Measurement data model establishing method, measurement method and process control method
By establishing a measurement data model, using the etching process and spectral characteristics of the reference control sheet, the problem of low efficiency and poor accuracy of the morphological characteristics of the deep groove structure in the prior art is solved, and efficient and low-cost morphological characteristics are achieved Measurement.
Patent Information
- Application Number
- CN202411090726.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-09
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-08-09
AI Technical Summary
In the prior art, the efficiency of measuring the morphological characteristics of the deep groove structure of semiconductor structures is low, the accuracy is poor, and the cost is high, so it is impossible to effectively measure the structure in which the angle between the side wall and the top surface of the deep groove is greater than 90° or the morphological abnormality point is too large. .
By establishing a measurement data model, using the reference control chip to perform the same etching process as the process wafer, a trench structure close to the morphological characteristics of the deep groove structure is obtained, and the trench structure spectral characteristics and deep groove structure shape are obtained according to different measurement conditions. Model the morphological characteristics so that the morphological characteristics can be obtained without directly measuring the deep groove structure.
It greatly improves the measurement efficiency of the morphological characteristics of the deep groove structure, reduces the measurement cost, and improves the measurement accuracy and data comprehensiveness.
Smart Images

Figure CN119008442A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of semiconductor integrated circuit manufacturing, and in particular relates to a method for establishing a measurement data model, a measurement method and a process control method. Background Art
[0002] In the prior art, TEM (Transmission Electron Microscope) or HVSEM (High-Voltage Scanning Electron Microscopy) is mainly used to measure the morphological characteristics of deep trench structures in semiconductor structures.
[0003] However, when using TEM for measurement, it is necessary to destructively slice the wafer to be measured and then scan it with a transmission electron microscope to obtain a test image, and then perform manual analysis and measurement to obtain the morphological characteristic parameters of the deep groove structure, which leads to a long process cycle and can only measure the actual image of a single extremely small area. Image analysis will also introduce manual errors, resulting in low measurement accuracy. When using HVSEM to measure the deep groove structure, the top-view image obtained by high-energy electron scattering imaging of the wafer to be measured is analyzed and measured. The top-view image makes it impossible to measure the morphological characteristics of the deep groove structure when the angle between the side wall and the top surface of the deep groove is greater than 90° or the morphological abnormality point is too large. At the same time, its measurement data is a high-energy electron scattering image of a single small area, which takes a long time to measure, has low measurement efficiency, high cost, and poor data comprehensiveness.
[0004] Therefore, there is an urgent need for a new method for measuring the morphological characteristics of deep groove structures, which can improve the measurement efficiency and accuracy of the morphological characteristics of deep groove structures and reduce the measurement cost.
[0005] It should be noted that the above introduction to the technical background is only for the convenience of providing a clear and complete description of the technical solutions of the present application and for the convenience of understanding by those skilled in the art. It cannot be considered that the above technical solutions are well known to those skilled in the art simply because these solutions are described in the background technology part of the present application. Summary of the invention
[0006] In view of the above shortcomings of the prior art, an object of the present invention is to provide a method for establishing a measurement data model, a measurement method and a process control method, so as to solve the problems of low efficiency and poor accuracy in measuring deep groove structure morphological features in the prior art.
[0007] To achieve the above object, the present invention provides a method for establishing a measurement data model, the method comprising:
[0008] Step A1: providing a process wafer, on which a first semiconductor structure is arranged according to preset process conditions; performing an etching process on the process wafer through the first semiconductor structure under preset etching conditions to obtain a complete deep groove structure; slicing the process wafer having the deep groove structure, and scanning the deep groove structure with a transmission electron microscope to obtain preset morphological features of the deep groove structure;
[0009] Step A2: providing m different preset etching conditions, n different first semiconductor structures, and k different process conditions for setting the first semiconductor structure, where m, n, and k are all integers greater than or equal to 1; determining more than one measurement condition according to a combination of different preset etching conditions, the first semiconductor structure, and the process conditions, and repeating step A1 under each measurement condition to obtain a preset morphological feature of the deep trench structure corresponding to each measurement condition;
[0010] Step A3: providing a reference control wafer, on which a second semiconductor structure identical to the first semiconductor structure obtained through the same process conditions as the first semiconductor structure is disposed; performing the same etching process as the process wafer on the reference control wafer under the same preset etching conditions as the process wafer, and stopping after the groove structure obtained on the reference control wafer reaches a first preset depth; performing optical scattering measurement on the groove structure to obtain the spectral characteristics of the groove structure; the first preset depth is a depth that enables the groove structure to measure the preset morphological characteristics corresponding to the deep groove structure through an optical scattering measurement method;
[0011] Step A4: Repeat step A3 under each measurement condition in step A2 to obtain the spectral characteristics of the groove structure corresponding to each measurement condition;
[0012] Step A5: establishing the measurement data model according to the preset morphological features of the deep groove structure and the corresponding spectral features of the groove structure corresponding to each measurement condition.
[0013] Optionally, the method further includes: when performing step A3, slicing the reference control sheet for obtaining the groove structure and scanning it with a transmission electron microscope to obtain the preset morphological features of the groove structure; verifying the correlation between the preset morphological features of the groove structure corresponding to each measurement condition in step A4 and the preset morphological features of the deep groove structure corresponding to each measurement condition in step A2; when the correlation is within a strong correlation range, judging that the measurement data model is reliable; when the correlation is outside the strong correlation range, increasing the first preset depth, repeating steps A3 to A5, and updating the measurement data model.
