Semiconductor structure and forming method thereof
By designing a copper pad shape and multi-layer open structure with high perimeter-to-area ratio in the semiconductor structure, the problem of copper pad stress on the interlayer dielectric layer is solved, and the reliability and performance of the device are improved.
Patent Information
- Application Number
- CN202310583489.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-23
- Publication Date
- 2024-11-26
AI Technical Summary
The stress problems of existing copper-welded pad structures between hard copper and interlayer dielectric layers have led to degradation of device reliability and performance. Especially in small technical nodes and copper-welded pad structures, the corner stress of the welding pad is high, and there is a lack of effective reduction. Measures for small stress.
By designing a special metal welding pad structure in a semiconductor structure, the contact area between the welding pad and the interlayer dielectric layer is increased and the weight of the welding pad is reduced. Multi-layer open structure and through-hole structure are adopted, and photoresist layer and mask technology are used to engrave The etching forms a welding pad shape with a high circumference and area ratio, reducing the stress of the welding pad on the interlayer dielectric layer.
It effectively reduces the stress of metal welding pads on the interlayer dielectric layer, improves the reliability and performance of the device, and ensures the stability of welding and bonding.
Smart Images

Figure CN119028939A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductor technology, and in particular to a semiconductor structure and a method for forming the same. Background Art
[0002] In the semiconductor back-end process, multi-layer metal pads and through-hole structures are usually used for electrical connection as metal wiring layers. However, in the current metal pad technology, especially for small technology nodes and copper pad structures, some reliability issues will occur due to the high stress between hard copper and interlayer dielectric layers. This is because copper pads are harder than aluminum pads and are always rectangular or square in shape. During processes such as deposition, chemical mechanical polishing processes or thermal cycles, stress is usually induced, especially at the pad corners. So far, there are no suitable measures to reduce the stress from the pad corners.
[0003] Therefore, it is necessary to provide a new copper pad design structure to reduce the stress of the copper pad on the interlayer dielectric layer, and ultimately improve the device performance. Summary of the invention
[0004] The present application provides a semiconductor structure and a method for forming the same, which can reduce the stress of a metal pad on an interlayer dielectric layer, thereby improving device reliability and device performance.
[0005] One aspect of the present application provides a method for forming a semiconductor structure, comprising: providing a substrate, wherein an interlayer dielectric layer is formed on the surface of the substrate; etching the interlayer dielectric layer to form a first opening that does not penetrate the interlayer dielectric layer; etching the interlayer dielectric layer at the bottom of the first opening to form a second opening that does not penetrate the interlayer dielectric layer, wherein the interlayer dielectric layer located at the bottom of the first opening and outside the second opening includes a first portion located at the center of the bottom of the first opening and a second portion surrounding the first portion; etching the interlayer dielectric layer located at the first portion to form a third opening exposing the substrate; filling a metal material layer in the first opening, the second opening, and the third opening, wherein the metal material layers in the first opening and the second opening constitute a metal pad, and the metal material layer in the third opening constitutes a through-hole structure.
[0006] In some embodiments of the present application, the method for forming the first opening includes: forming a hard mask layer on the surface of the interlayer dielectric layer; forming a patterned first photoresist layer on the surface of the hard mask layer, the patterned first photoresist layer defining the position of the first opening; etching the hard mask layer and the interlayer dielectric layer using the patterned first photoresist layer as a mask to form the first opening; and removing the patterned first photoresist layer.
[0007] In some embodiments of the present application, the method for forming the second opening includes: forming a first sacrificial layer in the first opening and on the surface of the hard mask layer; forming a patterned second photoresist layer on the surface of the first sacrificial layer, the patterned second photoresist layer defining the position of the second opening; etching the first sacrificial layer and the interlayer dielectric layer using the patterned second photoresist layer as a mask to form the second opening; and removing the patterned second photoresist layer and the first sacrificial layer.
[0008] In some embodiments of the present application, the method for forming the third opening includes: forming a second sacrificial layer in the first opening and the second opening and on the surface of the hard mask layer; forming a patterned third photoresist layer on the surface of the second sacrificial layer, the patterned third photoresist layer defining the position of the third opening; etching the second sacrificial layer and the interlayer dielectric layer using the patterned third photoresist layer as a mask to form the third opening; and removing the patterned third photoresist layer and the second sacrificial layer.
[0009] In some embodiments of the present application, the method for forming the metal pad and the through-hole structure includes: forming a metal material layer in the first opening, the second opening, and the third opening and on the surface of the hard mask layer; removing the metal material layer and the hard mask layer above the upper surface of the interlayer dielectric layer, the metal material layer in the first opening and the second opening constituting a metal pad, and the metal material layer in the third opening constituting a through-hole structure.
