Auxiliary film thickness detection device and method

By using an auxiliary film thickness detection device and method to adjust the position of the mask on the OLED display panel, the problems of high cost and difficulty in performance testing of vapor-deposited film thickness monitoring are solved, and efficient and accurate film thickness measurement and performance testing are achieved.

CN119012884APending Publication Date: 2024-11-22HEFEI VISIONOX TECH CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410091100.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-01-23
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In the manufacturing process of OLED display panels, the thickness deviation of the vapor-deposited film layer affects the performance of the display panel. Existing technologies are difficult to effectively monitor the thickness of the vapor-deposited film layer, are costly, and cannot accurately test the optical performance of the light-emitting elements.

Method used

An auxiliary film thickness detection device is used, including a vapor deposition plate, first and second photomasks, and a driving mechanism. The driving mechanism adjusts the positional relationship of the photomasks to form different film layers at different positions on the vapor deposition plate. The film thickness and performance are measured by combining the device with an ellipsometry.

Benefits of technology

It enables multiple measurements of different film thicknesses on the same vapor deposition plate, reducing costs and accurately testing the optical performance of light-emitting elements and the resistance and transmittance of metal films.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119012884A_ABST
    Figure CN119012884A_ABST
Patent Text Reader

Abstract

The embodiment of the invention provides an auxiliary film thickness detection device and method, and relates to the technical field of display. The driving mechanism can drive the mask opening in the second mask plate to move in the extension direction of the evaporation opening relative to the first mask plate, so that evaporation film layers can be formed at different positions of an evaporation area limited by the evaporation opening when the film layers are evaporated in different evaporation cavities; different evaporation film layers are formed on one evaporation plate, so that subsequent film layer thickness measurement is facilitated, the number of needed evaporation plates is reduced, and the cost for monitoring the thickness of the evaporation film layers is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of display technology, and in particular to an auxiliary film thickness detection device and method. Background Art

[0002] In the production process of organic light-emitting diode (OLED) display panels, many film layers are formed by evaporation. The thickness deviation of the evaporated film layer will affect the performance of the display panel, so it is particularly important to monitor the thickness of the evaporated film layer. Summary of the invention

[0003] In order to overcome the technical problems mentioned in the above technical background, the embodiments of the present application provide an auxiliary film thickness detection device and method.

[0004] In a first aspect of the present application, an auxiliary film thickness detection device is provided, the device comprising:

[0005] An evaporation plate, the evaporation plate is used for evaporating a film layer;

[0006] A first mask and a second mask, wherein the first mask is provided with a vapor deposition opening for defining a vapor deposition area on the vapor deposition plate, and the second mask is provided with a mask opening for defining a vapor deposition range in the vapor deposition area;

[0007] A driving mechanism is connected to the first mask and the second mask respectively, and is used to drive the first mask and the second mask to move relative to the evaporation plate.

[0008] In the above structure, the driving mechanism can drive the first mask and the second mask to move relative to the evaporation plate, so that when the film layer is evaporated in different evaporation chambers, the evaporated film layer can be formed at different positions of the evaporation area limited by the evaporation opening, so that different evaporated film layers are formed on one evaporation plate for subsequent film thickness measurement, thereby reducing the number of evaporation plates required and reducing the cost of monitoring the thickness of the evaporated film layer.

[0009] In a possible implementation manner of the present application, the first mask and the second mask are arranged in parallel;

[0010] Preferably, the mask opening is used to limit the evaporation range within the evaporation area each time.

[0011] In a possible implementation manner of the present application, the driving mechanism is further used to drive the second mask to move relative to the first mask, so that the mask opening on the second mask moves relative to the first mask in an extension direction of the evaporation opening.

[0012] In a possible implementation manner of the present application, the device further includes: a carrier;

[0013] The evaporation plate is arranged on one side of the carrier;

[0014] The first mask is located on a side of the evaporation plate away from the carrier;

[0015] The second mask is located on a side of the first mask away from the carrier.

[0016] In a possible implementation manner of the present application, the distance between the first mask and the second mask is 0.2 mm to 0.4 mm.

[0017] In a possible implementation manner of the present application, the driving mechanism includes a first driving mechanism, a second driving mechanism and a third driving mechanism;

[0018] The first driving mechanism is used to drive the first mask and the second mask to approach or move away from the evaporation plate from a first direction parallel to the plane where the evaporation plate is located;

[0019] The second driving mechanism is used to drive the first mask and the second mask to approach or move away from the evaporation plate from a second direction perpendicular to the plane where the evaporation plate is located;

[0020] The third driving mechanism is used to drive the second mask to move relative to the first mask, so that the mask opening moves along the third direction in which the evaporation opening extends;

[0021] Preferably, the first direction, the second direction and the third direction are perpendicular to each other.

[0022] In a possible implementation manner of the present application, the opening size of the evaporation opening is larger than the opening size of the mask opening;

[0023] The orthographic projection of the mask opening on the first mask is located within the evaporation opening.

[0024] In a possible implementation manner of the present application, the evaporation plate is a glass substrate;

[0025] Preferably, the first mask and the second mask are metal masks.

