Automobile roof, preparation method thereof and automobile

By using the combination of inorganic materials and resin materials in the car roof, a porous structure cooling layer is formed, which solves the problem of poor heat dissipation effect of existing car roofs in high temperature environments, and achieves effective cooling effect with low cost and low complexity , improves the comfort and energy-saving performance of passenger cars.

CN119036985AInactive Publication Date: 2024-11-29BYD CO LTD

Patent Information

Application Number
CN202411519265.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-29
Publication Date
2024-11-29
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing car ceiling has poor heat dissipation and cooling effect in high temperature environments, and is expensive in materials and complex in structure, requiring additional controllers, which affects the application.

Method used

Using a cooling layer including inorganic materials and resin materials, the high reflectivity and thermal radiation properties of inorganic materials, combined with the stability and processing properties of resin materials, form a porous car roof to achieve passive cooling and heat dissipation, with a simple structure and low cost. , no additional energy input and control devices are required.

Benefits of technology

It achieves good solar light reflection and thermal radiation performance, reduces the internal temperature of the vehicle, improves passenger comfort, reduces the energy consumption of air conditioners, has low material costs and simple structure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119036985A_ABST
    Figure CN119036985A_ABST
Patent Text Reader

Abstract

The invention provides an automobile roof and a preparation method thereof and an automobile, and belongs to the technical field of automobile parts. The cooling layer is arranged on at least one side of the substrate layer; wherein the cooling layer is made of an inorganic material and a resin material. According to the automobile roof, the cooling and heat dissipation purposes are achieved in a passive cooling mode, the structure is simple, the material cost is low, and extra energy input and control devices are not needed. In addition, the cooling layer can reflect energy and radiate energy to the outside at the same time, and the cooling and heat dissipation effects of the automobile roof are further guaranteed.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of vehicle parts, and in particular to an automobile roof and a preparation method thereof, and a vehicle. Background Art

[0002] As an important part of the vehicle interior, the car roof plays an important role in the structure of the whole vehicle. When the ambient temperature is high, the air conditioner needs to be turned on continuously inside the vehicle to reduce the temperature in the passenger compartment, which greatly increases energy consumption. Especially with the rapid development of new energy vehicles, for energy-saving considerations, how to dissipate heat and cool down through the car roof has become one of the research directions in this field. In the related technology, there have been studies on using the car roof for heat dissipation and cooling, but there are defects such as expensive materials, complex structure, and the need to add additional controllers, which affect its application in vehicles. Summary of the invention

[0003] The embodiments of the present application provide a car roof and a preparation method thereof, and a vehicle. The car roof has a simple structure, low cost, and good cooling and heat dissipation effects.

[0004] In order to achieve the above object, according to a first aspect of the present application, a car roof is provided, comprising: basal layer; A cooling layer, the cooling layer being arranged on at least one side of the base layer; Among them, the material of the cooling layer includes inorganic material and resin material; the inorganic material is inorganic material.

[0005] Optionally, the inorganic material includes at least one of silicon dioxide, titanium dioxide, silicon carbide, aluminum oxide, barium sulfate, calcium sulfate, calcium oxide, calcium carbonate and zirconium oxide, and the resin material includes at least one of polyethylene, polypropylene, polyvinyl chloride, polymethyl methacrylate, poly(acrylonitrile-butadiene-styrene) and polyamide.

[0006] Optionally, the mass ratio of the inorganic material to the resin material is 1:2-1:18.

[0007] Optionally, the thickness of the cooling layer is 2 mm-6 mm.

[0008] Optionally, the particle size of the inorganic material is 0.1 mm-0.5 mm.

[0009] Optionally, the inorganic material is at least one of silicon dioxide and titanium dioxide; And / or, the resin material is at least one of polymethyl methacrylate and poly(acrylonitrile-butadiene-styrene).

[0010] Optionally, the inorganic material is titanium dioxide, and the resin material is polymethyl methacrylate.

[0011] Optionally, the material of the cooling layer further includes an additive; The auxiliary agent includes at least one of a binder, a colorant and a hydrophobic agent.

[0012] Optionally, the mass ratio of the auxiliary agent to the resin material is 1:6-1:18.

[0013] Optionally, the automobile roof further comprises a primer layer, and the primer layer is arranged between the base layer and the cooling layer.

[0014] Optionally, the automobile roof further comprises a functional layer, and the functional layer is arranged on a side of the cooling layer away from the base layer.

[0015] Optionally, the functional layer includes at least one of a hydrophobic layer, a dustproof layer, an oleophobic layer, a weather-resistant layer and a wear-resistant layer.

[0016] Optionally, the thickness of the functional layer is 1 mm-3 mm.

[0017] Optionally, the cooling layer is a porous structure; the porosity of the cooling layer is 1%-15%.

[0018] Optionally, the pores in the cooling layer have a pore diameter of 2 nm-50 nm.

[0019] Optionally, the base layer includes a substrate layer and a decorative layer which are stacked, and the cooling layer is arranged on a side of the substrate layer away from the decorative layer; Wherein, the material of the substrate layer includes at least one of polyethylene terephthalate fiber, polyurethane, polypropylene fiber and hemp fiber; And / or, the decorative layer includes at least one of a non-woven fabric layer, a knitted fabric layer, a foam layer, a felt layer, a cotton and linen fiber layer, a polyethylene terephthalate fiber layer and a polyvinyl chloride layer.

[0020] Optionally, the automobile roof is suitable for reflecting light with a wavelength of 200nm-3000nm, and radiating infrared light with a wavelength of 1μm-20μm to the outside.

[0021] Optionally, the reflectivity of the automobile roof to light with a wavelength of 200nm-3000nm is greater than 85%, and the emissivity of infrared light with a wavelength of 1μm-20μm is greater than 85%.

