Manufacturing method of integrated resonant quartz accelerometer
Through the integrated resonant quartz accelerometer manufacturing method, the problems of cantilever beam width and sidewall electrode etching are solved, and higher sensitivity and mechanical stability are achieved. The width of cantilever beam reaches 30 μm, and the sensitivity is increased by 4 times.
Patent Information
- Application Number
- CN202411467855.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-21
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-10-21
AI Technical Summary
The existing quartz accelerometer manufacturing process is difficult to achieve the width of the cantilever beam less than 70 μm, and the side walls of the cantilever beam cannot etch the electrodeposited pattern, resulting in low sensitivity and insufficient mechanical stability.
Using an integrated resonant quartz accelerometer manufacturing method, quartz sheets are rinsed by pickling, alkaline washing and DI water to form a film layer of preset thickness, and wet etching is performed using a metal hard mask and an organic etching solution to eliminate The edges and cantilever beams and hinges are formed, and the electrodes are then coated and etched on the surface of the cantilever beam to achieve patterning of the sidewall electrodes.
The cantilever beam was successfully manufactured with a width of 30 μm, with an increase in sensitivity of about 4 times, enhanced mechanical stability, and a significant increase in electromechanical coupling coefficient.
Smart Images

Figure CN119018847A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of semiconductor sensor manufacturing, and in particular to a method for manufacturing an integrated resonant quartz accelerometer. Background Art
[0002] The sensitivity of a quartz accelerometer is affected by the width of its cantilever beam. The smaller the width of the cantilever beam, the higher its sensitivity. The existing manufacturing process of quartz accelerometers often makes it difficult to manufacture cantilever beams with smaller widths, and generally can only achieve a cantilever beam width of 70 μm. In addition, the existing manufacturing process also has the problem that the mechanical stability of the manufactured accelerometer is insufficient, and the cantilever beam is often etched with an electric polarization pattern on its surface, but it is impossible to etch the electric polarization pattern on the side wall surface of the cantilever beam. Summary of the invention
[0003] In view of the deficiencies of the prior art, an object of the present invention is to provide a method for manufacturing an integrated resonant quartz accelerometer, which can solve the problems described in the background technology.
[0004] The technical solution for achieving the purpose of the present invention is: a method for manufacturing an integrated resonant quartz accelerometer, comprising the following steps: Step 1: Select a quartz sheet, and sequentially perform acid washing, alkali washing, and DI water washing on the quartz sheet to obtain a treated quartz sheet; Step 2: coating the upper and lower surfaces of the processed quartz sheet in the thickness direction to form a film layer of a preset thickness; Step 3: forming a quartz wafer with a metal hard mask having an accelerometer structure pattern; Step 4: placing the quartz wafer with the metal hard mask into a first organic etching solution for wet etching to obtain a quartz wafer containing a preliminary accelerometer structure; Step 5: Eliminate the sidewalls on the quartz plate containing the preliminary accelerometer structure; Step 6: forming a metal hard mask on the lower surface of the quartz plate in the thickness direction of the hinge and forming a metal hard mask on the upper surface in the thickness direction of the cantilever beam, and then placing the quartz plate in a second organic etching solution for etching to obtain the cantilever beam and the hinge; Step 7: Remove the surface film layer of the quartz plate; Step 8: Make electrodes on the surface of the cantilever beam of the quartz accelerometer to obtain the final quartz accelerometer.
[0005] Furthermore, in step 2, magnetron sputtering is used for film coating, and the formed film layer includes a chromium film layer and a gold film layer formed in sequence in a direction away from the quartz sheet.
[0006] Furthermore, the specific implementation process of forming the quartz wafer with the metal hard mask having the accelerometer structure pattern includes the following steps: A positive photoresist of a preset thickness is spin-coated on the upper and lower surfaces of the quartz wafer in the thickness direction after the coating, and the preset thickness can be 2-5 μm. Then, the quartz wafer after the coating of the photoresist is sequentially exposed by an exposure machine in double-sided alignment, pre-baked on a hot plate at a temperature of 100°C, developed, and post-baked on a hot plate at a temperature of 107°C. The coating without the photoresist after the development process is etched away with an etching solution, and the etching solution is selected from gold and chromium etching solutions to etch away the gold film layer and the chromium film layer at the corresponding position, so as to form a metal hard mask with an accelerometer pattern on the upper and lower surfaces in the thickness direction of the quartz wafer. Then, the accelerometer pattern on the metal hard mask is transferred to the cured photoresist to obtain a quartz wafer with an accelerometer structure pattern.
[0007] Furthermore, the gold etching solution uses a solution composed of potassium iodide and iodine ion compounds, and the etching time of the gold etching solution is 30 seconds. The chromium etching solution uses a mixed solution of cerium ammonium nitrate, and the etching time is 60 seconds.