[0026] In a possible implementation manner of the present application, the evaporation openings include a first evaporation opening, a second evaporation opening, and a third evaporation opening;

[0027] The first evaporation opening is used to define a first evaporation area on the evaporation plate for evaporating an optical film layer, the second evaporation opening is used to define a second evaporation area on the evaporation plate for evaporating a non-metallic film layer, and the third evaporation opening is used to define a third evaporation area on the evaporation plate for evaporating a metal film layer;

[0028] The mask opening includes a first mask opening, a second mask opening and a third mask opening. The first mask opening is used to evaporate and form an optical film layer of the light-emitting element to be measured in the first evaporation area. The second mask opening is used to form different non-metallic film layers at different positions in the second evaporation area. The third mask opening is used to form two partially overlapping metal film layers in the third evaporation area.

[0029] In a possible implementation manner of the present application, in a direction along which the evaporation opening extends, a length of the first mask opening, a length of the third mask opening, and a length of the second mask opening decrease in sequence.

[0030] In a possible implementation manner of the present application, the length of the first mask opening is 19 mm to 22 mm, the length of the second mask opening is 4.7 mm to 5.2 mm, and the length of the third mask opening is 12 mm to 14 mm.

[0031] In a second aspect of the present application, there is further provided an auxiliary film thickness detection method, which is applied to the auxiliary film thickness detection device described in any one of the first aspects, and the method comprises:

[0032] Controlling the driving mechanism to move the first mask and the second mask to above the evaporation plate;

[0033] Different film layers are evaporated in the evaporation region by controlling the positional relationship between the mask opening and the evaporation opening.

[0034] In a possible implementation manner of the present application, the evaporation opening includes a first evaporation opening for defining a first evaporation area on the evaporation plate, the mask opening includes a first mask opening for evaporating a film layer in the first evaporation area, and the step of evaporating different film layers in the evaporation area by controlling the positional relationship between the mask opening and the evaporation opening includes:

[0035] Sequentially evaporating stacked film layers in the first evaporation region through the first mask opening to obtain a light-emitting material layer;

[0036] Controlling the driving mechanism to drive the second mask to move relative to the first mask, so that the first mask opening moves a first preset distance in the extension direction of the first evaporation opening, wherein the first preset distance is less than the length of the first mask opening in the extension direction of the first evaporation opening;

[0037] Depositing a metal film layer in the first deposition area through the first mask opening after position adjustment, wherein the metal film layer partially overlaps a side of the light-emitting material layer away from the deposition plate;

[0038] Preferably, the method further comprises:

[0039] The light-emitting performance of the light-emitting element is measured by forming a film layer in the first evaporation region.

[0040] In a possible implementation manner of the present application, the evaporation opening includes a second evaporation opening for defining a second evaporation area on the evaporation plate, the mask opening includes a second mask opening for forming different non-metallic film layers at different positions of the second evaporation area, and the step of evaporating different film layers in the evaporation area by controlling the positional relationship between the mask opening and the evaporation opening includes:

[0041] vapor-depositing a non-metallic film layer in the second vapor-deposition area through the second mask opening;

[0042] Controlling the driving mechanism to drive the second mask to move relative to the first mask, so that the second mask opening moves a second preset distance in the extension direction of the second evaporation opening, wherein the second preset distance is greater than or equal to three quarters of the length of the second mask opening in the extension direction of the second evaporation opening;

[0043] Repeat the above steps until all non-metallic film layers to be measured form film layers in the second evaporation region;

[0044] Preferably, the method further comprises:

[0045] The film thicknesses of different non-metallic film layers in the second evaporation region are measured respectively by using an ellipsometer.

[0046] In a possible implementation manner of the present application, the evaporation opening includes a third evaporation opening for defining a third evaporation area on the evaporation plate, the mask opening includes a third mask opening for forming a metal film layer in the third evaporation area, and the step of evaporating different film layers in the evaporation area by controlling the positional relationship between the mask opening and the evaporation opening includes:

[0047] vapor-depositing a first metal film layer in the third vapor-deposition area through the third mask opening;

[0048] Controlling the driving mechanism to drive the second mask to move relative to the first mask, so that the third mask opening moves a third preset distance in the extension direction of the third evaporation opening, wherein the third preset distance is less than the length of the third mask opening in the extension direction of the third evaporation opening;

[0049] vapor-depositing a second metal film layer in the third vapor-deposition region through the third mask opening whose position is adjusted, wherein the first metal film layer partially overlaps with the second metal film layer;

[0050] Preferably, the method further comprises:

[0051] Using an ellipsometer to measure the film thickness of the metal film layer and the film thickness of the second metal film layer respectively at a position where only the first metal film layer and the second metal film layer are distributed;

[0052] The resistance value and the transmittance of the metal film layer are measured at the overlapping position of the first metal film layer and the second metal film layer by using an ellipsometer.

[0053] The embodiments of the present application provide an auxiliary film thickness detection device and method, wherein a driving mechanism can drive a first mask plate and a second mask plate to move relative to an evaporation plate, so that when a film layer is evaporated in different evaporation chambers, an evaporated film layer can be formed at different positions of an evaporation area defined by an evaporation opening, so that different evaporated film layers are formed on one evaporation plate for subsequent film thickness measurement, thereby reducing the number of evaporation plates required and reducing the cost of monitoring the thickness of the evaporated film layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0054] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present application and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without paying creative work.

