Lead frame manufacturing process and lead frame

By designing inverted T-shaped design circuits and buckle bumps on the lead frame, the problem of insufficient binding force of the positioning frame is solved, the chip packaging and soldering reliability is improved, and the stability of the injection molding process and the tin crimping of the outer foot is ensured. ability.

CN119028830AActive Publication Date: 2024-11-26YINGTONG MICRO INNOVATION TECH (DONGGUAN) CO LTD
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
CN202411094922.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-11
Publication Date
2024-11-26
Estimated Expiration
2044-08-11

AI Technical Summary

Technical Problem

The binding force of the existing lead frame during the injection molding process is poor, resulting in a reduced reliability of the chip. In the subsequent SMT process, the external foot is not easy to form tin crawler, and the soldering reliability is low, especially for automotive products that require high packaging reliability. insufficient.

Method used

By performing the first semi-etch and the second etch on the design line of the lead frame, an inverted T-shaped cross-section of the design line is formed, and the bottom is bulging horizontally to form a buckle and convex convex to enhance the binding force of the positioning frame and at the top The first and second buckle bulges are made on the surface to increase the bonding force between the rubber shell and the lead frame and ensure that the injection molding pressure does not cause displacement.

Benefits of technology

It improves the packaging reliability and soldering reliability of the chip, prevents the displacement of the positioning frame, enhances the tin crawling ability of the outer foot, and improves the overall reliability of the chip.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119028830A_ABST
    Figure CN119028830A_ABST
Patent Text Reader

Abstract

A lead frame manufacturing process and a lead frame relate to the technical field of lead frames. The lead frame comprises a design circuit and a positioning frame, and the bottom of the design circuit transversely protrudes to form a buckle rubber transverse protrusion. The manufacturing process comprises the steps that first-time etching is conducted, specifically, according to a design circuit of the lead frame, half-etching is conducted on the area outside the design circuit in the longitudinal direction from the top face of the metal substrate, and half-etching refers to non-etching-through; glue filling: filling insulating plastic at the half-etched part to form a positioning frame so as to position the designed circuit; etching for the second time: longitudinally etching from the bottom surface of the metal substrate, and etching through the half-etched position in the step of etching for the first time; the etching area from the bottom surface of the metal substrate to the corresponding area is smaller than the etching area from the top surface of the metal substrate to the corresponding area, so that the bottom of the designed circuit transversely protrudes to form a buckle rubber transverse protrusion. And the buckle rubber transverse bulge supports the positioning frame on the bottom surface of the positioning frame, so that the positioning frame does not move downwards when bearing injection molding pressure, and the reliability of the chip is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of chip packaging, and in particular to the technical field of lead frames. Background Art

[0002] Semiconductor packaging is the production process of packaging crystal grains (also known as wafers) into chips. In this production process, the lead frame is one of the very important components needed.

[0003] The size of the grain is usually very small, but it has many ports that need to be electrically connected to the external circuit. These ports cannot be directly electrically connected to the external circuit due to the small size of the grain. Therefore, when packaging the grain, it is necessary to use a lead frame to lead out the ports that need to be electrically connected to the external circuit so that the chip formed after packaging can be directly electrically connected to the external circuit.

[0004] The Chinese patent with the patent number ZL201710677235.8 discloses a lead frame manufacturing process, which forms a design circuit after two etchings. The lateral width of the design circuit on the top and bottom surfaces is consistent, and its side is straight (see part d of Figure 3 of the patent specification). In the process of chip packaging, after attaching the die and welding wires, it is necessary to form a plastic shell to protect the die and welding wires through injection molding. There is injection molding pressure during the injection molding process, and the injection molding pressure is applied to the positioning frame from top to bottom. The positioning frame is only combined with the straight side of the design circuit, and the bonding force is poor. After bearing the above injection molding pressure, it may move downward, resulting in reduced reliability of the chip product. After the positioning frame moves downward, it is flush with the outer foot, resulting in the outer foot not protruding downward. In the subsequent SMT process, the outer foot is not easy to form tin creep, and the welding reliability is also reduced. Although this lead frame can be used in most IC products, there are still some shortcomings in reliability for automotive products with high packaging reliability requirements. Summary of the invention

[0005] In view of this, the lead frame manufacturing process and the lead frame provided by the present invention have higher reliability of the packaged chip.

