Thermal insulation material as well as preparation method and application thereof
By introducing nanotitanium dioxide-doped silica aerogel and UV-resistant modifiers into traditional exterior wall insulation coatings, materials with excellent thermal insulation and UV resistance are prepared, and the performance of traditional coatings is solved. The poor problem has achieved more efficient energy consumption reduction and durability improvement.
Patent Information
- Application Number
- CN202411292451.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-14
- Publication Date
- 2024-11-29
AI Technical Summary
Traditional exterior wall insulation and thermal insulation coating materials have poor thermal insulation performance and ultraviolet resistance, which is difficult to meet the dual requirements of modern buildings for thermal insulation performance and durability.
The preparation method of insulation materials is adopted, including the preparation of insulation through composite reaction and polymerization using nano-titanium dioxide doped silica aerogel, polydopamine modified aerogel, ultraviolet-resistant modifier and other components. Thermal insulation emulsion combines heavy calcium carbonate, talc powder and other ingredients to form a coating with excellent thermal insulation and ultraviolet resistance.
It significantly improves the thermal insulation effect of the building, reduces building energy consumption, has good UV resistance and stability, extends the service life of the coating, and is in line with the concept of green building.
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of thermal insulation, and in particular to a thermal insulation material and a preparation method and application thereof. Background Art
[0002] With the intensification of the energy crisis and the improvement of environmental awareness, the role of thermal insulation materials in energy conservation, emission reduction and environmental protection has become increasingly prominent. As one of the main parts of building energy consumption, the thermal insulation performance of the building's exterior wall has an important impact on the overall energy consumption of the building. Traditional thermal insulation materials, such as rock wool, glass wool, polyurethane foam, etc., although they have certain thermal insulation effects, have the problems of flammability, complex construction and high cost. Therefore, the use of exterior wall thermal insulation coating materials that are non-flammable, easy to construct and reasonably cost-effective has important practical significance and market prospects. However, traditional exterior wall thermal insulation coating materials often have the disadvantages of poor thermal insulation performance and UV resistance, and long-term exposure to sunlight causes accelerated aging, resulting in a significant decrease in the performance of the thermal insulation coating, and are easy to fall off, affecting the appearance, and it is difficult to meet the dual requirements of modern buildings for thermal insulation performance and durability. Summary of the invention
[0003] In order to overcome the above-mentioned technical problems, the purpose of the present invention is to provide a thermal insulation material and a preparation method and application thereof, which solves the problem that traditional exterior wall thermal insulation coating materials often have poor thermal insulation and UV resistance, and are difficult to meet the dual requirements of modern buildings for thermal insulation and durability. The purpose of the present invention can be achieved through the following technical solutions: A thermal insulation material comprises the following components in parts by weight: 60-70 parts of thermal insulation emulsion, 31-45 parts of heavy calcium carbonate, 12-24 parts of talc, 2.5-4.5 parts of wetting agent, 2-3 parts of dispersant, 1-3 parts of defoaming agent, 1-3 parts of film-forming aid, 0.3-0.5 parts of thickener and 25-50 parts of deionized water; Wherein, the thermal insulation emulsion is prepared by the following steps: Step s1: adding tetraethyl orthosilicate, anhydrous ethanol and deionized water into a three-necked flask equipped with a stirrer and a thermometer, stirring and reacting for 25-35 minutes at a temperature of 20-25°C and a stirring rate of 300-350r / min, then adjusting the pH to 2-3 with a hydrochloric acid solution, and then continuing to stir and react for 2-3 hours, then adding nano-titanium dioxide and continuing to stir and react for 5-10 minutes, then adjusting the pH to 7.5-8.5 with ammonia water, and then continuing to stir and react for 20-30 minutes, after the reaction is completed, the reaction product is allowed to stand for 2-3 hours, then heated to 50-55°C and allowed to stand for 3-5 hours, and then supercritically dried with carbon dioxide gas to obtain a composite aerogel; Step s2: adding the composite aerogel and deionized water to a three-necked flask equipped with a stirrer and a