[0010] In some embodiments of the present application, the cross-sectional shape of the first opening is a shape in which the ratio of the square of the perimeter to the area is greater than 16.
[0011] In some embodiments of the present application, the cross-sectional shape of the first opening includes a rounded rectangle, a bowl-cornered rectangle, a beveled rectangle, or an obtuse-cornered rectangle.
[0012] In some embodiments of the present application, a partial profile of the cross-sectional figure of the second opening is the same as a profile of the cross-sectional figure of the first opening.
[0013] In some embodiments of the present application, the shape of the second portion includes a circular ring, a polygonal ring, or a discontinuous ring.
[0014] In some embodiments of the present application, a depth of the first opening is 20% to 40% of a thickness of the interlayer dielectric layer.
[0015] In some embodiments of the present application, a depth of the second opening is 40% to 60% of a thickness of the interlayer dielectric layer.
[0016] Another aspect of the present application also provides a semiconductor structure, including: a substrate, an interlayer dielectric layer is formed on the surface of the substrate, a first opening that does not penetrate the interlayer dielectric layer is formed in the interlayer dielectric layer, a second opening that does not penetrate the interlayer dielectric layer is formed in the interlayer dielectric layer at the bottom of the first opening, the interlayer dielectric layer located at the bottom of the first opening and outside the second opening includes a first part located at the center of the bottom of the first opening and a second part surrounding the first part, the interlayer dielectric layer of the first part is etched to form a third opening exposing the substrate; a metal pad is located in the first opening and the second opening; and a through-hole structure is located in the third opening.
[0017] In some embodiments of the present application, the cross-sectional shape of the first opening is a shape in which the ratio of the square of the perimeter to the area is greater than 16.
[0018] In some embodiments of the present application, the cross-sectional shape of the first opening includes a rounded rectangle, a bowl-cornered rectangle, a beveled rectangle, or an obtuse-cornered rectangle.
[0019] In some embodiments of the present application, a partial profile of the cross-sectional figure of the second opening is the same as a profile of the cross-sectional figure of the first opening.
[0020] In some embodiments of the present application, the shape of the second portion includes a circular ring, a polygonal ring, or a discontinuous ring.
[0021] In some embodiments of the present application, a depth of the first opening is 20% to 40% of a thickness of the interlayer dielectric layer.
[0022] In some embodiments of the present application, a depth of the second opening is 40% to 60% of a thickness of the interlayer dielectric layer.
[0023] The present application provides a semiconductor structure and a method for forming the same, which improves the structure of a metal pad. On the one hand, the contact area between the metal pad and the interlayer dielectric layer is increased, and on the other hand, the weight of the metal pad is reduced, which can reduce the stress of the metal pad on the interlayer dielectric layer, thereby improving device reliability and device performance. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] The following figures describe in detail the exemplary embodiments disclosed in this application. The same reference numerals represent similar structures in several views of the drawings. Those skilled in the art will understand that these embodiments are non-limiting, exemplary embodiments, and the drawings are only for the purpose of illustration and description, and are not intended to limit the scope of this application. Other embodiments may also accomplish the inventive intent in this application. It should be understood that the drawings are not drawn to scale.
[0025] in:
[0026] Figures 1 to 16 It is a structural schematic diagram of each step in the method for forming a semiconductor structure described in an embodiment of the present application. DETAILED DESCRIPTION
[0027] The following description provides specific application scenarios and requirements of the present application, with the purpose of enabling those skilled in the art to make and use the content in the present application. It will be apparent to those skilled in the art that various local modifications to the disclosed embodiments are apparent, and the general principles defined herein may be applied to other embodiments and applications without departing from the spirit and scope of the present application. Therefore, the present application is not limited to the embodiments shown, but to the widest scope consistent with the claims.
[0028] The technical solution of the present invention is described in detail below in conjunction with the embodiments and drawings.
[0029] The stress at the edge corner of the metal pad is directly related to the pressure. The greater the pressure, the greater the stress. According to the pressure formula P = F / S, when the force (F) is large and the area (S) is small, the pressure (P) is large. The edge corner of the metal pad happens to be where the pressure is highest. Therefore, the stress at the corner is also the highest, which may cause reliability problems.
[0030] In response to the above problems, the present application provides a semiconductor structure and a method for forming the same based on the principle of the pressure formula, improves the structure of the metal pad, increases the contact area between the metal pad and the interlayer dielectric layer (that is, increases S), and reduces the weight of the metal pad (that is, reduces F) on the other hand, which can reduce the stress of the metal pad on the interlayer dielectric layer, thereby improving device reliability and device performance.
[0031] Figures 1 to 16 The following is a schematic diagram of the structure of each step in the method for forming a semiconductor structure according to an embodiment of the present application. The method for forming a semiconductor structure according to an embodiment of the present application is described in detail in conjunction with the accompanying drawings.