[0006] To achieve the above objectives, the present invention provides the following technical solutions.

[0007] 1. The lead frame manufacturing process includes the following steps: First etching: according to the design circuit of the lead frame, half-etching is performed longitudinally from the top surface of the metal substrate to the area outside the design circuit, where half-etching means that no etching is performed; Filling: Filling the semi-etched part with insulating plastic to form a positioning frame to position the designed circuit; Second etching: Etching vertically from the bottom surface of the metal substrate to etch through the half-etched position in the first etching step; The etching area of ​​the corresponding region from the bottom surface of the metal substrate is smaller than the etching area of ​​the corresponding region from the top surface of the metal substrate, so that the bottom of the designed circuit protrudes laterally to form a glue-locking transverse protrusion.

[0008] When the lead frame is used for chip packaging, plastic sealing is performed after the crystal grain is affixed to the top surface and the wires are bonded. Plastic sealing is performed by injection molding from the top surface to form a plastic shell of the chip to protect the crystal grain and the wire bonding circuits. There is injection pressure during the injection molding process, and this injection molding pressure is applied downward to the positioning frame. The lateral width of the designed circuit on the bottom surface is greater than its lateral width on the top surface, and a glue-locking horizontal convex is formed at the bottom. The longitudinal section of the designed circuit is similar to an inverted T shape. The glue-locking horizontal convex supports the positioning frame on the bottom surface of the positioning frame so that the positioning frame will not move downward when it is subjected to the above-mentioned injection molding pressure. On the one hand, this improves the reliability of the chip, and on the other hand, the positioning frame will not be flush with the part of the designed circuit on the bottom surface. Part of the bottom surface of the designed circuit is the outer foot, and the outer foot protrudes downward. In the subsequent SMT process, the outer foot is prone to tin creep, and the welding reliability is higher.

[0009] 2. On the basis of technical solution 1, the designed circuit includes pins and a base for attaching a chip. After the glue filling step, a first glue-locking protrusion that is upwardly protruding and conductive is formed on the top surface of the pin, and the first glue-locking protrusion extends laterally to clamp the positioning frame. After the positioning frame is formed by filling the glue, the top surface is usually ground and polished to remove the overflowing glue. The top surface is therefore flattened. When the crystal grain is attached to the top surface and the wire is welded, the bonding surface between the glue shell formed by the plastic sealing and the top surface of the lead frame is a plane, and the bonding force is poor, which is prone to lateral displacement, thereby reducing the reliability of the chip. The first glue-locking protrusion is formed in a partial area of ​​the top surface of the designed circuit (i.e., the inner foot), and the first glue-locking protrusion is inserted into the glue shell formed after the plastic sealing. The bonding surface between the glue shell and the top surface of the lead frame is not a plane, but has bumps and depressions, so the bonding force is strong, and the glue shell is not prone to lateral displacement, thereby improving the reliability of the chip.

[0010] 3. Based on Technical Solution 2, the longitudinal thickness of the first buckle protrusion is 5μm-150μm, and the lateral width extending laterally above the positioning frame is 5μm-200μm.

[0011] 4. Based on technical solution 2, the first glue bump is made by electroplating process. Electroplating is a necessary process for making lead frame. Using electroplating process to make the first glue bump can save process and no additional process needs to be designed for production.

[0012] 5. On the basis of technical solution 4, copper or nickel is electroplated to form a first buckle protrusion, and silver or nickel-palladium-gold is electroplated on the first buckle protrusion to form a welding line surface. The inner foot usually needs to be electroplated to form a welding line surface. The thickness of the welding line surface is usually relatively thin and cannot serve as the first buckle protrusion. Moreover, the welding line surface is usually electroplated with precious metals such as silver or nickel-palladium-gold. If a thicker welding line surface is electroplated to serve as the first buckle protrusion at the same time, the cost is relatively high. Therefore, copper or nickel is electroplated to form the first buckle protrusion first, and then silver or nickel-palladium-gold is electroplated on it to form the welding line surface, so as to reduce costs.

