Semiconductor structure and forming method thereof
By forming an opening in the bonding region of the semiconductor structure and increasing the vertical bonding force at the interface between the welding pad layer and the metallization layer under the bump, the bonding of the welding pad layer and the metallization layer under the bump in the prior art is solved. The problem of insufficient strength improves the performance and reliability of semiconductor structures.
Patent Information
- Application Number
- CN202310620913.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-29
- Publication Date
- 2024-11-29
AI Technical Summary
In the packaging process of existing semiconductor structures, the bonding force between the welding pad layer and the metallization layer under the bumps has only a horizontal interface, resulting in insufficient bonding force under thermal stress, increasing the risk of layering or gaps, and affecting performance.
An opening through the passivation layer is formed in the bonding region of the semiconductor structure, and a welding pad layer is formed in the opening, so that the welding pad layer is higher than the welding pad layer in the opening, and a convex is formed on the top and side walls of the welding pad layer. The metallization layer is made to ensure that its interface with the pad layer includes horizontal and vertical bonding forces.
By increasing the bonding force between the solder pad layer and the metallization layer under the bump, the risk of layering or gaps is reduced, and the performance and reliability of the semiconductor structure are improved.
Smart Images

Figure CN119050080A_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present invention relate to the field of semiconductor manufacturing, and in particular to a semiconductor structure and a method for forming the same. Background Art
[0002] With the continuous development of micro-nano technology, people have been increasing the number of transistors per unit area of the chip by continuously reducing the feature size, thereby greatly improving the performance and integration of the chip. However, it is becoming increasingly difficult to reduce the current process line width, and three-dimensional electronic packaging will be the best choice to further improve the integration density of chip functions.
[0003] Three-dimensional electronic packaging can effectively solve many thorny problems in the current semiconductor industry, such as heterogeneous integration, reducing power consumption, size, delay and cost, etc. Three-dimensional electronic packaging stacks multiple layers of interconnected vertical layers together through high-density vertical silicon vias, and can also stack multiple layers of chips that are incompatible with multiple processes together to achieve low-cost, low-parasitic integration. Summary of the invention
[0004] The problem solved by the embodiments of the present invention is to provide a semiconductor structure and a method for forming the same, which is beneficial to further improve the performance of the semiconductor structure.
[0005] To solve the above problems, an embodiment of the present invention provides a semiconductor structure, including: a first wafer, the first wafer including a bonding area; a first passivation layer protruding from the top of the first wafer; an opening located in the first passivation layer in the bonding area; a pad layer located in the opening and on the top of the first passivation layer, and the pad layer located on the top of the first passivation layer is higher than the pad layer located in the opening; an under-bump metallization layer located on the top and side walls of the pad layer; and a conductive bump covering the under-bump metallization layer.
[0006] Optionally, the shape of the opening is the same as the shape of the first passivation layer located in the bonding area.
[0007] Optionally, the shape of the opening includes one or more of a square, an inverted trapezoid and an inverted pyramid; the shape of the first passivation layer located in the bonding area includes one or more of a square, a trapezoid and a pyramid.
[0008] Optionally, the material of the pad layer includes aluminum.
[0009] Optionally, the semiconductor structure further includes: a second passivation layer located on the top of the first passivation layer at the side of the bonding area; and the under bump metallization layer also covers the sidewalls and the top of the second passivation layer.
[0010] Optionally, the material of the second passivation layer includes one or more of silicon nitride, silicon carbide and silicon oxynitride.
[0011] Optionally, the material of the conductive bump includes one or more of copper, nickel and tin.
[0012] Optionally, with the direction perpendicular to the sidewall of the opening as the lateral direction, the lateral dimension of the opening is 2 microns to 5 microns.
[0013] Correspondingly, an embodiment of the present invention also provides a method for forming a semiconductor structure, comprising: providing a first wafer, the first wafer comprising a bonding area, and a first passivation layer formed on the first wafer; forming one or more openings penetrating the first passivation layer in the bonding area, and the remaining first passivation layer protrudes from the top of the first wafer; forming a pad layer in the opening and on the top of the first passivation layer, and the pad layer located on the top of the first passivation layer is higher than the pad layer located in the opening; forming an under-bump metallization layer on the top and sidewalls of the pad layer; and forming a conductive bump covering the under-bump metallization layer.
[0014] Optionally, the step of forming one or more openings penetrating the first passivation layer in the bonding area includes: forming a mask layer having one or more mask openings on top of the first passivation layer, the mask opening being located on the top of the first passivation layer in the bonding area; using the mask layer as a mask, patterning the first passivation layer to form one or more openings penetrating the first passivation layer in the bonding area; and removing the mask layer.
[0015] Optionally, the process of forming one or more openings penetrating the first passivation layer in the bonding area includes a dry etching process.
[0016] Optionally, with the direction perpendicular to the sidewall of the opening as the lateral direction, the lateral dimension of the opening is 2 microns to 5 microns.
[0017] Optionally, the shape of the opening is the same as the shape of the first passivation layer located in the bonding area.
