Injection mold based on multiple cavities and injection molding method thereof
By designing injection molding liquid guide components and negative pressure systems in injection molds, the problem of injection molding liquid accumulation in the middle of the injection molding cavity is solved, ensuring that the injection molding liquid fills the cavity, and improving the quality of the workpiece and the injection molding stability.
Patent Information
- Application Number
- CN202411161820.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-23
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2044-08-23
AI Technical Summary
The injection molding liquid is prone to accumulate inside the injection molding cavity, resulting in insufficient injection molding liquid and affecting the quality of the workpiece.
Injection molding liquid guide components are designed, including end grooves, communication grooves, movable grooves, limiting plates and connecting rods. Negative pressure is generated through negative pressure pumps to prevent injection molding liquid from accumulating in the middle of the injection molding cavity, and to increase the mold by clamping and fixing the assembly. fixing effect and injection molding stability.
It effectively avoids the accumulation of injection molding liquid in the middle of the injection molding cavity, ensures that the injection molding liquid fills the cavity, improves the quality of the workpiece, and improves the injection molding stability and cutting efficiency.
Smart Images

Figure CN119036759A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of injection molds, and in particular relates to a multi-cavity injection mold and an injection molding method thereof. Background Art
[0002] The multi-cavity injection mold is an efficient and economical mold design solution. It can produce multiple products at the same time in one injection process, thereby significantly improving production efficiency and reducing costs. It is generally composed of an upper mold and a lower mold. The upper mold and the lower mold are equidistantly provided with mold grooves. The corresponding two mold grooves are combined to form an injection cavity. An injection pipe is provided at the top of the injection cavity. The injection liquid is introduced into the injection cavity through the injection pipe for injection molding. However, the following defects still exist:
[0003] Since the molding liquid is viscous, when the molding liquid enters the injection cavity, it tends to accumulate in the middle of the injection cavity, resulting in less molding liquid at both ends of the injection cavity, and thus the molding liquid cannot completely fill the injection cavity, thereby affecting the quality of the workpiece. Summary of the invention
[0004] In view of the above situation, in order to overcome the defects of the prior art, the present invention provides a multi-cavity injection mold and an injection molding method thereof, which effectively solves the problem that when the injection liquid enters the injection cavity, it is easy to accumulate in the middle of the injection cavity, resulting in less injection liquid at both ends of the injection cavity.
[0005] To achieve the above object, the present invention provides the following technical solution: a multi-cavity injection mold, comprising a lower mold and an upper mold, wherein the top of the lower mold is equidistantly provided with a lower mold cavity, the bottom of the upper mold is equidistantly provided with an upper mold cavity, the lower mold cavity corresponds to the upper mold cavity one by one, the lower mold cavity and the upper mold cavity are combined to form a complete injection cavity, and injection liquid guide components are installed on both sides of the length direction of the upper mold cavity;
[0006] The injection liquid guide assembly includes end grooves opened on the inner walls on both sides of the upper mold cavity, a connecting groove is opened on the side of the end groove away from the upper mold cavity, a movable groove is opened at one end of the connecting groove, the diameter of the end groove is larger than the diameter of the connecting groove, a baffle is movably installed inside the end groove, the outer wall of the baffle is in close contact with the inner wall of the end groove, a limit plate is movably installed inside the movable groove, a connecting rod is installed between the limit plate and the baffle, the diameter of the connecting rod is smaller than the inner diameter of the connecting groove, a first negative pressure groove is opened at the top of the connecting groove, a U-shaped negative pressure groove is opened inside the lower mold, the top of each first negative pressure groove is connected to the first negative pressure groove, a connecting pipe is installed on one side of the upper mold, the connecting pipe is connected to the U-shaped negative pressure groove, and a clamping fixing assembly is installed between the lower mold and the upper mold.
