Helium spray inspection method for multi-cavity shell

By designing calibration housing and spray gun spray or high-temperature baking treatment, the problem of helium adsorption in the housing of multi-cavity microwave components is alleviated, the detection accuracy and production efficiency are improved, and the detection inaccuracy and high misjudgment rate are solved. question.

CN118999928APending Publication Date: 2024-11-22YANGZHOU HAIKE ELECTRONICS TECH CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411308369.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-19
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

During the shell spray inspection of multi-cavity microwave assembly, helium adsorbing on the gold-plated layer leads to inaccurate detection, high misjudgment rate, and affects production efficiency.

Method used

The calibrated housing is the same as the case being inspected. The background leakage rate is measured using a helium mass spectrometer, spray guns and relieve helium adsorption by drying compressed air or high-temperature baking, recording the waiting time to ensure detection accuracy.

Benefits of technology

It effectively reduces the impact of helium adsorption on the detection results, improves detection accuracy and production efficiency, and reduces the probability of misjudgment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118999928A_ABST
    Figure CN118999928A_ABST
Patent Text Reader

Abstract

The invention discloses a helium spraying detection method for a multi-cavity shell. The helium spraying detection method comprises the following steps: S1, designing and processing a calibration shell which is the same as a detected shell in material, appearance and surface treatment; s2, using a helium mass spectrometer leak detector to measure the background leak rate of each calibration cavity without helium adsorption; s3, using a spray gun to spray and calibrate the shell; s4, purging the calibration shell by using dry compressed air or putting the calibration shell into a drying oven for high-temperature baking; s5, the waiting time of other cavities of the calibration shell is measured by using the same method as the step S3 and the step S4; s6, a spray gun is used for carrying out spray test on the first cavity installation device of the detected shell; s7, blowing and washing the detected shell by using dry compressed air or placing the detected shell in a drying oven for high-temperature baking for waiting time, and then carrying out spray inspection work on a second cavity mounting device of the detected shell; s8, using the same method as the step S7 to relieve helium adsorption of other detected shell cavities, and detecting the airtightness; and S9, after all the cavities are detected, the vacuum silicone grease is cleaned.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of sealing and leak detection of airtight packaged microwave components, and in particular relates to a helium spraying detection method for a multi-cavity shell. Background Art

[0002] As an important component of military and civilian electronic equipment, microwave components have the characteristics of high integration, light weight, and high reliability, and are widely used in active phased array radars. At present, microwave components mostly use microwave multi-chip assembly technology, and there are a large number of bare chips in the components. In order to ensure that microwave components can operate stably and reliably for a long time and are not corroded by the environment, microwave components usually have airtightness requirements.

[0003] The factors that affect the airtightness of microwave components mainly include the airtightness of insulators, cable heads, connectors and other installed devices, as well as the sealing after sealing. Before the shell is sealed, helium spray inspection should be carried out first to eliminate unqualified installed devices. The current multifunctional requirements of microwave components make the shell structure more complicated. For multi-cavity sealed shells, each cavity needs to be spray inspected in turn. Since the module is not capped, helium will be adsorbed on the loose and porous gold-plated layer of other cavities during the previous spray inspection. The slow release of the adsorbed helium in the subsequent spray inspection will cause the leakage rate value to increase, affecting the test results. In severe cases, it will cause misjudgment and eliminate qualified products, greatly reducing production efficiency.

[0004] Therefore, in order to solve the problem of helium adsorption during the spray inspection of the shell of multi-cavity microwave components, there is an urgent need for a method to eliminate or alleviate helium adsorption to improve the test accuracy and meet the high reliability requirements of the product. Summary of the invention

[0005] The purpose of the present invention is to solve the above problems and provide a multi-cavity shell helium spray inspection method that can solve the problem of inaccurate detection caused by helium adsorption during the spray inspection of the shell of a multi-cavity microwave component, reduce the probability of misjudgment, and improve product reliability.

