Solar cell, cell assembly and photovoltaic system

By setting the band gap width of the P-type doped layer in the solar cell to be smaller than that of the N-type doped layer, and by optimizing the passivation layer structure and doping concentration, the problem of poor current transport in the P-region was solved, a balance in current transport performance was achieved, and the cell efficiency was improved.

CN119008733APending Publication Date: 2024-11-22ZHEJIANG AIKO SOLAR ENERGY TECH CO LTD +5
View PDF 0 Cites 3 Cited by

Patent Information

Application Number
CN202411260478.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-06
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In existing solar cells, the current transport effect in the P-region is poor, resulting in low cell efficiency.

Method used

By setting the band gap width of the P-type doped layer to be smaller than that of the N-type doped layer, the resistance of the P-type doped layer is reduced, and its conductivity is improved. Furthermore, by adjusting parameters such as the structure and doping concentration of the passivation layer, a balance between the current transport effects in the P-region and the N-region is achieved.

Benefits of technology

This improves the current transport performance in the P-region and N-region, thereby increasing the overall efficiency of the solar cell.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008733A_ABST
    Figure CN119008733A_ABST
Patent Text Reader

Abstract

The invention is suitable for the technical field of solar cells, and provides a solar cell, a cell assembly and a photovoltaic system, the solar cell comprises a silicon substrate, the surface of which is provided with a P region and an N region; the first passivation layer is positioned in the P region and is arranged on the surface of the silicon substrate; the second passivation layer is positioned in the N region and is arranged on the surface of the silicon substrate; the P-type doping layer is arranged on one surface, deviating from the silicon substrate, of the first passivation layer; the N-type doping layer is arranged on one surface, deviating from the silicon substrate, of the second passivation layer; wherein the band gap width of the P-type doped layer is smaller than that of the N-type doped layer. According to the solar cell provided by the invention, by reducing the band gap width of the P-type doping layer, the conductive effect of the P-type doping layer can be improved, and the current transmission effect of the P region can be improved, so that the cell efficiency is effectively improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of solar cells, and in particular to a solar cell, a battery assembly and a photovoltaic system. Background Art

[0002] As fossil fuels are becoming less and less, solar energy has become the most common and clean renewable energy. Among them, solar cells are devices that use the photovoltaic effect to directly convert light energy into electrical energy. Solar cells mainly include double-sided solar cells and back-contact solar cells.

[0003] In the prior art, a bifacial solar cell has a P region on one side of its silicon substrate and an N region on the other side; a back contact solar cell has both a P region and an N region on its back side; wherein, in order to achieve a cell passivation effect, a first passivation layer and a P-type doping layer disposed on the first passivation layer are disposed in the P region of the bifacial solar cell and the back contact solar cell, and the electrode of the P region is in contact with the P-type doping layer; a second passivation layer and an N-type doping layer disposed on the second passivation layer are disposed in the N region of the bifacial solar cell and the back contact solar cell, and the electrode of the N region is in contact with the N-type doping layer. However, the P-type doping layer of a conventional solar cell has a larger resistance than the N-type doping layer, and the P-type doping layer has a poor conductive effect, resulting in poor current transmission effect in the P region and low cell efficiency. Summary of the invention

[0004] The present invention provides a solar cell, aiming to solve the problems of poor current transmission effect in the P region and low cell efficiency in the solar cell of the prior art.

[0005] The present invention is implemented by providing a solar cell, comprising:

[0006] A silicon substrate, wherein a P region and an N region are provided on the surface of the silicon substrate;

[0007] A first passivation layer located in the P region is disposed on the surface of the silicon substrate;

[0008] A second passivation layer located in the N region is disposed on the surface of the silicon substrate;

[0009] A P-type doped layer, disposed on a side of the first passivation layer away from the silicon substrate;

[0010] An N-type doped layer, disposed on a side of the second passivation layer away from the silicon substrate;

[0011] Wherein, the band gap width of the P-type doping layer is smaller than the band gap width of the N-type doping layer.

[0012] Preferably, the deposition temperature of the P-type doping layer is greater than the deposition temperature of the N-type doping layer.

[0013] Preferably, the diffusion temperature of the P-type doping layer is greater than the diffusion temperature of the N-type doping layer.

[0014] Preferably, the deposition temperature of the P-type doping layer is 595-630°C, and the deposition temperature of the N-type doping layer is 100-585°C.

