Elastic mixed material capable of shaping at body temperature and application of elastic mixed material
By using elastic mixed materials that are shaped at body temperature in earphones and earbuds, the problem that existing earbuds cannot maintain the fit shape at body temperature is solved, achieving rapid fit and efficient sound insulation, and the material can be repeated at different temperatures. , suitable for the production of personalized headphones and earplugs.
Patent Information
- Application Number
- CN202410934692.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-12
- Publication Date
- 2024-11-29
AI Technical Summary
The earplugs of existing earphones and hearing aids cannot maintain the fit shape at body temperature, and the customized in-ear products are long processing time and costly, and difficult to adjust, resulting in matching failure.
Using an elastic mixed material that is shaped at body temperature, including elastic phase materials and transformed phase materials, it is deformed and hardened at body temperature by preheating and cooling, maintaining the fit shape, and can restore the original shape when heated, suitable for Production of earphones and earplugs.
It achieves the effect of quickly and repeatedly fitting the inner ear contour at body temperature, improves the fit and comfort of the earbuds, enhances sound insulation, and reduces the risk of earbuds falling off. The material can be repeatedly shaped at different temperatures .
Smart Images

Figure CN119039797A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to an elastic material and application thereof, and in particular to an elastic mixed material capable of shaping at body temperature and application thereof. Background Art
[0002] Currently, headphones, hearing aids, earplugs, and other similar devices that enter the inner and outer auditory canals generally fall into two categories: one with a non-elastic earplug, and the other with a removable, highly elastic earplug. The second type of product, when inserted into the ear, adapts to the inner auditory canal through the elastic shape of the earplug. Because the earplug adapts to each individual's inner auditory canal through elastic deformation, it returns to its original shape after removal and cannot maintain the fit it once inserted into the ear. Currently, there are pure earplugs made of memory foam and earplugs that come with headphones on the market. However, memory foam is a sponge that slowly rebounds at room temperature / body temperature and cannot maintain a fixed fit after insertion.
[0003] Currently, most custom hearing aids are made by pre-obtaining a model of the client's inner ear, scanning it, and then using specialized processing methods (such as 3D printing) to achieve a custom fit. This process is not only time-consuming but also requires a variety of high-precision measurement and processing equipment, which is expensive. Furthermore, once manufactured, no adjustments can be made. Therefore, for custom in-ear products, any errors in the ear mold acquisition, measurement, and processing, or even the slightest change in the client's inner ear, will result in a mismatch. Summary of the Invention
[0004] Purpose of the invention: The purpose of the present invention is to provide an elastic hybrid material that can be quickly and repeatedly shaped to the contours of the inner ear at body temperature;
[0005] A second object of the present invention is to provide an application of the elastic hybrid material in an in-ear product.
[0006] Technical solution: The room-temperature plastic elastic material described in the present invention includes an elastic phase material and a transition phase material, and the volume ratio of the elastic phase material to the transition phase material is 55:45 to 70:30; the elastic phase material and the transition phase material are thermosetting or thermoplastic materials; when the elastic hybrid material is a non-porous material, the Shore hardness of the elastic phase material is less than 10A, and when the elastic hybrid material is a porous material, the Shore hardness of the elastic phase material is less than 40A; the melting point of the transition phase material is 45-100°C, and it hardens within 1 to 5 minutes at a body temperature of 30-38°C; the elastic phase material and the transition phase material are blended to form an elastic hybrid material. After the blending is completed, the material is preheated until the transition phase material melts and then cooled to body temperature. When the elastic hybrid material is a non-porous material, the Shore hardness of the elastic hybrid material is less than 10A, and when the elastic hybrid material is a porous material, the Shore hardness of the elastic hybrid material is less than 8C.
[0007] Among them, the principal tensile strain and principal compressive strain of the elastic hybrid material during body temperature shaping can reach more than 15% without the elastic hybrid material being damaged; when shaping at body temperature, this deformation is maintained by constraint, and the elastic hybrid material hardens within 1-5 minutes; after the elastic hybrid material hardens, the dimensional change in any direction before and after the constraint is removed is less than 2%.
[0008] Among them, the Shore hardness of the non-porous elastic hybrid material after complete hardening is 20A-50A; the Shore hardness of the porous elastic hybrid material after complete hardening is 11C-21C; after complete hardening, the dimensional change in any direction after 1 hour at 45°C is less than 0.5%.
