Method for integrally regulating and controlling morphology, size and purity of TATB prepared by chlorine-free process

Through the composite system dissolution and recrystallization technology, the morphology, size and purity of TATB are regulated, and the problems of low purity and irregular morphology in the preparation of chlorine-free TATB are solved, and the preparation of TATB with high purity and diverse particle sizes is achieved. Different application requirements.

CN119019259APending Publication Date: 2024-11-26INST OF CHEM MATERIAL CHINA ACADEMY OF ENG PHYSICS +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411011583.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-26
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

The existing chlorine-free TATB preparation process has problems such as low purity, irregular morphology and single size specifications, which are difficult to meet the needs of different application scenarios.

Method used

The composite system is used to dissolve and recrystallize TATB. By regulating the stirring rate, time and temperature, combined with appropriate solvents and crystal form control agents, the integrated regulation of TATB morphology, size and purity is achieved, and a high-purity spherical shape is prepared. TATB crystal.

Benefits of technology

The diffusion and bulk density of TATB are improved, with a purity of 99.3%-99.8%, and the particle size can be controlled within the range of 100nm-80μm according to the requirements, meeting the needs of different application scenarios.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119019259A_ABST
    Figure CN119019259A_ABST
Patent Text Reader

Abstract

The invention discloses a method for integrally regulating and controlling morphology, size and purity of TATB prepared by a chlorine-free process, which comprises the following steps: step 1, dissolving TATB: dissolving TATB in a solvent A, adding a crystal form control agent, heating and stirring to obtain a TATB solution; step 2, recrystallization of TATB: continuously dropwise adding a solvent B into the TATB solution, and controlling the temperature for stirring or ultrasonic treatment; and step 3, growth and post-treatment of TATB: continuously stirring the solution in the step 2 at a certain temperature to enable the crystal to grow for a period of time, filtering, washing and drying to obtain the recrystallized TATB crystal. The obtained TATB crystal is controllable in morphology and size, round and full in form, smooth in surface and good in free-running property, and the particle size can be regulated and controlled within the range of 100 nanometers to 80 micrometers; the purity is relatively high and can reach 99.8%. The method is simple in process, easy to control, safe and reliable, and provides a new thought for preparation of high-quality TATB.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of energetic material crystal form and purity control, and in particular to a method for integrated control of the morphology, size and purity of chlorine-free TATB. Background Art

[0002] 1,3,5-Triamino-2,4,6-trinitrobenzene (TATB) is a typical insensitive explosive with high crystal density, good thermal stability and insensitivity to mechanical stimulation. It is the most important insensitive explosive at present. So far, it is the only single-element insensitive explosive approved by the Explosive Safety Committee of the U.S. Department of Energy. The excellent thermal stability and low sensitivity determine that TATB is valued in civil and military fields and is increasingly widely used in this field. In civil applications, TATB is used to prepare raw materials for deep well perforating bullets and liquid crystal displays; in military applications, TATB can be used as a main explosive to prepare low-vulnerability explosives for modern weapons, aerospace and nuclear weapons. For example, the Livermore National Laboratory and the Los Alamos National Laboratory in the United States have developed the main explosive formulas LX-17 and PBX-9502 based on TATB, respectively, and have also developed the formulas PBXN-7 and PBXW-14 based on ultrafine TATB and compounding as insensitive boosters for nuclear weapons.

[0003] The preparation process of TATB can be divided into two categories: one is the chlorine-containing preparation process. The common synthesis route is to use 1,3,5-trichlorobenzene (TCB) as the starting material and obtain it through nitration and ammoniation. This process is relatively mature, with large output and suitable for large-scale industrial production. However, the product has a high content of chlorine impurities. A large number of application studies have found that chlorine-containing impurities will have serious adverse effects on the performance, application, long-term storage and aging of TATB, especially when the inorganic impurity NH4Cl accounts for more than 80% of the total impurity content, TATB will become black and rough, reducing the overall yield and changing the crystal surface morphology of TATB.

[0004] The other is the chlorine-free preparation process. Due to the influence of chlorine-containing impurities on the performance of TATB, the synthesis route of chlorine-free TATB has become a hot topic of research. In order to solve the influence of chlorine-containing impurities, scientific researchers have conducted a lot of research on methods to reduce chlorine-containing impurities in TATB. The most effective method is to use chlorine-free substances as raw materials and develop a synthesis process route for chlorine-free TATB. However, the existing chlorine-free TATB preparation process has some disadvantages, such as low purity (generally less than 97.5%), irregular morphology, and single size specifications.