[0015] Preferably, the diffusion temperature of the P-type doping layer is 750-950°C, and the diffusion temperature of the N-type doping layer is 100-900°C.

[0016] Preferably, the crystallization rate of the P-type doping layer is greater than the crystallization rate of the N-type doping layer.

[0017] Preferably, the band gap width of the P-type doping layer is 1.12 to 1.65 eV; the band gap width of the N-type doping layer is 1.1 to 1.6 eV.

[0018] Preferably, the first passivation layer contains a P-type dopant, the second passivation layer contains an N-type dopant, and the doping concentration of the P-type dopant in the first passivation layer is greater than the doping concentration of the N-type dopant in the second passivation layer.

[0019] Preferably, the thickness of the P-type doping layer is greater than the thickness of the N-type doping layer.

[0020] Preferably, the thickness of the first passivation layer is smaller than the thickness of the second passivation layer.

[0021] Preferably, both the first passivation layer and the second passivation layer are porous passivation layers, and the hole density of the first passivation layer is greater than the hole density of the second passivation layer.

[0022] Preferably, both the first passivation layer and the second passivation layer are porous passivation layers, and the average pore size of the holes in the first passivation layer is larger than the average pore size of the holes in the second passivation layer.

[0023] Preferably, the solar cell is a back-contact solar cell, and the P region and the N region are located on the same surface of the silicon substrate.

[0024] Preferably, the solar cell is a double-sided solar cell, and the P region and the N region are respectively located on two opposite sides of the silicon substrate.

[0025] The present invention also provides a battery assembly, comprising the above-mentioned solar cell.

[0026] The present invention also provides a photovoltaic system, comprising the above-mentioned battery assembly.

[0027] A solar cell provided by the present invention can improve the conductive effect of the P-type doping layer by setting the bandgap width of the P-type doping layer to be smaller than the bandgap width of the N-type doping layer, that is, by reducing the bandgap width of the P-type doping layer and reducing the resistance of the P-type doping layer, thereby improving the current transmission effect of the P region and achieving a balance between the current transmission effects of the P region and the N region. The problem of poor current transmission effect in the P region of a traditional solar cell can be solved, so that both the P region and the N region of the solar cell can achieve good current transmission effects, thereby effectively improving the battery efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] Figure 1 A schematic diagram of a solar cell provided by an embodiment of the present invention;

[0029] Figure 2 A schematic diagram of another solar cell provided by an embodiment of the present invention. DETAILED DESCRIPTION

[0030] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.

[0031] A solar cell provided by an embodiment of the present invention can improve the conductive effect of the P-type doping layer by setting the bandgap width of the P-type doping layer to be smaller than the bandgap width of the N-type doping layer, that is, by reducing the bandgap width of the P-type doping layer, thereby improving the current transmission effect of the P region, achieving a balance between the current transmission effects of the P region and the N region, and solving the problem of poor current transmission effect in the P region of traditional solar cells, so that both the P region and the N region of the solar cell can achieve good current transmission effects, thereby effectively improving the battery efficiency.

[0032] Please refer to Figure 1 and Figure 2 , an embodiment of the present invention provides a solar cell, comprising:

[0033] A silicon substrate 1, wherein a P region 11 and an N region 12 are provided on the surface of the silicon substrate 1;

[0034] The first passivation layer 2 located in the P region 11 is provided on the surface of the silicon substrate 1;

[0035] The second passivation layer 3 located in the N region 12 is provided on the surface of the silicon substrate 1;

[0036] A P-type doped layer 4 is provided on a side of the first passivation layer 2 facing away from the silicon substrate 1;

[0037] An N-type doped layer 5 is disposed on a side of the second passivation layer 3 facing away from the silicon substrate 1;

[0038] The band gap width of the P-type doping layer 4 is smaller than the band gap width of the N-type doping layer 5 .

[0039] In the embodiment of the present invention, the solar cell provided sets the bandgap width of the P-type doping layer 4 to be smaller than the bandgap width of the N-type doping layer 5. It can be understood that, under the premise that the bandgap width of the N-type doping layer 5 remains unchanged, by reducing the bandgap width of the P-type doping layer 4, the resistance of the P-type doping layer 4 is reduced, and the conductive effect of the P-type doping layer 4 is improved, so that the current transmission effect of the P region can be improved, and the current transmission effect of the P region 11 and the N region 12 can be balanced. The problem of poor current transmission effect of the P region 11 of the traditional solar cell can be solved, so that the P region 11 and the N region 12 of the solar cell can both achieve good current transmission effects, effectively improving the battery efficiency.