[0014] Optionally, the method further comprises:
[0015] Adopting inspection etching conditions, inspection first semiconductor structures and / or inspection process conditions that are different from the preset etching conditions, the first semiconductor structure and the process conditions in the measurement conditions, performing the etching process on a process wafer through the inspection first semiconductor structure under the inspection etching conditions to obtain a deep trench structure, and the inspection first semiconductor structure is prepared on the process wafer through the inspection process conditions;
[0016] Under the inspection etching conditions, the etching process is performed on the reference control wafer through the inspection second semiconductor structure that is the same as the inspection first semiconductor structure, and the etching process is stopped after the trench structure obtained on the reference control wafer reaches the first preset depth, and the inspection second semiconductor structure is prepared on the reference control wafer through the inspection process conditions;
[0017] Slicing the reference control wafer having the groove structure and the process wafer having the deep groove structure and scanning them with a transmission electron microscope to obtain the preset morphological feature measurement values of the groove structure and the deep groove structure;
[0018] Substituting the obtained preset morphological feature measurement value of the groove structure into the measurement data model to obtain the corresponding preset morphological feature calculation value of the deep groove structure, and comparing the preset morphological feature calculation value of the deep groove structure with the preset morphological feature measurement value;
[0019] When the difference between the calculated value of the preset morphological feature of the deep groove structure and the measured value of the preset morphological feature does not exceed the first preset difference, it is judged that the accuracy of the measurement data model meets the requirement; when the difference between the calculated value of the preset morphological feature of the deep groove structure and the measured value of the preset morphological feature exceeds the first preset difference, the preset morphological feature of the deep groove structure corresponding to each measurement condition and the corresponding spectral feature of the groove structure are combined, and the spectral feature of the groove structure obtained by inspecting the etching condition, inspecting the first semiconductor structure, and inspecting the process condition and the preset morphological feature of the deep groove structure are inspected, and the measurement data model is updated according to the preset morphological feature of the deep groove structure and the corresponding spectral feature of the groove structure;
[0020] Or when the ratio of the difference between the calculated value of the preset morphological feature of the deep groove structure and the measured value of the preset morphological feature and the calculated value of the preset morphological feature of the deep groove structure does not exceed the first preset ratio, it is judged that the accuracy of the measurement data model meets the requirements; when the difference between the calculated value of the preset morphological feature of the deep groove structure and the measured value of the preset morphological feature and the calculated value of the preset morphological feature of the deep groove structure exceeds the first preset ratio, the measurement data model is updated according to the preset morphological features of the deep groove structure and the corresponding spectral features of the groove structure in combination with the preset morphological features of the deep groove structure corresponding to each measurement condition and the spectral features of the groove structure obtained by inspecting the etching conditions, inspecting the first semiconductor structure, and inspecting the process conditions and the preset morphological features of the deep groove structure.
[0021] Optionally, the aspect ratio of the deep trench structure is greater than or equal to 10 and the depth of the deep trench structure is greater than or equal to 1 micrometer.
[0022] Optionally, the first preset depth is 100 nanometers-500 nanometers.
[0023] Optionally, the thickness of the reference control wafer is greater than or equal to the thickness of the process wafer.
[0024] Optionally, the preset morphological features of the deep groove structure include one or more of a critical dimension at the opening of the deep groove structure, a critical dimension of a second preset depth of the deep groove structure, an angle between the side wall and the top surface at the opening of the deep groove structure, or a position or size of a morphological anomaly point on the side of the deep groove structure, and the second preset depth is smaller than the first preset depth.
[0025] Optionally, the first semiconductor structure includes a photolithography layer; in the etching process, the patterned photolithography layer is obtained by exposing and developing the photolithography layer; and the process wafer is etched through the patterned photolithography layer to form the deep groove structure on the process wafer.
[0026] The present invention also provides a measurement method, which comprises:
[0027] Using the same process, a first semiconductor structure is arranged on the wafer to be measured, and a second semiconductor structure identical to the first semiconductor structure is arranged on the reference wafer;
[0028] The wafer to be measured is etched by the first semiconductor structure to obtain a complete deep groove structure; the reference control wafer is etched by the second semiconductor structure under the same etching conditions as the wafer to be measured, and the etching is stopped when the groove structure obtained by the reference control wafer reaches a first preset depth;
[0029] performing optical scattering measurement on the obtained groove structure to obtain a measurement value of a spectral characteristic of the groove structure;
[0030] According to the measurement data model obtained by any of the above-mentioned methods for establishing the measurement data model, the measured values of the spectral characteristics of the groove structure are substituted into the measurement data model to obtain the measured values of the preset morphological characteristics of the deep groove structure.
[0031] The present invention also provides a process control method, the process control method comprising:
[0032] Obtaining a measurement value of a preset morphological feature of the deep groove structure on the wafer to be measured by the above-mentioned measurement method, and comparing it with a target value of the preset morphological feature of the deep groove structure;
[0033] When it is detected that the difference between the measured value of the preset morphological feature of the deep groove structure and the target value of the preset morphological feature of the deep groove structure exceeds a second preset difference, the process of the wafer to be measured is stopped or the preset adjustment is made to the process of the wafer to be measured; or when it is detected that the ratio of the difference between the measured value of the preset morphological feature of the deep groove structure and the target value of the preset morphological feature of the deep groove structure and the measured value of the preset morphological feature of the deep groove structure exceeds a second preset ratio, the process of the wafer to be measured is stopped or the preset adjustment is made to the process of the wafer to be measured.
[0034] As described above, the method for establishing a measurement data model, the measurement method and the process control method of the present invention have the following beneficial effects:
[0035] The present invention obtains a groove structure close to the morphological characteristics of the deep groove structure by performing the same front part of the etching process as the process wafer on a reference control wafer, and establishes a measurement data model according to the spectral characteristics of the groove structure under different measurement conditions and the morphological characteristics of the deep groove structure, so that the morphological characteristics of the deep groove structure can be obtained in an application without measuring the deep groove structure, which greatly improves the efficiency of measuring the morphological characteristics of the deep groove structure and reduces the measurement cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] Figure 1 It is a flowchart of the steps in the first embodiment of the present invention.
[0037] Figure 2 It is a structural schematic diagram of setting a first semiconductor structure in step A1 of the first embodiment of the present invention.
[0038] Figure 3 It is a schematic structural diagram of the deep groove structure obtained in step A1 of the first embodiment of the present invention.
[0039] Figure 4It is a schematic structural diagram of setting a second semiconductor structure in step A3 of the first embodiment of the present invention.
[0040] Figure 5 It is a schematic structural diagram of the groove structure obtained in step A3 of the first embodiment of the present invention.
[0041] Figure 6 Shown is a schematic top view of a process wafer in the first embodiment of the present invention.
[0042] Figure 7 Shown is a schematic top view of a reference control sheet in the first embodiment of the present invention.
[0043] Figure 8 It is a schematic diagram of the structure of growing an etch-stop layer and a mask layer on a process wafer in the first embodiment of the present invention.
[0044] Fig. 9 It is a schematic diagram showing the structure of setting a photolithography layer on a process wafer in an example of an embodiment of the present invention.
[0045] Fig.10 It is a schematic diagram of the structure of the growth stop layer and the mask layer in the reference control wafer in an example of an embodiment of the present invention.
[0046] Fig.11 It is a schematic diagram showing the structure of setting a photolithography layer on a reference control wafer in an example of an embodiment of the present invention.