[0009] Among them, the shape of the elastic mixed material after it is completely hardened can be restored to its original shape when heated to 45-100°C, and can be reshaped again at body temperature.
[0010] Wherein, the elastic phase material is a polymer elastomer, including thermosetting / thermoplastic, foaming / non-foaming rubber; the foaming / non-foaming rubber is preferably silicone or latex.
[0011] The elastic phase material is preferably silicone or thermoplastic rubber (TPR), and more preferably SBS, SEBS, TPV, TPU, EVA, NR, SBR, BR, CR, NBR, HNBR, EPDM, SR, FPM, IIR, TR, ACM, ANM, CPE, or PVC.
[0012] Wherein, the phase transition material is at least one of polycaprolactone, polybutylene styrene, and polyurethane.
[0013] Among them, it also includes thermochromic materials with a color transition temperature of 37-40°C, which are used to indicate whether the current temperature of the material is higher than body temperature; or, it includes thermochromic materials with a color transition temperature at the temperature required for the material to completely melt, which are used to increase the temperature of whether the material has reached complete melting.
[0014] The application of the above-mentioned elastic hybrid material that can be shaped at body temperature in in-ear products.
[0015] Wherein, the in-ear product includes earphones and earplugs; the earphones include an earphone body and an in-ear part, and the in-ear part and the earplugs are made of the elastic mixed material according to claim 1.
[0016] Wherein, the ear-in portion includes an earphone plug for inserting into the ear; the earphone plug is made of the above-mentioned elastic mixed material.
[0017] The earpiece described in the present invention includes earphone heads that mimic the shape of conventional earphones without elastic earphone plugs, as well as earphone heads with elastic earphone plugs. The earphone plugs have an inner hole for installation in the earphone head and insertion into the ear. The elastomer blend described in the present invention can be used to prepare complete earphone heads without earphone plugs, or to prepare earphone plugs that fit into earphone heads.
[0018] The earplugs described in the present invention are earplugs that do not have electronic components and can be directly inserted into the ear for use, such as noise reduction earplugs.
[0019] Beneficial effects: Compared with the prior art, the present invention achieves the following significant effects: after preheating, it is soft and easy to deform at body temperature, and after being inserted into the ear canal, it has a high fit with the human ear canal, and after hardening, the shape retention is high; after shaping, it can be inserted again, fits well, is highly comfortable, and is well sealed, which improves the sound insulation ability and is not easy to fall off; since the softening temperature of the elastic hybrid material is much higher than the body temperature, the personalized fitting earphones or earplugs maintain the shape after shaping at room temperature. After being heated to the softening temperature, since it can be shaped at body temperature, the elastic hybrid material can be reshaped and fit again. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 This is the stress-strain relationship of the mixed material under cyclic tensile loading at room temperature in Example 1;
[0021] Figure 2 This is the stress-strain relationship of the mixed material under cyclic tensile loading at room temperature in Example 2;
[0022] Figure 3 This is the stress-strain relationship of the mixed material under cyclic tensile loading at room temperature in Example 3;
[0023] Figure 4 This is a schematic structural diagram of Example 1 of the in-ear product of the present invention;
[0024] Figure 5 3D ear model used for body temperature shaping test and earphones shaped at body temperature;
[0025] Figure 6 The original shape of the earphone plug, the earphone plug removed from the earphone after being shaped by body temperature, and the comparison of the original shape and the shaped shape of the earphone plug obtained by 3D scanning;
[0026] Figure 7 Comparison of the 3D scanned earphones after shaping and the ear model used for shaping;
[0027] Figure 8 This is a schematic structural diagram of Example 2 of the in-ear product of the present invention;
[0028] Figure 9These are photos of the earphones with the structure of Example 2 at room temperature and 40°C;
[0029] Figure 10 Here are some photos of the headphones after wearing them;
[0030] Figure 11 FIG3 is a schematic structural diagram of Example 3 of the in-ear product of the present invention. DETAILED DESCRIPTION
[0031] The present invention is described in further detail below.
[0032] Example 1
[0033] The body temperature shaping elastic hybrid material was prepared by hot mixing TPR with a Shore hardness of 0A produced by Nanjing Licong New Materials Co., Ltd. and PCL model PCL 500C produced by Shenzhen Guanghua Weiye Co., Ltd. at a volume ratio of 70:30.
