Inner wall anti-corrosion plastic coating device for steel pipeline machining and plastic coating method
By designing an internal anti-corrosion coating device for steel pipe processing, impurities on the inner surface of the steel pipe are cleaned and efficient coating is achieved, solving the problem that impurities after inner surface treatment affect the coating quality and improving coating efficiency and quality.
Patent Information
- Application Number
- CN202411118749.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-15
- Publication Date
- 2024-11-26
AI Technical Summary
During the process of plastic coating inside steel pipes, impurities still exist after the inner surface treatment, affecting the coating quality and resulting in low coating efficiency.
An anti-corrosion coating device for the inner wall of steel pipe processing was designed, including a drive mechanism, a moving mechanism, a cleaning mechanism, a coating mechanism, and a drying mechanism. The cleaning mechanism cleans impurities on the inner surface, the coating mechanism sprays paint, and the drying mechanism dries the paint, thus achieving efficient coating.
It effectively cleans impurities from the inner surface of steel pipes, improves coating quality and efficiency, ensures uniform paint application and rapid drying, and enhances the corrosion resistance of steel pipes.
Smart Images

Figure CN119016259A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of steel pipe processing, and specifically relates to an inner wall anti-corrosion plastic coating device and a plastic coating method for steel pipe processing. Background Art
[0002] Plastic coating inside steel pipe processing refers to coating the inner wall of the steel pipe with a layer of plastic material through a specific process to enhance the corrosion resistance and wear resistance of the steel pipe. This process usually involves the following key steps: Surface treatment of steel pipe: First, the steel pipe is subjected to surface treatments such as rust removal and oil removal to ensure that the plastic coating layer can be firmly attached to the surface of the steel pipe. Preparation of plastic coating layer: Select suitable plastic materials such as polyethylene (PE), epoxy resin (EP), etc. according to requirements, and heat them to a molten state to form a plastic coating liquid. Coating: Coat the molten plastic on the inner wall of the steel pipe. Commonly used methods include spraying, dipping, etc. to form a uniform plastic coating layer. Curing: The coated steel pipe needs to enter a curing furnace or undergo natural curing to completely cure the plastic coating layer to form a solid anti-corrosion layer.
[0003] At present, when plastic coating is carried out on the inside of a steel pipe, the inner surface of the steel pipe needs to be treated first to remove burrs and other impurities on the inner surface of the steel pipe. However, some impurities will still exist on the inner surface of the steel pipe after the inner surface treatment during plastic coating. The presence of these impurities will affect the quality of the plastic coating on the inner surface of the steel pipe. At the same time, each layer of plastic coating needs to be left to dry after completion, which affects the efficiency of plastic coating. Based on this, an inner wall anti-corrosion plastic coating device and a plastic coating method for steel pipeline processing are proposed. Summary of the invention
[0004] The purpose of the present invention is to provide an inner wall anti-corrosion plastic coating device and a plastic coating method for steel pipeline processing in order to solve the above-mentioned problems.
[0005] The present invention achieves the above-mentioned purpose through the following technical solutions:
[0006] The inner wall anti-corrosion plastic coating device for steel pipeline processing comprises a plastic coating device, the plastic coating device comprises a first mounting block, a connecting pipe and a second mounting block, the connecting pipe is installed between the first mounting block and the second mounting block, and further comprises:
[0007] A driving mechanism, which is installed on the plastic coating equipment to provide power for the plastic coating of the steel pipe;
[0008] A moving mechanism, the moving mechanism is installed on the outer surface of the plastic coating device, and the moving mechanism is used to make the plastic coating device move smoothly on the inner surface of the steel pipe;
[0009] A transmission mechanism, which is installed in the plastic coating device and is used to transmit power from the driving mechanism to enable the moving mechanism to work;
[0010] A cleaning mechanism, which is installed at the output end of the driving mechanism and is rotatably connected to the second mounting block, and is used to clean the inner surface of the steel pipe;
[0011] A plastic coating mechanism, which is mounted on the plastic coating device and rotates along the central axis of the plastic coating device under the operation of the driving mechanism;
[0012] A drying mechanism is installed on the plastic coating equipment and is used to dry the inner surface of the steel pipe after plastic coating.
[0013] As a further optimization scheme of the present invention, the cleaning mechanism includes a hollow disk rotatably connected to the end of the second mounting block, the outer wall of the hollow disk is fixedly connected to a sleeve, a sliding rod is slidably connected to the sleeve, one end of the sliding rod located in the sleeve is fixedly connected to a connecting spring, the connecting spring is fixedly connected in the sleeve, and the end of the sliding rod away from the connecting spring is fixedly connected to a cleaning ring, the cleaning ring is fixedly connected to hollow bristles, the cleaning ring is fixedly connected to balls, the hollow bristles are connected to the cleaning ring, the cleaning ring is connected to the sliding rod, the sliding rod is connected to the sleeve, the sleeve is connected to the hollow disk, and the hollow disk is connected to the second mounting block.
