Device and method for preparing large-scale monodisperse liquid drops and application of device and method

By designing a microfluidic chip device, monodispersed micro droplets are formed by using the shearing action of microchannels and steps, the problems of high throughput and uniformity in large-scale monodispersed liquid droplet preparation are solved, and efficient nanomaterial synthesis is achieved.

CN119015997APending Publication Date: 2024-11-26WANNAN MEDICAL UNIVERSITY
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411136078.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-19
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

When mass production of monodisperse droplets, it is difficult to ensure high throughput and automation. Traditional macro reactors have problems such as low reaction efficiency and poor product uniformity.

Method used

Design a microfluidic chip device, including a base layer and a flow channel layer, with an oil phase inlet, a water phase inlet, an oil phase flow channel, a water phase flow channel and a droplet generation structure on the flow channel layer, and passes through the microchannel and step The design forms monodispersed micro droplets in the droplet generation unit, and achieves high-efficiency droplet generation and uniform reaction through the runner structure of the microfluidic chip.

Benefits of technology

The high-throughput droplet generation capability is achieved, which significantly shortens the reaction time, provides a uniform reaction environment, ensures the uniformity of the size and mass of the nanomaterials, and reduces the reaction temperature and pressure conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119015997A_ABST
    Figure CN119015997A_ABST
Patent Text Reader

Abstract

The invention discloses a device and a method for preparing large-scale monodisperse liquid drops and application of the device and the method, and relates to the technical field of microfluidics, the device comprises a micro-fluidic chip, the micro-fluidic chip is formed by bonding a substrate layer and a runner layer, the flow channel layer is provided with an oil phase inlet, a water phase inlet, an oil phase flow channel, a water phase flow channel, a liquid drop generation structure and a liquid outlet, the two ends of the oil phase flow channel communicate with the oil phase inlet and the liquid outlet correspondingly, the high-flux liquid drop generation capacity is achieved, 400 liquid drop generation units work at the same time, the liquid drop production efficiency is improved, and the production cost is reduced. The method has the advantages of high-efficiency synthesis capability, substantial shortening of the reaction time required by the traditional synthesis method, high-uniformity synthesis capability, provision of a uniform reaction environment for micro-droplets, ensuring of the size and quality uniformity of the synthesized nano-material, reduction of the harsh reaction conditions, and realization of large-scale industrial production. And the temperature and pressure conditions required by the reaction are reduced by utilizing the characteristics of high-efficiency mass and heat transfer and large specific surface area of the micro-droplets.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of microfluidics technology, and in particular to a device, method and application thereof for preparing large-scale monodisperse droplets. Background Art

[0002] In recent years, microfluidic technology has been widely used in chemical synthesis, pharmaceuticals, and materials science. Traditional chemical reactions often rely on macroscopic reactors, which have problems such as low reaction efficiency and poor product uniformity. Microfluidic technology can significantly increase reaction rates, control reaction conditions, and improve product quality by controlling the flow and mixing of liquids at the microscale. The importance of microfluidic synthesis technology in fine chemical processing is becoming increasingly prominent. Through microfluidic chips, chemical reactions can be carried out in uniform confined microreactors, thereby achieving more efficient chemical synthesis. This technology is not only suitable for pharmaceuticals and chemical industries, but also shows great potential in biomedicine, materials science, and environmental monitoring.

[0003] In microfluidic synthesis, monodisperse droplets, as an important form of microreactor, are widely used in fine chemical processing due to their controllable size and uniform reaction environment. However, large-scale production of monodisperse droplets still faces challenges, especially under the premise of ensuring high throughput and automation. To this end, a device, method and application of large-scale monodisperse droplet preparation are proposed. Summary of the invention

[0004] The purpose of the present invention is to solve the problems in the prior art and to propose a device, method and application for large-scale monodisperse droplet preparation.

[0005] A device for preparing large-scale monodisperse droplets, comprising a microfluidic chip, wherein the microfluidic chip is formed by bonding a substrate layer and a flow channel layer, and the flow channel layer is provided with an oil phase inlet, a water phase inlet, an oil phase flow channel, a water phase flow channel, a droplet generation structure and a liquid outlet;

[0006] The two ends of the oil phase flow channel are respectively connected to the oil phase inlet and the liquid outlet, one end of the water phase flow channel is connected to the water phase inlet, and the other end is a dead end, the oil phase flow channel is bifurcated into two parallel flow channels at the oil phase inlet and converges at the liquid outlet, and the two parallel flow channels are distributed on both sides of the water phase flow channel;

[0007] The droplet generation structure includes 400 droplet generation units, and a plurality of the droplet generation units are symmetrically distributed on both sides of the wall of the water phase flow channel for connecting the water phase flow channel and the oil phase flow channel.

