Formation method of metal interconnection structure
By forming a repair layer on the groove side walls of the integrated circuit and using plasma bombardment filling, the resistance increase and circuit breakage problems caused by the weak points of the metal seed layer are solved, and the device life is improved.
Patent Information
- Application Number
- CN202310566571.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-18
- Publication Date
- 2024-11-22
AI Technical Summary
During the metal interconnection process of integrated circuits, there are weak points in the metal seed layer on the side wall of the groove, which causes the metal body resistance in the groove filling area to rise or even be disconnected, affecting the life of the device.
By forming sequentially stacked interconnection layers and dielectric layers on the substrate, forming metal seed layers in the grooves and forming weak points on their side walls, a first electrochemical plating process is performed to form a repair layer, followed by a plasma bombardment The process fills the repair layer to the weak point, and finally performs a second electrochemical electroplating process to fill the metal layer to form a local metal interconnect structure.
It effectively avoids the weakness of the metal layer in the groove, reduces the metal body resistance and circuit breaking probability when applied voltage, and improves the service life of the device.
Smart Images

Figure CN119008514A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of integrated circuits, and in particular to a method for forming a metal interconnection structure. Background Art
[0002] As the integration level increases, the metal interconnection technology of integrated circuits has also developed from simple to complex, and from single layer to multi-layer. In large-scale integrated circuits, two-layer and more-layer metal wiring has been widely used.
[0003] In the process of back-end metal interconnection, the thickness of the metal seed layer grown in the groove filling area is relatively thin, and the physical vapor deposition growth method is adopted, resulting in poor step coverage of the side wall. Therefore, when the electrochemical metal plating is performed, the metal cannot be electroplated at the weak point (week point) of the metal seed layer on the groove side wall. Therefore, after the metal layer is completely filled, the longitudinal cross-sectional area of the film weak point on the groove side wall becomes larger; since the deposition speed of the electrochemical plating process is relatively fast, it is easy to cause premature sealing (overhang) at the top of the groove, thereby forming a void. In the above two situations, when the device is working normally, under the action of the applied voltage, the metal body resistance in the groove filling area increases or even a short circuit occurs, thereby reducing the life of the device. Summary of the invention
[0004] The object of the present invention is to provide a method for forming a metal interconnect structure to solve the problem that the metal seed layer on the side wall of the groove has weak points, which leads to increased resistance of the metal body in the groove filling area or even a short circuit.
[0005] In order to solve the above technical problems, the present invention provides a method for forming a metal interconnect structure, comprising:
[0006] A substrate is provided, on which an interconnection layer and a dielectric layer stacked in sequence are formed, a groove is formed in the dielectric layer, and the groove penetrates the dielectric layer and exposes the interconnection layer;
[0007] forming a metal seed layer in the groove, wherein the metal seed layer covers the sidewall and the bottom of the groove, and the metal seed layer on the sidewall of the groove is formed with a weak point;
[0008] Performing a first electrochemical plating process to form a repair layer on the metal seed crystal layer, wherein the repair layer covers the metal seed crystal layer and has a weak point;
[0009] Performing a plasma bombardment process to fill a portion of the repair layer at the bottom of the groove to the weak point of the side wall of the groove;
[0010] A second electrochemical plating process is performed to form a metal layer in the groove, the metal layer fills the groove, and the metal layer, the repair layer and the metal seed layer form a local metal interconnection structure.
[0011] Optionally, the plasma in the plasma bombardment process is a dissociated inert gas.
[0012] Optionally, the plasma includes argon ions or copper ions.
[0013] Optionally, the interconnect layer, the metal seed layer, the repair layer and the metal layer are made of the same metal type.
[0014] Optionally, the metal of the interconnect layer, the metal seed layer, the repair layer and the metal layer includes copper.
[0015] Optionally, the weak points of the metal seed crystal layer include one or more of breakpoints, depressions and holes.