[0008] Furthermore, during the etching process, a quartz wafer is loaded with a crystal boat and placed in a gold etching solution and a chromium etching solution at 22°C to remove the coating film in the area not covered by the photoresist, and an interval time is set according to the concentration of the etching solution. The quartz wafer is pulled up and down at each interval time. After etching, the dried quartz wafer is immersed in an N-methylpyrrolidone solution and maintained for a first preset time, and then immersed in an IPA solution and maintained for a second preset time to remove the surface cured positive photoresist, and then the quartz wafer is placed in running DI water for cleaning. The quartz wafer after the positive photoresist is removed is placed in the first etching solution for etching. The first etching solution is a mixed solution of 40% HF and 45% NH4F. The mass ratio of the two solutions is 3:2. The etching is carried out at a constant temperature of 30 °C for 40 h, and then taken out and washed with DI water and dried in turn. The quartz wafer containing the preliminary accelerometer structure is obtained. Then, the quartz wafer was subjected to secondary photolithography: photoresist was sprayed on the surface of the quartz wafer in a closed chamber at 80 °C, and the thickness of the formed photoresist was 5 μm. After spraying the photoresist, the quartz wafer was placed on a hot plate at a temperature of 110 °C for heat baking for 90 s. After the heat baking, the quartz wafer was double-sided exposed using an exposure machine. After exposure, the quartz wafer was placed in a developer for development, and then the pattern on the mask was transferred to the surface of the solidified photoresist.
[0009] Furthermore, in step 4, the first organic etching solution is a mixed solution of 40% HF, 45% NH4F, and 30% KF, and the mass ratio of the three solutions is 1:2:1, and the etching is performed at a constant temperature of 23°C for 2 hours. Every half an hour, the quartz sheet is pulled up and down for one minute, and then immersed in a low concentration KOH solution.
[0010] Furthermore, in step 6, the second organic etching solution is a mixed solution consisting of BOE and 45% concentration of NH4F, and the ratio of the solutions is 1:1 by mass ratio.
[0011] Furthermore, the specific implementation process of making the electrode includes the following steps: Step 81: coating the cantilever beam to form a film layer, wherein the film layer includes a gold film layer and a chromium film layer, and the film layer includes a chromium film layer and a gold film layer sequentially formed in a direction away from the cantilever beam. After the film layer is formed, a 5 μm thick positive photoresist is sprayed on the upper and lower surfaces of the cantilever beam, and double-sided photolithography is performed. After passing through a gold etching solution and a chromium etching solution, a metal hard mask is formed on the upper and lower surfaces of the cantilever beam; Step 82: placing the quartz sheet forming the metal hard mask of the cantilever beam into a first organic etching solution for etching to obtain a symmetrical groove structure; Step 83: Repeat step 81 to obtain a new metal hard mask pattern at a position corresponding to the cantilever beam by designing a different metal mask; Step 84: placing the quartz wafer with the new metal hard mask pattern into the first organic etching solution again, and etching through the portion without the metal hard mask; Step 85: Execute step 81 again to obtain a new metal hard mask, and deposit metal on the sidewall of the cantilever beam 12; Step 86: using a combination of dry etching and wet etching to trim the cantilever beam; Step 87: Spray 5 μm thick positive photoresist on the upper and lower surfaces of the cantilever beam in the thickness direction. After double-sided photolithography, use gold etching solution and chromium etching solution to etch to remove excess metal hard mask, thereby forming electrodes on the upper and lower surfaces of the cantilever beam in the thickness direction.
[0012] Furthermore, the cantilever beam includes 6 electrodes, which are respectively recorded as the first electrode, the second electrode, the third electrode, the fourth electrode, the fifth electrode and the sixth electrode. The first electrode, the third electrode and the fifth electrode have the same polarity, the second electrode, the fourth electrode and the sixth electrode have the same polarity, the first electrode and the second electrode have opposite polarity, the length of the first electrode, the second electrode, the third electrode and the fourth electrode is half of the fifth electrode and the sixth electrode, and are all located on the upper side of the cantilever beam, the fifth electrode and the sixth electrode are located on the lower side of the cantilever beam, the first electrode and the third electrode are electrically connected, the third electrode and the fourth electrode are electrically connected, the fourth electrode is electrically connected to the second electrode and the fifth electrode respectively, and the second electrode and the sixth electrode are electrically connected.
[0013] Furthermore, in step 1, a quartz sheet with a thickness of 120 μm is selected, in step 2, the thickness of the gold film layer is 1000 Å, the thickness of the chromium film layer is 400 Å, and in step 81, the thickness of the gold film layer is 2000 Å, and the thickness of the chromium film layer is 500 Å.
