Acetic acid fabric low-temperature dyeing auxiliary agent and application process thereof
By adding modified gelatin microspheres to the acetate fabric dyeing additive, the characteristics of chitosan and gelatin balls are used to solve the coloring limitations and color fastness of acetate fibers during low-temperature dyeing, and a more uniform Dyeing effect and higher color fastness.
Patent Information
- Application Number
- CN202411239520.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-05
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2044-09-05
AI Technical Summary
During the dyeing process, cellulose acetate fabrics have problems such as high color limitations, easy to produce creases and chicken claw prints on the cloth body, and the temperature control is difficult, which affects the dyeing effect and color fastness.
Use acetic acid fabric low-temperature dyeing additives, and by adding modified gelatin microspheres to the printing and dyeing additives, the coloring effect and color fixing effect of acetate fibers at lower temperatures are improved. The additives include polyoxyethylene ether polyoxyethylene ether , sodium lignin sulfonate, acetic acid, dispersant QTQ-108, porous gelatin spheres and chitosan, use chitosan to bind to the active groups on the fiber surface to adsorb dyes, improving the adsorption ability of dyes.
At lower temperatures, the dyeing efficiency and color fastness of acetate fibers are significantly improved, the occurrence of creases and chicken claw prints is reduced, and the dyeing quality and color fastness is improved.
Abstract
Description
Technical Field
[0001] The invention relates to the field of printing and dyeing auxiliaries, and in particular to an acetic acid fabric low-temperature dyeing auxiliary and an application process thereof. Background Art
[0002] Cellulose acetate fiber, commonly known as acetate fiber, is produced from wood pulp. The cellulose in it is acetylated to form a cellulose ester derivative, which is then spun by dry spinning. It is one of the earliest developed chemical fibers in the world. According to the degree to which the hydroxyl group (-OH) in the cellulose is replaced by acetyl groups, acetate fiber is divided into diacetate cellulose fiber and triacetate cellulose fiber. Cellulose acetate fiber has a soft luster, excellent antistatic properties, good moisture absorption and quick drying properties, and the characteristics of flowing fabric. It is widely used in the development of women's clothing fabrics and is deeply loved by consumers. However, cellulose acetate fiber has low strength, is not resistant to high temperatures, is not resistant to alkalis (including weak alkalis), and is not resistant to oxidants. It is difficult to print and dye, has large coloring limitations, and is prone to creases and chicken claw marks on the fabric. In the process of dyeing acetate fabrics, it is very important to control the temperature because the temperature directly affects the solubility, diffusion rate and absorption capacity of the dye by the fiber. The appropriate temperature can ensure the uniform dyeing of the dye and improve the dyeing quality and color fastness. If the temperature is too low, the dye may not be fully dissolved, resulting in uneven dyeing and low dyeing rate; while too high a temperature may cause the dye to decompose or volatilize, affecting the dyeing effect and color fastness, but too high a temperature may affect the dimensional stability and feel of the fabric. Summary of the invention
[0003] Technical problem to be solved: The purpose of the present invention is to provide an acetic acid fabric low-temperature dyeing auxiliary agent and its application process, by adding modified gelatin microspheres to the printing and dyeing auxiliary agent, the coloring effect and color fixing effect of acetate fiber dyed at a lower temperature are improved.
[0004] Technical solution: A low-temperature dyeing auxiliary for acetate fabrics, the dyeing auxiliary comprising the following ingredients: polyoxyethylene ether polyoxyethylene ether, sodium lignin sulfonate, peregal O-20, acetic acid, dispersant QTQ-108, porous gelatin balls and chitosan. Preferably, the concentrations of the dyeing and finishing auxiliaries are: polyoxyethylene ether 1.8-2.5 g / L, sodium lignin sulfonate 0.2-0.45 g / L, peregal O-20 0.05-0.1 g / L, acetic acid 5-10 g / L, dispersant QTQ-108 0.5-1.2 g / L, porous gelatin spheres 10-20 g / L, chitosan 2-5 g / L, and the molecular weight of chitosan is 2000-5000 Da. Preferably, the preparation method of the porous gelatin spheres is: S11. Degumming the silk to obtain silk fibroin fibers, and chopping the silk fibroin fibers to obtain chopped silk fibroin fibers having a length of 0.5-2 cm; S12. adding the chopped silk fibers to a