[0022] According to a second aspect of the present application, a method for preparing a car roof is also provided, which is used to prepare the above car roof, comprising: Provides a base layer; Mixing the inorganic material with the resin material to obtain a mixed material; The mixed material is coated on the base layer and cured to form a cooling layer.

[0023] Optionally, an inorganic material is mixed with a resin material, including: Disperse the inorganic material into the resin material and keep it at 30℃-120℃ for 2h-5h.

[0024] Optionally, coating the mixed material on the base layer comprises: The mixed material is coated on the base layer by at least one of spraying, printing, coating or integrated film-forming technology.

[0025] Optionally, curing comprises high temperature curing or UV curing.

[0026] According to a third aspect of the present application, a vehicle is also provided, comprising the above automobile roof, or a automobile roof made by the above automobile roof preparation method.

[0027] The automobile roof provided in the embodiment of the present application includes a base layer and a cooling layer arranged on at least one side of the base layer. The material of the cooling layer includes an inorganic material and a resin material. The inorganic material can provide good reflection performance and thermal radiation performance, and has high heat resistance and thermal stability. The resin material can fully and evenly disperse the inorganic material to ensure the structural stability of the cooling layer, and can further enhance the reflection performance and thermal radiation performance of the cooling layer. The automobile roof provided in the present application achieves the purpose of cooling and heat dissipation through a passive cooling method, has a simple structure, low material cost, and does not require additional energy input and control devices. In addition, the cooling layer can reflect energy while radiating the absorbed heat to the outside world, further ensuring the cooling and heat dissipation effects of the automobile roof.

[0028] Other features and advantages of the present application will be described in detail in the subsequent detailed description. BRIEF DESCRIPTION OF THE DRAWINGS In order to more clearly illustrate the technical solutions in the embodiments of the present application, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present application, and those skilled in the art can obtain other drawings based on these drawings without creative work.

[0029] In order to more completely understand the present application and its beneficial effects, the following description will be given in conjunction with the accompanying drawings, wherein the same figure numbers represent the same parts in the following description.

[0030] Figure 1 This is a schematic diagram of the structure of the car roof provided in the embodiment of the present application. Figure 1 ; Figure 2 This is a schematic diagram of the structure of the car roof provided in the embodiment of the present application. Figure 2 .

[0031] Description of reference numerals: 1. Base layer; 11. Base material layer; 12. Decorative layer; 2. Cooling layer; 3. Primer layer; 4. Functional layer. DETAILED DESCRIPTION

[0032] The technical solutions in the embodiments of the present application will be described clearly and completely below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, rather than all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the present application.

[0033] In a first aspect, an embodiment of the present application provides a car roof, comprising a base layer 1 and a cooling layer 2 disposed on at least one side of the base layer 1. The material of the cooling layer 2 comprises an inorganic material and a resin material.

[0034] The base layer 1 can serve as the basic structure of the car roof, and the cooling layer 2 is arranged on at least one side of the base layer 1, which can achieve passive cooling. Specifically, the cooling layer 2 includes inorganic materials and resin materials. The inorganic material can have high reflectivity to sunlight and good thermal radiation performance. On the one hand, it can reduce the absorption of heat by the car roof by reflecting sunlight back to the atmosphere. On the other hand, it can convert the absorbed heat into far-infrared radiation and release it into the surrounding environment. The resin material has good processing performance, can be combined with the dispersed inorganic material, and has good compatibility with the inorganic material, which is convenient for forming the cooling layer 2 of the film structure, and can improve the weather resistance and stability of the cooling layer 2. In addition, the resin material also has good reflectivity to sunlight and thermal radiation performance. The cooling and heat dissipation effects of the cooling layer 2 can be significantly improved through the mutual combination of inorganic materials and resin materials.

[0035] Among them, inorganic materials have high heat resistance and thermal stability, can maintain stable performance at high temperatures, and have good reflectivity to sunlight and good thermal radiation performance to ensure cooling effect. In addition, inorganic materials also have good mechanical properties. Mixing inorganic materials with resin materials can ensure cooling performance while also ensuring good mechanical properties.

[0036] In some embodiments, the inorganic material includes at least one of silicon dioxide, titanium dioxide, silicon carbide, aluminum oxide, barium sulfate, calcium sulfate, calcium oxide, calcium carbonate and zirconium oxide. Such materials have a high reflectivity to sunlight. When applied to the cooling layer 2, the sunlight can be effectively reflected back into the atmosphere to reduce the absorption of heat by the roof of the car, thereby reducing the transfer of heat to the passenger compartment. In addition, such materials also have good thermal radiation performance, that is, these materials have a high emissivity in the far-infrared band, and can radiate the absorbed heat into the air in the form of far-infrared rays to achieve the cooling effect. And these materials also have excellent weather resistance and high stability. The resin material includes at least one of polyethylene, polypropylene, polyvinyl chloride, polymethyl methacrylate, poly (acrylonitrile-butadiene-styrene) and polyamide. These resin materials have good processing performance, weather resistance and stability, can further improve the stability of the cooling layer 2, and these resin materials themselves also have the ability of far-infrared radiation, which helps to improve the heat dissipation effect of the cooling layer 2.

[0037] In some embodiments, the mass ratio of the inorganic material to the resin material is 1:2-1:18. By controlling the mass ratio of the inorganic material to the resin material within this range, it is possible to ensure that the inorganic material is fully dispersed in the resin material, so that the inorganic material and the resin material are well combined, improve the overall performance of the cooling layer 2, make full use of the high reflectivity and thermal radiation performance of the inorganic material, achieve the purpose of cooling and heat dissipation, and control the cost within a reasonable range, and ensure that the cooling layer 2 has good weather resistance and stability.

