VCSEL chip and VCSEL laser

By designing a stepped structure on the surface of the P-type DBR part of the VCSEL chip, the problems of large internal resistance and poor heat dissipation of the chip are solved, and better thermal stability and high-speed modulation performance are achieved.

CN119050807AActive Publication Date: 2024-11-29SHENZHEN ZHONGKE OPTICAL SEMICON TECH CO LTD

Patent Information

Application Number
CN202411272600.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-11
Publication Date
2024-11-29
Estimated Expiration
2044-09-11

AI Technical Summary

Technical Problem

Existing VCSEL chips have problems such as excessive internal resistance and poor heat dissipation in high-speed modulation applications, which limits their modulation bandwidth and thermal stability.

Method used

By designing a step structure on the surface of the P-type DBR part, the step structure is formed using an etching process to increase the heat dissipation area and reduce the overall equivalent resistance, and improve the heat dissipation performance and thermal stability of the chip.

Benefits of technology

It effectively reduces the internal resistance of the VCSEL chip, improves heat dissipation performance and thermal stability, thereby enhancing its high-speed modulation performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119050807A_ABST
    Figure CN119050807A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of semiconductor lasers, in particular to a VCSEL chip and a VCSEL laser. The VCSEL chip is used for a semiconductor laser and comprises an N electrode, an N-type DBR part, an active part, a P-type DBR part and a P electrode, and the N electrode, the N-type DBR part, the active part, the P-type DBR part and the P electrode are sequentially arranged in a stacked mode from bottom to top. Wherein the P-type DBR part is arranged to be of a multi-layer structure which is stacked in sequence, and the transverse area of each layer of the multi-layer structure is gradually reduced from bottom to top; moreover, the adjacent layers of the multi-layer structure are set as follows: the edge distance of the upper end face of the lower DBR layer and the edge distance of the lower end face of the upper DBR layer have a certain distance. According to the embodiment of the invention, the surface of the P-type DBR part of the VCSEL is arranged to be of the stepped structure, so that the overall equivalent resistance of the VCSEL can be effectively reduced, the heat dissipation performance is improved, and the heat stability and high-speed modulation performance of a chip are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of semiconductor lasers, and in particular to a VCSEL chip and a VCSEL laser. Background Art

[0002] VCSEL is a semiconductor laser structure that forms an optical resonant cavity in a direction perpendicular to the semiconductor epitaxial wafer and emits a laser beam perpendicular to the substrate surface.

[0003] Vertical cavity surface emitting lasers often use GaAs (gallium arsenide) material as the substrate, but it is well known that the heat dissipation performance of GaAs material is not good, and the refractive index of GaAs material will change with the increase of temperature, so when the chip works at high temperature, the performance of the device will decrease.

[0004] In the process of realizing the present invention, the inventors of the present invention found that: currently, high-speed modulated VCSEL is a hot spot in the industry. Currently, VCSEL with a bandwidth of 25GHz has been mass-produced, and further improving the modulation speed of VCSEL faces many challenges. If you want to further improve the modulation bandwidth of VCSEL, you should consider two aspects: on the one hand, you need to further reduce the memory of such chips. It is difficult to further reduce the internal resistance of such chips using conventional designs to improve the modulation bandwidth; on the other hand, you need to further improve the heat dissipation performance of such devices. However, the current VCSEL chip structure cannot solve the problems of excessive internal resistance and poor heat dissipation at the same time, which restricts the development of high-speed modulated VCSEL. Summary of the invention

[0005] In view of the above problems, the present invention is proposed to provide a VCSEL chip, a VCSEL chip semiconductor laser and a control method that overcome the above problems or at least partially solve the above problems.

[0006] In a first aspect, an embodiment of the present invention provides a VCSEL chip for a semiconductor laser, comprising: An N-electrode, an N-type DBR portion, an active portion, a P-type DBR portion, and a P-electrode, wherein the N-electrode, the N-type DBR portion, the active portion, the P-type DBR portion, and the P-electrode are sequentially stacked from bottom to top; The P-type DBR part is configured as a multi-layer structure stacked in sequence, and the lateral area of ​​each layer of the multi-layer structure gradually decreases from bottom to top; Furthermore, the adjacent layers of the multilayer structure are arranged such that: the upper edge distance of the DBR layer at the lower position is the same as the lower edge distance of the DBR layer at the upper position.

[0007] Furthermore, the distance is controlled to be 0.8-2um.

[0008] Furthermore, the transverse cross-sectional shape of the P-type DBR portion includes a circle, an ellipse or a rectangle.

[0009] Furthermore, the number of layers of the P-type DBR part is 16-40 layers.

[0010] Furthermore, the thickness of each layer of the P-type DBR portion is controlled to be 1-1.5 um.

[0011] Further, the P-type DBR part is made of material Furthermore, the N-type electrode is AuGeNi alloy plated material with a thickness of 500Å; the P-type electrode is Ti / Au with a thickness of 500Å / 3000Å.

[0012] The second aspect also discloses a VCSEL laser, comprising: the VCSEL chip described in any one of the items.