[0007] Preferably, a liquid inlet groove is opened inside the upper mold, and distribution grooves are opened equidistantly at the bottom of the liquid inlet groove, the distribution grooves correspond to the upper mold cavity one by one, and the distribution grooves penetrate into the interior of the upper mold cavity, and a liquid inlet pipe is fixedly installed on the top of the upper mold, and the liquid inlet pipe is connected to the liquid inlet groove.
[0008] Preferably, a first spring is fixedly mounted on the side of the limit plate away from the upper mold cavity, a magnetic block is mounted on the limit plate, an electromagnet is fixedly mounted on the inner wall of one end of the movable groove away from the upper mold cavity, and the electromagnet is externally connected to a power supply.
[0009] Preferably, the clamping and fixing assembly includes a first longitudinal groove equidistantly opened inside the upper mold, a second negative pressure groove is opened between the first longitudinal groove and the U-shaped negative pressure groove, the second negative pressure grooves correspond to each other in pairs and are symmetrically arranged between the two upper mold cavities, the first longitudinal groove passes through to the bottom end of the upper mold, and second longitudinal grooves are equidistantly opened inside the lower mold, the second longitudinal groove passes through to the top of the lower mold, the second longitudinal groove corresponds to the first longitudinal groove one by one, when the lower mold is combined with the upper mold, the first longitudinal groove is connected to the second longitudinal groove, and a blanking and ejection assembly is installed between the two second longitudinal grooves.
[0010] Preferably, a movable frame is movably installed inside the second longitudinal groove, a top tube is fixedly installed on the top of the movable frame, the outer wall of the top tube is in close contact with the outer wall of the second longitudinal groove, a piston plate is movably installed inside the top tube, the outer wall of the piston plate is in close contact with the inner wall of the top tube, a connecting hole is opened at the bottom end of the top tube, a second spring is fixedly installed at the bottom end of the movable frame, and the bottom end of the second spring is fixedly connected to the inner bottom wall of the second longitudinal groove.
[0011] Preferably, rod grooves are opened at equal angles on the top tube, a clamping rod is movably installed inside the rod groove, a connecting rod is hinged at one end of the clamping rod, one end of the connecting rod is hinged to the top wall of the piston plate, and clamping grooves are opened at equal angles on the inner wall of the first longitudinal groove, and the diameter of the clamping grooves is the same as the diameter of the clamping rod.
[0012] Preferably, the blanking and ejecting assembly includes a side groove opened between two adjacent second longitudinal grooves, and bottom grooves are equidistantly opened inside the lower mold, the bottom groove is located below the lower mold cavity, and the two ends of the bottom groove are respectively connected with the corresponding two side grooves, a transverse plate is movably installed inside the bottom groove, a push rod is installed at the top of the transverse plate, the push rod is movably installed inside the top through groove, the top through groove is opened on the bottom wall of the lower mold cavity, the outer wall of the push rod is in close contact with the inner wall of the top through groove, and when the transverse plate moves downward to contact the inner bottom wall of the bottom groove, the top wall of the push rod is flush with the inner bottom wall of the lower mold cavity.
[0013] Preferably, two connecting plates are symmetrically provided inside the side groove, and the two connecting plates are fixedly installed on both sides of the transverse plate. A first tooth plate is fixedly installed on the side of the connecting plate away from the transverse plate, and a second tooth plate is fixedly installed on the side of the movable frame close to the first tooth plate. A gear is meshingly connected between the second tooth plate and the first tooth plate, and the gear is rotatably installed inside the side groove.