[0047] Fig.12 Shown is a schematic diagram of preset morphological features in an example of an embodiment of the present invention.
[0048] Fig.13 It is a schematic diagram of a partial data table of establishing a measurement data model in step A5 of the first embodiment of the present invention.
[0049] Component number description
[0050] 1. Process wafer; 11. First semiconductor structure; 111. Stop layer; 112. Mask layer; 113. Photolithography layer; 114. Deep groove structure; 12. Preliminary pattern; 2. Reference control wafer; 21. Second semiconductor structure; 211. Trench structure. DETAILED DESCRIPTION
[0051] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.
[0052] For example, when describing the embodiments of the present invention in detail, for the sake of convenience, the schematic diagrams showing the device structure will not be partially enlarged according to the general scale, and the schematic diagrams are only examples, which should not limit the scope of protection of the present invention. In addition, in actual production, the three-dimensional dimensions of length, width and depth should be included.
[0053] For convenience of description, spatially relative terms such as "under", "below", "below", "below", "above", "on", etc. may be used herein to describe the relationship of one element or feature shown in the drawings to other elements or features. It will be understood that these spatially relative terms are intended to encompass other orientations of the device in use or operation in addition to the orientation depicted in the drawings.
[0054] In the context of the present application, a structure in which a first feature is described as being "above" a second feature may include embodiments in which the first and second features are in direct contact, and may also include embodiments in which additional features are formed between the first and second features, such that the first and second features may not be in direct contact.
[0055] It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner, and therefore the illustrations only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.
[0056] Embodiment 1:
[0057] like Figure 1 As shown, this embodiment provides a method for establishing a measurement data model, the method comprising:
[0058] Step A1: providing a process wafer, on which a first semiconductor structure is arranged according to preset process conditions; performing an etching process on the process wafer through the first semiconductor structure under preset etching conditions to obtain a complete deep groove structure; slicing the process wafer having the deep groove structure, and scanning the deep groove structure with a transmission electron microscope to obtain preset morphological features of the deep groove structure;
[0059] Step A2: providing m different preset etching conditions, n different first semiconductor structures, and k different process conditions for setting the first semiconductor structure, where m, n, and k are all integers greater than or equal to 1; determining more than one measurement condition according to a combination of different preset etching conditions, the first semiconductor structure, and the process conditions, and repeating step A1 under each measurement condition to obtain a preset morphological feature of the deep trench structure corresponding to each measurement condition;
[0060] Step A3: providing a reference control wafer, on which a second semiconductor structure identical to the first semiconductor structure obtained through the same process conditions as the first semiconductor structure is disposed; performing the same etching process as the process wafer on the reference control wafer under the same preset etching conditions as the process wafer, and stopping after the groove structure obtained on the reference control wafer reaches a first preset depth; performing optical scattering measurement on the groove structure to obtain the spectral characteristics of the groove structure; the first preset depth is a depth that enables the groove structure to measure the preset morphological characteristics corresponding to the deep groove structure through an optical scattering measurement method;
[0061] Step A4: Repeat step A3 under each measurement condition in step A2 to obtain the spectral characteristics of the groove structure corresponding to each measurement condition;
[0062] Step A5: establishing the measurement data model according to the preset morphological features of the deep groove structure and the corresponding spectral features of the groove structure corresponding to each measurement condition.
[0063] The method for establishing the measurement data model of the present embodiment will be described in detail below with reference to the accompanying drawings. It should be noted that the above sequence does not strictly represent the sequence of the method for establishing the measurement data model protected by the present embodiment, and those skilled in the art may change it according to the actual preparation steps.
[0064] First, perform step A1, such as Figure 2 As shown, a process wafer 1 is provided, on which a first semiconductor structure 11 is arranged according to preset process conditions; Figure 3 As shown, under preset etching conditions, the process wafer 1 is etched through the first semiconductor structure 11 to obtain a complete deep groove structure 114; after slicing the process wafer 1 with the deep groove structure 114, a transmission electron microscope is used to scan the deep groove structure 114 to obtain the preset morphological features of the deep groove structure 114.
[0065] Then, perform step A2, provide m different preset etching conditions, n different first semiconductor structures, and k different process conditions for setting the first semiconductor structure 11, where m, n, and k are all integers greater than or equal to 1; determine more than one measurement condition based on the combination of different preset etching conditions, the first semiconductor structure, and the process conditions, repeat step A1 under each measurement condition, and obtain the preset morphological features of the deep groove structure 114 corresponding to each measurement condition.
[0066] Next, proceed to step A3, such as Figure 4As shown, a reference control wafer 2 is provided, on which a second semiconductor structure 21 identical to the first semiconductor structure 11 and obtained by the same process conditions as the first semiconductor structure 11 is disposed; Figure 5 As shown, the reference control wafer 2 is subjected to the same etching process as the process wafer 1 under the same preset etching conditions as the process wafer 1, and the etching process is stopped after the groove structure 211 obtained on the reference control wafer 2 reaches a first preset depth; an optical scattering measurement is performed on the groove structure 211 to obtain the spectral characteristics of the groove structure 211; the first preset depth is a depth that allows the groove structure 211 to be measured by an optical scattering measurement method to reach the preset morphological feature corresponding to the deep groove structure 114.
[0067] The present invention arranges the second semiconductor structure 21 on the reference control wafer 2 to obtain the same structure through the same process as the first semiconductor structure 11, so that the morphological features of the subsequently formed groove structure 211 are as close as possible to the deep groove structure 114, so as to improve the accuracy of establishing the measurement data model; and by adopting the same preset etching conditions as those for forming the deep groove structure 114 to perform the front part of the same etching process as the process wafer 1 on the reference control wafer 2, the morphological features similar to the opening of the deep groove structure 114 are obtained in the groove structure 211, so as to establish a corresponding relationship between the morphological features of the groove structure 211 and the morphological features of the deep groove structure 114 in the subsequent steps.
[0068] In one embodiment, the thickness of the reference control wafer 2 is greater than or equal to the thickness of the process wafer 1 .
[0069] The present invention sets the thickness of the reference control wafer 2 to be greater than the thickness of the process wafer 1, and utilizes the depth of the groove structure 211 to be formed on the reference control wafer 2 to be less than the depth of the deep groove structure 114 to be formed on the process wafer 1, so that the reference control wafer 2 can be reused. After forming a layer of groove structure 211 for measurement, the part containing the groove structure 211 is removed, and a new groove structure 211 is formed again with the remaining reference control wafer 2, thereby reducing the cost for establishing a measurement data model.
