Heat treatment line for hot-rolled strips
By using inductor heating and reducing protective gas cooling in an annealing furnace, non-oxidation heat treatment and continuous pickling are achieved, solving the problem of oxidation scale formation during the annealing of steel strips, improving yield and magnetic characteristics, and reducing the Environmental pollution.
Patent Information
- Application Number
- CN202380033145.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-06-23
- Filing Date
- 2023-04-06
- Publication Date
- 2024-11-22
AI Technical Summary
In the prior art, steel strips are prone to forming oxide scales during the annealing process, resulting in damage to magnetic properties, and the heating method of the annealing equipment relies on fossil fuel, resulting in high CO2 emissions and high cost of scale removal.
Using an airtight sealed annealing furnace, multiple consecutive inductors are used for heating, and reducing protective gas is introduced into the cooling section for cooling, realizing oxidation-free heat treatment and continuous pickling, avoiding the formation of oxide scales and traditional heating. Use of the device.
It significantly shortens heating time, improves yield, reduces surface roughness, improves magnetic properties, and avoids CO2 emissions and the use of open cooling water.
Smart Images

Figure CN119013524A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to an annealing plant, in particular an annealing furnace, for non-oxidative heat treatment of hot-rolled steel strips arranged for the production of electrical strips and / or stainless steel strips; a treatment line for continuous pickling and non-oxidative annealing of hot-rolled steel strips; and a method for continuous pickling and non-oxidative annealing of hot-rolled steel strips. Background Art
[0002] Electrical tape is one of the most important soft magnetic materials for magnetic cores and usually consists of an iron-silicon alloy. Electrical tape is currently classified into two different electrical tape grades. So-called non-grain-oriented electrical tape is uniformly magnetized in all directions and is mainly used in rotating electrical machines. In contrast, so-called grain-oriented electrical tape has a preferred magnetization direction and is generally used in power transformers, distribution transformers and smaller transformers of higher quality.
[0003] The electrical strips disclosed in patent document US2017 / 0283903 A1 are usually produced as follows: a specific metal steel composition (in weight percentage) which usually has 2.5% to 4.0% Si, 0.010% to 0.100% C, up to 0.150% Mn, up to 0.065% Al and up to 0.0150% N, and optionally 0.010% to 0.3% Cu, up to 0.060% S, up to 0.100% P, up to 0.2% As, Sn, Sb, Te and Bi, the remainder being iron and unavoidable impurities, is cast into a preformed material, such as a slab, a thin slab or a cast strip, and is directly hot-rolled into a so-called hot-rolled strip. The hot-rolled steel strip is then annealed and cold-rolled in a further step into a so-called cold-rolled strip. In order to obtain favorable magnetic properties, the cold-rolled strip is subsequently recrystallization-annealed in a continuous annealing and coating line and subsequently coated with an insulating coating.
[0004] For the annealing of hot-rolled steel strips, the presence of an oxide scale layer on the surface is usually tolerable, since further oxidation and thus further oxide scale formation (so-called annealing scale) in an open heated annealing furnace cannot be avoided. Therefore, in the prior art, the hot-rolled steel strips are first subjected to an annealing treatment and then to a descaling process in order to provide a scale-free hot-rolled strip for the subsequent cold rolling process. The combination of annealing and pickling is known as a so-called annealing pickling line. According to English usage, such a line is also referred to as a so-called "APL" (Annealing Pickling Line).
[0005] The descaling process first involves mechanical preliminary descaling, which is then supplemented by a chemical pickling process. Mechanical descaling is usually carried out with the aid of sandblasting equipment, which roughens the surface of the hot-rolled strip so that the resulting roughness is largely retained after cold rolling, thereby impairing the magnetic properties of the grain-oriented electrical strip or non-grain-oriented electrical strip.
