BOPP (Biaxially-oriented Polypropylene) pre-coating film for food preservation and preparation method of BOPP pre-coating film
By coating BOPP film with PGEF barrier coating and PVOH anti-fog coating, the problem of insufficient antibacterial properties of BOPP film is solved, its barrier and anti-fog properties are improved, and the shelf life of fresh products is extended.
Patent Information
- Application Number
- CN202411129596.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-16
- Publication Date
- 2024-11-26
AI Technical Summary
Existing BOPP films have insufficient antibacterial properties, short shelf life, and cannot effectively prevent the spoilage and oxidative deterioration of fresh produce.
By coating BOPP film with PGEF barrier coating and PVOH anti-fog coating, and by adjusting the proportion of each component and process steps, the barrier and anti-fog properties of the film are improved, thereby enhancing its freshness preservation ability.
It significantly improves the barrier and anti-fogging properties of BOPP film, extends the shelf life and shelf life of fresh produce, and reduces the risk of microbial growth and oxidative spoilage.
Smart Images

Figure CN119019735A_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to the technical field of pre-coated films, and in particular to a BOPP pre-coated film for food preservation and a preparation method thereof, and improves the preservation ability of the BOPP pre-coated film for food packaging by improving antibacterial properties and barrier properties and reducing wettability. [Background technology]
[0002] BOPP is the abbreviation of biaxially oriented polypropylene. It is a high-density, side-chain-free, highly crystalline linear polymer with the characteristics of beautiful transparency, stable performance, safety and non-toxicity. It is a representative material in the food packaging industry. The packaging materials of typical fresh commodities such as fresh vegetables, fruits, and flowers are required to have a certain preservation ability to extend the shelf life and shelf life of fresh commodities. There are two main reasons for the corruption and deterioration of fresh commodities. First, the fresh commodities have a high moisture content and a large temperature difference during transportation. The water mist condensed on the inner surface of the package provides conditions for the reproduction of microorganisms; second, the oxygen in the air promotes the growth of microorganisms and also promotes the oxidation and deterioration of fresh commodities. Therefore, the preservation ability of BOPP materials depends not only on its own antibacterial properties, but also on its barrier and anti-fogging properties. BOPP pre-coated film is a composite film with a laminated structure formed by polypropylene film and EVA hot melt adhesive. It can not only improve the shortcomings of ordinary PP film and give full play to the excellent performance of PP film, but also modify the surface of BOPP film through coating to improve its barrier and anti-fogging properties, thereby improving its preservation ability. [Summary of the invention]
[0003] The purpose of the present invention is to provide a BOPP pre-coated film for food packaging and a preparation method thereof in view of the defects and shortcomings of the existing BOPP film, and to modify the surface of the BOPP film by pre-coating, so as to effectively solve the problems of insufficient antibacterial property and short shelf life of the existing BOPP film.
[0004] To achieve the above-mentioned object, the present invention proposes a BOPP pre-coated film for food packaging, comprising a BOPP base film, a PGEF barrier coating and a PVOH anti-fog coating, wherein a PVOH anti-fog coating is provided between the BOPP base film and the PGEF barrier coating, wherein the weight ratio of the BOPP base film, the PGEF barrier coating and the PVOH anti-fog coating is 45-55:0.5-1.5:0.5-1.5.
[0005] Preferably, the weight ratio of the BOPP base film, the PGEF barrier coating and the PVOH anti-fog coating is 50:1:1.
[0006] Preferably, the PGEF barrier coating is composed of pure water, polyglycerol fatty acid ester PGEF and a composite barrier agent, and the mass ratio of the components is 100:1-5:1-2; the composite barrier agent is prepared from nano-alumina and nano-silicon oxide in a mass ratio of 1:1.
[0007] Preferably, the PVOH anti-fog coating is composed of a polyvinyl alcohol matrix, a composite anti-fog agent and borax, and the mass ratio of the components is 100:5-15:1-2; the composite anti-fog agent is prepared from tetraethyl orthosilicate TEOS, anhydrous alcohol and purified water in a mass ratio of 1:2:2.