[0070] Specifically, the difference between the process wafer 1 and the reference wafer 2 is that the process wafer 1 has gone through all the process flows of manufacturing products before preparing the deep groove structure 114, including the previously obtained graphics and other structures, such as Figure 6 FIG. 1 is a top view of a process wafer 1, including a preliminary pattern 12; and FIG. 2 is a reference wafer 2, which is only subjected to a process flow of setting a second semiconductor structure 21 before preparing a trench structure 211. Figure 7 The reference control sheet 2 is shown in a top view, which does not go through all the process steps, thereby reducing the overall production cost.
[0071] In one embodiment, when the process wafer 1 only includes a substrate layer serving as a device substrate before the first semiconductor structure 11 is set, the reference control wafer 2 also only includes the same substrate layer; when other structural layers requiring a deep groove structure 114 to be set have been prepared on the substrate layer before the process wafer 1 is set with the first semiconductor structure 11, the reference control wafer 2 should also be provided with the same structural layer, so that the obtained groove structure 211 is more strongly correlated with the preset morphological features of the deep groove structure 114.
[0072] In one embodiment, Figure 2 As shown, the first semiconductor structure 11 includes a photolithography layer 113. Figure 4 The second semiconductor structure 21 is shown as the same as the first semiconductor structure 11, including a photolithography layer 113; in the etching process, the photolithography layer 113 is exposed and developed to obtain the patterned photolithography layer 113; the process wafer 1 is etched by the patterned photolithography layer 113 to form the deep groove structure 114 on the process wafer 1. Specifically, the first semiconductor structure 11 may also include other structures, which may be arranged according to process requirements, and are all within the protection scope of the present invention.
[0073] In one embodiment, the steps of forming the first semiconductor structure 11 include: Figure 8 As shown, a stop layer 111 is grown on the process wafer 1, and a mask layer 112 is grown on the stop layer 111; Fig. 9 As shown, a photolithography layer 113 is disposed on the mask layer 112, and the stop layer 111, the mask layer 112, and the photolithography layer 113 on the process wafer 1 constitute a first semiconductor structure 11; the steps of forming the second semiconductor structure 21 include: Fig.10 As shown, a stop layer 111 is grown on the reference control wafer 2, and a mask layer 112 is grown on the stop layer 111; Fig.11 As shown, a photolithography layer 113 is arranged on the mask layer 112, and the stop layer 111, mask layer 112 and photolithography layer 113 on the reference control wafer 2 constitute a second semiconductor structure 21; the stop layer 111, mask layer 112 and photolithography layer 113 on the process wafer 1 and the stop layer 111, mask layer 112 and photolithography layer 113 on the reference control wafer 2 are obtained using exactly the same process conditions and process methods.
[0074] In one embodiment, Fig. 9As shown, the first semiconductor structure 11 includes a stop layer 111, a mask layer 112 and a photoresist layer 113 from bottom to top; in the etching process, the photoresist layer 113 is exposed and developed to obtain the patterned photoresist layer 113; the mask layer 112 and the stop layer 111 are etched through the patterned photoresist layer 113; the process wafer 1 is etched through the patterned mask layer 112 and the stop layer 111, and the process wafer 1 is formed as shown in FIG. Figure 3 The deep trench structure 114 is shown. Specifically, the first semiconductor structure 11 may not be provided with the stop layer 111 or other structural layers may be provided between the photolithography layer 113 and the process wafer 1, which are all within the protection scope of the present invention.
[0075] Specifically, Figure 3 and Figure 5 The figure shows the structure after the deep groove structure 114 and the groove structure 211 are obtained when the first semiconductor structure 11 and the second semiconductor structure 21 include the stop layer 111; when the first semiconductor structure 11 and the second semiconductor structure 21 do not include the stop layer 111, there is no stop layer 111 on the process wafer 1 after the deep groove structure 114 is set, and there is no stop layer 111 on the reference control wafer 2 after the groove structure 211 is set.
[0076] In one embodiment, Fig.12 As shown, the preset morphological features of the deep groove structure 114 include one or more of the critical dimension a at the opening of the deep groove structure 114, the critical dimension b of the second preset depth of the deep groove structure 114, the angle c between the side wall and the top surface at the opening of the deep groove structure 114, or the position or size of the morphological anomaly d on the side of the deep groove structure 114, and any combination thereof, and the second preset depth is less than the first preset depth.
[0077] Specifically, the morphological abnormal point can be Fig.12 The necking shown in the figure may also be other morphological anomaly points on the process wafer 1 that need to be measured; the preset morphological features may also use other morphological features of the deep groove structure 114 that need to be measured. Most of the above preset morphological features are morphological features located at the opening of the deep groove structure 114. Therefore, it is more suitable for the morphological feature measurement of the groove structure 211 formed on the reference control wafer 2 in the present invention and obtained using the same front part process as the deep groove structure 114, thereby reflecting the advantage of the solution of the present invention in solving the problem that the deep groove structure 114 is too deep and it is difficult to directly obtain the morphological features of the deep groove structure 114 through optical scattering measurement (OCD).
[0078] Specifically, when the depth of the morphological feature to be measured is too deep to make it impossible to use the OCD method to measure the morphological feature of the groove structure 211, it is not suitable to use the solution of the present invention for measurement. Therefore, the depth of the morphological feature to be measured needs to be less than or equal to the first preset depth of the groove structure 211.
[0079] Specifically, the groove structure 211 may be provided first, and then the deep groove structure 114 may be provided, or the groove structure 211 and the deep groove structure 114 may be provided simultaneously. Preferably, the groove structure 211 and the deep groove structure 114 are provided simultaneously to ensure that the etching process of the front part of the groove structure 211 and the deep groove structure 114 is completely the same, so as to ensure that the preset morphological features of the obtained groove structure 211 are highly correlated with the preset morphological structure of the deep groove structure 114.
[0080] In one embodiment, the aspect ratio of the deep trench structure 114 is greater than or equal to 10 and the depth of the deep trench structure 114 is greater than or equal to 1 micrometer.
[0081] Specifically, when the deep groove structure 114 meets the above conditions, it is an industry standard deep groove structure 114 and is more suitable for measuring the topographical features with the solution of the present invention.
[0082] In one embodiment, the first preset depth is 100 nanometers to 500 nanometers. Specifically, other first preset depths suitable for specific application scenarios can also be used to meet the conditions for optical scattering measurement of the groove structure 211 and obtain preset morphological features corresponding to the deep groove structure 114.