[0008] Preferably, each of the droplet generation units is composed of a microchannel and a step, the depth of the microchannel is much smaller than the depth of the water phase flow channel or the oil phase flow channel, the inlet and outlet of the microchannel are trumpet-shaped, and the height of the step is generally 2 to 4 times the depth of the microchannel.

[0009] Preferably, the water phase inlet is provided with an array of rectangular blocks with sizes ranging from large to small for filtering impurities and foreign matter in the water phase, and the oil phase inlet is provided with an array of rectangular blocks with sizes ranging from large to small for filtering impurities and foreign matter in the oil phase.

[0010] Preferably, the material of the flow channel layer is polydimethylsiloxane, and the material of the base layer is one of silicon dioxide, polydimethylsiloxane, polycarbonate or polymethyl methacrylate.

[0011] Preferably, the width of the water phase flow channel is 500 μm, the width of the oil phase flow channel is 2000 μm, the length of the microchannel in the droplet generation unit is 500 μm, the width of the microchannel is 20 μm, and the interval between two adjacent microchannels is 80 μm.

[0012] The present invention also provides a method for preparing droplets based on a device for preparing large-scale monodisperse droplets, characterized in that it comprises the following steps:

[0013] S1. Pump the oil phase solution into the microfluidic chip from the oil phase inlet, and control the flow rate at 200 μL / min. The oil phase solution serves as a continuous phase to ensure the stability of droplet generation;

[0014] S2, the aqueous phase reaction solution is pre-mixed through a three-way mixer and then pumped into the microfluidic chip from the aqueous phase inlet, with the flow rate controlled at 30 μL / min, wherein the aqueous phase solution contains nanomaterial precursors and other reactants;

[0015] S3. In the droplet generation unit, through the design of microchannels and step outlets, the water phase is sheared in the oil phase flow channel to form monodisperse microdroplets. The generated microdroplets are collected at the liquid outlet with a small centrifuge tube, and the collected microdroplet solution is placed at the required temperature for the experiment and allowed to stand for a corresponding time, so that the nanomaterials react evenly in the microdroplets.

[0016] S4. After the reaction is completed, use a centrifuge to perform centrifugal demulsification, remove the supernatant, retain the nanomaterials precipitated at the bottom, and wash the precipitate.

[0017] Preferably, in step S4, the precipitate needs to be cleaned three or more times.

[0018] A method for large-scale monodisperse droplet preparation was applied in the synthesis of Hemin@ZIF-8 nanomaterials.

[0019] Compared with the prior art, the present invention has the following advantages:

[0020] The present invention has high-throughput droplet generation capability, with 400 droplet generation units working simultaneously, thus improving droplet production efficiency and having efficient synthesis capability, significantly shortening the reaction time required for traditional synthesis methods, and having high uniformity synthesis capability. The microdroplets provide a uniform reaction environment, ensuring the uniformity of size and quality of the synthesized nanomaterials, and reducing harsh reaction conditions. The efficient mass and heat transfer and large specific surface area characteristics of the microdroplets are utilized to reduce the temperature and pressure conditions required for the reaction. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] Figure 1 Schematic diagram of the structure of the microfluidic chip in the present invention.

[0022] Figure 2 for Figure 1 Enlarged schematic diagram at point A in the middle.

[0023] Figure 3 This is a diagram of droplet generation according to the present invention.

[0024] Figure 4 This is an electron microscope characterization image of the synthetic material in the present invention.

[0025] In the figure: 1 substrate layer, 2 flow channel layer, 3 oil phase inlet, 4 water phase inlet, 5 oil phase flow channel, 6 water phase flow channel, 7 liquid outlet, 8 microchannel, 9 step. DETAILED DESCRIPTION

[0026] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further explained below in conjunction with specific implementation methods.

[0027] Reference Figure 1-2 As shown, a device for preparing large-scale monodisperse droplets includes a microfluidic chip, wherein the microfluidic chip is formed by bonding a substrate layer 1 and a flow channel layer 2, and the flow channel layer 2 is provided with an oil phase inlet 3, a water phase inlet 4, an oil phase flow channel 5, a water phase flow channel 6, a droplet generation structure and a liquid outlet 7;

[0028] The two ends of the oil phase flow channel 5 are respectively connected to the oil phase inlet 3 and the liquid outlet 7, one end of the water phase flow channel 6 is connected to the water phase inlet 4, and the other end is a dead end. The oil phase flow channel 5 is bifurcated into two parallel flow channels at the oil phase inlet 3 and converged at the liquid outlet 7, and the two parallel flow channels are distributed on both sides of the water phase flow channel 6;

[0029] The droplet generation structure includes 400 droplet generation units, and a plurality of the droplet generation units are symmetrically distributed on both sides of the wall of the water phase flow channel 6 for connecting the water phase flow channel 6 and the oil phase flow channel 5 .