[0055] Figure 1 A schematic diagram of the structure of the auxiliary film thickness detection device provided in this embodiment;

[0056] Figure 2 for Figure 1 A schematic diagram of the structure of the first mask;

[0057] Figure 3 for Figure 1 A schematic diagram of the structure of the second mask;

[0058] Figure 4 for Figure 2 and Figure 3 A schematic diagram of a first mask and a second mask stacked together;

[0059] Figure 5 Another schematic diagram of the structure of the auxiliary film thickness detection device provided in this embodiment;

[0060] Figure 6 A top view of the auxiliary film thickness detection device provided in this embodiment;

[0061] Figure 7 for Figure 1 Another structural schematic diagram of the first mask;

[0062] Figure 8 for Figure 1 Another structural schematic diagram of the second mask;

[0063] Fig. 9 A schematic diagram of a flow chart of the auxiliary film thickness detection method provided in this embodiment;

[0064] Fig.10 for Fig. 9 One of the flowchart diagrams for implementing step S12;

[0065] Fig.11 for Fig.10 The corresponding process diagram;

[0066] Fig.12 for Fig. 9 The second flowchart diagram of implementing step S12;

[0067] Fig.13 for Fig.12 The corresponding process diagram;

[0068] Fig.14 for Fig. 9 The third flowchart diagram of implementing step S12;

[0069] Fig.15 for Fig.14 Corresponding process diagram.

[0070] Icons: 1- auxiliary film thickness detection device; 10- evaporation plate; 20- first mask; 201- evaporation opening; 2011- first evaporation opening; 2012- second evaporation opening; 2013- third evaporation opening; 30- second mask; 301- mask opening; 3011- first mask opening; 3012- second mask opening; 3013- third mask opening; 40- driving mechanism; 50- carrier; 110- luminescent material layer; 120- metal film layer; 1201- first metal film layer; 1202- second metal film layer; 130- non-metallic film layer. DETAILED DESCRIPTION

[0071] In order to make the purpose, technical solution and advantages of the embodiments of the present application clearer, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, rather than all the embodiments. The components of the embodiments of the present application described and shown in the drawings here can be arranged and designed in various different configurations.

[0072] In the description of the present application, it should be noted that the terms "upper", "lower", etc. indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, or are the orientations or positional relationships in which the product of the application is usually placed when in use. They are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present application.

[0073] According to different evaporation principles, the thickness of the evaporated film layer is generally monitored in the following two ways. Method 1: When using the mask evaporation method, the film is formed and the film thickness is monitored by opening holes on the mask (MASK). The film forming positions in different evaporation chambers are different, and it is necessary to open holes in different positions on the mask, that is, the same mask cannot be used in the film layers evaporated by different evaporation chambers. Method 2: When using the maskless evaporation method, although this solution can greatly save the cost of the mask, product development time, and increase the product layout rate compared to method 1, there is a problem in the display panel manufacturing process that the thickness of the evaporated film layer and the performance of the light-emitting element cannot be monitored. For this reason, in the related technology, a evaporated film layer is evaporated using a piece of plain glass and then the film thickness is measured to monitor the film thickness. The production cost of this solution is too high, and the performance of the light-emitting element cannot be monitored.

[0074] At the same time, with the development of display technology, in order to reduce the difficulty of the evaporation process of the light-emitting material, the second method is mainly used in the manufacturing process of the display panel. In detail, an isolation structure is set on the pixel definition layer between the pixel openings. When the light-emitting material layer and the second electrode layer are evaporated in the entire layer, the light-emitting material layer and the second electrode layer between the adjacent pixel openings can be disconnected at the position of the isolation structure. Through multiple evaporation and multiple etching processes, corresponding sub-pixel device film layers can be formed in the pixel openings corresponding to the sub-pixel devices of different colors. Patent PCT / CN2023 / 134518, Patent 202310759370.2, Patent 202310740412.8, Patent 202310707209.0 and Patent 202311346196.5 record the relevant technical solutions of the isolation structure for reference.

[0075] In order to solve the above problems, the inventor innovatively designed the following technical solution, and the specific implementation scheme of the present application will be described in detail below in conjunction with the accompanying drawings. It should be noted that the defects existing in the above solutions in the prior art are the results obtained by the inventor after practice and careful research. Therefore, the discovery process of the above technical problems and the solutions proposed in this embodiment below for the above problems should all be the contributions made by the inventor to the present application in the process of invention and creation, and should not be understood as the technical content known to those skilled in the art.

