Online resistivity testing device and method

Through the online resistivity test device to detect the resistivity of the single crystal silicon rod in real time at high temperature and regulate the doping concentration, the resistivity measurement deviation caused by volatile doping elements is solved, and the production efficiency and qualification of the single crystal silicon rod are improved. Rate.

CN119024046APending Publication Date: 2024-11-26JINGAO SOLAR CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411237621.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

During the drawing process of single crystal silicon rods, volatile doped elements such as antimony cause resistance measurement deviations, resulting in low production efficiency and low pass rate. The existing technology requires the resistivity detection after the single crystal silicon rod is cooled to normal temperature. , the doping concentration cannot be adjusted in time.

Method used

Design an online resistivity testing device, including a sealing cavity, a resistivity measuring probe, a transmission mechanism and a sensing mechanism, which can detect the resistivity of a single crystal silicon rod in real time at high temperatures, and instantly regulate the doping of the silica solution based on the detection results. Concentration, calculate the resistivity at room temperature.

Benefits of technology

Real-time detection of resistivity during the drawing process of single crystal silicon rods, rapid adjustment of doping amount, and improve the pass rate and production efficiency of single crystal silicon rods, especially for volatile dopants, avoiding waiting for cooling. The resistivity of the monocrystalline silicon rod is not suitable for production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119024046A_ABST
    Figure CN119024046A_ABST
Patent Text Reader

Abstract

The invention discloses an online resistivity testing device and method. The on-line resistivity testing device comprises a sealing cavity, a resistivity measuring probe, a transmission mechanism, a sensing mechanism and a processor, and the sealing cavity is installed on the outer side wall of the single crystal furnace and communicated with the interior of a furnace barrel of the single crystal furnace; the resistivity measuring probe is connected with the transmission mechanism, moves between the interior of the furnace barrel and the sealing cavity under the driving of the transmission mechanism, and is used for detecting the high-temperature resistivity of the silicon single crystal rod; the sensing mechanism is arranged in the sealing cavity and is used for detecting the distance from the resistivity measuring probe to the silicon single crystal rod and the temperature of a detection position; the processor is in communication connection with the resistivity measuring probe, the sensing mechanism and the transmission mechanism; the processor calculates the first normal-temperature resistivity of the single crystal silicon rod at the normal temperature based on a set resistivity regulation and control strategy, the high-temperature resistivity, the distance from the resistivity measurement probe to the single crystal silicon rod and the temperature of the detection position. The on-line resistivity testing device can improve the qualified rate and the production efficiency of the produced silicon single crystal rod.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to an online resistivity testing device and method. Background Art

[0002] At present, the resistivity control method of single crystal silicon rods is mainly to test the resistivity of the single crystal silicon rods after the single crystal silicon rods are pulled and cooled to room temperature, and adjust the doping concentration of the dopant in the silicon solution used for subsequent pulling of the single crystal silicon rods based on the test results.

[0003] For doping with volatile doping elements such as antimony, due to the volatility of the dopant, the actual resistivity of the single crystal silicon rod deviates greatly from the target resistivity. It takes a long cooling time to cool the single crystal silicon rod to room temperature and then test the resistivity at room temperature. During this time period, continuous pulling of the single crystal silicon rod will result in a low pass rate of the pulled single crystal silicon rods, resulting in waste of silicon materials. If the pulling is stopped during this time period, the production efficiency of the single crystal silicon rod will be low. Summary of the invention

[0004] In view of this, the present invention provides an online resistivity testing device and method, which can effectively improve the qualification rate and production efficiency of produced single crystal silicon rods.

[0005] In order to solve the above technical problems, the present invention provides the following technical solutions:

[0006] In a first aspect, the present invention provides an online resistivity testing device, comprising: a sealed chamber, a resistivity measuring probe, a transmission mechanism, a sensor mechanism and a processor, wherein:

[0007] The sealed cavity is installed on the outer side wall of the single crystal furnace and is communicated with the interior of the single crystal furnace drum;

[0008] The resistivity measuring probe is connected to the transmission mechanism, and is driven by the transmission mechanism to move between the furnace drum and the sealed cavity, so as to detect the high temperature resistivity of the single crystal silicon rod in the pulling stage in the single crystal furnace;

[0009] The sensing mechanism is disposed in the sealed cavity and is used to detect the distance from the resistivity measuring probe to the single crystal silicon rod and the temperature at the detection position;

[0010] The processor is in communication connection with the resistivity measuring probe, the sensing mechanism and the transmission mechanism;

[0011] The processor is provided with a resistivity control strategy. Based on the resistivity control strategy, the first normal-temperature resistivity of the single crystal silicon rod at normal temperature is calculated according to the high-temperature resistivity of the single crystal silicon rod detected by the resistivity measurement probe, the distance from the resistivity measurement probe to the single crystal silicon rod detected by the sensing mechanism, and the temperature of the detection position.

[0012] In a second aspect, an embodiment of the present invention provides a single crystal furnace, comprising:

[0013] The furnace body comprises a main chamber and a sub-chamber, and a mounting hole for an online resistivity test device penetrating through the side wall of the main chamber and / or the sub-chamber is provided on the side wall;

[0014] One or more of the online resistivity testing devices provided in the above-mentioned first aspect embodiments are installed in the online resistivity testing device installation hole.

[0015] In a third aspect, an embodiment of the present invention provides an online resistivity testing method, which is completed based on the online resistivity testing device provided in the embodiment of the first aspect above. The online resistivity testing method includes:

[0016] Step 1, determining whether the head of the pulled single crystal silicon rod reaches the height where the resistivity measurement probe is located;

[0017] Step 2: When it is determined that the head of the pulled single crystal silicon rod reaches the height of the resistivity measuring probe, the processor sends a first driving signal to the transmission mechanism, the transmission mechanism drives the resistivity measuring probe to move toward the single crystal silicon rod, and starts detection, detects the high-temperature resistivity of the head of the single crystal silicon rod by the resistivity measuring probe, and simultaneously detects the distance from the resistivity measuring probe to the single crystal silicon rod and the temperature at the detection position by the sensing mechanism, sends the detected high-temperature resistivity of the head of the single crystal silicon rod, the distance from the resistivity measuring probe to the single crystal silicon rod, and the temperature at the detection position to the processor of the online resistivity testing device, and the processor calculates the first normal-temperature resistivity of the single crystal silicon rod at room temperature based on the resistivity control strategy, the high-temperature resistivity of the single crystal silicon rod detected by the resistivity measuring probe, the distance from the resistivity measuring probe to the single crystal silicon rod detected by the sensing mechanism, and the temperature at the detection position;

[0018] Step 2: After the detection is completed, the processor sends a second driving signal to the transmission mechanism, and the transmission mechanism drives the resistivity measurement probe to be retracted into the sealed cavity.