[0018] Optionally, the shape of the opening includes one or more of a square, an inverted trapezoid and an inverted pyramid; the shape of the first passivation layer located in the bonding area includes one or more of a square, a trapezoid and a pyramid.
[0019] Optionally, the process of forming the pad layer includes a sputtering process.
[0020] Optionally, after forming the pad layer and before forming the under-bump metallization layer, it also includes: forming a second passivation layer on top of the first passivation layer on the side of the bonding area; during the process of forming the under-bump metallization layer, the under-bump metallization layer also covers the side walls and top of the second passivation layer.
[0021] Optionally, the material of the second passivation layer includes one or more of silicon nitride, silicon carbide and silicon oxynitride.
[0022] Optionally, the process of forming the under bump metallization layer includes a physical vapor deposition process.
[0023] Optionally, the process of forming the conductive bump includes an electroplating process.
[0024] Compared with the prior art, the technical solution of the embodiment of the present invention has the following advantages:
[0025] An embodiment of the present invention provides a method for forming a semiconductor structure, wherein one or more openings penetrating the first passivation layer are formed in the bonding area, the remaining first passivation layer protrudes from the top of the first wafer, a pad layer is formed in the opening and on the top of the first passivation layer, the pad layer located on the top of the first passivation layer is higher than the pad layer located in the opening, and an under-bump metallization layer is formed on the top and sidewall of the pad layer, that is, the interface between the under-bump metallization layer and the pad layer includes the interface between the under-bump metallization layer and the pad layer in the horizontal direction, and the under-bump metallization layer. Compared with the existing solution in which the metallization layer under the bump and the pad layer have only a horizontal interface, the embodiment of the present invention provides an interface between the metallization layer under the bump and the pad layer in the vertical direction, so that the bonding force between the metallization layer under the bump and the pad layer includes a horizontal bonding force and a vertical bonding force, thereby increasing the bonding force between the metallization layer under the bump and the pad layer, reducing the risk of delamination or gaps between the metallization layer under the bump and the pad layer, and thus improving the performance of the semiconductor structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0026] Figure 1 It is a structural schematic diagram corresponding to a semiconductor structure;
[0027] Figure 2 is a schematic structural diagram of an embodiment of a semiconductor structure of the present invention;
[0028] Figures 3 to 8 It is a schematic structural diagram corresponding to each step in an embodiment of a method for forming a semiconductor structure of the present invention. DETAILED DESCRIPTION
[0029] At present, the performance of semiconductor structures still needs to be improved. Now we analyze the reasons why the performance needs to be improved by combining a semiconductor structure.
[0030] Figure 1 It is a structural schematic diagram corresponding to a semiconductor structure.
[0031] The semiconductor structure includes: a first wafer 10, the first wafer includes a bonding area 10A; a first passivation layer 11 protruding from the top of the first wafer 10; a pad layer 15 located on the top of the first passivation layer 11; a second passivation layer 17 located on the top of the pad layer 15 on the side of the bonding area 10A; an under bump metallization layer 21 located on the top of the pad layer 15 and the top and sidewalls of the second passivation layer 17; and a conductive bump 16 covering the under bump metallization layer 21.
[0032] Research has found that after the first wafer 10 and the circuit board are packaged, the pad layer 15 and the under bump metallization layer 21 are easily affected by thermal stress. Since the pad layer 15 and the under bump metallization layer 21 only have a horizontal interface, that is, the pad layer 15 and the under bump metallization layer 21 only have a horizontal bonding force, the horizontal bonding force between the pad layer 15 and the under bump metallization layer 21 is smaller than the thermal stress, thereby increasing the risk of delamination or gaps between the pad layer 15 and the under bump metallization layer 21, thereby affecting the performance of the semiconductor structure.
[0033] In order to solve the technical problem, an embodiment of the present invention provides a method for forming a semiconductor structure, including: providing a first wafer, the first wafer including a bonding area, and a first passivation layer formed on the first wafer; forming one or more openings penetrating the first passivation layer in the bonding area, and the remaining first passivation layer protrudes from the top of the first wafer; forming a pad layer in the opening and on the top of the first passivation layer, the pad layer located on the top of the first passivation layer is higher than the pad layer located in the opening; forming an under-bump metallization layer on the top and sidewalls of the pad layer; and forming a conductive bump covering the under-bump metallization layer.
[0034] An embodiment of the present invention provides a method for forming a semiconductor structure, wherein an under-bump metallization layer and a pad layer include an interface in a horizontal direction and an interface in a vertical direction, so that the bonding force between the under-bump metallization layer and the pad layer includes a bonding force in a horizontal direction and a bonding force in a vertical direction, thereby increasing the bonding force between the under-bump metallization layer and the pad layer, reducing the risk of delamination or gaps between the under-bump metallization layer and the pad layer, and thus improving the performance of the semiconductor structure.
[0035] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0036] Figure 2 It is a schematic structural diagram of an embodiment of a semiconductor structure of the present invention.
