Special compound emulsifier for emulsion explosive and preparation method of special compound emulsifier

By esterification reaction of sodium rosinate and Sipan-80 to form a modified Sipan-80 composite emulsifier, the problems of poor storage stability and insufficient emulsification capacity of emulsified explosives are solved, and the blasting performance and storage stability of emulsified explosives are significantly improved. sex.

CN119019207APending Publication Date: 2024-11-26JIANGXI GUOTAI LONGSHI TECH CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411107519.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-13
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

Commonly used emulsifiers such as sp-80 in existing emulsifying explosives have poor storage stability, while polyisobutylene succinic anhydride derivatives have weak emulsification capabilities, making it difficult to meet the needs of blasting performance and storage stability.

Method used

By esterifying sodium rosinate with multiple hydroxy sites of Sipan-80, a modified anionic carboxylate emulsifier is generated to form a high molecular weight modified Sipan-80 composite emulsifier for preparation Emulsified explosives.

Benefits of technology

The emulsifier of modified Sipan-80 improves the explosion performance and storage stability of emulsified explosives, the space volume of the lipophilic groups increases, and the interface film is closer, which significantly improves the performance of emulsified explosives.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0004991238730000041
    Figure BDA0004991238730000041
Patent Text Reader

Abstract

The invention discloses a special composite emulsifier for preparing emulsion explosives, which is a modified span-80 composite emulsifier obtained after an anionic carboxylate emulsifier and a plurality of hydroxyl sites of span-80 are subjected to esterification reaction, and the composite emulsifier has high molecular weight, so that the space volume of a lipophilic group is increased; an interfacial film is tighter, so that the blasting performance and the storage stability of the emulsion explosive are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of emulsion explosives, in particular to a special composite emulsifier for emulsion explosives. Background Art

[0002] Emulsion explosive is a mixed explosive, usually formed by uniformly dispersing an inorganic oxidant salt solution in an oil-phase continuous medium of porous materials such as bubbles or hollow glass microspheres under the action of an emulsifier to form an oil-in-water emulsion explosive. The components of emulsion explosives include: oxidant, combustible agent, emulsifier, sensitizer, foaming agent, stabilizer, etc. Among them, the role of the emulsifier is to prevent coagulation and reduce interfacial tension, which is essential for stabilizing the emulsified system.

[0003] At present, the most widely used in emulsion explosives are sp-80 (Span-80) and polyisobutylene succinic anhydride derivatives. The scientific name of sp-80 is sorbitan monooleate, which is a low molecular non-ionic surfactant. It is difficult to dissolve in water, but easily soluble in hot oil and organic solvents. The emulsion explosives prepared by it have poor storage stability. Polyisobutylene succinic anhydride derivatives have high molecular weight and can improve the stability of emulsion explosives to a certain extent, but have poor emulsification ability and weak emulsification ability.

[0004] Therefore, a new emulsifier is needed to improve the blasting performance and storage stability of emulsion explosives. Summary of the invention

[0005] In view of the above defects, the present invention provides a special composite emulsifier for preparing emulsion explosives, which comprises modified Span-80. The emulsion explosive prepared by the special composite emulsifier of the present invention has good blasting performance and storage stability.

[0006] One object of the present invention is to provide a composite emulsifier for preparing emulsion explosives, wherein the composite emulsifier is a composite emulsifier of modified Span-80 obtained by esterification reaction of anionic carboxylate emulsifier with multiple hydroxyl sites of Span-80.

[0007] Specifically, the anionic carboxylate emulsifier is sodium rosinate.

[0008] Another object of the present invention is to provide a method for preparing a special composite emulsifier for emulsion explosives, which specifically comprises the following steps:

[0009] Sodium rosinate was selected as an anionic carboxylate emulsifier to carry out esterification with multiple hydroxyl sites of nonionic surfactant Span-80 to generate modified Span-80.

[0010] Specifically, sodium rosinate and Span-80 in a molar mass ratio of 1-5:1 are weighed and heated at 60-80° C. for 6-8 hours under the catalysis of 98% concentrated sulfuric acid to obtain modified Span-80.

[0011] The beneficial technical effects of the present invention are as follows:

[0012] The traditional emulsifier Span-80 is a low molecular nonionic surfactant, which is difficult to dissolve in water, but easily soluble in hot oil and organic solvents. The emulsion explosive prepared by the emulsion explosive has poor storage stability. The present invention obtains a high molecular weight modified Span-80 by esterification reaction between anionic carboxylate emulsifier (sodium rosin acid) and multiple hydroxyl sites of Span-80. The composite emulsifier containing modified Span-80 increases the spatial volume of the lipophilic group and makes the interface film more compact, thereby improving the blasting performance and storage stability of the emulsion explosive. DETAILED DESCRIPTION

[0013] The embodiments of the present invention are described in detail below. The following embodiments are implemented on the premise of the technical solution of the present invention, and detailed implementation methods and specific operation processes are given, but the protection scope of the present invention is not limited to the following embodiments.

[0014] Example 1: Composite emulsifier 1 for emulsion explosives

[0015] Sodium rosinate and Span-80 in a molar mass ratio of 1:1 were weighed and heated at 60° C. for 8 h under the catalysis of 98% concentrated sulfuric acid to obtain modified Span-80.

[0016] Example 2: Composite emulsifier 2 for emulsion explosives

[0017] Sodium rosinate and Span-80 were weighed in a molar mass ratio of 2:1 and heated at 60° C. for 8 h under the catalysis of 98% concentrated sulfuric acid to obtain modified Span-80.