[0040] Of course, in some other embodiments, the band gap width of the P-type doping layer 4 may also be greater than or equal to the band gap width of the N-type doping layer 5 .

[0041] In the embodiment of the present invention, the P-type doping layer 4 includes one of P-type polycrystalline silicon, P-type microcrystalline silicon, P-type nanocrystalline silicon, P-type amorphous silicon, or a mixture of the above materials; the N-type doping layer includes one of N-type polycrystalline silicon, N-type microcrystalline silicon, N-type nanocrystalline silicon, N-type amorphous silicon, or a mixture of the above materials. In the embodiment of the present invention, the P-type doping layer 4 is electrically connected to the silicon substrate 1 through the first passivation layer 2, and the N-type doping layer 5 is electrically connected to the silicon substrate 1 through the second passivation layer 3.

[0042] The band gap is the energy difference between the lowest point of the conduction band and the highest point of the valence band. It is also called the energy gap. The larger the band gap, the more difficult it is for electrons to be excited from the valence band to the conduction band, the lower the intrinsic carrier concentration, and the lower the conductivity. Therefore, the embodiment of the present invention can improve the conductive effect of the P-type doping layer 4 by reducing the band gap width of the P-type doping layer 4, thereby improving the current transmission effect of the P region 11, and achieving a balance between the current transmission effects of the P region 11 and the N region 12.

[0043] In the embodiment of the present invention, the silicon substrate 1 may be a P-type silicon substrate 1 or an N-type silicon substrate 1. The surface of the silicon substrate 1 may be the backlight surface or the light-facing surface of the solar cell.

[0044] Please refer to Figure 1 As an embodiment of the invention, the solar cell is a back contact solar cell, and the P region 11 and the N region 12 are located on the same surface of the silicon substrate 1. The silicon substrate 1 includes a front surface 101 and a back surface 102 opposite to the front surface 101. The front surface 101 of the silicon substrate 1 is the light-facing surface of the back contact solar cell, and the back surface 102 of the silicon substrate 1 is the backlight surface of the back contact solar cell. The P region 11 and the N region 12 are both located on the back surface 102 of the silicon substrate 1.

[0045] There are multiple P regions 11 and multiple N regions 12, which are alternately arranged in sequence, and an isolation region 13 is arranged between adjacent P regions 11 and N regions 12. The isolation region 13 may be a groove or a gap.

[0046] In this embodiment, the front surface 101 of the silicon substrate 1 is further provided with an anti-reflection layer 10 to reduce the reflection of sunlight and improve the efficiency of the cell. Optionally, the anti-reflection layer 10 may be a silicon oxide layer or a silicon nitride layer.

[0047] Please refer to Figure 2 As another embodiment of the invention, the solar cell is a bifacial solar cell, and the P region 11 and the N region 12 are respectively located on two opposite sides of the silicon substrate 1. The silicon substrate 1 includes a front side 101 and a back side 102 opposite to the front side 101. The front side 101 of the silicon substrate 1 is the light-facing side of the bifacial solar cell, and the back side 102 of the silicon substrate 1 is the backlight side of the bifacial solar cell. One of the P region 11 and the N region 12 is located on the front side 101 of the silicon substrate 1, and the other is located on the back side 102 of the silicon substrate 1.

[0048] in, Figure 2 The P region 11 shown in the figure is located on the front side 101 of the silicon substrate 1, and the N region 12 is located on the back side 102 of the silicon substrate 1. The P region 11 may completely cover the front side 101 of the silicon substrate 1, or may only cover a part of the front side 101 of the silicon substrate 1; the N region 12 may completely cover the back side 102 of the silicon substrate 1, or may only cover a part of the back side 102 of the silicon substrate 1. There may also be multiple P regions 11 and N regions 12. Preferably, the P region 11 covers a part of the front side 101 of the silicon substrate 1, and an isolation region 13 is provided between two adjacent P regions 11; the N region 12 only covers a part of the back side 102 of the silicon substrate 1, and an isolation region 13 is provided between two adjacent N regions 12, which can reduce light parasitic absorption. The isolation region 13 may be a groove or a gap.

[0049] In the embodiment of the present invention, the doping polarities of the P-type doping layer 4 and the N-type doping layer 5 are opposite. The P-type doping layer 4 contains a P-type dopant, and the N-type doping layer 5 contains an N-type dopant. The P-type dopant is a IIIA group element dopant, and the N-type dopant is a VA group element dopant. For example, the P-type dopant may be a boron dopant, and the N-type dopant may be a phosphorus dopant.