[0014] As a further optimization scheme of the present invention, the plastic coating mechanism includes a transfer ring fixedly connected to the end of the second mounting block away from the hollow disk, the side wall of the transfer ring is fixedly connected with a paint supply pipe, the outer wall of the transfer ring is fixedly connected with a connecting pipe, the end of the connecting pipe is fixedly connected with a plastic coating ring, the outer surface of the plastic coating ring is rotatably connected with a plastic coating ring, the inner wall of the plastic coating ring is fixedly connected with a gear ring, the transfer ring is rotatably connected with a rotating shaft, the two ends of the rotating shaft are respectively fixedly connected with a sixth bevel gear and a transmission gear, the transmission gear is meshed with the gear ring, the paint supply pipe passes through the first mounting block and is fixedly connected to the first mounting block, and the rotating shaft passes through the connecting pipe and is rotatably connected to the connecting pipe.
[0015] As a further optimization scheme of the present invention, the drying mechanism includes an air pipe fixedly connected to the first mounting block, the end of the air pipe is fixedly connected to a fixing ring, the fixing ring is rotatably connected to a jet chamber, the outer wall of the jet chamber is fixedly connected to a jet pipe, and the jet chamber is fixedly connected to the plastic coated ring.
[0016] As a further optimization scheme of the present invention, the driving mechanism includes a motor fixedly connected to the first mounting block, the output end of the motor is fixedly connected to a rotating shaft, the portion of the rotating shaft located in the first mounting block is fixedly connected to a first bevel gear, the portion of the rotating shaft located in the connecting pipe is fixedly connected to a second bevel gear, the portion of the rotating shaft located in the second mounting block is fixedly connected to a fan blade, the second mounting block is fixedly connected to a dustproof net, and the dustproof net is rotatably connected to the rotating shaft.
[0017] As a further optimization solution of the present invention, the second bevel gear is meshed with the sixth bevel gear, and one end of the rotating shaft away from the motor is fixedly connected to the inner wall of the hollow disk.
[0018] As a further optimization scheme of the present invention, the moving mechanism includes a fixed plate fixedly connected to the plastic coating equipment, a sliding groove is opened on the fixed plate, a slide is slidably connected in the sliding groove, the slide is slidably connected to the fixed plate, a connecting shaft is rotatably connected to the slide, a moving wheel is fixedly connected to the connecting shaft, a clamping spring is fixedly connected to the bottom of the slide, and the clamping spring is fixedly connected to the outer surface of the plastic coating equipment.
[0019] As a further optimization scheme of the present invention, the transmission mechanism includes a transmission shaft rotatably connected to the first mounting block, one end of the transmission shaft is fixedly connected to the third bevel gear, the other end of the transmission shaft is provided with a hexagonal slot, a plug rod matching the slot is slidably connected in the slot, the top of the plug rod is fixedly connected to a rotating rod, the top of the rotating rod is fixedly connected to a fourth bevel gear, and a fifth bevel gear is meshed on the fourth bevel gear.
[0020] As a further optimization solution of the present invention, the third bevel gear is meshed with the first bevel gear, the fifth bevel gear is fixedly connected to the connecting shaft, and the rotating rod is rotatably connected to the slide.
[0021] The inner wall anti-corrosion plastic coating method for steel pipeline processing includes the following steps:
[0022] Step 1: The plastic coating device is stably placed in the steel pipe through a moving mechanism;
[0023] Step 2: Connect the plastic coating mechanism to the external primer paint;
[0024] Step 3: Start the driving mechanism to move the plastic coating device inside the steel pipe;
[0025] Step 4: During the movement, the cleaning mechanism cleans the inner surface of the steel pipe, the coating mechanism sprays paint on the cleaned inner surface of the steel pipe, and then the drying mechanism dries the inner surface of the steel pipe sprayed with paint;
[0026] Step 5: After the primer is sprayed, repeat the above steps until the topcoat is sprayed.
[0027] The beneficial effects of the present invention are:
[0028] 1. The present invention drives the cleaning mechanism to work through the operation of the driving mechanism, so that the cleaning mechanism rotates along the inner surface of the steel pipe, and the impurities remaining after the pretreatment of the inner surface of the steel pipe are cleaned from the inner surface of the steel pipe. At the same time, since the driving mechanism is provided with fan blades, the rotation of the fan blades will cause the cleaning mechanism to produce a suction effect, so that the cleaning mechanism draws the cleaned impurities into the cleaning mechanism, thereby achieving effective cleaning of the inner surface of the steel pipe. The use of suction can prevent impurities from falling everywhere and affecting the quality of subsequent coating, thereby ensuring the anti-corrosion quality of the steel pipe after coating.