[0030] Each of the droplet generation units is composed of a microchannel 8 and a step 9. The depth of the microchannel 8 is much smaller than the depth of the water phase flow channel 6 or the oil phase flow channel 5. The inlet and outlet of the microchannel 8 are trumpet-shaped, which can increase the shear effect of the fluid and help generate droplets. The height of the step 9 is generally 2 to 4 times the depth of the microchannel 8.

[0031] The water phase inlet 4 is provided with a rectangular block array with sizes ranging from large to small, which is used to filter impurities and foreign matter in the water phase. The oil phase inlet 3 is provided with a rectangular block array with sizes ranging from large to small, which is used to filter impurities and foreign matter in the oil phase to avoid clogging of the microchannel 8.

[0032] The material of the flow channel layer 2 is polydimethylsiloxane, and the material of the base layer 1 is one of silicon dioxide, polydimethylsiloxane, polycarbonate or polymethyl methacrylate.

[0033] The width of the water phase flow channel 6 is 500 μm, the width of the oil phase flow channel 5 is 2000 μm, the length of the microchannel 8 in the droplet generation unit is 500 μm, the width of the microchannel 8 is 20 μm, and the interval between two adjacent microchannels 8 is 80 μm.

[0034] A method for preparing droplets based on a device for preparing large-scale monodisperse droplets comprises the following steps:

[0035] S1, pumping the oil phase solution into the microfluidic chip from the oil phase inlet 3, with the flow rate controlled at 200 μL / min. The oil phase solution serves as a continuous phase to ensure the stability of droplet generation;

[0036] S2, the aqueous phase reaction solution is pre-mixed by a three-way mixer, and then pumped into the microfluidic chip from the aqueous phase inlet 4, with the flow rate controlled at 30 μL / min, wherein the aqueous phase solution contains nanomaterial precursors and other reactants;

[0037] S3. In the droplet generation unit, through the design of the microchannel 8 and the step 9 outlet, the water phase is sheared in the oil phase flow channel 5 to form monodisperse microdroplets. The generated microdroplets are collected at the liquid outlet 7 with a small centrifuge tube. The collected microdroplet solution is placed at the required temperature for the experiment and allowed to stand for a corresponding time, so that the nanomaterial reacts evenly in the microdroplets.

[0038] S4. After the reaction is completed, use a centrifuge to perform centrifugal demulsification, remove the supernatant, retain the nanomaterials precipitated at the bottom, and wash the precipitate.

[0039] In step S4, the precipitate needs to be cleaned three or more times to ensure the purity and quality of the nanomaterial.

[0040] A method for large-scale monodisperse droplet preparation was applied in the synthesis of Hemin@ZIF-8 nanomaterials by reacting Hemin solution, 2-methylimidazole solution and zinc acetate solution in microdroplets for 10 min.

[0041] Example 1

[0042] This embodiment is used to illustrate the structure and processing of the microfluidic chip of the present invention.

[0043] The microfluidic chip of the present invention is composed of a base layer 1 and a flow channel layer 2. The base layer 1 is made of a glass slide, and the flow channel layer 2 is made of polydimethylsiloxane (PDMS). The flow channel layer is processed by a casting method, and the template is made by a traditional soft photolithography process, and a double exposure method is used to achieve a double-layer structure. First, the silicon wafer is soaked in an acetone solution for 120 minutes, and then ultrasonically cleaned with isopropanol and deionized water for 120 seconds each; then, it is heated in an oven at 120°C for 15 minutes to remove surface moisture; then, SU-83025 photoresist is spin-coated, and a two-step spin coating process is used to achieve the desired thickness, and soft-baked at 95°C for 10-15 minutes; the first exposure uses 150mJ / cm 2 The energy of mercury lamp is 7.5mW / cm 2 After exposure, the film was exposed to a photolithography machine for 20 seconds; after exposure, a post-baking (PEB) of 65°C for 1 minute and 95°C for 5 minutes was performed; then, SU-83050 photoresist was spin-coated, and a soft bake was performed for 45 minutes, and the film was heated at 250 mJ / cm 2 The silicon wafer was exposed for the second time with an energy of 100°C; after 16 minutes of development, the silicon wafer was rinsed with isopropyl alcohol and the substrate was blown dry with compressed air, and finally post-baked at 150-200°C for 10 minutes; the PDMS mold was prepared by mixing the prepolymer and the cross-linking agent in a ratio of 10:1 and stirring them evenly, then poured onto the silicon wafer template and degassed in a vacuum drying oven; it was heated in a 70°C oven for 3 hours to complete the PDMS curing; after curing, the PDMS was peeled off and holes were punched; then, after plasma treatment, the PDMS was bonded to the cleaned glass slide; the chip structure and depth were tested for compliance using a microscope and a step profiler, respectively.