[0037] The semiconductor structure includes: a first wafer 200, the first wafer 200 includes a bonding area 200A; a first passivation layer 201 protruding from the top of the first wafer 200; an opening (not marked) located in the first passivation layer 201 in the bonding area 200A; a pad layer 205 located in the opening and on the top of the first passivation layer 201, and the pad layer 205 located on the top of the first passivation layer 201 is higher than the pad layer 205 located in the opening; an under bump metallization layer 210 located on the top and sidewalls of the pad layer 205; and a conductive bump 216 covering the under bump metallization layer 210.
[0038] By setting the pad layer 205 located on the top of the first passivation layer 201 to be higher than the pad layer 205 located in the opening, in the formation process of the under bump metallization layer 210, the under bump metallization layer 210 and the pad layer 205 include a horizontal interface and a vertical interface, so that the bonding force between the under bump metallization layer 210 and the pad layer 205 includes a horizontal bonding force and a vertical bonding force, thereby increasing the bonding force between the under bump metallization layer 210 and the pad layer 205, reducing the risk of delamination or gaps between the under bump metallization layer 210 and the pad layer 205, thereby improving the performance of the semiconductor structure.
[0039] Specifically, the first wafer 200 provides a process platform for the formation process of the semiconductor structure.
[0040] The first wafer 200 is a finished wafer, and the first wafer 200 can be manufactured using integrated circuit manufacturing technology.
[0041] In this embodiment, the first wafer 200 includes a substrate (not shown) and a dielectric layer (not shown) located on the substrate.
[0042] The substrate is a silicon substrate. In other embodiments, the material of the substrate may also be other materials such as germanium, silicon germanium, silicon carbide, gallium arsenide or indium gallium, and the substrate may also be other types of substrates such as a silicon substrate on an insulator or a germanium substrate on an insulator. The material of the substrate may be a material suitable for process requirements or easy to integrate.
[0043] It should be noted that the dielectric layer is used to electrically isolate the interconnection structure (not shown) disposed in the dielectric layer.
[0044] In this embodiment, the material of the dielectric layer is a dielectric material, and the material of the dielectric layer includes one or more of silicon oxide, tetraethyl orthosilicate, polyethylene oxide, silicon nitride and silicon carbide.
[0045] Specifically, silicon oxide, tetraethyl orthosilicate, polyethylene oxide, silicon nitride and silicon carbide nitride are all dielectric materials that can play a good role in electrically isolating adjacent interconnect structures.
[0046] In this embodiment, the bonding area 200A is a region where a pad layer 205 and an under bump metallization layer 210 are disposed.
[0047] Specifically, the first passivation layer 201 protects the top of the first wafer 200, and reduces the probability of damage to the first wafer 200 on the side of the bonding area 200A during the subsequent formation of the pad layer 205 and the under bump metallization layer 210, thereby improving the performance of the semiconductor structure.
[0048] In this embodiment, the material of the first passivation layer 201 includes one or more of silicon nitride, silicon carbide and silicon oxynitride.
[0049] It should be noted that the opening provides a space for setting the pad layer 205 .
[0050] It should also be noted that by forming one or more openings penetrating the first passivation layer 201, in the process of forming the pad layer 205, the top surface of the pad layer 205 located in the opening can be made lower than the top surface of the pad layer 205 located on the top of the first passivation layer 201. After the under bump metallization layer 210 is set in the opening, the interface between the under bump metallization layer 210 and the pad layer 205 can include the interface between the under bump metallization layer 210 and the pad layer 205 in the horizontal direction, and the interface between the under bump metallization layer 210 and the pad layer 205 in the vertical direction, that is, the bonding force between the under bump metallization layer 210 and the pad layer 205 includes the bonding force in the horizontal direction and the bonding force in the vertical direction, which increases the bonding force between the under bump metallization layer 210 and the pad layer 205 and reduces the risk of delamination or gaps between the under bump metallization layer 210 and the pad layer 205.
[0051] Specifically, taking the direction perpendicular to the side wall of the opening as the lateral direction, the lateral dimension of the opening should not be too large or too small. If the lateral dimension of the opening is too small, it is easy to cause the aspect ratio of the opening to be too large, and in the process of forming the pad layer 205, the process difficulty of forming the pad layer 205 is increased. At the same time, the lateral dimension of the opening is too small and it is easy to cause the formation rate of the pad layer 205 to be too fast during the setting of the pad layer 205, so that the height difference between the top surface of the pad layer 205 located in the opening and the top surface of the pad layer 205 located on the top of the first passivation layer 201 is too small. Accordingly, after the subsequent formation of the under bump metallization layer 210, the interface between the under bump metallization layer 210 and the pad layer 205 only includes the interface between the under bump metallization layer 210 and the pad layer 205 in the horizontal direction, that is, the bonding force between the under bump metallization layer 210 and the pad layer 205 only includes the bonding force in the horizontal direction, which reduces the bonding force between the under bump metallization layer 210 and the pad layer 205 and increases The risk of delamination or gap between the under bump metallization layer 210 and the pad layer 205 is reduced, thereby affecting the performance of the semiconductor structure; if the lateral size of the opening is too large, when the lateral size of the bonding area 200A is constant, the lateral size of the first passivation layer 201 located in the bonding area 200A is too small. Accordingly, in the formation process of the pad layer 205, the deposition rate of the pad layer 205 located on the top of the first passivation layer 201 is too fast, that is, the height difference between the top surface of the pad layer 205 located in the opening and the top surface of the pad layer 205 located on the top of the first passivation layer 201 is too large, resulting in an excessively large aspect ratio between adjacent pad layers 205 protruding from the top of the first passivation layer 201, which increases the difficulty of the subsequent process of forming the under bump metallization layer 210 on the top and sidewall of the pad layer 205, thereby affecting the performance of the semiconductor structure. To this end, in this embodiment, taking the direction perpendicular to the sidewall of the opening as the lateral direction, the lateral dimension of the opening is 2 micrometers to 5 micrometers.