[0014] Preferably, an injection molding method based on a multi-cavity injection mold is characterized in that the injection molding method is as follows:
[0015] S1. Assemble: Assemble the lower mold and the upper mold, energize the electromagnet to generate repulsive force on the magnetic block, so that the baffle enters the upper mold cavity, connect the connecting pipe to the negative pressure pump, turn on the negative pressure pump, and under the action of negative pressure, the top tube moves upward into the first longitudinal groove, and then the clamping rod is clamped into the clamping groove to clamp the lower mold and the upper mold;
[0016] S2, injection molding: injection liquid is introduced into each injection cavity from the liquid inlet pipe, the liquid inlet trough and each distribution trough. Under the action of negative pressure, negative pressure is generated at both ends of the injection cavity to prevent the injection liquid from accumulating in the middle of the injection cavity;
[0017] S3, unloading: After injection molding, turn off the negative pressure pump, so that the piston plate and the movable frame move back, and the transverse plate moves upward under the action of the gear, and the workpiece is ejected from the lower mold cavity for unloading.
[0018] Compared with the prior art, the present invention has the following beneficial effects:
[0019] 1) During operation, by setting the diameter of the connecting groove to be larger than the diameter of the connecting rod, when the baffle moves to the inside of the upper mold cavity, negative pressure suction can be generated at both ends of the injection cavity. When the injection molding liquid enters the injection molding cavity, it can generate force toward both ends for the injection molding liquid accumulated in the middle, which facilitates the injection molding liquid to fill the injection cavity and improve the quality of the workpiece. At the same time, when the injection molding liquid is about to be filled, pressure is generated on the baffle and it is pushed into the end groove, which is convenient for subsequent use;
[0020] 2) During operation, the first longitudinal groove is connected to the U-shaped negative pressure groove through the second negative pressure groove, and after the lower mold and the upper mold are combined, the first longitudinal groove is connected to the second longitudinal groove, and an upward force is generated on the piston plate under the action of negative pressure. When the piston plate moves upward, under the action of the clamping rod, the top cylinder is driven to move upward synchronously. When the clamping rod corresponds to the clamping groove, the piston plate moves upward relative to the top cylinder, pushing the clamping rod to clamp into the clamping groove, thereby improving the fixing effect of the lower mold and the upper mold and improving the injection molding stability;
[0021] 3) During operation, when the movable frame moves upward, the gear drives the transverse plate to move downward until the top wall of the ejector pin is flush with the inner bottom wall of the lower mold cavity, which is convenient for injection molding. After injection molding, the lower mold and the upper mold are disassembled and the negative pressure pump is turned off. The movable frame moves back downward to drive the transverse plate to move upward, so that the ejector pin enters the lower mold cavity to eject the workpiece, which is convenient for material unloading. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] The accompanying drawings are used to provide further understanding of the present invention and constitute a part of the specification. They are used to explain the present invention together with the embodiments of the present invention and do not constitute a limitation of the present invention.
[0023] In the attached picture:
[0024] Figure 1 It is a structural schematic diagram of a multi-cavity injection mold and an injection molding method thereof according to the present invention;
[0025] Figure 2 It is a schematic diagram of the internal structure of the upper mold and the lower mold of the present invention;
[0026] Figure 3 It is a schematic diagram of the internal structure of the upper mold of the present invention;
[0027] Figure 4 It is a schematic diagram of the structure of the injection liquid guide assembly of the present invention;
[0028] Figure 5 It is a schematic diagram of the structure of a U-shaped negative pressure tank of the present invention;
[0029] Figure 6 It is a schematic diagram of the enlarged structure of the first longitudinal groove A of the present invention;
[0030] Figure 7 It is a schematic diagram of the second longitudinal groove structure of the present invention;
[0031] Figure 8 It is a schematic diagram of the top tube structure of the present invention;
[0032] Fig. 9 For the present invention Figure 7 The enlarged structural diagram at A in the middle;
[0033] Fig.10 It is a schematic diagram of the transverse plate structure of the present invention.
