Process method for self-alignment etching of side wall of selection tube of SONOS (Silicon Oxide Nitride Oxide Semiconductor) memory

Through the self-alignment etching process of selecting the tube side wall, the problem of large spacing between the storage tube and the selection tube in SONOS memory is solved, further miniaturization and reliability improvement of the memory is achieved, contact hole design is simplified, and suitable for mass production.

CN119049966AInactive Publication Date: 2024-11-29SHANGHAI HUALI INTEGRATED CIRCUIT CORP
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411103571.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-12
Publication Date
2024-11-29
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The gap between the storage tube and the selection tube in traditional SONOS NOR memory is large, which limits the miniaturization and reliability of the memory and cannot effectively solve the market's demand for improved integration of Flash memory devices.

Method used

The self-alignment etching process of selecting tube side walls is adopted. By depositing polysilicon layer and hard mask layer, the self-alignment etching process is used to form grooves and side walls, so as to achieve flattening and miniaturization of the selecting tube structure and simplify contact. The design of hole CT reduces the chip area.

Benefits of technology

It improves the height uniformity of the selected tube structure, provides a vertical and flat surface, simplifies the selection tube design, reduces the chip area, enhances product competitiveness, and makes the process simple and easy to control, suitable for mass production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119049966A_ABST
    Figure CN119049966A_ABST
Patent Text Reader

Abstract

The invention provides an SONOS (Silicon Oxide Nitride Oxide Semiconductor) memory selection tube side wall self-alignment etching process method, which comprises the following steps of: 1) providing a semiconductor structure which comprises a semiconductor substrate and a memory tube structure; 2) forming a side wall on the side wall of the storage tube structure, and forming a gate oxide layer on the surface of the semiconductor substrate; (3) depositing a polycrystalline silicon layer and a first hard mask layer on the surface of the semiconductor structure formed in the step (2); (4) etching the first hard mask layer and the polycrystalline silicon layer by adopting a self-alignment etching process until a groove is formed between the polycrystalline silicon layer close to the first hard mask layer at the side part and the first hard mask layer at the side part; (5) forming a second hard mask layer on the surface of the semiconductor structure formed in the step (4); and (6) etching the second hard mask layer and the polycrystalline silicon layer by adopting a self-alignment etching process to form a selection tube structure. The selection tube structure with the flat surface is formed, and the problem that the interval between an existing storage tube and an existing selection tube is large is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of semiconductor manufacturing, and in particular to a process method for self-aligned etching of side walls of a SONOS memory selection tube. Background Art

[0002] As the market's requirements for the integration of Flash memory devices continue to increase, the contradiction between the reliability of data storage in traditional Flash devices and the device's operating speed, power consumption, size, etc. has become increasingly prominent. SONOS memory has the characteristics of small unit size, low operating voltage, and compatibility with CMOS technology. Moreover, the continuous improvement of SONOS technology is driving the development of semiconductor memory towards miniaturization, high performance, large capacity, and low cost.

[0003] Traditional SONOS NOR memory generally includes CG storage tube and SG selection tube. During chip operation, SG selection tube acts as a switch for non-selected storage cells. The polysilicon gate of the storage tube and the selection tube is directly patterned by exposure and etching using a mask. However, the interval between the storage tube and the selection tube cannot be miniaturized on a large scale due to the limitation of the minimum exposure line width of photolithography. Therefore, the unit storage area is large, which is not conducive to the further miniaturization of the memory. Summary of the invention

[0004] In view of the above-mentioned shortcomings of the prior art, the purpose of the present invention is to provide a process method for self-aligned etching of the sidewalls of a SONOS memory selection tube, which is used to form a selection tube structure with a flat surface to solve the problem of large spacing between the existing storage tube and the selection tube.