thermometer, ultrasonically dispersing for 20-30 minutes at an ultrasonic frequency of 35-45kHz, then stirring for reaction for 5-10 minutes at a temperature of 20-25°C and a stirring rate of 300-350r / min, then adding tris(hydroxymethyl)aminomethane hydrochloride and dopamine hydrochloride and continuing to stir for reaction for 4-5 hours, centrifuging the reaction product after the reaction is completed, washing the precipitate with distilled water for 2-3 times, and then placing it in a vacuum drying oven and drying it at a temperature of 50-55°C for 2-3 hours to obtain a modified aerogel; Step s3: Add 2,4-dihydroxybenzophenone, triethylamine and tetrahydrofuran to a three-necked flask equipped with a stirrer, a thermometer and a constant pressure dropping funnel, add chloroacetyl chloride solution dropwise while stirring at a temperature of 0-5°C and a stirring rate of 300-350r / min, and control the dropping rate to be 1-2 drops / s. After the dropwise addition is completed, continue to stir and react for 3-5h. After the reaction is completed, add the reaction product to ice water, then stand and separate, wash the organic phase with saturated brine for 2-3 times, then dry with anhydrous magnesium sulfate, then vacuum filter, and rotary evaporate the filtrate to remove the solvent to obtain a UV-resistant modifier; Step s4: add isophorone diisocyanate, polypropylene glycol, N-methylpyrrolidone and dibutyltin dilaurate to a three-necked flask equipped with an agitator, a thermometer and a nitrogen gas duct, introduce nitrogen protection, stir and react for 2-3 hours at a temperature of 85-90°C and a stirring rate of 300-350r / min, then cool to 50-60°C and add 1,4-butanediol and continue to stir and react for 1-1.5 hours, then add modified aerogel and UV-resistant modifier and continue to stir and react for 2-3 hours, after the reaction is completed, neutralize the reaction product with triethylamine for 30-50 minutes, and the neutralization degree is 100%, then add deionized water and continue to stir and react for 20-30 minutes, then rotary evaporate until the solid content is 25-30%, to obtain a thermal insulation emulsion. As a further solution of the present invention: the usage ratio of the tetraethyl orthosilicate, anhydrous ethanol, deionized water and nano titanium dioxide in step s1 is 10-12 g: 20-25 mL: 20-25 mL: 1.5-3.5 g. As a further solution of the present invention: the mass fraction of the hydrochloric acid solution in step s1 is 20-22%, and the mass fraction of the ammonia water is 25-27%. As a further solution of the present invention: the usage ratio of the composite aerogel, deionized water, tris(hydroxymethyl)aminomethane hydrochloride and dopamine hydrochloride in step s2 is 3g:60-70mL:0.1-0.12g:0.15-0.25g. As a further solution of the present invention: the usage ratio of the 2,4-dihydroxybenzophenone, triethylamine, tetrahydrofuran and chloroacetyl chloride solution in step s3 is 10 mmol: 11-13 mmol: 30-40 mL: 10-12 mL. As a further solution of the present invention: the chloroacetyl chloride solution in step s3 is a solution formed by dissolving chloroacetyl chloride in tetrahydrofuran at a ratio of 11-13 mmol:10 mL. As a further scheme of the present invention: the usage ratio of the isophorone diisocyanate, polypropylene glycol, N-methylpyrrolidone, dibutyltin dilaurate, 1,4-butanediol, modified aerogel, UV-resistant modifier and deionized water in step s4 is 7-8g:14-16g:2-4mL:0.01-0.03g:0.5-0.7g:1.2-3.6g:0.1-0.7g:60-80mL. As a further solution of the present invention: the polypropylene glycol is polypropylene glycol PPG1000. As a further solution of the present invention: a method for preparing a thermal insulation material comprises the following steps: Step 1: weigh 60-70 parts of thermal insulation emulsion, 31-45 parts of heavy calcium carbonate, 12-24 parts of talcum powder, 2.5-4.5 parts of wetting agent, 2-3 parts of dispersant, 1-3 parts of defoaming agent, 1-3 parts of film-forming aid, 0.3-0.5 parts of thickener and 25-50 parts of deionized water according to weight parts, and set aside; Step 2: Add thermal insulation emulsion, heavy calcium carbonate, talcum powder, wetting agent, dispersant, defoaming agent, film-forming aid, thickener and deionized water into a mixer, and then stir and mix for 2-3 hours at a temperature of 35-40°C and a stirring rate of 300-350r / min to obtain a thermal insulation material. As a further solution of the present invention: the wetting agent is wetting agent PE-100. As a further solution of the present invention: the dispersant is dispersant NNO. As a further solution of the present invention: the defoaming agent is defoaming agent AFE-1410. As a further solution of the present invention: the film-forming aid is alcohol ester dodecahydrate. As a further solution of the present invention: the thickener is thickener 466. As a further solution of the present invention: the thermal insulation material is used in preparing thermal insulation coating for the exterior walls of buildings. Beneficial effects of the present