[0005] Purity is an important indicator for testing the quality of explosives, which directly affects the performance of explosives such as detonation velocity, detonation heat, detonation pressure and thermal stability. When chlorine-containing TATB is used in the formulation, the trace amount of chlorine contained in it is easy to cause metal corrosion during the long-term storage and aging process of the material (Explosives, 1985(01):48-49), and may cause changes in compatibility and safety, affecting the normal storage, service and use of weapons. In addition, the use of chlorine-containing TATB in propellants may also increase the characteristic signal value. Gao Dayuan et al. studied the adiabatic decomposition characteristics of TATB and two chlorine-containing impurities. The results showed that the thermal decomposition temperature, rate and heat release of chlorine-containing impurities were very different from those of TATB. TATB only had one heat release process with a high initial heat release temperature and a fast heat release rate, while chlorine-containing impurities had multiple heat release processes, and the heat release each time was very small. Therefore, reducing or removing the chlorine content in TATB products is of great significance to improving the quality of TATB (Explosion and Shock, 2004, 24(1):69-74).

[0006] TATB molecules have extremely strong hydrogen bonds, which makes it easy for TATB to form irregular flake crystals with many defects. This kind of crystals are prone to a certain degree of orientation during the process of pressing and forming or even long-term storage, which leads to the separation of TATB from the binder, serious deformation of TATB-based explosives, and significant changes in performance, and even seriously reduces the reliability of weapons. The crystal shape of TATB has a certain influence on its sensitivity, detonation and other properties. Spherical TATB is superior to ordinary irregular TATB in terms of column forming, fluidity, and bulk density. In addition, spherical TATB has a higher surface area to volume ratio, better free flow characteristics, and higher bulk density. Preparing it into a mixed explosive can greatly increase the charge density and thus improve the detonation performance of the charge. Therefore, the preparation of spherical TATB is of great significance.

[0007] At present, in order to improve the crystal quality of TATB, domestic and foreign experts have conducted a lot of research on the morphology and application of TATB crystals (Journal of Explosives and Propellants, 2015, 38(5):1-9), and the method used is mainly recrystallization. Recrystallization is a good way to change the crystal morphology. Applying recrystallization to explosives can greatly improve the crystal quality and performance of explosives, so that explosives can meet different usage requirements. Recrystallization can also change the size of explosives, improve the packing density of explosives, the compatibility of other components, detonation performance and safety performance, etc. Foltz et al. used DMSO to recrystallize TATB to obtain large particles of TATB (size of 15um-246um). The study found that the cooling rate and stirring speed have a great influence on the morphology and particle size of TATB crystals, and the mother liquor of DMSO recrystallized TATB can be recycled to obtain TATB crystals with more regular shapes and fewer defects. Zhang Haobin et al. used the solvent-nonsolvent method to recrystallize TATB. By controlling the crystallization conditions such as solution saturation, stirring speed, anti-solvent addition amount, cooling speed, etc., several TATB crystals with different morphologies were obtained. It was found that the anti-solvent type, stirring speed, and anti-solvent addition amount all had a great influence on the morphology of TATB crystals (China Academy of Engineering Physics, 2011). Yang Guangcheng used concentrated sulfuric acid as solvent and water as anti-solvent to prepare nano-scale TATB crystals through solvent-non-solvent recrystallization method, but the particle diameter was small, the surface energy was high, and there was a serious agglomeration phenomenon.

[0008] TATB crystals with different crystal morphologies, purities, and sizes have different application scenarios, but the commonly used recrystallization methods are difficult to meet the needs of various application scenarios. Due to the strong hydrogen bonding between TATB molecules, TATB has high stability and is basically insoluble in all organic solvents at room temperature. It is challenging to use recrystallization methods to regulate the single field of TATB crystal morphology, size, or purity. Therefore, developing a method for integrated regulation of the morphology, size, and purity of chlorine-free TATB to meet application requirements is an urgent problem to be solved in this field. Summary of the invention

[0009] An object of the present invention is to solve at least the above problems and / or disadvantages and to provide at least the advantages which will be described hereinafter.

[0010] In order to achieve these purposes and other advantages according to the present invention, a method for integrated control of the morphology, size and purity of TATB prepared by a chlorine-free process is provided, comprising the following steps:

[0011] Step 1: Dissolving TATB: dissolving TATB in solvent A, adding a crystal control agent, heating and stirring to obtain a TATB solution;

[0012] Step 2: Recrystallization of TATB: continuously add solvent B dropwise into the above TATB solution, control the temperature and stir or perform ultrasound;

[0013] Step 3: Growth and post-treatment of TATB: The solution of step 2 is continuously stirred at a certain temperature to allow the crystals to grow for a period of time, and then filtered, washed and dried to obtain recrystallized TATB crystals.