[0019] In a fourth aspect, an embodiment of the present invention provides an online resistivity testing method, which is completed based on the online resistivity testing device provided in the embodiment of the first aspect above. The online resistivity testing method includes:

[0020] Step A, when the sensing mechanism can detect that the measurement start position reaches the height of the resistivity measuring probe of the online resistivity testing device, sending a signal indicating the start of measurement to the processor through the sensing mechanism;

[0021] Step B, sending a third driving signal to the transmission mechanism through the processor, driving the resistivity measurement probe to move toward the single crystal silicon rod through the transmission mechanism, and starting detection;

[0022] Step C, at set intervals, the high-temperature resistivity of the single crystal silicon rod at different axial positions is detected by the resistivity measuring probe, and the distance from the resistivity measuring probe to the single crystal silicon rod and the temperature of the detection position are simultaneously detected by the sensing mechanism, and the detected high-temperature resistivity of the head of the single crystal silicon rod, the distance from the resistivity measuring probe to the single crystal silicon rod, and the temperature of the detection position are sent to the processor, and the processor calculates the first normal-temperature resistivity of the single crystal silicon rod at room temperature based on the resistivity control strategy, the high-temperature resistivity of the single crystal silicon rod detected by the resistivity measuring probe, the distance from the resistivity measuring probe to the single crystal silicon rod detected by the sensing mechanism, and the temperature of the detection position;

[0023] Step D, when the sensing mechanism detects that the single crystal silicon rod reaches the height of the resistivity measuring probe of the online resistivity testing device at the measurement end position, the sensing mechanism sends a signal indicating the end of the test to the processor; and the processor sends a fourth driving signal to the transmission mechanism;

[0024] Step E: driving the resistivity measurement probe by the transmission mechanism to move the resistivity measurement probe in a direction away from the single crystal silicon rod.

[0025] The technical solution of the first aspect of the above invention has the following advantages or beneficial effects:

[0026] The online resistivity testing device provided by the embodiment of the present invention can detect the high-temperature resistivity of the single crystal silicon rod in the pulling stage, the distance from the resistivity measuring probe corresponding to the high-temperature resistivity to the pulled single crystal silicon rod, and the temperature of the detection position at high temperature during the single crystal silicon rod pulling process, and adjust the doping concentration of the silicon solution dopant based on these parameters to timely regulate the resistivity of the single crystal silicon rod, and based on the resistivity regulation strategy, the processor adjusts the resistivity of the single crystal silicon rod according to the high-temperature resistivity of the single crystal silicon rod detected by the resistivity measuring probe, the distance from the resistivity measuring probe to the single crystal silicon rod detected by the sensing mechanism, and the temperature of the detection position. degree, calculate the first room temperature resistivity of the single crystal silicon rod at room temperature, that is, through the high temperature resistivity detected online, the resistivity of the single crystal silicon rod at room temperature can be calculated. For the case where the actual resistivity of the single crystal silicon rod deviates greatly from the target resistivity due to doping with volatile dopants such as antimony, there is no need to wait until the single crystal silicon rod is pulled and cooled to room temperature before detecting the resistivity of the single crystal silicon rod. The real-time resistivity during the pulling process can be obtained, so that the doping amount of the next single crystal silicon rod can be quickly adjusted based on the real-time resistivity, avoiding the production of single crystal silicon rods with inappropriate resistivity during the waiting cooling period in the prior art. Therefore, the online resistivity testing device provided in the embodiment of the present invention can timely adjust the resistivity of the single crystal silicon rod, especially for the single crystal silicon rod doped with volatile dopants, which can effectively improve the qualified rate and production efficiency of the produced single crystal silicon rods. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 is a structural schematic diagram of a single crystal furnace with an online resistivity testing device in a first state according to an embodiment of the present invention;

[0028] Figure 2 is a structural schematic diagram of a second state of a single crystal furnace with an online resistivity testing device according to an embodiment of the present invention;

[0029] Figure 3 is a schematic diagram of a partially enlarged structure of a single crystal furnace according to an embodiment of the present invention;

[0030] Figure 4 This is a schematic diagram of the main process of a first online resistivity testing method according to an embodiment of the present invention;

[0031] Figure 5 It is a main flow chart of a second online resistivity testing method according to an embodiment of the present invention.

[0032] The reference numerals are as follows:

[0033] 10-online resistivity test device; 11-sealed chamber; 12-resistivity measurement probe; 13-transmission mechanism; 14-sensing mechanism; 15-processor; 20-single crystal furnace; 21-sub-chamber; 22-main chamber; 23-heater; 24-crucible; 25-water-cooled heat shield; 30-single crystal silicon rod. DETAILED DESCRIPTION

[0034] Resistivity is one of the important electrical performance characterization parameters of CZ silicon rods. At present, CZ silicon rods can be divided into P-type and N-type. In the production process of CZ silicon rods, the PN type and resistivity can be controlled by adding dopants or master alloys, where the P-type master alloy can contain one or more trivalent elements such as boron (B), aluminum (Al), gallium (Ga) and indium (In); the N-type dopant or master alloy can contain one or more pentavalent elements such as phosphorus (P), nitrogen (N), arsenic (As) and antimony (Sb).

[0035] At present, the resistivity can be controlled by calculating the doping amount of the dopant or the master alloy through the resistivity measurement formula. However, in actual production, factors such as temperature, furnace pressure, time, crystal rotation, and crucible rotation will affect the effective segregation of the dopant or each master alloy element. Therefore, the actual doping amount of the dopant or the master alloy will deviate from the theoretical calculation. Especially for volatile dopants, such as antimony, which will volatilize during the production process, resulting in a large deviation between the actual dopant doping amount and the theoretical calculation, and ultimately resulting in a large deviation between the actual resistivity of the single crystal silicon rod and the target resistivity.

