Method for determining replacement ratio of decarburized coal gas to coke of hydrogen-rich carbon cycle oxygen blast furnace

By determining the effective calorific value of CO and H2 and coke replacement ratio, and adjusting the gas composition and temperature of the furnace top, the thermal system problem of CO2 and H2O in the hydrogen-rich carbon circulating oxygen blast furnace is solved, and stable blast furnace operation and low fuel consumption are achieved. .

CN119049573APending Publication Date: 2024-11-29XINJIANG BAYI IRON & STEEL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411123194.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-15
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

In a hydrogen-rich carbon circulating oxygen blast furnace, the furnace top gas after removing CO2 still contains CO2 and H2O, which affects the replacement effect of reducing components (CO+H2) on coke, making it difficult to predict the changes in the thermal system and affects the refining Iron efficiency and fuel consumption.

Method used

By determining the effective calorific value of CO and H2 to the effective calorific value of coke, combining the volume fraction of CO2 and H2O, adjusting the composition and temperature of the furnace top gas, and calculating the displacement ratio of CO+H2 and coke, ensuring the heat balance in the furnace and Solid fuel consumption is the lowest.

Benefits of technology

It has achieved stable blast furnace conditions, reduced solid fuel consumption and carbon emissions, and improved iron smelting efficiency and production cost control.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119049573A_ABST
    Figure CN119049573A_ABST
Patent Text Reader

Abstract

The invention discloses a method for determining the replacement ratio of decarburized coal gas to coke of a hydrogen-rich carbon circulating oxygen blast furnace, which comprises the following steps: determining the sum of effective chemical heat of reductive effective components (CO + H2) after CO2 is removed from furnace top gas and physical heat of the reductive effective components (CO + H2) after heating to a certain temperature to determine the replacement relationship between the reductive effective components (CO + H2) and coke after CO2 is removed from the furnace top gas; meanwhile, according to the volume fraction of reductive effective components (CO + H2) after CO2 is removed from the injection furnace top gas, the injection amount of ton iron can be determined, the solid fuel ratio can be adjusted, the coke ratio can be determined, and the operation of the blast furnace is flexible, so that the problem that in the prior art, after CO2 is removed from decarburized gas, a small amount of CO2 and a small amount of saturated H2O are contained, and CO2, H2O and CO + H2 are injected into a blast furnace hearth at the same time, so that the production cost is reduced is solved. And CO2 and H2O react with C in coke, a certain amount of heat is consumed, and meanwhile, the replacement of the coke by reducing components (CO + H2) after CO2 is removed from the furnace top gas is influenced, so that the heat system change cannot be pre-judged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for determining the replacement ratio of decarbonized coal gas and coke in a hydrogen-rich carbon circulating oxygen blast furnace, belonging to the technical field of low-carbon hydrogen-rich carbon circulating oxygen blast furnace ironmaking. Background Art

[0002] The hydrogen-rich carbon cycle oxygen blast furnace uses oxygen blast to replace the traditional preheated air blast, and removes CO2 from the top gas for recycling. The recycling of the top gas increases the partial pressure of CO, enhances the reduction potential of the gas, strengthens the reduction of the iron-containing charge, reduces the direct reduction degree, improves the ironmaking production efficiency, reduces fuel consumption, and reduces carbon emissions. This process develops indirect reduction and reduces direct reduction. After removing CO2 from the top gas, a high concentration of reducing components (CO+H2) is produced, which are heated by the gas heating furnace and sprayed from the tuyere, making up for the thermodynamic conditions required for the physical and chemical reactions required by the blast furnace due to the full oxygen blast process of the oxygen blast furnace, the sharp reduction of N2, and the reduction of the amount of gas in the furnace. Therefore, after the CO2 is removed from the top gas circulation, the effective (CO+H2) components sprayed into the blast furnace are the key to ensuring that the hydrogen-rich carbon circulating oxygen blast furnace reduces solid fuel, especially reduces the consumption of coke. Since the decarbonized gas still contains a small amount of CO2 and a small amount of H2O after the CO2 is removed, CO2 and H2O are sprayed into the blast furnace hearth at the same time as CO+H2. CO2 and H2O will react with the C in the coke, which will consume a certain amount of heat and affect the replacement of the reducing components (CO+H2) for coke after the CO2 is removed from the top gas. Therefore, it is necessary to develop a method to determine the content of the effective reducing components (CO+H2) after the CO2 is removed from the top gas, and at the same time determine the replacement ratio of the effective components (CO+H2) for coke. Summary of the invention

[0003] The object of the present invention is to provide a method for determining the replacement ratio of hydrogen-rich carbon circulating oxygen blast furnace decarbonized coal gas and coke, by recycling the reducing components CO+H2 in the furnace top gas, a lower solid fuel consumption can be obtained, mainly a lower coke ratio and coal ratio.