[0013] The beneficial effects of the above technical solution provided by the embodiment of the present invention include at least: In an embodiment of the present invention, a VCSEL chip is provided, wherein the surface of the P-type DBR part of the VCSEL is set to a stepped structure, and each step of the stepped structure corresponds to each layer in the P-type DBR part, thereby effectively improving the overall performance of the P-type DBR part. As a result, the overall equivalent resistance of the VCSEL can be effectively reduced, and the heat dissipation is also improved, thereby improving the thermal stability and high-speed modulation performance of the chip.

[0014] In order to obtain a stepped structure on the surface of the P-type DBR portion, in an embodiment, a pattern structure on a mask is designed, and the pattern is etched into the P-type DBR portion through an etching process, thereby obtaining a stepped structure.

[0015] Other features and advantages of the present invention will be described in the following description, and partly become apparent from the description, or understood by practicing the present invention. The purpose and other advantages of the present invention can be realized and obtained by the structures particularly pointed out in the written description and the accompanying drawings.

[0016] The technical solution of the present invention is further described in detail below through the accompanying drawings and embodiments. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] In order to more clearly illustrate the specific embodiments of the present invention or the technical solutions in the prior art, the following is a brief introduction to the drawings required for the specific embodiments or the description of the prior art. In all the drawings, similar elements or parts are generally identified by similar reference numerals. In the drawings, the elements or parts are not necessarily drawn according to the actual scale.

[0018] Figure 1 This is a schematic diagram of the structure of a traditional VCSEL chip; Figure 2 is a schematic diagram of a VCSEL chip according to a first embodiment of the present invention; Figure 3 The present invention Figure 2 A schematic diagram from another perspective; Figure 4 The present invention Figure 3 A partial enlarged view of D; Figure 5 This is the LIV curve of the traditional VCSEL chip; Figure 6 is a LIV curve diagram of the VCSEL chip of this embodiment; Figure 7 is a schematic diagram of a first mask according to a first embodiment of the present invention; Figure 8 The present invention Figure 7 A partial enlarged view of; Fig. 9 The present invention Figure 7 A schematic diagram from another perspective; Fig.10 The present invention Fig. 9 B is a partial enlarged view; Fig.11 is a schematic diagram of a first mask according to a second embodiment of the present invention; Fig.12 The present invention Fig.11 A partial enlarged view of C; Fig.13 It is a flow chart of the method for preparing the VCSEL chip of the present invention.

[0019] Indicated in the figure: 10. P-type DBR part; 11. Active part; 12. N-type DBR part; 13. Substrate; 14. P electrode; 20. First mask; 21. Pattern layer; 22. Substrate; 210. Protruding structure; 211. Boss. DETAILED DESCRIPTION

[0020] The following embodiments of the technical solution of the present invention are described in detail in conjunction with the accompanying drawings. The following embodiments are only used to more clearly illustrate the technical solution of the present invention, and are therefore only used as examples, and cannot be used to limit the protection scope of the present invention.

[0021] It should be noted that, unless otherwise specified, the technical terms or scientific terms used in this application should have the common meanings understood by those skilled in the art to which the present invention belongs.

[0022] In the description of the present application, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.

[0023] In addition, the terms "first", "second", etc. are used for descriptive purposes only and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. In the description of the present invention, "plurality" means more than two, unless otherwise clearly and specifically defined.

[0024] In this application, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0025] In the present application, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may mean that the first and second features are in direct contact, or that the first and second features are in indirect contact through an intermediate medium. Moreover, a first feature being "above", "above" or "above" a second feature may mean that the first feature is directly above or obliquely above the second feature, or simply means that the first feature is higher in level than the second feature. A first feature being "below", "below" or "below" a second feature may mean that the first feature is directly below or obliquely below the second feature, or simply means that the first feature is lower in level than the second feature.

[0026] Embodiment, VCSEL is a semiconductor laser structure that forms an optical resonant cavity in a direction perpendicular to the semiconductor epitaxial wafer and emits a laser beam perpendicular to the substrate surface. It is widely used in consumer electronics, military, medical and other fields, such as 3D sensing, AR / VR, robots, laser radar, consumer electronics, intelligent manufacturing, Internet of Things, data centers and other fields. Specific applications include intelligent driving, video surveillance, laser radar, machine vision, gesture recognition, face recognition and other fields.

[0027] As the reflector of the resonant cavity, DBR is formed by alternating epitaxial growth of high and low refractive index media or semiconductor materials, and the optical thickness of each layer of material is 1 / 4 of the laser wavelength. Using the principle of thin film interference and reflection phase change, when light passes through a layer of thin film, it will be reflected twice on the upper and lower surfaces. The thickness of the film will affect the optical path difference of the two reflections. If the thickness of the film is controlled to be an integer multiple of (1 / 4+N) wavelengths, the optical path difference of the two reflections is (1 / 2+2N). The optical path difference corresponds to a 180° phase change, so the two reflections on the upper and lower interfaces are ultimately in phase, and the superposition enhancement increases the overall reflection coefficient; high and low refractive index media or semiconductor materials are alternately epitaxially grown, and light from the optically dense medium to the optically sparse medium will also undergo a 180° phase change at the interface, so the light passing through each layer of DBR will increase a certain reflection coefficient. For the light exit surface, DBR obtains a smaller reflection coefficient by appropriately reducing its number of layers to ensure that the laser is transmitted and emitted.