[0052] In this embodiment, the shape of the opening is the same as the shape of the first passivation layer 201 located in the bonding area 200A.
[0053] Specifically, the shape of the opening is the same as the shape of the first passivation layer 201 located in the bonding area 200A, which can make the side wall of the pad layer 205 set in the opening completely contact with the side wall of the first passivation layer 201 in the bonding area 200A, thereby avoiding the risk of gaps at the interface between the pad layer 205 and the first passivation layer 201. At the same time, the bonding force between the pad layer 205 and the first passivation layer 201 includes horizontal bonding force and vertical bonding force, reducing the risk of cracks between the first passivation layer 201 and the pad layer 205, thereby improving the performance of the semiconductor structure.
[0054] In this embodiment, the shape of the opening includes one or more of a square, an inverted trapezoid and an inverted pyramid.
[0055] It should be noted that by setting the shape of the opening to one or more of a square, an inverted trapezoid and an inverted pyramid, the bonding force between the pad layer 205 and the first passivation layer 201 includes a bonding force in the horizontal direction and a bonding force in the vertical direction, thereby reducing the risk of cracks between the first passivation layer 201 and the pad layer 205 due to thermal stress, thereby improving the performance of the semiconductor structure.
[0056] It should also be noted that the shape of the opening is the same as the shape of the first passivation layer 201 in the bonding area 200A. Accordingly, the shape of the first passivation layer 201 in the bonding area 200A includes one or more of a square, a trapezoid and a pyramid.
[0057] It should be noted that the pad layer 205 is used to realize the electrical connection between the interconnection structure in the first wafer 200 and the external circuit, and the pad layer 205 is also used to provide a process basis for the subsequent formation of a connection structure (eg, a bump).
[0058] It should also be noted that the under bump metallization layer 210 and the pad layer 205 include a horizontal interface and a vertical interface, so that the bonding force between the under bump metallization layer 210 and the pad layer 205 includes a horizontal bonding force and a vertical bonding force, thereby increasing the bonding force between the under bump metallization layer 210 and the pad layer 205 and reducing the risk of delamination or gaps between the under bump metallization layer 210 and the pad layer 205, thereby improving the performance of the semiconductor structure.
[0059] In this embodiment, the material of the pad layer 205 includes aluminum.
[0060] Specifically, aluminum material is a metal material that is easily available, which is beneficial for saving costs.
[0061] In this embodiment, the semiconductor structure further includes: a second passivation layer 207 located on the top of the first passivation layer 201 at the side of the bonding area 200A.
[0062] Specifically, the second passivation layer 207 protects the first wafer 200 at the side of the bonding area 200A.
[0063] In this embodiment, the material of the second passivation layer 207 includes one or more of silicon nitride, silicon carbide and silicon oxynitride.
[0064] It should be noted that silicon nitride, silicon carbide and silicon oxynitride are all commonly used materials for passivation layers, and have the characteristics of low process cost. At the same time, silicon nitride, silicon carbide and silicon oxynitride have relatively high material hardness and can protect the first wafer 200 on the side of the bonding area 200A.
[0065] Specifically, during the formation of the conductive bump 216, in order to prevent the metal ions and contamination ions in the conductive bump 216 from diffusing into the interconnect structure in the first wafer 200 and causing corrosion, an under bump metallization layer 210 (UBM) is formed on the top and side walls of the pad layer 205 as a transition layer.
[0066] It should be noted that the under bump metallization layer 210 includes an adhesive layer, a barrier layer located on the adhesive layer, a wetting layer located on the barrier layer, and an anti-oxidation layer located on the wetting layer.
[0067] The adhesive layer can enhance the adhesion between the conductive bump 216 and the pad layer 205 and provide a strong bonding interface. As an example, the adhesive layer material includes one or more of Cr, Ti, Ni, W, TiW and zincate.
[0068] The barrier layer is used to prevent metal ions and contamination ions in the conductive bump 216 from diffusing into the interconnect structure and the bonding layer in the first wafer 200 . The barrier layer material is usually one or more of Cr, W, Ti, TiW, Ni and Cr—Cu.
