Stirring device, growth equipment and growth method for growing GaN single crystal by flux method

In the stirring device for growing GaN single crystals in the flux method, the rotation shaft and rotary transmission assembly are used to realize the rotation and rotation of the reactor, which solves the problem of poor stirring effect in the prior art, and improves the dissociation speed of N ions and GaN The growth quality of single crystals simplifies the device structure and reduces costs.

CN119041003APending Publication Date: 2024-11-29DONGGUAN INST OF OPTO ELECTRONICS PEKING UNIV
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202411269545.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-10
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

The existing stirring device for growing GaN single crystals with flux method has poor stirring effect, resulting in a low dissociation rate of N ions, which cannot effectively distribute N ions evenly in the melt, limiting the growth rate and thickness of GaN single crystals.

Method used

A stirring device including a fixing frame, a rotary shaft, a rotary transmission assembly and a reactor loaded with melt were designed. The reactor was driven to rotate about its axis by a rotary shaft, and the rotation of the reactor was realized through a rotary transmission assembly, which enhanced the stirring force. , enables N ions to be distributed evenly.

Benefits of technology

It effectively improves the dissociation speed of N ions and the growth speed and quality of GaN single crystals, simplifies the device structure, reduces manufacturing costs, and adapts to high-temperature and high-pressure environments.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119041003A_ABST
    Figure CN119041003A_ABST
Patent Text Reader

Abstract

The invention discloses a stirring device, growth equipment and a growth method for growing a GaN single crystal by a flux method. The stirring device comprises a fixed frame, a rotating shaft, a rotating transmission assembly and a reaction kettle loaded with a melt, the rotating shaft is connected with a driving part, the driving part is used for driving the rotating shaft to rotate around the axis of the rotating shaft, the outer side of the rotating shaft is connected with at least one first transmission shaft, the reaction kettle is rotationally connected to the first transmission shaft, and a gas inlet channel for inputting nitrogen is formed in the reaction kettle; the reaction kettle is connected with the fixed frame through a rotary transmission assembly; when the driving part drives the rotating shaft to rotate, the reaction kettle revolves around the axis of the rotating shaft, and the reaction kettle rotates around the axis of the reaction kettle through the rotating transmission assembly. Through the design, the technical problems that the dissociation speed of N ions is low and the N ions cannot be effectively and uniformly distributed in a melt due to the fact that the stirring effect of an existing stirring device for growing GaN single crystals is poor can be effectively solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of GaN single crystal growth, and in particular to a stirring device, a growth device and a growth method for growing GaN single crystals by a flux method. Background Art

[0002] The process of growing single crystal GaN by the flux method is a gas-liquid-solid three-phase reaction process: the high-temperature nitrogen N2 in the furnace body dissociates in the high-temperature melt, and then the dissociated N ions combine with the Ga ions in the melt to grow into GaN single crystals. However, the solubility of high-temperature nitrogen in the melt is very small. For example, the solubility of nitrogen N2 in the Ga-Na melt at 850 degrees and 4MPa is usually less than 0.05%. Therefore, the growth time of GaN by the flux method is long, generally 96h to 300h, and the growth thickness is only a few hundred microns. Therefore, in order to increase the growth rate and growth thickness, the melt is generally stirred to accelerate the dissociation of nitrogen and the mass transfer of N ions.

[0003] The general stirring method of the melt in the reactor mainly includes: setting a rotating shaft in the furnace body, placing the reactor horizontally on the rotating shaft, and the rotating shaft drives the reactor to rotate to achieve the growth of GaN single crystals. However, in the actual growth process, the rotation speed of the rotating shaft is generally 5-25 revolutions per minute. During the rotation process, the high-temperature melt in the reactor is very likely to form a relatively static state with the reactor, and the contact area of ​​the gas-liquid interface is generally in a stable state. Therefore, the stirring force of this method is still insufficient, and the stirring effect is poor, which leads to a low dissociation rate of N ions and the technical problem that N ions cannot be effectively evenly distributed in the melt.