[0028] The entire process of the current VCSEL chip can be divided into two parts, epitaxial growth and chip manufacturing. The epitaxial process is crucial. The quality of the epitaxial structure basically determines the performance of the VCSEL device. At present, major manufacturers generally use MOCVD to grow, with a total thickness of about 8-10um, and a total of more than 200 layers in the whole structure. Generally, each single layer is grown first, and the quality, composition, carrier concentration and growth rate of the single layer are determined by various test equipment before further epitaxy of the entire structure. Changes in the parameters of each layer, such as the number of DBR layers, doping concentration or changes in the heterogeneous surface structure of the active area, will have a relatively large impact on the overall characteristics of the VCSEL.

[0029] See attached Figure 1 As shown, generally, the VCSEL includes a substrate 13, a first reflective portion, an active portion, a second reflective portion, and electrodes.

[0030] The substrate 13 allows the growth of the layers constituting the VCSEL. The substrate 13 provides a space where the layers can grow, and obtains power from the electrode to be arranged at the lower end of the substrate 13, and transmits it to the first reflection part. Accordingly, the laser (light) can be output from the active part from the power recognized to each reflection part. Among them, the substrate 13 can be implemented with GaAs, but is not necessarily limited to this, and can also be implemented with GaN SiC ZnC Si or sapphire, etc.

[0031] The first reflector can be implemented as an n-type semiconductor layer coated with an n-type coating agent, and can be composed of any of the semiconductor materials AlGaAs AlGaInP and AlInP containing Al. The first reflector can be composed of at least one n-type semiconductor layer, and can also include a layer forming a distributed Bragg cover or "distributed Bragg cover" (DBR). The first reflector can be formed on the substrate by any of the methods such as Epitaxy Chemical Deposition Method (CVD), Sputtering, Organic Accelerated Vapor Phase Growth Method (MOCVD) or Vapor Phase Gas Phase (HVPE).

[0032] The active part is a layer where the electrons generated in the first reflective part and the holes generated in the second reflective part meet and reconnect, and light is generated by the reconnection of electrons and holes. The active part may include a single quantum well (SQW) or a multiple quantum well (MQW) structure having multiple quantum well layers. If a multiple quantum well structure is included, the cavity layer has a structure in which well layers (micro-conductors) and barrier layers (micro-conductors) with different energy bands are alternately stacked one or more times.

[0033] The well layer / barrier layer of the active part can be composed of AlGaInP / AlGaInP AlGaInP / AlInP AlGaAs / AlGaAsAlGaAs / GaAs or AlGaAs / InGaAs, etc.

[0034] An oxide film layer is formed on the top of the active portion.

[0035] The oxide film layer undergoes an oxidation process to form an oxide portion of a certain length, and the diameter of the opening is determined according to the length of the oxide portion. The oxide film layer is composed of aluminum (Al) with a higher concentration than the first reflector and the second reflector. The higher the aluminum concentration, the greater the oxidation rate. As the oxide film layer is realized with a relatively higher aluminum concentration than the positive reflector, it can be selectively oxidized during subsequent oxidation. For example, the oxide film layer can be realized with 98% AlGaAs, and each reflector can be realized with 92% AlGaAs.

[0036] The second reflector may be composed of a semiconductor material coated with a p-type coating agent, or may be composed of any one of AlGaAs, AlGaInP and AlInP semiconductor materials containing Al, or may be composed of GaP. The second reflector may be composed of at least one layer, or may include a layer formed by a DBR. The second reflector may be formed by any one of methods such as epitaxy chemical deposition (CVD), sputtering, organic accelerated vapor phase growth (MOCVD) or vapor phase vapor phase (HVPE) on the cavity layer.

[0037] The electrode is formed on the second reflecting portion so as to supply power to the second reflecting portion.

[0038] The inventors of this application are continuing to study how to effectively solve the problem that the VCSEL chip structure cannot be improved at the same time, and solve the problem of excessive internal resistance and poor heat dissipation effect. The inventors' research at least includes: how to change the internal resistance and heat dissipation effect of the entire VCSEL by changing the number of DBR layers, doping concentration or heterogeneous surface structure of the active area, and by changing the structure of the DBR layer. After a lot of repeated research, the inventors proposed the VCSEL chip and laser of this application.

[0039] See attached Figure 2 As shown, an embodiment of the present invention provides a VCSEL chip, which is used for a semiconductor laser and includes: N-electrode, N-type DBR portion 12, active portion 11, P-type DBR portion 10 and P-electrode 14, and the N-electrode, the N-type DBR portion 12, the active portion 11, the P-type DBR portion 10 and the P-electrode 14 are sequentially stacked from bottom to top; The P-type DBR section 10 is configured as a multi-layer structure stacked in sequence, and the lateral area of ​​each layer of the multi-layer structure gradually decreases from bottom to top; Furthermore, the adjacent layers of the multilayer structure are arranged such that: the upper edge distance of the DBR layer at the lower position is the same as the lower edge distance of the DBR layer at the upper position.

