Electrostatic screening and cooling process for plastic granulation production
Through the electrostatic screening and cooling process, the problem of insufficient cooling of raw materials in plastic granulation production is solved, and the high-quality consistency and stability of the particles are achieved, equipment blockage and quality fluctuations are avoided, and different customer needs are met.
Patent Information
- Application Number
- CN202411119628.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-14
- Publication Date
- 2024-11-29
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Inadequate cooling of raw materials in plastic granulation production leads to defects such as gelatinization, adhesion, and pits on the surface of the particles, which affects the appearance and performance of the product. Inadequate cooling of particles is prone to stick to the equipment, causing clogging and wear, increasing maintenance costs, and not screened The particle quality is unstable.
The electrostatic screening cooling process is adopted, including raw material pretreatment, melt extrusion, electrostatic screening and impurity removal, cooling and curing and packaging storage. The impurities and special-shaped particles are separated by high-voltage electric field, the particle shape is cured by water cooling, and the particle shape is dried by infrared light and baked at low temperatures. Dry reduces internal stress.
It improves the quality consistency of plastic granulation, prevents equipment from being blocked and worn, ensures stable product appearance and performance, and realizes full curing and grading of particles to meet different customer needs.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of plastic granulation, in particular to electrostatic screening cooling in plastic granulation production. Background Art
[0002] Plastic granulation is to pass plastic materials through a specific machine, such as a plastic granulator, to crush, mix, heat, melt and other steps, and then cool them with cooling water or wind at appropriate temperature, pressure and rotation speed to finally make particles of a certain size and shape. These particles can be used for subsequent plastic product processing, such as injection molding, blow molding, etc.
[0003] In the production process of plastic granulation, insufficient cooling of raw materials will cause defects such as gelatinization, adhesion, and pits on the surface of the particles, which not only affects the appearance of the product but also reduces its performance and service life. Insufficiently cooled particles may be sticky and easily adhere to equipment or pipes, causing equipment blockage or wear, increasing the cost of maintenance and replacement of equipment. Failure to screen will lead to fluctuations and instability in product quality. Particles of different sizes may exhibit different performance in subsequent processing and use.
[0004] Therefore, we propose an electrostatic screening cooling process for plastic granulation production to solve the above problems. Summary of the invention
[0005] The purpose of the present invention is to provide an electrostatic screening and cooling process for plastic granulation production to solve the problem proposed in the above background technology that insufficient cooling of raw materials will cause defects such as gelatinization, adhesion, pits, etc. on the surface of particles, which not only affects the appearance of the product but also reduces its performance and service life. Particles that are not fully cooled may be sticky and easily adhere to equipment or pipelines, causing equipment blockage or wear, increasing the cost of maintenance and replacement of equipment, and failure to screen will lead to fluctuations and instability in product quality. Particles of different sizes may exhibit different performance in subsequent processing and use.
[0006] To achieve the above object, the present invention provides the following technical solutions:
[0007] An electrostatic screening cooling process for plastic granulation production comprises the following steps:
[0008] Raw material pretreatment: Raw material pretreatment includes crushing, cleaning and drying;
[0009] Crushing breaks large pieces of raw materials into small particles suitable for granulation. Washing removes impurities and contaminants on the surface of the raw materials, and drying ensures the moisture content of the raw materials.
[0010] Melt extrusion: The pretreated plastic raw material is heated to a molten state and extruded into continuous filaments or ribbons through an extruder.
[0011] Pellet forming: The extruded filaments or ribbons are cooled and cut to form initially formed plastic pellets.
[0012] Electrostatic screening and impurity removal: Use a high-voltage electric field to charge the particles so that they are separated by the electric charge in the electric field, separating impurities, irregular particles and particles that do not meet the requirements from qualified particles, thereby improving product quality and consistency.
[0013] Cooling and solidification: The plastic particles after electrostatic screening are cooled and solidified to fix the shape and structure of the particles.
[0014] Packaging and storage: After cooling and solidification, the plastic particles undergo subsequent drying, grading and packaging processing steps.
[0015] Furthermore, the raw material pretreatment utilizes high-speed rotating blades or hammers to break the raw materials into large pieces of plastic raw materials into small particles suitable for granulation, so as to better perform melt extrusion.