[0029] 2. The present invention cleans the inner surface of the steel pipe through a cleaning mechanism. Since the cleaning process is friction cleaning, the cleaning mechanism and the inner surface of the steel pipe will be heated up under the action of friction, so that the extracted impurities and air have heat. The hot air will enter the coating equipment and wrap around the outer surface of the paint pipe to insulate the paint in the paint pipe, thereby ensuring the fluidity of the paint inside the paint pipe, so that the paint can be better atomized, thereby ensuring the quality of the coating on the inner surface of the steel pipe, and the heating of the inner surface of the steel pipe can improve the adhesion of the paint, thereby ensuring the quality of the coating inside the steel pipe, and the hot air will directly act on the inner surface of the steel pipe after coating, so that the paint can dry quickly on the inner surface of the steel pipe, thereby improving the drying efficiency of the coated paint, thereby improving the processing efficiency of the inner surface of the steel pipe. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 It is a schematic diagram of the overall front three-dimensional structure of the present invention;
[0031] Figure 2 It is a schematic diagram of the overall side three-dimensional structure of the present invention;
[0032] Figure 3 It is a schematic diagram of the structure of the present invention cut away from the middle of the front side;
[0033] Figure 4 The present invention Figure 3 The enlarged structural diagram at A in the middle;
[0034] Figure 5 The present invention Figure 3 The enlarged structural diagram at B in the middle;
[0035] Figure 6 The present invention Figure 3 The enlarged structural diagram at C in the middle;
[0036] Figure 7 It is a schematic diagram of the three-dimensional structure of the cleaning mechanism and the moving mechanism of the present invention from the side;
[0037] Figure 8It is a front three-dimensional structural schematic diagram of the cleaning mechanism and the moving mechanism of the present invention;
[0038] Fig. 9 It is a three-dimensional structural schematic diagram of the mobile mechanism of the present invention;
[0039] Fig.10 It is a three-dimensional partially cutaway structural schematic diagram of the cleaning mechanism of the present invention.
[0040] In the figure: 1, plastic coating equipment; 101, first mounting block; 102, connecting pipe; 103, second mounting block; 2, driving mechanism; 201, motor; 202, rotating shaft; 203, first bevel gear; 204, second bevel gear; 205, fan blade; 206, dust screen; 3, transmission mechanism; 301, third bevel gear; 302, transmission shaft; 303, slot; 304, plug rod; 305, rotating rod; 306, fourth bevel gear; 307, fifth bevel gear; 4, moving mechanism; 401, fixed plate; 402, slide groove; 403, slide; 404, connecting shaft; 4 05. Moving wheel; 406. Clamping spring; 5. Cleaning mechanism; 501. Hollow disk; 502. Sleeve; 503. Sliding rod; 504. Connecting spring; 505. Cleaning ring; 506. Hollow bristles; 507. Ball; 6. Plastic coating mechanism; 601. Paint delivery pipe; 602. Transfer ring; 603. Connecting pipe; 604. Plastic coating ring; 605. Plastic coating ring; 606. Sixth bevel gear; 607. Rotating shaft; 608. Transmission gear; 609. Gear ring; 7. Drying mechanism; 701. Air delivery pipe; 702. Fixed ring; 703. Jet chamber; 704. Jet pipe. DETAILED DESCRIPTION
[0041] The present application is further described in detail below in conjunction with the accompanying drawings. It is necessary to point out here that the following specific implementation methods are only used to further illustrate the present application and cannot be understood as limiting the scope of protection of the present application. Technical personnel in this field can make some non-essential improvements and adjustments to the present application based on the above application content.
