Method for optimizing single-furnace single-machine ladle turnover rate and buggy ladle base
By optimizing the inner diameter of the converter outlet, the converter smelting strategy, automated fault detection and double ladle operation mode, combined with double-person operation and triangular ladle mount design, the problem of large thermal energy loss in ladle turnover is solved, and the steelmaking efficiency and turnover rate are improved , reducing costs and carbon emissions.
Patent Information
- Application Number
- CN202411179789.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-27
- Publication Date
- 2024-11-29
AI Technical Summary
In the converter direct-up casting process, the existing ladle turnover method leads to excessive thermal energy loss, affecting steelmaking efficiency.
By optimizing the inner diameter of the converter outlet, the hourly rate of the converter steel outlet, the ladle heating and process operation mode, the double ladle operation mode and automatic fault detection are adopted, combined with double-person operation and the optimized ladle car base design, the ladle turnover time is shortened.
It significantly improves the turnover rate of ladles and steelmaking efficiency, reduces thermal energy losses, and reduces steelmaking costs and carbon emissions.
Smart Images

Figure CN119040546A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of iron and steel metallurgy, and in particular to a method for optimizing the turnover rate of a ladle of a single furnace and a ladle car base. Background Art
[0002] Ladle is a container used to hold and handle liquid steel. The molten steel flows out through a port at the bottom for casting. The ladle usually consists of two parts: the outer shell and the lining. The outer shell is generally made of steel plate, while the lining uses refractory materials, such as refractory bricks, to ensure the safe handling and transportation of molten steel in a high temperature environment.
[0003] In the current converter direct continuous casting process, the ladle turnover usually adopts the "three in use and one in standby" mode: after the first ladle receives the molten steel output from the converter, it is transported to the continuous casting turntable by the crane, and the crane returns to the ladle waiting position to pull the second ladle to the converter to receive the molten steel. After the continuous casting of the first ladle is completed, the crane transports the first ladle to the ladle hot repair area, and then runs the second ladle that has received the molten steel to the continuous casting turntable. The crane returns to the ladle waiting position to pull the third ladle to the converter to receive the molten steel. After the hot repair of the first ladle is completed, the crane transports it to the ladle waiting position to wait, and the three ladles are circulated in the above order. As a result, the three-ladle turnover method ensures that there is always a ladle waiting in the ladle waiting position. Since the longer the turnover time during the ladle operation, the greater the loss of heat energy, the three-ladle turnover method can make the continuous casting process operate normally, but due to the long waiting time of the ladle, the heat energy loss is too large, which affects the steelmaking efficiency. Summary of the invention
[0004] The object of the present invention is to provide a method for optimizing the turnover rate of a single furnace and a single machine ladle and a ladle car base, so as to solve the problem of excessive heat energy loss caused by the existing ladle turnover mode.
[0005] To achieve the above object, the basic solution provided by the present invention is: a method for optimizing the ladle turnover rate of a single furnace and a single machine, comprising:
[0006] Optimize tapping time: optimize the inner diameter of the converter tapping port;
[0007] Optimize the converter steel-tapping rate: Before the molten iron enters the converter, obtain the molten iron information and guide the converter to smelt the molten iron according to different molten iron information;
[0008] Optimize ladle hot repair: Automatically detect faults of ladle nozzles and sliders, and replace them in time;
[0009] Optimize auxiliary processes: use a two-person operation mode to perform process operations on the ladle at the same time; the process operations include unhooking the hydraulic cylinder and adding drainage sand to the converter;
[0010] Optimize the ladle operation mode: optimize the original three-ladle operation mode to a double-ladle operation mode;
[0011] The double ladle operation mode specifically includes the following steps:
[0012] S1: transporting the first ladle to the ladle car under the steel outlet of the converter, so that the converter outputs the molten steel into the first ladle;
[0013] S2: When the first ladle is full, the first ladle is transported to the continuous casting ladle turret, so that the continuous casting ladle turret transfers the first ladle to the casting position for casting; the second ladle is transported to the ladle car under the steel outlet of the converter, so that the converter outputs the molten steel into the second ladle;
[0014] S3: transporting the first ladle after casting to the ladle hot repair area, so that the hot repair equipment in the ladle hot repair area performs hot repair on the first ladle to complete one turnover of the first ladle; when the second ladle is full, transporting the second ladle to the continuous casting ladle turntable, so that the continuous casting ladle turntable turns the second ladle to the casting position for casting;
[0015] S4: transporting the first ladle that has been hot-repaired to the ladle car under the converter outlet, so that the converter outputs the molten steel into the first ladle; transporting the second ladle that has been cast to the ladle hot-repair area, so that the hot-repair equipment in the ladle hot-repair area performs hot-repair on the second ladle to complete one turnover of the second ladle.
