional groups such as aldehyde and carboxyl groups, and improve the hydrophilicity and chemical activity of cellulose.

[0057] Step 10: Forming and packaging

[0058] The modified cellulose powder is made into a granular product by a granulator, and then the cellulose particles are made into the desired molded products by an extruder, a calender or other molding equipment, and the crushed cellulose particles are packaged by an automatic packaging machine.

[0059] Example 2

[0060] A bamboo pretreatment process and method for preparing bamboo-derived cellulose, characterized in that the steps are as follows: Step 1: Raw material preparation: collecting bamboo from a bamboo forest by mechanical or manual methods, and using a harvester to cut the bamboo into appropriate lengths and widths;

[0061] Step 2: Preprocessing

[0062] Precooking the bamboo in step 1 in a cooking pot or an autoclave to soften the bamboo, the precooking time is between 45 minutes, the precooking temperature is between 125° C., the precooking pressure value is between 1 MPa, and the pH value is 10;

[0063] Step 3: Grinding

[0064] Use a grinder to grind the pre-cooked bamboo from step 2 into pulp for 20 minutes;

[0065] Step 4: Enzymatic hydrolysis

[0066] Put the pulp in step 3 into the enzymolysis tank, mix the cellulase with the bamboo pulp, and perform enzymolysis reaction. At the same time, use a stirring device to decompose the cellulose into soluble sugars. The optimum temperature of the cellulase is 50°C and the pH value is 5.5. When the enzymolysis reaction reaches the expected effect, hot water or chemical reagents such as NaOH can be used to terminate the reaction and stop the activity of the enzyme.

[0067] Step 5: Extraction

[0068] The centrifuge centrifuges the mixture after enzymatic hydrolysis to separate the cellulose solution and the solid residue. The cellulose solution is collected in a stirring tank. A biodegradable solvent is added to the cellulose solution, and heating and stirring are performed at the same time to improve the mixing and dissolution efficiency. The biodegradable solvent can be ethanol or propanol, which is efficient and environmentally friendly and can reduce the impact on the environment. If ethanol is used as the biodegradable solvent in the stirring tank, the heating temperature is 50°C, and if propanol is used, the heating temperature is 60°C. The heating speed of the stirring tank should be increased slowly to avoid damage to the cellulose structure.

[0069] Step 6: Separation

[0070] Use membrane separation equipment to preliminarily purify the cellulose solution, and select microfiltration membrane, nanofiltration membrane or ultrafiltration membrane to meet the purification requirements of the cellulose solution;

[0071] Step 7: Purification

[0072] The separated cellulose solution is washed with a washing device to remove impurities. The cellulose solution can be washed with an alkaline or neutral washing liquid for 30 minutes;

[0073] Step 8: Drying

[0074] Drying the cellulose solution into cellulose powder using a fluidized bed dryer or a drum dryer;

[0075] Step 9: Modification

[0076] The cellulose is chemically modified using a reactor and corresponding chemical reagents to improve its specific physical and chemical properties; if etherification modification is used, strong acids such as sulfuric acid or phosphoric acid are used as catalysts to etherify cellulose with chloroacetic acid derivatives such as 2-chloroacetic acid or 3-chloro-2-hydroxypropionic acid to introduce hydroxyethyl or hydroxypropyl functional groups to improve the hydrophilicity and swelling properties of cellulose; if esterification modification is used, acid catalysts such as sulfuric acid or hydrochloric acid are used to esterify cellulose with formic acid, acetic acid or chloroacetic acid (etc.) to introduce methoxyl, acetate or chloroacetate groups to improve the solubility and biodegradability of cellulose; if acylation modification is used, sulfuric acid or phosphoric acid is used as a catalyst to esterify cellulose with formic acid, acetic acid or chloroacetic acid (etc.) to introduce methoxyl, acetate or chloroacetate groups to improve the solubility and biodegradability of cellulose. Using acid catalysts such as benzoyl chloride and p-toluenesulfonyl chloride to react cellulose with acylating agents such as benzoyl chloride and p-toluenesulfonyl chloride to introduce benzoyl or p-toluenesulfonyl groups, thereby improving the solubility and thermal stability of cellulose. For graft copolymerization modification, using free radical initiators such as benzoyl peroxide BPO and azobisisobutyronitrile AIBN to graft copolymerize cellulose with vinyl monomers such as acrylic acid and acrylonitrile to introduce polymer chains and improve the mechanical properties and functionality of cellulose. For oxidative modification, using oxidants such as potassium persulfate and potassium permanganate to oxidize cellulose, introduce functional groups such as aldehyde and carboxyl groups, and improve the hydrophilicity and chemical activity of cellulose.

[0077] Step 10: Forming and packaging

[0078] The modified cellulose powder is made into a granular product by a granulator, and then the cellulose particles are made into the desired molded products by an extruder, a calender or other molding equipment, and the crushed cellulose particles are packaged by an automatic packaging machine.