formic acid solution for swelling, shearing the swollen fibers at high speed, filtering and washing to obtain nano-silk fibers; S13. Adding the nano-silk fibers to water, uniformly dispersing by ultrasonication, and obtaining a nano-silk fiber dispersion having a concentration of 2-5 wt %; S14. Adding gelatin to water, and configuring a gelatin aqueous solution having a concentration of 10-20 wt %; S15. Add calcium carbonate to the gelatin solution, stir evenly, add the nanosilk fiber dispersion prepared in step S13, stir evenly, and obtain an aqueous phase; S16. The aqueous phase was added dropwise to the oil phase of liquid paraffin and Span 80 in a volume ratio of 19:1, the volume ratio of the aqueous phase to the oil phase was 1:10, and stirred vigorously to obtain an emulsion; S17. The emulsion is placed in an ice bath, and then glutaraldehyde is added to cross-link and solidify to obtain gelatin microspheres; S18. Add gelatin microspheres to a dilute hydrochloric acid solution, heat and stir until no bubbles are generated in the solution, then stir and react for 5-10 minutes, filter, wash, and dry to obtain porous gelatin microspheres. Preferably, in step S112, the concentration of formic acid is 80-98 wt %, the shearing speed is 2000-5000 r / min, and the shearing time is 5-10 min. Preferably, in step S15, the content of calcium carbonate in the gelatin solution is 3-6wt%, and the volume ratio of the gelatin solution to the nano-silk fiber dispersion is 1:1. Preferably, in step S17, the volume ratio of glutaraldehyde to emulsion is 1-2:100. Preferably, in step S178, the concentration of dilute hydrochloric acid is 0.1-0.5 mol / L, and the heating temperature is 20-30°C. The application process of the above-mentioned low-temperature dyeing auxiliary agent for acetate fabrics comprises the following steps: S1. Pretreatment: Desizing the acetate fabric to remove oil and sizing on the surface of the fabric; S2. Dyeing treatment: Place the pre-treated acetic acid fabric in a dyeing machine, heat the water temperature to 40°C, then add anti-wrinkle agent TF-208L, leveling agent TF-212W, keep warm for 5-10 minutes, add acetic acid, keep warm for 5 minutes, add chitosan, keep warm for 5 minutes, add polyoxyethylene ether polyoxyethylene ether, sodium lignin sulfonate, peregrin O-20, dispersant QTQ-108 and porous gelatin balls, keep warm for 5 minutes, add dye, run after 10 minutes, run for 10 minutes to heat to 70°C, heating rate 1-1.5°C / min, then heat to 95°C, heating rate 0.6°C / min, run for 30-60 minutes, cool to 70°C / min, cooling rate 2°C / min; S3. post-treating the dyed acetate fiber to obtain acetate fabric. Preferably, the concentration of the anti-wrinkle agent TF-208L is 0.5-1 g / L, and the concentration of the leveling agent TF-212W is 0.5-1 g / L. Beneficial effects: The low-temperature dyeing auxiliary agent for acetic acid fabrics of the present invention has the following advantages: 1. In the present invention, the surface of the acetate fiber has hydroxyl groups that are not replaced by acetyl groups, but the content of hydroxyl groups is relatively low. Chitosan has hydroxyl groups and amino groups. Chitosan plays a dual role in the auxiliary agent. First, chitosan can combine with the active groups on the surface of the acetate fiber to combine the porous gelatin balls on the surface of the fabric in the form of a bridge. Secondly, the hydroxyl groups and amino groups of chitosan can react with the active groups in the dye, thereby improving the fastness of the dye. In the present invention, chitosan with a relatively small molecular weight is selected, and the short molecular chain of chitosan will not affect the adsorption of the porous gelatin balls on the dye; 2. In the present invention, porous gelatin balls are added to the auxiliary agent. The gelatin balls are composed of gelatin and nano-silk fibers. The porous structure of the gelatin balls can absorb more dyes, and the nano-structure of the nano-silk fibers exposes more hydroxyl and carboxyl groups on the surface. When the acetic acid fabric is dyed, the adsorption capacity of the dye molecules can be improved. The porous structure can accommodate more dye molecules faster, thereby improving the dyeing efficiency of the acetic acid fabric. DETAILED DESCRIPTION The present invention will be further described below in conjunction with embodiments, which are explanations of the present invention and are not limited to the following embodiments: Example 1 The preparation method of porous gelatin spheres is as follows: S11. Degumming the silk to obtain silk fibroin fibers, and chopping the silk fibroin fibers to obtain chopped silk fibroin fibers having a length of 0.5-2 cm; S12. The chopped silk fibers were added to a formic acid solution having a concentration of 80 