Formation method of semiconductor structure
By preforming the protective layer in the semiconductor structure, the impact of the oxidation process of logic computing devices on flash memory devices is solved, erasing efficiency and performance stability are improved, and a process process with lower cost and shorter production time is achieved.
Patent Information
- Application Number
- CN202310602219.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-25
- Publication Date
- 2024-11-26
AI Technical Summary
In the prior art, the oxidation process of logic computing devices will lead to structural defects in flash memory devices, affecting erasing efficiency and reducing performance.
During the formation of the semiconductor structure, a protective layer is formed on the surface of the floating gate side wall in advance, and a silicon nitride protective layer is formed through an ion implantation process to protect the floating gate side wall and protrusions, reducing the impact of the oxidation process on the morphology of the floating gate. , and a gate oxide layer is formed in the logic region.
提高了存储器的擦除效率稳定性,防止浮栅凸出部的转角圆化,增强了器件性能,且采用离子注入方法降低了成本和制成时间。
Smart Images

Figure CN119031712A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a method for forming a semiconductor structure. Background Art
[0002] Embedded flash memory (flash) is a non-volatile memory widely used in the automotive, consumer and other fields. With the rapid increase in market demand for new energy vehicles in recent years, the demand for chip storage and processing performance and cost has also increased rapidly. At the same time, the demand for high-voltage devices has also increased. Therefore, various microcontroller and flash memory integration design solutions have emerged. Various research institutions focus on the layout and development of flash memory and BCD (Bipolar, CMOS, DMOS) process compatible process platforms, integrating memory, power devices and logic operation devices on the same wafer.
[0003] In the prior art, in order to maintain the reliability of the performance of the logic operation device, it is usually chosen to first form the device structure of the flash memory area, and then carry out the process preparation of the logic operation device. In the process of forming the logic operation device, due to the existence of a long oxidation process, the structure of the flash memory device is inevitably affected, so that it introduces structural defects due to excessive oxidation, resulting in the erasure efficiency of the flash memory being affected and the device performance being reduced. Summary of the invention
[0004] The technical problem solved by the present invention is to provide a method for forming a semiconductor structure, which reduces the influence of the oxidation process of the logic operation device on the flash memory device, reduces structural defects, and improves the performance stability of the flash memory device.
[0005] In order to solve the above technical problems, the technical solution of the present invention provides a method for forming a semiconductor structure, comprising: providing a substrate, the substrate comprising a storage area and a logic area; forming discrete and paired storage gate structures in the storage area, a first opening being provided between the paired storage gate structures, each storage gate structure comprising a floating gate located on the substrate, a control gate dielectric layer located on the floating gate, and a control gate located on the control gate dielectric layer, the first opening exposing at least a portion of the sidewall surface of the floating gate; forming a tunneling dielectric layer on the floating gate surface and the control gate surface exposed by the first opening; forming a protective layer on the surface of the tunneling dielectric layer; after forming the protective layer, forming a gate oxide layer on the surface of the logic area using an oxidation process.
[0006] Optionally, the control gate includes a first sidewall and a second sidewall opposite to each other, the first sidewall faces the first opening, and the floating gate includes a floating gate protrusion protruding relative to the first sidewall.
[0007] Optionally, a sidewall surface of the floating gate protrusion is perpendicular to the substrate surface; and a top surface of the floating gate protrusion is parallel to the substrate surface.
[0008] Optionally, the material of the protective layer includes silicon nitride.
[0009] Optionally, the thickness of the protective layer ranges from 0 to 100 angstroms.
[0010] Optionally, the method for forming the protective layer includes a chemical vapor deposition process.
[0011] Optionally, the thickness of the tunnel dielectric layer is in the range of 80 angstroms to 130 angstroms.
[0012] Optionally, the method for forming the protective layer includes an ion implantation process.
[0013] Optionally, the parameters of the ion implantation process include: an ion implantation energy of 0 to 30 keV; an ion implantation dose of 1E12 ions / cm 2 ~1E16 ions / cm 2 .
[0014] Optionally, the thickness of the tunnel dielectric layer ranges from 100 angstroms to 150 angstroms.
[0015] Optionally, the method for forming the gate oxide layer includes: one of a thermal oxidation process and a diffusion process or a combination of the two.