[0005] To achieve the above-mentioned purpose and other related purposes, the present invention provides a process method for self-aligned etching of the sidewall of a SONOS memory selector tube, the method comprising:

[0006] Step 1) providing a semiconductor structure, which is divided into storage areas distributed at intervals and a selection area located between each of the storage areas, the semiconductor structure comprising a semiconductor substrate, storage tube structures formed on the surface of the semiconductor substrate of the storage area and arranged at intervals, wherein the interval area between each of the storage tube structures in the same storage area is a spacing area;

[0007] Step 2) forming a sidewall spacer on the sidewall of the storage tube structure, and forming a gate oxide layer on the surface of the semiconductor substrate in the spacer area and the selection area;

[0008] Step 3) depositing a polysilicon layer and a first hard mask layer on the surface of the semiconductor structure formed in step 2), wherein the polysilicon layer fills the spacer area and forms a sidewall on a side of the storage tube structure close to the selection area, and the first hard mask layer includes a top first hard mask layer covering the upper surface of the polysilicon layer and a side first hard mask layer covering the sidewall of the polysilicon layer;

[0009] Step 4) etching the first hard mask layer and the polysilicon layer using a self-aligned etching process until a groove of a preset depth is formed between the polysilicon layer close to the side first hard mask layer and the side first hard mask layer;

[0010] Step 5) forming a second hard mask layer on the surface of the semiconductor structure formed in step 4), wherein the second hard mask layer fills the groove;

[0011] Step 6) using a self-aligned etching process to etch the second hard mask layer and the polysilicon layer to remove the polysilicon layer on the surface of the storage tube structure, and forming a selection tube structure with vertical sidewalls and a flat surface on the outer side of the sidewall.

[0012] Optionally, in step 2), the method of forming a sidewall spacer on the sidewall of the storage tube structure and forming the gate oxide layer on the surface of the semiconductor substrate in the spacer area and the selection area includes:

[0013] Forming an inner oxide layer and a nitride layer on the surface of the provided semiconductor structure, wherein the nitride layer is formed on the surface of the inner oxide layer;

[0014] Etching the nitride layer and the inner oxide layer to form an initial sidewall;

[0015] An outer oxide layer is formed on the surface of the semiconductor structure having the initial side wall, wherein the outer oxide layer formed on the surface of the initial side wall and the initial side wall serve together as the side wall, and the outer oxide layer formed on the surface of the semiconductor substrate in the isolation area and the selection area serves as the gate oxide layer.

[0016] Optionally, when etching the nitride layer, the etching process adopted is dry etching.

[0017] Optionally, when etching the inner oxide layer, the etching process adopted is wet etching.

[0018] Optionally, the depth of the groove includes

[0019] Optionally, the storage tube structure includes an ONO layer, a storage polysilicon gate formed on a surface of the ONO layer, and a mask layer formed on a surface of the storage polysilicon gate.

[0020] Optionally, the material of the mask layer includes silicon oxide and / or silicon nitride.

[0021] Optionally, materials of the first hard mask layer and the second hard mask layer both include silicon oxide and / or silicon nitride.

[0022] Optionally, the width of the selection area is greater than the width of the spacing area.

[0023] Optionally, the number of the storage tube structures in each storage area is 2.

[0024] As described above, the process method for self-aligned etching of the sidewall of the SONOS memory selection tube of the present invention adopts two deposition and two etching processes when forming the selection tube structure, and forms a groove by the first etching, and forms a thicker morphology structure at the groove when the hard mask layer is deposited for the second time, and obtains a selection tube structure with vertical sidewalls and flat surface by using the morphology structure during the second etching, so as to achieve further miniaturization of the memory. The above method can improve the uniformity of the height of the selection tube structure, provide a vertical and flat surface for the subsequent lead-out contact hole CT on the selection tube, increase the CT etching window, and the above method can greatly simplify the design of the pickup area of ​​the selection tube, further reduce the chip area, and improve the product competitiveness; further, the process manufacturing flow of the above method is simple and easy to control, and is suitable for mass production. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figures 1 to 8 It is a schematic cross-sectional structure diagram showing the process of forming the select gate of the present invention.

[0026] Fig. 9 The flowchart of the process method of self-aligned etching of the sidewall of the selector tube of the SONOS memory of the present invention is shown.

[0027] Description of Figure Numbers

[0028] 10: semiconductor structure; 11: semiconductor substrate; 12: storage tube structure; 121: ONO layer; 122: storage polysilicon gate; 123: mask layer; 20: sidewall; 21: inner oxide layer; 22: nitride layer; 30: gate oxide layer; 40: polysilicon layer; 51: first hard mask layer; 51a: top first hard mask layer; 51b: side first hard mask layer; 52: second hard mask layer; 60: groove; 70: selection tube structure DETAILED DESCRIPTION

[0029] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.

