Method for manufacturing ram of numerical control machine tool
By selecting steel plate materials and using cutting, welding, stress removal annealing and quenching processes, the problem of casting defects of CNC machine tools is solved, and high-strength, low-weight and short-cycle sliding pillow production is achieved, improving production efficiency and products quality.
Patent Information
- Application Number
- CN202411220140.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-02
- Publication Date
- 2024-11-29
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing CNC machine tool sliding pillows are prone to defects such as sand holes, pores, slag holes, shrinkage and cracks through the casting process, resulting in high waste rate, relatively poor rigidity and strength, and bulky, affecting production efficiency.
The sliding pillow is made by cutting, welding, stress removal annealing, quenching, sandblasting and coating to avoid casting defects, and through multi-layer multi-pass welding and non-destructive damage detection Ensure quality.
The high strength, low weight, short production cycle and simple equipment requirements of the sliding pillow are achieved, and casting defects are avoided and the product yield and production efficiency are improved.
Smart Images

Figure CN119035988A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of numerical control machine tools, and in particular relates to a method for manufacturing a ram of a numerical control machine tool. Background Art
[0002] The manufacture and development of CNC machine tools is one of the important indicators to measure a country's industrial level. In medium and large CNC machine tools, the ram, as a key component, plays a very important role in the entire CNC machine tool system. At present, the shape of the ram is mainly prismatic, and its cross-section can generally be divided into two types: square and "well" type. The use of the ram can generally be divided into two types: linear rail type and hydrostatic rail type, and the ram is usually made by casting.
[0003] For cast rams, the material is usually required to be high-strength gray cast iron, and no casting defects are allowed on the casting surface, and welding is not allowed. However, this type of casting is prone to casting defects such as sand holes, pores, slag holes, shrinkage and cracks, and the scrap rate is often high, which not only increases the manufacturing cost and reduces the product yield, but also may affect the production efficiency; in addition, the rigidity and strength of cast rams are relatively poor, and cast rams are also relatively bulky. Therefore, it is urgent to study a method for manufacturing a CNC machine tool ram to solve the above problems. Summary of the invention
[0004] The present invention provides a method for manufacturing a ram of a numerically controlled machine tool, the purpose of which is to solve the technical problems raised in the above-mentioned background technology.
[0005] In order to solve the above technical problems, the present invention is achieved through the following technical solutions:
[0006] The present invention is a method for manufacturing a ram of a numerically controlled machine tool, comprising the following steps:
[0007] Step 1: Material selection: Select one of No. 35 steel plate, Q235B steel plate and Q355B steel plate as the base material;
[0008] Step 2, cutting and blanking: selecting appropriate cutting equipment according to the thickness of the selected substrate, and using the cutting equipment to cut the substrate into sub-parts of the ram, the sub-parts of the ram including a first sealing plate (1), a second sealing plate (2), a third sealing plate (3), a fourth sealing plate (4), a first rib plate (5), a second rib plate (6), a third rib plate (7) and an end cover sealing plate (8);
[0009] Step 3: Beveling: Cut a single-sided V-shaped bevel on the third sealing plate (3) and the fourth sealing plate (4) respectively and polish them to make them smooth;
[0010] Step 4: Calibration and sandblasting: First, all sub-parts of the ram are leveled and straightened in sequence through a straightening machine, and then the surfaces of all sub-parts of the ram are sandblasted;
[0011] Step 5, welding: After the first sealing plate (1), the second sealing plate (2), the fourth sealing plate (4), the first rib plate (5), the second rib plate (6), the third rib plate (7) and the end cover sealing plate (8) are positioned by spot welding according to the design size requirements, the two main welds of the first sealing plate (1) and the fourth sealing plate (4), the second sealing plate (2) and the fourth sealing plate (4) are welded in multiple layers and multiple passes by using CO2 shielded welding, and then the first rib plate (5), the second rib plate (6), the third rib plate (7) and the end cover sealing plate (8) are welded in turn, and then the third sealing plate (3) is sealed and spot welded to position, and then the remaining welds are continuously welded in the above manner, and finally the ram welded blank is formed;
[0012] Step 6: Correction: Check the size, flatness and verticality of the ram blank. Straighten and correct the parts where the shape and position tolerances exceed the standard by fire attack;
[0013] Step 7: Stress relief annealing and flaw detection: First, stress relief annealing is used to eliminate the internal stress of the weld of the ram blank, and then non-destructive flaw detection is performed on each external weld of the ram blank by combining magnetic particle flaw detection and ultrasonic flaw detection;
[0014] Step 8, rough machining and secondary stress relief annealing: firstly, the four side faces and two end faces of the ram blank are rough machined with a machining allowance of 4-6 mm to obtain a ram semi-finished product, and then the ram semi-finished product is subjected to a second stress relief annealing aging treatment;
[0015] Step 9, semi-finishing and high-frequency quenching: firstly, semi-finishing the four sides, two end faces and internal rib plate holes of the semi-finished ram is processed, and a processing allowance of 0.15-0.25mm is left, and then the four sides of the semi-finished ram are processed by high-frequency quenching;
[0016] Step 10, tempering, sandblasting and painting: firstly, the semi-finished ram is subjected to low-temperature tempering aging treatment, then the surface of the semi-finished ram is subjected to sandblasting treatment, and the non-machined surface of the semi-finished ram is subjected to surface painting treatment;
[0017] Step 11: Grinding and guide rail straightness inspection: First, grind and cut the four side faces and two end faces of the semi-finished ram part on a high-precision guide rail grinder, and then use high-precision testing equipment to test and confirm the shape and position tolerance accuracy of the four side faces and two end faces of the semi-finished ram part;
[0018] Step 12, finishing of drilling and rib plate holes and final acceptance: First, all holes on the semi-finished ram parts are finished by CNC machine tools, and then all dimensional tolerances and geometric tolerances of the finished ram parts are confirmed and accepted according to the processing drawings of the ram.