[0069] The wetting layer located above the barrier layer can provide a wetting object for the conductive bump 216 thereon, and react with the conductive bump 216 to form a bond. As an example, the wetting layer metal includes one or more of Cu, Ni, Pd and Pt.
[0070] The topmost layer of the under bump metallization layer 210 is an optional anti-oxidation layer, the purpose of which is to prevent the oxidation of the wetting layer. As an example, the material of the anti-oxidation layer is Au.
[0071] In this embodiment, the under bump metallization layer 210 also covers the sidewalls and the top of the second passivation layer 207 .
[0072] The conductive bumps 216 are electrically connected to the pad layer 205 through the under bump metallization layer 210 , so that the pad layer 205 is electrically connected to the circuit board through the conductive bumps 216 , thereby achieving electrical connection between the first wafer 200 and the circuit board.
[0073] In this embodiment, the material of the conductive bump 216 includes one or more of copper, nickel and tin.
[0074] It should be noted that copper, nickel and tin materials are all commonly used metal materials in the conductive bump 216, and have the characteristics of low process cost. At the same time, copper, nickel and tin materials have low resistivity. While being able to reduce their own resistance value, they can also reduce the series resistance between the first wafer 200 and the circuit board, thereby improving the electrical performance of the semiconductor structure.
[0075] Figures 3 to 8 It is a schematic structural diagram corresponding to each step in an embodiment of a method for forming a semiconductor structure of the present invention.
[0076] refer to Figure 3 , providing a first wafer 100 , wherein the first wafer 100 includes a bonding area 100A, and a first passivation layer 101 is formed on the first wafer 100 .
[0077] Specifically, the first wafer 100 provides a process platform for the formation process of the semiconductor structure.
[0078] The first wafer 100 is a finished wafer, and the first wafer 100 can be manufactured using integrated circuit manufacturing technology.
[0079] In this embodiment, the first wafer 100 includes a substrate (not shown) and a dielectric layer (not shown) located on the substrate.
[0080] The substrate is a silicon substrate. In other embodiments, the material of the substrate may also be other materials such as germanium, silicon germanium, silicon carbide, gallium arsenide or indium gallium, and the substrate may also be other types of substrates such as a silicon substrate on an insulator or a germanium substrate on an insulator. The material of the substrate may be a material suitable for process requirements or easy to integrate.
[0081] It should be noted that the dielectric layer is used to electrically isolate the interconnection structure (not shown) disposed in the dielectric layer.
[0082] In this embodiment, the material of the dielectric layer is a dielectric material, and the material of the dielectric layer includes one or more of silicon oxide, tetraethyl orthosilicate, polyethylene oxide, silicon nitride and silicon carbide.
[0083] Specifically, silicon oxide, tetraethyl orthosilicate, polyethylene oxide, silicon nitride and silicon carbide nitride are all dielectric materials that can play a good role in electrically isolating adjacent interconnect structures.
[0084] In this embodiment, the bonding area 100A is a region where a pad layer and an under-bump metallization layer are subsequently formed.
[0085] Specifically, the first passivation layer 101 protects the top of the first wafer 100, and reduces the probability of damage to the first wafer 100 on the side of the bonding area 100A during the subsequent formation of the pad layer and the under bump metallization layer, thereby improving the performance of the semiconductor structure.
[0086] In this embodiment, the material of the first passivation layer 101 includes one or more of silicon nitride, silicon carbide and silicon oxynitride.
[0087] refer to Figure 4 One or more openings 103 penetrating the first passivation layer 101 are formed in the bonding area 100A, and the remaining first passivation layer 101 protrudes from the top of the first wafer 100 .
[0088] It should be noted that the opening 103 provides a space for the subsequent formation of a pad layer.
[0089] It should also be noted that by forming one or more openings 103 that penetrate the first passivation layer 101, in the process of subsequently forming a pad layer, the top surface of the pad layer located in the opening 103 can be made lower than the top surface of the pad layer located on the top of the first passivation layer 101. After the subsequent formation of the under bump metallization layer, the interface between the under bump metallization layer and the pad layer can include the interface between the under bump metallization layer and the pad layer in the horizontal direction, and the interface between the under bump metallization layer and the pad layer in the vertical direction, that is, the bonding force between the under bump metallization layer and the pad layer includes the bonding force in the horizontal direction and the bonding force in the vertical direction, which increases the bonding force between the under bump metallization layer and the pad layer and reduces the risk of delamination or gaps between the under bump metallization layer and the pad layer.
[0090] In this embodiment, the step of forming one or more openings 103 penetrating the first passivation layer 101 in the bonding area 100A includes: forming a mask layer having one or more mask openings 103 on the top of the first passivation layer 101, and the mask opening 103 is located on the top of the first passivation layer 101 in the bonding area 100A; using the mask layer as a mask, patterning the first passivation layer 101 to form one or more openings 103 penetrating the first passivation layer 101 in the bonding area 100A.
[0091] Specifically, the mask layer is used as an etching mask for forming the opening 103 .