[0040] It can be understood that in order to solve the problems of excessive internal resistance and poor heat dissipation in the current high-speed modulatable VCSEL, an embodiment is to set the cross-section of the P-type DBR portion 10 to a structure that gradually decreases from bottom to top, and at the same time, set a step structure on the outer surface of the P-type DBR portion 10. The step structure effectively increases the outer surface area of ​​the P-type DBR portion 10, thereby effectively solving the problem of poor heat dissipation. At the same time, the P-type DBR portion 10 with a stepped structure can effectively reduce the overall equivalent series resistance of the chip, that is, reduce the internal resistance of the VCSEL chip, thereby improving the thermal stability and high-speed modulation performance of the chip.

[0041] In the embodiment, the active portion 11 is specifically a non-doped active region, and the active portion 11 includes a light-emitting quantum well and a barrier layer thereof. The N-type DBR portion 12 and the P-type DBR portion 10 are both composed of two materials of different components (such as Al0.1GaAs and Al0.9GaAs), and the two materials of different components are arranged alternately layer by layer. Because they are composed of two materials of different components, they have different refractive indices.

[0042] See attached Figure 3 and4 As shown in the embodiment, the step structure here can be considered as: the adjacent layers of the multilayer structure are set to: the upper edge distance of the DBR layer at the lower position, and the lower edge distance of the DBR layer at the upper position. The step structure can also be considered as: the lower DBR layer protrudes a part than the upper DBR layer, thereby forming a staggered step structure.

[0043] At the same time, it can also be considered that the two adjacent layers from bottom to top are arranged so that a part of the upper end surface of the lower DBR layer is exposed to the outside, that is, the lower DBR layer protrudes a part relative to the upper DBR layer arranged above the DBR layer, so that the outer surface of the P-type DBR part 10 is provided with a step structure.

[0044] Here, the lower position means that among two adjacent layers in a multilayer structure, the layer located at the lower side is the lower position; and the upper position means that among two adjacent layers in a multilayer structure, the layer located at the upper side is the upper position. For example, in one embodiment, two DBR layers are stacked together, the layer located at the lower side is called the lower position, and the layer located at the upper side is called the upper position.

[0045] It can be understood that the structure of the VCSEL chip of this embodiment is roughly the same as that of the existing VCSEL chip. It can also be understood that this embodiment is an improvement based on the existing VCSEL chip. The difference of the VCSEL chip of this embodiment is that a stepped structure is set on the outer surface of the P-type DBR part 10 to solve the defects of the existing high-speed modulated VCSEL chip, effectively reduce the internal resistance of the VCSEL chip, and at the same time increase the heat dissipation effect, effectively ensuring the thermal stability and high-speed modulation performance of the VCSEL chip.

[0046] Figure 5 This is the LIV curve of the traditional VCSEL chip; Figure 6 is the LIV curve of the VCSEL chip of this embodiment. The LIV curve here refers to the curve relationship between the laser current (I), voltage (V) and light output power (P). Through the LIV curve, the output power of the laser at different working points can be understood, and its performance can be evaluated.

[0047] in, Figure 5 The number of layers of the P-type DBR part 10 of the VCSEL laser is 32, Width=35 and Width0=20, which are consistent with Figure 6 The number of layers of the P-type DBR portion 10 of the VCSEL laser is 32, Width=35 and Width0=20, and the step L of the P-type DBR portion 10 is 1 um.

[0048] Through the relationship between output voltage and output current, it can be concluded that Figure 5 The internal resistance of the VCSEL chip is R=182Ω. Figure 6 The internal resistance of the VCSEL chip is R=164Ω. It can be seen that by designing a stepped structure on the surface of the P-type DBR part 10, the internal resistance of the VCSEL chip can be effectively reduced by 10% when other designs are basically the same, thereby increasing the response speed and bandwidth of the device.

[0049] As described above, by setting the outer surface of the P-type DBR part 10 to a stepped structure, the overall internal resistance of the VCSEL is reduced. After the internal resistance is reduced, the heat generated by the internal resistance can be reduced, thereby reducing the heat to a certain extent.

[0050] See attached Figure 4 As shown, in the embodiment, the distance L is further controlled to be 0.8-2 um. At the same time, the height H of the step protrusion can also be controlled to be 0.8-2 um.

[0051] By appropriately setting the cross-sections of two adjacent layers in the P-type DBR part 10 of the multi-layer structure, there is a difference, wherein the sizes of the two adjacent layers have a certain difference. By effectively controlling the difference, it is ensured that the internal resistance of the vcsel chip can be effectively reduced, while the heat dissipation effect of the vcsel chip is increased.

[0052] In some embodiments, the distance between the edge of the upper end surface of the lower layer and the edge of the lower section of the upper layer in two adjacent layers of the P-type DBR portion 10 of the multi-layer structure is controlled to be 1um; in other embodiments, the distance between the edge of the upper end surface of the lower layer and the edge of the lower section of the upper layer in two adjacent layers of the P-type DBR portion 10 of the multi-layer structure is controlled to be 1.5um; in still other embodiments, the distance between the edge of the upper end surface of the lower layer and the edge of the lower section of the upper layer in two adjacent layers of the P-type DBR portion 10 of the multi-layer structure is controlled to be 2um.

[0053] See attached Figure 2 As shown, in a further embodiment, the transverse cross-sectional shape of the P-type DBR portion 10 includes a circle, an ellipse or a rectangle.