[0038] In some embodiments, the thickness of the cooling layer is 2 mm to 6 mm. Setting the thickness of the cooling layer 2 within this range can ensure the cooling effect and structural strength while reducing the material cost and the weight of the car roof.

[0039] In some embodiments, the particle size of the inorganic material is 0.1 mm-0.5 mm. By setting the particle size of the inorganic material to the above range, the compatibility between the inorganic material and the resin material can be improved, the inorganic material can be dispersed more evenly in the resin material, and the cooling and heat insulation performance of the cooling layer 2 can be improved.

[0040] In some embodiments, the inorganic material is at least one of silicon dioxide and titanium dioxide.

[0041] Among them, silicon dioxide has a high solar reflectivity, which can effectively reflect the heat of sunlight back into the atmosphere and reduce the absorption of heat. At the same time, silicon dioxide has good chemical stability, which can ensure stability during long-term use. Titanium dioxide can absorb, reflect and scatter sunlight, and it has good thermal radiation performance, which can convert the absorbed heat into far-infrared radiation and release it into the surrounding environment.

[0042] In some embodiments, the resin material is at least one of polymethyl methacrylate and poly(acrylonitrile-butadiene-styrene). Among them, polymethyl methacrylate (PMMA) has extremely high toughness, high transparency and heat resistance, and is easy to process and shape. Poly(acrylonitrile-butadiene-styrene) (PC / ABS) has both high toughness and high impact, and has good heat resistance, corrosion resistance and flame retardancy. At the same time, polymethyl methacrylate and poly(acrylonitrile-butadiene-styrene) also have high reflectivity and thermal radiation properties, which helps to further improve the cooling and heat dissipation performance of the cooling layer 2.

[0043] In some embodiments, the inorganic material is titanium dioxide and the resin material is polymethyl methacrylate. Titanium dioxide is a semiconductor material and can be controllably prepared into a porous material with uniform pore size. These material properties and structures make titanium dioxide the main material for radiative cooling. In addition, under the action of a dispersant, polymethyl methacrylate can better disperse titanium dioxide, making it easy to disperse titanium dioxide without affecting its function.

[0044] In some embodiments, the material of the cooling layer 2 further includes an auxiliary agent, wherein the auxiliary agent includes at least one of a binder, a colorant and a hydrophobic agent.

[0045] Specifically, a suitable auxiliary agent can be selected as needed. For example, when it is necessary to improve the bonding performance between the cooling layer 2 and the base layer 1, a bonding agent can be added.

[0046] It is understood that the binder can be selected from conventional reagents in the art, and its components are one or more of epoxy resin, polymethyl methacrylate and polyurethane. Exemplarily, the color of the colorant can be selected from white, off-white, light green, light yellow and gray, etc. The hydrophobic agent can be at least one of polytetrafluoroethylene, polyethylene, polyvinyl fluoride and polyisobutylene. The auxiliary agent can also be selected from an auxiliary agent with dustproof, oil-repellent, wear-resistant, self-cleaning and other functions.

[0047] In some embodiments, the mass ratio of the auxiliary agent to the resin material is 1:6-1:18. By setting the ratio of the auxiliary agent to the resin material within the above range, the function can be achieved while maintaining the performance of the resin material, without causing the original weather resistance and stability of the resin material to decrease, and the cost of the material is controlled within a reasonable range.

[0048] It is understood that the mass ratio of the auxiliary agent to the resin material refers to the mass ratio of the total mass of the auxiliary agent to the resin material. For example, when the auxiliary agent is only a binder, the mass ratio of the auxiliary agent to the resin material refers to the mass ratio of the binder to the resin material, and when the auxiliary agent includes both a binder and a colorant, the mass ratio of the auxiliary agent to the resin material refers to the mass ratio of the total mass of the binder and the colorant to the resin material.

[0049] In some embodiments, the automobile roof further includes a primer layer 3, which is disposed between the base layer 1 and the cooling layer 2. By arranging the primer layer 3 between the base layer 1 and the cooling layer 2, the bonding force between the cooling layer 2 and the base layer 1 can be improved, and the risk of the cooling layer 2 falling off can be reduced.

[0050] It is understandable that the material of the primer layer 3 can be selected from conventional primers in the art, and no specific limitation is made here.

[0051] In some embodiments, the automobile roof further includes a functional layer 4, which is disposed on the side of the cooling layer 2 away from the base layer 1. By disposing the functional layer 4 on the side of the cooling layer 2 away from the base layer 1, the cooling layer 2 can be protected while more functions can be realized, thereby improving the overall performance of the automobile roof.

[0052] Further, the functional layer 4 includes at least one of a hydrophobic layer, a dustproof layer, an oleophobic layer, a weather-resistant layer and a wear-resistant layer. Different functional layers 4 can be selected according to actual application requirements.

[0053] In some embodiments, the thickness of the functional layer 4 is 1 mm-3 mm. Setting the thickness of the functional layer 4 within this range can ensure that the functional layer 4 can play a specific role, maintain a certain structural strength, reduce the cost of material use, and reduce the weight of the car roof.

[0054] It is understood that the thickness of the functional layer 4 refers to the total thickness of the functional layer 4. For example, when the functional layer 4 includes only a hydrophobic layer, the thickness of the functional layer 4 refers to the thickness of the hydrophobic layer, and when the functional layer 4 includes both a hydrophobic layer and a dustproof layer, the thickness of the functional layer 4 is the total thickness of the hydrophobic layer and the dustproof layer.

[0055] In some embodiments, the cooling layer 2 is a porous structure. The porosity of the cooling layer 2 is 1%-15%. The cooling layer 2 with a porous structure increases the difficulty of heat conduction inside it while ensuring high reflective performance and thermal radiation performance, which can reduce the efficiency of thermal conduction and improve the thermal insulation performance of the cooling layer 2. Among them, setting the porosity of the cooling layer 2 to 1%-15% can not only ensure the thermal insulation performance, but also make the cooling layer 2 have good structural strength, and improve the weather resistance and stability of the cooling layer 2.