[0076] Please refer to Figure 1-Figure 4 , Figure 1 The schematic diagram of the structure of the auxiliary film thickness detection device provided in this embodiment is illustrated. Figure 2 The schematic diagram of the structure of the first mask is illustrated. Figure 3 The schematic diagram of the structure of the second mask is illustrated. Figure 4 The schematic diagram of the first mask and the second mask overlapping is illustrated. The auxiliary film thickness detection device 1 includes an evaporation plate 10, a first mask 20, a second mask 30 and a driving mechanism 40. The evaporation plate 10 is used to carry the evaporated film layer. The first mask 20 is provided with an evaporation opening 201 for defining an evaporation area on the evaporation plate 10. The second mask 30 is provided with a mask opening 301 for defining an evaporation range in the evaporation area. In this embodiment, the shapes of the evaporation opening 201 and the mask opening 301 can both be rectangular.

[0077] In this embodiment, the driving mechanism 40 is connected to the first mask 20 and the second mask 30 respectively, and the driving mechanism 40 can drive the first mask 20 and the second mask 30 to move as a whole, so as to adjust the positional relationship between the first mask 20 and the second mask 30 and the evaporation plate 10, so as to evaporate different film layers at different positions of the evaporation plate 10. The driving mechanism 40 can also drive the second mask 30 to move relative to the first mask 20, so that the mask opening 301 on the second mask 30 is relative to the first mask 20 in the extension direction of the evaporation opening 201 ( Figure 4 The film moves in the direction of the middle arrow (in the direction of the middle arrow), thereby obtaining evaporation positions corresponding to multiple mask openings 301 in the evaporation area.

[0078] The above structure can form evaporated film layers at different positions of the evaporation area defined by the evaporation opening 201 when evaporating film layers in different evaporation chambers, so that different evaporated film layers can be formed on one evaporation plate 10 for subsequent film thickness measurement, thereby reducing the number of required evaporation plates 10 and reducing the cost of monitoring the thickness of the evaporated film layers.

[0079] In this embodiment, the first mask 20 and the second mask 30 are arranged parallel to each other, and the mask opening 301 is used to limit the evaporation range within the evaporation area each time.

[0080] Furthermore, the driving mechanism 40 is also used to drive the second mask 30 to move relative to the first mask 20 , so that the mask opening 301 on the second mask 30 moves relative to the first mask 20 in the extension direction of the evaporation opening 201 .

[0081] For further information, please refer to Figure 5 In order to provide effective support for the evaporation plate 10, in this embodiment, the auxiliary film thickness detection device 1 further includes a carrier 50. The evaporation plate 10 is disposed on one side of the carrier 50, the first mask 20 is located on the side of the evaporation plate 10 away from the carrier 50, and the second mask 30 is located on the side of the first mask 20 away from the carrier 50, that is, the first mask 20 is located between the evaporation plate 10 and the second mask 30. In this embodiment, the evaporation plate 10 is parallel to the first mask 20 and the second mask 30.

[0082] In this embodiment, the distance between the first mask 20 and the second mask 30 is 0.2mm to 0.4mm. By way of example, the distance between the first mask 20 and the second mask 30 includes 0.2mm, 0.21mm, 0.235mm, 0.264mm, 0.285mm, 0.3mm, 0.312mm, 0.335mm, 0.356mm, 0.381mm and 0.4mm, etc.

[0083] Furthermore, in order to achieve the position adjustment of the first mask 20 and the second mask 30 by the driving mechanism 40, the driving mechanism 40 includes a first driving mechanism, a second driving mechanism and a third driving mechanism, wherein the first driving mechanism, the second driving mechanism and the third driving mechanism can be implemented by a driving motor. Figure 5 The driving output shaft of the first driving mechanism is connected to the first mask 20 and the second mask 30, driving the first mask 20 and the second mask 30 as a whole to approach or move away from the evaporation plate 10 from a first direction parallel to the plane where the evaporation plate is located (the X direction in the figure). The driving output shaft of the second driving mechanism is connected to the first mask 20 and the second mask 30, driving the first mask 20 and the second mask 30 as a whole to approach or move away from the evaporation plate 10 from a second direction perpendicular to the plane where the evaporation plate is located (the Y direction in the figure). Please refer to Figure 6 , the driving output shaft of the third driving mechanism is connected to the second mask 30, driving the second mask 30 to move relative to the first mask 20. Exemplarily, the third driving mechanism drives the second mask 30 to move relative to the first mask 20, so that the mask opening 301 moves relative to the third direction (Z direction in the figure) extending from the evaporation opening 201. In this embodiment, the first direction, the second direction and the third direction can be perpendicular to each other. Through the above arrangement, before the film layer is evaporated, the first and second mask plates can be adjusted to the top of the evaporation plate 10 by the first driving mechanism and the second driving mechanism to prepare for the evaporation of the film layer. When the film layer is evaporated, the position of the mask opening 301 in the evaporation area is adjusted in different evaporation chambers by the third driving mechanism, so that different evaporated film layers can be obtained at different positions in the evaporation area.

[0084] In this embodiment, the opening size of the evaporation opening 201 is larger than the opening size of the mask opening. Figure 6 As shown, in the first direction (X direction in the figure), the opening size a1 of the evaporation opening 201 is larger than the opening size a2 of the mask opening 301, and in the third direction (Z direction in the figure), the opening size b1 of the evaporation opening 201 is larger than the opening size b2 of the mask opening 301. The orthographic projection of the mask opening 301 on the first mask 20 is located within the evaporation opening 201, and such a design can ensure that the film layer formed by evaporation through the mask opening 301 can be located within the evaporation area defined by the evaporation opening 201.