[0006] Annealing furnaces known in the prior art include a heating section and a heat-insulating section and a cooling section connected thereto, the cooling section including an air cooling section and a water cooling section. In the heating section, the hot-rolled strip is heated in an open manner by a gas burner using fossil fuels, whereby CO2 emissions are high. Such annealing equipment is known, for example, from patent document US 5 472 528, which also teaches the use of an induction device arranged upstream or downstream of at least one conventional heating device in order to improve the inertia of the conventional heating method. The hot-rolled strip is then electrically heated in a nitrogen atmosphere in the holding section. In the subsequent air cooling section, the hot-rolled strip first undergoes slow cooling and then undergoes more intense water cooling. During the slow cooling period, the hot-rolled strip is further oxidized. The scale particles formed here are discharged along with the exhausted air, so a great cost must be invested for filtering. Additional scale is also produced during more intense water cooling, which must be removed from the cooling water, usually by a scale sedimentation tank.
[0007] Therefore, the industry still hopes to improve such methods. Summary of the invention
[0008] Against this background, the object of the present invention is to provide a device for the oxidation-free heat treatment of hot-rolled steel strips provided for the production of electrical strips and / or stainless steel strips, which improves the process compared to the prior art.
[0009] Furthermore, the object of the present invention is to provide a method for the continuous pickling and oxidation-free annealing of hot-rolled steel strips which is provided for the production of electrical strips and / or stainless steel strips which is improved compared to the prior art.
[0010] According to the invention, this object is achieved by an annealing device, in particular an annealing furnace, for non-oxidative heat treatment of hot-rolled steel strip having the features of claim 1, and also by a treatment line for continuous pickling and non-oxidative annealing of hot-rolled steel strip having the features of claim 9, and by a method for continuous pickling and non-oxidative annealing of hot-rolled steel strip having the features of claim 10.
[0011] According to the invention, an annealing device, in particular an annealing furnace, for non-oxidative heat treatment of hot-rolled steel strips configured for the production of electrical strips and / or stainless steel strips comprises a hermetically sealed furnace chamber having a heating section, optionally a holding section connected to the heating section, and a cooling section connected to the heating section or the holding section, wherein the heating section has a plurality of inductors connected in series, and wherein the cooling section comprises a cooling device, by means of which a reducing protective gas for cooling the hot-rolled steel strip can be introduced into the cooling section.
[0012] According to the present invention, a processing line for continuously pickling and non-oxidation annealing of hot-rolled steel strips configured to produce electrical strips and / or stainless steel strips comprises a pretreatment device in which the hot-rolled steel strips can be pickled, and the processing line also comprises an annealing device according to the present invention arranged after the pretreatment device in the strip conveying direction.
[0013] According to the method according to the invention for the continuous pickling and oxidation-free annealing of a hot-rolled steel strip which is provided for the production of electrical strip and / or stainless steel strip, the hot-rolled steel strip is firstly fed to a pretreatment device after an unwinding step, and pickled in the pretreatment device; then it is fed as a pickled steel strip to an annealing device and firstly inductively heated to an annealing temperature by means of a plurality of inductors connected in series under a reducing protective gas atmosphere, then annealed, and subsequently quenched and / or cooled using a reducing protective gas.
[0014] As steel strip for producing electrical strips, preference is given to using steels which (in percentage by weight) typically have 2.5% to 4.0% Si, 0.010% to 0.100% C, up to 0.150% Mn, up to 0.065% Al and up to 0.0150% N, and optionally respectively 0.010% to 0.3% Cu, up to 0.060% S, up to 0.100% P, up to respectively 0.2% As, Sn, Sb, Te and Bi, the remainder being iron and unavoidable impurities.
[0015] The annealing plant according to the invention allows a complete heat treatment in a reducing protective gas atmosphere, which has a reducing effect on the hot-rolled strip used, thereby enabling an oxidation-free steel strip surface. Very high power densities can be achieved by means of inductors, whereby the heating section can be significantly shortened compared to annealing furnaces known from the prior art. Therefore, conventional gas burners or radiant heating elements are not provided. This also enables the annealing plant to be operated economically in a reducing protective gas atmosphere. In addition, reducing protective gases (e.g. hydrogen) have an improved convective heat transfer compared to atmospheric air, whereby higher cooling rates, for example up to 50 K / s, can be achieved in the cooling section. This contributes to a shorter structural length of the annealing plant according to the invention, for example for non-grain-oriented electrical strips, or is particularly advantageous for quality reasons, for example in order to achieve quenching of grain-oriented electrical strips or stainless steel.