[0083] Then, step A4 is performed, and step A3 is repeated under each measurement condition in step A2 to obtain the spectrum characteristics of the trench structure 211 corresponding to each measurement condition.
[0084] Finally, step A5 is performed to establish the measurement data model according to the preset morphological features of the deep groove structure 114 and the corresponding spectral features of the groove structure 211 corresponding to each measurement condition.
[0085] In the prior art, when measuring the morphological features of the deep groove structure 114 by TEM (transmission electron microscope), it is necessary to destructively slice the wafer to be measured, resulting in a long measurement cycle and high cost, and only a very small area can be measured, and the measurement efficiency is very low. At the same time, since image analysis requires images obtained by manual measurement, system deviations will be introduced, resulting in low measurement accuracy; and when using HVSEM to measure the morphological features of the deep groove structure 114, since it can only perform image measurement through the top view image obtained by electron scattering imaging, it is impossible to measure morphological features that are difficult to identify in the top view, such as the deep groove structure 114 with an angle between the side wall and the top surface greater than 90° or a necking structure that is too large. It is difficult to use HVSEM to accurately measure the morphological features, so the data comprehensiveness is poor; and the method used in the prior art for measuring groove morphological features - optical scattering measurement (OCD) cannot be used in the morphological measurement of deep groove structures 114 with a depth greater than 1 micron because it is difficult to measure the morphological features of deep grooves with a depth exceeding 1 micron.
[0086] In the present invention, the groove structure 211 on the reference control wafer 2 is set to use the same etching conditions as the deep groove structure 114 for etching, but the etching is stopped only when it reaches the first preset depth (that is, the depth at which the preset morphological features can be measured). Therefore, the depth of the obtained groove structure 211 can be much smaller than the depth of the deep groove structure 114, so that the preset morphological features of the groove structure 211 can be obtained through optical scattering measurement, and the spectral characteristics of the groove structure 211 under different combinations of etching conditions, the first semiconductor structure 11 and the process conditions for setting the first semiconductor structure 11 are established through preliminary experiments. The measurement data model of the preset morphological features obtained by TEM of the deep groove structure 114 can, in actual applications, only measure the spectral features of the groove structure 211 to obtain the corresponding preset morphological features of the deep groove structure 114, without slicing the deep groove structure 114 to be measured, and only needs to perform optical scattering measurement, which can greatly improve the measurement efficiency and reduce the measurement cost, and can also measure various morphological features of the deep groove structure 114, the data is more comprehensive, and the relationship model established through the measurement data model can reduce the systematic error of the measurement, thereby obtaining a more accurate measurement result.
[0087] Specifically, the measurement data model is a data model used to characterize the correspondence between the preset morphological characteristics of the deep groove structure 114 and the corresponding spectral characteristics of the groove structure 211 under different combinations of the preset etching conditions, the first semiconductor structure 11 and the process conditions. The corresponding preset etching conditions, the first semiconductor structure 11, the process conditions and the spectral characteristics of the groove structure 211 can be substituted into the measurement data model to obtain the corresponding preset morphological characteristics of the deep groove structure 114.
[0088] In one embodiment, the method further includes: when performing step A3, slicing the reference control sheet 2 for obtaining the groove structure 211 and scanning it with a transmission electron microscope to obtain the preset morphological features of the groove structure 211; verifying the correlation between the preset morphological features of the groove structure 211 corresponding to each measurement condition in step A4 and the preset morphological features of the deep groove structure 114 corresponding to each measurement condition in step A2; when the correlation is within a strong correlation range, judging that the measurement data model is reliable; when the correlation is outside the strong correlation range, increasing the first preset depth, repeating steps A3 to A5, and updating the measurement data model.
[0089] The present invention can determine whether the morphological features of the deep groove structure 114 can be reflected by the morphological features of the groove structure 211 by checking the correlation between the preset morphological features of the groove structure 211 obtained by transmission electron microscopy scanning and the preset morphological features of the deep groove structure 114, thereby confirming the reliability of the measurement data model; and when the correlation between the preset morphological features of the groove structure 211 obtained by transmission electron microscopy scanning and the preset morphological features of the deep groove structure 114 is not strongly correlated, it means that the first preset depth selected at this time does not fully reflect the preset morphological features to be measured by the deep groove structure 114, so increasing the first preset depth and re-establishing the measurement data model can obtain the groove structure 211 that can reflect the preset morphological features of the deep groove structure 114, thereby improving the reliability of the measurement data model.
[0090] In one embodiment, the strong correlation range is the correlation index R 2 Specifically, those skilled in the art may also use different correlation parameters to set other suitable strong correlation ranges according to application requirements.
[0091] Specifically, in all actual experimental results, it can be found that the morphological features of the groove structure 211 and the deep groove structure 114 have a very strong linear correlation, so the morphological features of the corresponding deep groove structure 114 can generally be accurately obtained by directly measuring the morphological features of the groove structure 211 through optical scattering.
[0092] In one embodiment, the method further comprises:
[0093] Using inspection etching conditions, inspection first semiconductor structure 11 and / or inspection process conditions that are different from the preset etching conditions, the first semiconductor structure 11 and the process conditions in the measurement conditions, performing the etching process on the process wafer 1 through the inspection first semiconductor structure 11 under the inspection etching conditions to obtain a deep trench structure 114, the inspection first semiconductor structure 11 being prepared on the process wafer 1 through the inspection process conditions;
[0094] Under the inspection etching conditions, the inspection second semiconductor structure 21 is subjected to the same etching process as the inspection first semiconductor structure 11 on the reference control wafer 2, and the etching process is stopped after the trench structure 211 obtained on the reference control wafer 2 reaches the first preset depth. The inspection second semiconductor structure 21 is prepared on the reference control wafer 2 under the inspection process conditions;
[0095] After slicing the reference control wafer 2 having the groove structure 211 and the process wafer 1 having the deep groove structure 114, scanning with a transmission electron microscope is performed to obtain the preset morphological feature measurement values of the groove structure 211 and the deep groove structure 114;
[0096] Substituting the obtained preset morphological feature measurement value of the groove structure 211 into the measurement data model to obtain the corresponding preset morphological feature calculation value of the deep groove structure 114, and comparing the preset morphological feature calculation value of the deep groove structure 114 with the preset morphological feature measurement value;
[0097] When the difference between the calculated value of the preset morphological feature of the deep groove structure 114 and the measured value of the preset morphological feature does not exceed the first preset difference, it is judged that the accuracy of the measurement data model meets the requirement; when the difference between the calculated value of the preset morphological feature of the deep groove structure 114 and the measured value of the preset morphological feature exceeds the first preset difference, the preset morphological feature of the deep groove structure 114 corresponding to each measurement condition and the corresponding spectral feature of the groove structure 211 are combined, and the spectral feature of the groove structure 211 obtained by inspecting the etching condition, inspecting the first semiconductor structure, and inspecting the process condition and the preset morphological feature of the deep groove structure 114 are inspected, and the measurement data model is updated according to the preset morphological feature of the deep groove structure 114 and the corresponding spectral feature of the groove structure 211;
[0098] Or when the ratio of the difference between the calculated value of the preset morphological feature of the deep groove structure 114 and the measured value of the preset morphological feature and the calculated value of the preset morphological feature of the deep groove structure 114 does not exceed the first preset ratio, it is judged that the accuracy of the measurement data model meets the requirements; when the difference between the calculated value of the preset morphological feature of the deep groove structure 114 and the measured value of the preset morphological feature and the calculated value of the preset morphological feature of the deep groove structure 114 exceeds the first preset ratio, the measurement data model is updated according to the preset morphological features of the deep groove structure 114 and the corresponding spectral features of the groove structure 211 in combination with the preset morphological features of the deep groove structure 114 corresponding to each measurement condition and the spectral features of the groove structure 211 obtained by inspecting the etching conditions, inspecting the first semiconductor structure, and inspecting the process conditions and the preset morphological features of the deep groove structure 114.