[0092] In this embodiment, the material of the mask layer includes photoresist.
[0093] In other embodiments, the material of the mask layer may also be one or both of silicon nitride and silicon oxide.
[0094] In this embodiment, the process of forming one or more openings 103 penetrating the first passivation layer 101 in the bonding area 100A includes a dry etching process.
[0095] Specifically, the dry etching process is an anisotropic dry etching process. The anisotropic dry etching process has the characteristics of anisotropic etching, and its longitudinal etching rate is much greater than the lateral etching rate. In the process of patterning the first passivation layer 101, it can obtain quite accurate pattern transfer, and at the same time, it is also conducive to ensuring the quality of the sidewall morphology of the opening 103, which is conducive to the subsequent filling of the pad layer in the opening 103, reducing the risk of gaps at the interface between the pad layer and the first passivation layer 101, and improving the electrical performance of the semiconductor structure.
[0096] It should be noted that, with the direction perpendicular to the side wall of the opening 103 as the lateral direction, the lateral dimension of the opening 103 should not be too large or too small. If the lateral dimension of the opening 103 is too small, it is easy to cause the aspect ratio of the opening 103 to be too large, which increases the difficulty of forming the pad layer in the subsequent process of forming the pad layer. At the same time, the lateral dimension of the opening 103 is too small, which is easy to cause the formation rate of the pad layer to be too fast in the process of forming the pad layer, so that the height difference between the top surface of the pad layer located in the opening 103 and the top surface of the pad layer located on the top of the first passivation layer 101 is too small. Accordingly, after the subsequent formation of the under bump metallization layer, the interface between the under bump metallization layer and the pad layer only includes the interface between the under bump metallization layer and the pad layer in the horizontal direction, that is, the bonding force between the under bump metallization layer and the pad layer only includes the bonding force in the horizontal direction, which reduces the bonding force between the under bump metallization layer and the pad layer and increases the under bump metallization layer. The risk of delamination or gap between the passivation layer and the pad layer will be increased, thereby affecting the performance of the semiconductor structure; if the lateral size of the opening 103 is too large, when the lateral size of the bonding area 100A is constant, the lateral size of the first passivation layer 101 located in the bonding area 100A is too small, and accordingly, in the subsequent process of forming the pad layer, the deposition rate of the pad layer located at the top of the first passivation layer 101 is too fast, that is, the height difference between the top surface of the pad layer located in the opening 103 and the top surface of the pad layer located at the top of the first passivation layer 101 is too large, resulting in an excessively large depth-to-width ratio between the adjacent pad layers protruding from the top of the first passivation layer 101, which increases the difficulty of the subsequent process of forming the under-bump metallization layer on the top and sidewall of the pad layer, thereby affecting the performance of the semiconductor structure. To this end, in this embodiment, the lateral size of the opening 103 is 2 microns to 5 microns, with the direction perpendicular to the sidewall of the opening 103 as the lateral direction.
[0097] In this embodiment, the shape of the opening 103 is the same as the shape of the first passivation layer 101 located in the bonding area 100A.
[0098] Specifically, the shape of the opening 103 is the same as the shape of the first passivation layer 101 located in the bonding area 100A, which can enable the side wall of the pad layer subsequently formed in the opening 103 to be completely in contact with the side wall of the first passivation layer 101 in the bonding area 100A, thereby avoiding the risk of gaps at the interface between the pad layer and the first passivation layer 101. At the same time, the bonding force between the pad layer and the first passivation layer 101 includes horizontal bonding force and vertical bonding force, reducing the risk of cracks between the first passivation layer 101 and the pad layer, thereby improving the performance of the semiconductor structure.
[0099] In this embodiment, the shape of the opening 103 includes one or more of a square, an inverted trapezoid and an inverted pyramid.
[0100] It should be noted that by setting the shape of the opening 103 to one or more of a square, an inverted trapezoid and an inverted pyramid, the bonding force between the pad layer and the first passivation layer 101 includes a bonding force in the horizontal direction and a bonding force in the vertical direction, thereby reducing the risk of cracks between the first passivation layer 101 and the pad layer due to thermal stress, thereby improving the performance of the semiconductor structure.
[0101] It should also be noted that the shape of the opening 103 is the same as the shape of the first passivation layer 101 in the bonding area 100A. Accordingly, the shape of the first passivation layer 101 in the bonding area 100A includes one or more of a square, a trapezoid and a pyramid.
[0102] Specifically, after forming the opening 103 and before subsequently forming the pad layer, the method for forming the semiconductor structure further includes: removing the mask layer.
[0103] Removing the mask layer provides a process window for subsequently forming a pad layer.
[0104] In this embodiment, the process of removing the pad layer includes an ashing process or a wet etching process.
[0105] refer to Figure 5 A pad layer 105 is formed in the opening 103 and on the top of the first passivation layer 101 , and the pad layer 105 located on the top of the first passivation layer 101 is higher than the pad layer 105 located in the opening 103 .