[0034] In the figure: 1, lower mold; 2, upper mold; 3, lower mold cavity; 4, upper mold cavity; 5, injection liquid guide assembly; 501, end groove; 502, connecting groove; 503, movable groove; 504, limit plate; 505, connecting rod; 506, baffle; 507, first spring; 508, magnetic block; 509, electromagnet; 510, first negative pressure groove; 511, U-shaped negative pressure groove; 512, connecting pipe; 6, clamping fixing assembly; 601, first longitudinal groove; 602, second negative pressure groove ; 603, card slot; 604, second longitudinal slot; 605, movable frame; 606, top tube; 607, rod slot; 608, piston plate; 609, card rod; 610, connecting rod; 7, blanking and ejecting assembly; 701, side slot; 702, bottom slot; 703, transverse plate; 705, connecting plate; 706, first tooth plate; 707, second tooth plate; 708, gear; 709, top through slot; 710, ejector rod; 8, liquid inlet tank; 9, distribution tank; 10, liquid inlet pipe. DETAILED DESCRIPTION
[0035] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments; based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.
[0036] Embodiment 1, by Figure 1-10 The present invention relates to a multi-cavity injection mold, comprising a lower mold 1 and an upper mold 2, wherein a lower mold cavity 3 is equidistantly provided at the top of the lower mold 1, and an upper mold cavity 4 is equidistantly provided at the bottom of the upper mold 2, the lower mold cavity 3 corresponds to the upper mold cavity 4 one by one, and the lower mold cavity 3 and the upper mold cavity 4 are combined to form a complete injection cavity, and injection liquid guide components 5 are installed on both sides of the length direction of the upper mold cavity 4, a liquid inlet groove 8 is opened inside the upper mold 2, and distribution grooves 9 are equidistantly opened at the bottom end of the liquid inlet groove 8, and the distribution grooves 9 correspond to the upper mold cavity 4 one by one, and the distribution grooves 9 penetrate into the interior of the upper mold cavity 4, and a liquid inlet pipe 10 is fixedly installed on the top of the upper mold 2, and the liquid inlet pipe 10 is connected to the liquid inlet groove 8;
[0037] The injection liquid guide component 5 includes an end groove 501 formed on the inner wall of both sides of the upper mold cavity 4, a connecting groove 502 is formed on the side of the end groove 501 away from the upper mold cavity 4, a movable groove 503 is formed at one end of the connecting groove 502, the diameter of the end groove 501 is larger than the diameter of the connecting groove 502, a baffle 506 is movably installed inside the end groove 501, the outer wall of the baffle 506 is in close contact with the inner wall of the end groove 501, a limit plate 504 is movably installed inside the movable groove 503, a connecting rod 505 is installed between the limit plate 504 and the baffle 506, the diameter of the connecting rod 505 is smaller than the inner diameter of the connecting groove 502, a first negative pressure groove 510 is formed at the top of the connecting groove 502, a U-shaped negative pressure groove 511 is formed inside the lower mold 1, the top of each first negative pressure groove 510 is connected to the first negative pressure groove 510, and a connecting rod 504 is installed on one side of the upper mold 2. The connecting pipe 512 is connected to the U-shaped negative pressure groove 511, and a clamping fixing component 6 is installed between the lower mold 1 and the upper mold 2. A first spring 507 is fixedly installed on the side of the limit plate 504 away from the upper mold cavity 4, and a magnetic block 508 is installed on the limit plate 504. An electromagnet 509 is fixedly installed on the inner wall of the movable groove 503 away from the upper mold cavity 4. The electromagnet 509 is externally connected to a power supply. The diameter of the connecting groove 502 is larger than the diameter of the connecting rod 505. When the baffle 506 moves to the inside of the upper mold cavity 4, negative pressure suction can be generated at both ends of the injection cavity. When the injection molding liquid enters the injection molding cavity, a force can be generated toward the two ends for the injection molding liquid accumulated in the middle, which facilitates the injection molding liquid to fill the injection cavity and improve the quality of the workpiece. At the same time, when the injection molding liquid is about to be full, pressure is generated on the baffle 506 and it is pushed into the end groove 501 for subsequent use.