[0030] See also Figures 1 to 9 It should be noted that the illustrations provided in this embodiment are only schematic illustrations of the basic concept of the present invention. Although the illustrations only show components related to the present invention and are not drawn according to the number, shape and size of components in actual implementation, the form, quantity and proportion of each component in actual implementation may be changed arbitrarily, and the component layout may also be more complicated.

[0031] like Fig. 9 As shown, this embodiment provides a process method for self-aligned etching of the sidewall of a SONOS memory selection tube, the method comprising:

[0032] Step 1) providing a semiconductor structure 10, which is divided into storage areas A distributed at intervals and a selection area B located between each of the storage areas A, the semiconductor structure 10 includes a semiconductor substrate 11, and storage tube structures 12 formed on the surface of the semiconductor substrate 11 of the storage area A and arranged at intervals, wherein the interval area between each of the storage tube structures 12 of the same storage area A is a spacing area;

[0033] Step 2) forming a spacer 20 on the sidewall of the storage tube structure 12, and forming a gate oxide layer 30 on the surface of the semiconductor substrate 11 in the spacer area and the selection area B;

[0034] Step 3) depositing a polysilicon layer 40 and a first hard mask layer 51 on the surface of the semiconductor structure formed in step 2), wherein the polysilicon layer 40 fills the spacer area and forms a sidewall on the side of the storage tube structure 12 close to the selection area B, and the first hard mask layer 51 includes a top first hard mask layer 51a covering the upper surface of the polysilicon layer 40 and a side first hard mask layer 51b covering the sidewall of the polysilicon layer 40;

[0035] Step 4) etching the first hard mask layer 51 and the polysilicon layer 40 using a self-aligned etching process until a groove 60 of a preset depth is formed between the polysilicon layer 40 near the side first hard mask layer 51 b and the side first hard mask layer 51 b;

[0036] Step 5) forming a second hard mask layer 52 on the surface of the semiconductor structure formed in step 4), wherein the second hard mask layer 52 fills the groove 60;

[0037] Step 6) The second hard mask layer 52 and the polysilicon layer 40 are etched by a self-aligned etching process to remove the polysilicon layer 40 on the surface of the storage tube structure 12 and form a selection tube structure 70 with vertical sidewalls and a flat surface on the outer side of the sidewall 20 .

[0038] The following is combined with Figures 1 to 8 The process method for self-aligned etching of the sidewall of the SONOS memory selector provided in this embodiment is described in detail.

[0039] like Figure 1 As shown, in step 1), a semiconductor structure 10 is provided, which is divided into storage areas A distributed at intervals and selection areas B located in the area between each of the storage areas A. The semiconductor structure 10 includes a semiconductor substrate 11, and storage tube structures 12 formed on the surface of the semiconductor substrate 11 of the storage area A and arranged at intervals, wherein the interval area between each of the storage tube structures 12 of the same storage area A is a interval area.

[0040] In this embodiment, the semiconductor substrate 11 is a silicon substrate or a germanium substrate.

[0041] Specifically, the width of the selection area B is greater than the width of the spacing area.

[0042] Specifically, the number of the storage tube structures in each storage area A is 2.

[0043] Specifically, the storage tube structure 12 includes an ONO layer 121 , a storage polysilicon gate 122 formed on a surface of the ONO layer 121 , and a mask layer 123 formed on a surface of the storage polysilicon gate 122 .

[0044] More specifically, the material of the mask layer 123 includes silicon oxide and / or silicon nitride.

[0045] like Figure 4 In step 2), a spacer 20 is formed on the sidewall of the storage tube structure 12, and a gate oxide layer 30 is formed on the surface of the semiconductor substrate 11 in the spacer region and the selection region B.

[0046] In this embodiment, the side wall 20 serves as an intermediate isolation layer between the storage tube and the selection tube. The existence of the side wall can reduce the distance between the storage tube and the selection tube, so that the memory can be further miniaturized.