[0013] 6. Based on the technical solution 1, in the first etching step, a part of the area outside the design circuit on the top surface of the metal substrate is shielded, and the part of the area is located directly above the glue-locking transverse protrusion. During etching, the part of the area is cut off in the longitudinal direction to form a second glue-locking protrusion protruding upward on the glue-locking transverse protrusion. After the positioning frame is formed by filling the glue, the second glue-locking protrusion is inserted into the positioning frame, which can further increase the bonding force between the positioning frame and the design circuit, is not easy to loosen or break, and improves the reliability of the packaged chip.

[0014] 7. Based on Technical Solution 1, in the first etching step, the etching depth of the half etching is 1 / 2-4 / 5 of the thickness of the metal substrate.

[0015] 8. A lead frame is manufactured using the manufacturing process described in Technical Solution 1-7, including a design circuit and a positioning frame. The bottom of the design circuit protrudes laterally to form a glue-locking transverse protrusion to clamp the bottom surface of the positioning frame to prevent the positioning frame from moving downward.

[0016] 9. Based on technical solution 8, the design circuit includes a pin and a base for attaching a chip, and the top surface of the pin is provided with a first adhesive protrusion that is upwardly protruding and conductive, and the first adhesive protrusion extends laterally to clamp the positioning frame.

[0017] 10. Based on technical solution 8, a second glue buckle protrusion is provided on the glue buckle transverse protrusion, which protrudes upward and is inserted into the positioning frame. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a schematic structural diagram of the lead frame of the present invention.

[0019] Figure 2 For Figure 1 The AA section is a schematic diagram of each step of the lead frame manufacturing process of this embodiment.

[0020] Reference numerals include: Base 1, pin 2, inner pin 21, first glue buckle protrusion 211, welding line surface 212, outer pin 22, glue buckle transverse protrusion 221, second glue buckle protrusion 222, metal substrate 3, positioning frame 4, photosensitive film 5. DETAILED DESCRIPTION

[0021] The present invention is described in detail below in conjunction with specific embodiments.

[0022] like Figure 1 and Figure 2 As shown in part f of the figure, the lead frame of this embodiment includes a base 1, pins 2 and a positioning frame 4. In the process of manufacturing the lead frame, the base 1 and the pins 2 are collectively referred to as the design circuit. The base 1 and each pin 2 are fixed by the positioning frame 4, the relative position has been determined, and there is no electrical connection between them. After packaging the chip, there is no need to cut off the electrical connection between the base 1 and each pin 2 by cutting. Figure 2 As shown in part f, the top and bottom of the pin 2 are the inner pin 21 and the outer pin 22 respectively. The outer pin 22 protrudes laterally to form a glue-locking transverse protrusion 221. The base 1 is also formed with a similar glue-locking transverse protrusion 221. The cross-sectional shape of the base 1 and the pin 2 is similar to an inverted T shape. The glue-locking transverse protrusion 221 is stuck on the bottom surface of the positioning frame 4, so that the positioning frame 4 will not move downward when it is subjected to the injection pressure during the subsequent chip packaging process. This improves the reliability of the chip on the one hand, and on the other hand, the positioning frame 4 will not be flush with the outer pin 22 on the bottom surface. The outer pin 22 protrudes downward, and in the subsequent SMT process, the outer pin 22 is easy to form tin creep, and the welding reliability is higher.