[0036] At present, after the single crystal silicon rod is pulled, the resistivity is measured when the crystal rod cools to room temperature, and then the doping amount of dopant or the doping amount of the master alloy entering the silicon solution is adjusted based on the measured resistivity. However, it takes a long time for the single crystal silicon rod to be taken out and cooled to room temperature, and it is impossible to measure the accurate resistivity before the next rod is pulled, resulting in the resistivity of the next rod or the doping amount of dopant or the doping amount of the master alloy in the silicon solution can only be controlled according to the previous control method or theoretical calculation results or experience. If the resistivity of the single crystal silicon rod that has been pulled has deviations and does not meet the quality requirements, the next single crystal silicon rod pulled subsequently will also have deviations. Since the deviation of the next single crystal silicon rod cannot be detected and adjusted in time, it affects the qualified rate and effective output of the single crystal silicon rod.

[0037] In order to solve the above problems existing in the prior art, an embodiment of the present invention provides an online resistivity testing device and an online resistivity testing method implemented based on the online resistivity testing device.

[0038] in, Figure 1A schematic structural diagram showing, by way of example, a first state of a single crystal furnace having an online resistivity testing device; Figure 2 A schematic structural diagram showing, by way of example, a second state of a single crystal furnace having an online resistivity testing device; Figure 3 The schematic diagram of the structure of a single crystal furnace after partial enlargement is shown as an example.

[0039] like Figures 1 to 3 As shown, the online resistivity testing device 10 provided in the embodiment of the present invention may include the following structure:

[0040] A sealed chamber 11, a resistivity measuring probe 12, a transmission mechanism 13, a sensor mechanism 14 and a processor 15, wherein:

[0041] The sealed chamber 11 is installed on the outer wall of the single crystal furnace 20 and communicates with the interior of the furnace drum of the single crystal furnace 20;

[0042] The resistivity measuring probe 12 is connected to the transmission mechanism 13, and is driven by the transmission mechanism 13 to move between the furnace drum and the sealed chamber 11, so as to detect the high temperature resistivity of the single crystal silicon rod in the drawing stage in the single crystal furnace 20;

[0043] The sensing mechanism 14 is disposed in the sealed cavity 11 and is used to detect the distance between the resistivity measuring probe 12 and the single crystal silicon rod and the temperature at the detection position;

[0044] The processor 15 is in communication connection with the resistivity measuring probe 12, the sensing mechanism 14 and the transmission mechanism 13;

[0045] The processor 15 is provided with a resistivity control strategy. Based on the resistivity control strategy, the first normal-temperature resistivity of the single crystal silicon rod at room temperature is calculated according to the high-temperature resistivity of the single crystal silicon rod detected by the resistivity measuring probe 12, the distance from the resistivity measuring probe 12 to the single crystal silicon rod detected by the sensing mechanism 14, and the temperature of the detection position.

[0046] Specifically, Figure 1 and Figure 2As shown, the single crystal furnace 20 may include: a sub-chamber 21, a main chamber 22, a heater 23, a crucible 24 and a water-cooled heat shield 25, wherein the heater 23, the crucible 24 and the water-cooled heat shield 25 are arranged in the main chamber 22, the heater 23 is arranged around the crucible 24, and the water-cooled heat shield 25 is located above the crucible 24. The above-mentioned sealed chamber can be installed on the outer wall of the main chamber 22 and directly communicated with the main chamber 22. The sealed chamber 11 can also be installed on the outer wall of the sub-chamber 21 of the single crystal furnace 20; and directly communicated with the sub-chamber 21. It is worth noting that after the sealed chamber 11 is directly communicated with the sub-chamber 21, it is also communicated with the main chamber 22 through the sub-chamber 21. Regardless of whether the sealed chamber 11 is installed on the outer wall of the main chamber 22 or the outer wall of the sub-chamber 21, the sealed chamber 11 can be in a connected state with the main chamber 22 and the sub-chamber 21, or the online resistivity testing device can be in a non-working state, and one end of the sealed chamber 11 close to the main chamber 22 or the sub-chamber 21 is in a sealed state, and is connected with the main chamber 22 and the sub-chamber 21 only when the online resistivity testing device is in a working state.

[0047] It can be understood that when the sealed chamber 11 is connected with the main chamber 22 and the sub-chamber 21, the sealed chamber 11, the main chamber 22 and the sub-chamber 21 form a sealed environment. In other words, the sealed chamber 11 and the side wall of the sub-chamber 21 or the side wall of the main chamber 22 are sealed to ensure the single crystal silicon rod is pulled in a sealed environment.

[0048] Generally speaking, since the single crystal silicon rod 30 is pulled above the silicon solution, the online resistivity testing device is also located above the silicon solution. Preferably, the online resistivity testing device is located at the position of the sub-chamber 21, that is, the sealed chamber 11 can also be installed on the outer wall of the sub-chamber 21 of the single crystal furnace 20. More preferably, the online resistivity testing device is located at the lower position of the sub-chamber 21, close to the silicon solution.

[0049] By locating the online resistivity testing device at the position of the sub-chamber 21 (that is, the sealed chamber 11 can also be installed on the outer wall of the sub-chamber 21 of the single crystal furnace 20), the fluctuation of the test results caused by temperature is reduced, so that a better functional relationship can be established between the test results and the test results at room temperature, which is convenient for the subsequent timely adjustment of the doping amount of the dopant or master alloy in the silicon solution based on the online test results.

[0050] Among them, the resistivity measuring probe 12 can be a probe for testing resistivity, or it can be a rod-shaped structure including a support rod and a probe. For the rod-shaped structure including a support rod and a probe, an existing probe for testing resistivity can be installed at one end facing the inside of the furnace drum of the single crystal furnace 20, and the probe is connected to the processor 15 via a signal connection line.