wt % and swollen for 60 min, the swollen fibers were sheared at a high speed of 5000 r / min for a shearing time of 5 min, and the nano-silk fibers were filtered and washed to obtain; S13. Adding the nano-silk fibers to water, uniformly dispersing by ultrasonication, and obtaining a nano-silk fiber dispersion having a concentration of 2 wt %; S14. Adding gelatin to water to prepare a gelatin aqueous solution having a concentration of 10 wt %; S15. Calcium carbonate is added to the gelatin solution, the content of calcium carbonate in the gelatin solution is 3wt%, after stirring, the nano-silk fiber dispersion prepared in step S13 is added, the volume ratio of the gelatin solution to the nano-silk fiber dispersion is 1:1, and stirred to obtain an aqueous phase; S16. The aqueous phase was added dropwise to the oil phase of liquid paraffin and Span 80 in a volume ratio of 19:1, the volume ratio of the aqueous phase to the oil phase was 1:10, and stirred vigorously to obtain an emulsion; S17. The emulsion is placed in an ice bath, and then glutaraldehyde is added, the volume ratio of glutaraldehyde to the emulsion is 1:100, and cross-linking and curing are performed to obtain gelatin microspheres; S18. Add gelatin microspheres to a 0.1 mol / L dilute hydrochloric acid solution, heat to 20°C, stir until no bubbles are generated in the solution, and then stir and react for 10 minutes. Filter, wash, and dry to obtain porous gelatin microspheres. Example 2 The preparation method of porous gelatin spheres is as follows: S11. Degumming the silk to obtain silk fibroin fibers, and chopping the silk fibroin fibers to obtain chopped silk fibroin fibers having a length of 0.5-2 cm; S12. The chopped silk fibers were added to a 98 wt % formic acid solution for swelling for 20 min, the swollen fibers were sheared at a high speed of 2000 r / min for 10 min, and the nano-silk fibers were filtered and washed to obtain; S13. Adding the nano-silk fibers to water, uniformly dispersing by ultrasonication, and obtaining a nano-silk fiber dispersion having a concentration of 5 wt %; S14. Adding gelatin to water to prepare a gelatin aqueous solution having a concentration of 20 wt %; S15. Calcium carbonate is added to the gelatin solution, the content of calcium carbonate in the gelatin solution is 6 wt %, after stirring, the nano-silk fiber dispersion prepared in step S13 is added, the volume ratio of the gelatin solution to the nano-silk fiber dispersion is 1:1, and stirred to obtain an aqueous phase; S16. The aqueous phase was added dropwise to the oil phase of liquid paraffin and Span 80 in a volume ratio of 19:1, the volume ratio of the aqueous phase to the oil phase was 1:10, and stirred vigorously to obtain an emulsion; S17. The emulsion is placed in an ice bath, and then glutaraldehyde is added, the volume ratio of glutaraldehyde to the emulsion is 1:50, and cross-linking and curing is performed to obtain gelatin microspheres; S18. Add gelatin microspheres to a 0.5 mol / L dilute hydrochloric acid solution, heat to 30°C, stir until no bubbles are generated in the solution, and then stir and react for 5 minutes. Filter, wash, and dry to obtain porous gelatin microspheres. Example 3 The preparation method of porous gelatin spheres is as follows: S11. Degumming the silk to obtain silk fibroin fibers, and chopping the silk fibroin fibers to obtain chopped silk fibroin fibers having a length of 0.5-2 cm; S12. The chopped silk fibers were added to a 92 wt % formic acid solution for swelling for 50 min, the swollen fibers were sheared at a high speed of 4000 r / min for a shearing time of 5 min, and the nano-silk fibers were filtered and washed to obtain; S13. Adding the nano-silk fibers to water, uniformly dispersing by ultrasonication, and obtaining a nano-silk fiber dispersion having a concentration of 3 wt %; S14. Adding gelatin to water, and configuring a gelatin aqueous solution having a concentration of 13 wt %; S15. Calcium carbonate is added to the gelatin solution, the content of calcium carbonate in the gelatin solution is 5wt%, after stirring, the nano-silk fiber dispersion prepared in step S13 is added, the volume ratio of the gelatin solution to the nano-silk fiber dispersion is 1:1, and stirred to obtain an aqueous phase; S16. The aqueous phase was added dropwise to the oil phase of liquid paraffin and Span 80 in a volume ratio of 19:1, the volume ratio of the aqueous phase to the oil phase was 1:10, and stirred vigorously to obtain an emulsion; S17. The emulsion was placed in an ice bath, and then glutaraldehyde was added, the volume ratio of glutaraldehyde to the emulsion was 1.8:100, and cross-linked and cured to obtain gelatin microspheres; S18. Add gelatin microspheres to a 0.3 mol / L dilute hydrochloric acid solution, heat to 30°C, stir until no bubbles