[0042] Example
[0043] like Figure 1-Figure 3 , Figure 5-Figure 8As shown, the inner wall anti-corrosion plastic coating device for steel pipe processing includes a plastic coating device 1, which is composed of a first mounting block 101, a connecting pipe 102 and a second mounting block 103. The first mounting block 101, the connecting pipe 102 and the second mounting block 103 are all set to a hollow form, and a dust removal plate is installed at the bottom of the second mounting block 103. The connecting pipe 102 is installed between the first mounting block 101 and the second mounting block 103. It also includes: a driving mechanism 2, which is installed on the plastic coating device 1 to provide power for the steel pipe plastic coating. The driving mechanism 2 includes a motor 201 fixedly connected to the first mounting block 101, and the output end of the motor 201 is fixedly connected to a rotating shaft 202. The rotating shaft The part of 202 located in the first mounting block 101 is fixedly connected to the first bevel gear 203, the part of the rotating shaft 202 located in the connecting pipe 102 is fixedly connected to the second bevel gear 204, the part of the rotating shaft 202 located in the second mounting block 103 is fixedly connected to the fan blade 205, the second mounting block 103 is fixedly connected to the dustproof net 206, the dustproof net 206 is rotatably connected to the rotating shaft 202, the moving mechanism 4, the moving mechanism 4 is installed on the outer surface of the plastic coating equipment 1, and the moving mechanism 4 is used to make the plastic coating equipment 1 move smoothly on the inner surface of the steel pipe; the transmission mechanism 3, the transmission mechanism 3 is installed in the plastic coating equipment 1, and is used to transmit the power of the driving mechanism 2 to make the moving mechanism 4 work, and the moving mechanism 4 is used to move the moving mechanism 4 to the inner surface of the steel pipe. The driving mechanism 4 includes a fixed plate 401 fixedly connected to the plastic coating device 1, a slide groove 402 is provided on the fixed plate 401, a slide 403 is slidably connected in the slide groove 402, the slide 403 is slidably connected to the fixed plate 401, a connecting shaft 404 is rotatably connected to the slide 403, a moving wheel 405 is fixedly connected to the connecting shaft 404, a clamping spring 406 is fixedly connected to the bottom of the slide 403, the clamping spring 406 is fixedly connected to the outer surface of the plastic coating device 1, the clamping spring 406 and the fixed plate 401 are fixedly connected to the outer walls of the first mounting block 101 and the second mounting block 103, and the transmission mechanism 3 includes a transmission shaft 302 rotatably connected to the first mounting block 101 One end of the transmission shaft 302 is fixedly connected to the third bevel gear 301, and the other end of the transmission shaft 302 is provided with a hexagonal slot 303, in which a plug rod 304 matching with it is slidably connected, and a rotating rod 305 is fixedly connected to the top of the plug rod 304, and a fourth bevel gear 306 is fixedly connected to the top of the rotating rod 305, and a fifth bevel gear 307 is meshed on the fourth bevel gear 306, the third bevel gear 301 is meshed with the first bevel gear 203, and the fifth bevel gear 307 is fixedly connected to the connecting shaft 404, the rotating rod 305 is rotatably connected to the slide 403, and only the slide 403 on the first mounting block 101 is rotatably connected to the rotating rod 305.
[0044] When in use, the plastic coating device 1 is placed in a steel pipe. When placed, since the diameters of the steel pipes are different and the diameter of the steel pipe is smaller than the overall width of the plastic coating device 1, when the plastic coating device 1 is placed in the steel pipe, the steel pipe will push the moving wheel 405, and then push the slide 403 to slide into the slide groove 402 through the connecting shaft 404, and compress the pressing spring 406, so that the moving wheel 405 presses against the inner surface of the steel pipe, and the slide 403 located on the first mounting block 101 will push the insertion rod 305 to ... sliding wheel 405 to push the sliding wheel 405 to push the sliding wheel 405 to push the sliding wheel 405 to push the sliding wheel 405 to push the sliding wheel 405 to push the sliding wheel 405 to push the sliding wheel 405 to push the sliding wheel 405 to push the sliding wheel 405 to push the sliding wheel 405 to push the sliding wheel 405 to push the sliding wheel 405 to push the sliding wheel The rod 304 moves into the slot 303. After placement, the motor 201 can be started to rotate the shaft 202. The rotation of the shaft 202 will drive the first bevel gear 203 to rotate, and then drive the transmission shaft 302 to rotate through the third bevel gear 301. The rotation of the transmission shaft 302 will drive the rotating rod 305 to rotate through the slot 303 and the plug rod 304, and then drive the connecting shaft 404 to rotate through the fourth bevel gear 306 and the fifth bevel gear 307, so that the moving wheel 405 moves along the inner surface of the steel pipe;
[0045] The device can be applied to steel pipes with different inner diameters, thereby expanding the application range of the device and facilitating use.
[0046] like Figure 1-Figure 3 , Figure 7 , Figure 8 and Fig.10 As shown, the cleaning mechanism 5 is installed at the output end of the driving mechanism 2 and is rotatably connected to the second mounting block 103. The cleaning mechanism 5 is used to clean the inner surface of the steel pipe. The cleaning mechanism 5 includes a hollow disk 501 rotatably connected to the end of the second mounting block 103. The end of the rotating shaft 202 away from the motor 201 is fixedly connected to the inner wall of the hollow disk 501. The outer wall of the hollow disk 501 is fixedly connected with a sleeve 502. A sliding rod 503 is slidably connected in the sleeve 502. One end of the sliding rod 503 located in the sleeve 502 is fixedly connected There is a connecting spring 504, which is fixedly connected in the sleeve 502. The end of the sliding rod 503 away from the connecting spring 504 is fixedly connected with a cleaning ring 505, and hollow bristles 506 are fixedly connected to the cleaning ring 505. The cleaning ring 505 is fixedly connected with balls 507. The hollow bristles 506 are connected to the cleaning ring 505, and the cleaning ring 505 is connected to the sliding rod 503. The sliding rod 503 is connected to the sleeve 502, and the sleeve 502 is connected to the hollow disk 501, and the hollow disk 501 is connected to the second mounting block 103.