[0044] Example 2

[0045] This example is used to illustrate the configuration of the reaction solution of the present invention.

[0046] The aqueous phase solution of this embodiment includes a mixed solution of an aqueous phase solution containing Hemin and 2-methylimidazole and a zinc acetate solution containing Zn2+. First, an appropriate amount of Hemin is dissolved in deionized water, stirred evenly, and a 1mg / mL Hemin solution is prepared; then, an appropriate amount of 2-methylimidazole (2-Methylimidazole) is added to the Hemin solution, stirred evenly, and the final concentration reaches 50mM; then, an appropriate amount of zinc acetate (ZincAcetate) is weighed, dissolved in deionized water, stirred evenly, and a zinc acetate solution of the required concentration is prepared; the two solutions are mixed through a three-way before entering the chip to finally form an aqueous phase solution.

[0047] The oil phase solution of this embodiment is a hydrophobic organic solvent, such as mineral oil or fluorinated liquid. Mineral oil is used as the base solvent, and then 2% of the surfactant ABIL EM-90 is added, stirred evenly, to form the final oil phase solution; fluorinated liquid FC-40 or HFE-7500 is selected as the base solvent, and then 1% of the surfactant Krytox 157FSL is added, stirred evenly, to form the final oil phase solution.

[0048] Example 3

[0049] This example is used to illustrate the operation steps of synthesizing the Hemin@ZIF-8 nanomaterial of the present invention.

[0050] The oil phase solution is pumped into the microfluidic chip from the oil phase inlet 3, and the flow rate is controlled at 200 μL / min. At the same time, the aqueous phase reaction solution is pre-mixed through a three-way mixer and then pumped into the microfluidic chip from the aqueous phase inlet 4, and the flow rate is controlled at 30 μL / min. In the droplet generation unit, through the design of the microchannel 8 and the step 9 outlet, the aqueous phase is subjected to shearing and surface tension in the oil phase flow channel 5 to form microdroplets (such as Figure 3 As shown), the generated microdroplets are collected at the fluid outlet with a small centrifuge tube and placed at the required temperature for the experiment (such as room temperature or 37°C) for a corresponding period of time to complete the synthesis of Hemin@ZIF-8 nanomaterials; after the reaction is completed, a centrifuge is used for centrifugal demulsification (3000rpm, 10 minutes), the supernatant is removed, and the Hemin@ZIF-8 nanomaterials precipitated at the bottom are retained. The precipitate is washed at least three times (using ethanol and deionized water) to ensure purity and quality.

[0051] Example 4

[0052] This example is used to illustrate the characterization of the microfluidic synthesized Hemin@ZIF-8 nanomaterial of the present invention.

[0053] First, the morphology and particle size distribution of Hemin@ZIF-8 nanomaterials were observed using transmission electron microscopy (TEM), and the surface morphology of the nanomaterials was further confirmed by scanning electron microscopy (SEM). Then, the crystal structure of Hemin@ZIF-8 nanomaterials was analyzed by X-ray diffraction (XRD) to confirm the characteristic diffraction peaks of ZIF-8; in addition, the elemental composition of Hemin@ZIF-8 nanomaterials was analyzed by energy dispersive X-ray spectroscopy (EDX) to confirm the coexistence of Hemin and ZIF-8; then, the specific surface area of ​​Hemin@ZIF-8 nanomaterials was determined using nitrogen adsorption-desorption isotherm method (BET); finally, the catalytic performance of Hemin@ZIF-8 nanomaterials was evaluated by detecting the conversion rate of the target reactant and the product generation rate.

[0054] In summary, the present invention has high-throughput droplet generation capability, with 400 droplet generation units working simultaneously, which improves the droplet production efficiency and has efficient synthesis capability, significantly shortening the reaction time required for traditional synthesis methods, and at the same time has high uniformity synthesis capability. The microdroplets provide a uniform reaction environment, ensuring the uniformity of size and quality of the synthesized nanomaterials, and reducing the harsh reaction conditions. The efficient mass transfer and heat transfer and large specific surface area characteristics of the microdroplets are utilized to reduce the temperature and pressure conditions required for the reaction.