[0016] Optionally, before the step of forming the metal seed layer in the groove, the method further comprises:
[0017] forming a barrier layer in the groove, wherein the barrier layer covers the sidewall and the bottom of the groove and the top of the dielectric layer;
[0018] An adhesion layer is formed, the adhesion layer covers the barrier layer, and the adhesion layer is used to adhere the barrier layer and the metal seed layer.
[0019] Optionally, the barrier layer includes a tantalum nitride layer, and the adhesion layer includes a tantalum layer.
[0020] Optionally, before the step of forming a barrier layer in the groove, the method further comprises:
[0021] Performing a dry etching process to form the groove, wherein the bottom of the groove is exposed to the air to naturally form a metal oxide and the sidewall of the groove is etched with residual polymer generated in the dry etching process;
[0022] A pre-cleaning process is performed to remove the metal oxide at the bottom of the groove and the residual polymer at the sidewall of the groove.
[0023] Optionally, the pre-cleaning process includes a physical bombardment process, and the physical bombardment process removes the metal oxide based on a redox reaction between hydrogen ions and the metal oxide.
[0024] In a method for forming a metal interconnect structure provided by the present invention, when a metal seed layer is formed in a groove, a weak point is formed in the metal seed layer on the side wall of the groove, and a first electrochemical plating process is performed to form a repair layer on the metal seed layer, the repair layer covers the metal seed layer and forms a weak point, and a plasma bombardment process is performed to fill part of the repair layer at the bottom of the groove to the weak point of the side wall of the groove to make the side wall of the metal seed layer smooth; then a second electrochemical plating process is performed to fill the metal layer in the groove to form a metal interconnect structure. Since the side walls of the repair layer and the metal seed layer are already smooth before the metal layer is deposited, weak points in the metal layer in the groove are avoided, the resistance of the metal body in the groove and the probability of short circuit in the metal interconnect structure when an external voltage is applied are reduced, and the service life of the device is improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Those skilled in the art will appreciate that the accompanying drawings are provided for a better understanding of the present invention and do not constitute any limitation on the scope of the present invention.
[0026] Figure 1 is a flow chart of a method for forming a metal interconnect structure according to an embodiment of the present invention;
[0027] Figures 2 to 11 is a structural schematic diagram of corresponding steps of a method for forming a metal interconnect structure according to an embodiment of the present invention;
[0028] In the attached figure:
[0029] 10 - substrate; 11 - interconnection layer; 12 - dielectric layer; 13 - groove; 13a - polymer; 13b - metal oxide; 14 - barrier layer; 15 - adhesion layer; 16 - metal seed layer; 16a - weak point; 17 - repair layer; 18 - metal layer. DETAILED DESCRIPTION
[0030] In order to make the purpose, advantages and features of the present invention clearer, the present invention is further described in detail below in conjunction with the accompanying drawings and specific embodiments. It should be noted that the drawings are all in a very simplified form and are not drawn to scale, and are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention. In addition, the structure shown in the drawings is often a part of the actual structure. In particular, the emphasis of each drawing is different, and sometimes different scales are used.