[0016] In this respect, the annealing plant according to the invention allows a pickling treatment to be carried out before the heat treatment, which has a particularly advantageous effect on the heat treatment process of the hot-rolled strip, since it is not necessary to use scale breakers and / or sandblasting equipment. The pickling time can thus be shortened and the output can thus be increased. In addition, the surface roughness can be reduced, thereby improving the magnetic properties of the electrical strip.
[0017] Other advantages of the present invention are:
[0018] a) Avoid CO2 emissions;
[0019] b) non-oxidative heat treatment;
[0020] c) The structural length of the annealing equipment is shorter;
[0021] d) Avoid open cooling water;
[0022] e) Reduce dust emissions.
[0023] Further advantageous embodiments of the invention are given in the dependent claims. The features listed individually in the dependent claims can be combined with one another in a technically meaningful manner and can define further embodiments of the invention. In addition, the features given in the claims are presented and explained in detail in the description, wherein further preferred embodiments of the invention are presented.
[0024] It should be noted here that the annealing plant according to the invention is neither designed nor suitable for use in a hot strip galvanizing system (also known as a pickling and galvanising line (PGL)).
[0025] Advantageously, it is provided in this respect that the annealing device is designed as a horizontal structural type. In addition, it is preferably provided that the cooling section and / or the outlet door of the annealing device do not lead to the coating device.
[0026] In an advantageous embodiment variant of the method, the pickled steel strip is first heated in a heating section of an annealing plant at a heating rate of at least 20 K / s, more preferably at a heating rate of at least 25 K / s, even more preferably at a heating rate of at least 30 K / s to an annealing temperature of at least 800° C. However, the heating rate should not exceed a maximum value of 60 K / s, more preferably 55 K / s, most preferably 50 K / s.
[0027] It is advantageously provided that the pickled and thus completely scale-free steel strip is heated in the heating section via two separate stages. For this purpose, the annealing device preferably comprises a first stage with a plurality of longitudinal field inductors connected in series, in which the pickled steel strip is first heated to a temperature of at least 650° C. On the other hand, the annealing device has a plurality of transverse field inductors connected in series in the second stage, by means of which the steel strip is heated to an annealing temperature of at least 800° C.
[0028] In an annealing system, the respective number of inductors which can be used to achieve a heating rate of up to 100 K / (s*mm strip thickness) is dependent on the required total power and can therefore vary between 1 and 20.
[0029] To ensure good magnetic field coupling, the running gap for the steel strip should not be too large. Therefore, in the heating section, the running gap advantageously has a vertical extension of less than or equal to 300 mm, more preferably less than or equal to 250 mm, and most preferably less than or equal to 200 mm.
[0030] In order to keep the heat losses in the heating section as low as possible, it is provided in a further advantageous embodiment variant that the passage gap is delimited by thermal insulation layers which are arranged below and above the steel strip running plane and are provided with a gas-impermeable coating on the outside.
[0031] If the hot rolled steel strip is also provided for producing grain-oriented electrical strip and non-grain-oriented electrical strip, the hot rolled steel strip is preferably annealed in a holding section connected to the heating section at a temperature in the range of 800-1200° C. for at least 60 seconds.
[0032] Therefore, in a preferred embodiment variant, the annealing device may have a holding section, which particularly preferably includes three separate holding section levels. The first holding section level is directly connected to the heating section, wherein the second holding section level is directly connected upstream of the cooling section. On the one hand, both holding section levels include conventional electric heating elements, which can be arranged below the plane of travel of the steel strip. In addition, the two holding section levels include conventional cooling nozzles through which air flows, which cooling nozzles can be arranged, for example, above the plane of travel of the steel strip. The third holding section level is arranged between the first holding section level and the second holding section level in the holding section, and unlike these holding section levels, does not have a cooling nozzle, but only has an electric heating element.