[0085] In this embodiment, the evaporation plate 10 may be a glass substrate, the carrier plate 50 may be a glass carrier plate, and the first mask plate 20 and the second mask plate 30 may be metal masks made of metal with small deformation.

[0086] Further, in this embodiment, please refer to Figure 7The evaporation opening 201 includes a first evaporation opening 2011, a second evaporation opening 2012 and a third evaporation opening 2013. The first evaporation opening 2011 is used to define a first evaporation area for evaporating an optical film layer on the evaporation plate 10, the second evaporation opening 2012 is used to define a second evaporation area for evaporating a non-metallic film layer on the evaporation plate, and the third evaporation opening 2013 is used to define a third evaporation area for evaporating a metal film layer on the evaporation plate. Please refer to Figure 8 The mask opening 301 includes a first mask opening 3011, a second mask opening 3012 and a third mask opening 3013. The first mask opening 3011 is used to evaporate and form an optical film layer of the light-emitting element to be measured in the first evaporation area. The second mask opening 3012 is used to form different non-metallic film layers at different positions in the second evaporation area. The third mask opening 3013 is used to form two partially overlapping metal film layers in the third evaporation area.

[0087] The optical film layer evaporated in the first evaporation area includes a luminescent material layer and a metal film layer, wherein the luminescent material layer includes a hole injection layer (HIL, Hole Injection Layer), a hole transport layer (HTL, Hole Tranport Layer), a luminescent layer (EML, Emission layer), a hole blocking layer (HBL, Hole Block Layer), an electron transport layer (ETL, Electron Transport Layer) and an electron injection layer (EIL, Electron Injection Layer) stacked in sequence, and the metal film layer is used as the cathode of the light-emitting element, and the metal film layer can be at least partially overlapped on the side of the electron injection layer away from the evaporation plate 10. In this embodiment, a pixel circuit for driving the light-emitting element to emit light and an anode connected to the pixel circuit can be pre-made in the first evaporation area of ​​the evaporation plate 10, and the luminescent material layer is evaporated on the anode. When it is necessary to test the optical performance of the light-emitting element, it is only necessary to provide electrical signals to the anode and the cathode to perform the test. This solves the technical problem that the optical performance of the light-emitting element cannot be tested in the related art.

[0088] The non-metallic film layer evaporated in the second evaporation area includes all non-metallic film layers that need to be produced by the evaporation process in the display panel production process, including but not limited to the hole injection layer, hole transport layer, light-emitting layer, hole blocking layer, electron transport layer and electron injection layer described above. For example, the non-metallic film layer may also include an inorganic encapsulation layer and an organic encapsulation layer. By forming different non-metallic film layers at different positions in the second evaporation area, it can be ensured that each non-metallic film layer can form a single film layer structure in the second evaporation area, so that the film thickness of the non-metallic film layer at the position of the single film layer structure can be measured by an ellipsometer in the subsequent process. In order to solve the technical problem in the related art that the ellipsometer cannot measure the film thickness of each film layer in the overlapping film layer and needs to form the film layer separately on different carrier plates, resulting in waste of the carrier plate (such as plain glass) and high production cost.

[0089] In order to reduce the resistance of the metal film layer, the metal film layer is generally evaporated with multiple layers. For example, in the manufacturing process of the display panel, the metal film layer generally includes two metal film layers formed by successive evaporation from two metal evaporation sources, wherein the materials of the two metal film layers may be the same or different. Preferably, the materials of the two metal film layers are the same. In this embodiment, the metal film layer evaporated in the third evaporation range includes a partially overlapping first metal film layer and a second metal film layer, and the first metal film layer and the second metal film layer are evaporated from different metal evaporation sources. The film thickness of the first metal film layer can be obtained by testing a single-layer first metal film layer with an ellipsometer, the film thickness of the second metal film layer can be obtained by testing a single-layer second metal film layer with an ellipsometer, and the resistance value of the metal film layer and the transmittance of the metal film layer can be measured by measuring at the overlapping position of the first metal film layer and the second metal film layer with an ellipsometer.

[0090] In this embodiment, the first evaporation opening, the second evaporation opening and the third evaporation opening have the same extension direction. For example, the first evaporation opening, the second evaporation opening and the third evaporation opening all extend along a third direction (Z direction in the figure). With such a design, the second mask 30 can be controlled to move in the third direction relative to the first mask 20, so that a vapor deposition film layer can be formed at different positions in different evaporation areas.

[0091] In this embodiment, in the third direction (Z direction in the figure), the length of the first mask opening, the length of the third mask opening and the length of the second mask opening decrease in sequence. The length of the first mask opening is 19 mm to 22 mm, the length of the second mask opening is 4.7 mm to 5.2 mm, and the length of the third mask opening is 12 mm to 14 mm. Exemplarily, the length of the first mask opening includes 19mm, 19.2mm, 19.56mm, 19.83mm, 20.12mm, 20.46mm, 20.87mm, 21.23mm, 21.56mm and 22mm, the length of the second mask opening includes 4.7mm, 4.75um, 4.83um, 4.89um, 4.92um, 4.95um, 5.02um, 5.08um, 5.13um and 5.2um, and the length of the third mask opening includes 12um, 12.24um, 12.57um, 12.81um, 13.04um, 13.46um, 13.58um, 13.89um and 14um, etc.