[0008] A method for preparing a BOPP pre-coated film for food packaging comprises the following steps:
[0009] (1) Preparation of PGEF barrier coating liquid: First, prepare a composite barrier agent, which is mechanically mixed with nano-alumina and nano-silicon oxide at a mass ratio of 1:1; secondly, mix pure water, polyglycerol fatty acid ester and composite barrier agent at a mass ratio of 100:1-5:1-2, heat to 60°C and stir for 60 minutes at a stirring rate of 500R / min, and then keep warm for use;
[0010] (2) preheating the BOPP base film to 70° C., using a coating machine to evenly coat the PGEF barrier coating liquid prepared in step 1 on the surface of the BOPP base film, placing the coated BOPP base film in a drying oven for drying and then cooling naturally, the drying temperature being 70° C., to obtain a coated base film A;
[0011] (3) Preparing PVOH anti-fog coating: first, preparing polyvinyl alcohol matrix PVOH, placing polyvinyl alcohol PVC powder in pure water and heating it to 80°C, and stirring it for 90 minutes at a stirring rate of 800R / min, so that the polyvinyl alcohol is fully dissolved in the pure water, and the final concentration is 4-5% by mass; secondly, preparing a composite anti-fog agent, which is prepared by mixing tetraethyl orthosilicate TEOS, anhydrous alcohol, and pure water in a mass ratio of 1:2:2; finally, mixing the polyvinyl alcohol matrix, the composite anti-fog agent, and borax in a mass ratio of 100:5-15:1-2 and stirring it for 70 minutes at a stirring rate of 500R / min;
[0012] (4) stirring the PVOH anti-fog coating liquid prepared in step 3 at 80° C. for 30 min, applying the PVOH anti-fog coating liquid on the coating base film A prepared in step 2 using a coating machine, and drying the coated coating base film A in a drying oven for 2 hours to obtain a coating base film B;
[0013] (5) The coating base film B dried in step 4 is placed in a UV curing box for curing, with a light source intensity of 200-300 mW / cm2 and a curing time of 2-3 min, and then naturally cooled to obtain a BOPP pre-coated film.
[0014] Beneficial effects of the present invention: Compared with the prior art, the present invention modifies the surface of the BOPP film through a coating, thereby improving its barrier properties and anti-fogging properties, thereby improving its freshness-keeping ability.
[0015] The features and advantages of the present invention will be described in detail through embodiments in conjunction with the accompanying drawings.
Brief Description of the Drawings
[0016] Figure 1 It is a schematic structural diagram of a BOPP pre-coated film for food packaging of the present invention.
[0017] In the picture: 1-BOPP base film, 2-PGEF barrier coating, 3-PVOH anti-fog coating. [Specific implementation method]
[0018] The method of the present invention is further described in detail below with reference to specific examples.
[0019] The BOPP pre-coated film for food preservation and the preparation method thereof described in the present invention, on the basis of a conventional BOPP film base film, are coated with two layers of coatings with different components and functions in sequence, so as to improve the barrier property of the film on the one hand and the anti-fogging property of the film on the other hand, thereby jointly improving the preservation ability of the film.
[0020] Embodiment 1:
[0021] See also Figure 1 The present invention provides a BOPP pre-coated film for food packaging, comprising a BOPP base film 1, a PGEF barrier coating 2 and a PVOH anti-fog coating 3, wherein the PVOH anti-fog coating 3 is arranged between the BOPP base film 1 and the PGEF barrier coating 2, wherein the weight ratio of the BOPP base film 1 to the PGEF barrier coating 2 and the PVOH anti-fog coating 3 is 50:1:1.
[0022] The PGEF barrier coating 2 is composed of pure water, polyglycerol fatty acid ester PGEF and a composite barrier agent, and the mass ratio of the components is 100:3:1; the composite barrier agent is prepared from nano-aluminum oxide and nano-silicon oxide in a mass ratio of 1:1.
[0023] The PVOH anti-fog coating 3 is composed of a polyvinyl alcohol matrix, a composite anti-fog agent and borax, and the mass ratio of the components is 100:5:1; the composite anti-fog agent is prepared from tetraethyl orthosilicate TEOS, anhydrous alcohol and purified water in a mass ratio of 1:2:2.