[0016] Optionally, after forming the gate oxide layer, the method further includes: removing the protective layer on the storage area.
[0017] Optionally, after removing the protective layer, the method further includes: forming an erase gate in the first opening.
[0018] Optionally, the method further includes: forming a gate on the gate oxide layer.
[0019] Optionally, there is a floating gate dielectric layer between the floating gate and the substrate; the control gate sidewall, the control gate dielectric layer sidewall and a portion of the floating gate sidewall surface also have a sidewall structure, and the sidewall structure is formed before the tunneling oxide layer.
[0020] Optionally, the sidewall structure includes a first sidewall and a second sidewall, the first sidewall is located on the control gate sidewall and the control gate dielectric layer sidewall surface exposed by the first opening, the second sidewall is located on the sidewall surface on the other side of the control gate and the control gate dielectric layer, and the thickness of the first sidewall is greater than the thickness of the second sidewall.
[0021] Optionally, the method for forming the storage gate structure includes: forming a floating gate dielectric layer on the substrate; forming a floating gate material layer on the floating gate dielectric layer; forming two separate control gate dielectric layers and a control gate located on the surface of the control gate dielectric layer on the floating gate material layer, wherein a first opening is provided between adjacent control gates, and the first opening exposes the control gate sidewalls, the control gate dielectric layer sidewalls and the floating gate material layer surface; forming a sidewall structure on the control gate sidewalls and the control gate dielectric layer sidewall surfaces; using the sidewall structure as a mask, etching the floating gate material layer until the surface of the floating gate dielectric layer is exposed, thereby forming a floating gate, wherein the floating gate has a floating gate protrusion protruding toward the first opening.
[0022] Optionally, the method for forming the control gate dielectric layer and the control gate includes: forming a control gate dielectric material layer and a control gate material layer on the floating gate material layer; forming a mask layer on the control gate material layer, the mask layer exposing a portion of the surface of the control gate material layer on the storage area; using the mask layer as a mask, etching the control gate material layer and the control gate dielectric material layer until the surface of the floating gate material layer is exposed to form a control gate and a control gate dielectric layer.
[0023] Optionally, after etching the control gate material layer and the control gate dielectric material layer, the method further includes: etching a portion of the floating gate material layer; and forming the sidewall structure on the control gate sidewall, the control gate dielectric layer sidewall and a portion of the floating gate material layer sidewall surface.
[0024] Compared with the prior art, the technical solution of the embodiment of the present invention has the following beneficial effects:
[0025] In the method for forming a semiconductor structure provided by the technical solution of the present invention, before forming a gate oxide layer in the logic area, a protective layer is pre-formed on the surface of the floating gate side wall. Therefore, in the subsequent process of forming a gate oxide layer in the logic area, the protective layer can protect the floating gate side wall exposed by the first opening, reducing the influence of the oxidation process on the floating gate morphology, thereby improving the stability of the memory erase efficiency.
[0026] Furthermore, since the floating gate has a floating gate protrusion protruding toward the first opening, and the side wall surface of the floating gate protrusion is perpendicular to the substrate surface, and the top surface of the floating gate protrusion is parallel to the substrate surface, in the subsequent process of forming a gate oxide layer in the logic area, the protective layer can protect the floating gate sidewalls, top and corners of the floating gate protrusion exposed by the first opening, prevent the corners of the floating gate protrusion from being rounded, reduce the influence of the oxidation process on the floating gate morphology, and thereby improve the stability of the memory erase efficiency.
[0027] Furthermore, the method for forming the protective layer includes an ion implantation process. When the protective layer is formed by ion implantation, the thickness and density of the formed protective layer can be adjusted by adjusting the concentration, energy and other parameters of the ion implantation, so that the protective strength of the protective layer can be designed according to the requirements, thereby increasing the adjustability of the protective layer. In addition, the protective layer formed by the ion implantation method has lower cost and shorter production time. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] Figure 1 and Figure 2 is a cross-sectional schematic diagram of a method for forming a semiconductor structure;
[0029] Figures 3 to 11 It is a schematic cross-sectional structural diagram of a formation process of a semiconductor structure according to an embodiment of the present invention. DETAILED DESCRIPTION
[0030] As described in the background technology, in order to integrate memory, power devices and logic operation devices on the same wafer, it is necessary to use a process platform that is compatible with the memory process and the BCD process. In the prior art, in order to maintain the reliability of the performance of the logic operation device, it is usually chosen to first form the device structure of the storage area, and then perform the process preparation of the logic operation device. In the process of forming the logic operation device, due to the long oxidation process, the structure of the memory device is inevitably affected, so that it introduces structural defects due to excessive oxidation, resulting in the erasure efficiency of the memory being affected, and the device performance is reduced.