[0050] As an embodiment of the present invention, the solar cell further comprises:

[0051] A first electrode 6, disposed in the P region 11 and in contact with the P-type doped layer 4;

[0052] The second electrode 7 is disposed in the N region 12 and in contact with the N-type doped layer 5 .

[0053] In this embodiment, the first electrode 6 contacts the P-type doping layer 4 to form an ohmic contact, and the second electrode 7 contacts the N-type doping layer 5 to form an ohmic contact. Preferably, the depth of the first electrode 6 entering the P-type doping layer 4 is greater than the depth of the second electrode 7 entering the N-type doping layer 5, which can increase the contact area between the first electrode 6 and the P-type doping layer 4, further improve the conductivity of the P region 11, and improve the battery efficiency.

[0054] As an embodiment of the present invention, the deposition temperature of the P-type doping layer 4 is greater than the deposition temperature of the N-type doping layer 5 .

[0055] In this embodiment, the deposition temperature of the P-type doping layer 4 is the temperature at which the intrinsic amorphous silicon of the P-type doping layer 4 is deposited; and the deposition temperature of the N-type doping layer 5 is the temperature at which the intrinsic amorphous silicon of the N-type doping layer 5 is deposited. The deposition temperatures of the P-type doping layer 4 and the N-type doping layer 5 can be set according to actual needs, and it is only necessary to satisfy that the deposition temperature of the P-type doping layer 4 is greater than the deposition temperature of the N-type doping layer 5. Among them, by setting the deposition temperature of the P-type doping layer 4 to be greater than the deposition temperature of the N-type doping layer 5, the band gap width of the P-type doping layer 4 can be smaller than the band gap width of the N-type doping layer 5, and the implementation method is simple, which is conducive to reducing the implementation cost.

[0056] As an embodiment of the present invention, the deposition temperature of the P-type doping layer 4 is 595-630° C., and the deposition temperature of the N-type doping layer 5 is 100-585° C.

[0057] In this embodiment, the deposition temperature of the P-type doping layer 4 and the N-type doping layer 5 can be set according to actual needs, and it is only necessary to satisfy that the deposition temperature of the P-type doping layer 4 is greater than the deposition temperature of the N-type doping layer 5. For example, the deposition temperature of the P-type doping layer 4 can be 595°C, or 598°C, or 600°C, or 605°C, or 609°C, or 610°C, or 616°C, or 619°C, or 620°C, or 628°C, or 630°C; the deposition temperature of the N-type doping layer 5 can be 100°C, or 150°C, or 180°C, or 200°C, or 220°C, or 260°C, or 300°C, or 350°C, or 380°C, or 400°C, or 420°C, or 450°C, or 470°C, or 500°C, or 510°C, or 536°C, or 565°C, or 585°C. Of course, the deposition temperature of the P-type doping layer 4 may also be other values ​​in the range of 595-630° C., and the deposition temperature of the N-type doping layer 5 may also be other values ​​in the range of 100-585° C.

[0058] As an embodiment of the present invention, the diffusion temperature of the P-type doping layer 4 is greater than the diffusion temperature of the N-type doping layer 5 .

[0059] The diffusion temperature of the P-type doping layer 4 is the temperature at which the intrinsic amorphous silicon of the P-type doping layer 4 diffuses to form the P-type doping layer; the diffusion temperature of the N-type doping layer 5 is the temperature at which the intrinsic amorphous silicon of the N-type doping layer 5 diffuses to form the N-type doping layer. The diffusion temperatures of the P-type doping layer 4 and the N-type doping layer 5 can be set according to actual needs, and it is only necessary to satisfy that the diffusion temperature of the P-type doping layer 4 is greater than the diffusion temperature of the N-type doping layer 5. By setting the diffusion temperature of the P-type doping layer 4 to be greater than the diffusion temperature of the N-type doping layer 5, it is also possible to achieve that the band gap width of the P-type doping layer 4 is smaller than the band gap width of the N-type doping layer 5, and the implementation method is simple, which is conducive to reducing the implementation cost.

[0060] As an embodiment of the present invention, the diffusion temperature of the P-type doping layer 4 is 750-950° C., and the diffusion temperature of the N-type doping layer 5 is 100-900° C.