[0004] Therefore, finding a technical solution that can solve the above technical problems has become an important topic studied by technical personnel in this field. Summary of the invention

[0005] The embodiment of the present invention discloses a stirring device, a growth equipment and a growth method for growing GaN single crystals by a flux method, which are used to solve the technical problem that the stirring effect of the existing stirring device for growing GaN single crystals is poor, resulting in a low dissociation rate of N ions and an inability to effectively evenly distribute N ions in the melt.

[0006] The present invention provides a stirring device for growing GaN single crystal by flux method, comprising a fixed frame, a rotating shaft, a rotating transmission component and a reaction kettle loaded with melt;

[0007] The rotating shaft is connected to a driving member, and the driving member is used to drive the rotating shaft to rotate around its own axis. The outer side of the rotating shaft is connected to at least one first transmission shaft, the reactor is rotatably connected to the first transmission shaft, and the reactor is provided with an air inlet channel for nitrogen input. The fixed frame is arranged around the rotating shaft, and the reactor is connected to the fixed frame through the rotating transmission assembly;

[0008] When the driving member drives the rotating shaft to rotate, the reaction kettle revolves around the axis of the rotating shaft, and the reaction kettle rotates around its own axis through the rotating transmission component.

[0009] Optionally, the first transmission shaft and the rotating shaft are arranged at a preset inclination angle α, and the axis of the reactor coincides with the axis of the first transmission shaft.

[0010] Optionally, the rotating shaft is further connected to a bracket, and the bracket extends outwardly to have supporting side wings that are the same in number and corresponding in position to the first transmission shaft;

[0011] The bottom of the reactor is connected to a second transmission shaft, the top of the reactor is connected to a third transmission shaft, and the axes of the second transmission shaft and the third transmission shaft coincide with the axis of the reactor;

[0012] A first bearing is installed at the end of the first transmission shaft away from the rotating shaft, the second transmission shaft is rotatably connected to the first bearing, a second bearing is installed at the end of the supporting wing away from the bracket, and the third transmission shaft is rotatably connected to the second bearing.

[0013] Optionally, the air intake passage extends from the interior of the reactor through the third transmission shaft to the exterior of the reactor.

[0014] Optionally, the rotary transmission assembly includes an annular groove provided on the fixing frame and a transmission gear provided on the third transmission shaft;

[0015] The annular groove is arranged around the fixing frame, and an annular gear track is arranged in the annular groove, and the annular gear track includes a plurality of first gear teeth arranged at intervals, the transmission gear is meshed between two adjacent first gear teeth, and the spacing between two adjacent first gear teeth is the same as the gear tooth spacing on the outer side of the transmission gear.

[0016] Optionally, the rotary transmission assembly includes a second ring gear disposed on the fixed frame and a first ring gear disposed on the outer side wall of the reactor;

[0017] The second ring gear is disposed around the fixing frame, and the first ring gear is meshed with the second ring gear.

[0018] Optionally, the driving member is a motor.

[0019] The present invention provides a growth device for growing GaN single crystals by a flux method, comprising a furnace body, a heater and a stirring device for growing GaN single crystals by a flux method;

[0020] The stirring device is installed in the furnace body, and the heater is arranged outside the stirring device to heat the reaction kettle.

[0021] Optionally, the heater is a graphite heater.

[0022] The present invention provides a method for growing a GaN single crystal by a flux method, which is based on the above-mentioned growth equipment and comprises the following steps:

[0023] S1. Fix the seed crystal at the bottom of the reactor and put Ga, Na and C chemical raw materials into the reactor;

[0024] S2, introducing high-pressure nitrogen into the furnace body, and then starting the heater to heat the reactor. After the reactor reaches a preset temperature, the driving member drives the shaft to rotate at a set speed, and the reactor revolves around the axis of the shaft driven by the shaft, the first transmission shaft and the supporting wing;

[0025] S3, while the reactor is revolving, the reactor rotates around its own axis through the rotary transmission assembly, the high-temperature melt is tilted and stirred in the reactor, and the N ions in the high-temperature melt are combined with the Ga ions to grow GaN single crystals;

[0026] S4. After the growth is completed, the heater is turned off and the reactor is cooled down, the pressure is released, and the GaN single crystal is taken out.