[0032] refer to Figure 1 As shown, a substrate 100 is provided, and an interlayer dielectric layer 110 is formed on the surface of the substrate 100 .
[0033] In some embodiments of the present application, the base 100 may be a semiconductor substrate. The material of the semiconductor substrate includes (i) elemental semiconductors, such as silicon or germanium, etc.; (ii) compound semiconductors, such as silicon carbide, gallium arsenide, gallium phosphide or indium phosphide, etc.; (iii) alloy semiconductors, such as silicon germanium carbide, silicon germanium, gallium arsenide phosphide or indium gallium phosphide, etc.; or (iv) a combination of the above.
[0034] In some embodiments of the present application, the base 100 may also include a semiconductor substrate and a dielectric layer located on the surface of the semiconductor substrate.
[0035] In some embodiments of the present application, the base 100 may further include a semiconductor substrate, a dielectric layer located on a surface of the semiconductor substrate, and an etch stop layer located on a surface of the dielectric layer.
[0036] In some embodiments of the present application, a top metal layer 101 is further formed in the dielectric layer in the base 100. The top metal layer 101 is used to electrically connect active devices in the semiconductor substrate. The material of the top metal layer 101 is, for example, copper or aluminum.
[0037] In some embodiments of the present application, the material of the interlayer dielectric layer 110 includes silicon oxide or silicon oxynitride, etc. The method of forming the interlayer dielectric layer 110 includes a chemical vapor deposition process or a physical vapor deposition process, etc.
[0038] refer to Figures 2 to 7 As shown, the interlayer dielectric layer 110 is etched to form a first opening 121 that does not penetrate the interlayer dielectric layer 110 .
[0039] In some embodiments of the present application, the depth of the first opening 121 is 20% to 40% of the thickness of the interlayer dielectric layer. The depth of the first opening 121 is, for example, 1 micron to 2 microns, such as 1.2 microns, 1.5 microns or 1.8 microns.
[0040] In some embodiments of the present application, a method for etching the interlayer dielectric layer 110 to form a first opening 121 that does not penetrate the interlayer dielectric layer 110 includes: Figure 2 As shown, a hard mask layer 111 is formed on the surface of the interlayer dielectric layer 110. The material of the hard mask layer is, for example, silicon nitride. The method of forming the hard mask layer 111 includes a chemical vapor deposition process or a physical vapor deposition process.
[0041] In some embodiments of the present application, the method of etching the interlayer dielectric layer 110 to form the first opening 121 that does not penetrate the interlayer dielectric layer 110 further includes: Figure 3 and Figure 4 As shown, a patterned first photoresist layer (not shown in the figure) is formed on the surface of the hard mask layer 111, and the patterned first photoresist layer defines the position of the first opening 121; the hard mask layer 111 and the interlayer dielectric layer 110 are etched using the patterned first photoresist layer as a mask to form the first opening 121; and the patterned first photoresist layer is removed. Figure 4 yes Figure 3 A top view of Figure 3 is along Figure 4 The longitudinal section is made by the dotted line XX in FIG.
[0042] It should be noted that due to Figure 4 yes Figure 3 , so in Figure 4 The position of the first opening 121 should expose the interlayer dielectric layer 110. However, in order to clearly show the shape of the first opening 121, Figure 4 The exposed interlayer dielectric layer 110 is not shown in the figure, but the first opening 121 is shown. Since the first opening 121 exposes the interlayer dielectric layer 110, that is, the first opening 121 has the same shape as the exposed interlayer dielectric layer 110, such treatment does not affect the understanding of the technical solution by those skilled in the art. The subsequent figures also use the same treatment method to show the second opening and the third opening, which will not be repeated.
[0043] In some embodiments of the present application, the cross-sectional graph of the first opening 121 is a graph in which the ratio of the square of the perimeter to the area is greater than 16. When the depth of the first opening 121 remains unchanged, the area of the cross-sectional graph of the first opening 121 can represent the volume of the first opening 121, and further represent the weight of the metal pad filled in the first opening 121. When the weight of the metal pad remains unchanged, that is, when the area of the cross-sectional graph of the first opening 121 remains unchanged, increasing the perimeter of the cross-sectional graph of the first opening 121 can increase the side area of the first opening 121, that is, increasing the contact area between the metal pad filled in the first opening 121 and the interlayer dielectric layer (that is, increasing S when F remains unchanged). Therefore, setting a high perimeter-to-area ratio can effectively reduce the stress of the metal pad on the interlayer dielectric layer.
[0044] In some embodiments of the present application, the length (lateral dimension in the figure) of the first opening 121 is 30 micrometers to 80 micrometers, and the width (vertical dimension in the figure) of the first opening 121 is 30 micrometers to 80 micrometers.
