Welding process for connector on FPC (Flexible Printed Circuit)

By setting specific reinforcement board and solder paste template structures on the FPC circuit board, the problems of low efficiency and unstable quality in the welding process of traditional FPC connectors are solved, and more efficient soldering quality and cost savings are achieved, suitable for batch automatic Production.

CN119012555APending Publication Date: 2024-11-22GUANGZHOU AMPHENOL SINCERE FLEX CIRCUITS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411099289.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-12
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The welding process of traditional FPC connectors has glass fiber reinforced plates on both sides, resulting in low welding efficiency and unstable quality, prone to pin short circuit defects, and high production costs.

Method used

A first through-hole corresponding to the connector pin pad hole is provided on one side of the FPC circuit board, and a window is provided on the other side. The projection of the solder paste template is used to connect to the connector pin pad hole, and then tin is given after printing the solder paste. The paste penetrates the entire connector pin pad hole, fills the pad hole after reflow, and secures the connector.

Benefits of technology

It improves welding quality and efficiency, avoids the difficulties of manual welding and poor insulation problems caused by cleaning residues, reduces production costs, and realizes the possibility of mass automatic production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119012555A_ABST
    Figure CN119012555A_ABST
Patent Text Reader

Abstract

The invention discloses a process for welding a connector on an FPC (Flexible Printed Circuit), which comprises the following steps of: arranging reinforcing plates on two surfaces of an end part of an FPC circuit board for installing the connector, forming a first through hole corresponding to a connector pin bonding pad hole in the reinforcing plate on one surface, and forming a window in a position corresponding to the connector pin bonding pad hole in the reinforcing plate on the other surface; the solder paste template is attached to the reinforcing plate on the window face and the FPC circuit board; a solder paste template protruding part on the solder paste template is attached to the window of the reinforcing plate, and a second through hole of the solder paste template protruding part is in butt joint fit with a connector pin bonding pad hole; and after the solder paste is printed in the second through hole and the connector pin is inserted from the first through hole, the solder paste penetrates through the whole connector pin bonding pad hole, the solder paste is melted and retracted after reflow soldering to fill the connector pin bonding pad hole in the FPC circuit board, the connector is welded and fixed, and the solder paste template is taken down.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to an FPC welding connector, in particular to a connector welding process on an FPC. Background Art

[0002] FPC (Flexible Printed Circuit, FPC), also known as soft circuit board, flexible circuit board, is highly favored in the new energy field for its excellent characteristics such as light weight, thin thickness, and free bending and folding. The electronic components of FPC are assembled through SMT welding. During the SMT welding process, the connector on the FPC is welded. Due to the thin thickness of FPC, it is necessary to add glass fiber reinforcement plates on the upper and lower sides of the welding point between FPC and connector pins. However, in the traditional welding process, since there are reinforcement plates on both sides of FPC, when welding the connector, it is necessary to manually use a soldering iron with tin wire on one side, or perform wave soldering. However, wave soldering often causes pin short-circuit defects for fine pin welding, and the production cost is high, which makes the overall welding efficiency low and the quality unstable. Summary of the invention

[0003] The object of the present invention is to provide a connector welding process on an FPC with better welding quality, so as to improve the overall welding efficiency.

[0004] The connector welding process on the FPC of the present invention comprises the following steps: S1. Reinforcement plates are arranged on both sides of the end of the FPC circuit board where the connector is installed, wherein the reinforcement plate on one side is provided with a first through hole corresponding to the connector pin pad hole, and the reinforcement plate on the other side is provided with a window at a position corresponding to the connector pin pad hole; S2, attach the solder paste template to the reinforcing plate on the window surface and the FPC circuit board; S3, the solder paste template protrusion on the solder paste template fits the window of the reinforcement plate, and the second through hole of the solder paste template protrusion is butted with the connector pin pad hole; S4. After printing solder paste in the second through hole, the connector pin is inserted from the first through hole, and the solder paste is allowed to penetrate the entire connector pin pad hole. After reflow soldering, the solder paste melts and shrinks, filling the connector pin pad hole on the FPC circuit board, and the connector is soldered and fixed.