[0092] The auxiliary film thickness detection device provided above can form different evaporated film layers at different positions of the evaporation plate, so as to realize the measurement of different evaporated film layer thicknesses on one evaporation plate. In addition, the optical performance of the light-emitting element of the luminescent film layer evaporated on the evaporation plate can be tested, and the resistance and transmittance of the metal film layer evaporated on the evaporation plate can be tested.

[0093] Based on the same inventive concept, this embodiment also provides an auxiliary film thickness detection method, which can be applied to the auxiliary film thickness detection device 1 described above. Fig. 9 , Fig. 9 The flowchart of the auxiliary film thickness detection method provided in the present embodiment is illustrated. The auxiliary film thickness detection method provided in the present embodiment is described in detail below with reference to the accompanying drawings.

[0094] Step S11, controlling the driving mechanism to move the first mask and the second mask to above the evaporation plate.

[0095] In this step, the first mask and the second mask can be adjusted to above the evaporation plate by a driving mechanism to prepare for the evaporation of the film layer.

[0096] Step S12, vapor-depositing different film layers in the vapor-deposition area by controlling the positional relationship between the mask opening and the vapor-deposition opening.

[0097] In one implementation of this embodiment, the evaporation opening includes a first evaporation opening for defining a first evaporation region on the evaporation plate, and the mask opening includes a first mask opening for evaporating a film layer in the first evaporation region. Fig.10 and Fig.11, step S12 can be implemented in the following way.

[0098] Step S121 : the first mask opening 3011 is used to sequentially deposit stacked film layers in a first deposition area to obtain a light-emitting material layer 110 .

[0099] Among them, the light-emitting material layer 110 may include a stacked hole injection layer, a hole transport layer, a light-emitting layer, a hole blocking layer, an electron transport layer and an electron injection layer. In this step, the second mask 30 is not moved, so that the above-mentioned film layers are stacked together in sequence when the above-mentioned film layers are evaporated.

[0100] Step S122 , controlling the driving mechanism to drive the first mask opening 3011 to move in the extension direction of the first evaporation opening (in the direction of the arrow in the figure) by a first preset distance d1 .

[0101] The first preset distance d1 is smaller than a length b21 of the first mask opening 3011 in the extending direction of the first evaporation opening.

[0102] Step S123 , vapor-depositing the metal film layer 120 in the first vapor-deposition area through the first mask opening whose position has been adjusted.

[0103] The metal film layer 120 is partially overlapped on the side of the luminescent material layer 110 away from the evaporation plate 10. A pixel circuit for driving the luminescent element to emit light and an anode connected to the pixel circuit can be prefabricated in the first evaporation area of ​​the evaporation plate 10, and the luminescent material layer 110 is evaporated on the anode.

[0104] Furthermore, the auxiliary film thickness detection method provided in this embodiment also includes a step of measuring the luminescent performance of the light-emitting element by manufacturing a film layer in the first evaporation area. In this step, the luminescent performance test of the light-emitting element can be achieved by simply providing a test electrical signal to the anode and the cathode.

[0105] In another implementation of this embodiment, the evaporation opening includes a second evaporation opening for defining a second evaporation area on the evaporation plate 10, and the mask opening includes a second mask opening for forming different non-metallic film layers at different positions of the second evaporation area. Fig.12 and Fig.13 , step S12 can be implemented in the following way.

[0106] Step S124 , vapor-depositing a non-metallic film layer 130 in the second vapor-deposition region through the second mask opening 3012 .

[0107] Step S125 , detecting whether all the non-metallic film layers 130 to be evaporated have been evaporated.

[0108] If it is detected that the non-metallic film layer 130 to be evaporated has been completely evaporated, the process ends; if it is detected that the non-metallic film layer 130 to be evaporated has not been completely evaporated, the process goes to step S126.

[0109] Step S126 , controlling the driving mechanism to drive the second mask opening 3012 to move a second preset distance d2 in the extension direction of the second evaporation opening (the direction of the arrow in the figure).

[0110] In this step, the second preset distance d2 is greater than or equal to three quarters of the length b22 of the second mask opening 3012 in the extension direction of the second evaporation opening.

[0111] After completing step S126 , the process returns to step S124 until all non-metallic film layers 130 to be measured form film layers in the second evaporation region.

[0112] Furthermore, the auxiliary film thickness detection method provided in this embodiment also includes using an ellipsometer to measure the film thickness of different non-metallic film layers 130 in the second evaporation region. In detail, the ellipsometer is used to measure the single film layer position of the non-metallic film layer 130 in turn to obtain the film thickness of each non-metallic film layer 130.

[0113] In another implementation of this embodiment, the evaporation opening includes a third evaporation opening for defining a third evaporation region on the evaporation plate, and the mask opening includes a third mask opening for forming a metal film layer in the third evaporation region. Fig.14 and Fig.15 , step S12 can be implemented in the following way.