[0023] After the glue is filled to form the positioning frame 4, the top surface is usually polished to remove the overflowed glue. The top surface is thus ground flat. When the die is attached to the top surface and the wires are welded, the bonding surface between the plastic shell formed by the plastic sealing and the top surface of the lead frame is a flat surface, which has a poor bonding force and is prone to lateral displacement, thereby reducing the reliability of the chip. Figure 2 As shown in parts d and f, the top surface of the inner foot 21 is electroplated twice to form a first glue protrusion 211 and a welding surface 212. The first glue protrusion 211 extends horizontally to clamp the positioning frame. The first glue protrusion 211 is made of electroplated copper or nickel, and the welding surface 212 is made of electroplated silver or precious metals such as nickel-palladium-gold. In the subsequent chip packaging process, the first glue protrusion 211 and the welding surface 212 are inserted into the plastic shell formed after plastic packaging. The bonding surface between the plastic shell and the top surface of the lead frame is not flat, but has bumps and depressions, so the bonding force is strong, and the plastic shell is not prone to lateral displacement, thereby improving the reliability of the chip.

[0024] like Figure 2 As shown in parts e and f of the figure, a second glue protrusion 222 protruding upward is provided on the glue horizontal protrusion 221. After the positioning frame 4 is formed by filling the glue, the second glue protrusion 222 is inserted into the positioning frame 4, which can further increase the bonding force between the positioning frame 4 and the designed circuit, making it less likely to loosen or break, thereby improving the reliability of the packaged chip.

[0025] Figure 2 Part f is a cross-sectional view of the finished lead frame of this embodiment.

[0026] like Figure 2 As shown, the lead frame manufacturing process of this embodiment includes the following steps: The top surface is exposed and developed. Figure 2 As shown in part a of FIG. 1 , a photosensitive film 5 is attached to the top and bottom surfaces of the metal substrate 3, and then only the top surface is exposed and developed according to the design circuit, forming a portion of the top surface design circuit to be shielded, and a portion of the area next to the portion is also shielded. The top surface is the surface for attaching the grain.

[0027] The first etching. Figure 2 As shown in part b, half etching is performed longitudinally from the top surface of the metal substrate 3. Half etching means that it is not etched through. In this embodiment, the etching depth of half etching is 1 / 2-4 / 5 of the thickness of the metal substrate. The designed circuits such as the pin 2 and the base 1 are not etched. The top of the pin 2 is the inner pin 21. The shielding formed in the area beside the designed circuit is cut off by side etching during this etching process. Therefore, upward protrusions are formed at the corresponding positions at the bottom of the groove formed by etching. These protrusions are second glue-locking protrusions 222.

[0028] Filling. Figure 2 As shown in part c of the figure, the semi-etched part is filled with insulating plastic to form a positioning frame 4 to position the base 1 and the pin 2. The second glue-locking protrusion 222 is inserted into the positioning frame 4. After the positioning frame 4 is formed by filling the glue, the top surface is polished to remove impurities such as overflowing glue.

[0029] Two times electroplating. Figure 2 As shown in the d part, the top surface of the inner foot 21 is electroplated twice in succession. The first electroplating is copper or nickel to form a first buckle protrusion 211. The longitudinal thickness of the first buckle protrusion 211 is 5μm-150μm. The electroplating is performed on the flattened surface. As the electroplating thickness increases, the plating layer also grows to the side, so that the first buckle protrusion 211 extends horizontally to clamp the positioning frame 4. The horizontal width extending horizontally to the top of the positioning frame is 5μm-200μm. Silver or nickel palladium gold is electroplated on the first buckle protrusion 211 to form a welding line surface 212. The inner foot 21 usually needs to be electroplated to form a welding line surface 212. The thickness of the welding line surface 212 is usually relatively thin and cannot serve as the first buckle protrusion 211. Moreover, the welding line surface 212 is usually electroplated with precious metals such as silver or nickel palladium gold. If a thicker welding line surface 212 is electroplated to serve as the first buckle protrusion 211 at the same time, the cost is relatively high. Therefore, copper or nickel is electroplated first to form the first glue buckle protrusion 211, and then silver or nickel-palladium-gold is electroplated thereon to form the wire bonding surface 212, so as to reduce the cost.

[0030] The bottom surface is exposed and developed. Figure 2 As shown in part e, the bottom surface is developed and exposed according to the designed circuit.