[0019] As a preferred technical solution of the present invention, in the step five, the first rib plate (5), the second rib plate (6) and the third rib plate (7) are first spot welded to the fourth sealing plate (4) in sequence, and then the first sealing plate (1) and the second sealing plate (2) are spot welded to the fourth sealing plate (4), and then the first rib plate (5), the second rib plate (6) and the third rib plate (7) are respectively connected to the first sealing plate (1) and the second sealing plate (2) by spot welding, and then the first sealing plate (1), the second sealing plate (2) and the fourth sealing plate (4) are respectively connected to the end cover sealing plate (8) by spot welding.
[0020] As a preferred technical solution of the present invention, in step eight, the machining allowance is 5 mm.
[0021] As a preferred technical solution of the present invention, in step nine, the machining allowance is 0.2 mm.
[0022] The present invention has the following beneficial effects:
[0023] Compared with the prior art, the present invention is not only less likely to produce casting defects such as sand holes, air holes, slag holes, shrinkage, cracks, etc., but also the manufactured slide has strong rigidity and high strength. At the same time, the slide has a short production cycle, light weight, relatively simple production equipment and fast modification.
[0024] Of course, any product implementing the present invention does not necessarily need to achieve all of the advantages described above at the same time. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for describing the embodiments are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0026] Figure 1 It is a structural schematic diagram of the ram of a CNC machine tool of the present invention.
[0027] Figure 2 for Figure 1 The main view of the structure.
[0028] Figure 3 for Figure 1 Side view of the structure.
[0029] In the accompanying drawings, the components represented by the reference numerals are listed as follows:
[0030] 1-first sealing plate, 2-second sealing plate, 3-third sealing plate, 4-fourth sealing plate, 5-first rib plate, 6-second rib plate, 7-third rib plate, 8-end cover sealing plate. DETAILED DESCRIPTION
[0031] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0032] See also Figure 1-3 As shown, the present invention is a method for manufacturing a ram of a CNC machine tool, comprising the following steps:
[0033] Step 1: Material selection: Based on comprehensive factors such as material physical properties, welding performance characteristics, heat treatment methods, cutting performance characteristics and production costs, select one of 35 steel plates, Q235B steel plates and Q355B steel plates as the base material;
[0034] Step 2, cutting and blanking: select appropriate cutting equipment according to the thickness of the selected substrate, and use the cutting equipment to cut the substrate into sub-parts of the ram, the sub-parts of the ram include the first sealing plate 1, the second sealing plate 2, the third sealing plate 3, the fourth sealing plate 4, the first rib plate 5, the second rib plate 6, the third rib plate 7 and the end cover sealing plate 8; wherein, the cutting and blanking equipment can be selected from flame cutting machine, plasma cutting machine or laser cutting machine, etc.;
[0035] Step 3: Beveling: Cut single-sided V-shaped grooves on the third sealing plate 3 and the fourth sealing plate 4 respectively and polish them to make them smooth;
[0036] Step 4: Calibration and sandblasting: First, all sub-parts of the ram are leveled and straightened in sequence through a straightening machine, and then the surfaces of all sub-parts of the ram are sandblasted;
[0037] Step 5, welding: After the first sealing plate 1, the second sealing plate 2, the fourth sealing plate 4, the first rib plate 5, the second rib plate 6, the third rib plate 7 and the end cover sealing plate 8 are positioned by spot welding according to the design size requirements, the two main welds of the first sealing plate 1 and the fourth sealing plate 4, the second sealing plate 2 and the fourth sealing plate 4 are welded continuously in multiple layers and multiple passes by using CO2 shielded welding. In order to prevent excessive thermal deformation during welding, a low current, multi-layer and multi-pass symmetrical synchronous welding method should be adopted. Then, the first rib plate 5, the second rib plate 6, the third rib plate 7 and the end cover sealing plate 8 are welded in turn. After the third sealing plate 3 is sealed and spot welded in position, the remaining welds are welded continuously in the above manner. Finally, the blank of the ram welded part is formed.