are generated in the solution, and then stir and react for 5 minutes. Filter, wash, and dry to obtain porous gelatin microspheres. Example 4 The preparation method of porous gelatin spheres is as follows: S11. Degumming the silk to obtain silk fibroin fibers, and chopping the silk fibroin fibers to obtain chopped silk fibroin fibers having a length of 0.5-2 cm; S12. The chopped silk fibers were added to a 96 wt % formic acid solution for swelling for 40 min, the swollen fibers were sheared at a high speed of 3000 r / min for 10 min, and the nano-silk fibers were filtered and washed to obtain; S13. Adding the nano-silk fibers to water, uniformly dispersing by ultrasonication, and obtaining a nano-silk fiber dispersion having a concentration of 4 wt %; S14. Adding gelatin to water, and configuring a gelatin aqueous solution having a concentration of 18 wt %; S15. Calcium carbonate is added to the gelatin solution, the content of calcium carbonate in the gelatin solution is 4 wt %, after stirring, the nano-silk fiber dispersion prepared in step S13 is added, the volume ratio of the gelatin solution to the nano-silk fiber dispersion is 1:1, and stirred to obtain an aqueous phase; S16. The aqueous phase was added dropwise to the oil phase of liquid paraffin and Span 80 in a volume ratio of 19:1, the volume ratio of the aqueous phase to the oil phase was 1:10, and stirred vigorously to obtain an emulsion; S17. The emulsion was placed in an ice bath, and then glutaraldehyde was added, the volume ratio of glutaraldehyde to the emulsion was 1.2:100, and cross-linked and cured to obtain gelatin microspheres; S18. Add gelatin microspheres to a 0.4 mol / L dilute hydrochloric acid solution, heat to 20°C, stir until no bubbles are generated in the solution, and then stir and react for 10 minutes. Filter, wash, and dry to obtain porous gelatin microspheres. Porous gelatin microspheres Example 1 365.2 Example 2 333.9 Example 3 385.1 Example 4 365.8 Example 5 The application process of low-temperature dyeing auxiliary agent for acetate fabrics includes the following steps: S1. Pretreatment: Desizing the acetate fabric to remove oil and sizing on the surface of the fabric; S2. Dyeing treatment: Place the pre-treated acetic acid fabric in a dyeing machine, heat the water temperature to 40°C, then add anti-wrinkle agent TF-208L, leveling agent TF-212W, keep warm for 5 minutes, add acetic acid, keep warm for 5 minutes, add chitosan, keep warm for 5 minutes, add polyoxyethylene polyoxyethylene ether, sodium lignin sulfonate, peregrin O-20, dispersant QTQ-108 and porous gelatin balls, keep warm for 5 minutes, add dispersed black ECT, run after 10 minutes, heat to 70°C for 10 minutes, heating rate 1°C / min, then heat to 95°C, heating rate 0.6°C / min, run for 60 minutes, cool to 70°C / min, cooling rate 2°C / min; S3. The dyed acetate fiber is post-treated to obtain acetate fabric; Among them, the anti-wrinkle agent TF-208L is 1g / L, the leveling agent TF-212W is 0.5g / L, the polyoxyethylene ether polyoxyethylene ether is 1.8g / L, the sodium lignin sulfonate is 0.45g / L, the peregrine O-20 is 0.1g / L, the acetic acid is 5g / L, the dispersant QTQ-108 is 1.2g / L, the porous gelatin spheres prepared in Example 1 are 10g / L, and the chitosan is 2g / L, and the molecular weight of the chitosan is 2000Da. Example 6 The application process of low-temperature dyeing auxiliary agent for acetate fabrics includes the following steps: S1. Pretreatment: Desizing the acetate fabric to remove oil and sizing on the surface of the fabric; S2. Dyeing treatment: Place the pre-treated acetic acid fabric in a dyeing machine, heat the water temperature to 40°C, then add anti-wrinkle agent TF-208L, leveling agent TF-212W, keep warm for 10 minutes, add acetic acid, keep warm for 5 minutes, add chitosan, keep warm for 5 minutes, add polyoxyethylene polyoxyethylene ether, sodium lignin sulfonate, Peregal O-20, dispersant QTQ-108 and porous gelatin balls, keep warm for 5 minutes, add dispersed black ECT, run after 10 minutes, heat up to 70°C for 10 minutes, heating rate 1.5°C / min, then heat up to 95°C, heating rate 0.6°C / min, run for 30 minutes, cool down to 70°C / min, cooling rate 2°C / min; S3. The dyed acetate fiber is post-treated to obtain acetate fabric; Among them, the anti-wrinkle agent TF-208L is 0.5g / L, the leveling agent TF-212W is 1g / L, the polyoxyethylene ether polyoxyethylene ether is 2.5g / L, the sodium lignin sulfonate is 0.2g / L, the peregrine O-20 is 0.05g / L, the acetic acid is 10g / L, the dispersant QTQ-108 is 0.5g / L, the porous gelatin spheres prepared in Example 2 are 20g / L, and the chitosan is 5g / L, and the molecular weight of the chitosan is 5000Da. Example 7 The application process of low-temperature dyeing auxiliary agent for acetate fabrics