[0056] Furthermore, the porosity of the cooling layer 2 is preferably 3%-10%, so as to further ensure the high reflection performance and heat radiation performance of the cooling layer 2 and improve the heat insulation performance of the cooling layer 2.

[0057] The porosity of the cooling layer 2 can be measured by computer tomography, that is, by penetrating the material with X-rays to obtain a three-dimensional image of the interior of the cooling layer 2, and then calculating the porosity by image processing technology.

[0058] In some embodiments, the pores in the cooling layer 2 have a pore size of 2 nm to 50 nm. Setting the pore size in the cooling layer 2 within this range helps improve the thermal radiation performance of the cooling layer 2 and also helps achieve lightweighting of the cooling layer 2.

[0059] The pore size of the pores in the cooling layer 2 can be tested by nitrogen adsorption-desorption method.

[0060] It is understandable that the pores in the cooling layer 2 may be open pores and / or closed pores. The pores in the cooling layer 2 may come from the material itself, or may be formed during the preparation and dispersion process.

[0061] In some embodiments, the base layer 1 includes a substrate layer 11 and a decorative layer 12, and the cooling layer 2 is disposed on a side of the substrate layer 11 away from the decorative layer 12. The material of the substrate layer 11 includes at least one of polyethylene terephthalate fiber, polyurethane, polypropylene fiber and hemp fiber, and the decorative layer 12 includes at least one of a non-woven fabric layer, a knitted fabric layer, a foam layer, a felt layer, a cotton and linen fiber layer, a polyethylene terephthalate fiber layer and a polyvinyl chloride layer.

[0062] That is, the cooling layer 2 and the decorative layer 12 are respectively arranged on opposite sides of the substrate layer 11. The material of the substrate layer 11 includes at least one of polyethylene terephthalate fiber, polyurethane, polypropylene fiber and hemp fiber, which can make the substrate layer 11 have good mechanical properties, provide sufficient structural strength, and good stability, which helps to improve the bonding force of the cooling layer 2 on the substrate layer 11.

[0063] It can be understood that the decorative layer 12 is located inside the vehicle. By including at least one of a non-woven fabric layer, a knitted fabric layer, a foam layer, a felt layer, a cotton and linen fiber layer, a polyethylene terephthalate fiber layer and a polyvinyl chloride layer, the decorative layer 12 can improve the aesthetics while providing good protection.

[0064] In some embodiments, the automobile roof is suitable for reflecting light with a wavelength of 200nm-3000nm, and radiating infrared light with a wavelength of 1μm-20μm to the outside. The automobile roof provided in the embodiment of the present application utilizes the combination of inorganic materials and resin materials in the cooling layer 2, has good sunlight reflection performance, and good heat radiation performance, reduces the absorption of external heat, and can also radiate a small amount of absorbed heat to the external environment in the form of far-infrared light.

[0065] Furthermore, the car roof has a better reflection effect on optical fibers with a wavelength of 250nm-2500nm, and the wavelength radiated to the outside is preferably 2μm-16μm.

[0066] In some embodiments, the reflectivity of the automobile roof to light with a wavelength of 200nm-3000nm is greater than 85%, and the emissivity of infrared light with a wavelength of 1μm-20μm is greater than 85%. This can further improve the cooling and heat dissipation effects of the automobile roof and effectively reduce the temperature inside the car.

[0067] Furthermore, the reflectivity of the car roof to light with a wavelength of 200nm-3000nm is greater than 90%, and the emissivity of infrared light with a wavelength of 1μm-20μm is greater than 90%. By increasing the reflectivity of the car roof to the optical fiber and the emissivity of infrared light radiated to the outside world, the cooling effect of the car roof can be further improved.

[0068] In addition, in the automobile ceiling provided in the embodiment of the present application, by adopting a combination of inorganic materials and resin materials, the content of volatile organic compounds (VOC) can be controlled below 0.5%, which has a high safety while achieving a good cooling effect.

[0069] According to a second aspect of the present application, a method for preparing a car roof is also provided, which is used to prepare the above car roof, comprising: Providing a base layer 1; Mixing the inorganic material with the resin material to obtain a mixed material; The mixed material is coated on the base layer 1 and cured to form a cooling layer 2.

[0070] The method for preparing the automobile roof provided in the embodiment of the present application has a simple process and can directly form a cooling layer 2 on the base layer 1 by coating, without requiring major improvements to the structure of the original automobile roof and without adding additional circuit equipment and control devices.

[0071] In some embodiments, the inorganic material is mixed with the resin material, comprising: Disperse the inorganic material into the resin material and keep it at 30℃-120℃ for 2h-5h.

[0072] By maintaining the temperature at 30°C-120°C for 2h-5h, the dispersion performance of the inorganic material in the resin material can be improved, thereby improving the uniformity of the distribution of the inorganic material in the cooling layer 2 and ensuring the consistency of the cooling effect at different positions of the cooling layer 2.

[0073] Furthermore, after the inorganic material is dispersed in the resin material, it is preferably kept at 60° C.-80° C. for 2 h-3 h. This operation can ensure that the inorganic material is mixed evenly.

[0074] In some embodiments, coating the mixed material on the base layer 1 comprises: The mixed material is coated on the base layer 1 by at least one of spraying, printing, coating or integrated film-forming technology.

[0075] Furthermore, it is preferred to use a spraying or printing process. Among them, spraying has a higher construction efficiency, can ensure uniformity, and is convenient for automated operation. Printing has a higher precision and is convenient for large-scale production and application.