[0027] Compared with the prior art, the present invention has the following beneficial effects:

[0028] In the stirring device of this embodiment, the reactor can realize revolution around the axis of the rotating shaft under the drive of the rotating shaft, and at the same time, the reactor can also realize self-rotation around its own axis through the rotating transmission component. The self-rotation and revolution of the reactor can effectively improve the dissociation rate of N ions, so that N ions can be evenly distributed in the melt, which is beneficial to improve the growth rate and growth quality of GaN single crystals. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0030] Figure 1 A schematic structural diagram of a first specific embodiment of a stirring device for growing GaN single crystals by a flux method provided by the present invention;

[0031] Figure 2 A schematic structural diagram of a second specific embodiment of a stirring device for growing GaN single crystals by a flux method provided by the present invention;

[0032] Figure 3 A schematic flow chart of a method for growing GaN single crystals using a flux method provided by the present invention;

[0033] Illustrations: 1. Furnace body; 11. Heater; 12. High-temperature nitrogen; 2. Rotating shaft; 21. First transmission shaft; 211. First bearing; 22. Bracket; 221. Support wing; 222. Second bearing; 3. Reactor; 31. Air inlet channel; 32. Melt; 33. Seed crystal; 34. Second transmission shaft; 35. Third transmission shaft; 351. Transmission gear; 3511. Transmission gear teeth; 36. First ring gear; 37. Second ring gear; 4. Fixed frame; 41. Annular groove. DETAILED DESCRIPTION

[0034] The invention discloses a stirring device, a growth equipment and a growth method for growing GaN single crystal by a flux method, which are used to solve the technical problem that the stirring effect of the existing stirring device for growing GaN single crystal is poor, resulting in a low dissociation rate of N ions and failure to effectively make the N ions evenly distributed in the melt.

[0035] In order to enable those skilled in the art to better understand the scheme of the present invention, the present invention is further described in detail below in conjunction with the accompanying drawings and specific implementation methods. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0036] See also Figure 1 to Figure 2 , a stirring device for growing GaN single crystal by flux method provided in an embodiment of the present invention comprises a fixing frame 4, a rotating shaft 2, a rotating transmission assembly and a reaction kettle 3 loaded with melt 32;

[0037] The rotating shaft 2 is connected to a driving member, and the driving member is used to drive the rotating shaft 2 to rotate around its own axis. The outer side of the rotating shaft 2 is connected to at least one first transmission shaft 21, and the reactor 3 is rotatably connected to the first transmission shaft 21. The reactor 3 is provided with an air inlet channel 31 for inputting nitrogen 12. The fixed frame 4 is arranged around the rotating shaft 2, and the reactor 3 is connected to the fixed frame 4 through the rotating transmission assembly.

[0038] When the driving member drives the rotating shaft 2 to rotate, the reaction kettle 3 revolves around the axis of the rotating shaft 2, and the reaction kettle 3 rotates around its own axis through the rotating transmission component.

[0039] In the stirring device of this embodiment, the reactor 3 can realize orbital revolution around the axis of the rotating shaft 2 under the drive of the rotating shaft 2, and the reactor 3 can also realize self-rotation around its own axis through the rotating transmission component while orbiting. The self-rotation and revolution of the reactor 3 can effectively improve the dissociation rate of N ions, so that N ions can be evenly distributed in the melt 32, which is conducive to improving the growth rate and growth quality of GaN single crystals. In addition, a plurality of first transmission shafts 21 can be set on the above-mentioned rotating shaft 2, and each first transmission shaft 21 can be rotatably connected to a reactor 3, so that when the rotating shaft 2 rotates, multiple reactors 3 can realize synchronous orbital revolution and self-rotation.

[0040] In addition, in the prior art, a stirrer with a telescopic function is used to stir the melt 32. When the melt 32 in the reactor 3 rises to the required high temperature, the stirrer is driven to extend into the melt 32 for stirring. The size and telescopic accuracy of such a stirrer must be very high, and the use environment is a high temperature and high pressure environment, which places very high requirements on electromechanical equipment and is also very expensive. However, since the stirring device of this embodiment does not need to be designed with a telescopic function, the structure is simpler, the manufacturing cost is lower, and it can also adapt to high temperature and high pressure environments.