invention: The invention discloses a thermal insulation material and a preparation method and application thereof. The thermal insulation material is obtained by adding thermal insulation emulsion, heavy calcium carbonate, talcum powder, a wetting agent, a dispersant, a defoaming agent, a film-forming aid, a thickener and deionized water into a mixer and stirring and mixing. The preparation method uses the thermal insulation emulsion as a main raw material to prepare the thermal insulation material. The thermal insulation emulsion has excellent thermal insulation performance, so that the thermal insulation material can be applied to the exterior wall of the building to significantly improve the thermal insulation effect of the building, reduce the energy consumption of the building, comply with the concept of green building, have significant economic and social benefits, and have excellent anti-ultraviolet ability, thereby ensuring its stability and durability in practical applications. In the process of preparing thermal insulation materials, a thermal insulation emulsion is first prepared. First, nano-titanium dioxide-doped silica aerogel is prepared using tetraethyl orthosilicate and nano-titanium dioxide as raw materials to obtain a composite aerogel. Then, polydopamine is wrapped on the surface of the composite aerogel particles to obtain a modified aerogel. Then, 2,4-dihydroxybenzophenone and chloroacetyl chloride are reacted, and the hydroxyl group on the 2,4-dihydroxybenzophenone reacts with the acyl chloride group on the chloroacetyl chloride to introduce a chlorine atom to obtain a UV-resistant modifier. Finally, isophorone diisocyanate and polypropylene glycol are used as raw materials for polymerization to form a polyurethane emulsion, and the modified aerogel and the UV-resistant modifier are used to modify the polyurethane emulsion to obtain a thermal insulation emulsion. The silica aerogel has high porosity. The excellent properties of high specific surface area, low density and low thermal conductivity give the thermal insulation emulsion excellent thermal insulation performance. Doping with nano titanium dioxide can effectively improve its shading performance and anti-ultraviolet performance. After that, it is coated with polydopamine to effectively improve its dispersion performance, so that it can be evenly distributed in the emulsion, and the thermal insulation performance can be best displayed. Moreover, the added UV-resistant modifier can utilize chlorine atoms to be grafted to the polyurethane emulsion and modified aerogel in the form of chemical bonds, so that the three are effectively combined, and the anti-ultraviolet performance is greatly improved, which significantly improves the material's anti-ultraviolet ability and effectively prevents ultraviolet damage to the material, so that the thermal insulation performance of the material can be maintained for a long time, ensuring its stability and durability in practical applications. DETAILED DESCRIPTION The following will be combined with the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Embodiment 1: This embodiment is a method for preparing a thermal insulation material, comprising the following steps: Step A: 10g of tetraethyl orthosilicate, 20mL of anhydrous ethanol and 20mL of deionized water are added to a three-necked flask equipped with a stirrer and a thermometer, and stirred for 25min at a temperature of 20°C and a stirring rate of 300r / min, and then adjusted to pH 2 with a 20% hydrochloric acid solution, and then continued to stir for 2h, and then added 1.5g of nano-titanium dioxide and continued to stir for 5min, and then adjusted to pH 7.5 with 25% ammonia water, and then continued to stir for 20min, and after the reaction, the reaction product was allowed to stand for 2h, and then heated to 50°C and allowed to stand for 3h, and then supercritically dried with carbon dioxide gas to obtain a composite aerogel; Step B: 3 g of composite aerogel and 60 mL of deionized water were added to a three-necked flask equipped with a stirrer and a thermometer, and ultrasonically dispersed for 20 min at an ultrasonic frequency of 35 kHz, and then stirred for reaction at a temperature of 20° C. and a stirring rate of 300 r / min for 5 min, and then 0.1 g of tris(hydroxymethyl)aminomethane hydrochloride and 0.15 g of dopamine hydrochloride were added and continued to stir and react for 4 h. After the reaction was completed, the reaction product was centrifuged, and the precipitate was washed twice with distilled water, and then placed in a vacuum drying oven and dried at a temperature of 50° C. for 2 h to obtain a modified aerogel; Step C: 10 mmol 2,4-dihydroxybenzophenone, 11 mmol triethylamine and 30 mL tetrahydrofuran are added to a three-necked flask equipped with a stirrer, a thermometer and a constant pressure dropping funnel, and 10 mL chloroacetyl chloride is added dropwise while stirring at a temperature of 0°C and a stirring rate of 300 r / min. The chloroacetyl chloride solution formed by