[0061] In this embodiment, the diffusion temperatures of the P-type doping layer 4 and the N-type doping layer 5 can be set according to actual needs, as long as the diffusion temperature of the P-type doping layer 4 is greater than the diffusion temperature of the N-type doping layer 5. For example, the diffusion temperature of the P-type doping layer 4 can be 750°C, or 762°C, or 770°C, or 780°C, or 792°C, or 800°C, or 812°C, or 820°C, or 835°C, or 860°C, or 865°C, or 872°C, or 880°C, or 890°C, or 900°C, or 910°C, or 920°C, or 930°C, or 945°C, or 950°C; the diffusion temperature of the N-type doping layer 5 can be 10 0°C, or 120°C, or 140°C, or 150°C, or 160°C, or 170°C, or 190°C, or 200°C, or 240°C, or 285°C, or 300°C, or 340°C, or 380°C, or 400°C, or 466°C, or 500°C, or 550°C, or 580°C, or 600°C, or 620°C, or 700°C, or 760°C, or 800°C, or 840°C, or 880°C, or 900°C. Of course, the diffusion temperature of the P-type doping layer 4 may also be other values ​​in the range of 750 to 950°C, and the diffusion temperature of the N-type doping layer 5 may also be other values ​​in the range of 100 to 900°C.

[0062] As an embodiment of the present invention, the crystallization rate of the P-type doping layer 4 is greater than the crystallization rate of the N-type doping layer 5 .

[0063] In this embodiment, under the premise that the crystallization rate of the N-type doping layer 5 remains unchanged, the crystallization rate of the P-type doping layer 4 is increased so that the crystallization rate of the P-type doping layer 4 is higher than that of the N-type doping layer 5, and the band gap width of the P-type doping layer 4 can be reduced, thereby improving the conductivity of the P-type doping layer 4, which is beneficial to improving the photoelectric conversion efficiency of the battery.

[0064] In this embodiment, the crystallization rate of the P-type doped layer 4 and the crystallization rate of the N-type doped layer 5 both refer to the average crystallization rate, which can be obtained by measuring the crystallization rates of different regions in the P-type doped layer 4 and the N-type doped layer 5 respectively, and taking the average value of the measured multiple crystallization rates.

[0065] For example, the crystallization rate of the P-type doping layer 4 and the N-type doping layer 5 at different thicknesses can be tested to obtain an average crystallization rate. In a specific example, the P-type doping layer 4 and the N-type doping layer 5 can be divided into five equal parts in the thickness direction of the P-type doping layer 4 and the N-type doping layer 5, and the crystallization rate of each equal part can be tested to obtain an average crystallization rate. In other examples, the P-type doping layer 4 and the N-type doping layer 5 can also be divided into other numbers of equal parts in the thickness direction of the P-type doping layer 4 and the N-type doping layer 5 to obtain the average crystallization rate of the P-type doping layer 4 and the N-type doping layer 5.

[0066] In some embodiments, the crystallinity of the P-type doping layer 4 and the N-type doping layer 5 may be tested by Raman spectroscopy.

[0067] For example, the crystallization rate of the P-type doping layer 4 is 90% to 95%; and the crystallization rate of the N-type doping layer 5 is 85% to 90%.

[0068] As an embodiment of the present invention, the band gap width of the P-type doping layer 4 is 1.12-1.65 eV; the band gap width of the N-type doping layer 5 is 1.1-1.6 eV.

[0069] In this embodiment, the band gap widths of the P-type doping layer 4 and the N-type doping layer 5 are respectively set within the above ranges, which can balance the current transmission effects of the P region 11 and the N region 12 and facilitate the processing and preparation of the P-type doping layer 4 and the N-type doping layer 5.

[0070] The band gap widths of the P-type doping layer 4 and the N-type doping layer 5 can be set according to actual needs, and it is only necessary that the band gap width of the P-type doping layer 4 is greater than the band gap width of the N-type doping layer 5 . For example, the band gap width of the P-type doped layer 4 can be 1.12eV, or 1.15eV, or 1.17eV, or 1.19eV, or 1.2eV, or 1.35eV, or 1.4eV, or 1.46eV, or 1.50eV, or 1.58eV, or 1.6eV, or 1.61eV, or 1.63eV, or 1.65eV; the band gap width of the N-type doped layer 5 can be 1.1eV, or 1.12eV, or 1.17eV, or 1.2eV, or 1.24eV, or 1.3eV, or 1.36eV, or 1.4eV, or 1.42eV, or 1.46eV, or 1.52eV, or 1.58eV, or 1.6eV. Of course, the band gap width of the P-type doping layer 4 may also be other values ​​within the range of 1.2 to 1.65 eV, and the band gap width of the N-type doping layer 5 may also be other values ​​within the range of 1.1 to 1.6 eV.