[0004] The technical solution adopted by the present invention is: A method for determining the replacement ratio of hydrogen-rich carbon circulating oxygen blast furnace decarbonized coal gas to coke comprises the following steps: S1:1Nm 3 Determination of the effective calorific value of CO: The heat released by the reaction of CO and O2 to form CO2 is 283.4 kJ / mol, the utilization rate of CO is 40%, 1Nm 3 The number of moles of CO is 1000 / 22.4=44.6 mol, 1Nm 3The effective calorific value of CO is 283.4×44.6×40%=5060kJ / Nm 3 ; S2: Determine the effective calorific value of coke: specifically including the effective calorific value of C element in coke and the effective calorific value of CH4 in coke; S3: The effective calorific value of C element in specific coke: the heat released by the reaction of C and O2 to generate CO is 125.5 kJ / mol, the heat released by the reaction of CO and O2 to generate CO2 is 283.4 kJ / mol, the utilization rate of CO is 40%, the effective calorific value of 1 mol of C is 125.5 kJ / mol+283.4 kJ / mol×40%=238.96 kJ / mol, the mass fraction of C element in 1 kg of coke is 87%, the number of mols of C element in 1 kg of coke is 1×87%×1000 / 12=72.5 mol, and the effective calorific value of C element in 1 kg of coke is 72.5 mol×238.96 kJ / mol=17317.35 kJ / kg; S4: The effective calorific value of CH4 in coke is 1.16% of the CH4 mass fraction in 1kg coke volatile matter. The mass of CH4 in 1kg coke is 11.6g, and the number of moles is 11.6g÷16=0.725mol. The volume of CH4 that can be generated is 0.725mol×22.4 / 1000=0.0162Nm 3 , the calorific value of CH4 is 33440 kJ / Nm 3 The utilization rate of CH4 cracking into CO and H2 is 40%, and the effective heat of CH4 in volatile matter of 1kg coke is 0.0162Nm 3 ×33440kJ / Nm 3 ×40%=217.2 kJ / kg coke; S5: The specific effective calorific value of coke is the effective calorific value of C element in coke + the effective calorific value of CH4 in coke = 17317.35 kJ / kg + 217.2 kJ / kg = 17535 kJ / kg coke; S6: 1Nm 3 The replacement ratio of CO to coke is 5060 kJ / Nm 3 ÷17535kJ / kg=0.29kg / Nm 3 ; S7: The heat released by the reaction of H2 and O2 to generate H2O is 242 kJ / mol, and the heat released by the reaction of CO and O2 to generate CO2 is 283.4 kJ / mol. The calorific value of H2 and CO is converted to 242÷283.4=0.85 times. 3 The replacement ratio of H2 to coke can be 0.29kg / Nm 3 ×0.85=0.25kg / Nm3 ; Steps S1-S7 only determine the replacement ratio of pure CO and H2 to coke, which is the basis of a method for determining the replacement ratio of hydrogen-rich carbon cycle oxygen blast furnace decarbonization coal gas to coke. Since the coal gas after CO2 is removed from the hydrogen-rich carbon cycle oxygen blast furnace decarbonization coal gas still contains 1-3% CO2 volume fraction and 1-2% H2O volume fraction, the gas containing CO2 and H2O volume fractions is sprayed into the furnace, and the reaction with the C element in the hot coke inside the furnace is an endothermic reaction, which needs to be deducted from the heat consumed by the endothermic reaction of CO2 and H2O with C in the coke when CO2 and H2O are sprayed into the blast furnace furnace at the same time as CO+H2, and further determine the effective heat of the reducing gas such as CO+H2 sprayed into the furnace after deducting CO2 and H2O; the specific steps are as follows: S8: Select a set of volume fraction components of hydrogen-rich carbon cycle oxygen blast furnace decarbonized coal gas, the specific volume fractions of the components in the coal gas are CO%: 61.7, CO2%: 3, N2%: 29.6, H2%: 3.4, H2O%: 1.45, CH4%: 0.7, totaling 100%; S9: The heat released by the further reaction of C and O2 to generate CO is 125.5 kJ / mol, and the heat absorbed by the reaction of CO2 and C to generate CO is 166.2 kJ / mol. The calorific value of CO2 and CO is converted into 166.2÷125.5=1.32 times. The volume fraction of CO2 in S8 is 3%, and the volume fraction of CO that needs to be deducted is 1.32×3%=3.97%; S10: The heat absorbed by the further reaction of H2O and C to generate CO and H2 is 133.1 kJ / mol. The calorific value of H2O and CO is converted into 133.1÷125.5=1.06 times. The volume fraction of H2O in S8 is 1.45%, and the volume fraction of CO that needs to be deducted is 1.06×1.45%=1.54%; S11: The heat released by the further reaction of H2 and O2 to generate H2O is 242 kJ / mol, and the heat released by the reaction of CO and O2 to generate CO2 is 283.4 kJ / mol. The calorific value of H2 and CO is converted to 242÷283.4=0.85 times. The volume fraction of H2 in S8 is 3.4%, and the volume fraction of CO needs to be increased by 0.85×3.4%=2.9%; S12: Further hydrogen-rich carbon cycle oxygen blast furnace decarbonized coal gas CH4 calorific value 33440kJ / Nm 3 , the utilization rate of CH4 cracking into CO and H2 is 40%, and the volume fraction of CO needs to be increased by 0.7×33440÷5060×40%=1.7%; S13: The volume fraction of effective CO component in the further hydrogen-rich carbon cycle oxygen blast furnace decarbonized coal gas is 61.7%-3.97%-1.54%+2.9%+1.7%=60.2%; S14: Further S8 for every 1Nm 3 The volume of effective CO in the decarbonized coal gas is 0.602Nm 3 , its effective CO calorific value is 0.602×5061=3047kJ / Nm 3 Decarbonized coal gas; S15: Further decarbonized coal gas needs to be heated in a gas heating furnace to 900°C, 1000°C, 1100°C, 1150°C, and 1200°C. The heat capacity of the decarbonized coal gas of each component in S8 at each temperature is 1.423 kJ / Nm 3 ℃、1.436kJ / Nm 3 ℃、1.450kJ / Nm 3 ℃、1.456kJ / Nm 3 ℃、1.463kJ / Nm 3 ℃, the physical heat brought by the decarbonized coal gas of each component in each temperature S8 is 1280kJ / Nm 3 、1436kJ / Nm 3 、1594kJ / Nm 3 、1674kJ / Nm 3 、1755kJ / Nm 3 ; S16: Further heating to 900℃, 1000℃, 1100℃, 1150℃, 1200℃, the sum of the physical temperature of each component and the effective CO heat in S8 at each temperature is 3047+1280=4327kJ / Nm 3 、3047+1436=4483kJ / Nm 3 、3047.4+1594=4641kJ / Nm 3 、3047.4+1674=4721kJ / Nm 3 、3047.4+1755=4802kJ / Nm 3 ; S16: The replacement ratio of the sum of the physical temperature further heated to 900°C and the effective heat of CO to the effective calorific value of coke is: 4327 kJ / Nm 3 ÷17535kJ / kg=0.233kg / Nm 3 ; The replacement ratio of the sum of the physical temperature heated to 1000℃ and the effective heat of CO to the effective calorific value of coke is: 4483kJ / Nm 3÷17535kJ / kg=0.241kg / Nm 3 ; The replacement ratio of the sum of the physical temperature heated to 1100℃ and the effective heat of CO to the effective calorific value of coke is: 4641kJ / Nm 3 ÷17535kJ / kg=0.25kg / Nm 3 ; The replacement ratio of the sum of the physical temperature heated to 1150℃ and the effective heat of CO to the effective calorific value of coke is: 4721kJ / Nm 3 ÷17535kJ / kg=0.254kg / Nm 3 ; The replacement ratio of the sum of the physical temperature heated to 1200℃ and the effective heat of CO to the effective calorific value of coke is: 4802kJ / Nm 3 ÷17535kJ / kg=0.258kg / Nm 3 .