[0045] In some embodiments of the present application, the cross-sectional shape of the first opening 121 includes a round corner rectangular shape (refer to Figure 4 As shown), bowl corner rectangular (ref. Figure 5 As shown), slope corner rectangular (reference Figure 6 as shown) or an obtuse angle corner rectangular (refer to Figure 7As shown). These figures have a larger perimeter-to-area ratio than conventional right-angled rectangles, which can reduce stress. Of course, it should be understood that here are just a few regular and easy-to-design figures for demonstration, which is not a limitation of the present application. In practical applications, the cross-sectional figure of the first opening 121 can be any other shape that meets the requirements.
[0046] refer to Figures 8 to 12 As shown, the interlayer dielectric layer 110 at the bottom of the first opening 121 is etched to form a second opening 122 that does not penetrate the interlayer dielectric layer 110, and the interlayer dielectric layer 110 located at the bottom of the first opening 121 and outside the second opening 122 includes a first portion 131 located at the bottom center of the first opening 121 and a second portion 132 surrounding the first portion 131.
[0047] In some embodiments of the present application, the depth of the second opening 122 is 40% to 60% of the thickness of the interlayer dielectric layer 110. The depth of the second opening 122 may be the same as the depth of the first opening 121. The depth of the second opening 122 is, for example, 1 micron to 2 microns, such as 1.2 microns, 1.5 microns or 1.8 microns. The width of the portion of the second opening 122 located at the edge of the first opening 121 is 5 microns to 10 microns, such as 6 microns, 7.5 microns or 8 microns.
[0048] In some embodiments of the present application, the method for forming the second opening 122 includes: referring to Figure 8 and Fig. 9 As shown, a first sacrificial layer (not shown in the figure) is formed in the first opening 121 and on the surface of the hard mask layer 111; a patterned second photoresist layer (not shown in the figure) is formed on the surface of the first sacrificial layer, and the patterned second photoresist layer defines the position of the second opening 122; the first sacrificial layer and the interlayer dielectric layer 110 are etched using the patterned second photoresist layer as a mask to form the second opening 122; and the patterned second photoresist layer and the first sacrificial layer are removed. Fig. 9 yes Figure 8 A top view of Figure 8 is along Fig. 9 The longitudinal section is made by the dotted line XX in FIG.
[0049] refer to Fig. 9 As shown, in some embodiments of the present application, a partial contour of the cross-sectional figure of the second opening 122 (that is, a partial contour located at the edge of the first opening 121 ) is the same as the contour of the cross-sectional figure of the first opening 121 .
[0050] Continue to refer Fig. 9As shown, the first part 131 is located at the center of the first opening 121. The first part 131 is used to etch to form a third opening, and then fill the metal material to form a through-hole structure. The shape of the first part 131 is, for example, a square. The shape of the first part 131 is the same as the shape of the through-hole structure in the conventional structure. In the technical solution of the present application, the through-hole structure is kept unchanged while the metal pad structure is improved to ensure that the new metal pad structure can support bonding and welding. The second part 132 fully surrounds or semi-surrounds the first part 131, and the second part 132 is not subsequently etched, so the interlayer dielectric layer 110 of the second part 132 is retained and will not be filled with metal. Therefore, the existence of the second part 132 further increases the contact area between the interlayer dielectric layer 110 and the metal pad on the one hand, and reduces the volume of the metal pad on the other hand, which can further reduce the stress of the metal pad on the interlayer dielectric layer 110.
[0051] In some embodiments of the present application, the second portion 132 includes a rectangular groove (see Fig. 9 As shown), circular groove (refer to Fig.10 As shown), polygonal groove (reference Fig.11 As shown), discontinuous ring (randon groove) (reference Fig.12 shown).
[0052] refer to Fig. 9 As shown, when the shape of the second portion 132 is a rectangular ring, the second opening 122 is only located at the edge of the first opening 121. Figures 10 to 12 As shown, when the shape of the second portion 132 is a circular ring, a polygonal ring, or a discontinuous ring, the second opening 122 includes the portion located at the edge of the first opening 121 and all positions other than the first portion 131 and the second portion 132. In other words, the second opening 122 has no fixed shape, and the position of the second opening 122 is all the positions remaining after removing the shapes of the first portion 131 and the second portion 132 from the shape of the first opening 121.
[0053] refer to Fig.13 and Fig.14 As shown, the interlayer dielectric layer 110 located in the first portion 131 is etched to form a third opening 123 exposing the substrate 100. Fig.14 yes Fig.13 A top view of Fig.13 is along Fig.14 The longitudinal section is made by the dotted line XX in FIG.