[0047] When in use, when the device is placed in a steel pipe, the sliding rod 503 will slide into the sleeve 502 through the extrusion of the steel pipe, and the connecting spring 504 will be compressed to make the ball 507 fit the inner surface of the steel pipe, while leaving gaps for the hollow bristles 506 to clean the inner surface of the steel pipe, and the hollow bristles 506 are bent to fit the inner surface of the steel pipe to prevent the hollow bristles 506 from being squeezed on the inner surface of the steel pipe, which makes it impossible for the hollow bristles 506 to extract the cleaned impurities. When the shaft 202 rotates, the hollow disk 501 will be driven to rotate, and then the cleaning ring 505 will be driven to rotate through the sleeve 502 and the slide rod 503, so that the ball 507 rolls along the inner surface of the steel pipe, and the hollow bristles 506 clean the inner surface of the steel pipe. At the same time, the rotation of the shaft 202 will also drive the fan blades 205 to rotate, so that the fan blades 205 produce a suction effect, and then the hollow bristles 506 will suck the cleaned impurities and air into the second mounting block 103;
[0048] The impurities remaining on the inner surface of the steel pipe after pretreatment are cleaned off from the inner surface of the steel pipe, and the vacuum method can prevent the impurities from falling everywhere and affecting the quality of subsequent coating, thereby ensuring the anti-corrosion quality of the steel pipe after coating. In addition, since the hollow bristles 506 rotate along the inner surface of the steel pipe, the mutual friction will cause the inner surface of the steel pipe to heat up, thereby improving the adhesion of the paint on the inner surface of the steel pipe, thereby ensuring the quality of the coating inside the steel pipe.
[0049] like Figure 1 , Figure 2 , Figure 4 , Figure 6-Figure 8 As shown, the plastic coating mechanism 6 is installed on the plastic coating device 1, and rotates along the central axis of the plastic coating device 1 under the operation of the driving mechanism 2. The plastic coating mechanism 6 includes a transfer ring 602 fixedly connected to the end of the second mounting block 103 away from the hollow disk 501, the side wall of the transfer ring 602 is fixedly connected to the paint delivery pipe 601, the outer wall of the transfer ring 602 is fixedly connected to the connecting pipe 603, the end of the connecting pipe 603 is fixedly connected to the plastic coating ring 604, and the outer surface of the plastic coating ring 604 is rotatably connected to the plastic coating ring 60 5. The inner wall of the plastic coating ring 605 is fixedly connected with a gear ring 609, the transfer ring 602 is rotatably connected with a rotating shaft 607, the two ends of the rotating shaft 607 are respectively fixedly connected with a sixth bevel gear 606 and a transmission gear 608, the transmission gear 608 is meshed with the gear ring 609, the paint delivery pipe 601 passes through the first mounting block 101 and is fixedly connected to the first mounting block 101, the rotating shaft 607 passes through the connecting pipe 102 and is rotatably connected to the connecting pipe 102, and the second bevel gear 204 is meshed with the sixth bevel gear 606.
[0050] When in use, after the plastic coating device 1 is installed in the steel pipe, the paint delivery pipe 601 is connected to the external paint. When the plastic coating device 1 moves, the external paint is transported to the paint delivery pipe 601 by the pump body, and the paint entering the paint delivery pipe 601 will enter the transfer ring 602, and then enter the plastic coating ring 604 through the connecting pipe 603, and finally sprayed on the inner surface of the steel pipe through the plastic coating ring 605. In this process, the rotation of the rotating shaft 202 will drive the second bevel gear 204 to rotate, and then drive the rotating shaft 607 to rotate through the sixth bevel gear 606, so that the transmission gear 608 drives the gear ring 609 to rotate, and then the plastic coating ring 605 rotates and sprays;
[0051] The uniformity of paint spraying is improved, the quality of paint spraying is guaranteed, thereby ensuring the quality of anti-corrosion coating on the inner surface of the steel pipe.