[0006] In order to solve the above technical problems, the technical solution of the present invention is: a multi-cavity shell helium spray inspection method, comprising the following steps:

[0007] S1. Design and manufacture a calibration shell with the same material, shape and surface treatment as the shell under test;

[0008] S2. Use a helium mass spectrometer leak detector to measure the background leak rates R0, R1, R2…R of each calibration chamber without helium adsorption. n-1 ;

[0009] S3, use a spray gun to spray and calibrate the shell;

[0010] S4. Use dry compressed air to purge the calibration housing or place the calibration housing in an oven for high-temperature baking. Measure the background leakage rate value R1' of the second cavity of the calibration housing after the helium adsorption relief treatment at specific intervals until R1'<1.5R1, and record the waiting time t1.

[0011] S5, using the same method as step S3 and step S4 to measure the waiting time t2, t3, t4, ... t of the remaining cavities of the calibration shell. n-1 ;

[0012] S6. Use a spray gun to perform a spray test on the components installed in the first cavity of the shell under inspection;

[0013] S7, use dry compressed air to blow the shell under inspection or place the shell under inspection in an oven for high-temperature baking for a waiting time t1, and then perform spray inspection of the components installed in the second cavity of the shell under inspection;

[0014] S8, using the same method as step S7 to alleviate the helium adsorption in the remaining cavities of the shell under inspection, and detecting the air tightness of the components installed in the remaining cavities of the shell under inspection;

[0015] S9. After all cavity inspections are completed, clean the vacuum silicone grease.

[0016] Furthermore, the shell material in S1 is 6061 aluminum alloy, and the surface treatment method is to nickel-plate the surface of the welding installation with a thickness of 5μm, and then gold-plate its surface with a thickness of 0.5μm. The remaining non-welding surfaces are conductively oxidized with aluminum's natural color. The calibration shell does not have installation holes for the installation device.

[0017] Furthermore, n in S2 and S5 is the number of cavities to be inspected in the inspected shell.

[0018] Furthermore, the spray gun in S3 is connected to the pressure reducing valve and the helium cylinder through an air pipe, the outlet pressure is 70 kPa, and the spraying time of the spray gun is not less than 0.5 Ns, where N is the number of components installed in the first cavity of the inspected shell.

[0019] Furthermore, the recommended high temperature baking temperature in S4 is 125° C.-150° C., which is determined by the maximum temperature that the components and circuit boards in the housing can withstand, and the specific time is 10 minutes.

[0020] Furthermore, the spray gun in S6 is connected to the pressure reducing valve and the helium cylinder through an air pipe, the outlet pressure is 70 kPa, and the spray gun sprays each installed device for no less than 0.5 s.

[0021] Furthermore, the devices installed in S6 include radio frequency insulators, feed insulators, radio frequency coaxial connectors such as SMA and SMP, and rectangular connectors.

[0022] Furthermore, the high temperature baking temperature in S7 is consistent with the baking temperature in S4.

[0023] Furthermore, the method for cleaning the vacuum silicone grease in S9 is preferably wiping with a dust-free cloth followed by vapor phase cleaning, or wiping with a dust-free cloth followed by wiping with an alcohol cotton ball. Cleaning the vacuum silicone grease should be completed within 1 hour after the test is completed.

[0024] The beneficial effects of the present invention are:

[0025] 1. The multi-cavity shell helium spray inspection method provided by the present invention can effectively alleviate the influence of helium adsorption on the inspection results.

[0026] 2. The present invention utilizes a calibration shell to determine the waiting time for each cavity to relieve helium adsorption, which can effectively guide the formulation of a process plan for molded products.

[0027] 3. The present invention is aimed at large-scale helium spray inspection of multi-cavity shells. After the same cavity is sprayed, compressed air blowing or high-temperature baking is uniformly performed, which can effectively reduce the inspection time and improve production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 It is a flow chart of a multi-cavity shell helium spray inspection method of the present invention;

[0029] Figure 2 is a three-dimensional schematic diagram of the inspected shell of the present invention;

[0030] Figure 3 is a three-dimensional schematic diagram of the calibration housing of the present invention;

[0031] Figure 4 It is a schematic diagram of the helium spray inspection method of the present invention.