[0031] As used in the present invention, the singular forms "a", "an" and "the" include plural objects, the term "or" is generally used in a sense including "and / or", the term "several" is generally used in a sense including "at least one", and the term "at least two" is generally used in a sense including "two or more". In addition, the terms "first", "second" and "third" are used for descriptive purposes only and cannot be understood as indicating or suggesting relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first", "second", and "third" may explicitly or implicitly include one or at least two of the features. The term "proximal end" is usually the end close to the operator, and the term "distal end" is usually the end close to the patient. "One end" and "the other end" as well as "proximal end" and "distal end" usually refer to two corresponding parts, which include not only the endpoints. The terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral body; it can be a mechanical connection or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium, and it can be the internal connection of the two elements or the interaction relationship between the two elements. In addition, as used in the present invention, an element is arranged on another element, which usually only means that there is a connection, coupling, matching or transmission relationship between the two elements, and the connection, coupling, matching or transmission between the two elements can be direct or indirect through an intermediate element, and it cannot be understood as indicating or implying the spatial position relationship between the two elements, that is, one element can be in any position such as inside, outside, above, below or on one side of another element, unless the content clearly indicates otherwise. For those skilled in the art, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0032] Figure 1 : is a flow chart of a method for forming a metal interconnect structure according to an embodiment of the present invention. This embodiment provides a method for forming a metal interconnect structure, comprising:
[0033] Step S10, providing a substrate, on which an interconnection layer and a dielectric layer stacked in sequence are formed, a groove is formed in the dielectric layer, and the groove penetrates the dielectric layer and exposes the interconnection layer;
[0034] Step S20, forming a metal seed layer in the groove, wherein the metal seed layer covers the sidewall and the bottom of the groove, and the metal seed layer on the sidewall of the groove is formed with a weak point;
[0035] Step S30, performing a first electrochemical plating process to form a repair layer on the metal seed crystal layer, wherein the repair layer covers the metal seed crystal layer and has a weak point;
[0036] Step S40, performing a plasma bombardment process to fill a portion of the repair layer at the bottom of the groove to the weak point of the side wall of the groove;
[0037] Step S50 , performing a second electrochemical plating process to form a metal layer in the groove, wherein the metal layer fills the groove, and the metal layer, the repair layer, and the metal seed layer form a local metal interconnection structure.
[0038] Figures 2 to 11 1 is a schematic diagram of the corresponding steps of the method for forming a metal interconnect structure according to an embodiment of the present invention. Figures 2 to 11 The formation process of metal interconnect structure is introduced in detail.
[0039] Please refer to Figure 2 , a substrate 10 is provided, the substrate 10 may be a silicon substrate, or the material of the substrate 10 may be one of germanium, silicon germanium, silicon carbide, gallium arsenide or indium gallium, the substrate 10 may also be a silicon substrate on an insulator surface or a germanium substrate on an insulator surface. In addition, a device structure may be formed in the substrate 10, and the device structure may be a device structure formed in a semiconductor front-end process, such as a MOS transistor. An interconnection layer 11 and a dielectric layer 12 stacked in sequence are formed on the substrate 10, the interconnection layer 11 is, for example, a conductive layer, and further, in this embodiment, the material of the interconnection layer 11 is, for example, copper. The interconnection layer 11 may be formed by a physical vapor deposition process. The dielectric layer 12 is a dielectric layer with a low dielectric constant, and the material of the dielectric layer 12 includes, for example, a dielectric material composed of silicon, carbon and oxygen elements, and the dielectric layer 12 may be formed by a chemical vapor deposition process, and the dielectric layer 12 is a non-conductive material used to isolate adjacent interconnection layers.
[0040] Please refer to Figure 3 , a groove 13 is formed in the dielectric layer 12, and the groove 13 penetrates the dielectric layer 12 and exposes the interconnection layer 11. The groove 13 can be formed by a dry etching process. During the dry etching process, the polymer 13a formed by etching will remain on the sidewall of the groove 13, and the interconnection layer 11 exposed to the air by the groove 13 will be naturally oxidized. In this embodiment, the interconnection layer 11 is metal, so a metal oxide 13b will be naturally formed at the bottom of the groove 13. Since the naturally formed metal oxide 13b is a newly introduced impurity of the metal interconnection, it affects the conductive performance and therefore needs to be removed.