[0038] Step 6: Correction: Check the size, flatness and verticality of the ram blank. Straighten and correct the parts where the shape and position tolerances exceed the standard by fire attack;
[0039] Step 7: Stress relief annealing and flaw detection: In order to eliminate the welding internal stress of the ram blank, the ram blank should be subjected to aging treatment, and the internal stress of the weld should be eliminated by stress relief annealing; after the aging treatment of the ram blank, in order to detect the weld quality of the main weld of the appearance, each external weld of the ram blank should be subjected to non-destructive flaw detection, and the identification should be carried out by combining magnetic particle testing (MT) and ultrasonic testing (UT);
[0040] Step 8, rough machining and secondary stress relief annealing: firstly, the four side faces and two end faces of the ram blank are rough machined with a machining allowance of 4-6 mm to obtain a ram semi-finished product; in order to further eliminate the internal stress of the workpiece remaining from welding and machining of the ram semi-finished product, a second stress relief annealing aging treatment is performed on the ram semi-finished product; wherein the machining allowance is preferably 5 mm;
[0041] Step 9, semi-finishing and high-frequency quenching: first, semi-finishing the four side faces, two end faces and internal rib plate holes of the semi-finished ram is processed, and a processing allowance of 0.15-0.25mm is left; in order to improve the wear resistance and service life of the four side faces (guide rail surfaces) of the semi-finished ram, it is necessary to perform high-frequency quenching on these four side faces (guide rail surfaces); wherein, the processing allowance is preferably 0.2mm; in addition, high-frequency quenching is limited to the use of this quenching method in materials such as 35 steel or other medium-carbon alloy steels;
[0042] Step 10, tempering, sandblasting and painting: firstly, the semi-finished ram is subjected to low-temperature tempering aging treatment, then the semi-finished ram is subjected to surface sandblasting treatment, and the non-machined surface of the semi-finished ram is subjected to surface painting treatment to achieve the purpose of rust prevention; in addition, when the ram is designed to be installed with a linear guide rail, high-frequency quenching and tempering can be omitted;
[0043] Step 11, grinding and guide rail straightness inspection: In order to obtain high-precision form and position tolerances, that is, the straightness, flatness, parallelism of the four sides (guide rail surfaces) of the ram, and the perpendicularity between the two end surfaces, as well as the surface roughness of all planes, the four sides and two end surfaces of the ram semi-finished parts are ground and cut on a high-precision guide rail grinder, and then the four sides and two end surfaces of the ram semi-finished parts are inspected and confirmed for form and position tolerance accuracy by a three-coordinate measuring instrument or other high-precision testing equipment of the same level;
[0044] Step 12, finishing of drilling and rib plate holes and final acceptance: First, all holes on the semi-finished ram parts are finished by CNC machine tools, and then all dimensional tolerances and geometric tolerances of the finished ram parts are confirmed and accepted according to the processing drawings of the ram.
[0045] Among them, in step five, the first rib plate 5, the second rib plate 6 and the third rib plate 7 are spot welded to the fourth sealing plate 4 in sequence, and then the first sealing plate 1 and the second sealing plate 2 are spot welded to the fourth sealing plate 4, and then the first rib plate 5, the second rib plate 6 and the third rib plate 7 are respectively connected to the first sealing plate 1 and the second sealing plate 2 by spot welding, and then the first sealing plate 1, the second sealing plate 2 and the fourth sealing plate 4 are respectively connected to the end cover sealing plate 8 by spot welding.
[0046] The manufacturing method of the CNC machine tool slide of the present invention has the following advantages compared with the traditional casting slide: 1) the slide is not prone to casting defects such as sand holes, air holes, slag holes, shrinkage, cracks, etc.; 2) the slide has strong rigidity and high strength; 3) the slide has a short manufacturing cycle, light weight, relatively simple production equipment and fast modification.