[0014] Preferably, the solvent A is one or more of 1-butyl-3-methylimidazolium chloride / dimethyl sulfoxide, 1-butyl-3-methylimidazolium chloride / acetone, 1-butyl-3-methylimidazolium chloride / ethyl acetate, zinc chloride / dimethylformamide, N-methylmorpholine-N-oxide / dimethyl sulfoxide, N-methylmorpholine-N-oxide / acetone, N-methylmorpholine-N-oxide / ethyl acetate, pyrrole sulfate / tetrahydrofuran, tetrahydrofuran / dimethyl sulfoxide, tetrahydrofuran / acetone, tetrahydrofuran / ethyl acetate, N-methylpyrrolidone / pyrrole sulfate / dimethyl sulfoxide.

[0015] Preferably, the solvent B is one or more of distilled water, ethanol, n-butanol, isopropanol, ethyl acetate, butyl acetate, isoamyl acetate, acetic acid, propionic acid, dichloromethane, chloroform, carbon tetrachloride, ethylene dichloride, ether, petroleum ether, n-butane, and cyclohexane.

[0016] Preferably, the crystal form controlling agent is one or more of polyvinyl alcohol, polyethylene glycol, gelatin, sodium dodecylbenzene sulfonate, cetylpyridine, sodium dodecyl sulfate, sodium cetyl sulfate, sodium octadecyl sulfate, dioctane sodium sulfosuccinate, polyvinyl pyrrolidone, Span 20-80, and Tween 20-80.

[0017] Preferably, the gelatin is used after being modified. The preparation method of the modified gelatin is as follows: 3-15g of gelatin is added to 5-25g of deionized water, heated to 70-85°C, stirred to dissolve, then 0.1-0.3g of urea and 0.1-0.3g of sodium citrate are added, and the mixture is stirred at 70-85°C for 1-3 hours. The obtained product is dried, 2-5g of the dried product and 0.5-2g of polyvinyl alcohol are added to a supercritical carbon dioxide reactor, 25-35MPa CO2 is charged, the temperature is raised to 60-70°C to form supercritical carbon dioxide, the two materials are swelled and reacted in the supercritical carbon dioxide solvent for 0.5-2 hours, and then the exhaust valve of the supercritical carbon dioxide reactor is opened to quickly discharge CO2 to reduce the pressure in the reactor to normal pressure, thereby obtaining the modified gelatin.

[0018] Preferably, the mass volume ratio of the TATB to the solvent A is 0.1-1.5 g:30 mL; the mass volume ratio of the TATB to the solvent B is 0.1-1.5 g:100 mL.

[0019] Preferably, the added amount of the crystal form control agent is 0.01%-1% of the total mass of TATB.

[0020] Preferably, the stirring method is mechanical stirring or ultrasonic stirring.

[0021] Preferably, the temperature range of the heating and stirring in the step 1 is 25 to 150°C; the temperature range of the temperature-controlled stirring in the step 2 is 25 to 150°C; and the temperature range of continuing stirring at a certain temperature in the step 3 is 25 to 150°C.

[0022] Preferably, the stirring rate is 50 r / min-1500 r / min.

[0023] Preferably, in the step 2, the stirring time ranges from 0.5 to 8 hours, and in the step 3, the stirring time ranges from 0.5 to 8 hours.

[0024] The present invention at least includes the following beneficial effects: the present invention selects a suitable composite system to dissolve TATB, solves the problem of low solubility of TATB, and increases the fluidity, bulk density and other properties of TATB; the present invention spheroidizes TATB to obtain spherical TATB, regulates the size of TATB to obtain TATB with a size within 100nm-80μm, and purifies TATB with a purity of 99.3%-99.8%.

[0025] Other advantages, objectives and features of the present invention will be embodied in part through the following description, and in part will be understood by those skilled in the art through study and practice of the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 This is the scanning electron microscope image of the raw material TATB;

[0027] Figure 2 This is a scanning electron microscope image of the spherical TATB prepared in Example 1 of the present invention;

[0028] Figure 3 is the particle size distribution diagram of raw material TATB;

[0029] Figure 4 This is a particle size distribution diagram of the spherical TATB prepared in Example 1 of the present invention;

[0030] Figure 5 This is the XRD pattern of the spherical TATB prepared in Example 5 of the present invention;

[0031] Figure 6 The bulk density test diagram of the raw material TATB of the present invention;

[0032] Figure 7 The bulk density test graph of TATB obtained in Example 1 of the present invention;

[0033] Figure 8 The flowability test diagram of the raw material TATB of the present invention;

[0034] Fig. 9 The flowability test chart of TATB obtained in Example 1 of the present invention. DETAILED DESCRIPTION

[0035] The present invention is further described in detail below in conjunction with the accompanying drawings so that those skilled in the art can implement the invention with reference to the description.