[0032] Explanation of the reference numerals: 1. the first cavity of the shell to be inspected; 2. the second cavity of the shell to be inspected; 3. the third cavity of the shell to be inspected; 4. the sealing ring of the first cavity of the shell to be inspected; 5. the sealing ring of the second cavity of the shell to be inspected; 6. the sealing ring of the third cavity of the shell to be inspected; 7. the side wall RF insulator; 8. the through-feed coupler; 9. the side wall SMA connector; 10. the side wall SMP connector; 11. the through-feed insulator; 12. the through-RF insulator; 13. the side wall rectangular connector; 14. the first cavity of the calibration shell; 15. the second cavity of the calibration shell; 16. the third cavity of the calibration shell; 17. the sealing ring of the first cavity of the calibration shell; 18. the sealing ring of the second cavity of the calibration shell; 19. the sealing ring of the third cavity of the calibration shell. DETAILED DESCRIPTION

[0033] The present invention will be further described below in conjunction with the accompanying drawings and specific embodiments:

[0034] like Figures 1 to 4As shown, the present invention provides a multi-cavity shell helium spray inspection method, comprising the following steps:

[0035] S1. Design and manufacture a calibration shell with the same material, shape and surface treatment as the shell being inspected.

[0036] The shell material in S1 is 6061 aluminum alloy, and the surface treatment method is to nickel-plated the surface where welding and installation are required, with a thickness of 5μm, and then gold-plated on its surface with a thickness of 0.5μm. The remaining non-welding surfaces are conductively oxidized with aluminum's natural color. The calibration shell does not have mounting holes for mounting devices.

[0037] In this embodiment, the shell material to be tested is a microwave component material, such as Figure 2 As shown. The microwave component tested in this embodiment has three cavities to be tested, namely the first cavity 1 of the tested shell, the second cavity 2 of the tested shell and the third cavity 3 of the tested shell. The first cavity 1 of the tested shell and the second cavity 2 of the tested shell are on the same side, and the third cavity 3 of the tested shell is on the other side. The installed devices to be tested in the first cavity 1 of the tested shell include the side wall RF insulator 7 and the through-feed coupler 8, the installed devices to be tested in the second cavity 2 of the tested shell include the side wall SMA connector 9, the side wall SMP connector 10, the through-feed insulator 11 and the through-RF insulator 12, and the installed devices to be tested in the third cavity 3 of the tested shell include the side wall rectangular connector 13.

[0038] A first cavity sealing ring 4 of the inspected shell is provided on the first cavity 1 of the inspected shell, a second cavity sealing ring 5 of the inspected shell is provided on the second cavity 2 of the inspected shell, and a third cavity sealing ring 6 of the inspected shell is provided on the third cavity 3 of the inspected shell. The cross-sections of the first cavity sealing ring 4 of the inspected shell and the second cavity sealing ring 5 of the inspected shell are rectangular structures, and the cross-section shape of the third cavity sealing ring 6 of the inspected shell is the same as the cross-section shape of the third cavity 3 of the inspected shell.

[0039] Design and processing Figure 3 The three-dimensional schematic diagram of the calibration shell shown shows a calibration shell having the same material, shape and surface treatment as the shell to be inspected, wherein the calibration shell does not have mounting holes for mounting components.

[0040] The calibration shell has a similar structure to the shell under test, and comprises a first cavity 14 of the calibration shell, a second cavity 15 of the calibration shell and a third cavity 16 of the calibration shell. A first cavity sealing ring 17 of the calibration shell is provided on the first cavity 14 of the calibration shell, a second cavity sealing ring 18 of the calibration shell is provided on the second cavity 15 of the calibration shell, and a third cavity sealing ring 19 of the calibration shell is provided on the third cavity 16 of the calibration shell. Both the first cavity sealing ring 17 of the calibration shell and the second cavity sealing ring 18 of the calibration shell are of rectangular structure, and the cross-sectional shape of the third cavity sealing ring 19 of the calibration shell is the same as the cross-sectional shape of the third cavity 16 of the calibration shell.

[0041] S2. Use a helium mass spectrometer leak detector to measure the background leak rates R0, R1, R2…R of each calibration chamber without helium adsorption. n-1 .

