Method for applying coal gangue to ecological restoration of mining area
By preparing coal gangue powder, cement and aluminum powder into foams and forming a multi-layer structure on the land in the mining area, the problems of land destruction and resource waste in the mining area are solved, and the soil and water conservation capacity and material stability are significantly improved, thus achieving the The effectiveness of ecological restoration in mining areas.
Patent Information
- Application Number
- CN202411034344.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-11-29
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Land damage and resource waste caused by mining activities in mining areas, coal gangue has not been effectively utilized as an associated waste, and there is a lack of effective ecological restoration methods.
Coal gangue powder, cement and aluminum powder are foamed and dried and prepared into ecological restoration materials in coal gangue mining areas, and laid layer by layer on the land in the mining area to form a multi-layer structure to improve soil and water conservation capabilities.
It significantly improves the soil and water conservation capacity, reduces the water loss rate, enhances the stability and water retention capacity of the material, and forms a loose pore structure to enhance the natural recovery ability of the soil.
Smart Images

Figure HDA0004970673370000011
Abstract
Description
Technical Field
[0001] The invention belongs to the field of ecological restoration of mining areas, and in particular relates to a method for applying coal gangue to ecological restoration of mining areas. Background Art
[0002] Ecological restoration of mining areas refers to the process of repairing and restoring the ecological environment damaged by mining activities after mining is completed. This includes the restoration of land, vegetation, hydrology, and soil and water conservation to restore the natural ecological functions of the mining area and reduce or eliminate the negative impact of mining activities on the environment. Coal gangue is a common associated waste in mining operations. It mainly comes from coal mining and washing processes. Because it does not have the characteristics of fossil energy use, it is often stored as waste around the mining area, which leads to the occupation of a large amount of land resources. In addition, gangue mountains are prone to spontaneous combustion, which poses a great safety hazard. If coal gangue can be used for ecological restoration of mining areas, it will effectively reduce resource waste and economic benefits, and realize the closed loop of mining and waste recycling. However, there are currently few methods for applying coal gangue to ecological restoration in mining areas. Summary of the invention
[0003] In view of the above situation, in order to overcome the defects of the prior art, the present invention provides a method for applying coal gangue to ecological restoration of mining areas. The present invention uses coal gangue powder, cement, aluminum powder and water as raw materials to prepare coal gangue mining area ecological restoration materials, which have strong soil and water conservation capabilities.
[0004] In order to achieve the above-mentioned purpose, the following technical scheme is adopted: The present invention provides a method for applying coal gangue to ecological restoration of mining areas, comprising the following steps:
[0005] S1. Grind the gangue into gangue powder, mix it with cement, add water, and stir it in a water bath at 50°C to make a slurry. Then add aluminum powder to the slurry and stir it continuously. After 12 hours, pour the slurry into an iron mold and place it in a constant temperature and humidity incubator at 70°C to foam the slurry. After the foaming is completed, remove the mold to obtain a foamed body. Place the foamed body in an oven at 105°C for drying. After the drying is completed, crush the foamed body, screen out material particles with particle sizes of 1-3mm and 3-5mm, and obtain a gangue mining area ecological restoration material;
[0006] S2. Lay a layer of 3-5 mm coal gangue mining area ecological restoration material on the land to be treated to form a first coal gangue layer, then lay a layer of mining area lime on it to obtain a lime layer, then lay soil on the soil layer to obtain a soil layer, and then lay a layer of 1-3 mm coal gangue mining area ecological restoration material on the lime layer to form a second coal gangue layer.
[0007] Furthermore, the weight ratio of the coal gangue powder, cement, aluminum powder and water is 10-20:15-20:3-5:100-120.
[0008] Furthermore, the coal gangue powder is obtained by calcining coal gangue at 700-900° C. for 3-5 hours and then grinding it.
[0009] Furthermore, the particle size of the coal gangue powder is 50-100 mesh.
[0010] Furthermore, the thickness of the first gangue layer is 20-30 cm.
[0011] Furthermore, the particle size of the lime layer is 50-100 mesh, and the thickness of the lime layer is 10-20 cm.
[0012] Furthermore, the soil layer is taken from the land in the mining area, and the thickness of the soil layer is 15-30 cm.
[0013] Furthermore, the thickness of the second gangue layer is 10-20 cm.