[0054] That is to say, the cross section of the P-type DBR portion 10 can be etched into different shapes according to actual needs. In this example, the cross section of the P-type DBR portion 10 is etched into a circle through the first mask 20. Of course, it can also be etched into other shapes, such as an ellipse or a rectangle.

[0055] In a further embodiment, the number of layers of the P-type DBR section 10 is 16-40 layers.

[0056] That is to say, the actual number of layers of the P-type DBR section 10 can be set according to actual needs. In actual use, in some embodiments, the actual number of layers of the P-type DBR section 10 is set to 32 layers, that is, a structure of 16 pairs; in other embodiments, the actual number of layers of the P-type DBR section 10 is set to 16 layers, that is, a structure of 8 pairs; in still other embodiments, the actual number of layers of the P-type DBR section 10 is set to 40 layers, that is, a structure of 20 pairs. Since the number of layers of the P-type DBR section 10 may also cause changes in the overall VCSEL performance, the actual number of layers needs to be set according to actual conditions.

[0057] In a further embodiment, the thickness H of each layer of the P-type DBR portion 10 is controlled to be 1-1.5 um.

[0058] In some embodiments, the thickness of each layer of the P-type DBR portion 10 is controlled to be 1.2 um, and when the P-type DBR portion 10 has a 32-layer structure, the total thickness is 38.4 um; in other embodiments, the thickness of each layer of the P-type DBR portion 10 is controlled to be 0.8 um, and when the P-type DBR portion 10 has a 40-layer structure, the total thickness is 32 um; the thickness of each layer of the P-type DBR portion 10 is controlled to be 1.6 um, and when the P-type DBR portion 10 has a 16-layer structure, the total thickness is 25.6 um.

[0059] In a further embodiment, the P-type DBR part 10 is made of Al0.1GaAs and Al0.9GaAs.

[0060] In the embodiment, the P-type DBR portion 10 is composed of two materials of different components (Al0.1GaAs and Al0.9GaAs), and the two materials of different components are alternately arranged layer by layer to obtain the P-type DBR portion 10 .

[0061] In a further embodiment, the N-type electrode is AuGeNi alloy plated material with a thickness of 500Å; the P-type electrode is Ti / Au with a thickness of 500Å / 3000Å.

[0062] Based on the same inventive concept, a VCSEL laser is also disclosed, comprising: the VCSEL chip described in any one of the above.

[0063] For specific examples and descriptions of beneficial effects of the VCSEL laser described in this embodiment, reference may be made to the description of the above-mentioned VCSEL chip, which will not be repeated here.

[0064] Based on the same inventive concept, a method for preparing a VCSEL chip is also disclosed, the steps comprising: S001: Make epitaxial wafers and obtain the required epitaxial wafers through epitaxial growth technology.

[0065] In the embodiment, when preparing the VCSEL chip, a complex multilayer film structure is deposited on the substrate 13 by metal organic chemical vapor deposition (MOCVD) or molecular beam epitaxy (MBE) process.

[0066] Growth on substrate 13 is a key step in the entire process, which directly determines the quality and performance of the device. Usually, substrate 13 is gallium arsenide. In some embodiments, the step is to alternately grow GaAs and AlAs on substrate 13, and the alternately grown layers eventually form a Bragg reflector. Since GaAs and AlAs have significantly different refractive indices, but their lattice constants are basically the same, many layers can be alternately grown without dislocations, which is why a high-reflectivity mirror effect can be produced. During the growth process, it is necessary to control parameters such as growth rate, temperature, and pressure to obtain a high-quality epitaxial layer.

[0067] Epitaxial growth is the process of placing the cut silicon wafers in a high-temperature furnace and using vapor deposition to grow semiconductor materials with a specific energy level structure on the epitaxial layer, thus obtaining epitaxial wafers.

[0068] Embodiment: Before the next step is carried out, the epitaxial wafer needs to be cleaned and the cleanliness of the epitaxial wafer needs to be checked to prevent foreign objects from affecting other steps and causing defective products.

[0069] The specific steps include: using acetone and isopropanol chemical reagents to clean the epitaxial wafer for 5 minutes in sequence, then cleaning it with deionized water in sequence, and finally drying it. Then, the surface of the epitaxial wafer after cleaning and drying is checked under a microscope to specifically check whether there are foreign objects, dust, pollution, color patterns, water stains, etc. This ensures the cleanliness of the epitaxial wafer, prevents it from affecting the next process steps, and reduces the occurrence of defective products.

[0070] S002: Prepare a mask, and use photoresist to make a corresponding pattern on the substrate to obtain a first mask and a second mask.

[0071] In the embodiment, except that the structure of the first mesa is different from that of the existing vcsel chip, the structure of the second mesa and the electrode is the same as that of the existing vcsel chip, that is, during photolithography, the etching process of the first mesa is different from the existing etching process, while the etching process of the second mesa and the electrode is the same as the traditional etching process.