dissolving 11 mmol:10 mL in tetrahydrofuran is added dropwise, and the dropping rate is controlled to be 1 drop / s. After the dropwise addition is completed, the stirring reaction is continued for 3 hours. After the reaction is completed, the reaction product is added to ice water, and then allowed to stand for stratification. The organic phase is washed twice with saturated brine, and then dried with anhydrous magnesium sulfate, and then vacuum filtered. The filtrate is rotary evaporated to remove the solvent to obtain a UV-resistant modifier; Step D: 7g of isophorone diisocyanate, 14g of polypropylene glycol PPG1000, 2mL of N-methylpyrrolidone and 0.01g of dibutyltin dilaurate are added to a three-necked flask equipped with a stirrer, a thermometer and a nitrogen gas guide tube, and nitrogen protection is introduced. The mixture is stirred and reacted for 2h at a temperature of 85°C and a stirring rate of 300r / min, and then 0.5g of 1,4-butanediol is added and stirred for 1h after cooling to 50°C, and then 1.2g of modified aerogel and 0.1g of ultraviolet-resistant modifier are added and stirred for 2h. After the reaction is completed, the reaction product is neutralized with triethylamine for 30min, and the neutralization degree is 100%. Then 60mL of deionized water is added and stirred for 20min, and then rotary evaporation is performed until the solid content is 25%, to obtain a thermal insulation emulsion; Step E: weigh 60 parts of thermal insulation emulsion, 31 parts of heavy calcium carbonate, 12 parts of talcum powder, 2.5 parts of wetting agent, 2 parts of dispersant, 1 part of defoamer, 1 part of film-forming aid, 0.3 part of thickener and 25 parts of deionized water according to weight parts, and set aside; the wetting agent is wetting agent PE-100; the dispersant is dispersant NNO; the defoamer is defoamer AFE-1410; the film-forming aid is alcohol ester twelve; the thickener is thickener 466; Step F: Add thermal insulation emulsion, heavy calcium carbonate, talcum powder, wetting agent, dispersant, defoaming agent, film-forming aid, thickener and deionized water into a mixer, and then stir and mix for 2 hours at a temperature of 35° C. and a stirring rate of 300 r / min to obtain a thermal insulation material. Embodiment 2: This embodiment is a method for preparing a thermal insulation material, comprising the following steps: Step A: 11g of tetraethyl orthosilicate, 22mL of anhydrous ethanol and 22mL of deionized water are added to a three-necked flask equipped with a stirrer and a thermometer, and stirred for 30min at a temperature of 22°C and a stirring rate of 325r / min, and then adjusted to a pH of 2.5 with a 21% hydrochloric acid solution, and then continued to stir for 2.5h, and then added 2.5g of nano-titanium dioxide and continued to stir for 8min, and then adjusted to a pH of 8.0 with a 26% ammonia solution, and then continued to stir for 25min. After the reaction is completed, the reaction product is allowed to stand for 2.5h, and then heated to 52°C and allowed to stand for 4h, and then supercritically dried with carbon dioxide gas to obtain a composite aerogel; Step B: 3 g of composite aerogel and 65 mL of deionized water were added to a three-necked flask equipped with a stirrer and a thermometer, and ultrasonically dispersed for 25 min at an ultrasonic frequency of 40 kHz, and then stirred for reaction at a temperature of 22° C. and a stirring rate of 325 r / min for 7 min, and then 0.11 g of tris(hydroxymethyl)aminomethane hydrochloride and 0.20 g of dopamine hydrochloride were added and continued to stir and react for 4.5 h. After the reaction was completed, the reaction product was centrifuged, and the precipitate was washed twice with distilled water, and then placed in a vacuum drying oven and dried at a temperature of 52° C. for 2.5 h to obtain a modified aerogel; Step C: 10 mmol 2,4-dihydroxybenzophenone, 12 mmol triethylamine and 35 mL tetrahydrofuran are added to a three-necked flask equipped with a stirrer, a thermometer and a constant pressure dropping funnel, and 11 mL chloroacetyl chloride is added dropwise while stirring at a temperature of 3°C and a stirring rate of 325 r / min. The chloroacetyl chloride solution formed by dissolving 12 mmol:10 mL in tetrahydrofuran is added dropwise, and the dropping rate is controlled to be 1 drop / s. After the dropwise addition is completed, the stirring reaction is continued for 4 hours. After the reaction is completed, the reaction product is added to ice water, and then allowed to stand for stratification. The organic phase is washed twice with saturated brine, and then dried with anhydrous magnesium sulfate, and then vacuum filtered. The filtrate is rotary evaporated to remove the solvent to obtain a UV-resistant modifier; Step D: 7.5g of isophorone diisocyanate, 15g of polypropylene glycol PPG1000, 3mL of N-methylpyrrolidone and 0.02g of dibutyltin dilaurate are added to a three-necked flask equipped with a stirrer, a thermometer and a nitrogen gas guide tube, and nitrogen protection is introduced. The