[0038] The clamping fixing assembly 6 includes a first longitudinal groove 601 equidistantly opened inside the upper mold 2, a second negative pressure groove 602 is opened between the first longitudinal groove 601 and the U-shaped negative pressure groove 511, the second negative pressure grooves 602 correspond to each other and are symmetrically arranged between the two upper mold cavities 4, the first longitudinal groove 601 penetrates to the bottom end of the upper mold 2, and the second longitudinal grooves 604 are equidistantly opened inside the lower mold 1, and the second longitudinal grooves 604 penetrate to the top of the lower mold 1, and the second longitudinal grooves 604 correspond to the first longitudinal grooves 601 one by one, when the lower mold 1 and the upper mold 2 After the assembly is completed, the first longitudinal groove 601 is connected to the second longitudinal groove 604, a material discharge and ejection assembly 7 is installed between the two second longitudinal grooves 604, a movable frame 605 is movably installed inside the second longitudinal groove 604, a top tube 606 is fixedly installed on the top of the movable frame 605, the outer wall of the top tube 606 is in close contact with the outer wall of the second longitudinal groove 604, a piston plate 608 is movably installed inside the top tube 606, the outer wall of the piston plate 608 is in close contact with the inner wall of the top tube 606, a connecting hole is opened at the bottom of the top tube 606, and the movable frame 60 5 is fixedly installed with a second spring at the bottom end, and the bottom end of the second spring is fixedly connected to the inner bottom wall of the second longitudinal groove 604, a rod groove 607 is opened at an equal angle on the top tube 606, and a clamping rod 609 is movably installed inside the rod groove 607, and a connecting rod 610 is hinged at one end of the clamping rod 609, and one end of the connecting rod 610 is hinged to the top wall of the piston plate 608, and a clamping groove 603 is opened at an equal angle on the inner wall of the first longitudinal groove 601, and the diameter of the clamping groove 603 is the same as the diameter of the clamping rod 609. The first longitudinal groove 601 is connected to the U-shaped negative pressure groove through the second negative pressure groove 602. The grooves 511 are connected, and after the lower mold 1 and the upper mold 2 are combined, the first longitudinal groove 601 is connected with the second longitudinal groove 604, and an upward force is generated on the piston plate 608 under the action of negative pressure. When the piston plate 608 moves upward, under the action of the clamping rod 609, the top tube 606 is driven to move upward synchronously. When the clamping rod 609 corresponds to the clamping groove 603, the piston plate 608 moves upward relative to the top tube 606, pushing the clamping rod 609 to be clamped into the clamping groove 603, thereby improving the fixing effect of the lower mold 1 and the upper mold 2 and improving the injection molding stability.
[0039] The blanking and ejecting assembly 7 includes a side groove 701 opened between two adjacent second longitudinal grooves 604, and a bottom groove 702 is equidistantly opened inside the lower mold 1. The bottom groove 702 is located below the lower mold cavity 3, and the two ends of the bottom groove 702 are respectively connected to the corresponding two side grooves 701. A transverse plate 703 is movably installed inside the bottom groove 702, and a push rod 710 is installed on the top of the transverse plate 703. The push rod 710 is movably installed inside the top through groove 709. The top through groove 709 is opened on the bottom wall of the lower mold cavity 3. The outer wall of the push rod 710 is in close contact with the inner wall of the top through groove 709. When the transverse plate 703 moves downward to contact the inner bottom wall of the bottom groove 702, the top wall of the push rod 710 is flush with the inner bottom wall of the lower mold cavity 3. Two connecting plates 705 are symmetrically arranged inside the side groove 701. The two connecting plates 705 are fixedly installed on both sides of the transverse plate 703. The first tooth plate 706 is fixedly installed on the side of the connecting plate 705 away from the transverse plate 703. The second tooth plate 707 is fixedly installed on the side of the movable frame 605 close to the first tooth plate 706. The second tooth plate 707 is meshed with the first tooth plate 706 and is connected with a gear 708. The gear 708 is rotatably installed inside the side groove 701. When the movable frame 605 moves upward, the transverse plate 703 is driven to move downward through the gear 708 until the top wall of the ejector rod 710 is flush with the inner bottom wall of the lower mold cavity 3, which is convenient for injection molding. After injection molding, the lower mold 1 and the upper mold 2 are disassembled and the negative pressure pump is turned off. The movable frame 605 moves back downward to drive the transverse plate 703 to move upward, so that the ejector rod 710 enters the lower mold cavity 3 to eject the workpiece, which is convenient for material unloading.