[0076] In some embodiments, curing includes high temperature curing or UV curing.

[0077] Exemplarily, high temperature curing includes: maintaining the curing temperature at 40° C.-80° C. for 5 min-60 min.

[0078] According to a third aspect of the present application, a vehicle is also provided, comprising the above automobile roof, or a automobile roof made by the above automobile roof preparation method.

[0079] The vehicle provided in the embodiment of the present application can reduce the use of energy-consuming devices such as air conditioners in the vehicle by applying the car roof described above, optimize the vehicle's energy-saving and emission-reduction indicators, and increase the vehicle's passenger comfort.

[0080] The present invention will be further described below in conjunction with specific examples. It should be understood that these examples are only used to illustrate the present invention and are not intended to limit the scope of the present invention. The experimental methods in the following examples without specifying specific conditions are usually based on the conditions recommended by the manufacturer.

[0081] It should be noted that, unless otherwise specified, the parts in the examples refer to parts by mass.

[0082] Example 1 Providing a base layer, wherein the base layer comprises a decorative layer and a base layer which are stacked, the decorative layer is made of polyethylene terephthalate (number average molecular weight is 20,000), and the base layer is made of non-woven fabric; Dispersing 5 parts of silicon dioxide and 5 parts of a white colorant into 90 parts of polyvinyl chloride (number average molecular weight of 60,000), maintaining the mixture at 65° C. for 3 h, to obtain a mixed material; Use a high-pressure air gun to blow the surface of the substrate layer away from the decorative layer to make the substrate layer free of dust, impurities, particles, water droplets and other foreign matter; keep the room temperature and humidity at 20% during the blowing process; Apply a primer layer on the surface of the substrate layer away from the decorative layer; Add the mixed material into the spray gun, and the working pressure of the spray gun should be lower than 4.5Kg / cm 2, the atomization angle is 25°, the working distance between the spray gun nozzle and the substrate layer is set to 30 cm, the running speed of the spray gun is 60 cm / s, and the mixed material is evenly sprayed on the surface of the substrate layer through cross-type spraying for multiple times, and the spraying thickness is 1 mm; Curing at 80°C for 30 min to form a cooling layer on the surface of the substrate layer; A hydrophobic functional layer is arranged on the side of the cooling layer away from the substrate layer, wherein the hydrophobic functional layer comprises polytetrafluoroethylene (number average molecular weight is 600000) and the thickness of the hydrophobic functional layer is 3 mm, thereby obtaining a car roof.

[0083] Example 2 Providing a base layer, wherein the base layer comprises a decorative layer and a base layer which are stacked, the decorative layer is made of polyethylene terephthalate (number average molecular weight is 20,000), and the base layer is made of non-woven fabric; 8 parts of aluminum oxide and 6 parts of polytetrafluoroethylene (number average molecular weight of 60,000) were dispersed in 80 parts of polypropylene (number average molecular weight of 400,000), and the mixture was kept at 65°C for 3 hours to obtain a mixed material; Use a high-pressure air gun to blow the surface of the substrate layer away from the decorative layer to make the substrate layer free of dust, impurities, particles, water droplets and other foreign matter; keep the room temperature and humidity at 20% during the blowing process; Add the mixed material into the spray gun, and the working pressure of the spray gun should be lower than 4.5Kg / cm 2 , the atomization angle is 25°, the working distance between the spray gun nozzle and the substrate layer is set to 30 cm, the running speed of the spray gun is 60 cm / s, and the mixed material is evenly sprayed on the surface of the substrate layer through cross-type spraying for multiple times, and the spraying thickness is 1 mm; The curing was carried out at a curing temperature of 80°C for 30 min to form a cooling layer on the surface of the substrate layer, thereby obtaining a car roof.

[0084] Example 3 Providing a base layer, wherein the base layer comprises a decorative layer and a base layer which are stacked, the decorative layer is made of polyethylene terephthalate (number average molecular weight is 20,000), and the base layer is made of non-woven fabric; Dispersing 40 parts of silicon carbide and 13 parts of epoxy resin (number average molecular weight of 500) into 80 parts of polymethyl methacrylate (number average molecular weight of 500000), maintaining the mixture at 65° C. for 3 hours, to obtain a mixed material; Use a high-pressure air gun to blow the surface of the substrate layer away from the decorative layer to make the substrate layer free of dust, impurities, particles, water droplets and other foreign matter; keep the room temperature and humidity at 20% during the blowing process; Apply a primer layer on the surface of the substrate layer away from the decorative layer; Add the mixed material into the spray gun, and the working pressure of the spray gun should be lower than 4.5Kg / cm 2 , the atomization angle is 25°-30°, the working distance between the nozzle of the spray gun and the substrate layer is set to 25-30cm, the running speed of the spray gun is 60cm / s-70cm / s, and the mixed material is evenly sprayed on the surface of the substrate layer through cross-type gun reciprocating spraying for multiple times, and the spraying thickness is 1mm; Curing at 80°C for 30 min to form a cooling layer on the surface of the substrate layer; A weather-resistant functional layer is arranged on the side of the cooling layer away from the substrate layer. The weather-resistant layer includes polyester fiber (number average molecular weight is 20000) and the thickness of the weather-resistant functional layer is 2 mm, thereby obtaining a car roof.

[0085] Example 4 Providing a base layer, wherein the base layer comprises a decorative layer and a base layer which are stacked, the decorative layer is made of polyethylene terephthalate (number average molecular weight is 20,000), and the base layer is made of non-woven fabric; 8 parts of titanium dioxide and 6 parts of yellow colorant are dispersed in 80 parts of polyvinyl chloride (number average molecular weight is 60000), and maintained at a temperature of 65°C for 3 hours to obtain a mixed material; in this embodiment, stirring is added during the mixing process to keep the mixture uniform.