[0047] Specifically, Figure 2 and Figure 3 As shown, in step 2), the method of forming the sidewall 20 on the sidewall of the storage tube structure 12 and forming the gate oxide layer 30 on the surface of the semiconductor substrate 11 in the spacer area and the selection area B includes:

[0048] An inner oxide layer 21 and a nitride layer 22 are formed on the surface of the provided semiconductor structure, and the nitride layer 22 is formed on the surface of the inner oxide layer 21; the nitride layer 22 and the inner oxide layer 21 are etched to form an initial side wall; an outer oxide layer is formed on the surface of the semiconductor structure with the initial side wall, wherein the outer oxide layer formed on the surface of the initial side wall and the initial side wall together serve as the side wall 20, and the outer oxide layer formed on the surface of the semiconductor substrate 11 in the isolation area and the selection area B serves as the gate oxide layer 30.

[0049] In this embodiment, the process for forming the gate oxide layer 30 includes one of ISSG, LPRO, RTO, furnace, etc., and may also be a growth method in which different processes are superimposed.

[0050] Specifically, when etching the nitride layer 22 , the etching process adopted is dry etching.

[0051] In this embodiment, when etching the nitride layer 22, the inner oxide layer 21 serves as an etching stop layer. The material of the nitride layer 22 includes silicon nitride.

[0052] Specifically, when etching the inner oxide layer 21 , the etching process adopted is wet etching.

[0053] In this embodiment, the material of the inner oxide layer 21 includes silicon dioxide.

[0054] like Figure 5 As shown, in step 3), a polysilicon layer 40 and a first hard mask layer 51 are deposited on the surface of the semiconductor structure formed by step 2), wherein the polysilicon layer 40 fills the spacer area and a sidewall is formed on the side of the storage tube structure close to the selection area B, and the first hard mask layer 51 includes a top first hard mask layer 51a covering the upper surface of the polysilicon layer 40 and a side first hard mask layer 51b covering the sidewall of the polysilicon layer 40.

[0055] In this embodiment, the polysilicon layer formed in the same storage area forms a higher sidewall on the side of the storage tube structure close to the selection area, and the polysilicon layer between the sidewalls is relatively flat. In this embodiment, the material of the first hard mask layer 51 is silicon nitride.

[0056] like Figure 6 As shown, in step 4), the first hard mask layer 51 and the polysilicon layer 40 are etched by a self-aligned etching process until a groove 60 of a preset depth is formed between the polysilicon layer 40 and the side first hard mask layer 51b near the side first hard mask layer 51b.

[0057] Specifically, the depth of the groove 60 includes

[0058] like Figure 7 As shown, in step 5), a second hard mask layer 52 is formed on the surface of the semiconductor structure formed in step 4), wherein the second hard mask layer 52 fills the groove 60.

[0059] In this embodiment, the thickness of the second hard mask layer 52 includes

[0060] like Figure 8 As shown, in step 6), the second hard mask layer 52 and the polysilicon layer 40 are etched by a self-aligned etching process to remove the polysilicon layer 40 on the surface of the storage tube structure 12, and a selection tube structure 70 with vertical sidewalls and a flat surface is formed on the outer side of the sidewall 20.

[0061] Specifically, the materials of the first hard mask layer 51 and the second hard mask layer 52 both include silicon oxide and / or silicon nitride.

[0062] In this embodiment, the material of the second hard mask layer 52 is silicon nitride.

[0063] In summary, the process method for self-aligned etching of the sidewall of the SONOS memory selection tube of the present invention adopts two deposition and two etching processes when forming the selection tube structure, and forms a groove by the first etching, and forms a thicker morphology structure at the groove when the hard mask layer is deposited for the second time, and the selection tube structure with vertical sidewalls and flat surface is obtained by utilizing the morphology structure during the second etching, so as to achieve further miniaturization of the memory. The above method can improve the uniformity of the height of the selection tube structure, provide a vertical and flat surface for the subsequent lead-out contact hole CT on the selection tube, increase the CT etching window, and the above method can greatly simplify the design of the pickup area of ​​the selection tube, further reduce the chip area, and enhance the competitiveness of the product; further, the process manufacturing process of the above method is simple and easy to control, and is suitable for mass production. Therefore, the present invention effectively overcomes the various shortcomings of the prior art and has a high industrial utilization value.