[0042] In this embodiment, there are three cavities, namely R0, R1, and R2. Figure 4 The schematic diagram of the helium spray inspection method shown in the figure uses a stainless steel clamp and a fluororubber gasket to connect the helium mass spectrometer leak detector to the leak detection disk with a vacuum joint, and evenly applies vacuum silicone grease to the contact position between the leak detection disk and the sealing gasket, and places the sealing gasket on the leak detection disk and presses the sealing gasket lightly. Use vacuum silicone grease to evenly apply to the sealing ring 17 of the first cavity of the calibration housing, and place the first cavity 14 of the calibration housing downward on the sealing gasket (the leak hole of the leak detector must be in the detection cavity) to make the housing and the sealing gasket fit tightly. Use the helium mass spectrometer leak detector to detect the background leak rate R0 of the first cavity 14 of the calibration housing (no need to spray helium). After the detection is completed, press the STOP button of the helium mass spectrometer leak detector to release the pressure and remove the calibration housing. Use the same method to measure the background leak rate R1 of the second cavity 15 of the calibration housing and the background leak rate R2 of the third cavity 16 of the calibration housing.

[0043] S3. Use a spray gun to spray and calibrate the shell.

[0044] In step S3, the spray gun is connected to the pressure reducing valve and the helium cylinder through the air pipe, the outlet pressure is 70 kPa, and the spraying time of the spray gun is not less than 0.5 Ns, where N is the number of components installed in the first cavity 1 of the inspected shell.

[0045] Use a spray gun to evenly spray helium on the surface of the calibration shell so that a certain amount of helium is adsorbed on the shell surface. The spray gun is connected to the pressure reducing valve and the helium bottle through an air pipe. The outlet pressure is 70 kPa. The first cavity 1 of the shell under inspection includes a side wall RF insulator 7 and a through-feed coupling 8, a total of 2 installation devices. The spray gun spraying time is not less than 0.5×2=1 s.

[0046] S4. Use dry compressed air to purge the calibration shell or place the calibration shell in an oven for high-temperature baking. Measure the background leakage rate value R1' of the second cavity 2 of the calibration shell after the helium adsorption relief treatment at specific intervals until R1'<1.5R1, and record the waiting time t1.

[0047] The recommended high temperature baking temperature in step S4 is 125° C.-150° C., which is determined by the maximum temperature that the components and circuit boards in the housing can withstand. The specific time is 10 minutes.

[0048] In this embodiment, the calibration shell is placed in a 125°C oven for high temperature baking (dry compressed air can also be used to blow the calibration shell), and the background leakage rate value R1' of the second cavity 15 of the calibration shell after the helium adsorption treatment is relieved is measured every 10 minutes until R1'<1.5R1, and the waiting time t1 is recorded.

[0049] S5, using the same method as step S3 and step S4 to measure the waiting time t2, t3, t4, ... t of the remaining cavities of the calibration shell. n-1

[0050] In the present invention, n in S2 and S5 is the number of cavities to be inspected in the inspected shell. In this embodiment, the same method as step S3 and step S4 is used to measure the waiting time t2 of the third cavity of the calibration shell. Use a spray gun to evenly spray helium on the surface of the calibration shell. The second cavity 2 of the inspected shell includes a side wall SMA connector 9, a side wall SMP connector 10, a through-feed insulator 11 and a through-RF insulator 12, wherein the number of through-feed insulators 11 and through-RF insulators 12 is two, a total of 6 installation components, and the spray gun spraying time is not less than 0.5×6=3s. After the helium is adsorbed on the surface of the calibration shell, the calibration shell is placed in a 125°C oven for high-temperature baking (dry compressed air can also be used to purge the calibration shell), and the background leakage rate value R2' of the third cavity 16 of the calibration shell after the helium adsorption treatment is relieved is measured every 10 minutes until R2'<1.5R2, and the waiting time t2 is recorded.

[0051] S6. Use a spray gun to perform a spray test on the components installed in the first cavity 1 of the shell under inspection.