[0034] Figure 1 This is the stress-strain relationship derived from a cyclic tensile test at room temperature (20°C). The strain rate is 0.01 / s, and both strain and stress are engineering strain and engineering stress. The Shore hardness when shaped at body temperature is 5A, and the Shore hardness at room temperature is 30A.
[0035] Example 2
[0036] The two-component silicone E610 produced by Shenzhen Hongyejie Technology Co., Ltd. is used, which includes a matrix A and a cross-linker B. The matrix A and cross-linker B of the two-component silicone are pre-heat-mixed with PCL model PCL 500C produced by Shenzhen Guanghua Weiye Co., Ltd. in a volume ratio of 70:30. After the PCL is cooled to room temperature, the two parts are mixed again to form a body temperature shaping elastic hybrid material.
[0037] Figure 2 The stress-strain relationship is obtained from a cyclic tensile test at room temperature of about 20°C, where the strain rate is 0.01 / s and both the strain and stress are engineering strain and engineering stress.
[0038] Example 3
[0039] The two-component silicone E610 produced by Shenzhen Hongyejie Technology Co., Ltd. includes a matrix A and a crosslinker B. The matrix A and crosslinker B of the two-component silicone are pre-hot-mixed with TPU model TPU 2024A produced by Nanjing Hongxing New Material Technology Co., Ltd. in a volume ratio of 70:30. After the TPU is cooled to room temperature, the two parts are mixed again to form a body temperature shaping elastic hybrid material.
[0040] Figure 3The stress-strain relationship is obtained from a cyclic tensile test at room temperature of about 20°C, where the strain rate is 0.01 / s and both the strain and stress are engineering strain and engineering stress.
[0041] like Figure 4 As shown, an in-ear product comprises an earphone body 1 and an in-ear portion 2. The in-ear portion 2 is provided with an earphone plug 3. The earphone plug 3 is made of an elastic hybrid material that molds at body temperature and can conform to the contours of the inner ear at body temperature. The earphone plug has an inner hole, which is installed through the inner hole to the end of the earphone housing. The earphone plug is preheated to its softening temperature of 45-100°C. When it cools to near body temperature, it is installed on the earphone housing and inserted into the ear. After being molded at body temperature, the earphone is tailored to the individual's ear shape. After removal, the molded earphone plug retains its molded shape at room temperature. If re-molding is required, the earphone plug is removed and placed in hot water or heated to its softening temperature by other means, and the molding process can be repeated. The inner hole of the earphone plug can be of variable diameter to improve its grip on the corresponding part of the earphone and prevent excessive deformation of the earphone plug from obstructing the sound transmission part of the earphone.
[0042] Figure 5 Left: Earphone tip and earphone body before installation; Middle: Earphone after installation; Right: Earphone after shaping; Right: Earphone after shaping at body temperature; Ear mold used for test fit is also included. Figure 5 The upper part of the left picture is a 3D ear model used for shaping test at body temperature, the left side of the lower left picture is an earplug prepared by mixing soft silicone and PCL, and the right side of the lower left picture is a 3D printed earphone model; the material of the earphone plug is prepared according to Example 2.
[0043] Figure 6 To compare the original earphone plug and the shaped earphone plug, the corresponding Figure 5 The earphone plug is made of the material of Example 2.
[0044] Figure 7 Demonstrate the excellent fit between the earphone and the ear mold after shaping, corresponding Figure 5 The earphone plug is made of the material of Example 2.
[0045] like Figure 8As shown, an in-ear product includes an earphone body 4 and an in-ear portion 5 provided on the head of the earphone body. The in-ear portion 5 simulates the shape of the earphone head without an earphone plug in the prior art. The in-ear portion 5 is made of a body temperature shaping elastic hybrid material and is wrapped around the head of the earphone body 4. The thickness of the body temperature shaping elastic hybrid material is 0.1 to 4 mm. This layer of elastic hybrid material membrane can be disassembled and assembled by utilizing its elasticity, or assembled and unassembled after being preheated and softened. After preheating and softening, wait for it to cool to body temperature, insert it into the ear, and wait for it to harden to fit the earphone to the individual. After taking it out, the shaped in-ear portion maintains its shaped shape at normal room temperature. When it needs to be reshaped, it is heated again to its softening temperature and the aforementioned shaping process is repeated. The heating and softening temperature is 45 to 100°C.