[0054] In some embodiments of the present application, the method for forming the third opening 123 includes: forming a second sacrificial layer (not shown in the figure) in the first opening 121 and the second opening 122 and on the surface of the hard mask layer 111; forming a patterned third photoresist layer (not shown in the figure) on the surface of the second sacrificial layer, and the patterned third photoresist layer defines the position of the third opening 123; etching the second sacrificial layer and the interlayer dielectric layer 110 using the patterned third photoresist layer as a mask to form the third opening 123; and removing the patterned third photoresist layer and the second sacrificial layer.
[0055] In some embodiments of the present application, the third opening 123 further exposes the top metal layer 101 in the substrate 100 .
[0056] refer to Fig.15 and Fig.16 As shown, a metal material layer is filled in the first opening 121, the second opening 122, and the third opening 123, the metal material layer in the first opening 121 and the second opening 122 constitutes a metal pad 140, and the metal material layer in the third opening 123 constitutes a through-hole structure 150. Fig.16 yes Fig.15 A top view of Fig.15 is along Fig.16 The longitudinal section is made by the dotted line XX in FIG.
[0057] In some embodiments of the present application, the method for forming the metal pad 140 and the through-hole structure 150 includes: forming a metal material layer in the first opening 121, the second opening 122 and the third opening 123 and on the surface of the hard mask layer 111; removing the metal material layer and the hard mask layer above the upper surface of the interlayer dielectric layer 110, the metal material layer in the first opening 121 and the second opening 122 constitutes the metal pad 140, and the metal material layer in the third opening 123 constitutes the through-hole structure 150.
[0058] refer to Fig.16 As shown, due to Fig.16 yes Fig.15 The top view can only show the interlayer dielectric layer 110 and the metal pad 140 on the uppermost surface. However, in order to clearly show the structure and relationship between the metal pad 140 and the through hole structure 150, the position of the through hole structure 150 and the position of the third part 132 are indicated by a dotted frame.
[0059] In the technical solution of this application, on the one hand, reference is made to Fig.15As shown, due to the presence of the interlayer dielectric layer 110 of the third part 132, compared with the conventional structure (in the conventional structure, the third part 132 is also a metal pad), the contact area between the metal pad 140 and the interlayer dielectric layer 110 is increased and the weight of the metal pad 140 is reduced, which can greatly reduce the stress of the metal pad 140 on the interlayer dielectric layer 110; on the other hand, referring to Fig.16 As shown, the contour of the metal pad 140 is improved from a conventional rectangle to a rounded rectangle (or other shapes with a larger perimeter-to-area ratio), which further increases the contact area between the metal pad 140 and the interlayer dielectric layer 110, and can also reduce the stress of the metal pad 140 on the interlayer dielectric layer 110, thereby improving the reliability and performance of the semiconductor device.
[0060] The present application provides a method for forming a semiconductor structure, which improves the structure of a metal pad. On the one hand, the contact area between the metal pad and the interlayer dielectric layer is increased, and on the other hand, the weight of the metal pad is reduced, which can reduce the stress of the metal pad on the interlayer dielectric layer, thereby improving device reliability and device performance.
[0061] The embodiment of the present application also provides a semiconductor structure, referring to Fig.15 and Fig.16 As shown, it includes: a substrate 100, an interlayer dielectric layer 110 is formed on the surface of the substrate 100, a first opening 121 that does not penetrate the interlayer dielectric layer 110 is formed in the interlayer dielectric layer 110, a second opening 122 that does not penetrate the interlayer dielectric layer 110 is formed in the interlayer dielectric layer 110 at the bottom of the first opening 121, the interlayer dielectric layer 110 located at the bottom of the first opening 121 and outside the second opening 122 includes a first part 131 located at the bottom center of the first opening 121 and a second part 132 surrounding the first part 131, the interlayer dielectric layer 100 of the first part 131 is etched to form a third opening 123 exposing the substrate 100; a metal pad 140, located in the first opening 121 and the second opening 122; a through-hole structure 150, located in the third opening 123.
[0062] In some embodiments of the present application, the base 100 may be a semiconductor substrate. The material of the semiconductor substrate includes (i) elemental semiconductors, such as silicon or germanium, etc.; (ii) compound semiconductors, such as silicon carbide, gallium arsenide, gallium phosphide or indium phosphide, etc.; (iii) alloy semiconductors, such as silicon germanium carbide, silicon germanium, gallium arsenide phosphide or indium gallium phosphide, etc.; or (iv) a combination of the above.
[0063] In some embodiments of the present application, the base 100 may also include a semiconductor substrate and a dielectric layer located on the surface of the semiconductor substrate.
[0064] In some embodiments of the present application, the base 100 may further include a semiconductor substrate, a dielectric layer located on a surface of the semiconductor substrate, and an etch stop layer located on a surface of the dielectric layer.
[0065] In some embodiments of the present application, a top metal layer 101 is further formed in the dielectric layer in the base 100. The top metal layer 101 is used to electrically connect active devices in the semiconductor substrate. The material of the top metal layer 101 is, for example, copper or aluminum.