[0031] Figure 1 and Figure 2 The invention is a cross-sectional schematic diagram of a method for forming a semiconductor structure.
[0032] Please refer to Figure 1 , providing a substrate 100, the substrate 100 comprising a storage area I and a logic area II; forming two separate storage gate structures (not shown) in the storage area II, with a first opening (not shown) between the two storage gate structures, each storage gate structure comprising a floating gate dielectric layer 101 located on the substrate, a floating gate 103, a control gate dielectric layer 113 and a control gate 120 located on the control gate dielectric layer 113, the control gate 120 comprising a first sidewall and a second sidewall opposite to each other, the first sidewall facing the first opening, the floating gate 103 having a floating gate protrusion protruding relative to the first sidewall (such as Figure 1 A tunnel dielectric layer 126 is deposited on the surface of the floating gate 103 and the first sidewall surface exposed by the first opening.
[0033] In this embodiment, a mask structure 125 is further formed on the surface of the control gate 120, and the mask structure 125 is used to etch and form the control gate 120 and the control gate dielectric layer 113. Specifically, the control gate dielectric layer 113 includes a first silicon oxide layer 110, a silicon nitride layer 111 located on the first silicon oxide layer 110, and a second silicon oxide layer 112 located on the silicon nitride layer 111.
[0034] In this embodiment, the side walls of the control gate 120 and the control gate dielectric layer 113 are also formed with a first side wall 121 and a second side wall 122. The first side wall 121 is located on the side wall surfaces of the control gate 120 and the control gate dielectric layer 113, and the second side wall 122 is only located on the surface of the first side wall 121 on the control gate 120 and the control gate dielectric layer 113 exposed by the first opening. The first side wall 121 and the second side wall 122 are used to etch and form the floating gate 103.
[0035] Please refer to Figure 2 , a gate oxide layer 102 is formed in the logic region II.
[0036] In the process of forming the gate oxide layer 102, it is inevitable to affect the device structure already formed on the storage area I, especially the floating gate protrusion (such as Figure 2 As shown in A in the figure, the corners formed by the top and sidewall surfaces are more likely to be over-oxidized under the action of the oxidation process, thereby rounding the corners and introducing structural defects, resulting in reduced erase efficiency of the memory.
[0037] In order to solve the above technical problems, the technical solution of the present invention provides a method for forming a semiconductor structure, by forming a protective layer on the side wall surface of the floating gate before forming a gate oxide layer in the logic area, so that in the subsequent process of forming a gate oxide layer in the logic area, the protective layer can protect the side wall surface of the floating gate exposed by the first opening, reducing the influence of the oxidation process on the morphology of the floating gate, thereby improving the stability of the memory erase efficiency.
[0038] In order to make the above-mentioned objects, features and beneficial effects of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0039] Figures 3 to 11 It is a schematic cross-sectional structural diagram of a formation process of a semiconductor structure according to an embodiment of the present invention.
[0040] Please refer to Figure 3 , a substrate 200 is provided, wherein the substrate 200 includes a storage area I and a logic area II.
[0041] In this embodiment, the storage area I provides a platform for a flash memory device formed subsequently, and the logic area II provides a platform for a logic device formed subsequently.
[0042] The material of the substrate 200 includes silicon, silicon germanium, silicon carbide, silicon on insulator (SOI), germanium on insulator (GOI), etc. Specifically, in this embodiment, the material of the substrate 200 is silicon.
[0043] Next, separate and paired storage gate structures are formed in the storage area I, with a first opening between the paired storage gate structures, each storage gate structure comprising a floating gate located on the substrate 200, a control gate dielectric layer located on the floating gate, and a control gate located on the control gate dielectric layer, and the first opening exposes at least a portion of the sidewall surface of the floating gate. At least one pair of storage gate structures is formed in the storage area I, and the paired storage gate structures include two storage gate structures.