[0024] A method for preparing a BOPP pre-coated film for food packaging comprises the following steps:
[0025] (1) Preparation of PGEF barrier coating liquid: First, prepare a composite barrier agent, which is mechanically mixed with nano-alumina and nano-silicon oxide in a mass ratio of 1:1; secondly, mix pure water, polyglycerol fatty acid ester and composite barrier agent in a mass ratio of 100:3:1, heat to 60°C and stir for 60 minutes, with a stirring rate of 500R / min, and then keep warm for use;
[0026] (2) preheating the BOPP base film 1 to 70° C., using a coating machine to evenly coat the PGEF barrier coating liquid prepared in step 1 on the surface of the BOPP base film 1, placing the coated BOPP base film 1 in a drying oven for drying and then cooling naturally, the drying temperature being 70° C., to obtain a coated base film A;
[0027] (3) Preparation of PVOH anti-fog coating: First, prepare polyvinyl alcohol matrix PVOH, place polyvinyl alcohol PVC powder in pure water and heat it to 80°C, and stir for 90 minutes at a stirring rate of 800R / min, so that polyvinyl alcohol is fully dissolved in pure water, and the final concentration is 4-5% by mass; secondly, prepare a composite anti-fog agent, which is prepared by mixing tetraethyl orthosilicate TEOS, anhydrous alcohol, and pure water in a mass ratio of 1:2:2; finally, mix the polyvinyl alcohol matrix, the composite anti-fog agent, and borax in a mass ratio of 100:5:1 and stir for 70 minutes at a stirring rate of 500R / min;
[0028] (4) stirring the PVOH anti-fog coating liquid prepared in step 3 at 80° C. for 30 min, applying the PVOH anti-fog coating liquid on the coating base film A prepared in step 2 using a coating machine, and drying the coated coating base film A in a drying oven for 2 hours to obtain a coating base film B;
[0029] (5) The coating base film B dried in step 4 is placed in a UV curing box for curing, with a light source intensity of 200-300 mW / cm2 and a curing time of 2-3 min, and then naturally cooled to obtain a BOPP pre-coated film.
[0030] Embodiment 2:
[0031] The coating composition, method steps and parameters of Example 1 are adopted, except that the mass ratio of pure water, polyglycerol fatty acid ester PGEF and composite barrier agent is 100:3:2, and the mass ratio of polyvinyl alcohol matrix, composite antifogging agent and borax is 100:5:1.
[0032] Embodiment 3:
[0033] The coating composition, method steps and parameters of Example 1 are adopted, except that the mass ratio of pure water, polyglycerol fatty acid ester PGEF and composite barrier agent is 100:5:1, and the mass ratio of polyvinyl alcohol matrix, composite antifogging agent and borax is 100:5:1.
[0034] Embodiment 4:
[0035] The coating composition, method steps and parameters of Example 1 are adopted, except that the mass ratio of pure water, polyglycerol fatty acid ester PGEF and composite barrier agent is 100:5:2, and the mass ratio of polyvinyl alcohol matrix, composite antifogging agent and borax is 100:5:1.
[0036] Embodiment 5:
[0037] The coating composition, method steps and parameters of Example 1 are adopted, except that the mass ratio of pure water, polyglycerol fatty acid ester PGEF and composite barrier agent is 100:5:2, and the mass ratio of polyvinyl alcohol matrix, composite antifogging agent and borax is 100:5:2.
[0038] Embodiment 6:
[0039] The coating composition, method steps and parameters of Example 1 are adopted, except that the mass ratio of pure water, polyglycerol fatty acid ester PGEF and composite barrier agent is 100:5:2, and the mass ratio of polyvinyl alcohol matrix, composite antifogging agent and borax is 100:10:1.
[0040] Embodiment 7:
[0041] The coating composition, method steps and parameters of Example 1 are adopted, except that the mass ratio of pure water, polyglycerol fatty acid ester PGEF and composite barrier agent is 100:5:2, and the mass ratio of polyvinyl alcohol matrix, composite antifogging agent and borax is 100:10:2.
[0042] Embodiment 8:
[0043] The coating composition, method steps and parameters of Example 1 are adopted, except that the mass ratio of pure water, polyglycerol fatty acid ester PGEF and composite barrier agent is 100:5:2, and the mass ratio of polyvinyl alcohol matrix, composite antifogging agent and borax is 100:15:1.
[0044] Embodiment 9:
[0045] The coating composition, method steps and parameters of Example 1 are adopted, except that the mass ratio of pure water, polyglycerol fatty acid ester PGEF and composite barrier agent is 100:5:2, and the mass ratio of polyvinyl alcohol matrix, composite antifogging agent and borax is 100:15:2.
[0046] The BOPP pre-coated film for food preservation and its preparation method described in the present invention, the performance indicators brought by the composition and dosage of the barrier coating and anti-fog coating in all embodiments are obtained by using the above coating components and method steps and parameters. The size of the BOPP pre-coated film material specimen is length a = 20cm, width b = 15cm, thickness c = 60μm. The embodiments are shown in Table 1 below, and the base coating in the table is pure water.
[0047] Table 1 Design and composition of barrier coating, anti-fog coating and properties of BOPP film
[0048]
[0049] The BOPP pre-coated film for food preservation and the preparation method thereof described in the present invention are prepared according to the above method steps and coating components. The technical indicators achieved by the BOPP film are as follows:
[0050] 1. The BOPP film has good barrier properties, and its water vapor permeability is below 0.50×10-13g·m-1·s-1·Pa-1;
[0051] 2. The BOPP film has good anti-fog properties. It is difficult for water vapor to form water droplets on the inner surface of the BOPP film. After being in a 50°C water bath for 1 hour, the transmittance is still above 80%, and the value still reaches more than 90% of the transmittance before the water bath.