[0040] Working principle: When working, firstly, the lower mold 1 and the upper mold 2 are assembled and installed, so that the lower mold cavity 3 and the upper mold cavity 4 are assembled to form an injection cavity, so that multiple injection cavities are formed between the lower mold 1 and the upper mold 2, so as to perform injection molding of multiple workpieces at the same time;
[0041] The control electromagnet 509 is energized to generate a repulsive force on the magnetic block 508. Under the action of the repulsive force, the baffle 506 is pushed to leave the end groove 501 and enter the upper mold cavity 4, so that the first negative pressure groove 510 is connected to the injection cavity, and one end of the connecting pipe 512 is connected to the negative pressure pump, and the negative pressure pump is turned on to generate negative pressure, and the injection liquid is injected from the liquid inlet pipe 10. The injection liquid enters different pairs of injection cavities through the liquid inlet groove 8 and each distribution groove 9. When the injection liquid continuously enters the injection cavity, it accumulates in the middle of the injection cavity, and negative pressure exists at both ends of the length direction of the upper mold cavity 4. Under the action of negative pressure, the injection liquid entering the injection cavity flows toward the two ends, which is convenient for the injection liquid to fill the injection cavity and avoid the phenomenon of hollowing of the workpiece. When there is more injection liquid, pressure is generated on the baffle 506, which pushes the baffle 506 into the end groove 501 for sealing, which is convenient for subsequent use;
[0042] When the lower mold 1 is combined with the upper mold 2, the corresponding first longitudinal groove 601 and the second longitudinal groove 604 are connected, and the first longitudinal groove 601 is connected with the U-shaped negative pressure groove 511. Since the outer wall of the top tube 606 is in close contact with the inner wall of the second longitudinal groove 604, and the outer wall of the piston plate 608 is in close contact with the inner wall of the top tube 606, under the action of negative pressure, the piston plate 608 moves upward, and the end of the clamping rod 609 connected to the piston plate 608 through the connecting rod 610 contacts the inner wall of the second longitudinal groove 604, so that the piston plate 608 moves upward to drive the top tube 606 to move upward synchronously, until the top tube 606 enters the first longitudinal groove 601, and the clamping rod 609 corresponds to the clamping groove 603, the piston plate 608 moves upward relative to the top tube 606, and the clamping rod 609 is pushed by the connecting rod 610 to move outward and clamped into the clamping groove 603, so as to clamp the lower mold 1 and the upper mold 2, thereby improving the injection molding stability;
[0043] When the movable frame 605 moves upward, it drives the second tooth plate 707 to move upward, and drives the first tooth plate 706 to move downward through the gear 708. The first tooth plate 706 is fixedly connected to the transverse plate 703, thereby driving the transverse plate 703 to move downward until it contacts the inner bottom wall of the bottom groove 702, so that the top wall of the ejector pin 710 is flush with the inner bottom wall of the lower mold cavity 3. After injection molding, the negative pressure pump is turned off. At this time, the negative pressure disappears, and the piston plate 608 moves downward under the action of gravity, so that the clamping rod 609 is disengaged from the clamping groove 603. After the lower mold 1 is separated from the upper mold 2, the movable frame 605 moves back and drives the transverse plate 703 to move upward through the gear 708, so that the ejector pin 710 moves upward to eject the workpiece in the lower mold cavity 3, which is convenient for discharging.