[0055] It is known from common technical knowledge that the present invention can be implemented by other embodiments that do not deviate from its spirit or essential features. Therefore, the above disclosed embodiments are only illustrative in all respects and are not exclusive. All changes within the scope of the present invention or within the scope equivalent to the present invention are included in the present invention.

Claims

1. A device for large-scale monodisperse droplet preparation, characterized in that: The microfluidic chip comprises a substrate layer (1) and a flow channel layer (2) bonded together, and the flow channel layer (2) is provided with an oil phase inlet (3), a water phase inlet (4), an oil phase flow channel (5), a water phase flow channel (6), a droplet generation structure and a liquid outlet (7); The two ends of the oil phase flow channel (5) are respectively connected to the oil phase inlet (3) and the liquid outlet (7); one end of the water phase flow channel (6) is connected to the water phase inlet (4), and the other end is a dead end; the oil phase flow channel (5) is bifurcated into two parallel flow channels at the oil phase inlet (3) and converges at the liquid outlet (7), and the two parallel flow channels are distributed on both sides of the water phase flow channel (6); The droplet generation structure comprises 400 droplet generation units, and a plurality of the droplet generation units are symmetrically distributed on both sides of the wall of the water phase flow channel (6) for connecting the water phase flow channel (6) and the oil phase flow channel (5).

2. The device for large-scale monodisperse droplet preparation according to claim 1, characterized in that: Each of the droplet generation units is composed of a microchannel (8) and a step (9). The depth of the microchannel (8) is much smaller than the depth of the water phase flow channel (6) or the oil phase flow channel (5). The inlet and outlet of the microchannel (8) are trumpet-shaped. The height of the step (9) is generally 2 to 4 times the depth of the microchannel (8).

3. The device for large-scale monodisperse droplet preparation according to claim 1, characterized in that: The water phase inlet (4) is provided with an array of rectangular blocks of decreasing sizes for filtering impurities and foreign matter in the water phase, and the oil phase inlet (3) is provided with an array of rectangular blocks of decreasing sizes for filtering impurities and foreign matter in the oil phase.

4. The device for large-scale monodisperse droplet preparation according to claim 1, characterized in that: The material of the flow channel layer (2) is polydimethylsiloxane, and the material of the base layer (1) is one of silicon dioxide, polydimethylsiloxane, polycarbonate or polymethyl methacrylate.

5. The device for large-scale monodisperse droplet preparation according to claim 2, characterized in that: The width of the water phase flow channel (6) is 500 μm, the width of the oil phase flow channel (5) is 2000 μm, the length of the microchannel (8) in the droplet generation unit is 500 μm, the width of the microchannel (8) is 20 μm, and the interval between two adjacent microchannels (8) is 80 μm.

6. A method for preparing droplets based on the device for preparing large-scale monodisperse droplets according to any one of claims 1 to 5, characterized in that: The following steps are involved: S1, pumping the oil phase solution into the microfluidic chip from the oil phase inlet (3), with the flow rate controlled at 200 μL / min. The oil phase solution serves as a continuous phase to ensure the stability of droplet generation; S2, the aqueous phase reaction solution is pre-mixed through a three-way mixer, and then pumped into the microfluidic chip from the aqueous phase inlet (4), with the flow rate controlled at 30 μL / min, wherein the aqueous phase solution contains nanomaterial precursors and other reactants; S3. In the droplet generation unit, through the design of the outlet of the microchannel (8) and the step (9), the water phase is sheared in the oil phase flow channel (5) to form monodisperse microdroplets. The generated microdroplets are collected at the liquid outlet (7) using a small centrifuge tube. The collected microdroplet solution is placed at the temperature required for the experiment and allowed to stand for a corresponding period of time, so that the nanomaterial reacts evenly in the microdroplets. S4. After the reaction is completed, use a centrifuge to perform centrifugal demulsification, remove the supernatant, retain the nanomaterials precipitated at the bottom, and wash the precipitate.

7. A method for preparing large-scale monodisperse droplets according to claim 6, characterized in that: In step S4, the precipitate needs to be cleaned three or more times.

8. Application of the method for large-scale monodisperse droplet preparation according to claims 6-7 in the synthesis of Hemin@ZIF-8 nanomaterials.

Citation Information

Cited By

  • Microfluidic liquid bead preparation device and method based on channel shunting-capillary fixed-point shearing

    CN120940010A