[0014] Beneficial effects of the present invention: The present invention can manufacture the accelerometer, and adopts the sidewall electrode patterning process, so that the electrode pattern is not on the upper surface of the quartz plate, but on the side wall of the cantilever beam, so that the width of the cantilever beam of the accelerometer can reach about 30 microns, compared with the traditional 70 μm wide accelerometer, its sensitivity can be increased by about 4 times, and the corresponding structure of the manufactured quartz accelerometer ensures the mechanical stability of the accelerometer. In addition, the cantilever beam maintains lateral vibration in the in-plane mode, and the electrode pattern on the side of the cantilever beam is perpendicular to the vibration direction, thereby greatly increasing the electromechanical coupling coefficient. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 is a front view schematic diagram of a quartz accelerometer; Figure 2 is a schematic diagram of the three-dimensional structure of a quartz accelerometer; Figure 3 A process flow chart for the manufacturing method; Figure 4 It is a schematic diagram of the structure of the electrode of the cantilever beam; Figure 5 For Figure 4 Schematic diagram of the process of electrode output from the AA` section; Figure 6 For Figure 4 Schematic diagram of the process of electrode output in the middle BB` section; Figure 7 Schematic diagram of the process of electrode patterning for cantilever beams; Figure 8is a curve diagram of the relationship between the sensitivity and width of the cantilever beam, in which the abscissa represents the width of the cantilever beam and the ordinate represents the sensitivity of the cantilever beam; Fig. 9 is a stress distribution curve diagram of the cantilever beam, in which the abscissa represents the length of the cantilever beam and the ordinate represents the stress of the cantilever beam; Fig.10 for Figure 4 Schematic diagram of electrode distribution from the front view of the right side wall of the middle cantilever beam; Fig.11 for Figure 4 Schematic diagram of the electrode distribution on the upper surface of the middle cantilever beam from the front view; In the figure, 1-vertical connecting beam, 2-support seat, 3-mounting hole, 4-upper concave isolation hole, 5-transverse connecting beam, 6-first hinge, 7-outer frame, 8-right isolation hole, 9-lower concave isolation hole, 10-mass block, 11-second hinge, 12-cantilever beam, 13-end, 14-inner frame, 501-first electrode, 502-second electrode, 503-third electrode, 504-fourth electrode, 505-fifth electrode, 506-sixth electrode. DETAILED DESCRIPTION
[0016] The present invention will be further described below in conjunction with the accompanying drawings and specific embodiments: like Figure 1-Figure 11 As shown, a manufacturing method of an integrated resonant quartz accelerometer is provided, wherein the integrated resonant quartz accelerometer comprises an outer frame 7, an inner frame 14 and a beam-mass structure, wherein the inner frame 14 is fixedly connected to the outer frame 7 through a plurality of transverse connecting beams 5, and the inner frame 14 and the outer frame 7 are spaced apart by isolation holes except for the transverse connecting beams 5. The beam-mass structure is fixedly connected to the inner frame 14 through a vertical connecting beam 1, and the vertical connecting beam 1 is perpendicular to the transverse connecting beam 5, that is, the transverse connecting beam 5 is horizontally arranged, and the vertical connecting beam 1 is vertically arranged.
[0017] The outer frame 7 and the inner frame 14 are both closed structures, the inner frame 14 is located inside the outer frame 7 , and the beam-mass structural member is located inside the inner frame 14 .
[0018] Exemplarily, four transverse connecting beams 5 are included, and a group of transverse connecting beams 5 are respectively arranged on the left and right sides of the inner frame 14. The same group of transverse connecting beams 5 includes two transverse connecting beams 5 arranged in parallel and spaced apart, and an isolation hole is formed between the two transverse connecting beams 5 arranged in parallel and spaced apart. Therefore, a left isolation hole (not shown in the figure) and a right isolation hole 8 are respectively formed on the left and right sides of the inner frame 14, and the left isolation hole and the right isolation hole 8 are symmetrically arranged. An upper concave isolation hole 4 and a lower concave isolation hole 9 are also respectively arranged between the two groups of transverse connecting beams 5 in the upper and lower directions, and the upper concave isolation hole 4 and the lower concave isolation hole 9 are both concave and symmetrically arranged. That is, the isolation holes include a left isolation hole, a right isolation hole 8, an upper concave isolation hole 4, and a lower concave isolation hole 9.
[0019] refer to Figure 1 A group of transverse connecting beams 5 is arranged on the right side of the inner frame 14. Two transverse connecting beams 5 in the group of transverse connecting beams 5 are arranged in parallel and spaced apart along the up-down direction (i.e., the length direction of the outer frame 7). The two transverse connecting beams 5 are arranged horizontally (i.e., the width direction of the outer frame 7), and right isolation holes 8 are formed on the two transverse connecting beams 5 brackets. The right isolation holes 8 are in the shape of strips and extend along the up-down direction.
[0020] Exemplarily, the vertical connecting beam 1 is fixedly connected to one end of the inner frame 14 close to the upper concave isolation hole 4 and is located in the middle of the end.
[0021] Exemplarily, the outer frame 7 , the inner frame 14 and the beam-mass structural member are all manufactured on a quartz plate, and therefore, the outer frame 7 , the inner frame 14 and the beam-mass structural member are essentially an integrated structure.
