Adsorption member and suspension
By using a suspension with an alcohol component of less than 1% and a binder with hydrophilic groups in an adsorption heat exchanger, the crack problems caused by the swelling and shrinkage of the adsorbent layer are solved, and the equipment cost is reduced. Improves moisture absorption performance.
Patent Information
- Application Number
- CN202310636303.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-31
- Publication Date
- 2024-12-03
AI Technical Summary
The existing adsorption heat exchangers have problems such as cracks, peeling and performance fluctuations in the formation of adsorbent layer, and the use of flammable alcohol as solvent requires explosion-proof response, which increases equipment investment.
The adsorbent layer formed by using a suspension in which the alcohol component in the solvent is less than 1 mass % and adding hydrophilic groups such as hydroxyl groups, amino groups, carboxyl groups, etc. to the binder to reduce the deformation of the adsorbent shape and improve the Hygroscopicity.
No explosion-proof response measures are required, which reduces equipment costs, while improving the adsorbent layer's adhesion and moisture absorption performance, avoiding cracks and peeling problems.
Smart Images

Figure CN119056207A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to an adsorption component for an adsorption heat exchanger and a suspension for making the adsorption component. The suspension refers to a solution containing an adsorbent. Background Art
[0002] Adsorption heat exchangers having a heat exchanger body for exchanging heat between a heat transfer medium such as a refrigerant and air and an adsorbent layer formed on the surface of the heat exchanger body are widely known. For example, Patent Documents 1 and 2 disclose such adsorption heat exchangers.
[0003] The adsorbent layer of the adsorption heat exchanger contains an adsorbent that absorbs moisture from the air and releases moisture to the air. The adsorbent can be an inorganic material such as silica gel or zeolite, or an organic material having hygroscopicity. The adsorption heat exchangers disclosed in Patent Documents 1 and 2 use an adsorbent made of an organic polymer material, and the adsorbent adsorbs and absorbs water vapor.
[0004] The adsorbents disclosed in Patent Documents 1 and 2 are as follows: multiple polymer main chains having hydrophilic polar groups in the molecule are cross-linked with each other, and a three-dimensional structure is formed by the multiple cross-linked polymer main chains. Then, the adsorbent undergoes two phenomena: water vapor is adsorbed by the hydrophilic polar groups, and water vapor is absorbed by the three-dimensional structure formed by the polymer main chains. As a result, the adsorbent can capture a large amount of water vapor compared to zeolite, etc., which only adsorbs water vapor on the surface.
[0005] Paragraph 0055 of Patent Document 1 and Paragraph 0053 of Patent Document 2 disclose a method in which a powder of a particulate adsorbent is mixed with a solvent and then applied to a heat exchanger body, and then the solvent is evaporated to form an adsorbent layer on the surface of the heat exchanger body.
[0006] However, conventional adsorption heat exchangers do not take into account the deformation of the adsorbent shape, such as swelling and shrinkage of the adsorbent during the formation of the adsorbent layer. As a result, problems such as cracks in the adsorbent layer occur.
[0007] That is, the existing adsorption heat exchanger forms an adsorbent layer by coating a suspension of a mixture of an adsorbent and a solvent and drying the suspension, but water is mainly used as the solvent of the suspension. If water is used as the solvent, the adsorbent that temporarily swells after absorbing water shrinks during the drying process. As a result, there are problems such as cracks and peeling. In addition, there are problems such as the generation of coating spots and performance fluctuations due to the shrinkage of the adsorbent. In addition, there are problems such as the adhesive coverage rate of the adhesive covering the adsorbent increases and the water absorption performance decreases.
[0008] In addition, since the adsorbent swells again when the suspension is repeatedly applied, the gaps between the fins become narrow, the fluidity decreases, and the pores become clogged. Then, since the adhesive cannot withstand the swelling of the adsorbent, it peels off. In addition, since the adsorbent absorbs a large amount of water, the drying time is prolonged.
[0009] In response to this problem, Patent Document 3 conducted a long-term study on adsorbents that cause two phenomena: the phenomenon of water vapor being adsorbed by hydrophilic polar groups and the phenomenon of water vapor being absorbed by a three-dimensional structure formed by a polymer main chain. The results showed that by using alcohol as the main component of the solvent when forming an adsorbent layer containing the adsorbent, the shape deformation of the adsorbent can be suppressed.