[0044] For ease of understanding, in this embodiment, a pair of storage gate structures is formed in the storage area I, that is, two storage gate structures are formed in the storage area I. In other embodiments, multiple pairs of storage gate structures may be formed in the storage area, and the number of pairs of the storage gate structures is greater than or equal to 2.
[0045] Specifically, the process of forming the storage gate structure is as follows: Figures 4 to 7 shown.
[0046] Please refer to Figure 4 , a floating gate dielectric layer 201 is formed on the storage area I.
[0047] In this embodiment, the material of the floating gate dielectric layer 201 includes silicon oxide.
[0048] Specifically, the method for forming the floating gate dielectric layer 201 includes: forming an initial floating gate dielectric layer (not shown) on the surface of the substrate 200; removing the initial floating gate dielectric layer on the surface of the logic area II to form a floating gate dielectric layer 201 located on the surface of the storage area I.
[0049] Please refer to Figure 5 A floating gate material layer 203 is formed on the floating gate dielectric layer 201; two separate control gate dielectric layers 213 and a control gate 220 located on the surface of the control gate dielectric layer 213 are formed on the floating gate material layer 203, and a first opening 223 is provided between adjacent control gates 220, and the first opening 223 exposes the sidewalls of the control gate 220, the sidewalls of the control gate dielectric layer 213 and the surface of the floating gate material layer 203.
[0050] In this embodiment, the floating gate material layer 203 provides raw materials for a floating gate formed subsequently.
[0051] In this embodiment, the floating gate material layer 203 is made of polysilicon.
[0052] In this embodiment, the first opening 223 provides space for an erase gate to be formed subsequently.
[0053] In this embodiment, the method for forming the control gate dielectric layer 213 and the control gate 220 includes: forming a control gate dielectric material layer (not shown) and a control gate material layer (not shown) on the floating gate material layer 203; forming a mask layer 225 on the control gate material layer, the mask layer 225 exposing a portion of the control gate material layer surface on the storage area I; using the mask layer 225 as a mask, etching the control gate material layer and the control gate dielectric material layer until the surface of the floating gate material layer 203 is exposed to form the control gate 220 and the control gate dielectric layer 213.
[0054] In this embodiment, the material of the control gate 220 includes polysilicon.
[0055] In this embodiment, the control gate dielectric layer 213 includes: a first silicon oxide layer 210 located on the floating gate material layer 203 , a silicon nitride layer 211 located on the surface of the first silicon oxide layer 210 , and a second silicon oxide layer 212 located on the surface of the silicon nitride layer 211 .
[0056] Please refer to Figure 6 , etching a portion of the floating gate material layer 203 so that the bottom surface of the first opening 223 is lower than the bottom surface of the control gate dielectric layer 213 .
[0057] In this embodiment, the process of etching a portion of the floating gate material layer 203 includes a dry etching process.
[0058] Please refer to Figure 7 , forming a sidewall structure (not shown) on the sidewall of the control gate 220, the sidewall of the control gate dielectric layer 213 and the sidewall surface of part of the floating gate material layer 203; using the sidewall structure as a mask, etching the floating gate material layer 203 until the surface of the floating gate dielectric layer 201 is exposed, thereby forming a floating gate 204, and the floating gate 204 has a floating gate protrusion B protruding toward the first opening 223.
[0059] In this embodiment, the control gate 220 includes a first sidewall (not labeled) and a second sidewall (not labeled) opposite to each other, the first sidewall faces the first opening 223, and the floating gate protrusion B exposed by the first opening 223 is protruding relative to the first sidewall. Specifically, the sidewall surface of the floating gate protrusion B is perpendicular to the surface of the substrate 200; the top surface of the floating gate protrusion B is parallel to the surface of the substrate 200.
[0060] In this embodiment, the sidewall structure includes a first sidewall (not labeled) and a second sidewall (not labeled), wherein the first sidewall is located on the sidewall of the control gate 220, the sidewall of the control gate dielectric layer 213 and a portion of the sidewall surface of the floating gate material layer 203 exposed by the first opening 223, and the second sidewall is located on the sidewall surface on the other side of the control gate 220, the control gate dielectric layer 213 and the floating gate material layer 203, and the thickness of the first sidewall is greater than the thickness of the second sidewall.