[0051] Specifically, the transmission mechanism 13 drives the resistivity measuring probe 12 to move between the interior of the single crystal furnace 20 and the sealed chamber 11, and specifically means that when the online resistivity testing device is in the working state, the transmission mechanism 13 drives the resistivity measuring probe 12 to move toward the single crystal rod (i.e., the resistivity measuring probe 12 moves from the sealed chamber 11 to the interior of the single crystal furnace 20), and when the online resistivity testing device changes from the working state to the non-working state, the transmission mechanism 13 drives the resistivity measuring probe 12 to move in the direction away from the single crystal rod (i.e., the resistivity measuring probe 12 moves from the interior of the single crystal furnace 20 to the sealed chamber 11). The sealed chamber 11 and the transmission mechanism 13 cooperate to allow the resistivity measuring probe 12 to be recovered to the sealed chamber 11 in the non-working state. On the one hand, it will not affect the drawing of the single crystal silicon rod. On the other hand, the sealed chamber 11 protects the resistivity measuring probe 12 and ensures that the resistivity measuring probe 12 is always at the detection temperature, thereby avoiding the influence of large temperature fluctuations on the detection results of the resistivity measuring probe 12.

[0052] Specifically, the transmission mechanism 13 may include a driver and a telescopic rod, the telescopic rod may be a hard hollow rod, one end of the hard hollow rod is installed with the resistivity measuring probe 12, and the signal connecting line connected to the probe is located in the hard hollow rod. The driver is connected to the processor 15 through the signal connecting line. After receiving the driving signal sent by the processor 15, the driver drives the telescopic rod to extend toward the furnace barrel of the single crystal furnace 20, and the telescopic rod drives the resistivity measuring probe 12 to move into the furnace barrel; the driver can also drive the telescopic rod to shrink away from the furnace barrel of the single crystal furnace 20, and the telescopic rod drives the resistivity measuring probe 12 to move from the furnace barrel of the single crystal furnace 20 to the sealed cavity 11. In addition, the structure of the transmission mechanism 13 can also include: a driver, a slide rail located on the side wall of the sealed cavity 11 and a slide rod installed on the slide rail, the resistivity measuring probe 12 is installed on the slide rod at one end close to the furnace barrel of the single crystal furnace 20, the driver is electrically connected to the processor 15, and the driver drives the slide rod to move along the slide rail according to the driving signal sent by the processor 15, and the slide rod drives the resistivity measuring probe 12 to move into the furnace barrel of the single crystal furnace 20 or from the furnace barrel of the single crystal furnace 20 to the sealed cavity 11.

[0053] Among them, the sensing mechanism 14 may include a temperature sensor and a distance detection sensor. The temperature sensor and the distance detection sensor are fixed in the sealed cavity. For the temperature sensor included in the sensing mechanism 14, it detects the temperature at its location, and the temperature detected by the temperature sensor is used as the temperature of the detection position of the resistivity measurement probe 12 for the single crystal silicon rod. This is because the sealed cavity 11 is connected to the inside of the furnace drum, and heat from the furnace drum will enter the sealed cavity 11. The temperature of the area near the sealed cavity 11 inside the furnace drum will be basically consistent with the sealed cavity 11, and the area where the resistivity measurement probe 12 extends into the inside of the furnace drum is also close to the sealed cavity 11. The detection position of the resistivity measurement probe 12 for the single crystal silicon rod is also close to the sealed cavity 11. Therefore, the detection position of the resistivity measurement probe 12 for the single crystal silicon rod can be basically consistent with the temperature at the location of the temperature sensor. The temperature of the detection position generally refers to the temperature of the detection position of the resistivity measurement probe 12 for the single crystal silicon rod, that is, the detection position does not specifically refer to the location of the resistivity measurement probe 12, nor does it specifically refer to the location of the sensing mechanism 14.

[0054] In addition, the distance detection sensor included in the sensing mechanism 14 can detect the distance from the resistivity measurement probe 12 to the single crystal silicon rod, and can also detect whether the head of the single crystal silicon rod reaches the height where the resistivity measurement probe 12 is located. Specifically, a baffle that reflects light can be installed on the upper part of the resistivity measurement probe 12. The distance detection sensor generally emits light such as infrared or ultraviolet, and the light is reflected back to the distance detection sensor after reaching the baffle. The distance detector can obtain the distance between the distance detection sensor and the resistivity measurement probe 12 according to the reflection time of the light. In addition, the distance detector can also detect the distance between itself and the single crystal silicon rod through light. Based on the distance between the distance detection sensor and the resistivity measurement probe 12 and the distance between the distance detection sensor and the single crystal silicon rod, the distance from the resistivity measurement probe 12 to the single crystal silicon rod can be obtained. Whether the head of the single crystal silicon rod reaches the height of the resistivity measuring probe 12 detected by the distance detection sensor can be determined by the change of the light transmission time. Since the head of the single crystal silicon rod is the starting position of the single crystal silicon rod entering the equal diameter stage, before entering the equal diameter stage, the single crystal silicon rod is in the shoulder release stage. The diameter of the single crystal segment formed in the shoulder release stage is smaller than the diameter of the single crystal segment formed in the equal diameter stage. Therefore, compared with the single crystal segment formed in the equal diameter stage, the single crystal segment formed in the shoulder release stage reaches the height of the resistivity measuring probe 12, and the distance detection sensor receives the reflected light for a longer time. The single crystal segment formed in the equal diameter stage reaches the height of the resistivity measuring probe 12, and the distance detection sensor receives the reflected light for a shorter time. When the time for the distance detection sensor to receive the reflected light starts to shorten, it means that the head of the single crystal silicon rod reaches the height of the resistivity measuring probe 12. Further, the position of the single crystal silicon rod can also be detected by the sensing mechanism, so that the detection is started only after the height of the single crystal silicon rod reaches or exceeds the online resistivity testing device, which can further ensure the accuracy of the detection result.

[0055] Among them, the distance from the resistivity measurement probe 12 to the single crystal silicon rod generally refers to the shortest distance from the resistivity measurement probe 12 to the side wall of the single crystal silicon rod when the resistivity measurement probe 12 and the single crystal silicon rod are in a relatively static state after the resistivity measurement probe 12 is extended into the furnace, that is, the distance from the intersection of the extension line of the resistivity measurement probe 12 and the side wall of the single crystal silicon rod to the resistivity measurement probe 12.