[0086] Use a high-pressure air gun to blow the surface of the substrate layer away from the decorative layer to make the substrate layer free of dust, impurities, particles, water droplets and other foreign matter; keep the room temperature and humidity at 20% during the blowing process; Apply a primer layer on the surface of the substrate layer away from the decorative layer; Add the mixed material into the spray gun, and the working pressure of the spray gun should be lower than 4.5Kg / cm 2 , the atomization angle is 25°-30°, the working distance between the nozzle of the spray gun and the substrate layer is set to 25-30cm, the running speed of the spray gun is 60cm / s-70cm / s, and the mixed material is evenly sprayed on the surface of the substrate layer through cross-type gun reciprocating spraying for multiple times, and the spraying thickness is 1mm; Curing at 80°C for 30 min to form a cooling layer on the surface of the substrate layer; An oleophobic functional layer is arranged on the side of the cooling layer away from the substrate layer. The oleophobic functional layer includes nano-silicon dioxide and has a thickness of 2 mm to obtain a car roof.

[0087] Example 5 Providing a base layer, wherein the base layer comprises a decorative layer and a base layer which are stacked, the decorative layer is made of polyethylene terephthalate (number average molecular weight is 20,000), and the base layer is made of non-woven fabric; 8 parts of titanium dioxide and 6 parts of epoxy resin (number average molecular weight of 500) are dispersed into 80 parts of polymethyl methacrylate (number average molecular weight of 500000) material, and maintained at a temperature of 65°C for 3 hours to obtain a mixed material; in this embodiment, stirring is added during the mixing process to keep the mixture uniform.

[0088] Use a high-pressure air gun to blow the surface of the substrate layer away from the decorative layer to make the substrate layer free of dust, impurities, particles, water droplets and other foreign matter; keep the room temperature and humidity at 20% during the blowing process; Apply a primer layer on the surface of the substrate layer away from the decorative layer; Add the mixed material into the spray gun, and the working pressure of the spray gun should be lower than 4.5Kg / cm 2 , the atomization angle is 25°-30°, the working distance between the nozzle of the spray gun and the substrate layer is set to 25-30cm, the running speed of the spray gun is 60cm / s-70cm / s, and the mixed material is evenly sprayed on the surface of the substrate layer through cross-type gun reciprocating spraying for multiple times, and the spraying thickness is 1mm; Curing at 80°C for 30 min to form a cooling layer on the surface of the substrate layer; A hydrophobic functional layer is arranged on the side of the cooling layer away from the substrate layer. The hydrophobic functional layer includes polytetrafluoroethylene (number average molecular weight is 600000) and the thickness of the hydrophobic functional layer is 2 mm to obtain a car roof.

[0089] Example 6 Providing a base layer, wherein the base layer comprises a decorative layer and a base layer which are stacked, the decorative layer is made of polyethylene terephthalate (number average molecular weight is 20,000), and the base layer is made of non-woven fabric; 8 parts of titanium dioxide and 6 parts of yellow colorant are dispersed in 80 parts of polyvinyl chloride (number average molecular weight is 70000), and kept at a temperature of 65°C for 3 hours to obtain a mixed material; in this embodiment, stirring is added during the mixing process to keep the mixture uniform; Use a high-pressure air gun to blow the surface of the substrate layer away from the decorative layer to make the substrate layer free of dust, impurities, particles, water droplets and other foreign matter; keep the room temperature and humidity at 20% during the blowing process; Add the mixed material into the spray gun, and the working pressure of the spray gun should be lower than 4.5Kg / cm 2, the atomization angle is 25°-30°, the working distance between the nozzle of the spray gun and the substrate layer is set to 25-30cm, the running speed of the spray gun is 60cm / s-70cm / s, and the mixed material is evenly sprayed on the surface of the substrate layer through cross-type gun reciprocating spraying for multiple times, and the spraying thickness is 1mm; The curing temperature was 80°C for 30 min to form a cooling layer on the surface of the substrate layer.

[0090] Example 7 Providing a base layer, wherein the base layer comprises a decorative layer and a base layer which are stacked, the decorative layer is made of polyethylene terephthalate (number average molecular weight is 20,000), and the base layer is made of non-woven fabric; Disperse 1 part of titanium dioxide and 5 parts of epoxy resin (number average molecular weight of 500) into 80 parts of polymethyl methacrylate (number average molecular weight of 600000) material, keep the mixture at 65°C for 3 hours, and obtain a mixed material; in this embodiment, stirring is added during the mixing process to keep the mixture uniform.

[0091] Use a high-pressure air gun to blow the surface of the substrate layer away from the decorative layer to make the substrate layer free of dust, impurities, particles, water droplets and other foreign matter; keep the room temperature and humidity at 20% during the blowing process; Apply a primer layer on the surface of the substrate layer away from the decorative layer; Add the mixed material into the spray gun, and the working pressure of the spray gun should be lower than 4.5Kg / cm 2 , the atomization angle is 25°-30°, the working distance between the nozzle of the spray gun and the substrate layer is set to 25-30cm, the running speed of the spray gun is 60cm / s-70cm / s, and the mixed material is evenly sprayed on the surface of the substrate layer through cross-type gun reciprocating spraying for multiple times, and the spraying thickness is 1mm; Curing at 80°C for 30 min to form a cooling layer on the surface of the substrate layer; A hydrophobic functional layer is arranged on the side of the cooling layer away from the substrate layer, wherein the hydrophobic functional layer comprises polytetrafluoroethylene (number average molecular weight is 600000) and the thickness of the hydrophobic functional layer is 2 mm, thereby obtaining a car roof.