includes the following steps: S1. Pretreatment: Desizing the acetate fabric to remove oil and sizing on the surface of the fabric; S2. Dyeing treatment: Place the pre-treated acetic acid fabric in a dyeing machine, heat the water temperature to 40°C, then add anti-wrinkle agent TF-208L, leveling agent TF-212W, keep warm for 6 minutes, add acetic acid, keep warm for 5 minutes, add chitosan, keep warm for 5 minutes, add polyoxyethylene polyoxyethylene ether, sodium lignin sulfonate, Peregal O-20, dispersant QTQ-108 and porous gelatin balls, keep warm for 5 minutes, add dispersed black ECT, run after 10 minutes, heat up to 70°C for 10 minutes, heating rate 1°C / min, then heat up to 95°C, heating rate 0.6°C / min, run for 50 minutes, cool down to 70°C / min, cooling rate 2°C / min; S3. The dyed acetate fiber is post-treated to obtain acetate fabric; Among them, the anti-wrinkle agent TF-208L is 0.6g / L, the leveling agent TF-212W is 0.9g / L, polyoxyethylene ether polyoxyethylene ether is 2g / L, sodium lignin sulfonate is 0.25g / L, peregal O-20 is 0.06g / L, acetic acid is 6g / L, dispersant QTQ-108 is 0.8g / L, porous gelatin balls prepared in Example 3 are 13g / L, chitosan is 3g / L, and the molecular weight of chitosan is 3000Da. Example 8 The application process of low-temperature dyeing auxiliary agent for acetate fabrics includes the following steps: S1. Pretreatment: Desizing the acetate fabric to remove oil and sizing on the surface of the fabric; S2. Dyeing treatment: Place the pre-treated acetic acid fabric in a dyeing machine, heat the water temperature to 40°C, then add anti-wrinkle agent TF-208L, leveling agent TF-212W, keep warm for 9 minutes, add acetic acid, keep warm for 5 minutes, add chitosan, keep warm for 5 minutes, add polyoxyethylene polyoxyethylene ether, sodium lignin sulfonate, Peregal O-20, dispersant QTQ-108 and porous gelatin balls, keep warm for 5 minutes, add dispersed black ECT, run after 10 minutes, heat to 70°C for 10 minutes, heating rate 1.5°C / min, then heat to 95°C, heating rate 0.6°C / min, run for 40 minutes, cool to 70°C / min, cooling rate 2°C / min; S3. The dyed acetate fiber is post-treated to obtain acetate fabric; Among them, the anti-wrinkle agent TF-208L is 0.9g / L, the leveling agent TF-212W is 0.6g / L, the polyoxyethylene ether polyoxyethylene ether is 2.4g / L, the sodium lignin sulfonate is 0.4g / L, the peregrine O-20 is 0.09g / L, the acetic acid is 9g / L, the dispersant QTQ-108 is 1g / L, the porous gelatin balls prepared in Example 4 are 18g / L, and the chitosan is 4g / L, and the molecular weight of the chitosan is 4000Da. Comparative Example 1 The application process of low-temperature dyeing auxiliary agent for acetate fabrics includes the following steps: S1. Pretreatment: Desizing the acetate fabric to remove oil and sizing on the surface of the fabric; S2. Dyeing treatment: Place the pre-treated acetic acid fabric in a dyeing machine, heat the water temperature to 40°C, then add anti-wrinkle agent TF-208L, leveling agent TF-212W, keep warm for 9 minutes, add acetic acid, keep warm for 5 minutes, add chitosan, keep warm for 5 minutes, add polyoxyethylene polyoxyethylene ether, sodium lignin sulfonate, Peregal O-20, dispersant QTQ-108 and porous gelatin balls, keep warm for 5 minutes, add dispersed black ECT, run after 10 minutes, heat to 70°C for 10 minutes, heating rate 1.5°C / min, then heat to 95°C, heating rate 0.6°C / min, run for 40 minutes, cool to 70°C / min, cooling rate 2°C / min; S3. The dyed acetate fiber is post-treated to obtain acetate fabric; Among them, the anti-wrinkle agent TF-208L is 0.9g / L, the leveling agent TF-212W is 0.6g / L, the polyoxyethylene ether polyoxyethylene ether is 2.4g / L, the sodium lignin sulfonate is 0.4g / L, the peregrine O-20 is 0.09g / L, the acetic acid is 9g / L, the dispersant QTQ-108 is 1g / L, the porous gelatin balls prepared in Example 4 are 18g / L, and the chitosan is 3g / L, and the molecular weight of the chitosan is 2000Da. Comparative Example 2 The application process of low-temperature dyeing auxiliary agent for acetate fabrics includes the following steps: S1. Pretreatment: Desizing the acetate fabric to remove oil and sizing on the surface of the fabric; S2. Dyeing treatment: Place the pre-treated acetic acid fabric in a dyeing machine, heat the water temperature to 40°C, then add anti-wrinkle agent TF-208L, leveling agent TF-212W, keep warm for 9 minutes, add acetic acid, keep warm for 5 minutes, add polyoxyethylene ether polyoxyethylene ether, sodium lignin sulfonate, Peregal O-20, dispersant QTQ-108 and porous gelatin balls, keep warm for 5 minutes, add dispersed black ECT, run after 10 minutes, heat to 70°C for 10 minutes, heating rate 1.5°C / min, then heat to 95°C, heating rate 0.6°C / min, run for 40 minutes, cool