[0066] In some embodiments of the present application, the material of the interlayer dielectric layer 110 includes silicon oxide or silicon oxynitride.
[0067] refer to Figure 3 As shown, a first opening 121 is formed in the interlayer dielectric layer 110 and does not penetrate the interlayer dielectric layer 110 .
[0068] In some embodiments of the present application, the depth of the first opening 121 is 20% to 40% of the thickness of the interlayer dielectric layer. The depth of the first opening 121 is, for example, 1 micron to 2 microns, such as 1.2 microns, 1.5 microns or 1.8 microns.
[0069] In some embodiments of the present application, the cross-sectional graph of the first opening 121 is a graph in which the ratio of the square of the perimeter to the area is greater than 16. When the depth of the first opening 121 remains unchanged, the area of the cross-sectional graph of the first opening 121 can represent the volume of the first opening 121, and further represent the weight of the metal pad filled in the first opening 121. When the weight of the metal pad remains unchanged, that is, when the area of the cross-sectional graph of the first opening 121 remains unchanged, increasing the perimeter of the cross-sectional graph of the first opening 121 can increase the side area of the first opening 121, that is, increasing the contact area between the metal pad filled in the first opening 121 and the interlayer dielectric layer (that is, increasing S when F remains unchanged). Therefore, setting a high perimeter-to-area ratio can effectively reduce the stress of the metal pad on the interlayer dielectric layer.
[0070] In some embodiments of the present application, the length (lateral dimension in the figure) of the first opening 121 is 30 micrometers to 80 micrometers, and the width (vertical dimension in the figure) of the first opening 121 is 30 micrometers to 80 micrometers.
[0071] In some embodiments of the present application, the cross-sectional shape of the first opening 121 includes a round corner rectangular shape (refer to Figure 4 As shown), bowl corner rectangular (ref. Figure 5As shown), slope corner rectangular (reference Figure 6 as shown) or an obtuse angle corner rectangular (refer to Figure 7 As shown). These figures have a larger perimeter-to-area ratio than conventional right-angled rectangles, which can reduce stress. Of course, it should be understood that here are just a few regular and easy-to-design figures for demonstration, which is not a limitation of the present application. In practical applications, the cross-sectional figure of the first opening 121 can be any other shape that meets the requirements.
[0072] refer to Figure 8 As shown, a second opening 122 that does not penetrate the interlayer dielectric layer 110 is formed in the interlayer dielectric layer 110 at the bottom of the first opening 121, and the interlayer dielectric layer 110 located at the bottom of the first opening 121 and outside the second opening 122 includes a first portion 131 located at the bottom center of the first opening 121 and a second portion 132 surrounding the first portion 131.
[0073] In some embodiments of the present application, the depth of the second opening 122 is 40% to 60% of the thickness of the interlayer dielectric layer 110. The depth of the second opening 122 is the same as the depth of the first opening 121. The depth of the second opening 122 is, for example, 1 micron to 2 microns, such as 1.2 microns, 1.5 microns or 1.8 microns. The width of the portion of the second opening 122 located at the edge of the first opening 121 is 5 microns to 10 microns, such as 6 microns, 7.5 microns or 8 microns.
[0074] refer to Fig. 9 As shown, in some embodiments of the present application, a partial contour of the cross-sectional figure of the second opening 122 (that is, a partial contour located at the edge of the first opening 121 ) is the same as the contour of the cross-sectional figure of the first opening 121 .
[0075] Continue to refer Fig. 9As shown, the first part 131 is located at the center of the first opening 121. The first part 131 is used to etch to form a third opening, and then fill the metal material to form a through-hole structure. The shape of the first part 131 is, for example, a square. The shape of the first part 131 is the same as the shape of the through-hole structure in the conventional structure. In the technical solution of the present application, the through-hole structure is kept unchanged while the metal pad structure is improved to ensure that the new metal pad structure can support bonding and welding. The second part 132 fully surrounds or semi-surrounds the first part 131, and the second part 132 is not subsequently etched, so the interlayer dielectric layer 110 of the second part 132 is retained and will not be filled with metal. Therefore, the existence of the second part 132 further increases the contact area between the interlayer dielectric layer 110 and the metal pad on the one hand, and reduces the volume of the metal pad on the other hand, which can further reduce the stress of the metal pad on the interlayer dielectric layer 110.
[0076] In some embodiments of the present application, the second portion 132 includes a rectangular groove (see Fig. 9 As shown), circular groove (refer to Fig.10 As shown), polygonal groove (reference Fig.11 As shown), discontinuous ring (randon groove) (reference Fig.12 shown).