[0005] The method of the present invention is used to adjust the thermal system of a hydrogen-rich carbon-cycle oxygen blast furnace, stabilize the furnace condition of the blast furnace, and ensure stable and smooth operation of the blast furnace. The method determines the replacement relationship between the reducing effective components (CO+H2) after CO2 removal from the top gas and the coke by determining the effective heat of coke, the effective chemical heat of the reducing effective components (CO+H2) after CO2 removal from the top gas, and the sum of the physical heat after heating to a certain temperature. The method is simple and practical, and can guide the foreman of the hydrogen-rich carbon-cycle oxygen blast furnace to effectively adjust the thermal system of the hydrogen-rich carbon-cycle oxygen blast furnace to prevent the influence of fluctuations in the thermal system on the furnace condition. At the same time, it can also be adjusted according to the effective reducing components (CO+H2) after CO2 removal from the top gas. The volume fraction of the component (CO+H2) determines the injection amount per ton of iron, adjusts the solid fuel ratio, determines the coke ratio, and flexibly operates the blast furnace. It solves the problem that the existing technology still contains a small amount of CO2 in the decarbonized coal gas after CO2 is removed, and also contains a small amount of saturated H2O. CO2 and H2O are sprayed into the blast furnace hearth at the same time as CO+H2. CO2 and H2O will react with C in the coke, which will consume a certain amount of heat and affect the replacement of coke by the reducing component (CO+H2) after CO2 is removed from the top gas. The technical problem that the thermal system changes cannot be predicted.