[0016] Furthermore, the cooling and curing cooling method adopts water cooling, which is cooled by water convection and conduction. The water temperature is 20°C, ensuring that the particles are fully cured without deformation or cracks.
[0017] Furthermore, the drying method in the packaging and storage adopts low-temperature drying to reduce the temperature gradient of the plastic during the drying process and reduce internal stress, thereby preventing the plastic parts from deforming and ensuring the stable quality of the plastic parts.
[0018] Furthermore, the raw material pretreatment cleaning method uses high-pressure water spraying to ensure that impurities and contaminants on the surface of the plastic raw materials are removed, so as to avoid impurities and contaminants being brought into the product during the melting process and affecting the appearance and performance of the product;
[0019] After cleaning, the plastic raw materials need to be rinsed and dehydrated to ensure that there is no residual cleaning agent and moisture on the surface.
[0020] During the raw material pretreatment drying process, infrared and other heating methods are used to evaporate the excess water in the raw materials. At the same time, stirring or turning equipment is used to ensure that the raw materials are fully heated during the drying process to ensure the uniformity and efficiency of drying.
[0021] After drying, the raw materials are screened to remove lumps and uneven particles.
[0022] Furthermore, electrostatic screening and impurity removal electrostatic screeners use high voltage electric fields to charge particles, so that the particles are separated by the electric charge in the electric field. Electrostatic screeners usually include multiple electrodes and collectors. By adjusting parameters such as electric field strength, electrode spacing and particle passing speed, particles with different characteristics can be effectively separated.
[0023] Compared with the prior art, the present invention has the following beneficial effects:
[0024] 1. The present invention achieves effective separation of particles with different characteristics by adjusting parameters such as electric field strength, electrode spacing and particle passing speed. Electrostatic screening can remove impurities, irregular particles and particles that do not meet the requirements, improve product quality and consistency, and ensure the consistency of plastic granulation after production is completed.
[0025] 2. The present invention requires cooling of plastic particles to solidify the shape and structure of the particles, immersing the particles in cooling water and cooling them by water convection and conduction. The cooling time is 10 minutes, and the water temperature is 20°C, ensuring that the particles are fully solidified without deformation or cracks. DETAILED DESCRIPTION
[0026] In the description of the present invention, unless otherwise specified, "plurality" means two or more.
[0027] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood by specific circumstances.
[0028] Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in the field without making any creative work shall fall within the scope of protection of the present invention.
[0029] Example 1
[0030] An electrostatic screening cooling process for plastic granulation production of the present invention comprises the following steps:
[0031] 1. Raw material pretreatment: Before plastic granulation production, it is first necessary to select suitable plastic raw materials according to product requirements to ensure that the purity, color, melt index and other parameters of the raw materials meet the production requirements. Use high-speed rotating blades or hammers to break the raw materials into large pieces of plastic raw materials into small particles suitable for granulation, so as to better melt extrusion. The raw material cleaning method adopts high-pressure water spray to ensure the removal of impurities and contaminants on the surface of the plastic raw materials, and avoid impurities and contaminants being brought into the product during the melting process and affecting the appearance and performance of the product. After cleaning, the raw materials are heated by infrared and other methods to evaporate the excess water in the raw materials. At the same time, stirring or flipping equipment will be used to make the raw materials fully heated during the drying process to ensure the uniformity and efficiency of drying and the quality of the raw materials.
[0032] 2. Melt extrusion: Heat the pretreated plastic raw material to a molten state and extrude it into continuous filaments or ribbons through an extruder. Adjust parameters such as melt temperature, extrusion speed and mold shape according to the characteristics of the raw material and product requirements to ensure the fluidity of the melt and the extrusion effect. The extruded filaments or ribbons are cooled and cut.
[0033] 3. The plastic particles that have undergone preliminary forming enter the electrostatic screening stage. The electrostatic screener uses a high-voltage electric field to charge the particles, so that the particles are separated by the electric charge in the electric field. The electrostatic screener usually includes multiple electrodes and collectors. By adjusting parameters such as the electric field strength, the electrode spacing and the particle passing speed, the particles with different characteristics can be effectively separated. Electrostatic screening can remove impurities, irregular particles and particles that do not meet the requirements, and improve product quality and consistency. The plastic particles after electrostatic screening need to be cooled to solidify the shape and structure of the particles. The particles are immersed in cooling water and cooled by the convection and conduction of water. The cooling time is 10 minutes, and the water flow temperature is 20°C to ensure that the particles are fully solidified without deformation or cracking.