[0018] Example 3: Composite emulsifier 3 for emulsion explosives

[0019] Sodium rosinate and Span-80 were weighed in a molar mass ratio of 3:1 and heated at 60° C. for 8 h under the catalysis of 98% concentrated sulfuric acid to obtain modified Span-80.

[0020] Example 4: Composite emulsifier 4 for emulsion explosives

[0021] Sodium rosinate and Span-80 were weighed in a molar mass ratio of 4:1 and heated at 60° C. for 8 h under the catalysis of 98% concentrated sulfuric acid to obtain modified Span-80.

[0022] Example 5: Composite emulsifier 5 for emulsion explosives

[0023] Sodium rosinate and Span-80 were weighed in a molar mass ratio of 5:1 and heated at 60° C. for 8 h under the catalysis of 98% concentrated sulfuric acid to obtain modified Span-80.

[0024] Example 6: Performance Test

[0025] The above-mentioned composite emulsifier 1-5 for emulsion explosive, the emulsifier maleic acid sorbitan monooleate (Span-80 modified by maleic anhydride) of comparative example 1 and Span-80 of comparative example 2 are respectively used to prepare emulsion explosives. The specific preparation method is:

[0026] (1) Preparation of aqueous phase: 8 parts of water by mass are injected into the tank and steam-pressurized until the temperature is maintained at 100° C. and the steam pressure is maintained at 0.5 MPa; 7 parts of calcium nitrate by mass are first added to the tank and stirred to dissolve, and then 78 parts of ammonium nitrate by mass are added and stirred at 100° C. to dissolve; wherein the ammonium nitrate is an aqueous solution of ammonium nitrate with a mass content of 90%; the concentration of calcium nitrate is 30%;

[0027] (2) Preparation of oil phase: 2.5 parts by weight of composite wax and 2.2 parts by weight of composite emulsifier 1-5, maleic acid sorbitan monooleate and Span are mixed, stirred continuously and dissolved; wherein composite emulsifier 1-5 is a composite emulsifier of modified Span-80 obtained by esterification reaction of anionic carboxylate emulsifier with multiple hydroxyl sites of Span-80; the specific preparation method of the composite emulsifier is to weigh sodium rosinate and Span-80 in a molar mass ratio of 1-5:1, heat at 60°C for 8h under the catalysis of concentrated sulfuric acid to obtain a modified Span-80. Span-80, maleic acid sorbitan monooleate is obtained by modifying Span-80 with maleic anhydride. The specific method is: take a certain amount of maleic anhydride and solvent xylene, mix them, add an appropriate amount of catalyst toluenesulfonic acid, heat the components to 80°C, stir and react until all the water is removed, then gradually and slowly add Span-80, continue to heat to 140°C until the acid value remains unchanged, stop the reaction, and rotary evaporate the solvent to obtain maleic acid sorbitan monooleate, the molar mass ratio of maleic anhydride to Span-80 is 1:2;

[0028] (3) Emulsification and sensitization: The water phase and the oil phase are mixed in a ratio of 9:1 for emulsification, and then cooled and transferred into a sensitizer. A traditional foaming agent with a mass fraction of 0.4 parts is added and sprayed evenly. The mixture is stirred and sensitized in the upper and lower layers of the sensitizer, and finally loaded and packaged. The components of the traditional foaming agent include sodium nitrite: 10%, phosphoric acid: 10%, urea: 5%, and water: 75%.

[0029] The performance test of the prepared colloidal emulsion explosive was carried out, and the results are shown in the following table:

[0030]

[0031] By comparing Examples 1-5 with Comparative Examples 1-2, it can be seen that the modification of the polyhydroxyl sites of Span-80 by esterification reaction in the present invention has better storage stability and blasting performance. The reason is that the modified Span-80 increases the spatial volume of the lipophilic groups and makes the interface film tighter, thereby improving the blasting performance and storage stability of the emulsion explosive.

[0032] By carrying out esterification reaction of sodium rosin acid and Span-80 with different molar mass ratios, it was found that the larger the molar mass ratio, the better the blasting performance and storage stability of the emulsion explosive. The reason for this may be that the remaining sodium rosin acid as an anionic carboxylate emulsifier and the modified Span-80 form a composite emulsifier, which improves the emulsification properties to a certain extent, thereby greatly improving the blasting performance and storage stability of the emulsion explosive.

[0033] The present invention is not limited to the above embodiments. For those skilled in the art, several improvements can be made without departing from the principle of the present invention, and these improvements are also considered to be within the scope of protection of the present invention. The preparation of emulsion explosives in this specification is a prior art known to professional and technical personnel in the field, and no further elaboration is given here.

Claims

1. A composite emulsifier for preparing emulsion explosives, It is characterized in that The composite emulsifier is a composite emulsifier of modified Span-80 obtained by esterification reaction between anionic carboxylate emulsifier and multiple hydroxyl sites of Span-80.

2. The composite emulsifier according to claim 1, It is characterized in that The anionic carboxylate emulsifier is sodium rosinate.

3. A method for preparing the composite emulsifier according to claim 1, It is characterized in that The method comprises the following steps: weighing sodium rosinate and Span-80 in a molar mass ratio of 1-5:1 respectively, heating at 60-80°C for 6-8h under the catalysis of 98% concentrated sulfuric acid to obtain modified Span-80.

4. Use of the composite emulsifier according to claim 1, It is characterized in that Used in the preparation of emulsion explosives.

Citation Information

Patent Citations

  • Polymerizable emulsifier propylene acyloxy Span 80 as well as preparation method and uses thereof

    CN101182273A

  • Composite emulsifier for emulsion explosive

    CN117209339A

  • Colloidal emulsion explosive with high storage stability and preparation method thereof

    CN119591459A

  • Emulsified detonator and method for preparing same

    CN1594243A