[0046] Figure 9 The left picture is Figure 8 The photo of the earphones with the structure at room temperature shows that the cover layer made by mixing soft silicone and TPU is pink; Figure 9 The right picture is a photo of the earphone at 40℃. It can be seen that the cover layer made by mixing soft silicone and TPU is white. Figure 9 It can be seen that the color of the elastic hybrid material membrane changes at different temperatures.
[0047] Figure 10 This is a photo of wearing headphones after shaping, corresponding to Figure 9 headphones.
[0048] like Figure 11 As shown, an in-ear product is a pure body temperature shaping elastic earplug 6 made of a body temperature shaping elastic hybrid material with a support 7. The earplug 6 is made from the material of Example 2. The support 7 can be pre-installed into the earplug at room temperature and can be integral with the earplug and non-removable. The support can be removed, making it a pure unsupported earplug. Unlike a pure body temperature shaping elastic hybrid earplug with a support, the earplug does not require the step of attaching the support.
Claims
1. An elastic mixed material that can be shaped at body temperature, characterized in that: The invention comprises an elastic phase material and a transition phase material, wherein the volume ratio of the elastic phase material to the transition phase material is 55:45 to 70:30; the elastic phase material and the transition phase material are thermosetting or thermoplastic materials; when the elastic mixed material is a non-porous material, the Shore hardness of the elastic phase material is less than 10A, and when the elastic mixed material is a porous material, the Shore hardness of the elastic phase material is less than 40A; the melting point of the transition phase material is 45-100°C, and it hardens within 1 to 5 minutes at a body temperature of 30-38°C; the elastic phase material and the transition phase material are blended to form an elastic mixed material, and after the blending is completed, the elastic phase material is preheated until the transition phase material is melted, and then cooled to body temperature, when the elastic mixed material is a non-porous material, the Shore hardness of the elastic mixed material is less than 10A, and when the elastic mixed material is a porous material, the Shore hardness of the elastic mixed material is less than 8C.
2. The elastic hybrid material for shaping at body temperature according to claim 1, characterized in that: During body temperature shaping, the principal tensile strain and principal compressive strain of the elastic hybrid material can reach more than 15% without the elastic hybrid material being damaged; when shaping at body temperature, this deformation is maintained by constraints, and the elastic hybrid material hardens within 1-5 minutes; after the elastic hybrid material hardens, the dimensional change in any direction before and after the constraints are removed is less than 2%.
3. The elastic hybrid material for shaping at body temperature according to claim 2, characterized in that: The Shore hardness of the non-porous elastic hybrid material after full hardening is 20A-50A; the Shore hardness of the porous elastic hybrid material after full hardening is 11C-21C; after the elastic hybrid material is fully hardened, the dimensional change in any direction is less than 0.5% after 1 hour at 45°C.
4. The elastic hybrid material for shaping at body temperature according to claim 3, characterized in that: The shape of the elastic mixed material after it is completely hardened can be restored to its original shape when heated to 45-100°C and can be reshaped again at body temperature.
5. The elastic hybrid material for shaping at body temperature according to claim 1, characterized in that: The elastic phase material is a polymer elastomer, including thermosetting / thermoplastic, foaming / non-foaming rubber; silicone or thermoplastic rubber TPR.
6. The elastic hybrid material for shaping at body temperature according to claim 1, characterized in that: The transition phase material is at least one of polycaprolactone, polybutylene styrene or polyurethane.
7. The elastic hybrid material for shaping at body temperature according to claim 1, characterized in that: The elastic mixed material includes a temperature-sensitive color-changing material with a color transition temperature of 37-40°C, which is used to indicate whether the current temperature of the elastic mixed material is higher or lower than body temperature; the elastic mixed material also includes a temperature-sensitive color-changing material with a color transition temperature that is the temperature required for the material to be completely melted, which is used to indicate whether the material has reached the temperature for complete melting.
8. Use of the elastic hybrid material that can be shaped at body temperature as claimed in claim 1 in in-ear products.
9. The use according to claim 8, characterized in that: The in-ear product comprises an earphone and an earplug; the earphone comprises an earphone body and an in-ear part, and the in-ear part and the earplug are made of the elastic mixed material according to claim 1.
10. The use according to claim 9, characterized in that: The in-ear part comprises an earphone plug for inserting into the ear; the earphone plug is made of the elastic mixed material according to claim 1.