[0033] After the annealing treatment, the steel strip is quenched and / or cooled using a reducing protective gas. In an advantageous embodiment variant of the method, the annealed steel strip can be cooled in a cooling section of the annealing device directly connected to the heating section at an initial cooling rate of at least 15 K / s. Therefore, in this embodiment variant, the annealing device only comprises a heating section and a cooling section.
[0034] In another advantageous embodiment variant of the method, the annealed steel strip can be cooled in a cooling section of the annealing device directly connected to the holding section. In this case, the initial cooling rate is at least 40 K / s.
[0035] To this end, the cooling device advantageously comprises at least one nozzle through which the reducing protective gas can be blown onto the steel strip. However, it is more preferably provided that the cooling device comprises at least one nozzle arranged above the plane of travel of the steel strip and at least one nozzle arranged below the plane of travel of the steel strip. The at least one nozzle can be designed as a slit nozzle, which extends transversely to the transport direction of the steel strip in the cooling section. In another advantageous embodiment variant, the cooling device can have at least one distributor arranged above the plane of travel of the steel strip and at least one distributor arranged below the plane of travel of the steel strip, the distributor comprising a plurality of hole nozzles. The corresponding nozzles are advantageously configured so that the outlet velocity of the reducing protective gas can reach 50 to 150 m / s.
[0036] It is further advantageously provided that the cooling device comprises at least one blower device, via which the reducing protective gas can be supplied to at least one nozzle and, if necessary, to at least one distributor. Furthermore, the cooling device can comprise at least one heat exchanger, by means of which the reducing protective gas blown into the cooling section can be cooled.
[0037] Here, in a particularly advantageous embodiment variant, it is provided that the cooling device has a circulation system in which at least one nozzle and / or at least one distributor together with the nozzle, at least one blowing device and at least one heat exchanger are connected to one another, particularly preferably connected to one another in such a way that the reducing shielding gas is blown into the cooling section, particularly preferably onto the steel strip, by at least one blowing device and at least one nozzle and / or at least one distributor together with the nozzle, and is sucked away again by at least one blowing device and is cooled by means of at least one heat exchanger.
[0038] This cooling device can achieve 500 to 800 W / m2 of heat to the steel strip surface when using a reducing protective gas. 2 K, thereby achieving high cooling rates of more than 40 K / s.
[0039] Preferably, a hydrogen-rich gas is used as the reducing protective gas, which has a hydrogen content of at least 30 vol %, more preferably at least 50 vol %, even more preferably at least 75 vol %.
[0040] In principle, the reducing protective gas can be supplied to the furnace chamber at different locations in the annealing system. However, it is preferably provided that the reducing protective gas is supplied to the holding section in order to achieve the greatest reduction effect at the highest strip temperatures. In another preferred embodiment variant, the reducing protective gas can be supplied to the cooling section in order to increase the heat transfer. BRIEF DESCRIPTION OF THE DRAWINGS
[0041] The invention and the technical field are explained in more detail below with reference to the accompanying drawings. It should be noted that the invention is not intended to be limited to the illustrated embodiments. In particular, unless otherwise expressly stated, some aspects of the facts explained in the drawings may also be extracted and combined with other components and cognitions of the present specification and / or the drawings. In particular, it should be noted that the drawings and in particular the dimensional ratios shown are merely schematic. The same reference numerals denote the same objects, so that the explanations of other drawings may be supplemented if necessary. Among them:
[0042] Figure 1 An embodiment variant of the annealing device according to the invention is shown,
[0043] Figure 2 shows an embodiment variant of a processing line according to the invention,
[0044] Figure 3 shows heat treatment temperature profiles for grain-oriented electrical tape and non-grain-oriented electrical tape, and
[0045] Figure 4Shown is a heat treatment temperature profile for a stainless steel strip. DETAILED DESCRIPTION
[0046] Figure 1 A variant embodiment of an annealing plant 1 according to the invention is shown, which is arranged for use in a treatment line 2 for continuous pickling and non-oxidative annealing of a hot-rolled steel strip 3 (see Figure 2 ). Such a steel strip 3 is used to manufacture an electrical strip and / or a stainless steel strip and is usually sent to a cold rolling process after performing an annealing treatment or a heat treatment.