[0052] In step S6, the spray gun is connected to the pressure reducing valve and the helium cylinder through the air pipe, the outlet pressure is 70kPa, and the spray gun sprays each installation component for no less than 0.5s. The installation components in step S6 include RF insulators, feed insulators, RF coaxial connectors such as SMA and SMP, and rectangular connectors.

[0053] In this example, vacuum silicone grease is evenly applied to the sealing ring 4 of the first cavity of the shell to be inspected, and the first cavity 1 of the shell to be inspected is placed downward on the sealing gasket (the leak hole of the leak detector must be in the detection cavity) to make the shell and the sealing gasket fit tightly. The helium mass spectrometer leak detector is turned on, and a spray gun connected to a helium bottle is used to spray the side wall RF insulator 7 and the through-feed bus 8 in the first cavity 1 of the shell to be inspected in turn. The outlet pressure is 70 kPa. The spray gun sprays each installed component for no less than 0.5 s, and the leakage rate value of the cavity 1 of the shell to be inspected is recorded.

[0054] S7, use dry compressed air to blow the shell under inspection or place the shell under inspection in an oven for high-temperature baking. After waiting for t1, perform spray inspection of the components installed in the second cavity 2 of the shell under inspection.

[0055] The high temperature baking temperature in step S7 is consistent with the baking temperature in S4. In this embodiment, the shell to be inspected is placed in a 125°C oven for high temperature baking (dry compressed air can also be used to purge the calibration shell). After the waiting time t1 obtained in step S4, vacuum silicone grease is evenly applied to the sealing ring 5 of the second cavity of the shell to be inspected, and the second cavity 2 of the shell to be inspected is placed downward on the sealing gasket (the leak hole of the leak detector must be in the detection cavity) to make the shell and the sealing gasket fit tightly, turn on the helium mass spectrometer leak detector, and use a spray gun connected to a helium bottle to spray the side wall SMA connector 9, the side wall SMP connector 10, the through feed insulator 11 and the through RF insulator 12 in the second cavity 2 of the shell to be inspected in turn, the outlet pressure is 70kPa, and the spray gun sprays each installed device for no less than 0.5s, and records the leakage rate value of the second cavity 2 of the shell to be inspected.

[0056] S8. Use the same method as step S7 to relieve the helium adsorption in the remaining cavities of the shell under inspection, and detect the air tightness of the components installed in the remaining cavities of the shell under inspection.

[0057] Place the shell to be inspected in an oven at 125°C for high-temperature baking (dry compressed air can also be used to blow and calibrate the shell). After the waiting time t2 obtained in step S5, use vacuum silicone grease to evenly apply it to the sealing ring 6 of the third cavity of the shell to be inspected, and place the third cavity 3 of the shell to be inspected face down on the sealing gasket (the leak hole of the leak detector must be in the detection cavity) to make the shell and the sealing gasket fit tightly, turn on the helium mass spectrometer leak detector, and use a spray gun connected to a helium bottle to spray the side wall rectangular connector 13 in the third cavity 3 of the shell to be inspected. The outlet pressure is 70 kPa, and the spray gun sprays each installed component for no less than 0.5 s, and records the leakage rate value of the cavity 3 of the shell to be inspected.

[0058] S9. After all cavity inspections are completed, clean the vacuum silicone grease.

[0059] In step S9, the method for cleaning the vacuum silicone grease is preferably to wipe with a dust-free cloth and then clean it in the gas phase, or to wipe with a dust-free cloth and then wipe with an alcohol cotton ball. Cleaning the vacuum silicone grease should be completed within 1 hour after the detection is completed. In this embodiment, within 1 hour after all cavity detections are completed, the vacuum silicone grease is wiped with a dust-free cloth and then cleaned in the gas phase of the shell being inspected, or the vacuum silicone grease is wiped with a dust-free cloth and then wiped with an alcohol cotton ball to complete the cleaning of the shell being inspected.

[0060] The present invention can complete the helium spray inspection process of the multi-cavity shell through the above 9 steps, and use the calibration shell to determine the waiting time of each cavity, effectively alleviate the influence of helium adsorption on the detection result, and can truly reflect the airtightness of the product installation device.