[0014] The beneficial effects of the present invention are as follows: the present invention provides a method for applying coal gangue to ecological restoration of mining areas. The coal gangue itself has a rich pore structure. After the coal gangue is prepared into a coal gangue mining area ecological restoration material, the kaolinite content inside the material increases, and during the preparation of the material, the aluminum powder reacts to generate bubbles, resulting in a rich pore structure inside the material, wherein the semi-open pores, closed pores and connected pores inside the particles, including gaps formed by natural accumulation between material particles, all improve the water retention capacity of the material and reduce its loss rate. At the same time, the kaolinite content in the material is increased compared with the content of the coal gangue, which also improves the water retention capacity of the material, improves its stability, and reduces its loss rate; in addition, the agglomerate structure formed by the agglomeration of soil particles is relatively dense, which increases the resistance to water flow and reduces the soil's ability to retain water molecules. The stability of the soil aggregates is poor, resulting in a high loss rate, while the agglomerates formed after the particles of the material are agglomerated still have a loose structure, and some through holes are potentially formed between the materials, further improving the soil and water conservation capacity of the material. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 The figures are the test results of soil and water conservation capacity of various embodiments of the present invention and the soil in the mining area.
[0016] The accompanying drawings are used to provide further understanding of the present invention and constitute a part of the specification. They are used to explain the present invention together with the embodiments of the present invention and do not constitute a limitation of the present invention. DETAILED DESCRIPTION
[0017] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.
[0018] Unless otherwise defined, all professional and scientific terms used herein have the same meanings as those familiar to those skilled in the art. In addition, any methods and materials similar or equivalent to those described herein may be applied to the present invention. The preferred implementation methods and materials described herein are for demonstration purposes only and are not intended to limit the content of this application.
[0019] The experimental methods in the following examples are conventional methods unless otherwise specified, and the experimental materials used in the following examples are purchased from commercial channels unless otherwise specified.
[0020] Example 1
[0021] A method for applying coal gangue to ecological restoration of mining areas
[0022] The method comprises the following steps:
[0023] S1. Grind the gangue into gangue powder, mix it with cement, add water, and stir it in a water bath at 50°C to make a slurry. Then add aluminum powder to the slurry and stir it continuously. After 12 hours, pour the slurry into an iron mold and place it in a constant temperature and humidity incubator at 70°C to foam the slurry. After the foaming is completed, remove the mold to obtain a foamed body. Place the foamed body in an oven at 105°C for drying. After the drying is completed, crush the foamed body, screen out material particles with particle sizes of 1-3mm and 3-5mm, and obtain a gangue mining area ecological restoration material;
[0024] S2. Lay a layer of 3-5 mm coal gangue mining area ecological restoration material on the land to be treated to form a first coal gangue layer, then lay a layer of mining area lime on it to obtain a lime layer, then lay soil on the soil layer to obtain a soil layer, and then lay a layer of 1-3 mm coal gangue mining area ecological restoration material on the lime layer to form a second coal gangue layer.
[0025] The weight ratio of the coal gangue powder, cement, aluminum powder and water is 10:15:3:100.
[0026] The coal gangue powder is obtained by calcining coal gangue at 700° C. for 3 hours and then grinding it.
[0027] The particle size of the coal gangue powder is 50 mesh.
[0028] The thickness of the first coal gangue layer is 20 cm.
[0029] The particle size of the lime layer is 50 meshes, and the thickness of the lime layer is 10 cm.
[0030] The soil layer is taken from the land in the mining area, and the thickness of the soil layer is 15 cm.
[0031] The thickness of the second gangue layer is 10 cm.
[0032] Example 2
[0033] A method for applying coal gangue to ecological restoration of mining areas
[0034] The steps included in the method are the same as those in Example 1.
[0035] The weight ratio of the coal gangue powder, cement, aluminum powder and water is 20:20:5:120.
[0036] The coal gangue powder is obtained by calcining coal gangue at 900° C. for 5 hours and then grinding it.
[0037] The particle size of the coal gangue powder is 100 mesh.
[0038] The thickness of the first gangue layer is 30 cm.
[0039] The particle size of the lime layer is 100 meshes, and the thickness of the lime layer is 20 cm.
[0040] The soil layer is taken from the land in the mining area, and the thickness of the soil layer is 30 cm.