[0047] The annealing device 1 shown in this embodiment variant comprises a hermetically sealed furnace chamber 4 which is operated under a reducing protective gas atmosphere. The reducing protective gas can be supplied to the furnace chamber 4 at different locations, as is exemplarily indicated by reference numeral 100 .
[0048] The furnace chamber 4 comprises an entry door 5 through which the hot-rolled steel strip 3 enters the furnace chamber 4 and an exit door 6 through which the heat-treated steel strip 3 subsequently leaves the furnace chamber 4 again. Adjacent to the entry door 5, the annealing device 1 first has a heating section 7, which comprises a plurality of inductors 8, 9, 10, 11 connected in series, wherein the inductors 8, 9 form a first stage 12 of the heating section 7 and the two inductors 10, 11 form a second stage 13 of the heating section.
[0049] The inductors 8, 9 are designed as longitudinal field inductors and have corresponding longitudinal field inductor coils 14 for this purpose. In contrast, the inductors 10, 11 are designed as transverse field inductors and have corresponding transverse field inductor coils 15. Furthermore, each of the inductors 8, 9, 10, 11 has a heat insulation layer 18 arranged below the steel strip running plane 16 and a heat insulation layer 17 above, which is provided with an airtight coating 19 on the outside. As can be seen from the figure, a running gap 20 is generated in each of the inductors 8, 9, 10, 11 by the heat insulation layer 17, 18, which has a vertical extension of 150 mm in this embodiment variant in order to facilitate good magnetic field coupling. A roller stand 21 is also arranged between the individual inductors 8, 9, 10, 11, by means of which the strip sag of the steel strip 3 is limited. In this embodiment variant, the roller stand 21 is also provided with a heat insulation layer 18 arranged below the strip running plane 16 and a heat insulation layer 17 above, which is sealed on the outside with respect to the atmosphere by a gas-impermeable covering 19 .
[0050] In addition, the annealing device 1 comprises a holding section 22 connected to the heating section 7, which has three holding section stages 23, 24, 25, wherein each individual holding section stage 23, 24, 25 is provided with an electric heating element 26, which is arranged below the steel strip running plane 16. In the embodiment variant currently shown, the two outer holding section stages 23, 25 additionally comprise conventional cooling nozzles 27 through which air flows, which are arranged above the steel strip running plane 16. Also as shown Figure 1 As shown, the entire holding section 22 is also provided with an insulation layer 18 arranged below the steel strip running plane 16 and an insulation layer 17 above, which is sealed from the atmosphere on the outside by a gas-impermeable covering 19. Then, connected to the holding section 22 is a cooling section 28, which includes a cooling device 29. In the current embodiment variant, the cooling device 29 has two separate cooling stages 30, 31, through which the annealed steel strip 3 can be quenched or quenched with a reducing protective gas, such as hydrogen. For this purpose, each of the two cooling stages 30, 31 has a distributor 32, 33 arranged below and above the steel strip running plane 16, and the distributor is provided with a plurality of nozzles (not shown) oriented in the direction of the steel strip running plane 16. Each of the distributors 32, 33 is fluidly connected to a blast device 34, 35, such as a fan, arranged outside the furnace chamber 4 via a gas line, and the reducing protective gas can then be supplied to the distributor via the blast device. Furthermore, each of the two separate cooling stages 30, 31 comprises a heat exchanger 36, 37, which is also arranged outside the furnace chamber 4, by means of which the reducing protective gas blown into the respective cooling stage 30, 31 of the cooling section 28 can be cooled. For this purpose, the respective cooling stage 30, 31 is fluidically connected to the respective blower 34, 35 via a further gas line.