[0056] In addition, the transmission mechanism 13 cooperates with the sensor mechanism 14 to control the distance between the resistivity measuring probe 12 and the single crystal silicon rod in the working state to be between 1 mm and 15 mm. For example, the distance can be 1 mm, 2 mm, 3 mm, 5 mm, 7 mm, 9 mm, 10 mm, 12 mm, 15 mm, etc. Preferably, the distance between the resistivity measuring probe 12 and the single crystal silicon rod is controlled to be between 1 mm and 3 mm.

[0057] According to the solution provided in the embodiment of the present invention, the doping concentration of the dopant in the silicon solution in the single crystal furnace 20 can be adjusted based on the high temperature resistivity of the single crystal silicon rod 30, the distance from the resistivity measuring probe 12 to the single crystal silicon rod, and the temperature of the detection position. The dopant in the silicon solution in the single crystal furnace 20 can be a dopant containing only one doping element, or a composite dopant containing at least two dopants. In particular, the above technical solution is applied to the case where the silicon solution in the single crystal furnace 20 contains a volatile dopant.

[0058] Since the online resistivity test device can know in real time whether the resistivity of the single crystal silicon rod meets the requirement, when the resistivity of the single crystal silicon rod does not meet the requirement, the resistivity detected by the online resistivity test device can be used to quickly adjust the doping amount of the silicon solution for pulling the next single crystal silicon rod, thereby reducing the yield of unqualified single crystal silicon rods. In addition, when the online resistivity test device determines that the resistivity of the single crystal silicon rod does not meet the requirement, if the current single crystal silicon rod pulling has not been completed, the current pulling can also be stopped in time, thereby further reducing the yield of unqualified single crystal silicon.

[0059] Through the above-mentioned online resistivity testing device, the high-temperature resistivity of the single crystal silicon rod in the pulling stage, the distance from the resistivity measuring probe corresponding to the high-temperature resistivity to the pulled single crystal silicon rod, and the temperature of the detection position can be detected at high temperature during the single crystal silicon rod pulling process, and based on these parameters, the doping concentration of the silicon solution dopant is adjusted to timely regulate the resistivity of the single crystal silicon rod, and based on the resistivity regulation strategy, the processor calculates the single crystal silicon rod according to the high-temperature resistivity of the single crystal silicon rod detected by the resistivity measuring probe, the distance from the resistivity measuring probe to the single crystal silicon rod detected by the sensing mechanism, and the temperature of the detection position. The first room temperature resistivity of the crystalline silicon rod at room temperature, that is, the high temperature resistivity detected online, can be used to calculate the resistivity of the single crystal silicon rod at room temperature. In particular, for the case where the actual resistivity of the single crystal silicon rod deviates greatly from the target resistivity due to the doping of volatile dopants such as antimony, there is no need to wait until the single crystal silicon rod is pulled and cooled to room temperature before detecting the resistivity of the single crystal silicon rod. The real-time resistivity during the pulling process can be obtained, so that the doping amount of the next single crystal silicon rod can be quickly adjusted based on the real-time resistivity, avoiding the production of single crystal silicon rods with inappropriate resistivity during the waiting cooling period in the prior art. Therefore, the online resistivity testing device provided in the embodiment of the present invention can timely adjust the resistivity of the single crystal silicon rod, especially for the single crystal silicon rod doped with volatile dopants, and can effectively improve the qualified rate and production efficiency of the produced single crystal silicon rods.

[0060] Specifically, the working principle of the above-mentioned online resistivity testing device can be as follows: the single crystal silicon rod 30 is continuously taken out from the silicon solution, and the single crystal silicon rod 30 is continuously moved upward under the action of the upper pulling. When the single crystal silicon rod 30 moves to the horizontal position of the online resistivity testing device, the sensing mechanism 14 will feed back the information to the processor 15. When the processor 15 recognizes the position of the single crystal silicon rod 30, the processor 15 sends a first driving signal to the transmission mechanism 13. The transmission mechanism 13 drives the resistivity measuring probe 12 to move to one side of the single crystal silicon rod 30 so that the resistivity measuring probe 12 moves from Figure 1 and Figure 3 The status shown changes to Figure 2 In the state shown, after the resistivity measuring probe 12 stops moving, the sensing mechanism 14 detects the distance between the resistivity measuring probe 12 and the single crystal silicon rod, and provides the distance to the processor 15. After the resistivity measuring probe 12 detects the resistivity, the resistivity is provided to the processor 15. After receiving the resistivity, the processor 15 sends a second driving signal to the transmission mechanism 13. The transmission mechanism 13 drives the resistivity measuring probe 12 again to move in a direction away from the single crystal silicon rod 30, that is, the resistivity measuring probe 12 moves away from the single crystal silicon rod 30. Figure 2 Status restored to Figure 1 and Figure 3 Status shown.

[0061] Moreover, when the resistivity measuring probe 12 is required to continuously detect the resistivity of the single crystal silicon rod, the sensing mechanism 14 can detect the measurement start position and the measurement end position. When the sensing mechanism 14 detects the measurement start position, the information that the single crystal silicon rod reaches the measurement start position can be fed back to the processor 15. The processor 15 sends a first drive signal to the transmission mechanism 13. The transmission mechanism 13 drives the resistivity measuring probe 12 to move toward one side of the single crystal silicon rod 30 to make the resistivity measuring probe 12 move. After the resistivity measuring probe 12 stops moving, the sensing mechanism 14 detects the resistivity. The distance from the measuring probe 12 to the single crystal silicon rod and the temperature of the detection position of the single crystal silicon rod are measured, and the distance and temperature are provided to the processor 15. As the single crystal silicon rod is pulled, the resistivity measuring probe 12 continuously detects the resistivity of the single crystal silicon rod at set time intervals. When the sensing mechanism 14 detects the end position of the measurement, the information that the single crystal silicon rod has reached the end position of the measurement can be fed back to the processor 15. The processor 15 sends a second driving signal to the transmission mechanism 13, and the transmission mechanism 13 then drives the resistivity measuring probe 12 to move away from the single crystal silicon rod 30.

[0062] The processor 15 is used to improve the automated control and processing of the online resistivity testing device, and can automatically calculate the first room-temperature resistivity of the single crystal silicon rod at room temperature and the doping concentration of the silicon solution dopant in the single crystal furnace 20, thereby reducing manual intervention and improving processing efficiency.