mixture is stirred and reacted for 2.5h at a temperature of 88°C and a stirring rate of 325r / min. After the temperature is lowered to 55°C, 0.6g of 1,4-butanediol is added and the stirring reaction is continued for 1.2h. Then, 2.4g of modified aerogel and 0.6g of ultraviolet-resistant modifier are added and the stirring reaction is continued for 2.5h. After the reaction is completed, the reaction product is neutralized with triethylamine for 40min, and the neutralization degree is 100%. Then, 70mL of deionized water is added and the stirring reaction is continued for 25min, and then rotary evaporation is performed until the solid content is 28%, to obtain a thermal insulation emulsion; Step E: weigh 65 parts of thermal insulation emulsion, 39 parts of heavy calcium carbonate, 18 parts of talcum powder, 3.5 parts of wetting agent, 2.5 parts of dispersant, 2 parts of defoaming agent, 2 parts of film-forming aid, 0.4 parts of thickener and 37 parts of deionized water according to weight parts, and set aside; the wetting agent is wetting agent PE-100; the dispersant is dispersant NNO; the defoaming agent is defoaming agent AFE-1410; the film-forming aid is alcohol ester twelve; the thickener is thickener 466; Step F: Add thermal insulation emulsion, heavy calcium carbonate, talcum powder, wetting agent, dispersant, defoaming agent, film-forming aid, thickener and deionized water into a mixer, and then stir and mix for 2.5 hours at a temperature of 38° C. and a stirring rate of 325 r / min to obtain a thermal insulation material. Embodiment 3: This embodiment is a method for preparing a thermal insulation material, comprising the following steps: Step A: 12g of tetraethyl orthosilicate, 25mL of anhydrous ethanol and 25mL of deionized water are added to a three-necked flask equipped with a stirrer and a thermometer, and stirred for 35min at a temperature of 25°C and a stirring rate of 350r / min, and then adjusted to pH 3 with a 22% hydrochloric acid solution, and then continued to stir for 3h, and then added 3.5g of nano-titanium dioxide and continued to stir for 10min, and then adjusted to pH 8.5 with 27% ammonia water, and then continued to stir for 30min. After the reaction, the reaction product was allowed to stand for 3h, and then heated to 55°C and allowed to stand for 5h, and then supercritically dried with carbon dioxide gas to obtain a composite aerogel; Step B: 3 g of composite aerogel and 70 mL of deionized water were added to a three-necked flask equipped with a stirrer and a thermometer, and ultrasonic dispersion was performed for 30 min at an ultrasonic frequency of 45 kHz, and then the mixture was stirred for reaction at a temperature of 25° C. and a stirring rate of 350 r / min for 10 min, and then 0.12 g of tris(hydroxymethyl)aminomethane hydrochloride and 0.25 g of dopamine hydrochloride were added and the stirring reaction was continued for 5 h. After the reaction was completed, the reaction product was centrifuged, and the precipitate was washed 3 times with distilled water, and then placed in a vacuum drying oven and dried at a temperature of 55° C. for 3 h to obtain a modified aerogel; Step C: 10 mmol 2,4-dihydroxybenzophenone, 13 mmol triethylamine and 40 mL tetrahydrofuran are added to a three-necked flask equipped with a stirrer, a thermometer and a constant pressure dropping funnel, and 12 mL of chloroacetyl chloride is added dropwise while stirring at a temperature of 5°C and a stirring rate of 350 r / min. The chloroacetyl chloride solution formed by dissolving 13 mmol:10 mL of chloroacetyl chloride in tetrahydrofuran is controlled at a dropping rate of 2 drops / s. After the dropwise addition is completed, the stirring reaction is continued for 5 hours. After the reaction is completed, the reaction product is added to ice water, and then allowed to stand for stratification. The organic phase is washed 3 times with saturated brine, and then dried with anhydrous magnesium sulfate, and then vacuum filtered. The filtrate is rotary evaporated to remove the solvent to obtain a UV-resistant modifier; Step D: 8 g of isophorone diisocyanate, 16 g of polypropylene glycol PPG1000, 4 mL of N-methylpyrrolidone and 0.03 g of dibutyltin dilaurate were added to a three-necked flask equipped with a stirrer, a thermometer and a nitrogen gas guide tube, and nitrogen protection was introduced. The mixture was stirred and reacted for 3 h at a temperature of 90 ° C and a stirring rate of 350 r / min. After the temperature was lowered to 60 ° C, 0.7 g of 1,4-butanediol was added and the stirring reaction was continued for 1.5 h. Then, 3.6 g of modified aerogel and 0.7 g of ultraviolet resistant modifier were added and the stirring reaction was continued for 3 h. After the reaction was completed, the reaction product was neutralized with triethylamine for 50 min, and the neutralization degree was 100%. Then, 80 mL of deionized water was added and the stirring reaction was continued for 30 min. Then, the mixture was rotary evaporated until the solid content was 30%, and a