[0016] With regard to the optimization of the ladle turnover rate, the present invention optimizes the factors affecting the ladle turnover, namely, optimizes the inner diameter of the converter tapping port to reduce the tapping time, controls the converter for differentiated smelting according to different molten irons, so as to improve the converter tapping rate, and automatically detects and replaces the ladle nozzle and the slider, thereby reducing the ladle fault detection time and ensuring the normal operation of the ladle. The ladle is simultaneously processed by two people, which shortens the manual operation time and further reduces the ladle turnover time. Since the turnover time of three ladles is too long, the present invention utilizes two ladles for turnover, so that two ladles are always in the converter direct-on continuous casting process flow, thereby reducing the ladle turnover time and improving the ladle turnover rate and steelmaking efficiency.
[0017] Preferably, optimizing the steel tapping time includes: optimizing the inner diameter of the converter tapping port to Φ190 mm.
[0018] By increasing the size of the converter outlet, the flow rate of molten steel output from the converter is increased, the waiting time for the ladle to receive the molten steel is reduced, and the ladle turnover rate is further improved.
[0019] Preferably, the converter tapping rate is optimized, specifically including:
[0020] Measure the temperature of the current molten iron before entering the furnace to obtain the current molten iron temperature;
[0021] Get the current molten iron composition information;
[0022] According to the current molten iron temperature and the current molten iron composition information, a converter smelting operation matching the current molten iron is determined from the preset converter smelting strategy;
[0023] According to the converter smelting operation matching the current molten iron, the current molten iron is smelted by the converter to obtain molten steel.
[0024] By determining the converter smelting operation that matches the current molten iron from the preset converter smelting strategy based on the current molten iron temperature and the current molten iron composition information before the molten iron enters the converter, corresponding guidance is given to the smelting according to molten iron of different temperatures and compositions, thereby improving the converter one-time turnover rate and the converter full-time steel tapping rate, reducing the time for the ladle to wait for steel tapping, thereby shortening the ladle turnover time and improving the ladle turnover rate.
[0025] Preferably, the ladle thermal repair is optimized, specifically comprising:
[0026] Automatic fault detection of the slider and nozzle of the first or second ladle;
[0027] If a slider fault is detected, the slider of the first ladle or the second ladle is replaced; if a water outlet fault is detected, the water outlet of the first ladle or the second ladle is replaced.
[0028] By performing a fault detection on the sliders and nozzles of the first ladle and the second ladle in each round of turnover, the sliders and nozzles are replaced in time to ensure the normal turnover of the next ladle and improve the stability of the ladle turnover.
[0029] Preferably, optimizing the hot repair of the ladle further comprises:
[0030] If it is detected that the slider and the water inlet of the first ladle or the second ladle are simultaneously faulty, the first ladle or the second ladle is replaced by a spare ladle.
[0031] Since it takes too long to replace the water inlet and the slider at the same time, the present invention provides a spare ladle. When the water inlet and the slider of the first ladle or the second ladle are damaged, the spare ladle is used to replace them, thereby saving hot repair time and reducing the ladle turnover time.
[0032] After the molten iron is output to the first ladle or the second ladle and before the first ladle or the second ladle is transported to the continuous casting ladle turret in step S2 and step S3, the method further includes:
[0033] The first ladle or the second ladle is nitrogen blown, and the nitrogen blowing time is controlled within the range of 4.5-5 minutes.
[0034] By blowing nitrogen into the molten steel after the ladle receives it, the molten steel can be degassed, inclusions can be reduced, and the composition and temperature can be uniform.
[0035] The present invention also provides a ladle car base, which comprises a bottom plate and two baffles, wherein the baffles are respectively arranged at two ends of the bottom plate, and the cross-section shape of the baffles is a triangle.
[0036] The cross-sectional shape of the baffles at both ends of the existing ladle base is mostly square. During operation, the crane lifts the ladle to the top of the ladle car and drops it into the slot of the ladle car base. Since the slots on both sides are square baffles, personnel are required to direct the lifting process and accurately drop it into the slot, which wastes turnover time. Therefore, the present invention sets the cross-sectional shape of the baffles at both ends of the ladle base to a triangle. When the ladle is lifted to the ladle base, it will slide into the ladle car base along with the baffle, so as to reduce the lifting time of the ladle, thereby shortening the turnover time of the ladle and improving the turnover rate of the ladle. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] Figure 1 It is a cross-sectional view of a ladle car base of the present invention. DETAILED DESCRIPTION
[0038] The present invention is further described in detail below through specific embodiments:
[0039] The reference numerals in the drawings of the specification include: 1. bottom plate; 2. baffle.