[0106] It should be noted that the pad layer 105 is used to realize the electrical connection between the interconnection structure in the first wafer 100 and the external circuit, and the pad layer 105 is also used to provide a process basis for the subsequent formation of a connection structure (eg, a bump).
[0107] It should also be noted that the under bump metallization layer and the pad layer 105 include a horizontal interface and a vertical interface, so that the bonding force between the under bump metallization layer and the pad layer 105 includes a horizontal bonding force and a vertical bonding force, thereby increasing the bonding force between the under bump metallization layer and the pad layer 105 and reducing the risk of delamination or gaps between the under bump metallization layer and the pad layer 105, thereby improving the performance of the semiconductor structure.
[0108] In this embodiment, the material of the pad layer 105 includes aluminum.
[0109] Specifically, aluminum material is a metal material that is easily available, which is beneficial for saving costs.
[0110] In this embodiment, the process for forming the pad layer 105 includes a sputtering process. Specifically, the sputtering process has low cost and high process compatibility. In the process of forming the pad layer 105 by the sputtering process, the probability of generating bubble defects in the pad layer 105 is reduced, thereby affecting the performance of the semiconductor structure. At the same time, the yield of the subsequently formed conductive bumps is also affected.
[0111] It should be noted that, in the process of forming the pad layer 105 , the pad layer 105 also covers the top of the first passivation layer 101 located at the side of the bonding area 100A.
[0112] refer to Figure 6 After forming the pad layer 105 and before subsequently forming the under bump metallization layer, the method further includes: forming a second passivation layer 107 on top of the first passivation layer 101 at the side of the bonding area 100A.
[0113] Specifically, the second passivation layer 107 protects the first wafer 100 at the side of the bonding area 100A, and also plays a buffering role in the subsequent process.
[0114] In this embodiment, the material of the second passivation layer 107 includes one or more of silicon nitride, silicon carbide and silicon oxynitride.
[0115] It should be noted that silicon nitride, silicon carbide and silicon oxynitride are all commonly used materials for passivation layers, and have the characteristics of low process cost. At the same time, silicon nitride, silicon carbide and silicon oxynitride have relatively high material hardness and can protect the first wafer 100 on the side of the bonding area 100A.
[0116] It should also be noted that, in the process of forming the second passivation layer 107 , the second passivation layer 107 also covers the pad layer 105 on the top of the first passivation layer 101 located at the side of the bonding area 100A.
[0117] refer to Figure 7An under bump metallization layer 110 is formed on the top and sidewalls of the pad layer 105 .
[0118] Specifically, in the subsequent process of forming the conductive bump, in order to prevent the metal ions and contamination ions in the conductive bump from diffusing into the interconnect structure in the first wafer 100 and causing corrosion, an under bump metallization layer 110 (UBM) is formed on the top and side walls of the pad layer 105 as a transition layer.
[0119] It should be noted that the under bump metallization layer 110 includes an adhesive layer, a barrier layer located on the adhesive layer, a wetting layer located on the barrier layer, and an anti-oxidation layer located on the wetting layer.
[0120] The adhesive layer can enhance the adhesion between the conductive bump and the pad layer 105 and provide a strong bonding interface. As an example, the adhesive layer material includes one or more of Cr, Ti, Ni, W, TiW and zincate.
[0121] The barrier layer is used to prevent metal ions and contamination ions in the conductive bump from diffusing into the interconnect structure and the bonding layer in the first wafer 100 . The barrier layer material is usually one or more of Cr, W, Ti, TiW, Ni and Cr—Cu.
[0122] The wetting layer located above the barrier layer can provide a wetting object for the conductive bumps thereon and react with the conductive bumps to form a bond. As an example, the wetting layer metal includes one or more of Cu, Ni, Pd and Pt.
[0123] The topmost layer of the under bump metallization layer 110 is an optional anti-oxidation layer, the purpose of which is to prevent the oxidation of the wetting layer. As an example, the material of the anti-oxidation layer is Au.
[0124] In this embodiment, during the process of forming the under bump metallization layer 110 , the under bump metallization layer 110 also covers the sidewalls and the top of the second passivation layer 107 .
[0125] In this embodiment, the process of forming the under bump metallization layer 110 includes a physical vapor deposition process.
[0126] It should be noted that the physical vapor deposition process can be divided into two types: evaporation process and sputtering process. The former uses high temperature to melt and evaporate the metal and then coat it on the wafer, while the latter uses high-speed particles to impact the target material to excite the target surface atoms or molecules to fall on the wafer. Both processes must be completed under vacuum conditions. Considering the high cost of evaporation, as an example, the process for forming the under bump metallization layer 110 is a sputtering process.
[0127] refer to Figure 8 , forming a conductive bump 116 covering the under bump metallization layer 110 .
[0128] The conductive bumps 116 are electrically connected to the pad layer 105 through the under bump metallization layer 110 , so that the pad layer 105 is electrically connected to the circuit board through the conductive bumps 116 , thereby achieving electrical connection between the first wafer 100 and the circuit board.
[0129] In this embodiment, the process of forming the conductive bump 116 includes an electroplating process.