[0072] In order to obtain the step structure on the outer surface of the VCSEL chip, the embodiment prepares a first mask 20, and the step structure can be etched on the epitaxial wafer through the first mask 20 during photolithography. The other structures are the same as the traditional structures, so the masks required for photolithography in other stages, such as the second mask, can refer to the existing mask manufacturing process. The manufacturing process steps of the first mask 20 are as follows: In a further embodiment, the first mask 20 is manufactured by a two-photon polymerization 3D printing process, and the specific steps include: On the substrate 22, a positive photoresist is printed into a soft mask using a 3D printing process; A plurality of uniform protruding structures 210 are printed on the soft mask, and bosses 211 are printed uniformly distributed along a direction on the surface of each protruding structure 210 .

[0073] See attached Figure 7 As shown, the embodiment further includes: the first mask 20, used for VCSEL chip lithography pattern, including: A substrate 22 and a pattern layer 21, wherein the pattern layer 21 is disposed on one side of the substrate 22; A plurality of protruding structures 210 are disposed on the side of the pattern layer 21 away from the substrate 22 , and the protruding structures 210 are arranged in sequence and side by side along a straight line, and bosses 211 are evenly disposed on the surfaces of the protruding structures 210 .

[0074] It is understandable that due to the current structure of the current high-speed modulated VCSEL chip, there are problems of large internal resistance and poor thermal effect. In order to be able to obtain a P-type DBR part 10 that can reduce the internal resistance and has a good heat dissipation effect when the P-type DBR part 10 is used for VCSEL chips. In an embodiment, a pattern layer 21 is arranged above the substrate 22, and a plurality of protruding structures 210 are arranged on the side of the pattern layer 21 away from the substrate 22, and the protruding structures 210 are arranged in sequence side by side in a straight line direction, and bosses 211 are evenly arranged on the surface of the protruding structures 210. In this way, the protruding structures 210 of the pattern layer 21 and the bosses 211 on the protruding structures 210 can be obtained in the P-type DBR part 10 through etching technology to obtain the required structure, so that the VCSEL chip has a better heat dissipation effect and reduces the internal resistance of the VCSEL chip.

[0075] When working in real time, when preparing a VCSEL chip, the mask is set on a photolithography machine to perform photolithography on the epitaxial wafer, and the pattern on the pattern layer 21 on the mask can be etched onto the epitaxial wafer to obtain the desired shape and pattern, so that the VCSEL chip prepared using the mask can achieve reduced internal resistance and better heat dissipation.

[0076] Since the pattern layer 21 of the mask is away from the side of the substrate 22, a plurality of protruding structures 210 are provided, and the protruding structures 210 are arranged in a straight line in sequence, and bosses 211 are evenly arranged on the surface of the protruding structures 210. During photolithography, the thinner position on the pattern layer 21 will disappear first, and then the other parts will gradually disappear, so that the pattern on the pattern layer 21 is photolithographically transferred to the epitaxial wafer, so that the outer surface of the P-type DBR part 10 has a stepped shape. The protruding structure 210 is set to a structure with both sides gradually protruding toward the center. See attached Figure 8 As shown, in a further embodiment, the bosses 211 are evenly arranged along the side straight lines of the protruding structures 210 and are connected in sequence.

[0077] It can be understood that, on the side of the protruding structure 210, the bosses 211 are sequentially arranged along the edge of the side, and the bosses 211 are arranged to be connected at the end, that is, by arranging the pattern layer 21 on the upper side of the substrate 22, the pattern layer 21 is arranged with multiple protruding structures 210, and the protruding structure 210 is a gradually protruding structure during photolithography, and the bosses 211 are evenly arranged on the protruding structure 210, so that when the photolithography continues, a step structure can be effectively formed on the surface of the P-type DBR part 10. To ensure the accuracy of photolithography, the step structure formed on the surface of the P-type DBR part 10 can effectively reduce the internal resistance of the chip as a whole and improve the efficiency of heat dissipation.

[0078] See attached Fig. 9 and 10 As shown, in the embodiment, the protrusion height of the boss 211 is controlled to be 1-1.5 um.

[0079] It can be understood that the height difference between the two sides of the two adjacent bosses 211 of the boss 211 that are parallel to the substrate 22 is 0.8-2um. In the embodiment, by controlling the protrusion height of the boss 211, the structural height of the P-type DBR part 10 obtained during photolithography is achieved. It can also be considered that by controlling the height of the boss 211, the height of the step structure formed on the surface of the P-type DBR part 10 during photolithography can be achieved.

[0080] In some embodiments, the height of the boss 211 can be set according to the thickness of each layer in the P-type DBR section 10 obtained by epitaxial wafer growth. For example, when the thickness of each layer in the P-type DBR section 10 is 1 um, when the boss 211 of the mask is manufactured, the height of the boss 211 is set to 1 um; when the thickness of each layer in the P-type DBR section 10 is 2 um, when the boss 211 of the mask is manufactured, the height of the boss 211 is set to 2 um; when the thickness of each layer in the P-type DBR section 10 is 0.8 um, when the boss 211 of the mask is manufactured, the height of the boss 211 is set to 0.8 um.

[0081] See attached Fig.10 As shown, in a further embodiment, the boss 211 includes a first side surface, and the first side surface is connected to the substrate 22 .

[0082] In order to ensure the stepped shape of the P-type DBR portion 10 of the VCSEL chip, so that the overall VCSEL chip obtains the required structure, so that the overall internal resistance of the P-type DBR portion 10 can be effectively reduced, and the heat dissipation effect will be better, in an embodiment, at least one first side surface is provided on the boss 211, and the first side surface is parallel to the substrate 22.