[0051] Figure 2An embodiment variant of a processing line 2 according to the invention is shown by way of example, the processing line comprising a pretreatment device 38 and an annealing device 1 arranged downstream thereof in the strip conveying direction. Specifically, the processing line 2 shown comprises a first coiling device 39, through which a hot-rolled strip coil 40 is first unrolled. The unrolled hot-rolled steel strip 3 is then sent to a first separation device 41 in order to produce a clean edge for a subsequent welding process by means of the first separation device. After welding in the welding device 42, the steel strip 3 is sent to a trimming device 43, in which the strip edge of the steel strip 3 is trimmed. After passing through the inlet storage 44, the steel strip 3 enters the pretreatment device 38, in which the steel strip undergoes pickling, rinsing and then drying. The pickled steel strip 3 is then fed to the annealing plant 1 and therein first heated to the annealing temperature under a reducing protective gas atmosphere, annealed and then chilled or quenched before being coiled again via the outlet storage 45 .
[0052] Figure 3 The corresponding temperature profiles for the heat treatment of a hot-rolled steel strip 3 which is also provided for producing a grain-oriented electrical strip 48 and a non-grain-oriented electrical strip 49 are shown.
[0053] In the present embodiment, the hot-rolled steel strip 3 provided for manufacturing the grain-oriented electrical strip 48 has a width of 1280 mm and a strip thickness of 2300 μm, and is subjected to non-oxidative heat treatment at a strip speed of 75 m / min in the annealing device 1. On the other hand, the hot-rolled steel strip 3 provided for manufacturing the non-grain-oriented electrical strip 49 has a width of 1280 mm and a strip thickness of 2600 μm, and is subjected to non-oxidative heat treatment at a strip speed of 80 m / min in the annealing device 1.
[0054] For this purpose, the corresponding hot-rolled steel strip 3, which has been previously pickled in a pretreatment device 38, is introduced into a furnace chamber 4 with a reducing protective gas atmosphere through an inlet door 5. A hydrogen-rich gas with a hydrogen content of 75 vol% is used as the reducing protective gas. The corresponding hot-rolled steel strip first passes through a heating section 7, in which it is heated to a Curie temperature of 700° C. by means of two longitudinal field inductors 8, 9. Above the Curie temperature, the steel strip generally loses its paramagnetic properties, and is therefore heated by means of two transverse field inductors 10, 11 until a corresponding annealing temperature of 1120° C. (grain-oriented electrical strip 48) or 1050° C. (non-grain-oriented electrical strip 49) is reached.
[0055] The corresponding steel strip 3 heated to the annealing temperature then passes through a holding section 22, in which the steel strip is annealed according to a specific heat treatment process. Figure 3As shown, the grain-oriented electrical tape 48 is slowly cooled to a temperature of 900° C. in the first holding stage 23, and then passes through the second holding stage 24 and the third holding stage 25 at 900° C. On the other hand, the non-grain-oriented electrical tape 49 first passes through the two holding stages 23, 24 at a preset annealing temperature of 1050° C., and is not slowly cooled to a temperature of 800° C. until in the third holding stage 25.
[0056] The corresponding annealed steel strip 3 then passes through a cooling section 28, in which the steel strip is quenched by means of a reducing protective gas. The grain-oriented electrical strip 48 is cooled here at an initial cooling rate of 40 K / s to a temperature of 420° C. and then at a cooling rate of less than 20 K / s to an outlet temperature of 130° C. On the other hand, the non-grain-oriented electrical strip 49 is cooled at a constant cooling rate of 25 K / s to an outlet temperature of 130° C.
[0057] Figure 4 Shown is a temperature profile for a heat treatment of a hot-rolled steel strip 3 which is also provided for producing a stainless steel strip 30 .
[0058] In the present embodiment, the hot-rolled steel strip 3 of austenitic grade AISI 300, which is provided for producing the stainless steel strip 50, has a width of 1280 mm and a strip thickness of 2600 μm and is subjected to a non-oxidative heat treatment in the annealing device 1 at a strip speed of 80 m / min. Figure 1 The annealing plant 1 shown differs in that the furnace chamber 4 is formed by a heating section 7 and a cooling section 28, wherein the heating section 7 still only has a row of transverse field inductors 10, 11. The hot-rolled steel strip 3, which has been pickled beforehand in a pretreatment plant 38, is likewise introduced through an inlet door 5 into the furnace chamber 4, which has a reducing protective gas atmosphere with a hydrogen content of 75 vol%. The hot-rolled steel strip 3 first passes through the heating section 7, in which the steel strip is heated to an annealing temperature of 1050° C. by means of the transverse field inductors 10, 11. The briefly annealed steel strip 3 then passes through the cooling section 28, in which the steel strip is cooled to an outlet temperature of 80° C. by means of a reducing protective gas at a constant cooling rate of 18 K / s.