[0092] Example 8 Providing a base layer, wherein the base layer comprises a decorative layer and a base layer which are stacked, the decorative layer is made of polyethylene terephthalate (number average molecular weight is 20,000), and the base layer is made of non-woven fabric; 100 parts of titanium dioxide and 5 parts of epoxy resin (number average molecular weight of 500) are dispersed into 80 parts of polymethyl methacrylate (number average molecular weight of 600000) material, and maintained at a temperature of 65°C for 3 hours to obtain a mixed material; in this embodiment, stirring is added during the mixing process to keep the mixture uniform.

[0093] Use a high-pressure air gun to blow the surface of the substrate layer away from the decorative layer to make the substrate layer free of dust, impurities, particles, water droplets and other foreign matter; keep the room temperature and humidity at 20% during the blowing process; Apply a primer layer on the surface of the substrate layer away from the decorative layer; Add the mixed material into the spray gun, and the working pressure of the spray gun should be lower than 4.5Kg / cm 2 , the atomization angle is 25°-30°, the working distance between the nozzle of the spray gun and the substrate layer is set to 25-30cm, the running speed of the spray gun is 60cm / s-70cm / s, and the mixed material is evenly sprayed on the surface of the substrate layer through cross-type gun reciprocating spraying for multiple times, and the spraying thickness is 1mm; Curing at 80°C for 30 min to form a cooling layer on the surface of the substrate layer; A hydrophobic functional layer is arranged on the side of the cooling layer away from the substrate layer, wherein the hydrophobic functional layer comprises polytetrafluoroethylene (number average molecular weight is 600000) and the thickness of the hydrophobic functional layer is 2 mm, thereby obtaining a car roof.

[0094] Comparative Example 1 The base layer is directly used as the automobile roof, wherein the base layer includes a decorative layer and a base layer which are stacked, the decorative layer is made of, and the base layer is made of; A high-pressure air gun is used to blow the surface of the substrate layer away from the decorative layer to ensure that the substrate layer is free of dust, impurities, particles, water droplets and other foreign matter; the room temperature is maintained during the blowing process and the humidity is controlled at 20%.

[0095] The car ceilings in Examples 1-8 and Comparative Example 1 were respectively subjected to a solar reflectivity test, an infrared emissivity test, a pull-out adhesion test, a volatile organic compound (VOC) test, and a passenger car cooling effect test.

[0096] Among them, the sunlight reflectivity test is tested with reference to the methods specified in GB / T 2680-2021 and ASTM E1980-11 (2019). After testing, the reflectivity of the car roof to sunlight in Examples 1-8 is 91%, 91%, 92%, 96%, 97%, 10% and 35%, respectively, and the reflectivity of the car roof to sunlight in Comparative Example 1 is 8%.

[0097] The mid-infrared radiation rate test was carried out according to the method specified in GB / T 30127-2013. After testing, the mid-infrared radiation rates of the car ceilings in Examples 1-8 were 87%, 88%, 89%, 92%, 95%, 90%, 22% and 25% respectively, and the mid-infrared radiation rate of the car ceiling in Comparative Example 1 was 2%.

[0098] The pull adhesion test was conducted according to the method specified in ASTM D4541-17. After testing, the pull adhesion of the automobile roof in Example 1 was 60 kg / cm, which can meet the use requirements of the automobile roof. However, since there is no cooling layer on the automobile roof in Comparative Example 1, no relevant test was performed.

[0099] The volatile organic compound (VOC) test was conducted according to the method specified in GB / T 23986-2009 10.2. After testing, the test results of volatile organic compounds in the car ceiling in Examples 1-8 were 0.1%, 0.2%, 0.1%, 0.1%, 0.1%, ND, ND and 0.5%, respectively, which met the use requirements of the car ceiling. However, since there was no cooling layer in Comparative Example 1, no relevant test was conducted. Among them, ND means not detected.

[0100] The method for testing the cooling effect of a passenger car is as follows: after parking the vehicles equipped with the car roofs in Examples 1-8 and Comparative Example 1 for 60 minutes outdoors, monitor the temperature changes in the cabin, and record the temperature at different cabin positions and at different times in the same vehicle. After testing, in the vehicles equipped with the car roofs in Examples 1-8, when the ambient temperature is 42°C, the temperature in the cabin is reduced by 6°C, 8°C, 8°C, 10°C, 15°C, 8°C, 2°C and 3°C respectively relative to the ambient temperature. When the ambient temperature is between 30°C, the temperature in the cabin is reduced by 4°C, 4°C, 6°C, 10°C, 15°C, 6°C, 2°C and 3°C respectively relative to the ambient temperature. In the vehicle equipped with the car roof in Comparative Example 1, the temperature in the cabin is increased by about 5°C compared to the ambient temperature.

[0101] In summary, the car roof provided in the embodiments of the present application has good sunlight reflection performance and mid-infrared radiation performance. The materials used in the car roof meet the mechanical properties and volatile organic compound requirements of the materials used in the car, the overall material cost is low, and the effect is obvious. In addition, after the car roof is applied to the vehicle, it has a significant cooling effect on the cabin, which can improve the comfort of the passenger environment of the passenger car. Among them, the thermal insulation and cooling performance of the car roof in Examples 1-6 is better than that in Examples 7-8, mainly because a more reasonable ratio of inorganic materials, additives and resin materials is used in Examples 1-6, thereby having better sunlight reflectivity and mid-infrared radiation rate, and improving the cooling and heat insulation effect.

[0102] In the description of this application, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more features. In the description of this application, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.

[0103] In the above embodiments, the description of each embodiment has its own emphasis. For parts that are not described in detail in a certain embodiment, reference can be made to the relevant descriptions of other embodiments.

[0104] The embodiments, implementation methods and related technical features of the present application can be combined and replaced with each other without conflict.