[0044] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.
[0045] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A multi-cavity injection mold, comprising a lower mold (1) and an upper mold (2), Features: The top of the lower mold (1) is provided with a lower mold cavity (3) at an equal distance, and the bottom of the upper mold (2) is provided with an upper mold cavity (4) at an equal distance, the lower mold cavity (3) corresponds to the upper mold cavity (4) one by one, the lower mold cavity (3) and the upper mold cavity (4) are combined to form a complete injection molding cavity, and injection liquid guide components (5) are installed on both sides of the length direction of the upper mold cavity (4); The injection liquid guide assembly (5) comprises end grooves (501) formed on the inner walls of both sides of the upper mold cavity (4); a connecting groove (502) is formed on the side of the end groove (501) away from the upper mold cavity (4); a movable groove (503) is formed at one end of the connecting groove (502); the diameter of the end groove (501) is larger than the diameter of the connecting groove (502); a baffle (506) is movably installed inside the end groove (501); the outer wall of the baffle (506) is in close contact with the inner wall of the end groove (501); a limit plate (504) is movably installed inside the movable groove (503); the limit plate (504) A connecting rod (505) is installed between the baffle (506), the diameter of the connecting rod (505) is smaller than the inner diameter of the connecting groove (502), a first negative pressure groove (510) is provided at the top end of the connecting groove (502), a U-shaped negative pressure groove (511) is provided inside the lower mold (1), the top end of each first negative pressure groove (510) is connected to the first negative pressure groove (510), a connecting pipe (512) is installed on one side of the upper mold (2), the connecting pipe (512) is connected to the U-shaped negative pressure groove (511), and a clamping fixing component (6) is installed between the lower mold (1) and the upper mold (2).
2. A multi-cavity injection mold according to claim 1, Features: The upper mold (2) is provided with a liquid inlet groove (8) inside, and distribution grooves (9) are equidistantly provided at the bottom end of the liquid inlet groove (8), the distribution grooves (9) correspond to the upper mold cavity (4) one by one, and the distribution grooves (9) penetrate into the interior of the upper mold cavity (4), and a liquid inlet pipe (10) is fixedly installed at the top end of the upper mold (2), and the liquid inlet pipe (10) is connected to the liquid inlet groove (8).
3. A multi-cavity injection mold according to claim 1, Features: A first spring (507) is fixedly mounted on the side of the limit plate (504) away from the upper die cavity (4), a magnetic block (508) is mounted on the limit plate (504), and an electromagnet (509) is fixedly mounted on the inner wall of one end of the movable groove (503) away from the upper die cavity (4), and the electromagnet (509) is externally connected to a power source.
4. The multi-cavity injection mold according to claim 1, Features: The clamping and fixing assembly (6) comprises a first longitudinal groove (601) equidistantly provided inside the upper mold (2); a second negative pressure groove (602) is provided between the first longitudinal groove (601) and the U-shaped negative pressure groove (511); the second negative pressure grooves (602) correspond to each other in pairs and are symmetrically arranged between the two upper mold cavities (4); the first longitudinal groove (601) extends through the bottom end of the upper mold (2); second longitudinal grooves (604) are equidistantly provided inside the lower mold (1); the second longitudinal grooves (604) extend through the top of the lower mold (1); the second longitudinal grooves (604) correspond to the first longitudinal grooves (601) one by one; when the lower mold (1) and the upper mold (2) are assembled, the first longitudinal groove (601) is connected to the second longitudinal groove (604); a blanking and ejecting assembly (7) is installed between the two second longitudinal grooves (604).