to 70°C / min, cooling rate 2°C / min; S3. The dyed acetate fiber is post-treated to obtain acetate fabric; Among them, the anti-wrinkle agent TF-208L is 0.9g / L, the leveling agent TF-212W is 0.6g / L, the polyoxyethylene ether polyoxyethylene ether is 2.4g / L, the sodium lignin sulfonate is 0.4g / L, the peregrine O-20 is 0.09g / L, the acetic acid is 6g / L, the dispersant QTQ-108 is 1g / L, and the porous gelatin balls prepared in Example 4 are 18g / L. Comparative Example 3 The application process of low-temperature dyeing auxiliary agent for acetate fabrics includes the following steps: S1. Pretreatment: Desizing the acetate fabric to remove oil and sizing on the surface of the fabric; S2. Dyeing treatment: Place the pre-treated acetic acid fabric in a dyeing machine, heat the water temperature to 40°C, then add anti-wrinkle agent TF-208L, leveling agent TF-212W, keep warm for 5 minutes, add acetic acid, keep warm for 5 minutes, add chitosan, keep warm for 5 minutes, add polyoxyethylene polyoxyethylene ether, sodium lignin sulfonate, peregrin O-20, dispersant QTQ-108 and porous gelatin balls, keep warm for 5 minutes, add dispersed black ECT, run after 10 minutes, heat to 70°C for 10 minutes, heating rate 1°C / min, then heat to 95°C, heating rate 0.6°C / min, run for 60 minutes, cool to 70°C / min, cooling rate 2°C / min; S3. The dyed acetate fiber is post-treated to obtain acetate fabric; Among them, the anti-wrinkle agent TF-208L is 1g / L, the leveling agent TF-212W is 0.5g / L, polyoxyethylene polyoxyethylene ether is 1.8g / L, sodium lignin sulfonate is 0.45g / L, peregal O-20 is 0.1g / L, acetic acid is 5g / L, dispersant QTQ-108 is 1.2g / L, porous gelatin spheres are 10g / L, chitosan is 2g / L, and the molecular weight of chitosan is 3000Da; The preparation method of porous gelatin spheres is as follows: S11. Adding gelatin to water to prepare a gelatin aqueous solution having a concentration of 10 wt %; S12. Calcium carbonate is added to the gelatin solution, the content of calcium carbonate in the gelatin solution is 5wt%, and the mixture is stirred to obtain an aqueous phase; S13. The aqueous phase is added dropwise to the oil phase of liquid paraffin and Span 80 in a volume ratio of 19:1, the volume ratio of the aqueous phase to the oil phase is 1:10, and the mixture is stirred vigorously to obtain an emulsion; S14. The emulsion was placed in an ice bath, and then glutaraldehyde was added, the volume ratio of glutaraldehyde to the emulsion was 1.8:100, and cross-linked and cured to obtain gelatin microspheres; S15. Add gelatin microspheres to a 0.3 mol / L dilute hydrochloric acid solution, heat to 30°C, stir until no bubbles are generated in the solution, and then stir and react for 5 minutes. Filter, wash, and dry to obtain porous gelatin microspheres. Comparative Example 4 The application process of low-temperature dyeing auxiliary agent for acetate fabrics includes the following steps: S1. Pretreatment: Desizing the acetate fabric to remove oil and sizing on the surface of the fabric; S2. Dyeing treatment: Place the pre-treated acetic acid fabric in a dyeing machine, heat the water temperature to 40°C, then add anti-wrinkle agent TF-208L, leveling agent TF-212W, keep warm for 5 minutes, add acetic acid, keep warm for 5 minutes, add chitosan, keep warm for 5 minutes, add polyoxyethylene polyoxyethylene ether, sodium lignin sulfonate, peregrin O-20, dispersant QTQ-108 and porous gelatin balls, keep warm for 5 minutes, add dispersed black ECT, run after 10 minutes, heat to 70°C for 10 minutes, heating rate 1°C / min, then heat to 95°C, heating rate 0.6°C / min, run for 60 minutes, cool to 70°C / min, cooling rate 2°C / min; S3. The dyed acetate fiber is post-treated to obtain acetate fabric; Among them, the anti-wrinkle agent TF-208L is 1g / L, the leveling agent TF-212W is 0.5g / L, polyoxyethylene polyoxyethylene ether is 1.8g / L, sodium lignin sulfonate is 0.45g / L, peregal O-20 is 0.1g / L, acetic acid is 5g / L, dispersant QTQ-108 is 1.2g / L, porous gelatin spheres are 10g / L, chitosan is 2g / L, and the molecular weight of chitosan is 3000Da; The preparation method of porous gelatin spheres is as follows: S11. Degumming the silk to obtain silk fibroin fibers, and chopping the silk fibroin fibers to obtain chopped silk fibroin fibers having a length of 0.5-2 cm; S12. The chopped silk fibers were added to a 92 wt % formic acid solution for swelling for 50 min, the swollen fibers were sheared at a high speed of 4000 r / min for a shearing time of 5 min, and the nano-silk fibers were filtered and washed to obtain; S13. Adding the nano-silk fibers to water, uniformly dispersing by ultrasonication, and obtaining a nano-silk fiber dispersion having a concentration of 3 wt %; S14. Adding gelatin to water, and configuring a