[0063] In addition, through the above process, the resistivity of the single crystal silicon rod can be detected when the single crystal silicon rod is pulled. When the resistivity deviates, the process can be directly adjusted to improve the yield rate of the produced single crystal silicon rod.

[0064] Further, the resistivity control strategy included in the processor 15 is obtained through training, for example, training is performed based on the high temperature resistivity of multiple single crystal silicon rods detected by the resistivity measurement probe 12, the distance from the resistivity measurement probe 12 to the single crystal silicon rod, the temperature at the detection position, and the corresponding second normal temperature resistivity detected by the same single crystal silicon rod at room temperature, to obtain a relationship function between the high temperature resistivity of the single crystal silicon rod, the distance from the resistivity measurement probe to the single crystal silicon rod, the temperature at the detection position, and the corresponding normal temperature resistivity of the single crystal silicon rod, and the relationship function is used as the resistivity control strategy. According to the resistivity control strategy, the normal temperature resistivity can be calculated based on the high temperature resistivity, distance, and temperature monitored in real time.

[0065] That is to say, the processor 15 obtains multiple sample data of the high temperature resistivity of multiple single crystal silicon rods 30 tested by the online resistivity testing device, the detection distance corresponding to the high temperature resistivity (the distance from the resistivity test probe 12 to the single crystal silicon rod 30), and the temperature corresponding to the detection position of the high temperature resistivity, and after the multiple single crystal silicon rods 30 are pulled, the temperature drops to room temperature, and the resistivity of the single crystal silicon rod 30 at room temperature is measured according to the feedback crystal position information to obtain the second normal temperature resistivity sample data. The high temperature resistivity of multiple single crystal silicon rods 30, the detection distance corresponding to the high temperature resistivity, the detection position corresponding to the high temperature resistivity, and the corresponding second normal temperature resistivity at room temperature are analyzed by the processor 15 to obtain the relationship function, which is the resistivity control strategy. In other words, the processor 15 can fit the temperature of the detection position, the detection position, and the distance from the resistivity test probe 12 to the single crystal silicon rod 30 according to the online measurement data and the normal temperature measurement data. The larger the amount of sample data, the more accurate the training result.

[0066] It can be understood that the second room temperature resistivity refers to the resistivity of multiple single crystal silicon rods at room temperature detected in the process of constructing the relationship function. The first room temperature resistivity is the result calculated by the processor 15 relationship function combined with the high temperature resistivity detected by the online resistivity test device, the distance from the resistivity measurement probe 12 to the single crystal silicon rod, and the temperature of the detection position. It is worth noting that the "first", "second", etc. involved in the embodiments of the present invention are to distinguish the sources of different parameters or structures, but not to limit the number or order of parameters or structures.

[0067] Since resistivity is related to carrier mobility, and carrier mobility is related to temperature, resistivity changes with temperature. Therefore, the processor 15 of the embodiment of the present invention trains a relationship function between resistivity and temperature through multiple sets of data. Based on the relationship function, the processor 15 of the present technical solution can calculate the first normal temperature resistivity at room temperature according to the high temperature resistivity measured in real time under a high temperature environment. This allows users to adjust the doping amount in the silicon solution based on the first normal temperature resistivity to ensure the accuracy of the adjustment.

[0068] Furthermore, the processor 15 can further calculate the doping amount of the dopant at the measuring point according to the calculated resistivity at room temperature, so that the operator can more intuitively adjust the doping amount of the next rod.

[0069] Furthermore, if Figure 1 and Figure 2 As shown, an embodiment of the present invention further provides a single crystal furnace 20. The single crystal furnace 20 may include a furnace body, the furnace body includes a main chamber and a sub-chamber, and a side wall of the main chamber and / or the sub-chamber is provided with an online resistivity test device installation hole penetrating the side wall; one or more online resistivity test devices provided in any of the above embodiments are installed in the online resistivity test device installation hole.

[0070] like Figure 1 and Figure 2 As shown, in the case where the single crystal furnace 20 includes a plurality of online resistivity testing devices, the plurality of online resistivity testing devices are evenly distributed along the circumference of the single crystal furnace 20. Preferably, the plurality of online resistivity testing devices are evenly distributed along the circumference of the sub-chamber 21 of the single crystal furnace 20.

[0071] More specifically, there are two online resistivity test devices. The line connecting the two online resistivity test devices passes through the cross-sectional diameter of the sub-chamber 21. That is, the line connecting the two online resistivity test devices passes through the diameter of the single crystal silicon rod in the radial direction, and the resistivity of the single crystal silicon rod can be measured in real time when the single crystal silicon rod grows, so that multiple online resistivity test devices can detect the resistivity of the single crystal silicon rod, making the detection result more accurate, thereby more accurately regulating the doping amount in the silicon solution.

[0072] Furthermore, based on the online resistivity testing device provided in the above embodiment, the embodiment of the present invention also provides two online resistivity testing methods.

[0073] Specifically, Figure 4 As shown, the first online resistivity testing method provided by the embodiment of the present invention. The online resistivity testing is performed based on the online resistivity testing device provided by the above embodiment. The online resistivity testing method may include the following steps:

[0074] Step S401: determining whether the head of the pulled single crystal silicon rod reaches the height where the resistivity measurement probe 12 is located;

[0075] Specifically, this step can be implemented in two specific ways.

[0076] The first implementation of this step is: the processor 15 estimates the height of the head of the single crystal silicon rod according to the pulling rate of the single crystal silicon rod and the time when the single crystal silicon rod starts to be pulled, and judges whether the head of the single crystal silicon rod reaches the height of the resistivity measurement probe 12 according to the result of the estimation. The pulling rate of the single crystal silicon rod is preset in the pulling program, and the time when the single crystal silicon rod starts to be pulled can also be obtained from the controller of the single crystal furnace.