[0034] 4. After cooling, the plastic pellets can be further processed, such as drying, grading and packaging. The drying process can remove moisture from the surface of the pellets to prevent the pellets from sticking or deteriorating during storage and transportation. Grading is based on the characteristics of the pellets, such as particle size, color and appearance, to meet the needs of different customers. Finally, the qualified plastic pellets are packaged for storage and transportation.
[0035] It will be apparent to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above and that the present invention can be implemented in other specific forms without departing from the spirit or essential features of the present invention. Therefore, the embodiments should be considered exemplary and non-restrictive in all respects, and the scope of the present invention is defined by the appended claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims be included in the present invention.
[0036] In addition, it should be understood that although the present specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.
Claims
1. An electrostatic screening cooling process for plastic granulation production, comprising the following steps: (1) Raw material pretreatment: Raw material pretreatment includes crushing, cleaning and drying; Crushing breaks large pieces of raw materials into small particles suitable for granulation. Washing removes impurities and contaminants on the surface of the raw materials, and drying ensures the moisture content of the raw materials. (2) Melt extrusion: The pretreated plastic raw material is heated to a molten state and extruded into continuous filaments or ribbons through an extruder. (3) Pellet forming: The extruded filaments or ribbons are cooled and cut to form initially formed plastic pellets. (4) Electrostatic screening and impurity removal: Use a high-voltage electric field to charge the particles so that they are separated by the electric charge in the electric field. Impurities, irregular particles, and particles that do not meet the requirements are separated from qualified particles, thereby improving product quality and consistency. (5) Cooling and solidification: The plastic particles after electrostatic screening are cooled and solidified to fix the shape and structure of the particles. (6) Packaging and storage: After cooling and solidification, the plastic particles undergo subsequent drying, grading and packaging processing steps.
2. The electrostatic screening cooling process for plastic granulation production according to claim 1, characterized in that: Raw material pretreatment (1) Use high-speed rotating blades or hammers to break the raw materials into small particles suitable for granulation, so as to better perform melt extrusion.
3. The electrostatic screening cooling process for plastic granulation production according to claim 1 is characterized in that: The cooling and solidification (5) is performed by water cooling, which is performed by convection and conduction of water. The water temperature is 20° C., which ensures that the particles are fully solidified without deformation or cracks.
4. The electrostatic screening cooling process for plastic granulation production according to claim 1, characterized in that: The drying method in the packaging and storage (6) adopts low-temperature drying to reduce the temperature gradient of the plastic during the drying process and reduce the internal stress, thereby preventing the plastic parts from deforming and ensuring the stable quality of the plastic parts.
5. The electrostatic screening cooling process for plastic granulation production according to claim 1, characterized in that: Raw material pretreatment (1) The cleaning method uses high-pressure water spray to ensure that impurities and contaminants on the surface of the plastic raw materials are removed to prevent impurities and contaminants from being brought into the product during the melting process and affecting the appearance and performance of the product; After cleaning, the plastic raw materials need to be rinsed and dehydrated to ensure that there is no residual cleaning agent and moisture on the surface. Raw material pretreatment (1) During the drying process, infrared and other heating methods are used to evaporate the excess water in the raw materials. At the same time, stirring or turning equipment is used to ensure that the raw materials are fully heated during the drying process to ensure the uniformity and efficiency of drying; After drying, the raw materials are screened to remove lumps and uneven particles.
6. The electrostatic screening cooling process for plastic granulation production according to claim 4, characterized in that: Electrostatic screening and impurity removal (4) Electrostatic screeners use high voltage electric fields to charge particles, so that the particles are separated by the electric charge in the electric field. Electrostatic screeners usually include multiple electrodes and collectors. By adjusting parameters such as electric field strength, electrode spacing and particle passing speed, effective separation of particles with different characteristics can be achieved.