gelatin aqueous solution having a concentration of 13 wt %; S15. Calcium carbonate is added to the gelatin solution, the content of calcium carbonate in the gelatin solution is 5wt%, after stirring, the nano-silk fiber dispersion prepared in step S13 is added, the volume ratio of the gelatin solution to the nano-silk fiber dispersion is 1:1, and stirred to obtain an aqueous phase; S16. The aqueous phase was added dropwise to the oil phase of liquid paraffin and Span 80 in a volume ratio of 19:1, the volume ratio of the aqueous phase to the oil phase was 1:10, and stirred vigorously to obtain an emulsion; S17. The emulsion was placed in an ice bath, and then glutaraldehyde was added, the volume ratio of glutaraldehyde to the emulsion was 1.8:100, and cross-linked and cured to obtain gelatin microspheres; S18. Add gelatin microspheres to a 0.3 mol / L dilute hydrochloric acid solution, heat to 30°C and stir until no bubbles are generated in the solution, filter, wash and dry to obtain porous gelatin microspheres. Comparative Example 5 The application process of low-temperature dyeing auxiliary agent for acetate fabrics includes the following steps: S1. Pretreatment: Desizing the acetate fabric to remove oil and sizing on the surface of the fabric; S2. Dyeing treatment: Place the pre-treated acetic acid fabric in a dyeing machine, heat the water temperature to 40°C, then add anti-wrinkle agent TF-208L, leveling agent TF-212W, keep warm for 5 minutes, add acetic acid, keep warm for 5 minutes, add chitosan, keep warm for 5 minutes, add polyoxyethylene polyoxyethylene ether, sodium lignin sulfonate, peregrin O-20, dispersant QTQ-108 and porous gelatin balls, keep warm for 5 minutes, add dispersed black ECT, run after 10 minutes, heat to 70°C for 10 minutes, heating rate 1°C / min, then heat to 95°C, heating rate 0.6°C / min, run for 60 minutes, cool to 70°C / min, cooling rate 2°C / min; S3. The dyed acetate fiber is post-treated to obtain acetate fabric; Among them, the anti-wrinkle agent TF-208L is 1g / L, the leveling agent TF-212W is 0.5g / L, polyoxyethylene polyoxyethylene ether is 1.8g / L, sodium lignin sulfonate is 0.45g / L, peregal O-20 is 0.1g / L, acetic acid is 5g / L, dispersant QTQ-108 is 1.2g / L, porous gelatin spheres are 10g / L, chitosan is 2g / L, and the molecular weight of chitosan is 3000Da; The preparation method of porous gelatin spheres is as follows: S11. The silk fibroin powder was added to water and uniformly dispersed by ultrasonication to obtain a 3 wt % silk fibroin powder dispersion; S12. Adding gelatin to water to prepare a gelatin aqueous solution having a concentration of 13 wt %; S13. Adding calcium carbonate to the gelatin solution, the content of calcium carbonate in the gelatin solution is 5wt%, stirring evenly, adding the silk fibroin powder dispersion prepared in step S11, the volume ratio of the gelatin solution to the silk fibroin powder dispersion is 1:1, stirring evenly, and obtaining an aqueous phase; S14. The aqueous phase was added dropwise to the oil phase of liquid paraffin and Span 80 in a volume ratio of 19:1, the volume ratio of the aqueous phase to the oil phase was 1:10, and stirred vigorously to obtain an emulsion; S15. The emulsion was placed in an ice bath, and then glutaraldehyde was added, the volume ratio of glutaraldehyde to the emulsion was 1.8:100, cross-linked and cured to obtain gelatin microspheres; S16. Add gelatin microspheres to a 0.3 mol / L dilute hydrochloric acid solution, heat to 30°C and stir until no bubbles are generated in the solution, filter, wash and dry to obtain porous gelatin microspheres. Color fastness test: Color fastness to rubbing: tested according to GB / T3920-2008; Color fastness to washing: tested according to GB / T3921-2008; Color fastness to water: tested according to GB / T5713-2013. Color fastness to rubbing Dry friction / grade Wet friction / grade Example 5 5 4-5 Example 6 5 5 Example 7 5 4-5 Example 8 5 4-5 Comparative Example 1 4-5 4 Comparative Example 2 4 3-4 Comparative Example 3 3-4 3-4 Comparative Example 4 4-5 4 Comparative Example 5 4 3-4 Color fastness to washing Color change / level Hair staining / grade Cotton staining / grade Example 5 4-5 4-5 4-5 Example 6 5 4-5 4-5 Example 7 5 5 4-5 Example 8 4-5 5 4-5 Comparative Example 1 4 4 3-4 Comparative Example 2 4 3-4 4 Comparative Example 3 3-4 3-4 3-4 Comparative Example 4 4 4 4 Comparative Example 5 4 4 4 Color fastness to washing Color change / level Hair staining / grade Cotton staining / grade Example 5 4-5 5 4-5 Example 6 5 5 4-5 Example 7 4-5 4-5 5 Example 8 5 5 4-5 Comparative Example 1 4 4 4 Comparative Example 2 4 3-4 3-4 Comparative Example 3 3-4 4 3-4 Comparative Example 4 4 4-5 4 Comparative Example 5 4 4 4 Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection of the invention.