[0061] Specifically, the first spacer includes: a first structure 221 located on the sidewall of the control gate 220, the sidewall of the control gate dielectric layer 213, and the sidewall surface of a part of the floating gate material layer 203 exposed by the first opening 223; and a second structure 222 located on the surface of the first structure 221. The second spacer only includes the first structure 221 located on the sidewall of the control gate 220, the sidewall of the control gate dielectric layer 213, and the sidewall surface of a part of the floating gate material layer 203. Therefore, by forming the spacer structure, the morphology of the floating gate 204 formed in the end is adjusted. The thickness of the first spacer and the second spacer determines the size of the floating gate protrusion, that is, the size of the floating gate protrusion B exposed by the first opening 223 is larger than the size of the floating gate protrusion on the other side of the storage gate structure. The size is the size of the floating gate protrusion in the direction parallel to the surface of the substrate 200.
[0062] Among them, the floating gate protrusion B exposed by the first opening 223 is larger in size. Therefore, after the erase gate is subsequently formed in the first opening 223, during the erase operation of the erase gate, the electric field at the protruding corner of the floating gate protrusion B is more concentrated, which is beneficial for the electrons in the floating gate 204 to tunnel into the erase gate through the floating gate protrusion B, thereby obtaining a higher erasing efficiency and improving the performance of the device and the yield of the chip.
[0063] In another embodiment, the thickness of the first sidewall is equal to that of the second sidewall.
[0064] In another embodiment, the spacer structure is formed only on the sidewalls of the control gate and the sidewalls of the control gate dielectric layer exposed by the first opening.
[0065] In another embodiment, after etching the control gate material layer and the control gate dielectric material layer to form the control gate and the control gate dielectric layer, the floating gate material layer is no longer etched, and a sidewall structure is directly formed on the exposed floating gate material layer. Therefore, with the sidewall structure as a mask, the top surface of the floating gate protrusion formed by etching the floating gate material layer is flush with the bottom surface of the control gate dielectric layer.
[0066] In other embodiments, after a mask layer is formed on the control gate material layer, the control gate material layer, the control gate dielectric material layer and the floating gate material layer are etched using the mask layer as a mask until the surface of the floating gate dielectric layer is exposed to form a control gate, a control gate dielectric layer and a floating gate, and the side wall surfaces of the control gate, the control gate dielectric layer and the floating gate are located on the same plane.
[0067] Please refer to Figure 8 A tunneling dielectric layer 230 is formed on the surface of the floating gate 204 , the surface of the control gate 220 , and the surface of the control gate dielectric layer 213 exposed by the first opening 223 .
[0068] In this embodiment, the material of the tunnel dielectric layer 230 includes silicon oxide.
[0069] In this embodiment, the thickness of the tunnel dielectric layer 230 is in the range of 80 angstroms to 130 angstroms.
[0070] In this embodiment, the tunnel dielectric layer 230 is also located on the sidewall of the storage gate structure (not shown) away from the first opening 223; the tunnel dielectric layer 230 is also located on the surface of the floating gate dielectric layer 201 and the surface of the logic region II.
[0071] Please refer to Fig. 9 , forming a protection layer 240 on the surface of the tunnel dielectric layer 230 .
[0072] In this embodiment, the protective layer 240 covers the side walls, top and corners of the floating gate protrusion B of the floating gate 204 exposed by the first opening 223. Therefore, in the subsequent process of forming a gate oxide layer in the logic area II, the protective layer 240 can protect the side walls, top and corners of the floating gate protrusion B of the floating gate 204 exposed by the first opening 223, reduce the influence of the oxidation process on the morphology of the floating gate 204, prevent the rounding of the corners of the floating gate protrusion, and thus improve the stability of the memory erase efficiency.
[0073] In this embodiment, the material of the protection layer 240 includes silicon nitride.
[0074] In this embodiment, the thickness of the protection layer 240 ranges from 0 to 100 angstroms. Under this thickness, the floating gate 204 can be effectively protected.
[0075] In this embodiment, the method for forming the protection layer 240 includes a chemical vapor deposition process, and the protection layer 240 is directly formed on the surface of the tunnel dielectric layer 230 .