[0077] refer to Fig. 9 As shown, when the shape of the second portion 132 is a rectangular ring, the second opening 122 is only located at the edge of the first opening 121. Figures 10 to 12 As shown, when the shape of the second portion 132 is a circular ring, a polygonal ring, or a discontinuous ring, the second opening 122 includes the portion located at the edge of the first opening 121 and all positions other than the first portion 131 and the second portion 132. In other words, the second opening 122 has no fixed shape, and the position of the second opening 122 is all the positions remaining after removing the shapes of the first portion 131 and the second portion 132 from the shape of the first opening 121.
[0078] refer to Fig.13 As shown, the interlayer dielectric layer 100 of the first portion 131 is etched to form a third opening 123 exposing the substrate 100 .
[0079] In some embodiments of the present application, the third opening 123 further exposes the top metal layer 101 in the substrate 100 .
[0080] refer to Fig.15 and Fig.16 As shown, metal pads 140 are formed in the first opening 121 and the second opening 122 , and a through-hole structure 150 is formed in the third opening 123 .
[0081] In the technical solution of this application, on the one hand, reference is made to Fig.15 As shown, due to the presence of the interlayer dielectric layer 110 of the third part 132, compared with the conventional structure (in the conventional structure, the third part 132 is also a metal pad), the contact area between the metal pad 140 and the interlayer dielectric layer 110 is increased and the weight of the metal pad 140 is reduced, which can greatly reduce the stress of the metal pad 140 on the interlayer dielectric layer 110; on the other hand, referring to Fig.16 As shown, the contour of the metal pad 140 is improved from a conventional rectangle to a rounded rectangle (or other shapes with a larger perimeter-to-area ratio), which further increases the contact area between the metal pad 140 and the interlayer dielectric layer 110, and can also reduce the stress of the metal pad 140 on the interlayer dielectric layer 110, thereby improving the reliability and performance of the semiconductor device.
[0082] The present application provides a semiconductor structure and a method for forming the same, which improves the structure of a metal pad. On the one hand, the contact area between the metal pad and the interlayer dielectric layer is increased, and on the other hand, the weight of the metal pad is reduced, which can reduce the stress of the metal pad on the interlayer dielectric layer, thereby improving device reliability and device performance.
[0083] In summary, after reading the contents of this application, those skilled in the art will appreciate that the aforementioned application contents may be presented only in an exemplary manner and may not be restrictive. Although not explicitly stated herein, those skilled in the art will appreciate that this application is intended to encompass various reasonable changes, improvements and modifications to the embodiments. These changes, improvements and modifications are within the spirit and scope of the exemplary embodiments of this application.
[0084] It should be understood that the term "and / or" used in this embodiment includes any or all combinations of one or more of the associated listed items. It should be understood that when an element is referred to as being "connected" or "coupled" to another element, it can be directly connected or coupled to another element, or there can also be intermediate elements.
[0085] Similarly, it should be understood that when an element such as a layer, region, or substrate is referred to as being "on" another element, it can be directly on the other element or there can be intervening elements. In contrast, the term "directly" means that there are no intervening elements. It should also be understood that the terms "comprising," "containing," "including," or "comprising," when used in this application document, indicate the presence of the recited features, wholes, steps, operations, elements, and / or components, but do not exclude the presence or addition of one or more other features, wholes, steps, operations, elements, components, and / or groups thereof.
[0086] It should also be understood that although the terms first, second, third, etc. can be used to describe various elements, these elements should not be limited by these terms. These terms are only used to distinguish one element from another element. Therefore, without departing from the teachings of the present application, the first element in some embodiments can be referred to as the second element in other embodiments. The same reference numerals or the same reference signs represent the same elements throughout the specification.
[0087] In addition, the present specification describes exemplary embodiments by reference to idealized exemplary cross-sectional views and / or plan views and / or stereograms. Therefore, differences from the illustrated shapes due to, for example, manufacturing techniques and / or tolerances are foreseeable. Therefore, the exemplary embodiments should not be interpreted as being limited to the shapes of the regions shown herein, but should include deviations in shapes caused by, for example, manufacturing. For example, an etched region shown as a rectangle will typically have circular or curved features. Therefore, the region shown in the figure is schematic in nature, and its shape is not intended to illustrate the actual shape of the region of the device nor to limit the scope of the exemplary embodiments.
Claims
1. A method for forming a semiconductor structure, characterized in that: include: Providing a substrate, wherein an interlayer dielectric layer is formed on the surface of the substrate; Etching the interlayer dielectric layer to form a first opening that does not penetrate the interlayer dielectric layer; The interlayer dielectric layer at the bottom of the first opening is etched to form a second opening that does not penetrate the interlayer dielectric layer, and the interlayer dielectric layer located at the bottom of the first opening and outside the second opening includes a first portion located at the center of the bottom of the first opening and a second portion surrounding the first portion; Etching the interlayer dielectric layer located in the first portion to form a third opening exposing the substrate; A metal material layer is filled in the first opening, the second opening and the third opening. The metal material layers in the first opening and the second opening constitute a metal pad, and the metal material layer in the third opening constitutes a through-hole structure.