thermal insulation emulsion was obtained; Step E: weigh 70 parts of thermal insulation emulsion, 45 parts of heavy calcium carbonate, 24 parts of talcum powder, 4.5 parts of wetting agent, 3 parts of dispersant, 3 parts of defoaming agent, 3 parts of film-forming aid, 0.5 parts of thickener and 50 parts of deionized water according to weight parts, and set aside; the wetting agent is wetting agent PE-100; the dispersant is dispersant NNO; the defoaming agent is defoaming agent AFE-1410; the film-forming aid is alcohol ester twelve; the thickener is thickener 466; Step F: Add thermal insulation emulsion, heavy calcium carbonate, talcum powder, wetting agent, dispersant, defoaming agent, film-forming aid, thickener and deionized water into a mixer, and then stir and mix for 3 hours at a temperature of 40° C. and a stirring rate of 350 r / min to obtain a thermal insulation material. Comparative Example 1: This comparative example is a method for preparing a thermal insulation material, comprising the following steps: Step A: weigh 70 parts of waterborne polyurethane resin emulsion WPU-3015, 45 parts of heavy calcium carbonate, 24 parts of talcum powder, 4.5 parts of wetting agent, 3 parts of dispersant, 3 parts of defoaming agent, 3 parts of film-forming aid, 0.5 parts of thickener and 50 parts of deionized water according to weight parts, and set aside; the wetting agent is wetting agent PE-100; the dispersant is dispersant NNO; the defoaming agent is defoaming agent AFE-1410; the film-forming aid is alcohol ester twelve; the thickener is thickener 466; Step B: Add waterborne polyurethane resin emulsion WPU-3015, heavy calcium carbonate, talcum powder, wetting agent, dispersant, defoaming agent, film-forming aid, thickener and deionized water into a mixer, and then stir and mix for 3 hours at a temperature of 40° C. and a stirring rate of 350 r / min to obtain a thermal insulation material. Comparative Example 2: This comparative example is a method for preparing a thermal insulation material, comprising the following steps: Step A: 10 mmol 2,4-dihydroxybenzophenone, 13 mmol triethylamine and 40 mL tetrahydrofuran are added to a three-necked flask equipped with a stirrer, a thermometer and a constant pressure dropping funnel, and 12 mL of chloroacetyl chloride is added dropwise while stirring at a temperature of 5°C and a stirring rate of 350 r / min. The chloroacetyl chloride solution formed by dissolving 13 mmol:10 mL of chloroacetyl chloride in tetrahydrofuran is controlled at a dropping rate of 2 drops / s. After the dropwise addition is completed, the stirring reaction is continued for 5 hours. After the reaction is completed, the reaction product is added to ice water, and then allowed to stand for stratification. The organic phase is washed 3 times with saturated brine, and then dried with anhydrous magnesium sulfate, and then vacuum filtered. The filtrate is rotary evaporated to remove the solvent to obtain a UV-resistant modifier; Step B: 8g of isophorone diisocyanate, 16g of polypropylene glycol PPG1000, 4mL of N-methylpyrrolidone and 0.03g of dibutyltin dilaurate are added to a three-necked flask equipped with a stirrer, a thermometer and a nitrogen gas guide tube, and nitrogen protection is introduced. The mixture is stirred and reacted for 3h at a temperature of 90°C and a stirring rate of 350r / min, and then 0.7g of 1,4-butanediol is added and stirred for 1.5h under the condition of cooling to 60°C, and then 0.7g of UV-resistant modifier is added and stirred for 3h. After the reaction is completed, the reaction product is neutralized with triethylamine for 50min, and the neutralization degree is 100%. Then 80mL of deionized water is added and stirred for 30min, and then rotary evaporation is performed until the solid content is 30%, to obtain a thermal insulation emulsion; Step C: weigh 70 parts of thermal insulation emulsion, 45 parts of heavy calcium carbonate, 24 parts of talcum powder, 4.5 parts of wetting agent, 3 parts of dispersant, 3 parts of defoaming agent, 3 parts of film-forming aid, 0.5 parts of thickener and 50 parts of deionized water according to weight parts, and set aside; the wetting agent is wetting agent PE-100; the dispersant is dispersant NNO; the defoaming agent is defoaming agent AFE-1410; the film-forming aid is alcohol ester twelve; the thickener is thickener 466; Step D: Add thermal insulation emulsion, heavy calcium carbonate, talcum powder, wetting agent, dispersant, defoaming agent, film-forming aid, thickener and deionized water into a mixer, and then stir and mix for 3 hours at a temperature of 40° C. and a stirring rate of 350 r / min to obtain a thermal insulation material. Comparative Example 3: This comparative example is a method for preparing a thermal insulation material, comprising the following steps: Step A: 12g of tetraethyl orthosilicate, 25mL of anhydrous ethanol and 25mL of deionized water are added to a three-necked flask equipped with a stirrer and a thermometer, and stirred for 35min at a temperature of 25°C and a stirring