[0031] Second etching. Figure 2As shown in part f, the metal substrate 3 is etched longitudinally from the bottom surface to etch through the half-etched position in the first etching step, so that the bottom of the lead forms an outer leg 22. The etching area of ​​this etching is smaller than the etching area of ​​the first etching. Therefore, the lateral width of the outer leg 22 is greater than the lateral width of the inner leg 21, and the lateral width of the bottom of the base 1 is greater than the lateral width of the top of the base 1. The outer leg 22 and the bottom of the base 1 both protrude laterally to form a glue-fastening transverse protrusion 221.

[0032] It should be noted that the process disclosed in the Chinese patent with patent number ZL201710677235.8 can also be adopted, first electroplating to form the first glue protrusion 211 and then performing the first etching.

[0033] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention, rather than to limit the scope of protection of the present invention. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the essence and scope of the technical solution of the present invention.

Claims

1. Lead frame manufacturing process, characterized by: The following steps are involved: First etching: according to the design circuit of the lead frame, half-etching is performed longitudinally from the top surface of the metal substrate to the area outside the design circuit, where half-etching means that no etching is performed; Filling: Filling the semi-etched part with insulating plastic to form a positioning frame to position the designed circuit; Second etching: Etching vertically from the bottom surface of the metal substrate to etch through the half-etched position in the first etching step; The etching area of ​​the corresponding region from the bottom surface of the metal substrate is smaller than the etching area of ​​the corresponding region from the top surface of the metal substrate, so that the bottom of the designed circuit protrudes laterally to form a glue-locking transverse protrusion.

2. The lead frame manufacturing process according to claim 1, characterized in that: The designed circuit includes pins and a base for attaching a chip. After the glue filling step, a first glue-locking protrusion that is upwardly protruding and conductive is formed on the top surface of the pin, and the first glue-locking protrusion extends horizontally to clamp the positioning frame.

3. The lead frame manufacturing process according to claim 2, characterized in that: The longitudinal thickness of the first buckle glue protrusion is 5 μm-150 μm, and the lateral width extending laterally to the top of the positioning frame is 5 μm-200 μm.

4. The lead frame manufacturing process according to claim 2, characterized in that: The first buckle protrusion is made by electroplating process.

5. The lead frame manufacturing process according to claim 4, characterized in that: The first buckle protrusion is formed by electroplating copper or nickel, and silver or nickel-palladium-gold is electroplated on the first buckle protrusion to form a welding line surface.

6. The lead frame manufacturing process according to claim 1, characterized in that: In the first etching step, a partial area outside the designed circuit on the top surface of the metal substrate is blocked, and the partial area is located directly above the glue buckle transverse protrusion. During etching, the partial area is etched off in the longitudinal upper side to form a second glue buckle protrusion protruding upward on the glue buckle transverse protrusion.

7. The lead frame manufacturing process according to claim 1, characterized in that: In the first etching step, the etching depth of the half etching is 1 / 2-4 / 5 of the thickness of the metal substrate.

8. A lead frame, characterized in that It is made by the manufacturing process described in claims 1-7, and includes a design circuit and a positioning frame. The bottom of the design circuit protrudes laterally to form a glue-locking transverse protrusion to clamp the bottom surface of the positioning frame to prevent the positioning frame from moving downward.

9. The lead frame according to claim 8, wherein: The designed circuit includes a pin and a base for attaching a chip. The top surface of the pin is provided with a first adhesive buckle protrusion which is upwardly protruding and conductive. The first adhesive buckle protrusion extends out horizontally to clamp the positioning frame.

10. The lead frame according to claim 8, wherein: The glue buckle transverse protrusion is provided with a second glue buckle protrusion which protrudes upward and is inserted into the positioning frame.

Citation Information

Patent Citations

  • QFN (quad flat non-lead) package with multiple circles of pins and manufacturing method thereof

    CN102339809A

  • Manufacturing method for pre-packaged lead frame

    CN105470232A

  • Lead frame manufacturing method

    CN107393896A

  • Lead frame and manufacturing technology thereof

    CN107492536A

  • Method for forming lead frame structure

    CN116266540A