[0077] The second implementation of this step is: the head of the single crystal silicon rod is detected by the sensor mechanism 14, and after the head of the single crystal silicon rod is detected, a signal indicating the start of detection is sent to the processor 15; after receiving the signal indicating the start of detection, the processor 15 determines that the head of the single crystal silicon rod has reached the height of the resistivity measurement probe 12. Among them, the sensor mechanism 14 emits light perpendicular to the axis of the single crystal silicon rod and receives the reflected light corresponding to the light. When the head of the single crystal silicon rod has not reached the height of the resistivity measurement probe 12, the time required for the sensor mechanism 14 to receive the reflected light is relatively long. When the head of the single crystal silicon rod reaches the height of the resistivity measurement probe 12, the time required for the sensor mechanism 14 to receive the reflected light is shortened. That is to say, at the time point when the time required for the sensor mechanism 14 to receive the reflected light changes significantly, it indicates that the head of the single crystal silicon rod has reached the height of the resistivity measurement probe 12.

[0078] Step S402: when it is determined that the head of the pulled single crystal silicon rod reaches the height of the resistivity measuring probe 12, the processor 15 sends a first driving signal to the transmission mechanism 13, the transmission mechanism 13 drives the resistivity measuring probe 12 to move toward the single crystal silicon rod, and starts detection, the high temperature resistivity of the head of the single crystal silicon rod is detected by the resistivity measuring probe 12, and the distance from the resistivity measuring probe 12 to the single crystal silicon rod and the temperature of the detection position are simultaneously detected by the sensing mechanism 14, the high temperature resistivity of the head of the single crystal silicon rod, the distance from the resistivity measuring probe 12 to the single crystal silicon rod and the temperature of the detection position are sent to the processor 15 of the online resistivity testing device, and the processor 15 calculates the first normal temperature resistivity of the single crystal silicon rod at room temperature based on the resistivity control strategy, according to the high temperature resistivity of the single crystal silicon rod detected by the resistivity measuring probe 12, the distance from the resistivity measuring probe 12 to the single crystal silicon rod detected by the sensing mechanism 14 and the temperature of the detection position;

[0079] Step S403 : after the detection is completed, the processor 15 sends a second driving signal to the transmission mechanism 13 , and the transmission mechanism 13 drives the resistivity measurement probe 12 to be retracted into the sealed cavity 11 .

[0080] Above Figure 4 The technical solution provided is mainly aimed at online detection of the high-temperature resistivity of the head of the single crystal silicon rod. The subsequent processor 15 can also use the above-mentioned trained relationship function, combined with the high-temperature resistivity of the head of the single crystal silicon rod, the distance from the resistivity measurement probe 12 to the head of the single crystal silicon rod, and the temperature of the head of the single crystal silicon rod, to calculate the resistivity of the head of the single crystal silicon rod at room temperature.

[0081] In addition, if Figure 5 As shown, the second online resistivity testing method provided by the embodiment of the present invention. The online resistivity testing is performed based on the online resistivity testing device provided by the above embodiment. The online resistivity testing method may include the following steps:

[0082] Step S501: When the sensor mechanism 14 detects that the measurement start position reaches the height of the resistivity measurement probe 12 of the online resistivity testing device, a signal indicating the start of measurement is sent to the processor 15 through the sensor mechanism 14;

[0083] The measurement start position may be set by the user according to the requirements. For example, the measurement start position may be the head of the single crystal silicon rod or the position where the single crystal silicon rod begins to shoulder.

[0084] Step S502: sending a third driving signal to the transmission mechanism 13 through the processor 15, driving the resistivity measurement probe 12 to move toward the single crystal silicon rod through the transmission mechanism 13, and starting detection;

[0085] Step S503: at set intervals, the high-temperature resistivity of the single crystal silicon rod at different axial positions is detected by the resistivity measuring probe 12, and the distance from the resistivity measuring probe 12 to the single crystal silicon rod and the temperature of the detection position are detected by the sensing mechanism 14 simultaneously, and the detected high-temperature resistivity of the head of the single crystal silicon rod, the distance from the resistivity measuring probe 12 to the single crystal silicon rod and the temperature of the detection position are sent to the processor 15, and the processor 15 calculates the first normal-temperature resistivity of the single crystal silicon rod at room temperature based on the resistivity control strategy, the high-temperature resistivity of the single crystal silicon rod detected by the resistivity measuring probe 12, the distance from the resistivity measuring probe 12 to the single crystal silicon rod detected by the sensing mechanism 14 and the temperature of the detection position;

[0086] Step S504: When the sensing mechanism 14 detects that the single crystal silicon rod reaches the height of the resistivity measuring probe 12 at the measurement end position, the sensing mechanism 14 sends a signal indicating the end of the test to the processor 15; the processor 15 sends a fourth driving signal to the transmission mechanism 13;

[0087] The measurement end position may also be set according to actual needs. For example, the measurement end position may be the end position of the equal diameter stage of the single crystal silicon rod, or may be the position of half the equal diameter length of the single crystal silicon rod.

[0088] Step S505: driving the resistivity measurement probe 12 through the transmission mechanism 13 to move the resistivity measurement probe 12 in a direction away from the single crystal silicon rod.

[0089] The introduction provided in the above steps is only used to help understand the structure, method and core idea of ​​the present invention. For ordinary technicians in this technical field, without departing from the principle of the present invention, several improvements and modifications can be made to the present invention, and these improvements and modifications also belong to the scope of protection of the claims of the present invention.

Claims

1. An online resistivity testing device, characterized in that: include: A sealed chamber (11), a resistivity measuring probe (12), a transmission mechanism (13), a sensor mechanism (14), and a processor (15), wherein: The sealed cavity (11) is installed on the outer wall of the single crystal furnace (20) and is in communication with the interior of the furnace barrel of the single crystal furnace (20); The resistivity measuring probe (12) is connected to the transmission mechanism (13), and is driven by the transmission mechanism (13) to move between the furnace barrel and the sealed chamber (11), so as to detect the high-temperature resistivity of the single crystal silicon rod in the drawing stage in the single crystal furnace (20); The sensing mechanism (14) is arranged in the sealed cavity (11) and is used to detect the distance between the resistivity measuring probe (12) and the single crystal silicon rod and the temperature at the detection position; The processor (15) is communicatively connected with the resistivity measuring probe (12), the sensing mechanism (14) and the transmission mechanism (13); The processor (15) is provided with a resistivity control strategy, and based on the resistivity control strategy, a first normal temperature resistivity of the single crystal silicon rod at normal temperature is calculated according to the high temperature resistivity of the single crystal silicon rod detected by the resistivity measurement probe (12), the distance from the resistivity measurement probe (12) to the single crystal silicon rod detected by the sensor mechanism (14), and the temperature of a detection position.