[0036] It should be understood that terms such as “having”, “including” and “comprising” used herein do not specify the existence or addition of one or more other elements or combinations thereof.

[0037] The TATB of the present invention has a high stability due to the strong hydrogen bonds within and between molecules. It is basically insoluble in all single organic solvents at room temperature. It is challenging to regulate the single field of TATB crystal morphology, size or purity by recrystallization method. Conventional recrystallization methods need to consider the solubility of TATB, and on this basis, modify the morphology, size or purity of TATB in one aspect. In terms of the regulation method, the present invention selects a suitable composite system to dissolve TATB, which solves the problem of low solubility of TATB. At the same time, by regulating the stirring rate and stirring time in step two and step three, the size of TATB can be changed (increasing the stirring rate and shortening the stirring time can obtain a smaller TATB; conversely, reducing the stirring rate and increasing the stirring time to make the crystal grow, a larger TATB can be obtained). The morphology of TATB is spherical, which is caused by the precipitation of TATB through the solvent-non-solvent system during the recrystallization process. At the same time, the purity of TATB will also be improved through the process of the present invention. The present invention can improve the morphology, size and purity of TATB at the same time through one process, and can prepare spherical high-purity TATB of different sizes to meet application requirements.

[0038] Embodiment 1:

[0039] Step 1, dissolving TATB: dissolving 0.5 g of TATB (purity 97.8%) prepared by a chlorine-free process in 30 ml of a mixed solvent of 1-butyl-3-methylimidazolium chloride / dimethyl sulfoxide (the mixed solvent is prepared by dissolving 10 g of 1-butyl-3-methylimidazolium chloride in 30 ml of dimethyl sulfoxide), adding 0.001 g of polyvinyl alcohol, and stirring at 80° C. until TATB is dissolved to obtain a TATB solution;

[0040] Step 2: Recrystallization of TATB: 100 ml of distilled water was continuously added dropwise to the above solution, and stirred at 50°C for 2 h at a stirring speed of 300 r / min;

[0041] Step 3: Growth and post-treatment of TATB: The solution of step 2 is stirred at 80° C. for 3 h, filtered, washed and dried to obtain recrystallized TATB crystals.

[0042] The prepared TATB crystals were tested and the median particle size of TATB was 20 μm, the crystals were round, and the purity was 99.5%.

[0043] 0.6 g of TATB prepared by the chlorine-free process and 0.6 g of TATB obtained in this example were placed in test tubes of the same size and compacted by vibration. The upper surfaces were flat and no longer sagged. The heights of the TATB prepared by the chlorine-free process and the TATB obtained in this example were measured respectively. Figure 6 and Figure 7 It can be seen that the height of TATB obtained in this example in the test tube is about 0.8 cm ( Figure 7 ), which is significantly lower than TATB prepared by chlorine-free process ( Figure 6 , height about 1.1 cm), indicating that the TATB prepared in this example has a larger compaction density.

[0044] The repose angle method was used to measure the repose angles of 0.6 g of TATB prepared by the chlorine-free process and 0.6 g of TATB prepared in this example. Figure 8 It can be seen that the repose angle of TATB prepared by the chlorine-free process is 47.1°, while the repose angle of TATB prepared in this example is 38.3°, which is significantly lower than the repose angle of TATB prepared by the chlorine-free process, indicating that the TATB obtained by the method of the present invention has higher fluidity.

[0045] Embodiment 2:

[0046] Step 1, dissolving TATB: dissolving 0.5 g of TATB (purity 97.8%) prepared by a chlorine-free process in 30 ml of a mixed solvent of N-methylmorpholine-N-oxide (NMMO) / dimethylformamide (the mixed solvent is prepared by dissolving 10 g of N-methylmorpholine-N-oxide in 30 ml of dimethylformamide), adding 0.001 g of polyvinyl alcohol, and stirring at 80° C. until TATB is dissolved to obtain a TATB solution;

[0047] Step 2: Recrystallization of TATB: 100 ml of ethanol was continuously added dropwise into the above solution, and stirred at 30°C for 1 hour at a stirring speed of 300 r / min;

[0048] Step 3: Growth and post-treatment of TATB: The solution of step 2 is stirred at 30° C. for 4 h, filtered, washed and dried to obtain recrystallized TATB crystals.