2. The method for forming a semiconductor structure according to claim 1, wherein: The method of forming the first opening includes: forming a hard mask layer on the surface of the interlayer dielectric layer; forming a patterned first photoresist layer on the surface of the hard mask layer, wherein the patterned first photoresist layer defines a position of the first opening; Using the patterned first photoresist layer as a mask, etching the hard mask layer and the interlayer dielectric layer to form the first opening; The patterned first photoresist layer is removed.
3. The method for forming a semiconductor structure according to claim 2, wherein: The method of forming the second opening includes: forming a first sacrificial layer in the first opening and on the surface of the hard mask layer; forming a patterned second photoresist layer on the surface of the first sacrificial layer, wherein the patterned second photoresist layer defines the position of the second opening; Using the patterned second photoresist layer as a mask, etching the first sacrificial layer and the interlayer dielectric layer to form the second opening; The patterned second photoresist layer and the first sacrificial layer are removed.
4. The method for forming a semiconductor structure according to claim 3, wherein: The method of forming the third opening includes: forming a second sacrificial layer in the first opening and the second opening and on the surface of the hard mask layer; forming a patterned third photoresist layer on the surface of the second sacrificial layer, wherein the patterned third photoresist layer defines the position of the third opening; Using the patterned third photoresist layer as a mask, etching the second sacrificial layer and the interlayer dielectric layer to form the third opening; The patterned third photoresist layer and the second sacrificial layer are removed.
5. The method for forming a semiconductor structure according to claim 4, wherein: The method of forming the metal pad and through-hole structure includes: forming a metal material layer in the first opening, the second opening, the third opening and on the surface of the hard mask layer; The metal material layer and the hard mask layer above the upper surface of the interlayer dielectric layer are removed, the metal material layer in the first opening and the second opening constitutes a metal pad, and the metal material layer in the third opening constitutes a through-hole structure.
6. The method for forming a semiconductor structure according to claim 1, wherein: The cross-sectional shape of the first opening is a shape in which the ratio of the square of the perimeter to the area is greater than 16.
7. The method for forming a semiconductor structure according to claim 6, wherein: The cross-sectional shape of the first opening includes a rounded rectangle, a bowl-angle rectangle, an oblique-angle rectangle or an obtuse-angle rectangle.
8. The method for forming a semiconductor structure according to claim 1, wherein: A partial profile of the cross-sectional shape of the second opening is the same as a profile of the cross-sectional shape of the first opening.
9. The method for forming a semiconductor structure according to claim 1, wherein: The shape of the second part includes a circular ring, a polygonal ring, and a discontinuous ring.
10. The method for forming a semiconductor structure according to claim 1, wherein: The depth of the first opening is 20% to 40% of the thickness of the interlayer dielectric layer.
11. The method for forming a semiconductor structure according to claim 1, wherein: The depth of the second opening is 40% to 60% of the thickness of the interlayer dielectric layer.
12. A semiconductor structure, characterized in that: include: A substrate, wherein an interlayer dielectric layer is formed on a surface of the substrate, a first opening that does not penetrate the interlayer dielectric layer is formed in the interlayer dielectric layer, a second opening that does not penetrate the interlayer dielectric layer is formed in the interlayer dielectric layer at the bottom of the first opening, the interlayer dielectric layer located at the bottom of the first opening and outside the second opening comprises a first portion located at the center of the bottom of the first opening and a second portion surrounding the first portion, and the interlayer dielectric layer at the first portion is etched to form a third opening exposing the substrate; A metal pad is located in the first opening and the second opening; The through hole structure is located in the third opening.
13. The semiconductor structure according to claim 12, wherein: The cross-sectional shape of the first opening is a shape in which the ratio of the square of the perimeter to the area is greater than 16.
14. The semiconductor structure according to claim 13, wherein: The cross-sectional shape of the first opening includes a rounded rectangle, a bowl-angle rectangle, an oblique-angle rectangle or an obtuse-angle rectangle.
15. The semiconductor structure according to claim 12, wherein: A partial profile of the cross-sectional shape of the second opening is the same as a profile of the cross-sectional shape of the first opening.
16. The semiconductor structure according to claim 12, characterized in that: The shape of the second part includes a circular ring, a polygonal ring, and a discontinuous ring.
17. The semiconductor structure according to claim 12, characterized in that: The depth of the first opening is 20% to 40% of the thickness of the interlayer dielectric layer.
18. The semiconductor structure according to claim 12, characterized in that: The depth of the second opening is 40% to 60% of the thickness of the interlayer dielectric layer.