[0040] Example
[0041] This embodiment provides a method for optimizing the ladle turnover rate of a single furnace and a single machine, specifically comprising:
[0042] Optimize tapping time: optimize the inner diameter of the converter tapping port.
[0043] It should be noted that the inner diameter of the outlet port casing used in the converter of the existing steel plant is φ170mm, and the average steel-tapping time is 4.5min. In order to shorten the steel-tapping time, the inner diameter of the steel-tapping port Guantao is set to φ190mm in this embodiment, so that the average steel-tapping time is 3.5min, which shortens the steel-tapping time by one minute, thereby shortening the waiting time for the ladle to receive molten steel and improving the turnover efficiency.
[0044] Optimize the converter steel-tapping rate: Before the molten iron enters the converter, obtain the molten iron information and guide the converter to smelt the molten iron according to different molten iron information.
[0045] It should be understood that there are differences in the process parameters required for smelting molten iron of different temperatures and compositions in a converter. Therefore, the present embodiment provides a preset converter smelting strategy, in which the preset converter smelting strategy is provided with the process parameters and related operations required for smelting molten iron of different temperatures and compositions in a converter, so as to achieve corresponding guidance for smelting according to molten iron of different temperatures and compositions, thereby improving the converter pouring rate and the converter tapping rate at the whole time, reducing the time for the ladle to wait for tapping, thereby shortening the ladle turnover time and improving the ladle turnover rate.
[0046] Optimize ladle thermal repair: Automatically detect faults in the ladle’s nozzle and slider, and replace them in a timely manner.
[0047] Specifically, the method includes: performing automated fault detection on the slider and water nozzle of the first ladle or the second ladle; if a slider fault is detected, replacing the slider of the first ladle or the second ladle; if a water nozzle fault is detected, replacing the water nozzle of the first ladle or the second ladle; if both the slider and the water nozzle of the first ladle or the second ladle are detected to be faulty at the same time, replacing the first ladle or the second ladle with a spare ladle; performing a fault detection on the slider and the water nozzle of the first ladle and the second ladle in each round of turnover, replacing the slider and the water nozzle in time, and providing a spare ladle; when the water nozzle and the slider of the first ladle or the second ladle are both damaged, replacing them with the spare ladle, thereby saving hot repair time, ensuring the normal turnover of the next ladle, and improving the turnover stability of the ladle.
[0048] Optimize auxiliary processes: Use a two-person operation mode to perform process operations on the ladle simultaneously; the process operations include unhooking the hydraulic cylinder and adding drainage sand to the converter.
[0049] It should be understood that each ladle is respectively provided with two water inlets, and each water inlet is respectively provided with a hydraulic cylinder. Therefore, the embodiment also arranges process operations such as detaching and hanging the hydraulic cylinder and adding drainage sand to the converter to be performed by two operators at the same time, so as to shorten the operation time, reduce the ladle turnover time, and improve the ladle turnover rate.
[0050] Optimize the ladle operation mode: optimize the original three-ladle operation mode to a double-ladle operation mode;
[0051] The double ladle operation mode specifically includes the following steps:
[0052] S1: transporting the first ladle to the ladle car under the steel outlet of the converter, so that the converter outputs molten steel into the first ladle.
[0053] S2: When the first ladle is full, the first ladle is transported to the continuous casting ladle turret, so that the continuous casting ladle turret transfers the first ladle to the casting position for casting; the second ladle is transported to the ladle car under the steel outlet of the converter, so that the converter outputs the molten steel into the second ladle.
[0054] In step S2 and step S3, after the molten iron is output to the first ladle or the second ladle, and before the first ladle or the second ladle is transported to the continuous casting ladle turntable, the present embodiment also performs nitrogen blowing on the first ladle or the second ladle, and controls the nitrogen blowing time within the range of 4.5-5 minutes to achieve degassing of the molten steel, reduction of inclusions, uniform composition, and uniform temperature.
[0055] S3: transporting the first ladle after casting to the ladle hot repair area, so that the hot repair equipment in the ladle hot repair area performs hot repair on the first ladle to complete one turnover of the first ladle; when the second ladle is full, transporting the second ladle to the continuous casting ladle turntable, so that the continuous casting ladle turntable turns the second ladle to the casting position for casting.