[0041] Please refer to Figure 4, perform a pre-cleaning process to remove the metal oxide 13b at the bottom of the groove 13 and the polymer 13a on the side wall of the groove. The pre-cleaning process includes a physical bombardment process and a wet cleaning process. The physical bombardment process is a remote plasma (Remote plasma) bombarding the metal oxide 13b at the bottom of the groove 13 by physical sputtering, and removing the metal oxide 13b based on the redox reaction of the dissociated hydrogen ions and the metal oxide 13b. The polymer 13a on the side wall of the groove is removed by the wet cleaning process. The wet cleaning process includes EKC cleaning and DHF cleaning. The EKC cleaning time is, for example, 80 seconds to 120 seconds, and the DHF cleaning time is, for example, 15 seconds to 25 seconds.
[0042] Please refer to Figure 5 , a barrier layer 14 is formed in the groove 13, and the barrier layer 14 covers the sidewalls and the bottom of the groove 13 and the top of the dielectric layer 12; the barrier layer 14 includes a tantalum nitride (TaN) layer, and the thickness of the tantalum nitride layer is, for example, 25 angstroms to 35 angstroms, and the barrier layer 14 is deposited by a physical vapor deposition process. The barrier layer 14 is used to block the diffusion of metal from the metallization area to the dielectric layer 12 area, and improve the electrical performance of the device such as electromigration.
[0043] Please refer to Figure 6 , forming an adhesion layer 15, the adhesion layer 15 covers the barrier layer 14, and the adhesion layer 15 is used to adhere the barrier layer 14 and the metal seed layer 16. The adhesion layer 15 is, for example, a tantalum layer. The thickness of the tantalum layer is, for example, 35 angstroms to 45 angstroms. The adhesion layer 15 is deposited by a physical vapor deposition process.
[0044] Please refer to Figure 7A metal seed layer 16 is formed in the groove 13, the metal seed layer 16 covers the sidewalls, the bottom and the top of the dielectric layer 12 of the groove 13, and the metal seed layer 16 on the sidewalls of the groove 13 is formed with a weak point 16a, and the weak point 16a of the metal seed layer includes one or more of a breakpoint, a depression and a hole. The metal seed layer 16 is, for example, a copper seed layer, and the formed metal seed layer 16 is a copper crystal plane with a certain crystal orientation, and the crystal orientation is, for example, <111> Crystal orientation, for subsequent electrochemical plating repair layer 17. In this embodiment, the metal seed layer 16 is formed by physical vapor deposition process. Since the barrier layer 14 grown in the filling area of the groove 13 is relatively thin, and the growth method of the physical vapor deposition process is adopted, the step coverage of the side wall of the groove 13 is poor, that is, the uniformity of the metal seed layer 16 film on the side wall of the groove 13 is generally poor, and different areas of the side wall of the groove 13 show obvious weak points 16a, that is, the metal seed layer 16 here is relatively thin, which is not conducive to the growth of the subsequent repair layer 17.
[0045] Please refer to Figure 8 , a first electrochemical plating (ECP) process is performed to form a repair layer 17 on the metal seed layer 16, and the repair layer 17 covers the metal seed layer 16. Since there is a weak point 16a in the metal seed layer 16 on the side wall of the groove, that is, the thickness of the metal seed layer 16 on the side wall of the groove is uneven, the resistance of the thin position of the metal seed layer 16 is large, and the repair layer 17 cannot be electroplated and filled at the thin position of the metal seed layer 16 on the side wall of the groove. Therefore, as the film thickness of the repair layer 17 accumulates, the repair layer also forms a weak point at the weak point 16a of the metal seed layer 16, and the weak point of the repair layer corresponds to the weak point 16a of the metal seed layer 16, and the longitudinal cross-sectional area becomes larger. The current of the first electrochemical plating process is, for example, 4 amperes to 5 amperes. The metal of the repair layer 17 is the same as that of the metal seed layer 16. The metal of the repair layer 17 is, for example, copper.