Claims
1. A low-temperature dyeing auxiliary agent for acetic acid fabrics, characterized in that: The dyeing auxiliary comprises the following ingredients: polyoxyethylene ether, sodium lignin sulfonate, peregal O-20, acetic acid, dispersant QTQ-108, porous gelatin balls and chitosan.
2. The low-temperature dyeing auxiliary agent for acetate fabric according to claim 1, characterized in that: The concentrations of the dyeing and finishing auxiliaries are: polyoxyethylene ether 1.8-2.5 g / L, sodium lignin sulfonate 0.2-0.45 g / L, peregal O-20 0.05-0.1 g / L, acetic acid 5-10 g / L, dispersant QTQ-108 0.5-1.2 g / L, porous gelatin spheres 10-20 g / L, chitosan 2-5 g / L, and the molecular weight of chitosan is 2000-5000 Da.
3. The low-temperature dyeing auxiliary agent for acetate fabric according to claim 1, characterized in that: The preparation method of the porous gelatin spheres is as follows: S11. Degumming the silk to obtain silk fibroin fibers, and chopping the silk fibroin fibers to obtain chopped silk fibroin fibers having a length of 0.5-2 cm; S12. adding the chopped silk fibers to a formic acid solution for swelling, shearing the swollen fibers at high speed, filtering and washing to obtain nano-silk fibers; S13. The nano-silk fibers are added to water and uniformly dispersed by ultrasonication to obtain a nano-silk fiber dispersion having a concentration of 2-5 wt %; S14. Adding gelatin to water to prepare a gelatin aqueous solution having a concentration of 10-20wt%; S15. Add calcium carbonate to the gelatin solution, stir evenly, add the nanosilk fiber dispersion prepared in step S13, stir evenly, and obtain an aqueous phase; S16. The aqueous phase was added dropwise to the oil phase of liquid paraffin and Span 80 in a volume ratio of 19:1, the volume ratio of the aqueous phase to the oil phase was 1:10, and stirred vigorously to obtain an emulsion; S17. The emulsion is placed in an ice bath, and then glutaraldehyde is added to cross-link and solidify to obtain gelatin microspheres; S18. Add gelatin microspheres to a dilute hydrochloric acid solution, heat and stir until no bubbles are generated in the solution, then stir and react for 5-10 minutes, filter, wash, and dry to obtain porous gelatin microspheres.
4. The low-temperature dyeing auxiliary agent for acetate fabric according to claim 3, characterized in that: In step S112, the concentration of formic acid is 80-98 wt %, the shearing speed is 2000-5000 r / min, and the shearing time is 5-10 min.
5. The low-temperature dyeing auxiliary agent for acetate fabric according to claim 3, characterized in that: In the step S15, the content of calcium carbonate in the gelatin solution is 3-6wt%, and the volume ratio of the gelatin solution to the nano-silk fiber dispersion is 1:
1.
6. The low-temperature dyeing auxiliary agent for acetate fabric according to claim 3, characterized in that: In step S17, the volume ratio of glutaraldehyde to emulsion is 1-2:
100.
7. The low-temperature dyeing auxiliary agent for acetate fabric according to claim 3, characterized in that: In step S178, the concentration of dilute hydrochloric acid is 0.1-0.5 mol / L, and the heating temperature is 20-30°C.
8. The application process of the low-temperature dyeing auxiliary agent for acetate fabrics according to any one of claims 1 to 7, characterized in that: The following steps are involved: S1. Pretreatment: Desizing the acetate fabric to remove oil and sizing on the surface of the fabric; S2. Dyeing treatment: Place the pre-treated acetic acid fabric in a dyeing machine, heat the water temperature to 40°C, then add anti-wrinkle agent TF-208L, leveling agent TF-212W, keep warm for 5-10 minutes, add acetic acid, keep warm for 5 minutes, add chitosan, keep warm for 5 minutes, add polyoxyethylene ether polyoxyethylene ether, sodium lignin sulfonate, peregrin O-20, dispersant QTQ-108 and porous gelatin balls, keep warm for 5 minutes, add dye, run after 10 minutes, run for 10 minutes to heat to 70°C, heating rate 1-1.5°C / min, then heat to 95°C, heating rate 0.6°C / min, run for 30-60 minutes, cool to 70°C / min, cooling rate 2°C / min; S3. post-treating the dyed acetate fiber to obtain acetate fabric.
9. The application process of the low-temperature dyeing auxiliary agent for acetate fabric according to claim 8, characterized in that: The concentration of the anti-wrinkle agent TF-208L is 0.5-1 g / L, and the concentration of the leveling agent TF-212W is 0.5-1 g / L.
Citation Information
Patent Citations
Temperature-controlled structural color dye, and preparation and application thereof
CN110003882A
Plant dyeing agent for triacetate fabric
CN116145440A
Preparation and application of biocompatible porous hydrogel
CN117164893A
Preparation process of high-color-fastness polyamide-polyester-spandex fabric and prepared fabric
CN118147807A