[0079] Example 3

[0080] A bamboo pretreatment process and method for preparing bamboo-derived cellulose, characterized in that the steps are as follows: Step 1: Raw material preparation: collecting bamboo from a bamboo forest by mechanical or manual methods, and using a harvester to cut the bamboo into appropriate lengths and widths;

[0081] Step 2: Preprocessing

[0082] Use a cooking pot or an autoclave to precook the bamboo in step 1 to soften the bamboo, the precooking time is 1 hour, the precooking temperature is 150° C., the precooking pressure value is 2 MPa, and the pH value is 12;

[0083] Step 3: Grinding

[0084] Use a grinder to grind the pre-cooked bamboo from step 2 into pulp for 30 minutes;

[0085] Step 4: Enzymatic hydrolysis

[0086] Put the pulp in step 3 into the enzymolysis tank, mix the cellulase with the bamboo pulp, and perform enzymolysis reaction. At the same time, use a stirring device to decompose the cellulose into soluble sugars. The optimum temperature of the cellulase is 50°C and the pH value is 5.5. When the enzymolysis reaction reaches the expected effect, hot water or chemical reagents such as NaOH can be used to terminate the reaction and stop the activity of the enzyme.

[0087] Step 5: Extraction

[0088] The centrifuge centrifuges the mixture after enzymatic hydrolysis to separate the cellulose solution and the solid residue. The cellulose solution is collected in a stirring tank, and a biodegradable solvent is added to the cellulose solution, and heating and stirring are performed at the same time to improve the mixing and dissolution efficiency. The biodegradable solvent can be ethanol or propanol, which is efficient and environmentally friendly and can reduce the impact on the environment. If ethanol is used as the biodegradable solvent in the stirring tank, the heating temperature is 60°C, and if propanol is used, the heating temperature is 70°C. The heating speed of the stirring tank should be increased slowly to avoid damage to the cellulose structure.

[0089] Step 6: Separation

[0090] Use membrane separation equipment to preliminarily purify the cellulose solution, and select microfiltration membrane, nanofiltration membrane or ultrafiltration membrane to meet the purification requirements of the cellulose solution;

[0091] Step 7: Purification

[0092] The separated cellulose solution is washed with a washing device to remove impurities. The cellulose solution can be washed with an alkaline or neutral washing liquid for 50 minutes;

[0093] Step 8: Drying

[0094] Drying the cellulose solution into cellulose powder using a fluidized bed dryer or a drum dryer;

[0095] Step 9: Modification

[0096] The cellulose is chemically modified using a reactor and corresponding chemical reagents to improve its specific physical and chemical properties; if etherification modification is used, strong acids such as sulfuric acid or phosphoric acid are used as catalysts to etherify cellulose with chloroacetic acid derivatives such as 2-chloroacetic acid or 3-chloro-2-hydroxypropionic acid to introduce hydroxyethyl or hydroxypropyl functional groups to improve the hydrophilicity and swelling properties of cellulose; if esterification modification is used, acid catalysts such as sulfuric acid or hydrochloric acid are used to esterify cellulose with formic acid, acetic acid or chloroacetic acid (etc.) to introduce methoxyl, acetate or chloroacetate groups to improve the solubility and biodegradability of cellulose; if acylation modification is used, sulfuric acid or phosphoric acid is used as a catalyst to esterify cellulose with formic acid, acetic acid or chloroacetic acid (etc.) to introduce methoxyl, acetate or chloroacetate groups to improve the solubility and biodegradability of cellulose. Using acid catalysts such as benzoyl chloride and p-toluenesulfonyl chloride to react cellulose with acylating agents such as benzoyl chloride and p-toluenesulfonyl chloride to introduce benzoyl or p-toluenesulfonyl groups, thereby improving the solubility and thermal stability of cellulose. For graft copolymerization modification, using free radical initiators such as benzoyl peroxide BPO and azobisisobutyronitrile AIBN to graft copolymerize cellulose with vinyl monomers such as acrylic acid and acrylonitrile to introduce polymer chains and improve the mechanical properties and functionality of cellulose. For oxidative modification, using oxidants such as potassium persulfate and potassium permanganate to oxidize cellulose, introduce functional groups such as aldehyde and carboxyl groups, and improve the hydrophilicity and chemical activity of cellulose.

[0097] Step 10: Forming and packaging

[0098] The modified cellulose powder is made into a granular product by a granulator, and then the cellulose particles are made into the desired molded products by an extruder, a calender or other molding equipment, and the crushed cellulose particles are packaged by an automatic packaging machine.