[0052] like Figure 1 , Figure 2 , Figure 4 , Figure 7 and Figure 8 As shown, the drying mechanism 7 is installed on the plastic coating equipment 1, and is used to dry the inner surface of the steel pipe after plastic coating. The drying mechanism 7 includes an air pipe 701 fixedly connected to the first mounting block 101, and the end of the air pipe 701 is fixedly connected to a fixing ring 702, and the fixing ring 702 is rotatably connected to a jet chamber 703, and the outer wall of the jet chamber 703 is fixedly connected to a jet pipe 704, and the jet chamber 703 is fixedly connected to the plastic coating ring 605.
[0053] When in use, the impurities and hot air extracted by the fan blades 205 are filtered through the dustproof net 206, so that the hot air enters the first installation block 101, and the hot air entering the first installation block 101 will wrap around the outer surface of the paint delivery pipe 601, and keep the paint in the paint delivery pipe 601 warm. Then the hot air will pass through the air delivery pipe 701 and enter the injection chamber 703, and finally pass through the injection pipe 704 to be sprayed on the inner surface of the steel pipe sprayed with paint. In this process, due to the rotation of the plastic coating ring 605, the injection chamber 703 will be driven to rotate, so that the hot air can act more on the inner surface of the steel pipe sprayed with paint.
[0054] The rapid drying of the paint is achieved, ensuring the quality and efficiency of the plastic coating on the inner surface of the steel pipe.
[0055] like Figure 1-Figure 10 As shown, the inner wall anti-corrosion plastic coating method for steel pipeline processing includes the following steps:
[0056] Step 1: The plastic coating device 1 is stably placed in the steel pipe through the moving mechanism 4;
[0057] The plastic coating device 1 is placed in the steel pipe. When placing the plastic coating device 1, since the diameters of the steel pipes are not the same and the diameter of the steel pipe is smaller than the overall width of the plastic coating device 1, when the plastic coating device 1 is placed in the steel pipe, the steel pipe will push the moving wheel 405, and then push the slide 403 to slide into the slide groove 402 through the connecting shaft 404, and compress the pressing spring 406, so that the moving wheel 405 is pressed against the inner surface of the steel pipe, and the slide 403 located on the first mounting block 101 will push the insertion rod 304 to move into the slot 303 through the rotating rod 305. After the placement is completed, the motor 201 can be started to rotate the rotating shaft 202. The rotation of the rotating shaft 202 will drive the first bevel gear 203 to rotate, and then drive the transmission shaft through the third bevel gear 301 302 rotates, and the rotation of the transmission shaft 302 will drive the rotating rod 305 to rotate through the slot 303 and the plug rod 304, and then drive the connecting shaft 404 to rotate through the fourth bevel gear 306 and the fifth bevel gear 307, so that the moving wheel 405 moves along the inner surface of the steel pipe. When the device is placed in the steel pipe, the sliding rod 503 will slide into the sleeve 502 through the extrusion of the steel pipe, and the connecting spring 504 will be compressed to make the ball 507 fit with the inner surface of the steel pipe, and at the same time, a gap will be left for the hollow bristles 506 to clean the inner surface of the steel pipe, and the hollow bristles 506 will be bent to fit the inner surface of the steel pipe to prevent the hollow bristles 506 from being squeezed on the inner surface of the steel pipe, so that the hollow bristles 506 cannot extract the cleaned impurities;
[0058] Step 2: Connect the plastic coating mechanism 6 to the external primer paint;
[0059] After the plastic coating equipment 1 is installed in the steel pipe, the paint delivery pipe 601 is connected to the external paint;
[0060] Step 3: Start the driving mechanism 2 to move the plastic coating device 1 inside the steel pipe;
[0061] After the placement is completed, the motor 201 can be started to rotate the rotating shaft 202. The rotation of the rotating shaft 202 will drive the first bevel gear 203 to rotate, and then drive the transmission shaft 302 to rotate through the third bevel gear 301. The rotation of the transmission shaft 302 will drive the rotating rod 305 to rotate through the slot 303 and the plug rod 304, and then drive the connecting shaft 404 to rotate through the fourth bevel gear 306 and the fifth bevel gear 307, so that the moving wheel 405 moves along the inner surface of the steel pipe;
[0062] Step 4: During the movement, the cleaning mechanism 5 cleans the inner surface of the steel pipe, the coating mechanism 6 sprays paint on the cleaned inner surface of the steel pipe, and then the drying mechanism 7 dries the inner surface of the steel pipe sprayed with paint;
[0063] When the rotating shaft 202 rotates, the hollow disk 501 will be driven to rotate, and then the cleaning ring 505 will be driven to rotate through the sleeve 502 and the slide rod 503, so that the ball 507 rolls along the inner surface of the steel pipe, and the hollow bristles 506 clean the inner surface of the steel pipe. At the same time, the rotation of the rotating shaft 202 will also drive the fan blades 205 to rotate, so that the fan blades 205 produce a suction effect, and then the hollow bristles 506 will suck the cleaned impurities and air into the second mounting block 103;