[0061] Those skilled in the art will appreciate that the embodiments described herein are intended to help readers understand the principles of the present invention, and should be understood that the protection scope of the present invention is not limited to such specific statements and embodiments. Those skilled in the art can make various other specific variations and combinations that do not deviate from the essence of the present invention based on the technical revelations disclosed by the present invention, and these variations and combinations are still within the protection scope of the present invention.

Claims

1. A multi-cavity shell helium spray inspection method, characterized in that: The following steps are involved: S1. Design and manufacture a calibration shell with the same material, shape and surface treatment as the shell under test; S2. Use a helium mass spectrometer leak detector to measure the background leak rates R0, R1, R2…R of each calibration chamber without helium adsorption. n-1 ; S3, use a spray gun to spray and calibrate the shell; S4, using dry compressed air to purge the calibration housing or placing the calibration housing in an oven for high-temperature baking, measuring the background leakage rate value R1' of the second cavity (2) of the calibration housing after the helium adsorption relief treatment at specific intervals until R1'<1.5R1, and recording the waiting time t1; S5, using the same method as step S3 and step S4 to measure the waiting time t2, t3, t4, ... t of the remaining cavities of the calibration shell. n-1 ; S6, using a spray gun to perform a spray test on the components installed in the first cavity (1) of the shell under inspection; S7, using dry compressed air to purge the shell under inspection or placing the shell under inspection in an oven for high-temperature baking after a waiting time t1, and then spraying the components installed in the second cavity (2) of the shell under inspection; S8, using the same method as step S7 to alleviate the helium adsorption in the remaining cavities of the shell under inspection, and detecting the air tightness of the components installed in the remaining cavities of the shell under inspection; S9. After all cavity inspections are completed, clean the vacuum silicone grease.

2. A multi-cavity shell helium spray inspection method according to claim 1, characterized in that: The shell material in S1 is 6061 aluminum alloy, and the surface treatment method is to nickel-plate the surface of the welding installation with a thickness of 5μm, and then gold-plate the surface with a thickness of 0.5μm. The other non-welding surfaces are conductively oxidized with aluminum's natural color. The calibration shell does not have installation holes for the installation device.

3. A multi-cavity shell helium spray inspection method according to claim 1, characterized in that: The n in S2 and S5 is the number of cavities to be inspected in the inspected housing.

4. A multi-cavity shell helium spray inspection method according to claim 1, characterized in that: The spray gun in S3 is connected to the pressure reducing valve and the helium cylinder through an air pipe, the outlet pressure is 70 kPa, and the spraying time of the spray gun is not less than 0.5 Ns, where N is the number of components installed in the first cavity (1) of the shell to be inspected.

5. A multi-cavity shell helium spray inspection method according to claim 1, characterized in that: The recommended high temperature baking temperature of S4 is 125° C.-150° C., which depends on the maximum temperature that the components and circuit boards in the housing can withstand. The specific time is 10 minutes.

6. A multi-cavity shell helium spray inspection method according to claim 1, characterized in that: The spray gun in S6 is connected to the pressure reducing valve and the helium cylinder through an air pipe, the outlet pressure is 70 kPa, and the spray gun sprays each installed device for no less than 0.5 s.

7. A multi-cavity shell helium spray inspection method according to claim 1, characterized in that: The components installed in S6 include radio frequency insulators, feed insulators, radio frequency coaxial connectors such as SMA and SMP, and rectangular connectors.

8. A multi-cavity shell helium spray inspection method according to claim 1, characterized in that: The high temperature baking temperature in S7 is consistent with the baking temperature in S4.

9. A multi-cavity shell helium spray inspection method according to claim 1, characterized in that: The method for cleaning the vacuum silicone grease in S9 is preferably wiping with a dust-free cloth followed by vapor phase cleaning, or wiping with a dust-free cloth followed by wiping with an alcohol cotton ball. Cleaning the vacuum silicone grease should be completed within 1 hour after the test is completed.

Citation Information

Cited By

  • Manufacturing process of high-reliability copper optical module