[0071] As an embodiment of the present invention, the first passivation layer 2 contains a P-type dopant, the second passivation layer 3 contains an N-type dopant, and the doping concentration of the P-type dopant in the first passivation layer 2 is greater than the doping concentration of the N-type dopant in the second passivation layer 3 .

[0072] In this embodiment, since the doping concentration of the P-type dopant of the first passivation layer 2 is greater than the doping concentration of the N-type dopant of the second passivation layer 3, that is, by increasing the doping concentration of the P-type dopant of the first passivation layer 2, reducing the resistivity of the first passivation layer 2, and improving the conductivity of the first passivation layer 2, the current transmission effect of the P region 11 can be further improved, thereby improving the battery efficiency.

[0073] As an embodiment of the present invention, the doping concentration of the P-type dopant in the first passivation layer 2 is 1×10 19 ~8×10 21 atoms / cm 3 The doping concentration of the N-type dopant in the second passivation layer 3 is 5×10 18 ~5×10 21 atoms / cm 3 .

[0074] In this embodiment, the doping concentrations of the first passivation layer 2 and the second passivation layer 3 can be set according to actual needs, as long as the doping concentration of the P-type dopant in the first passivation layer 2 is greater than the doping concentration of the N-type dopant in the second passivation layer 3 .

[0075] Among them, the doping concentration of the P-type dopant is the average value or peak value of the doping concentration of the P-type dopant, and the doping concentration of the N-type dopant is the average value or peak value of the doping concentration of the N-type dopant; wherein the peak value is the maximum doping concentration value. When comparing the doping concentrations, the comparison is made at the same time with the average value of the doping concentration or at the same time with the peak value of the doping concentration. It can be understood that the average value of the doping concentration of the P-type dopant in any area of ​​the first passivation layer 2 is greater than the average value of the doping concentration of the N-type dopant in any area of ​​the second passivation layer 3; it can also be that the peak value of the doping concentration of the P-type dopant in any area of ​​the first passivation layer 2 is greater than the peak value of the doping concentration of the N-type dopant in any area of ​​the second passivation layer 3.

[0076] In the embodiment of the present invention, the doping concentration of the P-type dopant may be the doping concentration of the activated P-type dopant, and the doping concentration of the N-type dopant may be the doping concentration of the activated N-type dopant, and the doping concentrations of the activated P-type dopant and the N-type dopant may be measured by a spreading resistance profile (SRP) or an electrochemical capacitance-voltage method (ECV). Of course, the doping concentration of the P-type dopant may also be the sum of the doping concentration of the activated P-type dopant and the doping concentration of the inactivated P-type dopant, and the doping concentration of the N-type dopant may also be the sum of the doping concentration of the activated N-type dopant and the doping concentration of the inactivated N-type dopant, and may be measured by secondary ion mass spectrometry (SIMS).

[0077] As an embodiment of the present invention, both the first passivation layer 2 and the second passivation layer 3 are porous passivation layers, and the hole density of the first passivation layer 2 is greater than the hole density of the second passivation layer 3 .

[0078] In this embodiment, the holes on the first passivation layer 2 vertically penetrate the first passivation layer 2, and the holes on the second passivation layer 3 vertically penetrate the second passivation layer 3. Among them, the P-type doped layer 4 contacts the silicon substrate 1 using the holes on the first passivation layer 2, and the N-type doped layer 5 contacts the silicon substrate 1 using the holes on the second passivation layer 3, which is beneficial to reduce current loss and improve battery conversion efficiency. Since the hole density of the first passivation layer 2 is greater than the hole density of the second passivation layer 3, that is, the number of holes per unit area of ​​the first passivation layer 2 is greater than the number of holes per unit area of ​​the second passivation layer 3, the resistance of the first passivation layer 2 can be reduced, so that the resistance of the first passivation layer 2 is less than the resistance of the second passivation layer 3, the conductivity of the first passivation layer 2 is improved, and the conductivity effect of the P region 11 is improved, and the implementation method is simple.