[0076] Specifically, the method for forming the protective layer 240 includes: forming a protective layer 240 on the surface of the tunneling dielectric layer 230 in the storage area I and the surface of the tunneling dielectric layer 230 in the logic area II; removing the protective layer 240 in the logic area II to expose the tunneling dielectric layer 230 on the surface of the logic area II.
[0077] In another embodiment, the method for forming the protective layer includes an ion implantation process. By implanting nitrogen ions on the surface of the tunnel dielectric layer, the top area of the tunnel dielectric layer can be converted into a protective layer. In this embodiment, the protective layer is formed by ion implantation. The thickness and density of the formed protective layer can be adjusted by adjusting the concentration, energy and other parameters of the ion implantation, so that the protective strength, morphology, thickness, etc. of the protective layer can be designed according to the requirements, thereby increasing the adjustability of the protective layer. The protective layer is formed by ion implantation, which is lower in cost and shorter in preparation time.
[0078] Specifically, the parameters of the ion implantation process include: the energy of the ion implantation is 0-30 keV; the ion implantation dose is 1E12 ions / cm 2 ~1E16 ions / cm 2 Before the protective layer is formed, the tunnel dielectric layer needs to have a thickness ranging from 100 angstroms to 150 angstroms.
[0079] Please refer to Fig.10 , an oxidation process is used to form a gate oxide layer 250 on the surface of the logic region II.
[0080] In this embodiment, the gate oxide layer 250 is used in a high voltage MOS device.
[0081] Specifically, the method for forming the gate oxide layer 250 includes: one of a thermal oxidation process and a diffusion process or a combination of the two. A relatively thick gate oxide layer 250 can be formed by a relatively long thermal oxidation process or a diffusion process, thereby ensuring that it can meet the gate voltage requirements of the high-voltage MOS device.
[0082] In the process of forming the gate oxide layer 250 using the thermal oxidation process and the diffusion process, since the protective layer 240 has been formed in advance on the surface of the tunnel dielectric layer 230 on the storage area I, the protective layer 240 can protect the side wall of the floating gate 204 exposed by the first opening 223, so that the oxygen in the oxidation process cannot penetrate and reach the floating gate 204, reducing the influence of the oxidation process on the morphology of the floating gate 204, avoiding the rounding of the floating gate protrusion B, thereby improving the stability of the memory erase efficiency. In addition, in the process of adjusting the parameters of the oxidation process, only the morphology and thickness of the gate oxide layer 250 on the logic area II need to adjust the parameters of the oxidation process, without considering its influence on the device structure formed in the storage area I, thereby making the process window larger and the effect and efficiency of process control higher.
[0083] Please refer to Fig.11 After forming the gate oxide layer 250, the protection layer 240 on the storage area I is removed to expose the surface of the tunnel dielectric layer 230.
[0084] In this embodiment, the method for removing the protective layer 240 includes a wet etching process, which can completely remove the protective layer 240 without affecting the tunnel dielectric layer 230 .
[0085] Next, an erase gate (not shown) is formed in the first opening 223; a gate (not shown) and a source and drain (not shown) located in the logic area II on both sides of the gate are formed on the gate oxide layer 250, so that the storage area I and the logic area II can perform corresponding device functions.
[0086] In this embodiment, the device structure formed on the storage area I is suitable for a Nor Flash device.
[0087] In this embodiment, the method for forming the device structure on the storage area I and the device structure on the logic area II is applicable to technology platform nodes including 28nm, 40nm, 55nm and 70nm.
[0088] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.
Claims
1. A method for forming a semiconductor structure, characterized in that: include: Providing a substrate, the substrate comprising a storage area and a logic area; Separate and paired memory gate structures are formed in the memory region, a first opening is provided between the paired memory gate structures, each memory gate structure comprises a floating gate located on a substrate, a control gate dielectric layer located on the floating gate, and a control gate located on the control gate dielectric layer, and the first opening exposes at least a portion of a sidewall surface of the floating gate; forming a tunneling dielectric layer on the floating gate surface and the control gate surface exposed by the first opening; forming a protective layer on the surface of the tunnel dielectric layer; After forming the protection layer, an oxidation process is adopted to form a gate oxide layer on the surface of the logic region.