[0114] Step S127 , evaporating the first metal film layer 1201 in the third evaporation region through the third mask opening 3013 .

[0115] In order to reduce the resistance of the metal film layer, the metal film layer 120 is generally evaporated with multiple layers. For example, in the manufacturing process of the display panel, the cathode generally includes a first metal film layer 1201 and a second metal film layer 1202 formed by sequential evaporation from two metal evaporation sources.

[0116] Step S128 , controlling the driving mechanism to drive the third mask opening 3013 to move a third preset distance d3 in the extension direction of the third evaporation opening (the direction of the arrow in the figure).

[0117] In this step, the third preset distance d3 is smaller than a length b23 of the third mask opening in the extending direction (the direction of the arrow in the figure) of the third evaporation opening.

[0118] Step S129 , vapor-depositing the second metal film layer 1202 in the third vapor-deposition area through the third mask opening 3013 after the position adjustment.

[0119] In this embodiment, the first metal film layer 1201 and the second metal film layer 1202 partially overlap.

[0120] Furthermore, the auxiliary film thickness detection method provided in this embodiment also includes using an ellipsometer to respectively measure the film thickness of the first metal film layer 1201 and the film thickness of the second metal film layer 1202 at a position where only the first metal film layer 1201 and the second metal film layer 1202 are distributed; using an ellipsometer to measure the metal film layer resistance and the metal film layer transmittance at the overlapping position of the first metal film layer 1201 and the second metal film layer 1202.

[0121] It can be understood that in this embodiment, the film layers required for the three tests of luminescence performance test, non-metallic film layer film thickness test and metal film layer test can be realized by multiple complete film layer evaporation processes, wherein one complete film layer evaporation process includes the film layer evaporation steps corresponding to evaporating all non-metallic film layers (luminescent material layers) and all metal film layers (cathode layers). Exemplarily, the film layers required for the luminescence performance test can be produced by one complete film layer evaporation process, and the film layers required for the non-metallic film layer film thickness test and the metal film layer test can be produced by one complete film layer evaporation process or by different complete film layer evaporation processes.

[0122] The auxiliary film thickness detection method provided above can form different evaporated film layers at different positions of the same evaporation plate to facilitate the measurement of the thickness of different evaporated film layers. It can also test the optical properties of the light-emitting elements of the luminescent film layer evaporated on the evaporation plate, and test the resistance and transmittance of the metal film layer evaporated on the evaporation plate.

[0123] To summarize, the auxiliary film thickness detection device and method provided in the present embodiment, the driving mechanism can drive the mask opening on the second mask plate to move relative to the first mask plate in the extension direction of the evaporation opening, so that when the film layer is evaporated in different evaporation chambers, the evaporated film layer can be formed at different positions of the evaporation area defined by the evaporation opening, so that different evaporated film layers are formed on one evaporation plate for subsequent film thickness measurement, thereby reducing the number of evaporation plates required and reducing the cost of monitoring the thickness of the evaporated film layer.

[0124] The above description is only the preferred embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application shall be included in the protection scope of the present application.

Claims

1. An auxiliary film thickness detection device, characterized in that: The device comprises: An evaporation plate, the evaporation plate is used for evaporating a film layer; A first mask and a second mask, wherein the first mask is provided with a vapor deposition opening for defining a vapor deposition area on the vapor deposition plate, and the second mask is provided with a mask opening for defining a vapor deposition range in the vapor deposition area; A driving mechanism is connected to the first mask and the second mask respectively, and is used to drive the first mask and the second mask to move relative to the evaporation plate.

2. The auxiliary film thickness detection device according to claim 1, characterized in that: The first mask and the second mask are arranged in parallel; Preferably, the mask opening is used to limit the evaporation range within the evaporation area each time.

3. The auxiliary film thickness detection device according to claim 1, characterized in that: The driving mechanism is further used to drive the second mask to move relative to the first mask, so that the mask opening on the second mask moves relative to the first mask in the extension direction of the evaporation opening.

4. The auxiliary film thickness detection device according to claim 1, characterized in that: The device further comprises: a carrier; The evaporation plate is arranged on one side of the carrier; The first mask is located on a side of the evaporation plate away from the carrier; The second mask is located on a side of the first mask away from the carrier.

5. The auxiliary film thickness detection device according to claim 1, characterized in that: The distance between the first mask and the second mask is 0.2 mm to 0.4 mm.

6. The auxiliary film thickness detection device according to claim 1, characterized in that: The driving mechanism includes a first driving mechanism, a second driving mechanism and a third driving mechanism; The first driving mechanism is used to drive the first mask and the second mask to approach or move away from the evaporation plate from a first direction parallel to the plane where the evaporation plate is located; The second driving mechanism is used to drive the first mask and the second mask to approach or move away from the evaporation plate from a second direction perpendicular to the plane where the evaporation plate is located; The third driving mechanism is used to drive the second mask to move relative to the first mask, so that the mask opening moves along the third direction in which the evaporation opening extends; Preferably, the first direction, the second direction and the third direction are perpendicular to each other.