[0049] The prepared TATB crystals were tested and the median particle size of TATB was 28 μm, the crystals were round and the purity was 99.7%.

[0050] Embodiment 3:

[0051] Step 1, dissolving TATB: dissolving 0.5 g of TATB (purity 97.8%) prepared by a chlorine-free process in 30 ml of a mixed solvent of N-methylmorpholine-N-oxide / dimethyl sulfoxide (the mixed solvent is prepared by dissolving 10 g of N-methylmorpholine-N-oxide in 30 ml of dimethyl sulfoxide), adding 0.001 g of gelatin, and stirring at 80° C. until TATB is dissolved to obtain a TATB solution;

[0052] Step 2: Recrystallization of TATB: 100 mL of ethyl acetate was continuously added dropwise into the above solution, and stirred at 30°C for 2 h at a stirring speed of 200 r / min;

[0053] Step 3: Growth and post-treatment of TATB: The solution of step 2 is stirred at 30° C. for 4 h, filtered, washed and dried to obtain recrystallized TATB crystals.

[0054] The prepared TATB crystals were tested and the median particle size of TATB was 30 μm, the crystals were round and the purity was 99.4%.

[0055] 0.6 g of TATB obtained in this example was tested for bulk density and fluidity. The height of the TATB obtained in this example in the test tube was about 0.85 cm. The angle of repose of the TATB prepared in this example was 38.5°.

[0056] Embodiment 4:

[0057] Step 1, dissolving TATB: dissolving 1.0 g of TATB (purity 97.8%) prepared by a chlorine-free process in 30 ml of a pyrrole sulfate / tetrahydrofuran mixed solvent (the mixed solvent is prepared by dissolving 10 g of pyrrole sulfate in 30 ml of tetrahydrofuran), adding 0.001 g of polyvinyl pyrrolidone, and stirring at 80° C. until TATB is dissolved to obtain a TATB solution;

[0058] Step 2: Recrystallization of TATB: 100 mL of distilled water was continuously added dropwise to the above solution, and stirred at 50°C for 1 h at a stirring speed of 50 r / min;

[0059] Step 3: Growth and post-treatment of TATB: The solution of step 2 was stirred at 30° C. for 8 h, filtered, washed and dried to obtain recrystallized TATB crystals.

[0060] The prepared TATB crystals were tested and the TATB particle size was 58 μm, the crystals were round and the purity was 99.5%.

[0061] Embodiment 5:

[0062] Step 1, dissolving TATB: dissolving 0.5 g of TATB (purity 97.8%) prepared by a chlorine-free process in 30 ml of a mixed solvent of N-methylpyrrolidone / pyrrole sulfate / dimethyl sulfoxide (the mixed solvent is prepared by dissolving 5 g of N-methylpyrrolidone and 5 g of pyrrole sulfate in 30 ml of dimethyl sulfoxide), adding 0.001 g of hexadecylpyridine, and stirring at 80° C. until TATB is dissolved to obtain a TATB solution;

[0063] Step 2: Recrystallization of TATB: 100 mL of dichloromethane was continuously added dropwise to the above solution, and stirred at 50°C for 1 h at a stirring speed of 1000 r / min;

[0064] Step 3. Growth and post-treatment of TATB: The solution of step 2 was stirred at 50° C. for 1 h, filtered, washed and dried to obtain recrystallized TATB crystals.

[0065] The prepared TATB crystals were tested and the median particle size of TATB was 6 μm, the crystals were round and the purity was 99.7%.

[0066] Embodiment 6:

[0067] Step 1, dissolving TATB: dissolving 0.5 g of TATB (purity 97.8%) prepared by a chlorine-free process in 30 ml of a pyrrole sulfate / tetrahydrofuran mixed solvent (preparation method of the mixed solvent: dissolving 10 g of pyrrole sulfate in 30 ml of tetrahydrofuran), adding 0.001 g of dioctane sodium sulfosuccinate, stirring at 80° C. until TATB is dissolved, to obtain a TATB solution;

[0068] Step 2: Recrystallization of TATB: 100 mL of distilled water was continuously added dropwise to the above solution, and stirred at 25°C for 1 h at a stirring speed of 1000 r / min;

[0069] Step 3. Growth and post-treatment of TATB: The solution of step 2 was stirred at 25° C. for 0.5 h, filtered, washed and dried to obtain recrystallized TATB crystals.