2. The method for forming a semiconductor structure according to claim 1, wherein: The control gate includes a first sidewall and a second sidewall opposite to each other, the first sidewall faces the first opening, and the floating gate includes a floating gate protrusion protruding relative to the first sidewall.
3. The method for forming a semiconductor structure according to claim 2, wherein: The sidewall surface of the floating gate protrusion is perpendicular to the substrate surface; the top surface of the floating gate protrusion is parallel to the substrate surface.
4. The method for forming a semiconductor structure according to claim 1, wherein: The material of the protection layer includes silicon nitride.
5. The method for forming a semiconductor structure according to claim 1, wherein: The thickness of the protective layer ranges from 0 to 100 angstroms.
6. The method for forming a semiconductor structure according to claim 1, wherein: The method for forming the protective layer includes a chemical vapor deposition process.
7. The method for forming a semiconductor structure according to claim 6, wherein: The thickness of the tunnel dielectric layer is in the range of 80 angstroms to 130 angstroms.
8. The method for forming a semiconductor structure according to claim 1, wherein: The method for forming the protective layer includes an ion implantation process.
9. The method for forming a semiconductor structure according to claim 8, wherein: The parameters of the ion implantation process include: the energy of ion implantation is 0-30 keV; the ion implantation dose is 1E12 ions / cm 2 ~1E16 ions / cm 2 .
10. The method for forming a semiconductor structure according to claim 8, wherein: The thickness of the tunnel dielectric layer ranges from 100 angstroms to 150 angstroms.
11. The method for forming a semiconductor structure according to claim 1, wherein: The method of forming the gate oxide layer includes: a thermal oxidation process and a diffusion process or a combination of the two.
12. The method for forming a semiconductor structure according to claim 1, wherein: After forming the gate oxide layer, the method further includes: removing the protection layer on the storage area.
13. The method for forming a semiconductor structure according to claim 12, wherein: After removing the protection layer, the method further includes: forming an erase gate in the first opening.
14. The method for forming a semiconductor structure according to claim 1, wherein: Also includes: A gate is formed on the gate oxide layer.
15. The method for forming a semiconductor structure according to claim 1, wherein: There is a floating gate dielectric layer between the floating gate and the substrate; the control gate sidewall, the control gate dielectric layer sidewall and part of the floating gate sidewall surface also have a sidewall structure, and the sidewall structure is formed before the tunneling oxide layer.
16. The method for forming a semiconductor structure according to claim 15, wherein: The sidewall structure includes a first sidewall and a second sidewall. The first sidewall is located on the control gate sidewall and the control gate dielectric layer sidewall surface exposed by the first opening. The second sidewall is located on the sidewall surface on the other side of the control gate and the control gate dielectric layer. The thickness of the first sidewall is greater than the thickness of the second sidewall.
17. The method for forming a semiconductor structure according to claim 15, wherein: The method for forming the storage gate structure includes: forming a floating gate dielectric layer on the substrate; forming a floating gate material layer on the floating gate dielectric layer; forming two separate control gate dielectric layers and a control gate located on the surface of the control gate dielectric layer on the floating gate material layer, wherein a first opening is provided between adjacent control gates, and the first opening exposes the control gate sidewalls, the control gate dielectric layer sidewalls and the floating gate material layer surface; forming a sidewall structure on the control gate sidewalls and the control gate dielectric layer sidewall surfaces; using the sidewall structure as a mask, etching the floating gate material layer until the surface of the floating gate dielectric layer is exposed, thereby forming a floating gate, wherein the floating gate has a floating gate protrusion protruding toward the first opening.
18. The method for forming a semiconductor structure according to claim 17, wherein: The method for forming the control gate dielectric layer and the control gate comprises: forming a control gate dielectric material layer and a control gate material layer on the floating gate material layer; forming a mask layer on the control gate material layer, wherein the mask layer exposes a portion of the control gate material layer surface on the storage area; using the mask layer as a mask, etching the control gate material layer and the control gate dielectric material layer until the surface of the floating gate material layer is exposed to form a control gate and a control gate dielectric layer.
19. The method for forming a semiconductor structure according to claim 18, wherein: After etching the control gate material layer and the control gate dielectric material layer, the method further includes: etching a portion of the floating gate material layer; the sidewall structure is formed on the control gate sidewall, the control gate dielectric layer sidewall and a portion of the floating gate material layer sidewall surface.