[0083] In the embodiment, the first side surface may be a plane or other planes. It can be understood that by setting the shape of the first side surface of the boss 211, the desired selection can be obtained on the P-type DBR portion 10 during photolithography. For example, in the embodiment, the first side surface is set as a plane, and the first side surface is set parallel to the substrate 22. When the epitaxial wafer is photolithographically processed, a corresponding plane can be obtained on the P-type DBR portion 10.

[0084] In a further embodiment, the distance between the protrusion structures 210 is 0-1 um.

[0085] It can be understood that the distance between the protruding structures 210 can be considered as the distance between the closest positions of two protruding structures 210 that are close to each other. The distance can be 0, or the two can be separated by a certain distance.

[0086] In some embodiments, the distance between two adjacent protrusion structures 210 is set to 0, that is, the closest position of the two is in contact with each other; in other embodiments, the distance between two adjacent protrusion structures 210 is set to 0.5 um, that is, the closest position of the two is at a certain distance; in still other embodiments, the distance between two adjacent protrusion structures 210 is set to 0.8 um, that is, the closest position of the two is at a certain distance.

[0087] See attached Fig.11As shown, in a further embodiment, the transverse cross-section of the protrusion structure 210 is triangular or trapezoidal.

[0088] It can be understood that the transverse cross section here can be considered as a cross section opposite to the end face of the protruding structure 210, or the protruding structure 210 can be considered as a structure extending in one direction, and the cross section here is a cross section perpendicular to the extending direction.

[0089] In one embodiment, the transverse cross section of the protruding structure 210 is set to a triangular structure, where the angle of the triangle can be rounded, and when performing photolithography, the pattern will show a phenomenon that the cross-sectional area of ​​the triangle gradually decreases, or the cross-sectional area of ​​the triangle is proportionally reduced; in another embodiment, the transverse cross section of the protruding structure 210 is set to a trapezoidal structure, where the angle of the trapezoid can be rounded, and when performing photolithography, the pattern will show a phenomenon that the cross-sectional area of ​​the trapezoid gradually decreases. Of course, the protruding structure 210 can also be designed into other shapes according to the actual chip design requirements, which are not listed here one by one.

[0090] In a further embodiment, the pattern layer 21 is a film layer made of positive photoresist.

[0091] It can be understood that in order to ensure that the P-type DBR portion 10 of the VCSEL chip can obtain a stepped shape, an embodiment is that a pattern layer 21 is made of positive photoresist. During photolithography, the raised structure 210 on the pattern layer 21 is a gradually raised structure, and a boss 211 is provided on the raised structure 210. During photolithography, the pattern layer 21 made of the positive photoresist gradually disappears. The disappearance here starts from the part closest to the substrate 22 and gradually proceeds to the highest part of the boss 211 structure.

[0092] It should be noted that the characteristic of positive photoresist is that after the coating is exposed and developed, the exposed part is dissolved and the unexposed part remains. Therefore, when using positive photoresist for photolithography, the photoresist on the exposed part will gradually disappear, while the photoresist on the unexposed part will remain to form the desired image.

[0093] In a further embodiment, the substrate 22 is a quartz plate.

[0094] S003: Etching the pattern on the first mask 20 onto the VCSEL by etching to obtain a first mesa.

[0095] In the embodiment, the etching can be achieved by an existing etching process method, which is not described in detail here. The embodiment uses an existing etching process to etch the pattern on the first mask 20 onto the epitaxial wafer, thereby obtaining a stepped shape in the P-type DBR part 10.

[0096] In the embodiment, after obtaining the first table, the accuracy of the boss 211 on the first table is measured by a step meter. Specifically, the step meter is used to measure the etching depth of four to six points randomly selected on the surface of the first table to determine the accuracy of the etching.

[0097] S004: After obtaining the first mesa, the VCSEL is placed in a wet oxidation device for oxidation.

[0098] In the embodiment, the wet oxidation of VCSEL is between the etching of the first mesa and the etching of the second mesa. Specifically, the VCSEL after the etching of the first mesa is placed in a wet oxidation device for oxidation, and the high aluminum component layer in the epitaxial structure of the VCSEL will be oxidized by a large amount of water vapor carried by nitrogen. Then, the oxidation time and rate are controlled, and the infrared light source charge coupled device image sensor (CCD) system is used to perform real-time observation to achieve the purpose of accurately controlling the size of the oxidation aperture.

[0099] S005: Etching the pattern on the second mask onto the VCSEL by etching to obtain a second mesa.

[0100] In the embodiment, the etching process used includes three parts, including etching to obtain the first mesa, the second mesa and the P-type electrode region conductive layer, etc. In the embodiment, the etching process can refer to the existing etching process, which is not described in detail here.

[0101] Furthermore, in the embodiment, the etching process steps and parameters of the first mesa, the second mesa and the conductive layer in the P-type electrode region are consistent, except that photolithography is performed using masks with different patterns.

[0102] That is, after the second mesa etching is performed, the P-type electrode region conductive layer is then etched, thus completing the etching step.

[0103] S006: VCSEL sets the N-type electrode by evaporation, and sets the P-type electrode and P / N ohmic contact by sputtering.