[0059] Reference numerals list
[0060] 1Annealing equipment / annealing furnace
[0061] 2 processing lines
[0062] 3Hot-rolled steel strip / hot-rolled strip
[0063] 4 Furnace Chamber
[0064] 5 Entrance door
[0065] 6 Exit Door
[0066] 7 Heating section
[0067] 8 sensors / longitudinal field sensor
[0068] 9Sensors / Longitudinal Field Sensors
[0069] 10 sensors / lateral field sensors
[0070] 11Sensor / lateral field sensor
[0071] 12 Level 1
[0072] 13 Level 2
[0073] 14 Longitudinal field sensor coil
[0074] 15 Transverse Field Inductor Coil
[0075] 16 Steel strip travel plane
[0076] 17 Insulation
[0077] 18 Insulation
[0078] 19 Airtight cover
[0079] 20 Travel Clearance
[0080] 21 Roller rack
[0081] 22 Hold segment
[0082] 23 First hold stage
[0083] 24 Second hold stage
[0084] 25 Third hold stage
[0085] 26 Heating element
[0086] 27 Cooling nozzle
[0087] 28 Cooling section
[0088] 29 Cooling equipment
[0089] 30 First cooling stage
[0090] 31 Second Cooling Stage
[0091] 32 Allocator
[0092] 33 Distributor
[0093] 34 Blower equipment / fan
[0094] 35 Blower equipment / fan
[0095] 36 Heat Exchanger
[0096] 37 Heat Exchanger
[0097] 38 Pretreatment equipment
[0098] 39 First coiling equipment
[0099] 40 Hot rolled strip coil
[0100] 41. First separation equipment
[0101] 42 Welding equipment
[0102] 43 Dressing equipment
[0103] 44 Entrance Storage
[0104] 45 Export storage
[0105] 46 Second separation equipment
[0106] 47 Second coiling equipment
[0107] Annealing treatment of 48 grain oriented electrical strip
[0108] 49 Annealing of non-grain oriented electrical strip
[0109] 50 Annealing of stainless steel strip
[0110] 100 Shielding gas supply.
Claims
1. An annealing plant (1), in particular an annealing furnace, for the non-oxidative heat treatment of hot-rolled steel strips (3) for the production of electrical strips and / or stainless steel strips, preferably for use in a treatment line (2) for continuous pickling and non-oxidative annealing of hot-rolled steel strips (3), the annealing plant comprising: A hermetically sealed furnace chamber (4) having a heating section (7), optionally a holding section (22) connected to the heating section (7), and a cooling section (28) connected to the heating section (7) and optionally to the holding section (22), wherein: The heating section (7) has a plurality of inductors (8, 9, 10, 11) which are connected in series, and the cooling section (28) comprises a cooling device (29) through which a reducing protective gas for cooling the hot-rolled steel strip (3) can be introduced into the cooling section (28).
2. The annealing device (1) according to claim 1, wherein: The cooling device (29) comprises at least one nozzle, through which the reducing protective gas can be blown onto the steel strip (3).
3. The annealing device (1) according to claim 1 or 2, wherein: The cooling device (29) comprises at least one blowing device (34, 35), by means of which the reducing protective gas can be supplied, preferably to at least one nozzle.
4. Annealing device (1) according to any one of the preceding claims, wherein: The cooling device (29) comprises at least one heat exchanger (36, 37), via which the reducing protective gas blown into the cooling section (28) can be cooled.