[0099] Specifically, in the above method, it may be that the etching condition is different from the preset etching condition in the measurement condition, or the first semiconductor structure 11 is different from the first semiconductor structure 11 in the measurement condition, or the process condition is different from the process condition in the measurement condition; it may also be that the etching condition is different from the preset etching condition in the measurement condition, and the first semiconductor structure 11 is different from the first semiconductor structure 11 in the measurement condition; or the etching condition is different from the preset etching condition in the measurement condition, and the process condition is different from the process condition in the measurement condition; or the first semiconductor structure 11 is different from the first semiconductor structure 11 in the measurement condition, and the process condition is different from the process condition in the measurement condition; or the etching condition is different from the preset etching condition in the measurement condition, and the first semiconductor structure 11 is different from the first semiconductor structure 11 in the measurement condition, and the process condition is different from the process condition in the measurement condition; it may also be that the etching condition is different from the preset etching condition in the measurement condition, and the first semiconductor structure 11 is different from the first semiconductor structure 11 in the measurement condition, and the process condition is different from the process condition in the measurement condition.
[0100] The present invention adds the comparison of measured values and calculated values under the conditions of checking etching conditions, checking the first semiconductor structure 11, and checking process conditions, so as to check the applicability of the obtained measurement data model to process variables other than the combination of the preset etching conditions, the first semiconductor structure 11, and the process conditions for setting the first semiconductor structure 11 in the measurement conditions, so as to judge the generalization availability of the measurement data model; when the gap between the measured value and the calculated value is large, a new measurement data model is obtained by incorporating the combination of checking etching conditions, checking the first semiconductor structure 11, and checking process conditions, so as to improve the availability of the measurement data model, so as to be used for a wider range of etching conditions and improve the reliability of the measurement results.
[0101] In one embodiment, Fig.13 The table shows part of the data when the measurement data model is established, wherein the first column represents different etching conditions, the second column represents the type of wafer, the third column represents the same photolithography process flow for setting the first semiconductor structure 11 and the second semiconductor structure 21, the fourth column represents the full process for setting the deep groove structure 114 and the front part of the process for setting the groove structure 211, the third and fourth columns belong to known process controllable factors, the fifth to eighth columns represent the corresponding morphological characteristic parameters obtained by slicing the corresponding wafers after the corresponding etching conditions and the corresponding process flow by TEM (transmission electron microscope), the ninth to twelfth columns represent the corresponding morphological characteristic parameters obtained by optical scattering measurement (OCD, also known as SCD, SpectraCD) of the corresponding wafers after the corresponding etching conditions and the corresponding process flow, wherein the process wafer 1 cannot be measured by SCD, so the corresponding SCD parameter is n / a;
[0102] According to the correlation of the morphological characteristic parameters of the deep groove structure 114 and the groove structure 211 obtained by TEM measurement of the process wafer 1 and the reference control wafer 2 under different etching conditions in the data table, the reflection of the morphological characteristics of the deep groove structure 114 in the process wafer 1 by the groove structure 211 in the reference control wafer 2 can be verified;
[0103] After confirming that the morphological features of the deep groove structure 114 and the groove structure 211 are highly correlated, a measurement data model is established based on the TEM measurement results of the deep groove structure 114 in the process wafer 1 under different etching conditions and the SCD measurement results of the groove structure 211 of the reference control wafer 2;
[0104] By adjusting and expanding the range of process controllable factors, the TEM measurement results of the deep groove structure 114 of the new process wafer 1 and the SCD measurement results of the groove structure 211 of the new reference control wafer 2 are obtained. The SCD measurement results of the groove structure 211 of the new reference control wafer 2 are substituted into the measurement data model to obtain the calculation results of the morphological characteristics of the deep groove structure 114. The calculation results of the morphological characteristics of the deep groove structure 114 are compared with the TEM measurement results to verify the applicability of the measurement data model in a larger range of process controllable factors.
[0105] Specifically, Fig.13 Only the measured variables under different etching conditions are shown, and the experimental design of the first semiconductor structure 11, the process conditions for setting the first semiconductor structure 11 (including the photolithography process in the third column) and the etching conditions under different combinations are not shown. When this scheme is actually used, these three controllable factors can be set to measure the morphological characteristics and spectral characteristics under different combinations to jointly obtain a measurement data model.