[0005] The connector welding process on the FPC described in the present invention is to open a first through hole corresponding to the connector pin pad hole on the reinforcement plate on one side of the FPC circuit board, and open a window at a position corresponding to the connector pin pad hole on the reinforcement plate on the other side, and the second through hole of the protruding portion of the solder paste template and the connector pin pad hole are docked and matched with each other, and solder paste is printed on the second through hole. After the connector pin is inserted from the first through hole, the solder paste is allowed to pass through the entire connector pin pad hole. After reflow soldering, the solder paste melts and shrinks to fill the connector pin pad hole on the FPC circuit board, thereby overcoming the difficulty of manual soldering required for double-sided reinforcement plate back welding, and the welding quality is better and the overall welding efficiency is higher. In addition, since no cleaning and manual soldering are required, the problem of poor insulation caused by cleaning residues is avoided. In addition, compared with the existing technology, the company's costs are saved overall, and while the welding efficiency of the product is improved, the purpose of automatic mass production can be achieved in terms of quality assurance.

[0006] As a preferred solution of the present invention, step S2 comprises: S2-1, locating the positioning holes set on the reinforcement plate and the positioning points set on the solder paste template; S2-2. Fit the solder paste template to the reinforcement plate on the window surface and the FPC circuit board according to the positioned solder paste template.

[0007] As a preferred solution of the present invention, both ends of the solder paste template are provided with positioning points, and both end reinforcement plates of the FPC circuit board are provided with positioning holes matching with the positioning points.

[0008] As a preferred solution of the present invention, multiple rows of positioning points and multiple rows of solder paste template protrusions are provided at both ends of the solder paste template, and one solder paste template is bonded to multiple FPC circuit boards.

[0009] As a preferred solution of the present invention, the second through hole of the raised portion of the solder paste template is configured as a stepped recessed second through hole.

[0010] As a preferred embodiment of the present invention, the depth of the step is 0.15-0.25 mm.

[0011] As a preferred solution of the present invention, the solder paste template is a steel solder paste template. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 A schematic diagram of a process flow of a connector welding process on an FPC according to the present invention; Figure 2 This is the main view of the FPC circuit board; Figure 3 This is the rear view of the FPC circuit board; Figure 4 This is the front view of the solder paste template. DETAILED DESCRIPTION

[0013] The following will be combined with the accompanying drawings to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0014] A connector welding process on FPC, such as Figure 1 As shown, the following steps are included: S1. A reinforcing plate 2 is arranged on both sides of the end of the FPC circuit board 1 where the connector is installed. The reinforcing plate on one side has a first through hole 3 corresponding to the connector pin pad hole, and the reinforcing plate on the other side has a window 4 at a position corresponding to the connector pin pad hole.

[0015] Since both ends of the FPC circuit board need to be connected to the connector, reinforcement plates are set at the connector pin pad holes at both ends of the FPC circuit board. Reinforcement plates are added on both sides of the FPC circuit board to increase the strength of the FPC circuit board. The reinforcement plates and the FPC circuit board are fixed together with glue.

[0016] In this embodiment, a reinforcing plate with a first through hole corresponding to the connector pin pad hole is pasted on the front side of the FPC circuit board, and the opening position of the first through hole is tangent to the position of the connector pin pad hole ring. A reinforcing plate with a window is pasted on the back side of the FPC circuit board, and the window is a rectangular window. The connector pin pad holes have two rows and are located in the middle of the rectangular window.

[0017] S2. Fit the solder paste template to the reinforcement plate on the window surface and the FPC circuit board.

[0018] Step S2 includes: S2-1, positioning the positioning holes 5 set on the reinforcement plate and the positioning points 6 set on the solder paste template; S2-2, laminating the reinforcement plate and the FPC circuit board on the window surface according to the positioned solder paste template. Positioning by the positioning holes 5 on the reinforcement plate and the positioning points 6 on the solder paste template makes it easier to laminarize the FPC circuit board on the solder paste template, further improving the welding efficiency.