[0056] S4: transporting the first ladle that has been hot-repaired to the ladle car under the converter outlet, so that the converter outputs the molten steel into the first ladle; transporting the second ladle that has been cast to the ladle hot-repair area, so that the hot-repair equipment in the ladle hot-repair area performs hot-repair on the second ladle to complete one turnover of the second ladle.
[0057] It can be understood that the present embodiment sets three process points, namely the ladle car under the converter steel outlet, the continuous casting ladle turntable and the ladle hot repair area. The ladle is transported by the crane and then switched among the three process points. The crane transports the ladle to the ladle car under the converter steel outlet to receive the molten steel output by the converter. After receiving the molten steel, the crane transports the ladle to the continuous casting ladle turntable, and the continuous casting ladle turntable rotates the ladle to the casting position to cast the molten steel in the ladle into the intermediate ladle. After the casting is completed, the continuous casting ladle turntable transfers the ladle to the waiting position, and the crane transports the ladle on the waiting position to the ladle hot repair area for hot repair to complete one turnover of the ladle, thereby realizing that the two ladles are always in the converter direct continuous casting process flow, reducing the ladle turnover time, and improving the ladle turnover rate and steelmaking efficiency.
[0058] The original ladle operation adopts three-ladle operation, and the double-ladle operation proposed in this embodiment has a turnover time as shown in Table 1 in actual operation. It can be seen that the turnover time of the double-ladle turnover is significantly less than that of the three-ladle turnover, which saves turnover time and improves the ladle turnover rate.
[0059] Table 1: Comparison of the cycle of three-ladle turnover and double-ladle turnover
[0060] Serial number Links Three ladle turnover (reasonable time) Double ladle turnover (reasonable time) Comparisons 1 Steel tapping 215 215 0 2 Nitrogen blowing 300 300 0 3 Lifting continuous casting 228 228 0 4 Casting time 2400 2400 0 5 Lifting to hot repair 230 230 0 6 Hot repair time 300 300 0 7 Hoist to the ground 120 120 0 8 Ground waiting time 730 -730 9 Lifting to ladle car 90 180 90 10 Waiting for steel tapping 840 -840 11 Summary(s) 5453 3973 -1480 12 Summary (min) 90.88 66.22 -24.67
[0061] In addition, when three ladles are in operation, the tapping temperature of the ladle is high, resulting in high steelmaking processing costs. The double ladle operation adopted in this embodiment can reduce the tapping temperature, reduce the steelmaking processing costs, and reduce carbon emissions. For example, HPB300 steel series steel is refined according to the double ladle mode and the three-ladle mode, and the tapping temperature comparison shown in Table 2 is obtained. It can be seen that the tapping temperature in the double ladle mode is significantly lower than the tapping temperature in the three-ladle mode, which can achieve a better steelmaking effect. Table 2 is shown below:
[0062] Table 2: Comparison of tapping temperature between three-ladle and two-ladle operation
[0063]
[0064]
[0065] For example, as shown in Table 3, when the double ladle turnover was not enabled in 2022, the ladle turnover rate was 15%. Since 2023, the double ladle operation has been gradually implemented in real time. As the double ladle execution rate increases, the ladle turnover rate is also increasing, and the tapping temperature is also decreasing. Every 1°C decrease in the tapping temperature reduces 1kg of molten iron (increases production by 1kg), and the annual output of molten iron is 1.24 million tons, and the profit per ton of steel is 286 yuan (refer to the profit in 2023). Increased production of 124*17.24 / 1000=21,400 tons, profit of 214*286=6.12 million yuan, saving 21,400 tons of molten iron, carbon emission intensity of molten iron in the ironmaking plant of 1.06t / t, and annual reduction of CO2 emissions of 2.14*1.06=22,700 tons. Therefore, it is proved that under the double ladle turnover mode provided in this embodiment, the turnover rate is significantly improved, and the production cost of steelmaking is reduced, and carbon emissions are reduced. Specific Table 3 is shown in the figure below:
[0066] Table 3: Comparison of turnover rate and tapping temperature before and after double ladle implementation
[0067]
[0068] like Figure 1 As shown, this embodiment provides a ladle car base, including a bottom plate 1 and two baffles 2, the baffles 2 are respectively arranged at both ends of the bottom plate 1, and the cross-sectional shape of the baffles 2 is a triangle.
[0069] The cross-sectional shape of the baffles at both ends of the existing ladle base is mostly square. During operation, the crane lifts the ladle to the top of the ladle car and drops it into the slot of the ladle car base. Since the slots on both sides are square baffles, personnel are required to direct the lifting process and accurately drop it into the slot, which wastes turnover time. Therefore, in this embodiment, the cross-sectional shape of the baffles 2 at both ends of the ladle base is set to a triangle. When the ladle is lifted to the ladle base, it will slide into the ladle car base along with the baffles 2, so as to reduce the lifting time of the ladle, thereby shortening the turnover time of the ladle and improving the turnover rate of the ladle.