[0022] The beam-mass structure comprises a support seat 2, a cantilever beam 12, a mass block 10 and two hinges, the two hinges being respectively denoted as a first hinge 6 and a second hinge 11. The upper end of the support seat 2 is fixedly connected to the vertical connecting beam 1, so that the beam-mass structure is fixedly connected to the inner frame 14, the lower end section of the support seat 2 is respectively fixedly connected to one end of the two hinges, and the other end of the two hinges is fixedly connected to the mass block 10. The first hinge 6 and the second hinge 11 are arranged in parallel and spaced apart, and the length and width of the first hinge 6 and the second hinge 11 are the same. The ends 13 at the upper and lower ends of the cantilever beam 12 are respectively fixedly connected to the support seat 2 and the mass block 10, the ends 13 extend into the grooves pre-dug in the mass block 10 and the support seat 2, and the width of the ends 13 is greater than the width of the main body of the cantilever beam 12. The ends 13 are fixedly connected to the inner bottom wall of the groove, and are spaced apart from the side walls on both sides of the groove. The cantilever beam 12 is located between the two hinges, and is spaced apart from the two hinges in parallel.
[0023] Exemplarily, the two hinges (the first hinge 6 and the second hinge 11) are both H-shaped, or the hinges are in an I-shaped structure from the horizontal direction. That is, the hinge includes two vertical beams parallel to the cantilever beam 12, and the two vertical beams are connected by a horizontal beam, and the horizontal beam is arranged perpendicular to the vertical beam. The purpose of setting the vertical beam in the H-shaped hinge is that the vertical beam connects the mass block 10 with the support seat 2, and the moment of inertia can be reduced while ensuring that the hinge stiffness remains unchanged, so that the cross-sectional end 13 of the cantilever beam 12 obtains greater stress.
[0024] In addition, the center of gravity of the cantilever beam 12 and the hinge are at the same height in the vertical direction (ie, the coordinates of the Y axis are the same), so that the accelerometer flip torque can be suppressed.
[0025] The thickness of the two hinges is the same and is smaller than the thickness of the mass block 10. Preferably, the thickness H1 of the hinge and the thickness H2 of the mass block 10 have the following relationship: H1=a*H2, a=1 / 4-1 / 3. That is, the thickness of the hinge is 1 / 4 to 1 / 3 of the thickness of the mass block 10.
[0026] The thickness of the cantilever beam 12 is the same as that of the hinge, and the width of the cantilever beam 12 (ie, the main body width of the cantilever beam 12 ) is 30 μm (micrometers), which is much smaller than the width of the hinge. The central axis of the cantilever beam 12 coincides with the central axis of the vertical connecting beam 1 .
[0027] Exemplarily, the outer frame 7 and the inner frame 14 are both rectangular, and a mounting hole 3 is respectively provided at the four corners of the outer frame 7. The accelerometer can be mounted externally, for example, on a packaging base, through the mounting hole 3.
[0028] When the accelerometer is subjected to acceleration caused by an external force, the mass block 10 will cause an inertial force, which will cause the stress of the cross-sectional ends 13 at both ends of the cantilever beam wall to change, so that the acceleration can be calculated by measuring the resonant frequency of the cantilever beam wall.
[0029] The outer frame 7 is connected to the inner frame 14 through several (four in this example) transverse connecting beams 5, and the beam-mass structure is connected to the inner frame 14 through the vertical connecting beam 1. The cantilever beam wall is perpendicular to the support seat 2 and the mass block 10, so that the parasitic modes around the resonance of the cantilever beam 12 can be suppressed, and the anti-interference ability of the accelerometer is improved. The hinges on both sides of the cantilever beam 12 can ensure that the cantilever beam 12 can withstand a larger acceleration measurement range, and the H-shaped hinge can reduce the stress distribution by exchanging the hinge rotational inertia, so that the stress generated by the mass block 10 when sensing the acceleration is concentrated at the ends 13 at both ends of the cantilever beam 12. Among them, the hinges are provided with isolation holes along the length direction (i.e., the up and down direction) of the cantilever beam 12, so that the stress is concentrated at the cantilever beam 12, ensuring that the cantilever beam 12 accurately responds to the change of the inertial force and produces corresponding stress changes, thereby ensuring the accuracy of the measured acceleration.
[0030] In addition, the beam-mass 10 is connected to the inner frame 14 through the vertical connecting beam 1, so that the beam-mass 10 and the inner frame and the outer frame 7 maintain a vertical design, thereby extending the heat propagation path of the accelerometer during operation and reducing anchoring losses.
[0031] The quartz accelerometer has a stable structure and strong anti-interference performance, and the stress is concentrated at both ends of the cantilever beam 12 by reducing the stress distribution, thereby improving the accuracy and sensitivity of the quartz accelerometer.
[0032] refer to Figure 3-Figure 9 The present invention provides an integrated resonant quartz accelerometer, which can be obtained based on a manufacturing method of an integrated resonant quartz accelerometer, and the manufacturing method comprises the following steps: Step 1: Select a quartz sheet with a preset thickness, the preset thickness is selected according to the actual situation, and the preset thickness in this embodiment is 120 μm. The quartz sheet is sequentially acid-washed, alkaline-washed and rinsed with DI water to obtain a treated quartz sheet.