[0079] The holes of the first passivation layer 2 and the second passivation layer 3 can be prepared by chemical corrosion, dry etching or thermal diffusion impact, etc., which are prepared according to actual use needs and are not specifically limited here. When the first passivation layer 2 and the second passivation layer 3 are observed from a top view angle, the first passivation layer 2 and the second passivation layer 3 present a porous structure, and when the first passivation layer 2 and the second passivation layer 3 are observed from a cross-sectional angle, the first passivation layer 2 and the second passivation layer 3 show a multi-channel structure.

[0080] As an embodiment of the present invention, the first passivation layer 2 and the second passivation layer 3 are both porous passivation layers, and the average pore size of the pores of the first passivation layer 2 is greater than the average pore size of the pores of the second passivation layer 3 .

[0081] In this embodiment, the apertures of the holes in the first passivation layer 2 may be equal or unequal; similarly, the apertures of the holes in the second passivation layer 3 may be equal or unequal. The average aperture of the holes in the first passivation layer 2 may be understood as the average aperture of all holes in the first passivation layer 2 or the average aperture of all holes in a unit area; the average aperture of the holes in the second passivation layer 3 may be understood as the average aperture of all holes in the second passivation layer 3 or the average aperture of all holes in a unit area. By setting the average aperture of the holes in the first passivation layer 2 to be larger than the average aperture of the holes in the second passivation layer 3, the resistance of the first passivation layer 2 may also be reduced, so that the resistance of the first passivation layer 2 is smaller than the resistance of the second passivation layer 3, the conductivity of the first passivation layer 2 is improved, and the conductivity effect of the P region 11 is improved, and the implementation method is simple.

[0082] As an optional embodiment of the present invention, the hole diameters of the first passivation layer 2 and the second passivation layer 3 are less than 10 um, and the average hole diameter of the first passivation layer 2 and the second passivation layer 3 is greater than the average hole diameter of the second passivation layer 3 .

[0083] As an embodiment of the present invention, the thickness of the first passivation layer 2 is smaller than the thickness of the second passivation layer 3 .

[0084] In this embodiment, the thickness of the first passivation layer 2 is less than the thickness of the second passivation layer 3, that is, by thinning the thickness of the first passivation layer 2, it is beneficial to the setting of holes, which is beneficial to improving the tunneling effect of the first passivation layer 2, improving the conductive effect of the P region 11, and further improving the battery transmission effect of the P region 11.

[0085] As an embodiment of the present invention, the materials of the first passivation layer 2 and the second passivation layer 3 may be the same or different. For example, the first passivation layer 2 and the second passivation layer 3 may be one or a combination of silicon oxide, silicon oxynitride, and silicon nitride, respectively. When the materials of the first passivation layer 2 and the second passivation layer 3 are different, the material resistivity of the first passivation layer 2 is less than the material resistivity of the second passivation layer 3, so as to facilitate the realization of different resistivities of the first passivation layer 2 and the second passivation layer 3; when the materials of the first passivation layer 2 and the second passivation layer 3 are the same, the resistivity of the first passivation layer 2 can be achieved by changing the doping concentration of the first passivation layer 2 and the second passivation layer 3, the processing technology, etc. to achieve that the resistivity of the first passivation layer 2 is less than the resistivity of the second passivation layer 3.

[0086] As an embodiment of the present invention, the thickness of the P-type doping layer 4 is greater than the thickness of the N-type doping layer 5 .

[0087] In this embodiment, the thickness of the P-type doping layer 4 is greater than the thickness of the N-type doping layer 5, which can ensure that the P-type doping layer 4 has a good ability to prevent electrode burn-through and make the P region 11 have a good passivation effect. Of course, in some other embodiments, the thickness of the P-type doping layer 4 can also be less than or equal to the thickness of the N-type doping layer 5.

[0088] As an embodiment of the present invention, it also includes:

[0089] A first back passivation layer 8 is provided on a side of the P-type doped layer 4 facing away from the silicon substrate 1;

[0090] The second back passivation layer 9 is disposed on a side of the N-type doped layer 5 facing away from the silicon substrate 1 .

[0091] Among them, the first back passivation layer 8 and the second back passivation layer 9 may both include at least one or a combination of aluminum oxide film layers, silicon oxide film layers, silicon nitride film layers, silicon carbide film layers, and silicon oxynitride film layers. For example, in some embodiments, the first back passivation layer 8 and the second back passivation layer 9 may include aluminum oxide film layers and silicon nitride film layers stacked in sequence, and there is no specific limitation here.