[0106] Specifically, by Fig.13In the data table shown, when a measurement data model is established by only including the preset etching conditions described in the measurement conditions, the first semiconductor structure 11, and the spectral characteristics of the groove structure 211 corresponding to the process conditions for setting the first semiconductor structure 11, and the preset morphological characteristics of the deep groove structure 114, the obtained corresponding relationship model can realize a high correlation correspondence between the spectral characteristics of the groove structure 211 and the preset morphological characteristics of the deep groove structure 114 under the preset etching conditions described in the measurement conditions, the first semiconductor structure 11, and the process conditions; and when the preset etching conditions described in the measurement conditions, the first semiconductor structure 11, and the process conditions for setting the first semiconductor structure 11 are combined, the spectral characteristics of the groove structure 211 corresponding to the preset morphological characteristics of the deep groove structure 114 are realized. When the measurement data model is re-established based on the spectral characteristics and the preset morphological characteristics of the deep groove structure 114 obtained by corresponding to the spectral characteristics of the groove structure 211 obtained by inspecting the etching conditions, inspecting the first semiconductor structure 11, and inspecting the process conditions, the obtained correspondence model can achieve a highly correlated correspondence between the spectral characteristics of the groove structure 211 and the preset morphological characteristics of the deep groove structure 114 under the preset etching conditions, the first semiconductor structure 11, setting the process conditions of the first semiconductor structure 11 and inspecting the etching conditions, inspecting the first semiconductor structure 11, and inspecting the process conditions in the measurement conditions, thereby expanding the range of conditions that the obtained correspondence model can adapt to.
[0107] Embodiment 2:
[0108] This embodiment provides a measurement method, wherein it should be noted that the following sequence does not strictly represent the sequence of the measurement method protected by this embodiment, and those skilled in the art may change it according to the actual preparation steps.
[0109] First, step B1 is performed, in which a first semiconductor structure 11 is disposed on the wafer to be measured, and a second semiconductor structure 21 identical to the first semiconductor structure 11 is disposed on the reference wafer 2 by using the same process.
[0110] Then, step B2 is performed, in which the wafer to be measured is etched through the first semiconductor structure 11 to obtain a complete deep groove structure 114; under the same etching conditions as the wafer to be measured, the reference control wafer 2 is etched through the second semiconductor structure 21 in the same manner as the wafer to be measured, and the groove structure 211 obtained by the reference control wafer 2 reaches a first preset depth and stops.
[0111] Next, step B3 is performed to perform optical scattering measurement on the obtained trench structure 211 to obtain a measurement value of the spectral characteristic of the trench structure 211 .
[0112] Finally, step B4 is performed, and the measured values of the spectral characteristics of the groove structure 211 are substituted into the measurement data model obtained according to the measurement data model establishment method described in Example 1 to obtain the measured values of the preset morphological characteristics of the deep groove structure 114.
[0113] The present invention uses the measurement data model obtained in Example 1 to directly measure the spectral characteristics of the groove structure 211 obtained by optical scattering measurement in actual applications, and can calculate the preset morphological characteristics of the deep groove structure 114. The measurement efficiency is high, the cost is low, and the accuracy is high. At the same time, the morphological characteristics of the deep groove structure 114 with a deeper depth can be measured, and the data comprehensiveness is good.
[0114] Embodiment three:
[0115] This embodiment provides a process control method, which includes:
[0116] Obtaining the measurement value of the preset morphological feature of the deep groove structure 114 on the wafer to be measured by the measurement method of the second embodiment, and comparing it with the target value of the preset morphological feature of the deep groove structure 114;
[0117] When it is detected that the difference between the measured value of the preset morphological feature of the deep groove structure 114 and the target value of the preset morphological feature of the deep groove structure 114 exceeds a second preset difference, the process of the wafer to be measured is stopped or the preset adjustment is made to the process of the wafer to be measured; or when it is detected that the difference between the measured value of the preset morphological feature of the deep groove structure 114 and the target value of the preset morphological feature of the deep groove structure 114 and the ratio of the measured value of the preset morphological feature of the deep groove structure 114 exceeds a second preset ratio, the process of the wafer to be measured is stopped or the preset adjustment is made to the process of the wafer to be measured.
[0118] The present invention uses the measurement data model obtained in Example 1 and the measurement method in Example 2 to measure the preset morphological features of the deep groove structure 114 of the wafer to be measured, and utilizes its characteristic of being able to quickly and efficiently obtain measurement results to achieve real-time monitoring of the morphological features of the deep groove structure 114, so that the process can be stopped or adjusted in time when the morphological features of the deep groove structure 114 become abnormal, so as to avoid the loss of a large number of wafers caused by abnormalities in the process environment, thereby reducing the overall production cost.
[0119] In summary, the measurement data model establishment method, measurement method and process control method of the present invention can obtain a groove structure close to the morphological characteristics of the deep groove structure by performing the front part of the etching process that is the same as the process wafer through a reference control wafer, and establish a measurement data model based on the spectral characteristics of the groove structure and the morphological characteristics of the deep groove structure under different measurement conditions, so that the morphological characteristics of the deep groove structure can be obtained without measuring the deep groove structure in the application, which greatly improves the efficiency of measuring the morphological characteristics of the deep groove structure and reduces the measurement cost.
[0120] Therefore, the present invention effectively overcomes various shortcomings in the prior art and has high industrial utilization value.
[0121] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.
Claims
1. A method for establishing a measurement data model, It is characterized in that The method comprises: Step A1: providing a process wafer, on which a first semiconductor structure is arranged according to preset process conditions; performing an etching process on the process wafer through the first semiconductor structure under preset etching conditions to obtain a complete deep groove structure; slicing the process wafer having the deep groove structure, and scanning the deep groove structure with a transmission electron microscope to obtain preset morphological features of the deep groove structure; Step A2: providing m different preset etching conditions, n different first semiconductor structures, and k different process conditions for setting the first semiconductor structure, where m, n, and k are all integers greater than or equal to 1; determining more than one measurement condition according to a combination of different preset etching conditions, the first semiconductor structure, and the process conditions, and repeating step A1 under each measurement condition to obtain a preset morphological feature of the deep trench structure corresponding to each measurement condition; Step A3: providing a reference control wafer, on which a second semiconductor structure identical to the first semiconductor structure obtained through the same process conditions as the first semiconductor structure is disposed; performing the same etching process as the process wafer on the reference control wafer under the same preset etching conditions as the process wafer, and stopping after the groove structure obtained on the reference control wafer reaches a first preset depth; performing optical scattering measurement on the groove structure to obtain the spectral characteristics of the groove structure; the first preset depth is a depth that enables the groove structure to measure the preset morphological characteristics corresponding to the deep groove structure through an optical scattering measurement method; Step A4: Repeat step A3 under each measurement condition in step A2 to obtain the spectral characteristics of the groove structure corresponding to each measurement condition; Step A5: establishing the measurement data model according to the preset morphological features of the deep groove structure and the corresponding spectral features of the groove structure corresponding to each measurement condition.