2. The online resistivity testing device according to claim 1, characterized in that: The sealed cavity (11) is installed on the outer side wall of the sub-chamber (21) of the single crystal furnace (20); The sealed chamber (11) is in communication with the secondary chamber (21).

3. The online resistivity testing device according to claim 1, characterized in that: The resistivity control strategy is obtained by training multiple sample data based on the high temperature resistivity of the single crystal silicon rod, the distance from the resistivity measurement probe (12) to the single crystal silicon rod, the temperature of the detection position, and the room temperature resistivity of the single crystal silicon rod.

4. The online resistivity testing device according to claim 3, characterized in that: The resistivity control strategy is a relationship function between the high-temperature resistivity of the single crystal silicon rod, the distance from the resistivity measurement probe (12) to the single crystal silicon rod, the temperature at the detection position, and the room-temperature resistivity of the single crystal silicon rod obtained by training based on multiple sample data of the high-temperature resistivity of the single crystal silicon rod, the distance from the resistivity measurement probe (12) to the single crystal silicon rod, the temperature at the detection position, and the room-temperature resistivity of the single crystal silicon rod.

5. A single crystal furnace, characterized in that: include: The furnace body comprises a main chamber and a sub-chamber, and a side wall of the main chamber and / or the sub-chamber is provided with an installation hole for an online resistivity test device penetrating the side wall; One or more online resistivity testing devices according to any one of claims 1 to 4 are installed in the online resistivity testing device installation hole.

6. The single crystal furnace according to claim 5, characterized in that: In the case where there are multiple online resistivity testing devices, The plurality of online resistivity testing devices are evenly distributed along the circumference of the single crystal furnace (20).

7. An online resistivity testing method, characterized in that: Based on the online resistivity testing device described in any one of claims 1 to 4, the online resistivity testing method includes: Step 1, determining whether the head of the pulled single crystal silicon rod reaches the height where the resistivity measuring probe (12) is located; Step 2: When it is determined that the head of the pulled single crystal silicon rod reaches the height where the resistivity measuring probe (12) is located, the processor (15) sends a first drive signal to the transmission mechanism (13), and the transmission mechanism (13) drives the resistivity measuring probe (12) to move in the direction of the single crystal silicon rod and starts detection, and detects the high-temperature resistivity of the head of the single crystal silicon rod through the resistivity measuring probe (12), and simultaneously detects the distance from the resistivity measuring probe (12) to the single crystal silicon rod and the temperature at the detection position through the sensing mechanism (14), and detects the high-temperature resistivity of the head of the single crystal silicon rod. The measured high-temperature resistivity of the head of the single crystal silicon rod, the distance from the resistivity measuring probe (12) to the single crystal silicon rod, and the temperature at the detection position are sent to a processor (15) of the online resistivity testing device; the processor (15) calculates a first normal-temperature resistivity of the single crystal silicon rod at normal temperature based on the resistivity control strategy, the high-temperature resistivity of the single crystal silicon rod detected by the resistivity measuring probe (12), the distance from the resistivity measuring probe (12) to the single crystal silicon rod detected by the sensing mechanism (14), and the temperature at the detection position; Step 2: After the detection is completed, the processor (15) sends a second drive signal to the transmission mechanism (13), and the transmission mechanism (13) drives the resistivity measurement probe (12) to be retracted into the sealed cavity (11).

8. The online resistivity testing method according to claim 7, characterized in that: Step 1 includes: The processor (15) estimates the height of the head of the single crystal silicon rod according to the pulling rate of the single crystal silicon rod and the time when the single crystal silicon rod starts to be pulled, and determines whether the head of the single crystal silicon rod reaches the height of the resistivity measurement probe (12) according to the estimation result.

9. The online resistivity testing method according to claim 7, characterized in that: Step 1 includes: The head of the single crystal silicon rod is detected by the sensing mechanism (14), and after the head of the single crystal silicon rod is detected, a signal indicating the start of detection is sent to the processor (15); after receiving the signal indicating the start of detection, the processor (15) determines that the head of the single crystal silicon rod has reached the height at which the resistivity measurement probe (12) is located.

10. An online resistivity testing method, characterized in that: Based on the online resistivity testing device described in any one of claims 1 to 4, the online resistivity testing method includes: Step A, when the sensor mechanism (14) detects that the measurement start position reaches the height of the resistivity measurement probe (12) of the online resistivity testing device, sending a signal indicating the start of measurement to the processor (15) through the sensor mechanism (14); Step B: sending a third drive signal to the transmission mechanism (13) via the processor (15), driving the resistivity measurement probe (12) to move in the direction of the single crystal silicon rod via the transmission mechanism (13), and starting detection; Step C: at set intervals, the resistivity measuring probe (12) is used to detect the high-temperature resistivity of the single crystal silicon rod at different axial positions, and the sensing mechanism (14) is used to simultaneously detect the distance from the resistivity measuring probe (12) to the single crystal silicon rod and the temperature at the detection position, and the detected high-temperature resistivity of the head of the single crystal silicon rod, the distance from the resistivity measuring probe (12) to the single crystal silicon rod, and the temperature at the detection position are sent to a processor (15); the processor (15) calculates a first normal-temperature resistivity of the single crystal silicon rod at normal temperature based on the resistivity control strategy, the high-temperature resistivity of the single crystal silicon rod detected by the resistivity measuring probe (12), the distance from the resistivity measuring probe (12) to the single crystal silicon rod, and the temperature at the detection position detected by the sensing mechanism (14); Step D: When the sensing mechanism (14) detects that the single crystal silicon rod has reached the height of the resistivity measuring probe (12) of the online resistivity testing device at the measurement end position, the sensing mechanism (14) sends a signal indicating the end of the test to the processor (15); and the processor (15) sends a fourth drive signal to the transmission mechanism (13); Step E: driving the resistivity measurement probe (12) by the transmission mechanism (13) to move the resistivity measurement probe (12) in a direction away from the single crystal silicon rod.