[0006] The present invention is based on all-oxygen smelting, realizes the top gas circulation, removes CO2, and after heating, generates high-temperature reducing gas to be sprayed into the furnace, replaces the reducing agent and heating agent of coke in the solid fuel, models and calculates the effective components (CO+H2) of the reducing injection gas after removing CO2 and its effective calorific value, and also models and calculates the effective calorific value of coke, obtains the effective replacement ratio of the reducing injection gas and coke after removing CO2, calculates the influence of the reducing injection gas after removing CO2 on the coke ratio, thereby guiding production, reducing solid fuel consumption, reducing carbon emissions, and reducing molten iron costs. The present invention is simple, clear, easy to operate, and has strong practicality for technical personnel. BRIEF DESCRIPTION OF THE DRAWINGS

[0007] Figure 1 It is a schematic diagram of the process structure of the present invention. DETAILED DESCRIPTION

[0008] Reference Figure 1 The present invention is further described below by way of examples. The present invention is based on the hydrogen-rich carbon cycle oxygen blast furnace process. After the traditional blast furnace process is reconstructed, the hydrogen-rich carbon cycle oxygen blast furnace process adopts full oxygen blast. It is necessary to invent a method for determining the replacement ratio of decarbonized coal gas and coke in the hydrogen-rich carbon cycle oxygen blast furnace. Based on the hydrogen-rich carbon cycle oxygen blast furnace process adopting full oxygen blast, the process flow can be found in Figure 1 The main components of the top gas of the hydrogen-rich carbon circulating oxygen blast furnace are CO, CO2, H2, H2O, N2, and CH4. The CO2 in the gas is removed by the decarbonization device, but the decarbonization device has certain efficiency problems in removing CO2. After the top gas is removed by CO2, although the volume fraction of (CO+H2) in the gas is relatively increased by 25-30%, the gas after the decarbonization device removes CO2 still contains 1-3% of CO2 volume fraction and 1-2% of H2O volume fraction. Therefore, when adjusting the thermal system of blast furnace operation, especially when adjusting the ore-coke ratio, in order to maintain a certain heat balance of the blast furnace, it is necessary to determine the volume fraction of the reducing effective component (CO+H2) after removing CO2, that is, it is necessary to offset the CO2 and H2O that are sprayed into the blast furnace hearth at the same time as CO+H2, and CO2 and H2O will react with C in the coke to consume heat.