[0105] The above are only preferred embodiments of the present application and do not constitute any form of limitation to the present application. However, any simple modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present application without departing from the content of the technical solution of the present application are still within the scope of the technical solution of the present application.

Claims

1. A car roof, It is characterized in that include: basal layer (1); A cooling layer (2), the cooling layer (2) being arranged on at least one side of the base layer (1); Wherein, the material of the temperature-reducing layer (2) comprises inorganic material and resin material.

2. The automobile roof according to claim 1, It is characterized in that The inorganic material includes at least one of silicon dioxide, titanium dioxide, silicon carbide, aluminum oxide, barium sulfate, calcium sulfate, calcium oxide, calcium carbonate and zirconium oxide; the resin material includes at least one of polyethylene, polypropylene, polyvinyl chloride, polymethyl methacrylate, poly(acrylonitrile-butadiene-styrene) and polyamide.

3. The automobile roof according to claim 1, It is characterized in that The mass ratio of the inorganic material to the resin material is 1:2-1:

18.

4. The automobile roof according to claim 1, It is characterized in that The thickness of the cooling layer (2) is 2 mm to 6 mm.

5. The automobile roof according to claim 1, It is characterized in that The particle size of the inorganic material is 0.1 mm-0.5 mm.

6. The automobile roof according to claim 1, It is characterized in that The inorganic material is at least one of silicon dioxide and titanium dioxide; And / or, the resin material is at least one of polymethyl methacrylate and poly(acrylonitrile-butadiene-styrene).

7. The automobile roof according to claim 6, It is characterized in that The inorganic material is titanium dioxide, and the resin material is polymethyl methacrylate.

8. The automobile roof according to claim 1, It is characterized in that The material of the temperature-reducing layer (2) further comprises an auxiliary agent; the auxiliary agent comprises at least one of a binder, a colorant and a hydrophobic agent.

9. The automobile roof according to claim 8, It is characterized in that The mass ratio of the auxiliary agent to the resin material is 1:6-1:

18.

10. The automobile roof according to claim 1, It is characterized in that The automobile roof further comprises a primer layer (3), wherein the primer layer (3) is arranged between the base layer (1) and the temperature-reducing layer (2).

11. The automobile roof according to claim 1, It is characterized in that The automobile roof further comprises a functional layer (4), wherein the functional layer (4) is arranged on a side of the cooling layer (2) facing away from the base layer (1).

12. The vehicle roof according to claim 11, It is characterized in that The functional layer (4) comprises at least one of a hydrophobic layer, a dustproof layer, an oleophobic layer, a weather-resistant layer and a wear-resistant layer.

13. The automobile roof according to claim 11, It is characterized in that The thickness of the functional layer (4) is 1 mm-3 mm.

14. The automobile roof according to claim 1, It is characterized in that The cooling layer (2) is a porous structure; the porosity of the cooling layer (2) is 1%-15%.

15. The vehicle roof according to claim 14, It is characterized in that The pores in the cooling layer (2) have a pore diameter of 2 nm to 50 nm.

16. The automobile roof according to claim 1, It is characterized in that The base layer (1) comprises a base material layer (11) and a decorative layer (12) which are stacked, and the temperature-reducing layer (2) is arranged on a side of the base material layer (11) away from the decorative layer (12); Wherein, the material of the substrate layer (11) includes at least one of polyethylene terephthalate fiber, polyurethane, polypropylene fiber and hemp fiber; And / or, the decorative layer (12) comprises at least one of a non-woven fabric layer, a knitted fabric layer, a foam layer, a felt layer, a cotton and linen fiber layer, a polyethylene terephthalate fiber layer and a polyvinyl chloride layer.

17. The automobile roof according to any one of claims 1 to 16, It is characterized in that The automobile roof is suitable for reflecting light with a wavelength of 200 nm-3000 nm, and radiating infrared light with a wavelength of 1 μm-20 μm to the outside.

18. The vehicle roof according to claim 17, It is characterized in that The reflectivity of the automobile roof to light with a wavelength of 200nm-3000nm is greater than 85%, and the emissivity of infrared light with a wavelength of 1μm-20μm radiated outwards is greater than 85%.

19. A method for preparing a car roof, for preparing the car roof as claimed in any one of claims 1 to 18, It is characterized in that include: Providing a base layer (1); Mixing the inorganic material with the resin material to obtain a mixed material; The mixed material is coated on the base layer (1) and cured to form a temperature-reducing layer (2).

20. The method for preparing the automobile roof according to claim 19, It is characterized in that The step of mixing the inorganic material with the resin material comprises: The inorganic material is dispersed in the resin material and maintained at 30° C.-120° C. for 2 h-5 h.

21. The method for preparing a car roof according to claim 19, It is characterized in that The step of coating the mixed material on the base layer (1) comprises: The mixed material is coated on the base layer (1) by at least one of spraying, printing, coating or integrated film-forming technology.

22. The method for preparing a car roof according to claim 19, It is characterized in that The curing includes high temperature curing or ultraviolet curing.

23. A vehicle, It is characterized in that It comprises the automobile roof as described in any one of claims 1 to 18, or the automobile roof made by the method for making the automobile roof as described in any one of claims 19 to 22.

Citation Information

Patent Citations

  • Sun-blocking multilayered sheet and hand-held parasol, tent, tarp, canopy, hat, and fixed parasol comprising said sun-blocking multilayered sheet

    CN105228821A

  • Radiation cooling material and preparation method and application thereof

    CN110103559A

  • Selective radiation refrigeration coating and composite material and application method thereof

    CN110317521A

  • Radiation cooling film based on synergistic reflection of micropores and inorganic particles and preparation method of radiation cooling film

    CN115610060A

  • Radiative cooling structures and systems

    US20170248381A1

Cited By

  • Method for preparing passive cooling film from recycled plastic bottles and passive cooling film