rate of 350r / min, and then adjusted to pH 3 with a 22% hydrochloric acid solution, and then continued to stir for 3h, and then added 3.5g of nano-titanium dioxide and continued to stir for 10min, and then adjusted to pH 8.5 with 27% ammonia water, and then continued to stir for 30min. After the reaction, the reaction product was allowed to stand for 3h, and then heated to 55°C and allowed to stand for 5h, and then supercritically dried with carbon dioxide gas to obtain a composite aerogel; Step B: 3 g of composite aerogel and 70 mL of deionized water were added to a three-necked flask equipped with a stirrer and a thermometer, and ultrasonic dispersion was performed for 30 min at an ultrasonic frequency of 45 kHz, and then the mixture was stirred for reaction at a temperature of 25° C. and a stirring rate of 350 r / min for 10 min, and then 0.12 g of tris(hydroxymethyl)aminomethane hydrochloride and 0.25 g of dopamine hydrochloride were added and the stirring reaction was continued for 5 h. After the reaction was completed, the reaction product was centrifuged, and the precipitate was washed 3 times with distilled water, and then placed in a vacuum drying oven and dried at a temperature of 55° C. for 3 h to obtain a modified aerogel; Step C: 8 g of isophorone diisocyanate, 16 g of polypropylene glycol PPG1000, 4 mL of N-methylpyrrolidone and 0.03 g of dibutyltin dilaurate are added to a three-necked flask equipped with a stirrer, a thermometer and a nitrogen gas guide tube, and nitrogen protection is introduced. The mixture is stirred and reacted for 3 h at a temperature of 90 ° C and a stirring rate of 350 r / min. After the temperature is lowered to 60 ° C, 0.7 g of 1,4-butanediol is added and the stirring reaction is continued for 1.5 h. Then, 3.6 g of modified aerogel is added and the stirring reaction is continued for 3 h. After the reaction is completed, the reaction product is neutralized with triethylamine for 50 min, and the neutralization degree is 100%. Then, 80 mL of deionized water is added and the stirring reaction is continued for 30 min. Then, rotary evaporation is performed until the solid content is 30%, and a thermal insulation emulsion is obtained; Step D: 70 parts of thermal insulation emulsion, 45 parts of heavy calcium carbonate, 24 parts of talcum powder, 4.5 parts of wetting agent, 3 parts of dispersant, 3 parts of defoaming agent, 3 parts of film-forming aid, 0.5 parts of thickener and 50 parts of deionized water are weighed according to weight parts for use; the wetting agent is wetting agent PE-100; the dispersant is dispersant NNO; the defoaming agent is defoaming agent AFE-1410; the film-forming aid is alcohol ester twelve; the thickener is thickener 466; Step E: Add thermal insulation emulsion, heavy calcium carbonate, talcum powder, wetting agent, dispersant, defoaming agent, film-forming aid, thickener and deionized water into a mixer, and then stir and mix for 3 hours at a temperature of 40° C. and a stirring rate of 350 r / min to obtain a thermal insulation material. An aluminum plate with a size of 100 mm × 60 mm × 0.3 mm was selected and polished with sandpaper, then soaked in ethanol and cleaned with deionized water to remove impurities on the surface. After drying, the thermal insulation materials of Examples 1-3 and Comparative Examples 1-3 were sprayed on one side, respectively, with a coating thickness of 1 mm. The coating was naturally dried until solid, and the performance of the coating was tested. The test results are as follows: sample hardness Thermal conductivity, W / (m·K) <![CDATA[Anti-ultraviolet performance (0.80W / m 2 、1000h)]]> Example 1 4H 0.041 No powdering, blistering or cracking Example 2 4H 0.036 No powdering, blistering or cracking Example 3 4H 0.032 No powdering, blistering or cracking Comparative Example 1 2H 0.156 Severe powdering, heavy blistering and cracking Comparative Example 2 2H 0.138 No powdering, blistering or cracking Comparative Example 3 4H 0.056 Severe powdering, heavy blistering and cracking Referring to the data in the above table, according to the comparison between Examples 1-3 and Comparative Examples 1-3, it can be known that the thermal insulation effect and anti-ultraviolet performance of the thermal insulation material are greatly improved after the polyurethane emulsion is modified by using modified aerogel and UV-resistant modifier as modifiers. In the description of this specification, the description with reference to the terms "one embodiment", "example", "specific example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the present invention. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner. The above contents are merely examples and explanations of the present invention. Those skilled in the art may make various modifications or additions to the specific embodiments described or replace them in a similar manner. As long as they do not deviate from the invention or exceed the scope defined by the claims, they shall all fall within the protection scope of the present invention.