[0070] The prepared TATB crystals were tested and the TATB particle size was 0.9 μm, the crystals were round, and the purity was 99.6%.

[0071] Embodiment 7:

[0072] Step 1, dissolving TATB: dissolving 0.5 g of TATB (purity 97.8%) prepared by chlorine-free process in 30 ml of N-methylpyrrolidone / pyrrole sulfate / dimethyl sulfoxide mixed solvent (mixed solvent preparation method: taking 5 g of N-methylpyrrolidone and 5 g of pyrrole sulfate and dissolving them in 30 ml of dimethyl sulfoxide) mixed solvent, adding 0.001 g of polyethylene glycol, stirring at 80° C. until TATB is dissolved, to obtain a TATB solution;

[0073] Step 2: Recrystallization of TATB: 100 ml of cyclohexane was continuously added dropwise to the above solution, and stirred at 80°C for 1 h at a stirring speed of 1000 r / min;

[0074] Step 3: Growth and post-treatment of TATB: The solution of step 2 was stirred at 80° C. for 0.5 h, filtered, washed and dried to obtain recrystallized TATB crystals.

[0075] The prepared TATB crystals were tested and the median particle size of TATB was 0.7 microns, the crystals were round, and the purity was 99.5%.

[0076] Embodiment 8:

[0077] Step 1, dissolving TATB: dissolving 0.5 g of TATB (purity 97.8%) prepared by a chlorine-free process in 30 ml of a mixed solvent of N-methylmorpholine-N-oxide / dimethyl sulfoxide (the mixed solvent is prepared by dissolving 10 g of N-methylmorpholine-N-oxide in 30 ml of dimethyl sulfoxide), adding 0.001 g of modified gelatin, and stirring at 80° C. until TATB is dissolved to obtain a TATB solution;

[0078] Step 2: Recrystallization of TATB: 100 mL of ethyl acetate was continuously added dropwise into the above solution, and stirred at 30°C for 2 h at a stirring speed of 200 r / min;

[0079] Step 3, growth and post-treatment of TATB: the solution of step 2 is stirred at 30°C for 4 hours, filtered, washed and dried to obtain recrystallized TATB crystals;

[0080] The preparation method of the modified gelatin is as follows: 5g of gelatin is added to 10g of deionized water, the temperature is raised to 80°C, and the mixture is stirred to dissolve, and then 0.2g of urea and 0.1g of sodium citrate are added, the mixture is stirred at 80°C for 2 hours, and the obtained product is dried to obtain the modified gelatin;

[0081] The prepared TATB crystals were tested and the median particle size of TATB was 31 μm, the crystals were round, and the purity was 99.5%.

[0082] 0.6 g of TATB obtained in this example was tested for bulk density and fluidity. The height of the TATB obtained in this example in the test tube was about 0.8 cm. The angle of repose of the TATB prepared in this example was 38.1°.

[0083] Embodiment 9:

[0084] Step 1, dissolving TATB: dissolving 0.5 g of TATB (purity 97.8%) prepared by a chlorine-free process in 30 ml of a mixed solvent of N-methylmorpholine-N-oxide / dimethyl sulfoxide (the mixed solvent is prepared by dissolving 10 g of N-methylmorpholine-N-oxide in 30 ml of dimethyl sulfoxide), adding 0.001 g of modified gelatin, and stirring at 80° C. until TATB is dissolved to obtain a TATB solution;

[0085] Step 2: Recrystallization of TATB: 100 mL of ethyl acetate was continuously added dropwise into the above solution, and stirred at 30°C for 2 h at a stirring speed of 200 r / min;

[0086] Step 3, growth and post-treatment of TATB: the solution of step 2 is stirred at 30°C for 4 hours, filtered, washed and dried to obtain recrystallized TATB crystals;

[0087] The preparation method of the modified gelatin is as follows: 5g of gelatin is added to 10g of deionized water, the temperature is raised to 80°C, and the mixture is stirred to dissolve, then 0.2g of urea and 0.1g of sodium citrate are added, the mixture is kept at 80°C and stirred for 2 hours, the obtained product is dried, 3g of the dried product and 1g of polyvinyl alcohol are added to 10g of water, the temperature is raised to 65°C, the mixture is stirred to react for 1 hour, and the mixture is dried to obtain the modified gelatin;

[0088] The prepared TATB crystals were tested and the median particle size of TATB was 32 μm, the crystals were round and the purity was 99.6%.