[0033] Step 2: The upper and lower surfaces of the processed quartz plate in the thickness direction are coated by magnetron sputtering to form a film layer of preset thickness, wherein the film layer includes a chromium film layer and a gold film layer formed in sequence along a direction away from the quartz plate, that is, the chromium film layer is plated first and then the gold film layer is plated. The thickness of the gold film layer is 1000 Å (angstroms), and the thickness of the chromium film layer is 400 Å (angstroms).
[0034] In this step, chromium, which has a thermal expansion coefficient close to that of the quartz wafer, is selected as the adhesion layer, and then magnetron sputtering is continued on the surface of the chromium film layer to form a 1000 Å thick gold film layer, which serves as a protective layer during the wet etching process of the quartz wafer hard mask in the subsequent steps to protect the quartz wafer.
[0035] Step 3: Spin-coat a preset thickness of positive photoresist on the upper and lower surfaces of the quartz wafer in the thickness direction after coating, and the preset thickness can be 2-5 μm. Then, the quartz wafer after coating the photoresist is sequentially exposed by an exposure machine in double-sided alignment, pre-baked on a hot plate at a temperature of 100°C, developed, and post-baked on a hot plate at a temperature of 107°C, and the coating without photoresist after development is etched away with an etching solution, and the etching solution is selected from gold and chromium etching solutions to etch away the gold film layer and chromium film layer at the corresponding positions, thereby forming a metal hard mask with an accelerometer pattern on the upper and lower surfaces in the thickness direction of the quartz wafer. Then, the accelerometer pattern on the metal hard mask is transferred to the cured photoresist to obtain a quartz wafer with an accelerometer structure pattern.
[0036] In this step, the accelerometer pattern on the mask is also the structural pattern of the integrated resonant quartz accelerometer.
[0037] Among them, the gold etching solution uses a solution composed of potassium iodide and iodine ion compounds, and the etching time of the gold etching solution is 30 seconds. The chromium etching solution uses a mixed solution of ammonium cerium nitrate, and the etching time is 60 seconds. During the etching process, the quartz wafer is loaded with a crystal boat and kept stationary in the gold etching solution and chromium etching solution at 22 ° C to remove the coating in the area not covered by the photoresist. During the etching process, no stirring component is used for stirring, and the interval time is set according to the concentration of the etching solution. At each interval, the quartz wafer is pulled up and down to avoid the formation of complexes on the surface of the quartz wafer, thereby avoiding affecting the etching rate. After etching, the quartz wafer is placed in a natural ventilation environment to dry. After the quartz wafer is dried, the quartz wafer is immersed in N-methylpyrrolidone (NMP) solution to remove the surface cured positive photoresist. Among them, the immersion time is maintained for 30 minutes, and then immersed in IPA solution (isopropyl alcohol solution) and maintained for 10 minutes. After being soaked in NMP solution and IPA solution in turn, the quartz sheet was placed in flowing DI water for cleaning.
[0038] The quartz wafer after the positive photoresist is removed is placed in a first etching solution for etching. The first etching solution is a mixed solution of 40% HF (hydrogen fluoride) and 45% NH4F (ammonium fluoride). The mass ratio of the two solutions is 3:2. The etching is carried out at a constant temperature of 30°C for 40 hours, and then taken out and washed and dried with DI water in turn to obtain a quartz wafer containing a preliminary accelerometer structure. The quartz wafer includes an outer frame 7, an inner frame 14 and a cantilever beam 12, as well as a transverse connecting beam 5 and a vertical connecting beam 1.
[0039] Then, the quartz wafer was subjected to secondary photolithography: the surface of the quartz wafer was sprayed with photoresist in a closed chamber at 80°C, and the thickness of the formed photoresist was 5 μm. After spraying the photoresist, the quartz wafer was placed on a hot plate at 110°C for heat baking for 90 seconds. After the heat baking, the quartz wafer was exposed on both sides by an exposure machine. After exposure, the quartz wafer was placed in a developer for development, and then the pattern on the mask was transferred to the surface of the cured photoresist.
[0040] Step 4: placing the quartz wafer with the accelerometer structure pattern into a first organic etching solution for wet etching to obtain a quartz wafer containing a preliminary accelerometer structure.
[0041] In this step, the first organic etching solution is a mixed solution of 40% HF (hydrogen fluoride), 45% NH4F (ammonium fluoride), and 30% KF (potassium fluoride). The mass ratio of the three solutions is 1:2:1, and the etching is carried out at a constant temperature of 23 °C for 2 hours. Every half an hour, the quartz wafer is pulled up and down for one minute to avoid the deposition of complexes on the etched surface. Then, it is immersed in a low concentration KOH (potassium hydroxide) solution to improve the surface roughness of the quartz wafer.
[0042] Step 5: De-edge the sidewalls on the quartz plate containing the preliminary accelerometer structure.