[0041] Furthermore, in this embodiment, the first transmission shaft 21 and the rotating shaft (2) are arranged at a preset inclination angle α, and the axis of the reaction kettle 3 coincides with the axis of the first transmission shaft 21.

[0042] It should be noted that, through the above design, the reactor 3 can be tilted, which can effectively promote the sliding degree of the contact interface between the substrate and the melt 32, and to a certain extent also play a role in enhancing stirring, which can further increase the dissociation rate of N ions and enable N ions to be evenly distributed in the melt 32. In addition, the above-mentioned tilt angle α needs to be selected according to the actual production process and conditions, and this embodiment does not limit this.

[0043] Furthermore, the rotating shaft 2 in this embodiment is also connected to a bracket 22, and the bracket 22 extends outward to have supporting side wings 221 that are the same in number and corresponding in position to the first transmission shaft 21;

[0044] The bottom of the reactor 3 is connected to a second transmission shaft 34, and the top of the reactor 3 is connected to a third transmission shaft 35, and the axes of the second transmission shaft 34 and the third transmission shaft 35 are both coincident with the axis of the reactor 3;

[0045] A first bearing 211 is installed at the end of the first transmission shaft 21 away from the rotating shaft 2, the second transmission shaft 34 is rotatably connected to the first bearing 211, a second bearing 222 is installed at the end of the supporting wing 221 away from the bracket 22, and the third transmission shaft 35 is rotatably connected to the second bearing 222.

[0046] It should be noted that, through the design of the above-mentioned first bearing 211 and the second bearing 222, the reactor can rotate around the first bearing 211 and the second bearing 222 without friction, which can make the reactor 3 smoother and more stable when rotating. Furthermore, in this embodiment, the smoother the first bearing 211 and the second bearing 222, the lower the friction resistance, and the smaller the resistance to the rotation of the reactor.

[0047] In addition, the above-mentioned bracket 22 and supporting wing 221 are designed because the reactor 3 is heavy and the rotating transmission assembly brings a large torque to the reactor 3. If there is no design of the bracket 22 and supporting wing 221, when the entire stirring device runs for a long time, it may cause adverse consequences such as the shaft 2 being stuck and the driving parts being damaged. Through the design of the above-mentioned bracket 22 and supporting wing 221, the reactor 3 can be driven to rotate with less torque, and the friction force when the reactor 3 rotates can be reduced, which effectively supports the reactor 3 and improves the stability of the reactor 3 when it rotates.

[0048] Furthermore, the air intake passage 31 in this embodiment extends from the inside of the reactor 3 through the third transmission shaft 35 to the outside of the reactor 3 .

[0049] It should be noted that, in the above design, the length of the air inlet channel 31 is equivalent to the length of the third transmission shaft 35 . The above design can prevent the Na—Ga steam in the reactor 3 from overflowing the reactor 3 .

[0050] Furthermore, the rotary transmission assembly in this embodiment has various structural forms, such as Figure 1 As shown, in the first specific embodiment, the rotary transmission assembly in this embodiment includes an annular groove 41 provided on the fixing frame 4 and a transmission gear 351 provided on the third transmission shaft 35;

[0051] The annular groove 41 is arranged around the fixing frame 4, and an annular gear track is arranged in the annular groove 41, and the annular gear track includes a plurality of first gear teeth arranged at intervals. The transmission gear 351 is meshed between two adjacent first gear teeth, and the spacing between two adjacent first gear teeth is the same as the gear tooth spacing on the outer side of the transmission gear 351.

[0052] It should be noted that, through the above design, when the driving member drives the rotating shaft 2 to rotate and thus drives the reactor 3 to revolve, the transmission gear 351 on the third transmission shaft 35 meshes and rotates in the annular groove 41, thereby driving the reactor 3 to revolve and rotate around itself at the same time.

[0053] like Figure 2 As shown, in the second specific implementation of this embodiment, the rotary transmission assembly in this embodiment includes a second ring gear 37 arranged on the fixing frame 4 and a first ring gear 36 arranged on the outer side wall of the reaction kettle 3;

[0054] The second ring gear 37 is disposed around the fixing frame 4 , and the first ring gear 36 is meshed with the second ring gear 37 .