[0019] In this embodiment, if Figure 2 and Figure 3 As shown in the figure, the solder paste template uses a steel solder paste template. There are positioning points at both ends of the solder paste template. The reinforcement plates at both ends of the FPC circuit board are equipped with positioning holes that match the positioning points. The positioning points at both ends of the solder paste template make it easier for the FPC circuit board to fit on the solder paste template, further improving the welding yield. Figure 4As shown, three rows of positioning points and multiple rows of solder paste template protrusions are provided at both ends of the solder paste template. One solder paste template is bonded to three FPC circuit boards, thereby further improving the overall welding efficiency.

[0020] S3. The solder paste template protrusion 7 on the solder paste template fits the window of the reinforcement plate, and the second through hole 8 of the solder paste template protrusion is butted against the connector pin pad hole.

[0021] The second through hole of the raised portion of the solder paste template is set as a stepped recessed second through hole, and the depth of the step is 0.15-0.25mm, so that the solder paste can be more sufficient to fill the entire connector pin pad hole, thereby reducing the phenomenon of cold soldering of the connector pin. Therefore, this process is more advantageous for fine-pitch pin welding.

[0022] S4. After printing solder paste in the second through hole, the connector pin is inserted from the first through hole, and the solder paste is allowed to pass through the entire connector pin pad hole. After reflow soldering, the solder paste melts and shrinks, filling the connector pin pad hole on the FPC circuit board, and the connector is soldered and fixed, and the solder paste template is removed.

[0023] This process overcomes the difficulty of manual welding for the rear welding of double-sided reinforcement plates, and has better welding quality and higher overall welding efficiency. In addition, since it does not require cleaning and manual welding, it avoids poor insulation problems caused by cleaning residues. In addition, compared with existing technologies, it saves the company costs overall, improves the welding efficiency of the product, and can also achieve the goal of automatic mass production in terms of quality assurance.

[0024] The above embodiments are only used to illustrate the detailed scheme of the present invention, and the present invention is not limited to the above detailed scheme, that is, it does not mean that the present invention must rely on the above detailed scheme to be implemented. Those skilled in the art should understand that any improvement of the present invention, equivalent replacement of various raw materials of the product of the present invention, addition of auxiliary components, selection of specific methods, etc., all fall within the protection scope and disclosure scope of the present invention.

Claims

1. A connector welding process on FPC, The following steps are involved: S1. Reinforcement plates are arranged on both sides of the end of the FPC circuit board where the connector is installed, wherein the reinforcement plate on one side is provided with a first through hole corresponding to the connector pin pad hole, and the reinforcement plate on the other side is provided with a window at a position corresponding to the connector pin pad hole; S2, attach the solder paste template to the reinforcing plate on the window surface and the FPC circuit board; S3, the solder paste template protrusion on the solder paste template fits the window of the reinforcement plate, and the second through hole of the solder paste template protrusion is butted with the connector pin pad hole; S4. After printing solder paste in the second through hole, the connector pin is inserted from the first through hole, and the solder paste is allowed to pass through the entire connector pin pad hole. After reflow soldering, the solder paste melts and shrinks, filling the connector pin pad hole on the FPC circuit board, and the connector is soldered and fixed, and the solder paste template is removed.

2. The connector welding process on the FPC according to claim 1, It is characterized in that The step S2 comprises: S2-1, locating the positioning holes set on the reinforcement plate and the positioning points set on the solder paste template; S2-2. Fit the solder paste template to the reinforcement plate on the window surface and the FPC circuit board according to the positioned solder paste template.

3. The connector welding process on the FPC according to claim 2, It is characterized in that Both ends of the solder paste template are provided with positioning points, and both end reinforcement plates of the FPC circuit board are provided with positioning holes that match the positioning points.

4. The connector welding process on the FPC according to claim 3, It is characterized in that Multiple rows of positioning points and multiple rows of solder paste template protrusions are provided at both ends of the solder paste template, and one solder paste template is bonded to multiple FPC circuit boards.

5. The connector welding process on the FPC according to claim 1, It is characterized in that The second through hole of the raised portion of the solder paste template is configured as a stepped recessed second through hole.

6. The connector welding process on the FPC according to claim 5, It is characterized in that The depth of the step is 0.15-0.25mm.

7. The connector welding process on the FPC according to any one of claims 1 to 6, It is characterized in that The solder paste template is a steel solder paste template.