Claims
1. A thermal insulation material, characterized in that: It comprises the following components in parts by weight: 60-70 parts of thermal insulation emulsion, 31-45 parts of heavy calcium carbonate, 12-24 parts of talc, 2.5-4.5 parts of wetting agent, 2-3 parts of dispersant, 1-3 parts of defoaming agent, 1-3 parts of film-forming aid, 0.3-0.5 parts of thickener and 25-50 parts of deionized water; Wherein, the thermal insulation emulsion is prepared by the following steps: Step s1: stirring ethyl orthosilicate, anhydrous ethanol and deionized water for reaction, then adjusting the pH with hydrochloric acid solution, then adding nano titanium dioxide and continuing stirring the reaction, then adjusting the pH with ammonia water, then continuing stirring the reaction, and after the reaction is completed, the reaction product is allowed to stand, and then supercritical drying with carbon dioxide gas is performed to obtain a composite aerogel; Step s2: ultrasonically dispersing the composite aerogel and deionized water, then adding tris(hydroxymethyl)aminomethane hydrochloride and dopamine hydrochloride to react by stirring, centrifuging the reaction product after the reaction is completed, washing and drying the precipitate to obtain a modified aerogel; Step s3: stirring 2,4-dihydroxybenzophenone, triethylamine and tetrahydrofuran for reaction, then adding chloroacetyl chloride solution dropwise while stirring, continuing stirring for reaction after the addition is complete, adding the reaction product into ice water after the reaction is complete, then standing for stratification, washing and drying the organic phase, then vacuum filtering, and rotary evaporating the filtrate to obtain a UV-resistant modifier; Step s4: stirring isophorone diisocyanate, polypropylene glycol, N-methylpyrrolidone and dibutyltin dilaurate to react, then adding 1,4-butanediol, modified aerogel and UV-resistant modifier to continue stirring the reaction, neutralizing the reaction product after the reaction is completed, then adding deionized water to continue stirring the reaction, and then rotary evaporation to obtain a thermal insulation emulsion.
2. A thermal insulation material according to claim 1, characterized in that: The usage ratio of the tetraethyl orthosilicate, anhydrous ethanol, deionized water and nano-titanium dioxide in step s1 is 10-12 g: 20-25 mL: 20-25 mL: 1.5-3.5 g.
3. The thermal insulation material according to claim 1, characterized in that: The mass fraction of the hydrochloric acid solution in step s1 is 20-22%, and the mass fraction of the ammonia water is 25-27%.
4. The thermal insulation material according to claim 1, characterized in that: The usage ratio of the composite aerogel, deionized water, tris(hydroxymethyl)aminomethane hydrochloride and dopamine hydrochloride in step s2 is 3 g: 60-70 mL: 0.1-0.12 g: 0.15-0.25 g.
5. The thermal insulation material according to claim 1, characterized in that: The usage ratio of the 2,4-dihydroxybenzophenone, triethylamine, tetrahydrofuran and chloroacetyl chloride solution in step s3 is 10 mmol: 11-13 mmol: 30-40 mL: 10-12 mL.
6. The thermal insulation material according to claim 1, characterized in that: The chloroacetyl chloride solution in step s3 is a solution formed by dissolving chloroacetyl chloride in tetrahydrofuran at a ratio of 11-13 mmol:10 mL.
7. The thermal insulation material according to claim 1, characterized in that: The dosage ratio of the isophorone diisocyanate, polypropylene glycol, N-methylpyrrolidone, dibutyltin dilaurate, 1,4-butanediol, modified aerogel, UV-resistant modifier and deionized water in step s4 is 7-8g: 14-16g: 2-4mL: 0.01-0.03g: 0.5-0.7g: 1.2-3.6g: 0.1-0.7g: 60-80mL; the polypropylene glycol is polypropylene glycol PPG1000.
8. A method for preparing a thermal insulation material, characterized in that: The following steps are involved: Step 1: weigh 60-70 parts of thermal insulation emulsion, 31-45 parts of heavy calcium carbonate, 12-24 parts of talcum powder, 2.5-4.5 parts of wetting agent, 2-3 parts of dispersant, 1-3 parts of defoaming agent, 1-3 parts of film-forming aid, 0.3-0.5 parts of thickener and 25-50 parts of deionized water according to weight parts, and set aside; Step 2: Add thermal insulation emulsion, heavy calcium carbonate, talcum powder, wetting agent, dispersant, defoaming agent, film-forming aid, thickener and deionized water into a mixer, and then stir and mix for 2-3 hours at a temperature of 35-40°C and a stirring rate of 300-350r / min to obtain a thermal insulation material.
9. The method for preparing a thermal insulation material according to claim 8, characterized in that: The wetting agent is wetting agent PE-100; the dispersant is dispersant NNO; the defoaming agent is defoaming agent AFE-1410; the film-forming aid is alcohol ester dodecahydrate; and the thickener is thickener 466.
10. Use of the thermal insulation material according to any one of claims 1 to 7 in preparing thermal insulation coatings for building exterior walls.
Citation Information
Cited By
TPE (thermoplastic elastomer) composition for protective film adhesive layer and preparation method of TPE composition