[0043] Step 6: Spray a 5 μm thick positive photoresist on the upper and lower surfaces of the quartz plate in the thickness direction, and perform double-sided photolithography on the quartz plate to obtain a metal hard mask on the lower surface of the hinge (including the first hinge 6 and the second hinge 11) of the quartz plate in the thickness direction and a metal hard mask on the upper surface of the cantilever beam 12 in the thickness direction.
[0044] The quartz plate is then placed in a second organic etching solution for etching, so that the cantilever beam 12 and the hinge are single-sidedly etched through the metal hard mask on the lower surface and the metal hard mask on the upper surface to obtain the cantilever beam 12 and the hinge.
[0045] The second organic etching solution is a mixed solution of BOE (buffered oxide etching solution) and 45% NH4F, and the mass ratio of the solution is 1:1. The second organic etching solution is intended to eliminate the side edges of the quartz sheet and improve the roughness.
[0046] Step 7: removing the metal film on the surface of the quartz plate, that is, removing the film layers on the upper and lower surfaces of the quartz plate, to obtain an accelerometer, that is, to obtain the integrated resonant quartz accelerometer.
[0047] Figure 3 That is the process flow diagram of step 1 to step 7.
[0048] refer to Figure 4-Figure 7 After obtaining the body-type resonant quartz accelerometer, it is necessary to make electrodes on the surface of the cantilever beam 12 of the quartz accelerometer. The specific implementation process of making the electrodes includes the following steps: Step 81: The upper and lower surfaces of the cantilever beam 12 in the thickness direction are plated by metal sputtering to form a film layer, wherein the film layer includes a gold film layer and a chromium film layer. The film layer includes a chromium film layer and a gold film layer sequentially formed along a direction away from the cantilever beam 12, that is, the chromium film layer is plated first and then the gold film layer is plated. The thickness of the gold film layer is 2000 A, and the thickness of the chromium film layer is 500 A.
[0049] After the film layer is formed, a 5 μm thick positive photoresist is sprayed on the upper and lower surfaces of the cantilever beam 12 , and double-sided photolithography is performed. After passing through a gold etching solution and a chromium etching solution, a metal hard mask is formed on the upper and lower surfaces of the cantilever beam 12 .
[0050] Step 82: Place the quartz sheet forming the metal hard mask of the cantilever beam 12 into the first organic etching solution for etching to obtain a symmetrical groove structure, but do not etch through to ensure that the side wall of the cantilever beam 12 is as steep as possible.
[0051] Step 83 : Repeat step 81 to obtain a new metal hard mask pattern at a position corresponding to the cantilever beam 12 by designing a different metal mask.
[0052] Step 84: Place the quartz wafer with the new metal hard mask pattern into the first organic etching solution again to etch through the portion without the metal hard mask.
[0053] Step 85: Execute step 81 again to obtain a new metal hard mask and deposit metal on the sidewalls of the cantilever beam 12 .
[0054] Step 86: The cantilever beam 12 is subjected to edge trimming by combining dry etching and wet etching.
[0055] Step 87: Spray 5 μm thick positive photoresist on the upper and lower surfaces of the cantilever beam 12 in the thickness direction. After double-sided photolithography, use gold etching solution and chromium etching solution to etch to remove excess metal hard mask, thereby forming electrodes on the upper and lower surfaces of the cantilever beam 12 in the thickness direction.
[0056] It should be noted that Figure 6 The changes brought about by steps 4 and 5 in the above process are substantially the same. In addition, the metal film acts as an etching protection layer during the etching process of the quartz wafer, and the metal film forms an electrode after passing through the metal mask. Figure 5 and Figure 6 The etching of the quartz protective layer and the formation of the electrodes of the quartz accelerometer can be performed simultaneously.
[0057] refer to Figure 4-Figure 6 , Figure 4 Schematic diagram of the electrode structure of the cantilever beam 12. The cantilever beam 12 includes 6 electrodes, which are respectively recorded as the first electrode 501, the second electrode 502, the third electrode 503, the fourth electrode 504, the fifth electrode 505 and the sixth electrode 506. The polarity of the first electrode 501, the third electrode 503 and the fifth electrode 505 is the same, the polarity of the second electrode 502, the fourth electrode 504 and the sixth electrode 506 is the same, and the polarity of the first electrode 501 and the second electrode 502 is opposite. The length of the first electrode 501, the second electrode 502, the third electrode 503 and the fourth electrode 504 is half of that of the fifth electrode 505 and the sixth electrode 506, and they are all located on the upper side of the cantilever beam 12, and the fifth electrode 505 and the sixth electrode 506 are located on the lower side of the cantilever beam 12. The first electrode 501, the third electrode 503 and the fifth electrode 505 are electrically connected, and the second electrode 502, the fourth electrode 504 and the sixth electrode 506 are electrically connected.
[0058] refer to Figure 4 , Figure 10-11 It should be noted that the electrodes of the cantilever beam 12 are mainly distributed on the two side walls of the cantilever beam 12 , and fewer electrodes are distributed on the upper and lower surfaces of the cantilever beam 12 .