5. A multi-cavity injection mold according to claim 4, Features: A movable frame (605) is movably installed inside the second longitudinal groove (604), a top tube (606) is fixedly installed on the top of the movable frame (605), the outer wall of the top tube (606) is in close contact with the outer wall of the second longitudinal groove (604), a piston plate (608) is movably installed inside the top tube (606), the outer wall of the piston plate (608) is in close contact with the inner wall of the top tube (606), a connecting hole is opened at the bottom end of the top tube (606), a second spring is fixedly installed at the bottom end of the movable frame (605), and the bottom end of the second spring is fixedly connected to the inner bottom wall of the second longitudinal groove (604).
6. A multi-cavity injection mold according to claim 5, Features: The top tube (606) is provided with a rod groove (607) at an equal angle, a clamping rod (609) is movably installed inside the rod groove (607), one end of the clamping rod (609) is hinged with a connecting rod (610), one end of the connecting rod (610) is hinged to the top wall of the piston plate (608), and a clamping groove (603) is provided on the inner wall of the first longitudinal groove (601) at an equal angle, and the diameter of the clamping groove (603) is the same as the diameter of the clamping rod (609).
7. A multi-cavity injection mold according to claim 4, Features: The blanking and ejecting assembly (7) comprises a side groove (701) opened between two adjacent second longitudinal grooves (604); bottom grooves (702) are opened equidistantly inside the lower mold (1); the bottom groove (702) is located below the lower mold cavity (3); and the two ends of the bottom groove (702) are respectively connected to the corresponding two side grooves (701); a transverse plate (703) is movably installed inside the bottom groove (702); a push rod (710) is installed at the top end of the transverse plate (703); the push rod (710) is movably installed inside the top through groove (709); the top through groove (709) is opened on the bottom wall of the lower mold cavity (3); the outer wall of the push rod (710) is in close contact with the inner wall of the top through groove (709); when the transverse plate (703) moves downward to contact the inner bottom wall of the bottom groove (702), the top wall of the push rod (710) is flush with the inner bottom wall of the lower mold cavity (3).
8. A multi-cavity injection mold according to claim 7, Features: Two connecting plates (705) are symmetrically arranged inside the side groove (701), and the two connecting plates (705) are fixedly installed on both sides of the transverse plate (703). A first tooth plate (706) is fixedly installed on the side of the connecting plate (705) away from the transverse plate (703), and a second tooth plate (707) is fixedly installed on the side of the movable frame (605) close to the first tooth plate (706). A gear (708) is meshed and connected between the second tooth plate (707) and the first tooth plate (706), and the gear (708) is rotatably installed inside the side groove (701).
9. An injection molding method based on a multi-cavity injection mold according to any one of claims 1 to 8, It is characterized in that The injection molding method is as follows: S1. Combination: The lower mold (1) is combined with the upper mold (2), and the electromagnet (509) is energized to generate a repulsive force on the magnetic block (508), so that the baffle (506) enters the interior of the upper mold cavity (4), and the connecting pipe (512) is connected to the negative pressure pump. The negative pressure pump is turned on. Under the action of negative pressure, the top tube (606) moves upward and enters the first longitudinal groove (601), and then the clamping rod (609) is clamped into the clamping groove (603), so as to clamp the lower mold (1) and the upper mold (2); S2, injection molding: injection liquid is introduced into each injection cavity from the liquid inlet pipe (10), the liquid inlet groove (8) and each distribution groove (9), and negative pressure is generated at both ends of the injection cavity under the action of negative pressure to prevent the injection liquid from accumulating in the middle of the injection cavity; S3, unloading: After injection molding, the negative pressure pump is turned off, so that the piston plate (608) and the movable frame (605) move back, and the transverse plate (703) moves upward under the action of the gear (708), and the workpiece is ejected from the lower mold cavity (3) for unloading.
Citation Information
Patent Citations
Injection mold and injection molding method for PET plastic bottle blank
CN118024513A
Injection mold capable of reducing bubbles
CN216760676U
Novel plastic floor positive and negative pressure forming device
CN220219438U
Liquid silica gel mold
CN221392068U