[0009] A method for determining the replacement ratio of hydrogen-rich carbon circulating oxygen blast furnace decarbonized coal gas to coke comprises the following steps: S1:1Nm 3 Determination of the effective calorific value of CO: The heat released by the reaction of CO and O2 to form CO2 is 283.4 kJ / mol, the utilization rate of CO is 40%, 1Nm 3 The number of moles of CO is 1000 / 22.4=44.6 mol, 1Nm 3The effective calorific value of CO is 283.4×44.6×40%=5060kJ / Nm 3 ; S2: Determine the effective calorific value of coke: specifically including the effective calorific value of C element in coke and the effective calorific value of CH4 in coke; S3: The effective calorific value of C element in specific coke: the heat released by the reaction of C and O2 to generate CO is 125.5 kJ / mol, the heat released by the reaction of CO and O2 to generate CO2 is 283.4 kJ / mol, the utilization rate of CO is 40%, the effective calorific value of 1 mol of C is 125.5 kJ / mol+283.4 kJ / mol×40%=238.96 kJ / mol, the mass fraction of C element in 1 kg of coke is 87%, the number of mols of C element in 1 kg of coke is 1×87%×1000 / 12=72.5 mol, and the effective calorific value of C element in 1 kg of coke is 72.5 mol×238.96 kJ / mol=17317.35 kJ / kg; S4: The effective calorific value of CH4 in coke is 1.16% of the CH4 mass fraction in 1kg coke volatile matter. The mass of CH4 in 1kg coke is 11.6g, and the number of moles is 11.6g÷16=0.725mol. The volume of CH4 that can be generated is 0.725mol×22.4 / 1000=0.0162Nm 3 , the calorific value of CH4 is 33440 kJ / Nm 3 The utilization rate of CH4 cracking into CO and H2 is 40%, and the effective heat of CH4 in volatile matter of 1kg coke is 0.0162Nm 3 ×33440kJ / Nm 3 ×40%=217.2 kJ / kg coke; S5: The specific effective calorific value of coke is the effective calorific value of C element in coke + the effective calorific value of CH4 in coke = 17317.35 kJ / kg + 217.2 kJ / kg = 17535 kJ / kg coke; S6: 1Nm 3 The replacement ratio of CO to coke is 5060 kJ / Nm 3 ÷17535kJ / kg=0.29kg / Nm 3 ; S7: The heat released by the reaction of H2 and O2 to generate H2O is 242 kJ / mol, and the heat released by the reaction of CO and O2 to generate CO2 is 283.4 kJ / mol. The calorific value of H2 and CO is converted to 242÷283.4=0.85 times. 3 The replacement ratio of H2 to coke can be 0.29kg / Nm 3 ×0.85=0.25kg / Nm3 ; Steps S1-S7 only determine the replacement ratio of pure CO and H2 to coke, which is the basis of a method for determining the replacement ratio of hydrogen-rich carbon cycle oxygen blast furnace decarbonization coal gas to coke. Since the coal gas after CO2 is removed from the hydrogen-rich carbon cycle oxygen blast furnace decarbonization coal gas still contains 1-3% CO2 volume fraction and 1-2% H2O volume fraction, the gas containing CO2 and H2O volume fractions is sprayed into the furnace, and the reaction with the C element in the hot coke inside the furnace is an endothermic reaction, which needs to be deducted from the heat consumed by the endothermic reaction of CO2 and H2O with C in the coke when CO2 and H2O are sprayed into the blast furnace furnace at the same time as CO+H2, and further determine the effective heat of the reducing gas such as CO+H2 sprayed into the furnace after deducting CO2 and H2O; the specific steps are as follows: S8: Select a set of volume fraction components of hydrogen-rich carbon cycle oxygen blast furnace decarbonized coal gas, the specific volume fractions of the components in the coal gas are CO%: 61.7, CO2%: 3, N2%: 29.6, H2%: 3.4, H2O%: 1.45, CH4%: 0.7, totaling 100%; S9: The heat released by the further reaction of C and O2 to generate CO is 125.5 kJ / mol, and the