[0046] Please refer to Fig. 9 and Fig.10, a plasma bombardment process is performed to fill part of the repair layer 17 at the bottom of the groove to the weak point 16a of the side wall of the groove. The power of the plasma bombardment process is, for example, 900W to 1100W, and the time of the plasma bombardment process is, for example, 15 seconds to 25 seconds. In the plasma bombardment process, the substrate 10 is sputtered instead of the target material. In this embodiment, the repair layer 17 at the bottom of the groove is sputtered. The plasma in the plasma bombardment process is a dissociated inert gas. The plasma includes argon ions or copper ions. Specifically, an inert gas (such as argon) is introduced into the vacuum device to keep the vacuum degree within the range of 0.1 Pa to 1 Pa, and a voltage of 800 volts to 1500 volts is applied to the positive and negative electrodes. At this time, a DC glow discharge effect is generated in the vacuum device and ions are generated. The ions accelerated by the electric field bombard the surface of the substrate. In this embodiment, the repair layer 17 in the groove 13 is bombarded. Since the repair layer 17 is a metal layer, the repair layer 17 can be used as a cathode to directly bombard the repair layer 17 with accelerated cations. The thickness of several atomic layers is removed from the surface of the repair layer 17 at the bottom of the groove, and the atoms or molecules on the surface of the repair layer 17 that escape after the repair layer 17 is bombarded are filled into the thin position of the metal seed layer 16 on the side wall of the groove 13, and the metal seed layer 16 and the repair layer 17 on the side wall of the groove 13 are repaired to make the metal seed layer 16 and the repair layer 17 on the side wall of the groove 13 smooth, as shown in FIG. Fig.10 As shown, in other words, the plasma bombardment process can improve the problem of overhang of the metal seed layer 16 and the repair layer 17 on the top of the groove side wall, avoid the generation of weak points when the subsequent metal layer 18 is filled, thereby reducing the connection resistance of the metal interconnect structure and improving the service life of the device.
[0047] Please refer to Fig.11, a second electrochemical plating process is performed to form a metal layer 18 in the groove 13, the metal layer 18 fills the groove 13, and the metal layer 18 forms a local metal interconnection structure with the repair layer 17 and the metal seed layer 16. In this embodiment, the metal types of the interconnection layer 11, the metal seed layer 16, the repair layer 17 and the metal layer 18 are the same. Further, the metal of the metal layer 18 is, for example, copper. The second electrochemical plating process for forming the metal layer 18 includes a first stage, a second stage and a third stage. The first stage is the initial filling of the metal layer 18; in the initial stage, the repair layer 17 is repaired once by a high speed and low plating current method to improve the defects in the repair layer 17 process and protect the repair layer 17 from being corroded by the plating solution. The second stage is structural filling; in the second stage, by continuing to maintain a high speed, gradually increasing the plating current and giving sufficient time for the inhibitor and accelerator to reach the waist and bottom of the groove to prevent the waist from being sealed in advance, the copper filling of each position of the groove is completed in stages. The third stage is rapid filling. In the third stage, after the grooves 13 are filled, the rotation speed is reduced, and the electroplating current is continued to be increased to quickly complete the buffer layer process of the metal layer 18 grinding process, providing a process window for the chemical mechanical grinding process.
[0048] Typically, the metal seed layer 16, the repair layer 17 and the metal layer 18 will also extend to the top of the dielectric layer 12. After completing the second electrochemical plating process of the metal layer 18, a chemical mechanical polishing process is required to remove the barrier layer 14, the adhesion layer 15, the metal seed layer 16, the repair layer 17 and the metal layer 18 on the top of the dielectric layer 12.
[0049] In summary, it can be seen that in a method for forming a metal interconnect structure provided by an embodiment of the present invention, when a metal seed layer is formed in a groove, a weak point is formed in the metal seed layer on the side wall of the groove, and a first electrochemical plating process is performed to form a repair layer on the metal seed layer, the repair layer covers the metal seed layer and forms a weak point, and by performing a plasma bombardment process, a portion of the repair layer at the bottom of the groove is filled to the weak point of the side wall of the groove to make the side wall of the metal seed layer smooth; then a second electrochemical plating process is performed to fill the groove with the metal layer to form a metal interconnect structure. Since the side walls of the repair layer and the metal seed layer are already smooth before the metal layer is deposited, weak points in the metal layer in the groove are avoided, the resistance of the metal body in the groove and the probability of short circuit in the metal interconnect structure when an external voltage is applied are reduced, and the service life of the device is improved.