[0064] When the plastic coating device 1 moves, the external paint is transported by the pump body to the paint delivery pipe 601, and the paint entering the paint delivery pipe 601 will enter the transfer ring 602, and then enter the plastic coating ring 604 through the connecting pipe 603, and finally sprayed on the inner surface of the steel pipe through the plastic coating ring 605. In this process, the rotation of the rotating shaft 202 will drive the second bevel gear 204 to rotate, and then drive the rotating shaft 607 to rotate through the sixth bevel gear 606, so that the transmission gear 608 drives the gear ring 609 to rotate, and then the plastic coating ring 605 rotates and sprays;
[0065] After the impurities and hot air extracted by the fan blades 205 are filtered through the dustproof net 206, the hot air enters the first mounting block 101. The hot air entering the first mounting block 101 will wrap around the outer surface of the paint delivery pipe 601 to keep the paint in the paint delivery pipe 601 warm. Then the hot air will enter the jet chamber 703 through the air delivery pipe 701, and finally be sprayed on the inner surface of the steel pipe sprayed with paint through the jet pipe 704. In this process, due to the rotation of the plastic coating ring 605, the jet chamber 703 will be driven to rotate, so that the hot air can act more on the inner surface of the steel pipe sprayed with paint, thereby achieving rapid drying of the paint and ensuring the quality and efficiency of the plastic coating on the inner surface of the steel pipe.
[0066] Step 5: After the primer is sprayed, repeat the above steps until the topcoat is sprayed.
[0067] The above-mentioned embodiments only express several implementation methods of the present invention, and the description thereof is relatively specific and detailed, but it cannot be understood as limiting the scope of the present invention. It should be pointed out that, for ordinary technicians in this field, several variations and improvements can be made without departing from the concept of the present invention, which all belong to the protection scope of the present invention.
Claims
1. An inner wall anti-corrosion plastic coating device for steel pipeline processing, comprising a plastic coating device (1), It is characterized in that The plastic coating device (1) is composed of a first mounting block (101), a connecting pipe (102) and a second mounting block (103), wherein the connecting pipe (102) is installed between the first mounting block (101) and the second mounting block (103), and further comprises: A driving mechanism (2), wherein the driving mechanism (2) is installed on the plastic coating device (1) and provides power for plastic coating of the steel pipe; A moving mechanism (4), the moving mechanism (4) being installed on the outer surface of the plastic coating device (1), the moving mechanism (4) being used to enable the plastic coating device (1) to move smoothly on the inner surface of the steel pipe; A transmission mechanism (3), the transmission mechanism (3) being installed in the plastic coating device (1) and used for transmitting power of the driving mechanism (2) to enable the moving mechanism (4) to work; A cleaning mechanism (5), the cleaning mechanism (5) being mounted on the output end of the driving mechanism (2) and being rotatably connected to the second mounting block (103), the cleaning mechanism (5) being used to clean the inner surface of the steel pipe; A plastic coating mechanism (6), wherein the plastic coating mechanism (6) is installed on the plastic coating device (1) and rotates along the central axis of the plastic coating device (1) under the operation of the driving mechanism (2); A drying mechanism (7), wherein the drying mechanism (7) is installed on the plastic coating equipment (1) and is used to dry the inner surface of the steel pipe after plastic coating.
2. The inner wall anti-corrosion plastic coating device for steel pipeline processing according to claim 1, Features: The cleaning mechanism (5) comprises a hollow disk (501) rotatably connected to the end of the second mounting block (103); the outer wall of the hollow disk (501) is fixedly connected to a sleeve (502); a sliding rod (503) is slidably connected inside the sleeve (502); one end of the sliding rod (503) located inside the sleeve (502) is fixedly connected to a connecting spring (504); the connecting spring (504) is fixedly connected inside the sleeve (502); and one end of the sliding rod (503) away from the connecting spring (504) is fixedly connected to the sleeve (502). A cleaning ring (505) is connected, hollow bristles (506) are fixedly connected to the cleaning ring (505), balls (507) are fixedly connected to the cleaning ring (505), the hollow bristles (506) are connected to the cleaning ring (505), the cleaning ring (505) is connected to the sliding rod (503), the sliding rod (503) is connected to the sleeve (502), the sleeve (502) is connected to the hollow disk (501), and the hollow disk (501) is connected to the second mounting block (103).