[0089] 0.6 g of TATB obtained in this example was tested for bulk density and fluidity. The height of the TATB obtained in this example in the test tube was about 0.76 cm. The angle of repose of the TATB prepared in this example was 37.5°.

[0090] Embodiment 10:

[0091] Step 1, dissolving TATB: dissolving 0.5 g of TATB (purity 97.8%) prepared by a chlorine-free process in 30 ml of a mixed solvent of N-methylmorpholine-N-oxide / dimethyl sulfoxide (the mixed solvent is prepared by dissolving 10 g of N-methylmorpholine-N-oxide in 30 ml of dimethyl sulfoxide), adding 0.001 g of modified gelatin, and stirring at 80° C. until TATB is dissolved to obtain a TATB solution;

[0092] Step 2: Recrystallization of TATB: 100 mL of ethyl acetate was continuously added dropwise into the above solution, and stirred at 30°C for 2 h at a stirring speed of 200 r / min;

[0093] Step 3, growth and post-treatment of TATB: the solution of step 2 is stirred at 30°C for 4 hours, filtered, washed and dried to obtain recrystallized TATB crystals;

[0094] The preparation method of the modified gelatin is as follows: 5g of gelatin is added to 10g of deionized water, the temperature is raised to 80°C, and the mixture is stirred to dissolve. Then, 0.2g of urea and 0.1g of sodium citrate are added, and the mixture is stirred at 80°C for 2 hours. The obtained product is dried, 3g of the dried product and 1g of polyvinyl alcohol are added to a supercritical carbon dioxide reactor, and a 30MPa CO2, heated to 65°C to form supercritical carbon dioxide, the two materials swelled and reacted in the supercritical carbon dioxide solvent for 1 hour, and then the exhaust valve of the supercritical carbon dioxide reactor was opened to quickly discharge CO2 to reduce the pressure in the reactor to normal pressure, thereby obtaining modified gelatin; in the experimental process of the present invention, the inventor added the dried product and polyvinyl alcohol to the supercritical carbon dioxide solvent, and through the swelling effect of supercritical carbon dioxide, when gelatin and polyvinyl alcohol were swollen, the two could be more effectively cross-linked with gelatin, so that the prepared modified gelatin, when used as a crystal form controller, can significantly improve the crystal form of TATB crystals, and the modified gelatin can more effectively improve the purity of TATB crystals. At the same time, the obtained TATB has a lower bulk density and repose angle, indicating that it has better fluidity.

[0095] The prepared TATB crystals were tested and the median particle size of TATB was 34 μm, the crystals were more rounded, and the purity was 99.8%.

[0096] 0.6 g of TATB obtained in this example was tested for bulk density and fluidity. The height of the TATB obtained in this example in the test tube was about 0.7 cm. The angle of repose of the TATB prepared in this example was 36.9°.

[0097] Comparative Example 1:

[0098] Step 1: Dissolving TATB: Dissolve 0.5 g of TATB (purity 97.8%) prepared by a chlorine-free process in 30 ml of dimethyl sulfoxide, add 0.001 g of polyvinyl alcohol, and stir at 80° C. until TATB is dissolved to obtain a TATB solution;

[0099] Step 2: Recrystallization of TATB: 100 ml of distilled water was continuously added dropwise to the above solution, and stirred at 50°C for 2 h at a stirring speed of 300 r / min;

[0100] Step 3: Growth and post-treatment of TATB: The solution of step 2 is stirred at 80° C. for 3 h, filtered, washed and dried to obtain recrystallized TATB crystals.

[0101] The prepared TATB crystals were tested and found to have a purity of 98.3%;

[0102] 0.6 g of TATB obtained in this example was tested for bulk density and fluidity. The height of the TATB obtained in this example in the test tube was about 0.95 cm. The angle of repose of the TATB prepared in this example was 39.6°.

[0103] Comparative Example 2:

[0104] Step 1, dissolving TATB: dissolving 0.5 g of TATB (purity 97.8%) prepared by a chlorine-free process in 30 ml of dimethyl sulfoxide, adding 0.001 g of gelatin, and stirring at 80° C. until TATB is dissolved to obtain a TATB solution;

[0105] Step 2: Recrystallization of TATB: 100 ml of ethyl acetate was continuously added dropwise into the above solution, and stirred at 30°C for 2 h at a stirring speed of 200 r / min;

[0106] Step 3: Growth and post-treatment of TATB: The solution of step 2 is stirred at 30° C. for 4 h, filtered, washed and dried to obtain recrystallized TATB crystals.

[0107] The prepared TATB crystals were tested and found to have a purity of 98.1%.