heat absorbed by the reaction of CO2 and C to generate CO is 166.2 kJ / mol. The calorific value of CO2 and CO is converted into 166.2÷125.5=1.32 times. The volume fraction of CO2 in S8 is 3%, and the volume fraction of CO that needs to be deducted is 1.32×3%=3.97%; S10: The heat absorbed by the further reaction of H2O and C to generate CO and H2 is 133.1 kJ / mol. The calorific value of H2O and CO is converted into 133.1÷125.5=1.06 times. The volume fraction of H2O in S8 is 1.45%, and the volume fraction of CO that needs to be deducted is 1.06×1.45%=1.54%; S11: The heat released by the further reaction of H2 and O2 to generate H2O is 242 kJ / mol, and the heat released by the reaction of CO and O2 to generate CO2 is 283.4 kJ / mol. The calorific value of H2 and CO is converted to 242÷283.4=0.85 times. The volume fraction of H2 in S8 is 3.4%, and the volume fraction of CO needs to be increased by 0.85×3.4%=2.9%; S12: Further hydrogen-rich carbon cycle oxygen blast furnace decarbonized coal gas CH4 calorific value 33440kJ / Nm 3 , the utilization rate of CH4 cracking into CO and H2 is 40%, and the volume fraction of CO needs to be increased by 0.7×33440÷5060×40%=1.7%; S13: The volume fraction of effective CO component in the further hydrogen-rich carbon cycle oxygen blast furnace decarbonized coal gas is 61.7%-3.97%-1.54%+2.9%+1.7%=60.2%; S14: Further S8 for every 1Nm 3 The volume of effective CO in the decarbonized coal gas is 0.602Nm 3 , its effective CO calorific value is 0.602×5061=3047kJ / Nm 3 Decarbonized coal gas; S15: Further decarbonized coal gas needs to be heated in a gas heating furnace to 900°C, 1000°C, 1100°C, 1150°C, and 1200°C. The heat capacity of the decarbonized coal gas of each component in S8 at each temperature is 1.423 kJ / Nm 3 ℃、1.436kJ / Nm 3 ℃、1.450kJ / Nm 3 ℃、1.456kJ / Nm 3 ℃、1.463kJ / Nm 3 ℃, the physical heat brought by the decarbonized coal gas of each component in each temperature S8 is 1280kJ / Nm 3 、1436kJ / Nm 3 、1594kJ / Nm 3 、1674kJ / Nm 3 、1755kJ / Nm 3 ; S16: Further heating to 900℃, 1000℃, 1100℃, 1150℃, 1200℃, the sum of the physical temperature of each component and the effective CO heat in S8 at each temperature is 3047+1280=4327kJ / Nm 3 、3047+1436=4483kJ / Nm 3 、3047.4+1594=4641kJ / Nm 3 、3047.4+1674=4721kJ / Nm 3 、3047.4+1755=4802kJ / Nm 3 ; S16: The replacement ratio of the sum of the physical temperature further heated to 900°C and the effective heat of CO to the effective calorific value of coke is: 4327 kJ / Nm 3 ÷17535kJ / kg=0.233kg / Nm 3 ; The replacement ratio of the sum of the physical temperature heated to 1000℃ and the effective heat of CO to the effective calorific value of coke is: 4483kJ / Nm 3÷17535kJ / kg=0.241kg / Nm 3 ; The replacement ratio of the sum of the physical temperature heated to 1100℃ and the effective heat of CO to the effective calorific value of coke is: 4641kJ / Nm 3 ÷17535kJ / kg=0.25kg / Nm 3 ; The replacement ratio of the sum of the physical temperature heated to 1150℃ and the effective heat of CO to the effective calorific value of coke is: 4721kJ / Nm 3 ÷17535kJ / kg=0.254kg / Nm 3 ; The replacement ratio of the sum of the physical temperature heated to 1200℃ and the effective heat of CO to the effective calorific value of coke is: 4802kJ / Nm 3 ÷17535kJ / kg=0.258kg / Nm 3 .

[0010] Example: Specifically, the effective components (CO+H2) of the reducing coal injection gas after the removal of CO2 and its effective calorific value are modeled and calculated. At the same time, the effective calorific value of coke is also modeled and calculated to obtain the effective replacement ratio of the reducing coal injection gas after the removal of CO2 and coke.