7. The auxiliary film thickness detection device according to claim 1, characterized in that: The opening size of the evaporation opening is larger than the opening size of the mask opening; The orthographic projection of the mask opening on the first mask is located within the evaporation opening.

8. The auxiliary film thickness detection device according to claim 1, characterized in that: The evaporation plate is a glass substrate; Preferably, the first mask and the second mask are metal masks.

9. The auxiliary film thickness detection device according to any one of claims 1 to 8, characterized in that: The evaporation openings include a first evaporation opening, a second evaporation opening, and a third evaporation opening; The first evaporation opening is used to define a first evaporation area on the evaporation plate for evaporating an optical film layer, the second evaporation opening is used to define a second evaporation area on the evaporation plate for evaporating a non-metallic film layer, and the third evaporation opening is used to define a third evaporation area on the evaporation plate for evaporating a metal film layer; The mask opening includes a first mask opening, a second mask opening and a third mask opening. The first mask opening is used to limit the formation of an optical film layer of the light-emitting element to be measured in the first evaporation area, the second mask opening is used to limit the formation of different non-metallic film layers at different positions in the second evaporation area, and the third mask opening is used to limit the formation of two partially overlapping metal film layers in the third evaporation area.

10. The auxiliary film thickness detection device according to claim 9, characterized in that: Along the extending direction of the evaporation opening, the length of the first mask opening, the length of the third mask opening and the length of the second mask opening decrease in sequence.

11. The auxiliary film thickness detection device according to claim 10, characterized in that: The length of the first mask opening is 19 mm to 22 mm, the length of the second mask opening is 4.7 mm to 5.2 mm, and the length of the third mask opening is 12 mm to 14 mm.

12. An auxiliary film thickness detection method, characterized in that: The auxiliary film thickness detection device according to any one of claims 1 to 11, wherein the method comprises: Controlling the driving mechanism to move the first mask and the second mask to above the evaporation plate; Different film layers are evaporated in the evaporation region by controlling the positional relationship between the mask opening and the evaporation opening.

13. The auxiliary film thickness detection method according to claim 12, characterized in that: The evaporation opening includes a first evaporation opening for defining a first evaporation area on the evaporation plate, the mask opening includes a first mask opening for evaporating a film layer in the first evaporation area, and the step of evaporating different film layers in the evaporation area by controlling the positional relationship between the mask opening and the evaporation opening includes: Sequentially evaporating stacked film layers in the first evaporation region through the first mask opening to obtain a light-emitting material layer; Controlling the driving mechanism to drive the second mask to move relative to the first mask, so that the first mask opening moves a first preset distance in the extension direction of the first evaporation opening, wherein the first preset distance is less than the length of the first mask opening in the extension direction of the first evaporation opening; Depositing a metal film layer in the first deposition area through the first mask opening after position adjustment, wherein the metal film layer partially overlaps a side of the light-emitting material layer away from the deposition plate; Preferably, the method further comprises: The light-emitting performance of the light-emitting element is measured by forming a film layer in the first evaporation region.

14. The auxiliary film thickness detection method according to claim 12, characterized in that: The evaporation opening includes a second evaporation opening for defining a second evaporation area on the evaporation plate, the mask opening includes a second mask opening for forming different non-metallic film layers at different positions of the second evaporation area, and the step of evaporating different film layers in the evaporation area by controlling the positional relationship between the mask opening and the evaporation opening includes: vapor-depositing a non-metallic film layer in the second vapor-deposition area through the second mask opening; Controlling the driving mechanism to drive the second mask to move relative to the first mask, so that the second mask opening moves a second preset distance in the extension direction of the second evaporation opening, wherein the second preset distance is greater than or equal to three quarters of the length of the second mask opening in the extension direction of the second evaporation opening; Repeat the above steps until all non-metallic film layers to be measured form film layers in the second evaporation region; Preferably, the method further comprises: The film thicknesses of different non-metallic film layers in the second evaporation region are measured respectively by using an ellipsometer.

15. The auxiliary film thickness detection method according to claim 12, characterized in that: The evaporation opening includes a third evaporation opening for defining a third evaporation area on the evaporation plate, the mask opening includes a third mask opening for forming a metal film layer in the third evaporation area, and the step of evaporating different film layers in the evaporation area by controlling the positional relationship between the mask opening and the evaporation opening includes: vapor-depositing a first metal film layer in the third vapor-deposition area through the third mask opening; Controlling the driving mechanism to drive the second mask to move relative to the first mask, so that the third mask opening moves a third preset distance in the extension direction of the third evaporation opening, wherein the third preset distance is less than the length of the third mask opening in the extension direction of the third evaporation opening; vapor-depositing a second metal film layer in the third vapor-deposition region through the third mask opening whose position is adjusted, wherein the first metal film layer partially overlaps with the second metal film layer; Preferably, the method further comprises: Using an ellipsometer to measure the film thickness of the metal film layer and the film thickness of the second metal film layer respectively at a position where only the first metal film layer and the second metal film layer are distributed; The resistance value and the transmittance of the metal film layer are measured at the overlapping position of the first metal film layer and the second metal film layer by using an ellipsometer.