[0064] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A process method for self-aligned etching of the sidewall of a SONOS memory selector tube, characterized in that: The method comprises: Step 1) providing a semiconductor structure, which is divided into storage areas distributed at intervals and a selection area located between each of the storage areas, the semiconductor structure comprising a semiconductor substrate, storage tube structures formed on the surface of the semiconductor substrate of the storage area and arranged at intervals, wherein the interval area between each of the storage tube structures in the same storage area is a spacing area; Step 2) forming a sidewall spacer on the sidewall of the storage tube structure, and forming a gate oxide layer on the surface of the semiconductor substrate in the spacer area and the selection area; Step 3) depositing a polysilicon layer and a first hard mask layer on the surface of the semiconductor structure formed in step 2), wherein the polysilicon layer fills the spacer area and forms a sidewall on a side of the storage tube structure close to the selection area, and the first hard mask layer includes a top first hard mask layer covering the upper surface of the polysilicon layer and a side first hard mask layer covering the sidewall of the polysilicon layer; Step 4) etching the first hard mask layer and the polysilicon layer using a self-aligned etching process until a groove of a preset depth is formed between the polysilicon layer close to the side first hard mask layer and the side first hard mask layer; Step 5) forming a second hard mask layer on the surface of the semiconductor structure formed in step 4), wherein the second hard mask layer fills the groove; Step 6) using a self-aligned etching process to etch the second hard mask layer and the polysilicon layer to remove the polysilicon layer on the surface of the storage tube structure, and forming a selection tube structure with vertical sidewalls and a flat surface on the outer side of the sidewall.

2. The process method for self-aligned etching of the sidewall of the SONOS memory selection tube according to claim 1, characterized in that: In step 2), the method of forming a sidewall on the sidewall of the storage tube structure and forming the gate oxide layer on the surface of the semiconductor substrate in the spacer area and the selection area includes: Forming an inner oxide layer and a nitride layer on the surface of the provided semiconductor structure, wherein the nitride layer is formed on the surface of the inner oxide layer; Etching the nitride layer and the inner oxide layer to form an initial sidewall; An outer oxide layer is formed on the surface of the semiconductor structure having the initial side wall, wherein the outer oxide layer formed on the surface of the initial side wall and the initial side wall serve together as the side wall, and the outer oxide layer formed on the surface of the semiconductor substrate in the isolation area and the selection area serves as the gate oxide layer.

3. The process method for self-aligned etching of the sidewall of the SONOS memory selection tube according to claim 2, characterized in that: When etching the nitride layer, the etching process adopted is dry etching.

4. The process method for self-aligned etching of the sidewall of a SONOS memory selector tube according to claim 2 or 3, characterized in that: When etching the inner oxide layer, the etching process adopted is wet etching.

5. The process method for self-aligned etching of the sidewall of the SONOS memory selection tube according to claim 1, characterized in that: The depth of the groove includes 6. The process method for self-aligned etching of the sidewall of a SONOS memory selector according to claim 1, characterized in that: The storage tube structure includes an ONO layer, a storage polysilicon gate formed on the surface of the ONO layer, and a mask layer formed on the surface of the storage polysilicon gate.

7. The process method for self-aligned etching of the sidewall of the SONOS memory selection tube according to claim 6, characterized in that: The material of the mask layer includes silicon oxide and / or silicon nitride.

8. The process method for self-aligned etching of sidewalls of a SONOS memory selector tube according to claim 1, characterized in that: The materials of the first hard mask layer and the second hard mask layer both include silicon oxide and / or silicon nitride.

9. The process method for self-aligned etching of sidewalls of a SONOS memory selector tube according to claim 1, characterized in that: The width of the selection area is greater than the width of the spacing area.

10. The process method for self-aligned etching of sidewalls of a SONOS memory selector tube according to claim 1, characterized in that: The number of the storage pipe structures in each storage area is 2.

Citation Information

Patent Citations

  • Split Gate Flash Memory Structure with a Damage Free Select Gate and a Method of Making the Split Gate Flash Memory Structure

    CN105206612A

  • Memory Cell and Manufacturing Method Thereof

    US20150270277A1

  • Memory gate first approach to forming a split gate flash memory cell device

    US9257571B1