[0092] In this embodiment, the first back passivation layer 8 and the second back passivation layer 9 can further enhance the battery passivation effect and improve the battery efficiency.

[0093] The embodiment of the present invention also provides a battery assembly, which includes the solar cell of the above embodiment. It should be noted that the battery assembly and the solar cell have the same or similar beneficial effects, and the relevant parts between the two can be referenced to each other. In order to avoid repetition, they will not be repeated here.

[0094] The embodiment of the present invention further provides a photovoltaic system, which includes the battery assembly of the above embodiment. It should be noted that the photovoltaic system has the same or similar beneficial effects as the above solar cell, and the relevant parts between the two can be referenced to each other. In order to avoid repetition, it will not be repeated here.

[0095] A solar cell provided by an embodiment of the present invention can improve the conductive effect of the P-type doping layer 4 by setting the bandgap width of the P-type doping layer 4 to be smaller than the bandgap width of the N-type doping layer 5, that is, by reducing the bandgap width of the P-type doping layer 4, thereby improving the current transmission effect of the P region, achieving a balance between the current transmission effects of the P region and the N region, and solving the problem of poor current transmission effect in the P region of traditional solar cells, so that both the P region and the N region of the solar cell can achieve good current transmission effects, thereby effectively improving the battery efficiency.

[0096] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A solar cell, characterized in that: include: A silicon substrate, wherein a P region and an N region are provided on the surface of the silicon substrate; A first passivation layer located in the P region is disposed on the surface of the silicon substrate; A second passivation layer located in the N region is disposed on the surface of the silicon substrate; A P-type doped layer, disposed on a side of the first passivation layer away from the silicon substrate; An N-type doped layer, disposed on a side of the second passivation layer away from the silicon substrate; Wherein, the band gap width of the P-type doping layer is smaller than the band gap width of the N-type doping layer.

2. The solar cell according to claim 1, characterized in that The deposition temperature of the P-type doping layer is greater than the deposition temperature of the N-type doping layer.

3. The solar cell according to claim 1, characterized in that The diffusion temperature of the P-type doping layer is greater than the diffusion temperature of the N-type doping layer.

4. The solar cell according to claim 2, characterized in that: The deposition temperature of the P-type doping layer is 595-630° C., and the deposition temperature of the N-type doping layer is 100-585° C.

5. The solar cell according to claim 3, characterized in that: The diffusion temperature of the P-type doping layer is 750-950°C, and the diffusion temperature of the N-type doping layer is 100-900°C.

6. The solar cell according to claim 1, characterized in that The crystallization rate of the P-type doping layer is greater than the crystallization rate of the N-type doping layer.

7. The solar cell according to claim 1, characterized in that The band gap width of the P-type doping layer is 1.12-1.65 eV; the band gap width of the N-type doping layer is 1.1-1.6 eV.

8. The solar cell according to claim 1, characterized in that The first passivation layer contains a P-type dopant, and the second passivation layer contains an N-type dopant. The doping concentration of the P-type dopant in the first passivation layer is greater than the doping concentration of the N-type dopant in the second passivation layer.

9. The solar cell according to claim 1, characterized in that: The thickness of the P-type doping layer is greater than the thickness of the N-type doping layer.

10. The solar cell according to claim 1, characterized in that: The thickness of the first passivation layer is smaller than the thickness of the second passivation layer.

11. The solar cell according to claim 1, characterized in that: The first passivation layer and the second passivation layer are both porous passivation layers, and the hole density of the first passivation layer is greater than the hole density of the second passivation layer.

12. The solar cell according to claim 1, characterized in that The first passivation layer and the second passivation layer are both porous passivation layers, and the average pore size of the holes in the first passivation layer is larger than the average pore size of the holes in the second passivation layer.

13. The solar cell according to claim 1, characterized in that The solar cell is a back contact solar cell, and the P region and the N region are located on the same surface of the silicon substrate.

14. The solar cell according to claim 1, characterized in that The solar cell is a double-sided solar cell, and the P region and the N region are respectively located on two opposite sides of the silicon substrate.

15. A battery assembly, characterized in that: A solar cell comprising any one of claims 1 to 14.

16. A photovoltaic system, characterized in that: A battery assembly comprising the battery assembly described in claim 15 above.

Citation Information

Cited By

  • Solar cell and photovoltaic module

    CN120500166A

  • Solar cell and photovoltaic module

    CN120500166B

  • Cell, module, and photovoltaic system

    WO2026051714A1