[0055] It should be noted that, through the above design, when the driving member drives the rotating shaft 2 to rotate and thus drives the reactor 3 to revolve, the first ring gear 36 and the second ring gear 37 on the reactor 3 mesh and rotate, thereby driving the reactor 3 to rotate around its own axis while revolving.

[0056] Furthermore, the driving member in this embodiment is preferably a motor.

[0057] See also Figure 1 to Figure 2 , a growth device for growing GaN single crystal by flux method provided in an embodiment of the present invention comprises a furnace body 1, a heater 11 and a stirring device for growing GaN single crystal by flux method as described above;

[0058] The stirring device is installed in the furnace body 1 , and the heater 11 is arranged outside the stirring device to heat the reaction kettle 3 .

[0059] It should be noted that the heater 11 is mainly used to heat the reaction kettle 3 so that the reaction kettle 3 can reach a preset temperature.

[0060] Specifically, the heater 11 in this embodiment is a graphite heater.

[0061] In the growth device of this embodiment, the rotation and revolution of the reactor 3 can effectively increase the dissociation rate of N ions, so that the N ions can be evenly distributed in the melt 32, which is beneficial to improving the growth rate and growth quality of the GaN single crystal.

[0062] See also Figures 1 to 3 The embodiment of the present invention provides a method for growing a GaN single crystal by a flux method, which is based on the above-mentioned growth device and includes the following steps:

[0063] S1, fixing the seed crystal 33 at the bottom of the reactor 3, and putting Ga, Na, and C chemical raw materials into the reactor 3;

[0064] S2, introducing high-pressure nitrogen 12 into the furnace body 1, and then starting the heater 11 to heat the reactor 3. After the reactor 3 reaches a preset temperature, the driving member drives the shaft 2 to rotate at a set speed, and the reactor 3 revolves around the axis of the shaft 2 driven by the shaft 2, the first transmission shaft 21 and the supporting wing 221;

[0065] S3, while the reactor 3 is revolving, the reactor 3 is rotating around its own axis through the rotary transmission assembly, the high-temperature melt 32 is tilted and stirred in the reactor 3, and the N ions in the high-temperature melt 32 are combined with the Ga ions to grow a GaN single crystal;

[0066] S4. After the growth is completed, the heater 11 is turned off and the reactor 3 starts to cool down and release the pressure, and the GaN single crystal is taken out.

[0067] In the growth method of this embodiment, the rotation and revolution of the reactor 3 can effectively increase the dissociation rate of N ions, so that the N ions can be evenly distributed in the melt 32, which is beneficial to improving the growth rate and growth quality of the GaN single crystal.

[0068] The above is a detailed introduction to the stirring device, growth equipment and growth method for growing GaN single crystal by the flux method provided by the present invention. For a person skilled in the art, according to the idea of ​​the embodiment of the present invention, there may be changes in the specific implementation method and application scope. In summary, the content of this specification should not be understood as a limitation on the present invention.

Claims

1. A stirring device for growing GaN single crystal by flux method, characterized in that: It comprises a fixed frame (4), a rotating shaft (2), a rotating transmission component and a reaction kettle (3) loaded with a melt (32); The rotating shaft (2) is connected to a driving member, the driving member is used to drive the rotating shaft (2) to rotate around its own axis, the outer side of the rotating shaft (2) is connected to at least one first transmission shaft (21), the reaction kettle (3) is rotatably connected to the first transmission shaft (21), and the reaction kettle (3) is provided with an air inlet channel (31) for inputting nitrogen (12), the fixed frame (4) is arranged around the rotating shaft (2), and the reaction kettle (3) is connected to the fixed frame (4) via the rotating transmission assembly; When the driving member drives the rotating shaft (2) to rotate, the reaction kettle (3) revolves around the axis of the rotating shaft (2), and the reaction kettle (3) rotates around its own axis through the rotating transmission component.