2. The method for establishing a measurement data model according to claim 1, It is characterized in that The method also includes: when performing step A3, slicing the reference control sheet for obtaining the groove structure and scanning it with a transmission electron microscope to obtain the preset morphological features of the groove structure; checking the correlation between the preset morphological features of the groove structure corresponding to each measurement condition in step A4 and the preset morphological features of the deep groove structure corresponding to each measurement condition in step A2; when the correlation is within a strong correlation range, judging that the measurement data model is reliable; when the correlation is outside the strong correlation range, increasing the first preset depth, repeating steps A3 to A5, and updating the measurement data model.
3. The method for establishing a measurement data model according to claim 1 or 2, It is characterized in that The method further includes: adopting an inspection etching condition, an inspection first semiconductor structure and / or an inspection process condition different from the preset etching condition, the first semiconductor structure and the process condition in the measurement condition, performing the etching process on a process wafer through the inspection first semiconductor structure under the inspection etching condition to obtain a deep trench structure, and the inspection first semiconductor structure is prepared on the process wafer through the inspection process condition; Under the inspection etching conditions, the etching process is performed on the reference control wafer through the inspection second semiconductor structure that is the same as the inspection first semiconductor structure, and the etching process is stopped after the trench structure obtained on the reference control wafer reaches the first preset depth, and the inspection second semiconductor structure is prepared on the reference control wafer through the inspection process conditions; Slicing the reference control wafer having the groove structure and the process wafer having the deep groove structure and scanning them with a transmission electron microscope to obtain the preset morphological feature measurement values of the groove structure and the deep groove structure; Substituting the obtained preset morphological feature measurement value of the groove structure into the measurement data model to obtain the corresponding preset morphological feature calculation value of the deep groove structure, and comparing the preset morphological feature calculation value of the deep groove structure with the preset morphological feature measurement value; When the difference between the calculated value of the preset morphological feature of the deep groove structure and the measured value of the preset morphological feature does not exceed the first preset difference, it is judged that the accuracy of the measurement data model meets the requirement; when the difference between the calculated value of the preset morphological feature of the deep groove structure and the measured value of the preset morphological feature exceeds the first preset difference, the preset morphological feature of the deep groove structure corresponding to each measurement condition and the corresponding spectral feature of the groove structure are combined, and the spectral feature of the groove structure obtained by inspecting the etching condition, inspecting the first semiconductor structure, and inspecting the process condition and the preset morphological feature of the deep groove structure are inspected, and the measurement data model is updated according to the preset morphological feature of the deep groove structure and the corresponding spectral feature of the groove structure; Or when the ratio of the difference between the calculated value of the preset morphological feature of the deep groove structure and the measured value of the preset morphological feature and the calculated value of the preset morphological feature of the deep groove structure does not exceed the first preset ratio, it is judged that the accuracy of the measurement data model meets the requirements; when the difference between the calculated value of the preset morphological feature of the deep groove structure and the measured value of the preset morphological feature and the calculated value of the preset morphological feature of the deep groove structure exceeds the first preset ratio, the measurement data model is updated according to the preset morphological features of the deep groove structure and the corresponding spectral features of the groove structure in combination with the preset morphological features of the deep groove structure corresponding to each measurement condition and the spectral features of the groove structure obtained by inspecting the etching conditions, inspecting the first semiconductor structure, and inspecting the process conditions and the preset morphological features of the deep groove structure.
4. The method for establishing a measurement data model according to claim 1, It is characterized in that The aspect ratio of the deep trench structure is greater than or equal to 10 and the depth of the deep trench structure is greater than or equal to 1 micrometer.
5. The method for establishing a measurement data model according to claim 4, It is characterized in that The first preset depth is 100 nanometers to 500 nanometers.
6. The method for establishing a measurement data model according to claim 1, It is characterized in that The thickness of the reference control wafer is greater than or equal to the thickness of the process wafer.
7. The method for establishing a measurement data model according to claim 1, It is characterized in that The preset morphological features of the deep groove structure include one or more of the following: a critical dimension at the opening of the deep groove structure, a critical dimension of a second preset depth of the deep groove structure, an angle between the side wall and the top surface at the opening of the deep groove structure, or the position or size of a morphological anomaly point on the side of the deep groove structure, and any combination thereof, wherein the second preset depth is smaller than the first preset depth.
8. The method for establishing a measurement data model according to claim 1, It is characterized in that The first semiconductor structure includes a photolithography layer; in the etching process, the patterned photolithography layer is obtained by exposing and developing the photolithography layer; The process wafer is etched through the patterned photolithography layer to form the deep groove structure on the process wafer.
9. A method of measuring It is characterized in that The measuring method comprises: Using the same process, a first semiconductor structure is arranged on the wafer to be measured, and a second semiconductor structure identical to the first semiconductor structure is arranged on the reference wafer; The wafer to be measured is etched by the first semiconductor structure to obtain a complete deep groove structure; the reference control wafer is etched by the second semiconductor structure under the same etching conditions as the wafer to be measured, and the etching is stopped when the groove structure obtained by the reference control wafer reaches a first preset depth; performing optical scattering measurement on the obtained groove structure to obtain a measurement value of a spectral characteristic of the groove structure; According to the measurement data model obtained by the method for establishing a measurement data model according to any one of claims 1 to 8, the measured values of the spectral characteristics of the groove structure are substituted into the measurement data model to obtain the measured values of the preset morphological characteristics of the deep groove structure.
10. A process control method, It is characterized in that The process control method comprises: Obtaining a measurement value of a preset morphological feature of the deep groove structure on the wafer to be measured by the measurement method described in claim 9, and comparing it with a target value of the preset morphological feature of the deep groove structure; When it is detected that the difference between the measured value of the preset morphological feature of the deep groove structure and the target value of the preset morphological feature of the deep groove structure exceeds a second preset difference, the process of the wafer to be measured is stopped or the preset adjustment is made to the process of the wafer to be measured; or when it is detected that the ratio of the difference between the measured value of the preset morphological feature of the deep groove structure and the target value of the preset morphological feature of the deep groove structure and the measured value of the preset morphological feature of the deep groove structure exceeds a second preset ratio, the process of the wafer to be measured is stopped or the preset adjustment is made to the process of the wafer to be measured.
Citation Information
Patent Citations
Method for accurately controlling overall morphology and performance of shallow trench isolation
CN108010869A
Method for optimizing shallow trench isolation etching morphology under different light transmittance
CN108091560A
Method for optimizing deep groove etching morphology in double-groove process based on light transmittance
CN115346911A
Method and system for establishing optical critical dimension database
CN115524943A
Establishment method of optical critical dimension database, optical measurement structure and method thereof
CN115876097A