3. The inner wall anti-corrosion plastic coating device for steel pipeline processing according to claim 2, Features: The plastic coating mechanism (6) comprises a transfer ring (602) fixedly connected to the end of the second mounting block (103) away from the hollow disk (501), the side wall of the transfer ring (602) is fixedly connected to the paint delivery pipe (601), the outer wall of the transfer ring (602) is fixedly connected to the connecting pipe (603), the end of the connecting pipe (603) is fixedly connected to the plastic coating ring (604), the outer surface of the plastic coating ring (604) is rotatably connected to the plastic coating ring (605), and the inner wall of the plastic coating ring (605) is fixedly connected to the outer surface of the plastic coating ring (604). A gear ring (609) is connected, a rotating shaft (607) is rotatably connected to the intermediate ring (602), and both ends of the rotating shaft (607) are respectively fixedly connected to a sixth bevel gear (606) and a transmission gear (608), and the transmission gear (608) is meshed with the gear ring (609), the paint delivery pipe (601) passes through the first mounting block (101) and is fixedly connected to the first mounting block (101), and the rotating shaft (607) passes through the connecting pipe (102) and is rotatably connected to the connecting pipe (102).
4. The inner wall anti-corrosion plastic coating device for steel pipeline processing according to claim 3, Features: The drying mechanism (7) comprises an air supply pipe (701) fixedly connected to the first mounting block (101), the end of the air supply pipe (701) being fixedly connected to a fixing ring (702), an injection chamber (703) being rotatably connected to the fixing ring (702), an injection pipe (704) being fixedly connected to the outer wall of the injection chamber (703), and the injection chamber (703) being fixedly connected to the plastic coating ring (605).
5. The inner wall anti-corrosion plastic coating device for steel pipeline processing according to claim 4, Features: The driving mechanism (2) comprises a motor (201) fixedly connected to a first mounting block (101); an output end of the motor (201) is fixedly connected to a rotating shaft (202); a portion of the rotating shaft (202) located in the first mounting block (101) is fixedly connected to a first bevel gear (203); a portion of the rotating shaft (202) located in the connecting pipe (102) is fixedly connected to a second bevel gear (204); a portion of the rotating shaft (202) located in the second mounting block (103) is fixedly connected to a fan blade (205); a dust screen (206) is fixedly connected in the second mounting block (103); and the dust screen (206) is rotatably connected to the rotating shaft (202).
6. The inner wall anti-corrosion plastic coating device for steel pipeline processing according to claim 5, Features: The second bevel gear (204) is meshed with the sixth bevel gear (606), and one end of the rotating shaft (202) away from the motor (201) is fixedly connected to the inner wall of the hollow disk (501).
7. The inner wall anti-corrosion plastic coating device for steel pipeline processing according to claim 5, Features: The moving mechanism (4) comprises a fixed plate (401) fixedly connected to the plastic coating device (1), a sliding groove (402) is provided on the fixed plate (401), a slide (403) is slidably connected in the sliding groove (402), the slide (403) is slidably connected to the fixed plate (401), a connecting shaft (404) is rotatably connected to the slide (403), a moving wheel (405) is fixedly connected to the connecting shaft (404), a clamping spring (406) is fixedly connected to the bottom of the slide (403), and the clamping spring (406) is fixedly connected to the outer surface of the plastic coating device (1).
8. The inner wall anti-corrosion plastic coating device for steel pipeline processing according to claim 7, Features: The transmission mechanism (3) comprises a transmission shaft (302) rotatably connected to the first mounting block (101); one end of the transmission shaft (302) is fixedly connected to a third bevel gear (301); the other end of the transmission shaft (302) is provided with a hexagonal slot (303); a plug rod (304) adapted thereto is slidably connected in the slot (303); a rotating rod (305) is fixedly connected to the top of the plug rod (304); a fourth bevel gear (306) is fixedly connected to the top of the rotating rod (305); a fifth bevel gear (307) is meshed with the fourth bevel gear (306).
9. The inner wall anti-corrosion plastic coating device for steel pipeline processing according to claim 8, Features: The third bevel gear (301) is meshed with the first bevel gear (203), the fifth bevel gear (307) is fixedly connected to the connecting shaft (404), and the rotating rod (305) is rotatably connected to the sliding bracket (403).
10. A method for coating inner wall of steel pipeline for anti-corrosion, using the device for coating inner wall of steel pipeline for anti-corrosion according to any one of claims 1 to 9. It is characterized in that The steps include: Step 1: The plastic coating device (1) is stably placed in the steel pipe through the moving mechanism (4); Step 2: connecting the plastic coating mechanism (6) to the external primer paint; Step 3: starting the driving mechanism (2) to move the plastic coating device (1) inside the steel pipe; Step 4: During the movement, the cleaning mechanism (5) cleans the inner surface of the steel pipe, the coating mechanism (6) sprays paint on the cleaned inner surface of the steel pipe, and then the drying mechanism (7) dries the inner surface of the steel pipe sprayed with paint; Step 5: After the primer is sprayed, repeat the above steps until the topcoat is sprayed.