[0104] Embodiment: After the etching process, in order to provide circuit transmission and reflection, the VCSEL needs to be provided with corresponding electrodes through metal evaporation and electroplating processes. The details are as follows: First, electron beam evaporation is used to obtain an N-type electrode on the VCSEL. The metal material used for the N-type electrode is AuGeNi alloy plating material, and the thickness of the N-type electrode is 500Å. Next, the VCSEL plated with the N-type electrode is planarized using the BCB planarization process; Next, a P-type electrode is disposed on the top of the first mesa of the VCSEL using a magnetron sputtering coating process, wherein the metal material used for the P-type electrode is Ti / Au, and the thickness of the P-type electrode is 500Å / 3000Å; Finally, the VCSEL with plated electrodes is placed in a rapid annealing furnace for rapid annealing to achieve the purpose of alloying, so that the electrodes form good ohmic contact with the semiconductor material and improve the electrical properties of the device.

[0105] In the embodiment, after the evaporation process, a silicon dioxide protective layer needs to be deposited on the VCSEL. Specifically, silicon nitride (Si3N4) or silicon dioxide (SiO2) is used as a passivation insulating protective layer and an exit window protection and anti-reflection layer by a thin film deposition process. The thickness of the passivation insulating protective layer is generally about 2000Å; the exit window protection and anti-reflection layer are generally coated with a thin film with an optical thickness of λ / 4.

[0106] In the present application, the surface of the P-type DBR part 10 of the VCSEL is set to a stepped structure, and each step of the stepped structure corresponds to each layer in the P-type DBR part 10, thereby effectively improving the overall performance of the P-type DBR part 10. As a result, the overall equivalent resistance of the VCSEL can be effectively reduced, and the heat dissipation is also improved, thereby improving the thermal stability and high-speed modulation performance of the chip.

[0107] In order to obtain a stepped structure on the surface of the P-type DBR portion 10 , in an embodiment, a pattern structure on a mask is designed, and the pattern is etched into the P-type DBR portion 10 through an etching process, thereby obtaining a stepped structure.

[0108] In the embodiment, each step of the stepped structure corresponds to each layer in the P-type DBR section 10. For example, the P-type DBR section 10 has 32 layers in total, and the height of each layer is 1um. The steps also have 32 steps, and the height of each step is 1um. The steps can also be considered as the layers in the P-type DBR section 10, which are gradually staggered from the bottom right to the top.

[0109] For specific examples and descriptions of beneficial effects of the method described in this embodiment, reference may be made to the description of the saturable absorber described above, which will not be repeated here.

[0110] Obviously, various changes and modifications may be made to the present invention by those skilled in the art without departing from the spirit and scope of the present invention. The present disclosure is not limited to the precise structure described above and shown in the accompanying drawings, and various changes and modifications may be made without departing from the scope thereof. The scope of the present disclosure is limited only by the appended claims. Thus, if these changes and modifications of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these changes and modifications.

Claims

1. A VCSEL chip for semiconductor laser, characterized in that: include: An N-electrode, an N-type DBR portion, an active portion, a P-type DBR portion, and a P-electrode, wherein the N-electrode, the N-type DBR portion, the active portion, the P-type DBR portion, and the P-electrode are sequentially stacked from bottom to top; The P-type DBR part is configured as a multi-layer structure stacked in sequence, and the lateral area of ​​each layer of the multi-layer structure gradually decreases from bottom to top; Furthermore, the adjacent layers of the multilayer structure are arranged such that: the upper edge distance of the DBR layer at the lower position is the same as the lower edge distance of the DBR layer at the upper position.

2. The VCSEL chip according to claim 1, characterized in that: The distance is controlled to be 0.8-2um.

3. The VCSEL chip according to claim 1, characterized in that: The transverse cross-sectional shape of the P-type DBR portion includes a circle, an ellipse or a rectangle.

4. The VCSEL chip according to claim 1, characterized in that: The number of layers of the P-type DBR part is 16-40 layers.

5. The VCSEL chip according to claim 1, characterized in that: The thickness of each layer of the P-type DBR part is controlled to be 1-1.5 um.

6. The VCSEL chip according to claim 1, characterized in that: The P-type DBR part is made of material.

7. The VCSEL chip according to claim 1, characterized in that: The N-type electrode is AuGeNi alloy plated material with a thickness of 500Å; the P-type electrode is Ti / Au with a thickness of 500Å / 3000Å.

8. A VCSEL laser, characterized in that: include: The VCSEL chip according to any one of claims 1 to 7.

9. A mask, characterized in that: Used for etching the VCSEL chip described in any one of claims 1 to 7.

Citation Information

Patent Citations

  • Vertical cavity surface emitting laser with controllable laser phase distribution and manufacturing method thereof

    CN111613966A

  • VCSEL chip and preparation method thereof

    CN113451883A

  • Vertical cavity surface emitting laser and preparation method thereof

    CN117913651A

  • VCSEL Chip Having a Step, VCSEL Array and Method for Manufacturing thereof

    KR102412761B1

  • Vertical-cavity surface-emitting transistor laser, t-vcsel and method for producing the same

    US20150318666A1

Cited By

  • VCSEL chip preparation method and VCSEL chip

    CN119050808A