Claims

1. A bamboo pretreatment process and method for preparing bamboo-derived cellulose, characterized in that: The steps are as follows: Step 1: Raw material preparation Collect bamboo from bamboo forests mechanically or manually, using harvesters to cut the bamboo into appropriate lengths and widths; Step 2: Preprocessing Pre-cook the bamboo in step 1 using a steamer or autoclave to soften the bamboo. The pre-cooking time ranges from 15 minutes to 1 hour. Step 3: Grinding Use a grinder to grind the pre-cooked bamboo from step 2 into pulp; Step 4: Enzymatic hydrolysis Put the pulp in step 3 into the enzymolysis tank, mix the cellulase with the bamboo pulp, and perform enzymolysis reaction. At the same time, use a stirring device to decompose the cellulose into soluble sugars. The optimum temperature of the cellulase is between 40°C and 50°C, and the pH value is between 4.5 and 5.

5. When the enzymolysis reaction reaches the expected effect, hot water or chemical reagents such as NaOH can be used to terminate the reaction and stop the activity of the enzyme. Step 5: Extraction The centrifuge centrifuges the enzymatically hydrolyzed mixture to separate the cellulose solution and solid residue. The cellulose solution is collected in a stirred tank, and a biodegradable solvent is added to the cellulose solution. Heating and stirring are performed simultaneously to improve mixing and dissolving efficiency; Step 6: Separation Use membrane separation equipment to preliminarily purify the cellulose solution, and select microfiltration membrane, nanofiltration membrane or ultrafiltration membrane to meet the purification requirements of the cellulose solution; Step 7: Purification The separated cellulose solution is washed using a washing device to remove impurities; Step 8: Drying Drying the cellulose solution into cellulose powder using a fluidized bed dryer or a drum dryer; Step 9: Modification The cellulose is chemically modified using a reactor and corresponding chemical reagents to improve its specific physical and chemical properties. For etherification modification, strong acids such as sulfuric acid or phosphoric acid are used as catalysts to react cellulose with chloroacetic acid derivatives such as 2-chloroacetic acid or 3-chloro-2-hydroxypropionic acid to introduce hydroxyethyl or hydroxypropyl functional groups to improve the hydrophilicity and swelling properties of cellulose. For esterification modification, acid catalysts such as sulfuric acid or hydrochloric acid are used to react cellulose with formic acid, acetic acid or chloroacetic acid (etc.) to react with cellulose. Introducing methoxy, acetate or chloroacetate groups to improve the solubility and biodegradability of cellulose; If acylation modification is used, an acid catalyst such as sulfuric acid or phosphoric acid is used to react cellulose with an acylating agent such as benzoyl chloride or p-toluenesulfonyl chloride to introduce benzoyl or p-toluenesulfonyl groups to improve the solubility and thermal stability of cellulose. If graft copolymerization modification is used, a free radical initiator such as benzoyl peroxide BPO, azobisisobutyronitrile AIBN, etc. is used to graft copolymerize cellulose with vinyl monomers such as acrylic acid and acrylonitrile to introduce polymer chains to improve the mechanical properties and functionality of cellulose. If oxidative modification is used, cellulose is oxidized using oxidants such as potassium persulfate and potassium permanganate. Introducing functional groups such as aldehyde and carboxyl to improve the hydrophilicity and chemical activity of cellulose; Step 10: Forming and packaging The modified cellulose powder is made into a granular product by a granulator, and then the cellulose particles are made into the desired molded products by an extruder, a calender or other molding equipment, and the crushed cellulose particles are packaged by an automatic packaging machine.

2. A bamboo material pretreatment process and method for preparing bamboo-derived cellulose according to claim 1, characterized in that: In step 2, the pre-cooking temperature is between 100° C. and 150° C., the pre-cooking pressure is between 0.1 MPa and 2 MPa, and the pH value is between 8 and 12.

3. The bamboo material pretreatment process and method for preparing bamboo-derived cellulose according to claim 1, characterized in that: In step 3, the refining time is between 8 minutes and 30 minutes.

4. The bamboo material pretreatment process and method for preparing bamboo-derived cellulose according to claim 1, characterized in that: In step five, the biodegradable solvent can be ethanol or propanol, which is highly efficient and environmentally friendly and can reduce the impact on the environment.

5. A bamboo material pretreatment process and method for preparing bamboo-derived cellulose according to claim 4, characterized in that: If ethanol is used as the biodegradable solvent in the stirred tank, the heating temperature is between 40°C and 60°C, and if propanol is used, the heating temperature is between 50°C and 70°C.

6. A bamboo material pretreatment process and method for preparing bamboo-derived cellulose according to claim 5, characterized in that: The heating rate of the stirred tank should be increased slowly to avoid damage to the cellulose structure.

7. The bamboo material pretreatment process and method for preparing bamboo-derived cellulose according to claim 1, characterized in that: In step seven, an alkaline or neutral washing liquid may be used to wash the cellulose solution, and the washing time is between 10 minutes and 50 minutes.