[0052] 3. The polyglycerol fatty acid ester in the barrier coating reduces the water vapor permeability of the film; nano-aluminum oxide and nano-silicon oxide reduce the oxygen permeability of the film; the combined effect of the two effectively increases the barrier properties of the film.
[0053] 4. By adding ethyl orthosilicate into the coating, the hydrophilicity of the film is reduced, which increases the barrier properties of the film while gradually reducing the accumulation of water droplets on the surface of the film, reduces bacterial growth, and further increases the film's ability to preserve freshness.
[0054] The above embodiments are intended to illustrate the present invention, not to limit the present invention. Any solution that is a simple transformation of the present invention belongs to the protection scope of the present invention.
Claims
1. A BOPP pre-coated film for food packaging, characterized in that: The invention comprises a BOPP base film (1), a PGEF barrier coating (2) and a PVOH anti-fog coating (3), wherein the PVOH anti-fog coating (3) is arranged between the BOPP base film (1) and the PGEF barrier coating (2), wherein the weight ratio of the BOPP base film (1), the PGEF barrier coating (2) and the PVOH anti-fog coating (3) is 45-55: 0.5-1.5:0.5-1.5。 2. A BOPP pre-coated film for food packaging as claimed in claim 1, characterized in that: The weight ratio of the BOPP base film (1), the PGEF barrier coating (2), and the PVOH anti-fog coating (3) is 50:1:
1.
3. A BOPP pre-coated film for food packaging as claimed in claim 1, characterized in that: The PGEF barrier coating (2) is composed of pure water, polyglycerol fatty acid ester (PGEF) and a composite barrier agent, wherein the mass ratio of the components is 100:1-5:1-2; the composite barrier agent is prepared from nano-aluminum oxide and nano-silicon oxide in a mass ratio of 1:
1.
4. A BOPP pre-coated film for food packaging as claimed in claim 1, characterized in that: The PVOH anti-fog coating (3) is composed of a polyvinyl alcohol matrix, a composite anti-fog agent and borax, and the mass ratio of the components is 100:5-15:1-2; the composite anti-fog agent is prepared from tetraethyl orthosilicate (TEOS), anhydrous alcohol and purified water in a mass ratio of 1:2:
2.
5. A method for preparing a BOPP pre-coated film for food packaging according to any one of claims 1 to 4, characterized in that: The following steps are involved: (1) Preparation of PGEF barrier coating liquid: First, prepare a composite barrier agent, which is mechanically mixed with nano-alumina and nano-silicon oxide at a mass ratio of 1:1; secondly, mix pure water, polyglycerol fatty acid ester and composite barrier agent at a mass ratio of 100:1-5:1-2, heat to 60°C and stir for 60 minutes at a stirring rate of 500R / min, and then keep warm for use; (2) preheating the BOPP base film (1) to 70° C., using a coating machine to evenly coat the PGEF barrier coating liquid prepared in step 1 on the surface of the BOPP base film (1), placing the coated BOPP base film (1) in a drying oven for drying and then cooling naturally, the drying temperature being 70° C., to obtain a coated base film A; (3) Preparation of PVOH anti-fog coating: First, prepare a polyvinyl alcohol matrix (PVOH), place polyvinyl alcohol (PVC) powder in pure water and heat it to 80°C, and stir it for 90 minutes at a stirring rate of 800R / min, so that the polyvinyl alcohol is fully dissolved in the pure water, and the final concentration is 4-5% by mass; secondly, prepare a composite anti-fog agent, which is prepared by mixing tetraethyl orthosilicate (TEOS), anhydrous alcohol, and pure water in a mass ratio of 1:2:2; finally, mix the polyvinyl alcohol matrix, the composite anti-fog agent, and borax in a mass ratio of 100:5-15:1-2 and stir for 70 minutes at a stirring rate of 500R / min; (4) stirring the PVOH anti-fog coating liquid prepared in step 3 at 80° C. for 30 min, applying the PVOH anti-fog coating liquid on the coating base film A prepared in step 2 using a coating machine, and drying the coated coating base film A in a drying oven for 2 hours to obtain a coating base film B; (5) The coating base film B dried in step 4 is placed in a UV curing box for curing, with a light source intensity of 200-300 mW / cm2 and a curing time of 2-3 min, and then naturally cooled to obtain a BOPP pre-coated film.