[0041] The thickness of the second gangue layer is 20 cm.
[0042] Example 3
[0043] A method for applying coal gangue to ecological restoration of mining areas
[0044] The steps included in the method are the same as those in Example 1.
[0045] The weight ratio of the coal gangue powder, cement, aluminum powder and water is 15:18:4:110.
[0046] The coal gangue powder is obtained by calcining coal gangue at 800° C. for 4 hours and then grinding it.
[0047] The particle size of the coal gangue powder is 80 meshes.
[0048] The thickness of the first coal gangue layer is 15 cm.
[0049] The particle size of the lime layer is 70 meshes, and the thickness of the lime layer is 15 cm.
[0050] The soil layer is taken from the land in the mining area, and the thickness of the soil layer is 20 cm.
[0051] The thickness of the second gangue layer is 15 cm.
[0052] Results Analysis
[0053] The soil and water conservation capacity of the mining area soil of each embodiment and soil was tested, and the water conservation test results are shown in Figure 1 .
[0054] Depend on Figure 1 It can be seen that the coal gangue mining area ecological restoration material prepared by the present invention has a water retention rate far greater than that of ordinary Qu soil, which proves that it has good soil and water conservation ability.
[0055] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
[0056] The present invention and its implementation methods are described above, which is not restrictive. The drawings are only one of the implementation methods of the present invention, and the actual application is not limited thereto. In short, if ordinary technicians in the field are inspired by it and design methods and embodiments similar to the technical solution without creativity without departing from the purpose of the invention, they should all fall within the protection scope of the present invention.
Claims
1. A method for applying coal gangue to ecological restoration of mining areas, characterized in that: The steps include: S1. Grind the gangue into gangue powder, mix it with cement, add water, and stir it in a water bath at 50°C to make a slurry. Then add aluminum powder to the slurry and stir it continuously. After 12 hours, pour the slurry into an iron mold and place it in a constant temperature and humidity incubator at 70°C to foam the slurry. After the foaming is completed, remove the mold to obtain a foamed body. Place the foamed body in an oven at 105°C for drying. After the drying is completed, crush the foamed body, screen out material particles with particle sizes of 1-3mm and 3-5mm, and obtain a gangue mining area ecological restoration material; S2. Lay a layer of 3-5 mm coal gangue mining area ecological restoration material on the land to be treated to form a first coal gangue layer, then lay a layer of mining area lime on it to obtain a lime layer, then lay soil on the soil layer to obtain a soil layer, and then lay a layer of 1-3 mm coal gangue mining area ecological restoration material on the lime layer to form a second coal gangue layer.
2. The method of applying coal gangue to ecological restoration of mining areas according to claim 1, characterized in that: The weight ratio of the coal gangue powder, cement, aluminum powder and water is 10-20:15-20:3-5:100-120.
3. The method of applying coal gangue to ecological restoration of mining areas according to claim 2, characterized in that: The coal gangue powder is obtained by calcining coal gangue at 700-900° C. for 3-5 hours and then grinding it.
4. The method of applying coal gangue to ecological restoration of mining areas according to claim 3 is characterized in that: The particle size of the coal gangue powder is 50-100 meshes.
5. The method of applying coal gangue to ecological restoration of mining areas according to claim 4, characterized in that: The thickness of the first gangue layer is 20-30 cm.
6. The method of applying coal gangue to ecological restoration of mining areas according to claim 5, characterized in that: The particle size of the lime layer is 50-100 meshes, and the thickness of the lime layer is 10-20 cm.
7. The method of applying coal gangue to ecological restoration of mining areas according to claim 6, characterized in that: The soil layer is taken from the land in the mining area, and the thickness of the soil layer is 15-30 cm.
8. The method of applying coal gangue to ecological restoration of mining areas according to claim 7, characterized in that: The thickness of the second gangue layer is 10-20 cm.
Citation Information
Patent Citations
Method for conducting ecological restoration in mine geological disaster region
CN104255109A
Coal gangue porous soil conditioner and preparation method thereof
CN111117629A
Material suitable for ecological restoration of northern mining area and preparation method thereof
CN114591743A
Method for repairing mine by filling coal mine subsidence area and gully region with coal gangue
CN116043874A
Vegetation recovery method for acid coal gangue mountain
CN116998270A