[0011] Step 1: Determine the volume fraction composition of the hydrogen-rich carbon cycle oxygen blast furnace decarbonized coal gas, as shown in the following table: CO CO2 N2 H2 H2O CH4 total 61.7 3 29.6 3.4 1.45 0.7 100 Step 2: 1Nm 3 The modeling and calculation of the effective calorific value of CO is shown in the following table 1Nm 3 Determination of the effective calorific value of CO: The heat released by the reaction of CO and O2 to form CO2 is 283.4 kJ / mol, the utilization rate of CO is 40%, 1Nm 3 The number of moles of CO is 1000 / 22.4=44.6 mol, 1Nm 3 The effective calorific value of CO is 283.4×44.6×40%=5060kJ / Nm 3 ; Step 3: Model and calculate the effective calorific value of C element in coke, as shown in the following table The effective calorific value of C in coke: The heat released by the reaction of C and O2 to generate CO is 125.5 kJ / mol, the heat released by the reaction of CO and O2 to generate CO2 is 283.4 kJ / mol, the utilization rate of CO is 40%, the effective calorific value of 1 mol of C is 125.5 kJ / mol+283.4 kJ / mol×40%=238.96 kJ / mol, the mass fraction of C in 1 kg of coke is 87%, the number of moles of C in 1 kg of coke is 1×87%×10 00 / 12=72.5mol, the effective calorific value of C element in 1kg coke is 72.5mol×238.96kJ / mol=17317.35kJ / kg; the effective calorific value of CH4 in coke is 1.16% of the CH4 mass fraction in 1kg coke volatile matter, the mass of CH4 in 1kg coke is 11.6g, the number of moles is 11.6g÷16=0.725mol, the volume of CH4 that can be produced is 0.725mol×22.4 / 1000=0.0162Nm 3 , the calorific value of CH4 is 33440 kJ / Nm 3 The utilization rate of CH4 cracking into CO and H2 is 40%, and the effective heat of CH4 in volatile matter of 1kg coke is 0.0162Nm 3 ×33440kJ / Nm 3 ×40%=217.2kJ / kg coke; the effective calorific value of coke is the effective calorific value of C element in coke + the effective calorific value of CH4 in coke = 17317.35kJ / kg + 217.2kJ / kg = 17535kJ / kg coke; Step 4: Modeling and calculation of the volume fraction of effective CO components in the hydrogen-rich carbon cycle oxygen blast furnace decarbonization gas, as shown in the following table Reaction heat CO2 / CO multiple Decarbonized coal gas CO2 deduction CO% CH4 equivalent CO% CO2+C=2CO,△H=166.2kJ / mol 166.2 1.32 3.97 1.7 2C+O2=2CO,△H=125.5kJ / mol 125.5 HO2 / CO ratio Decarbonized coal gas HO2 deduction CO% CO effective calorific value kJ / Nm3 (chemical heat) H2O+C=CO+H2,△H=133.1kJ / mol 133.1 1.06 1.54 3047 H2+O2=H2O,△H=242kJ / mol 242 H2 / CO multiple Decarbonized coal gas H2 equivalent CO% CO Offset and Equivalency % CO+O2=CO2,△H=283.4kJ / mol 283.4 0.85 2.9 60.2 The heat released by the reaction of C and O2 to generate CO is 125.5 kJ / mol, and the heat absorbed by the reaction of CO2 and C to generate CO is 166.2 kJ / mol. The calorific value of CO2 and CO is converted to 166.2÷125.5=1.32 times. The volume fraction of CO2 is 3%, and the volume fraction of CO that needs to be deducted is 1.32×3%=3.97%; The heat absorbed by the reaction of H2O and C to generate CO and H2 is 133.1 kJ / mol. The calorific value of H2O and CO is converted to 133.1÷125.5=1.06 times. The volume fraction of H2O is 1.45%, and the volume fraction of CO that needs to be deducted is 1.06×1.45%=1.54%; The heat released by the reaction of H2 and O2 to generate H2O is 242 kJ / mol, and the heat released by the reaction of CO and O2 to generate CO2 is 283.4 kJ / mol. The calorific value of H2 and CO is converted to 242÷283.4=0.85 times. The volume fraction of H2 is 3.4%, and the volume fraction of CO needs to be increased by 0.85×3.4%=2.9%; The calorific value of CH4 in the decarbonized coal gas of hydrogen-rich carbon cycle oxygen blast furnace is 33440kJ / Nm 3 , the utilization rate of CH4 cracking into CO and H2 is 40%, and the volume fraction of CO needs to be increased by 0.7×33440÷5060×40%=1.7%; The volume fraction of effective CO component in hydrogen-rich carbon cycle oxygen blast furnace decarbonization gas is 61.7%-3.97%-1.54%+2.9%+1.7%=60.2%; Step 5: The decarbonized coal gas is heated to 900°C, 1000°C, 1100°C, 1150°C, and 1200°C. The heat capacity of the decarbonized coal gas of each temperature and each component, the sum of the physical temperature and the effective CO heat, and the replacement ratio of the sum of the physical temperature and the effective CO heat to the effective calorific value of coke are comprehensively modeled as shown in the following table: Gas temperature ℃ CO CO2 N2 H2 H2O CH4 Average heat content of each component (kJ / Nm3℃) Physical heat input kJ CO effective calorific value kJ / Nm3 (chemical + physical) Replacement ratio kg / Nm3 900 1.400 2.19 1.38 1.321 1.68 2.59 1.423 1280 4327.8 0.233 1000 1.413 2.22 1.39 1.325 1.71 2.69 1.436 1436 4483.6 0.241 1100 1.425 2.26 1.40 1.333 1.74 2.78 1.450 1594 4641.9 0.250 1150 1.432 2.270 1.409 1.338 1.750 2.824 1.456 1674 4721.9 0.254 Decarbonized coal gas needs to be heated in a gas heating furnace to 900℃, 1000℃, 1100℃, 1150℃, and 1200℃. The heat capacity of the decarbonized coal gas of each component at each temperature is 1.423kJ / Nm 3 ℃、1.436kJ / Nm 3 ℃、1.450kJ / Nm 3 ℃、1.456kJ / Nm 3 ℃、1.463kJ / Nm 3 ℃, the physical heat brought by the decarbonized coal gas of each component at each temperature is 1280kJ / Nm 3 、1436kJ / Nm 3 、1594kJ / Nm 3 、1674kJ / Nm 3 、1755kJ / Nm 3 The sum of the physical temperature of each component and the effective CO heat is 4327 kJ / Nm 3 、4483kJ / Nm 3 、4641kJ / Nm 3 、4721kJ / Nm 3 、4802kJ / Nm 3 ; The replacement ratio of the sum of effective CO heat and the effective calorific value of coke is: 0.233kg / Nm 3 ; 0.241kg / Nm 3 ; 0.25kg / Nm 3 ; 0.254kg / Nm 3 ; 0.258kg / Nm 3 。 In a word, in a word, the present invention is based on the basis of all-oxygen smelting, realizes the top gas circulation, removes CO2, and after heating, generates high-temperature reducing gas to be sprayed into the furnace, replaces the reducing agent and heating agent of coke in solid fuel, models and calculates the effective components (CO+H2) of the reducing injection gas after removing CO2 and its effective calorific value, and also models and calculates the effective calorific value of coke, obtains the effective replacement ratio of the reducing injection gas and coke after removing CO2, and calculates the influence of the reducing injection gas after removing CO2 on the coke ratio, thereby guiding production, reducing solid fuel consumption, reducing carbon emissions, and reducing molten iron costs. The present invention is simple, clear and easy to operate, and has strong practicality for technical personnel.