[0130] It should be noted that forming the conductive bump 116 through the electroplating process can improve the efficiency of the subsequent packaging process. Moreover, the conductive bump 116 formed through the electroplating process is of high quality and can reduce the probability of forming voids in the conductive bump 116, thereby improving the electrical performance of the semiconductor structure.
[0131] In this embodiment, the material of the conductive bump 116 includes one or more of copper, nickel and tin.
[0132] It should be noted that copper, nickel and tin materials are all commonly used metal materials in the conductive bumps 116, and have the characteristics of low process cost. At the same time, copper, nickel and tin materials have low resistivity. While being able to reduce their own resistance value, they can also reduce the series resistance between the first wafer 100 and the circuit board, thereby improving the electrical performance of the semiconductor structure.
[0133] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.
Claims
1. A semiconductor structure, characterized in that: include: a first wafer, the first wafer comprising a bonding area; A first passivation layer protrudes from the top of the first wafer; an opening located in the first passivation layer of the bonding region; A pad layer is located in the opening and on top of the first passivation layer, and the pad layer located on top of the first passivation layer is higher than the pad layer located in the opening; An under-bump metallization layer, located on the top and sidewalls of the pad layer; A conductive bump covers the under-bump metallization layer.
2. The semiconductor structure according to claim 1, wherein: The shape of the opening is the same as that of the first passivation layer located in the bonding area.
3. The semiconductor structure according to claim 1, wherein: The shape of the opening includes one or more of a square, an inverted trapezoid and an inverted pyramid; The shape of the first passivation layer located in the bonding area includes one or more of a square, a trapezoid and a pyramid.
4. The semiconductor structure according to claim 1, wherein: The material of the pad layer includes aluminum.
5. The semiconductor structure according to claim 1, wherein: The semiconductor structure further includes: a second passivation layer located on top of the first passivation layer at the side of the bonding region; The under bump metallization layer also covers the sidewalls and the top of the second passivation layer.
6. The semiconductor structure according to claim 5, characterized in that: The material of the second passivation layer includes one or more of silicon nitride, silicon carbide and silicon oxynitride.
7. The semiconductor structure according to claim 1, wherein: The material of the conductive bump includes one or more of copper, nickel and tin.
8. The semiconductor structure according to claim 1, wherein: Taking the direction perpendicular to the sidewall of the opening as the lateral direction, the lateral dimension of the opening is 2 microns to 5 microns.
9. A method for forming a semiconductor structure, characterized in that: include: Providing a first wafer, wherein the first wafer comprises a bonding region, and a first passivation layer is formed on the first wafer; forming one or more openings penetrating the first passivation layer in the bonding area, with the remaining first passivation layer protruding from the top of the first wafer; forming a pad layer in the opening and on top of the first passivation layer, wherein the pad layer located on top of the first passivation layer is higher than the pad layer located in the opening; forming an under bump metallization layer on the top and sidewalls of the pad layer; A conductive bump is formed covering the under bump metallization layer.
10. The method for forming a semiconductor structure according to claim 9, wherein: The step of forming one or more openings penetrating the first passivation layer in the bonding area includes: forming a mask layer having one or more mask openings on top of the first passivation layer, wherein the mask openings are located on the top of the first passivation layer in the bonding area; using the mask layer as a mask, patterning the first passivation layer to form one or more openings penetrating the first passivation layer in the bonding area; and removing the mask layer.
11. The method for forming a semiconductor structure according to claim 9, wherein: The process of forming one or more openings penetrating the first passivation layer in the bonding region includes a dry etching process.
12. The method for forming a semiconductor structure according to claim 9, wherein: Taking the direction perpendicular to the sidewall of the opening as the lateral direction, the lateral dimension of the opening is 2 microns to 5 microns.
13. The method for forming a semiconductor structure according to claim 9, wherein: The shape of the opening is the same as that of the first passivation layer located in the bonding area.
14. The method for forming a semiconductor structure according to claim 9, wherein: The shape of the opening includes one or more of a square, an inverted trapezoid and an inverted pyramid; The shape of the first passivation layer located in the bonding area includes one or more of a square, a trapezoid and a pyramid.
15. The method for forming a semiconductor structure according to claim 9, wherein: The process of forming the pad layer includes a sputtering process.
16. The method for forming a semiconductor structure according to claim 9, wherein: After forming the pad layer and before forming the under bump metallization layer, the method further includes: forming a second passivation layer on top of the first passivation layer at the side of the bonding area; During the process of forming the under bump metallization layer, the under bump metallization layer also covers the sidewalls and the top of the second passivation layer.
17. The method for forming a semiconductor structure according to claim 16, wherein: The material of the second passivation layer includes one or more of silicon nitride, silicon carbide and silicon oxynitride.
18. The method for forming a semiconductor structure according to claim 9, wherein: The process of forming the under bump metallization layer includes a physical vapor deposition process.
19. The method for forming a semiconductor structure according to claim 9, wherein: The process of forming the conductive bump includes an electroplating process.