[0050] It should be noted that the various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other. In addition, the different parts between the various embodiments can also be used in combination with each other, and the present invention is not limited to this.
[0051] In addition, it should be recognized that although the present invention has been disclosed as a preferred embodiment, the above embodiment is not intended to limit the present invention. For any technician familiar with the art, without departing from the scope of the technical solution of the present invention, the technical content disclosed above can be used to make many possible changes and modifications to the technical solution of the present invention, or modified into equivalent embodiments of equivalent changes. Therefore, any simple modification, equivalent change and modification made to the above embodiment according to the technical essence of the present invention without departing from the content of the technical solution of the present invention still belongs to the scope of protection of the technical solution of the present invention.
Claims
1. A method for forming a metal interconnect structure, It is characterized in that include: A substrate is provided, on which an interconnection layer and a dielectric layer stacked in sequence are formed, a groove is formed in the dielectric layer, and the groove penetrates the dielectric layer and exposes the interconnection layer; forming a metal seed layer in the groove, wherein the metal seed layer covers the sidewall and the bottom of the groove, and the metal seed layer on the sidewall of the groove is formed with a weak point; Performing a first electrochemical plating process to form a repair layer on the metal seed crystal layer, wherein the repair layer covers the metal seed crystal layer and has a weak point; Performing a plasma bombardment process to fill a portion of the repair layer at the bottom of the groove to the weak point of the side wall of the groove; A second electrochemical plating process is performed to form a metal layer in the groove, the metal layer fills the groove, and the metal layer, the repair layer and the metal seed layer form a local metal interconnection structure.
2. The method for forming a metal interconnect structure according to claim 1, It is characterized in that The plasma in the plasma bombardment process is a dissociated inert gas.
3. The method for forming a metal interconnect structure according to claim 2, It is characterized in that The plasma includes argon ions or copper ions.
4. The method for forming a metal interconnect structure according to claim 1, It is characterized in that The interconnection layer, the metal seed layer, the repair layer and the metal layer are of the same metal type.
5. The method for forming a metal interconnection structure according to claim 4, It is characterized in that The metal of the interconnect layer, the metal seed layer, the repair layer, and the metal layer includes copper.
6. The method for forming a metal interconnect structure according to claim 1, It is characterized in that The weak points of the metal seed crystal layer include one or more of breakpoints, depressions and holes.
7. The method for forming a metal interconnect structure according to claim 1, It is characterized in that Before the step of forming the metal seed layer in the groove, the method includes: forming a barrier layer in the groove, wherein the barrier layer covers the sidewall and the bottom of the groove and the top of the dielectric layer; An adhesion layer is formed, the adhesion layer covers the barrier layer, and the adhesion layer is used to adhere the barrier layer and the metal seed layer.
8. The method for forming a metal interconnection structure according to claim 7, It is characterized in that The barrier layer includes a tantalum nitride layer, and the adhesion layer includes a tantalum layer.
9. The method for forming a metal interconnection structure according to claim 7, It is characterized in that Before the step of forming a barrier layer in the groove, the method comprises: Performing a dry etching process to form the groove, wherein the bottom of the groove is exposed to the air to naturally form a metal oxide and the sidewall of the groove has residual polymer generated in the dry etching process; A pre-cleaning process is performed to remove the metal oxide at the bottom of the groove and the residual polymer at the sidewall of the groove.
10. The method for forming a metal interconnection structure according to claim 9, It is characterized in that The pre-cleaning process includes a physical bombardment process, and the physical bombardment process removes the metal oxide based on a redox reaction between hydrogen ions and the metal oxide.