[0059] The purpose of dry etching is to remove the edge of the side wall of the cantilever beam 12. Metal chromium can be sputtered on the surface of the quartz plate as a metal hard mask, and C4F8 (octafluorocyclobutane) and SF6 (sulfur hexafluoride) gases are used for etching.
[0060] In an alternative embodiment, Fig.10 The two electrodes (shaded areas) in the upper left corner and the upper right corner are different in size, and the electrode in the upper left corner is larger in size than the electrode in the upper right corner. As another alternative embodiment, the two electrodes in the upper left corner and the upper right corner may also be the same in size, and the effect brought by the two electrodes of the same size is better than the solution corresponding to the two electrodes of different sizes.
[0061] Through the above steps, the accelerometer can be manufactured, and the sidewall electrode patterning process is adopted, so that the electrode pattern is not on the upper surface of the quartz plate, but on the side wall of the cantilever beam 12, so that the width of the cantilever beam 12 of the accelerometer can reach about 30 microns, compared with the traditional 70 μm wide accelerometer, its sensitivity can be increased by about 4 times, and the mechanical stability of the accelerometer is ensured by the corresponding structure of the manufactured quartz accelerometer. In addition, the cantilever beam 12 maintains lateral vibration in the in-plane mode, and the electrode pattern on the side of the cantilever beam 12 is perpendicular to the vibration direction, thereby greatly increasing the electromechanical coupling coefficient.
[0062] The embodiment disclosed in this specification is only an example of a unilateral feature of the present invention, and the protection scope of the present invention is not limited to this embodiment, and any other functionally equivalent embodiments fall within the protection scope of the present invention. For those skilled in the art, various other corresponding changes and deformations can be made according to the technical solutions and concepts described above, and all of these changes and deformations should fall within the protection scope of the claims of the present invention.
Claims
1. A method for manufacturing an integrated resonant quartz accelerometer, characterized in that: The following steps are involved: Step 1: Select a quartz sheet, and sequentially perform acid washing, alkali washing, and DI water washing on the quartz sheet to obtain a treated quartz sheet; Step 2: coating the upper and lower surfaces of the processed quartz sheet in the thickness direction to form a film layer of a preset thickness; Step 3: forming a quartz wafer with a metal hard mask having an accelerometer structure pattern; Step 4: placing the quartz wafer with the metal hard mask into a first organic etching solution for wet etching to obtain a quartz wafer containing a preliminary accelerometer structure; Step 5: Eliminate the sidewalls on the quartz plate containing the preliminary accelerometer structure; Step 6: forming a metal hard mask on the lower surface of the quartz plate in the thickness direction of the hinge and forming a metal hard mask on the upper surface in the thickness direction of the cantilever beam, and then placing the quartz plate in a second organic etching solution for etching to obtain the cantilever beam and the hinge; Step 7: Remove the surface film layer of the quartz plate; Step 8: Make electrodes on the surface of the cantilever beam of the quartz accelerometer to obtain the final quartz accelerometer.
2. The method for manufacturing an integrated resonant quartz accelerometer according to claim 1, characterized in that: In step 2, magnetron sputtering is used for film coating, and the formed film layers include a chromium film layer and a gold film layer formed in sequence in a direction away from the quartz sheet.
3. The method for manufacturing an integrated resonant quartz accelerometer according to claim 1, characterized in that: The specific implementation process of forming a quartz wafer with a metal hard mask having an accelerometer structure pattern includes the following steps: A positive photoresist of a preset thickness is spin-coated on the upper and lower surfaces of the quartz wafer in the thickness direction after the coating, and the preset thickness can be 2-5 μm. Then, the quartz wafer after the coating of the photoresist is sequentially exposed by an exposure machine in double-sided alignment, pre-baked on a hot plate at a temperature of 100°C, developed, and post-baked on a hot plate at a temperature of 107°C. The coating without the photoresist after the development process is etched away with an etching solution, and the etching solution is selected from gold and chromium etching solutions to etch away the gold film layer and the chromium film layer at the corresponding position, so as to form a metal hard mask with an accelerometer pattern on the upper and lower surfaces in the thickness direction of the quartz wafer. Then, the accelerometer pattern on the metal hard mask is transferred to the cured photoresist to obtain a quartz wafer with an accelerometer structure pattern.
4. The method for manufacturing an integrated resonant quartz accelerometer according to claim 3, characterized in that: The gold etching solution uses a solution composed of potassium iodide and iodine ion compounds, and the etching time of the gold etching solution is 30 s. The chromium etching solution uses a mixed solution of cerium ammonium nitrate, and the etching time is 60 s.