[0070] The above is only an embodiment of the present invention, and the common knowledge such as the known specific structure and characteristics in the scheme is not described in detail here. It should be pointed out that for those skilled in the art, several deformations and improvements can be made without departing from the structure of the present invention, which should also be regarded as the protection scope of the present invention, and these will not affect the effect of the implementation of the present invention and the practicality of the patent. The scope of protection required by this application shall be based on the content of its claims, and the specific implementation methods and other records in the specification can be used to interpret the content of the claims.
Claims
1. A method for optimizing the ladle turnover rate of a single furnace and a single machine, characterized in that: include: Optimize tapping time: optimize the inner diameter of the converter tapping port; Optimize the converter steel-tapping rate: before the molten iron enters the converter, obtain the molten iron information, and guide the converter to smelt the molten iron according to different molten iron information; Optimize ladle hot repair: Automatically detect faults of ladle nozzles and sliders, and replace them in time; Optimize auxiliary processes: use a two-person operation mode to perform process operations on the ladle at the same time; the process operations include unhooking the hydraulic cylinder and adding drainage sand to the converter; Optimize the ladle operation mode: optimize the original three-ladle operation mode to a double-ladle operation mode; The double ladle operation mode specifically includes the following steps: S1: transporting the first ladle to a ladle car under the steel outlet of the converter, so that the converter outputs molten steel into the first ladle; S2: when the first ladle is full, the first ladle is transported to the continuous casting ladle turret, so that the continuous casting ladle turret transfers the first ladle to the casting position for casting; the second ladle is transported to the ladle car under the steel outlet of the converter, so that the converter outputs the molten steel into the second ladle; S3: transporting the first ladle after casting to the ladle hot repair area, so that the hot repair equipment in the ladle hot repair area performs hot repair on the first ladle to complete one turnover of the first ladle; when the second ladle is full, transporting the second ladle to the continuous casting ladle turntable, so that the continuous casting ladle turntable turns the second ladle to the casting position for casting; S4: transporting the first ladle that has been hot-repaired to the ladle car under the converter outlet, so that the converter outputs molten steel into the first ladle; transporting the second ladle that has been cast to the ladle hot-repair area, so that the hot-repair equipment in the ladle hot-repair area performs hot-repair on the second ladle to complete one turnover of the second ladle.
2. The method for optimizing the ladle turnover rate of a single furnace and a single machine according to claim 1, characterized in that ,The optimization of steel tapping time includes: optimizing the inner diameter of the converter steel tapping port to Φ190mm.
3. The method for optimizing the ladle turnover rate of a single furnace and a single machine according to claim 1, characterized in that The optimization of converter steel tapping rate specifically includes: Measure the temperature of the current molten iron before entering the furnace to obtain the current molten iron temperature; Get the current molten iron composition information; According to the current molten iron temperature and the current molten iron composition information, determining a converter smelting operation matching the current molten iron from a preset converter smelting strategy; According to the converter smelting operation matching the current molten iron, the current molten iron is smelted by the converter to obtain molten steel.
4. The method for optimizing the ladle turnover rate of a single furnace and a single machine according to claim 1, characterized in that: The optimization of ladle thermal repair specifically includes: Performing automated fault detection on a slider and a nozzle of the first ladle or the second ladle; If a slider fault is detected, the slider of the first ladle or the second ladle is replaced; if a water outlet fault is detected, the water outlet of the first ladle or the second ladle is replaced.
5. The method for optimizing the ladle turnover rate of a single furnace and a single machine according to claim 3, characterized in that: The optimization of ladle hot repair specifically includes: If it is detected that the slider and the water nozzle of the first ladle or the second ladle are simultaneously faulty, the first ladle or the second ladle is replaced by a spare ladle.
6. The method for optimizing the ladle turnover rate of a single furnace and a single machine according to claim 1, characterized in that In step S2 and step S3, after the molten iron is output to the first ladle or the second ladle, and before the first ladle or the second ladle is transported to the continuous casting ladle turntable, the method further includes: The first ladle or the second ladle is nitrogen blown, and the nitrogen blowing time is controlled within 4.5-5 minutes.
7. A ladle car base, characterized in that: It comprises a bottom plate (1) and two baffles (2), wherein the baffles (2) are respectively arranged at two ends of the bottom plate (1), and the cross-section of the baffles (2) is in the shape of a triangle.