2. The stirring device for growing GaN single crystal by flux method according to claim 1, characterized in that: The first transmission shaft (21) and the rotating shaft (2) are arranged at a preset inclination angle α, and the axis of the reaction kettle (3) coincides with the axis of the first transmission shaft (21).

3. The stirring device for growing GaN single crystal by flux method according to claim 1, characterized in that: The rotating shaft (2) is also connected to a bracket (22), and the bracket (22) has supporting side wings (221) extending outwards, the same number as the first transmission shaft (21) and corresponding in position; The bottom of the reaction kettle (3) is connected to a second transmission shaft (34), and the top of the reaction kettle (3) is connected to a third transmission shaft (35), and the axis of the second transmission shaft (34) and the axis of the third transmission shaft (35) both coincide with the axis of the reaction kettle (3); A first bearing (211) is mounted on an end of the first transmission shaft (21) away from the rotating shaft (2); the second transmission shaft (34) is rotatably connected to the first bearing (211); a second bearing (222) is mounted on an end of the supporting wing (221) away from the bracket (22); and the third transmission shaft (35) is rotatably connected to the second bearing (222).

4. The stirring device for growing GaN single crystal by flux method according to claim 3, characterized in that: The air intake passage (31) extends from the inside of the reaction kettle (3) through the third transmission shaft (35) to the outside of the reaction kettle (3).

5. The stirring device for growing GaN single crystal by flux method according to claim 3, characterized in that: The rotary transmission assembly comprises an annular groove (41) provided on the fixing frame (4) and a transmission gear (351) provided on the third transmission shaft (35); The annular groove (41) is arranged around the fixing frame (4), and an annular gear track is arranged in the annular groove (41), the annular gear track includes a plurality of first gear teeth arranged at intervals, the transmission gear (351) is meshed between two adjacent first gear teeth, and the spacing between two adjacent first gear teeth is the same as the spacing between gear teeth on the outer side of the transmission gear (351).

6. The stirring device for growing GaN single crystal by flux method according to claim 1, characterized in that: The rotary transmission assembly comprises a second ring gear (37) arranged on the fixed frame (4) and a first ring gear (36) arranged on the outer side wall of the reaction kettle (3); The second ring gear (37) is arranged around the fixing frame (4), and the first ring gear (36) is meshed with the second ring gear (37).

7. The stirring device for growing GaN single crystal by flux method according to claim 1, characterized in that: The driving member is a motor.

8. A growth device for growing GaN single crystals by a flux method, characterized in that: It comprises a furnace body (1), a heater (11) and a stirring device for growing GaN single crystal by a flux method as claimed in any one of claims 1 to 7; The stirring device is installed in the furnace body (1), and the heater (11) is arranged outside the stirring device to heat the reaction kettle (3).

9. The growth equipment for growing GaN single crystal by flux method according to claim 8, characterized in that: The heater (11) is a graphite heater.

10. A method for growing GaN single crystals by a flux method, based on the growth device according to any one of claims 8 to 9, characterized in that: The following steps are involved: S1, fixing the seed crystal (33) at the bottom of the reaction kettle (3), and putting Ga, Na, and C chemical raw materials into the reaction kettle (3); S2, introducing high-pressure nitrogen (12) into the furnace body (1), then starting the heater (11) to heat the reactor (3), and after the reactor (3) reaches a preset temperature, the driving member drives the rotating shaft (2) to rotate at a set speed, and the reactor (3) is driven by the rotating shaft (2), the first transmission shaft (21) and the supporting wing (221) to revolve around the axis of the rotating shaft (2); S3, while the reaction kettle (3) is revolving, the reaction kettle (3) is rotating around its own axis through the rotating transmission component, the high-temperature melt (32) is tilted and stirred in the reaction kettle (3), and the N ions in the high-temperature melt (32) are combined with the Ga ions to grow a GaN single crystal; S4. After the growth is completed, the heater (11) is turned off and the reaction kettle (3) starts to cool down and release the pressure, and the GaN single crystal is taken out.

Citation Information

Cited By

  • Growth device and method suitable for mass production of crystals by flux method / liquid phase method

    CN120776440A

  • Growth apparatus and method suitable for batch production of crystals by liquid phase method

    CN120776440B