5. The annealing device (1) according to any one of claims 2 to 4, wherein: The cooling device (29) has a circulation system, in which the at least one nozzle, the at least one blast device (34, 35) and the at least one heat exchanger (36, 37) are connected to each other, preferably so that the reducing protective gas is blown into the cooling section (28) via the at least one blast device (34, 35) and the at least one nozzle, particularly preferably blown onto the steel strip (3), and the reducing protective gas is sucked out again via the at least one blast device (34, 35) and cooled by means of the at least one heat exchanger (36, 37).
6. Annealing device (1) according to any one of the preceding claims, wherein: The heating section (7) has a first stage (12) with a plurality of longitudinal field inductors (8, 9) connected in series, and a second stage (13) with a plurality of transverse field inductors (10, 11) connected in series.
7. Annealing device (1) according to any one of the preceding claims, wherein: The heating section (7) has a passage gap (20) for the steel strip (3), which is delimited by thermal insulation layers (17, 18).
8. The annealing device (1) according to claim 7, wherein: The running gap (20) has a vertical extension of less than or equal to 300 mm, preferably less than or equal to 250 mm.
9. A treatment line (2) for continuous pickling and non-oxidative annealing of hot rolled steel strip (3) arranged for the production of electrical strip and / or stainless steel strip, comprising: a pretreatment device (38) in which the hot-rolled steel strip (3) can be pickled; as well as An annealing plant (1) according to any one of the preceding claims, which is arranged downstream of the pretreatment plant in the direction of transport of the strip.
10. A method for the continuous pickling and non-oxidative annealing of a hot rolled steel strip (3) for producing electrical strip and / or stainless steel strip, wherein: The hot-rolled steel strip (3) is first fed to a pretreatment device (38) after an unfolding step if necessary and pickled in the pretreatment device; then fed to an annealing device (1) as a pickled steel strip (3) and in the annealing device is first inductively heated to an annealing temperature by a plurality of inductors (8, 9, 10, 11) connected in succession under a reducing protective gas atmosphere, then annealed, and subsequently quenched and / or cooled using a reducing protective gas.
11. The method according to claim 10, wherein: The pickled steel strip (3) is first heated in a heating section (7) of the annealing device (1) to an annealing temperature of at least 800° C. at a heating rate of at least 20 K / s.
12. The method according to claim 11, wherein: The pickled steel strip (3) is annealed in a holding section (22) of the annealing device (1) connected to the heating section (7) at a temperature in the range of 800-1200° C. for at least 60 seconds.
13. The method according to claim 11 or 12, wherein: The annealed steel strip (3) is cooled in a cooling section (28) of the annealing device (1) connected to the heating section (7) and, if necessary, to the holding section (22) at an initial cooling rate of at least 15 K / s.
14. The method according to any one of claims 10 to 13, wherein: The pickled steel strip (3) is preferably heated in the heating section (7) via two stages (12, 13) in the following manner, i.e., the pickled steel strip (3) is first heated to a temperature of at least 650° C. in the first stage (12) and then heated to an annealing temperature of at least 800° C. in the second stage (13).
15. The method according to claim 14, wherein: The pickled steel strip (3) is heated in the first stage (12) by means of a plurality of longitudinal field inductors (8, 9) connected in succession, and in the second stage (13) by means of a plurality of transverse field inductors (10, 11) connected in succession.
16. The method according to any one of claims 10 to 15, wherein: The annealed steel strip (3) is cooled in the cooling section (28) of the annealing device (1) by means of a cooling device (29) in the following manner, i.e., a reducing protective gas is blown onto the annealed steel strip (3) by the cooling device, the reducing protective gas is sucked out of the cooling section (28) by means of a blast device (34, 35), and, if necessary, the reducing protective gas is cooled by means of a heat exchanger (36, 37).
17. The method according to any one of claims 10 to 16, wherein: The reducing protective gas is a hydrogen-rich gas which preferably has a hydrogen content of at least 30 vol %, preferably at least 50 vol %, and more preferably at least 75 vol %.
Citation Information
Patent Citations
Process for producing grain-oriented electrical steel strip and grain-oriented electrical steel strip obtained according to said process
US20170283903A1
Heat-treatment method for metal strips
US5472528A