[0012] To sum up, the above is only used to illustrate the technical solution of the present invention rather than to limit it. Other modifications or equivalent substitutions made to the technical solution of the present invention by ordinary technicians in this field should be included in the scope of the claims of the present invention as long as they do not depart from the spirit and scope of the technical solution of the present invention.

Claims

1. A method for determining the replacement ratio of hydrogen-rich carbon circulating oxygen blast furnace decarbonized coal gas to coke, characterized in that The following steps are included: S1:1Nm 3 Determination of the effective calorific value of CO: The heat released by the reaction of CO and O2 to form CO2 is 283.4 kJ / mol, the utilization rate of CO is 40%, 1Nm 3 The number of moles of CO is 1000 / 22.4=44.6 mol, 1Nm 3 The effective calorific value of CO is 283.4×44.6×40%=5060kJ / Nm 3 ; S2: Determine the effective calorific value of coke: specifically including the effective calorific value of C element in coke and the effective calorific value of CH4 in coke; S3: The effective calorific value of C element in specific coke: the heat released by the reaction of C and O2 to generate CO is 125.5 kJ / mol, the heat released by the reaction of CO and O2 to generate CO2 is 283.4 kJ / mol, the utilization rate of CO is 40%, the effective calorific value of 1 mol of C is 125.5 kJ / mol+283.4 kJ / mol×40%=238.96 kJ / mol, the mass fraction of C element in 1 kg of coke is 87%, the number of mols of C element in 1 kg of coke is 1×87%×1000 / 12=72.5 mol, and the effective calorific value of C element in 1 kg of coke is 72.5 mol×238.96 kJ / mol=17317.35 kJ / kg; S4: The effective calorific value of CH4 in coke is 1.16% of the CH4 mass fraction in 1kg coke volatile matter. The mass of CH4 in 1kg coke is 11.6g, and the number of moles is 11.6g÷16=0.725mol. The volume of CH4 that can be generated is 0.725mol×22.4 / 1000=0.0162Nm 3 , the calorific value of CH4 is 33440 kJ / Nm 3 The utilization rate of CH4 cracking into CO and H2 is 40%, and the effective heat of CH4 in volatile matter of 1kg coke is 0.0162Nm 3 ×33440kJ / Nm 3 ×40%=217.2 kJ / kg coke; S5: The specific effective calorific value of coke is the effective calorific value of C element in coke + the effective calorific value of CH4 in coke = 17317.35 kJ / kg + 217.2 kJ / kg = 17535 kJ / kg coke; S6: 1Nm 3 The replacement ratio of CO to coke is 5060 kJ / Nm 3 ÷17535kJ / kg=0.29kg / Nm 3 ; S7: The heat released by the reaction of H2 and O2 to generate H2O is 242 kJ / mol, and the heat released by the reaction of CO and O2 to generate CO2 is 283.4 kJ / mol. The calorific value of H2 and CO is converted to 242÷283.4=0.85 times. 3 The replacement ratio of H2 to coke can be 0.29kg / Nm 3 ×0.85=0.25kg / Nm 3 ; S8: Select a set of volume fraction components of hydrogen-rich carbon cycle oxygen blast furnace decarbonized coal gas, the specific volume fractions of the components in the coal gas are CO%: 61.7, CO2%: 3, N2%: 29.6, H2%: 3.4, H2O%: 1.45, CH4%: 0.7, totaling 100%; S9: The heat released by the further reaction of C and O2 to generate CO is 125.5 kJ / mol, and the heat absorbed by the reaction of CO2 and C to generate CO is 166.2 kJ / mol. The calorific value of CO2 and CO is converted into 166.2÷125.5=1.32 times. The volume fraction of CO2 in S8 is 3%, and the volume fraction of CO that needs to be deducted is 1.32×3%=3.97%; S10: The heat absorbed by the further reaction of H2O and C to generate CO and H2 is 133.1 kJ / mol. The calorific value of H2O and CO is converted into 133.1÷125.5=1.06 times. The volume fraction of H2O in S8 is 1.45%, and the volume fraction of CO that needs to be deducted is 1.06×1.45%=1.54%; S11: The heat released by the further reaction of H2 and O2 to generate H2O is 242 kJ / mol, and the heat released by the reaction of CO and O2 to generate CO2 is 283.4 kJ / mol. The calorific value of H2 and CO is converted to 242÷283.4=0.85 times. The volume fraction of H2 in S8 is 3.4%, and the volume fraction of CO needs to be increased by 0.85×3.4%=2.9%; S12: Further hydrogen-rich carbon cycle oxygen blast furnace decarbonized coal gas CH4 calorific value 33440kJ / Nm 3 , the utilization rate of CH4 cracking into CO and H2 is 40%, and the volume fraction of CO needs to be increased by 0.7×33440÷5060×40%=1.7%; S13: The volume fraction of effective CO component in the further hydrogen-rich carbon cycle oxygen blast furnace decarbonized coal gas is 61.7%-3.97%-1.54%+2.9%+1.7%=60.2%; S14: Further S8 for every 1Nm 3 The volume of effective CO in the decarbonized coal gas is 0.602Nm 3 , its effective CO calorific value is 0.602×5061=3047kJ / Nm 3 Decarbonized coal gas; S15: Further decarbonized coal gas needs to be heated in a gas heating furnace to 900°C, 1000°C, 1100°C, 1150°C, and 1200°C. The heat capacity of the decarbonized coal gas of each component in S8 at each temperature is 1.423 kJ / Nm 3 ℃、1.436kJ / Nm 3 ℃、1.450kJ / Nm 3 ℃、1.456kJ / Nm 3 ℃、1.463kJ / Nm 3 ℃, the physical heat brought by the decarbonized coal gas of each component in each temperature S8 is 1280kJ / Nm 3 、1436kJ / Nm 3 、1594kJ / Nm 3 、1674kJ / Nm 3 、1755kJ / Nm 3 ; S16: Further heating to 900℃, 1000℃, 1100℃, 1150℃, 1200℃, the sum of the physical temperature of each component and the effective CO heat in S8 at each temperature is 3047+1280=4327kJ / Nm 3 、3047+1436=4483kJ / Nm 3 、3047.4+1594=4641kJ / Nm 3 、3047.4+1674=4721kJ / Nm 3 、3047.4+1755=4802kJ / Nm 3 ; S17: The replacement ratio of the sum of the physical temperature further heated to 900°C and the effective heat of CO to the effective calorific value of coke is: 4327 kJ / Nm 3 ÷17535kJ / kg=0.233kg / Nm 3 ; The replacement ratio of the sum of the physical temperature heated to 1000℃ and the effective heat of CO to the effective calorific value of coke is: 4483kJ / Nm 3 ÷17535kJ / kg=0.241kg / Nm 3 ; The replacement ratio of the sum of the physical temperature heated to 1100℃ and the effective heat of CO to the effective calorific value of coke is: 4641kJ / Nm 3 ÷17535kJ / kg=0.25kg / Nm 3 ; The replacement ratio of the sum of the physical temperature heated to 1150℃ and the effective heat of CO to the effective calorific value of coke is: 4721kJ / Nm 3 ÷17535kJ / kg=0.254kg / Nm 3 ; The replacement ratio of the sum of the physical temperature heated to 1200℃ and the effective heat of CO to the effective calorific value of coke is: 4802kJ / Nm 3 ÷17535kJ / kg=0.258kg / Nm 3 .