5. The method for manufacturing an integrated resonant quartz accelerometer according to claim 3 or 4, characterized in that: During the etching process, a quartz wafer is loaded on a crystal boat and placed in a gold etching solution and a chromium etching solution at 22°C to remove the coating in the area not covered by the photoresist, and an interval is set according to the concentration of the etching solution. The quartz wafer is pulled up and down at intervals. After etching, the dried quartz wafer is immersed in an N-methylpyrrolidone solution for a first preset time, and then immersed in an IPA solution for a second preset time to remove the surface cured positive photoresist. Then, the quartz wafer is placed in flowing DI water for cleaning. The quartz plate after the positive photoresist is removed is placed in the first etching solution for etching. The first etching solution is a mixed solution of 40% HF and 45% NH4F. The mass ratio of the two solutions is 3:
2. The etching is carried out at a constant temperature of 30 °C for 40 hours, and then taken out and washed with DI water and dried in turn to obtain a quartz plate containing a preliminary accelerometer structure. Then, the quartz wafer was subjected to secondary photolithography: photoresist was sprayed on the surface of the quartz wafer in a closed chamber at 80 °C, and the thickness of the formed photoresist was 5 μm. After spraying the photoresist, the quartz wafer was placed on a hot plate at a temperature of 110 °C for heat baking for 90 s. After the heat baking, the quartz wafer was double-sided exposed using an exposure machine. After exposure, the quartz wafer was placed in a developer for development, and then the pattern on the mask was transferred to the surface of the solidified photoresist.
6. The method for manufacturing an integrated resonant quartz accelerometer according to claim 1, characterized in that: In step 4, the first organic etching solution is a mixed solution of 40% HF, 45% NH4F, and 30% KF. The mass ratio of the three solutions is 1:2:1, and the etching is carried out at a constant temperature of 23°C for 2 hours. Every half an hour, the quartz plate is pulled up and down for one minute, and then immersed in a low concentration KOH solution.
7. The method for manufacturing an integrated resonant quartz accelerometer according to claim 1, characterized in that: In step 6, the second organic etching solution is a mixed solution composed of BOE and 45% NH4F, and the ratio of the solutions is 1:1 by mass ratio.
8. The method for manufacturing an integrated resonant quartz accelerometer according to claim 1, characterized in that: The specific implementation process of making electrodes includes the following steps: Step 81: coating the cantilever beam to form a film layer, wherein the film layer includes a gold film layer and a chromium film layer, and the film layer includes a chromium film layer and a gold film layer sequentially formed in a direction away from the cantilever beam. After the film layer is formed, a 5 μm thick positive photoresist is sprayed on the upper and lower surfaces of the cantilever beam, and double-sided photolithography is performed. After passing through a gold etching solution and a chromium etching solution, a metal hard mask is formed on the upper and lower surfaces of the cantilever beam; Step 82: placing the quartz sheet forming the metal hard mask of the cantilever beam into a first organic etching solution for etching to obtain a symmetrical groove structure; Step 83: Repeat step 81 to obtain a new metal hard mask pattern at a position corresponding to the cantilever beam by designing a different metal mask; Step 84: placing the quartz wafer with the new metal hard mask pattern into the first organic etching solution again, and etching through the portion without the metal hard mask; Step 85: Execute step 81 again to obtain a new metal hard mask, and deposit metal on the sidewall of the cantilever beam 12; Step 86: using a combination of dry etching and wet etching to trim the cantilever beam; Step 87: Spray 5 μm thick positive photoresist on the upper and lower surfaces of the cantilever beam in the thickness direction. After double-sided photolithography, use gold etching solution and chromium etching solution to etch to remove excess metal hard mask, thereby forming electrodes on the upper and lower surfaces of the cantilever beam in the thickness direction.
9. The method for manufacturing an integrated resonant quartz accelerometer according to claim 8, characterized in that: The cantilever beam includes 6 electrodes, which are respectively recorded as the first electrode, the second electrode, the third electrode, the fourth electrode, the fifth electrode and the sixth electrode. The first electrode, the third electrode and the fifth electrode have the same polarity, the second electrode, the fourth electrode and the sixth electrode have the same polarity, the first electrode and the second electrode have opposite polarity, the length of the first electrode, the second electrode, the third electrode and the fourth electrode is half of the fifth electrode and the sixth electrode, and they are all located on the upper side of the cantilever beam, the fifth electrode and the sixth electrode are located on the lower side of the cantilever beam, the first electrode and the third electrode are electrically connected, the third electrode and the fourth electrode are electrically connected, the fourth electrode is electrically connected to the second electrode and the fifth electrode respectively, and the second electrode is electrically connected to the sixth electrode.
10. The method for manufacturing an integrated resonant quartz accelerometer according to claim 8, characterized in that: In step 1, a quartz sheet with a thickness of 120 μm is selected, in step 2, the thickness of the gold film layer is 1000 A, the thickness of the chromium film layer is 400 A, and in step 81, the thickness of the gold film layer is 2000 A, and the thickness of the chromium film layer is 500 A.
Citation Information
Patent Citations
Capacitive acceleration transducer for bending elastic beam and manufacturing method
CN102879608A
Integrated quartz double-vibrating-beam accelerometer and preparation method
CN109254170A
Manufacturing method of monocrystalline silicon pendulous reed
CN109580986A
Processing method of integrated quartz vibrating beam side electrode
CN111943131A
Processing method and device of quartz crystal resonator
CN113452335A
Cited By
High-performance quartz vibrating beam accelerometer and preparation method thereof