[0047] The preferred embodiments of the present invention disclosed above are only used to help illustrate the present invention. The preferred embodiments do not describe all the details in detail, nor do they limit the invention to the specific implementation methods described. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the present invention, so that those skilled in the art can understand and use the present invention well. The present invention is limited only by the claims and their full scope and equivalents.
Claims
1. A method for manufacturing a ram of a CNC machine tool, characterized in that: The steps include: Step 1: Material selection: Select one of No. 35 steel plate, Q235B steel plate and Q355B steel plate as the base material; Step 2, cutting and blanking: selecting appropriate cutting equipment according to the thickness of the selected substrate, and using the cutting equipment to cut the substrate into sub-parts of the ram, the sub-parts of the ram including a first sealing plate (1), a second sealing plate (2), a third sealing plate (3), a fourth sealing plate (4), a first rib plate (5), a second rib plate (6), a third rib plate (7) and an end cover sealing plate (8); Step 3: Beveling: Cut a single-sided V-shaped bevel on the third sealing plate (3) and the fourth sealing plate (4) respectively and polish them to make them smooth; Step 4: Calibration and sandblasting: First, all sub-parts of the ram are leveled and straightened in sequence through a straightening machine, and then the surfaces of all sub-parts of the ram are sandblasted; Step 5, welding: After the first sealing plate (1), the second sealing plate (2), the fourth sealing plate (4), the first rib plate (5), the second rib plate (6), the third rib plate (7) and the end cover sealing plate (8) are positioned by spot welding according to the design size requirements, the two main welds of the first sealing plate (1) and the fourth sealing plate (4), the second sealing plate (2) and the fourth sealing plate (4) are welded in multiple layers and multiple passes by using CO2 shielded welding, and then the first rib plate (5), the second rib plate (6), the third rib plate (7) and the end cover sealing plate (8) are welded in turn, and then the third sealing plate (3) is sealed and spot welded to position, and then the remaining welds are continuously welded in the above manner, and finally the ram welded blank is formed; Step 6: Correction: Check the size, flatness and verticality of the ram blank. Straighten and correct the parts where the shape and position tolerances exceed the standard by fire attack; Step 7: Stress relief annealing and flaw detection: First, stress relief annealing is used to eliminate the internal stress of the weld of the ram blank, and then non-destructive flaw detection is performed on each external weld of the ram blank by combining magnetic particle flaw detection and ultrasonic flaw detection; Step 8, rough machining and secondary stress relief annealing: firstly, the four side faces and two end faces of the ram blank are rough machined with a machining allowance of 4-6 mm to obtain a ram semi-finished product, and then the ram semi-finished product is subjected to a second stress relief annealing aging treatment; Step 9, semi-finishing and high-frequency quenching: firstly, semi-finishing the four sides, two end faces and internal rib plate holes of the semi-finished ram is processed, and a processing allowance of 0.15-0.25mm is left, and then the four sides of the semi-finished ram are processed by high-frequency quenching; Step 10, tempering, sandblasting and painting: firstly, the semi-finished ram is subjected to low-temperature tempering aging treatment, then the surface of the semi-finished ram is subjected to sandblasting treatment, and the non-machined surface of the semi-finished ram is subjected to surface painting treatment; Step 11: Grinding and guide rail straightness inspection: First, grind and cut the four side faces and two end faces of the semi-finished ram part on a high-precision guide rail grinder, and then use high-precision testing equipment to test and confirm the shape and position tolerance accuracy of the four side faces and two end faces of the semi-finished ram part; Step 12, finishing of drilling and rib plate holes and final acceptance: First, all holes on the semi-finished ram parts are finished by CNC machine tools, and then all dimensional tolerances and geometric tolerances of the finished ram parts are confirmed and accepted according to the processing drawings of the ram.
2. The method for manufacturing a ram of a CNC machine tool according to claim 1, characterized in that: In the step five, the first rib plate (5), the second rib plate (6) and the third rib plate (7) are first spot welded to the fourth sealing plate (4) in sequence, and then the first sealing plate (1) and the second sealing plate (2) are spot welded to the fourth sealing plate (4), and then the first rib plate (5), the second rib plate (6) and the third rib plate (7) are respectively connected to the first sealing plate (1) and the second sealing plate (2) by spot welding, and then the first sealing plate (1), the second sealing plate (2) and the fourth sealing plate (4) are respectively connected to the end cover sealing plate (8) by spot welding.
3. The method for manufacturing a ram of a CNC machine tool according to claim 1 or 2, characterized in that: In the step eight, the machining allowance is 5 mm.
4. The method for manufacturing a ram of a CNC machine tool according to claim 3, characterized in that: In the step nine, the machining allowance is 0.2 mm.
Citation Information
Cited By
Controllable nuclear fusion coil box production device and method
CN121245502A