[0108] 0.6 g of TATB obtained in this example was tested for bulk density and fluidity. The height of the TATB obtained in this example in the test tube was about 0.97 cm. The angle of repose of the TATB prepared in this example was 39.8°.

[0109] Although the embodiments of the present invention have been disclosed as above, they are not limited to the applications listed in the specification and the implementation modes, and they can be fully applied to various fields suitable for the present invention. For those familiar with the art, additional modifications can be easily implemented. Therefore, without departing from the general concept defined by the claims and the scope of equivalents, the present invention is not limited to the specific details and the illustrations shown and described herein.

Claims

1. A method for integrated control of the morphology, size and purity of TATB prepared by a chlorine-free process, characterized in that: The steps include: Step 1: Dissolving TATB: dissolving TATB in solvent A, adding a crystal control agent, heating and stirring to obtain a TATB solution; Step 2: Recrystallization of TATB: continuously add solvent B dropwise into the above TATB solution, control the temperature and stir or perform ultrasound; Step 3: Growth and post-treatment of TATB: The solution of step 2 is continuously stirred at a certain temperature to allow the crystals to grow for a period of time, and then filtered, washed and dried to obtain recrystallized TATB crystals.

2. The method for integrated control of the morphology, size and purity of TATB prepared by a chlorine-free process as claimed in claim 1, characterized in that: The solvent A is one or more of 1-butyl-3-methylimidazolium chloride / dimethyl sulfoxide, 1-butyl-3-methylimidazolium chloride / acetone, 1-butyl-3-methylimidazolium chloride / ethyl acetate, zinc chloride / dimethylformamide, N-methylmorpholine-N-oxide / dimethyl sulfoxide, N-methylmorpholine-N-oxide / acetone, N-methylmorpholine-N-oxide / ethyl acetate, pyrrole sulfate / tetrahydrofuran, tetrahydrofuran / dimethyl sulfoxide, tetrahydrofuran / acetone, tetrahydrofuran / ethyl acetate, N-methylpyrrolidone / pyrrole sulfate / dimethyl sulfoxide.

3. The method for integrated control of the morphology, size and purity of TATB prepared by a chlorine-free process as claimed in claim 1, characterized in that: The solvent B is one or more of distilled water, ethanol, n-butanol, isopropanol, ethyl acetate, butyl acetate, isoamyl acetate, acetic acid, propionic acid, dichloromethane, chloroform, carbon tetrachloride, ethylene dichloride, ether, petroleum ether, n-butane, and cyclohexane.

4. The method for integrated control of the morphology, size and purity of TATB prepared by a chlorine-free process as claimed in claim 1, characterized in that: The crystal form control agent is one or more of polyvinyl alcohol, polyethylene glycol, gelatin, sodium dodecylbenzene sulfonate, cetylpyridine, sodium dodecyl sulfate, sodium cetyl sulfate, sodium octadecyl sulfate, dioctane sodium sulfosuccinate, polyvinyl pyrrolidone, Span 20-80, and Tween 20-80.

5. The method for integrated control of the morphology, size and purity of TATB prepared by a chlorine-free process as claimed in claim 1, characterized in that: The mass volume ratio of the TATB to the solvent A is 0.1-1.5 g:30 mL; the mass volume ratio of the TATB to the solvent B is 0.1-1.5 g:100 mL.

6. The method for integrated control of the morphology, size and purity of TATB prepared by a chlorine-free process as claimed in claim 1, characterized in that: The addition amount of the crystal form control agent is 0.01%-1% of the total mass of TATB.

7. The method for integrated control of the morphology, size and purity of TATB prepared by a chlorine-free process as claimed in claim 1, characterized in that: The stirring method is mechanical stirring or ultrasonic stirring.

8. The method for integrated control of the morphology, size and purity of TATB prepared by a chlorine-free process as claimed in claim 1, characterized in that: The temperature range of heating and stirring in the step 1 is 25 to 150° C.; the temperature range of temperature-controlled stirring in the step 2 is 25 to 150° C.; and the temperature range of continuing stirring at a certain temperature in the step 3 is 25 to 150° C.

9. The method for integrated control of the morphology, size and purity of TATB prepared by a chlorine-free process as claimed in claim 1, characterized in that: The stirring rate is 50r / min-1500r / min.

10. The method for integrated control of the morphology, size and purity of TATB prepared by a chlorine-free process as claimed in claim 1, characterized in that: In the step 2, the stirring time ranges from 0.5 to 8 hours. In the step 3, the stirring time ranges from 0.5 to 8 hours.