[0010] Prior art literature
[0011] Patent Literature
[0012] Patent Document 1: International Application Publication No. 2006 / 077672
[0013] Patent Document 2: Japanese Patent Application Publication No. 2007-132614
[0014] Patent Document 3: International Application Publication No. 2010 / 134315 Pamphlet Summary of the invention
[0015] Problems to be solved by the invention
[0016] However, as described in Patent Document 3, in the manufacturing process of the adsorption heat exchanger, the adsorbent, the binder (polymer resin) and the solvent are mixed to form a suspension (fluid), and the adsorbent is attached to the substrate sheet. At this time, since flammable alcohol is used as the solvent, explosion-proof measures are required in the manufacturing equipment, which leads to the problem of increased equipment investment.
[0017] Technical means to solve problems
[0018] The present invention has been made in view of the above problems, and its object is to provide an adsorption component that does not require explosion-proof measures. In addition, the present invention also aims to provide a suspension for forming an adsorbent layer of the above adsorption component.
[0019] Specifically, the inventors focused on the solvent used to form the adsorbent layer of the adsorption component, specifically, instead of using alcohol as the main component of the solvent, the solvent contained a smaller amount of alcohol component, and found a group (hydrophilic group) contained in the adhesive that can easily react chemically with the hydrophilic layer components of the fin.
[0020] Specifically, the technical solution of the present invention is as follows.
[0021] The first aspect of the invention is an adsorption component for an adsorption heat exchanger, characterized in that an adsorbent layer containing an adsorbent is coated on the surface of a substrate sheet of the adsorption component, and the content of alcohol components in the adsorbent layer is 1% by mass or less.
[0022] The second invention is based on the first invention, wherein the base sheet is surface treated.
[0023] The third invention is the second invention, wherein the surface treatment is to sequentially stack a corrosion-resistant layer and a hydrophilic layer on the substrate sheet.
[0024] The fourth aspect of the invention is directed to a suspension used to form an adsorbent layer of an adsorption component in an adsorption heat exchanger, characterized in that the suspension is obtained by mixing an adsorbent, a binder and a solvent, wherein the alcohol component in the solvent accounts for less than 20% by mass of the entire suspension.
[0025] The fifth invention is the fourth invention, wherein the suspension is applied to a substrate sheet to obtain an adsorption member.
[0026] The sixth invention is the invention according to the fourth or fifth aspect, wherein the binder contains a hydrophilic group.
[0027] The seventh invention is that in the sixth invention, the hydrophilic group is at least one of a hydroxyl group, an amino group, a carboxyl group and a metal sulfonic acid group.
[0028] The eighth invention is the fourth invention, characterized in that an elastomer is further added.
[0029] The ninth aspect of the invention is directed to a heat exchanger using the adsorption member according to any one of the first to third aspects, or the adsorption member having an adsorbent layer formed of the suspension according to any one of the fourth to eighth aspects.
[0030] The tenth invention is directed to a humidity control device equipped with the heat exchanger according to the ninth invention.
[0031] Effects of the Invention
[0032] According to the present invention, an adsorption component that does not require explosion-proof measures can be provided. In addition, a suspension can be provided for forming an adsorbent layer of the adsorption component. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] 1(A) and 1(B) are piping system diagrams showing the refrigerant circuit structure of the humidity control device, FIG. 1(A) shows the operation in the first operation, and FIG. 1(B) shows the operation in the second operation.
[0034] Figure 2 This is a schematic perspective view of an adsorption heat exchanger.
[0035] Figure 3 It is a side view of a heat exchanger unit constituting the adsorption heat exchanger.
[0036] Figure 4 Yes means Figure 3 Section view of section AA in the figure.
[0037] Figure 5 This is a process diagram showing a method for manufacturing an adsorption heat exchanger.
[0038] 6(A) to (E) are structural diagrams schematically showing the states of the adsorbent and the binder in the suspension according to the present embodiment. DETAILED DESCRIPTION
[0039] <Suspension>
[0040] First, the suspension and its constituent components for forming the adsorbent layer of the adsorption member of the present embodiment will be described in detail.
[0041] The suspension of this embodiment contains an adsorbent, a binder, and a solvent. As an example of the specific composition of the suspension, it is as follows: 100 parts by mass of the adsorbent, 30 parts by mass of the binder, 470 parts by mass of water, and less than 30 parts by mass of alcohol. In other words, the solvent is composed of 470 parts by mass of water and 30 parts by mass of alcohol. And, the binder and water are used in the form of a water-based resin (hydrophilic resin).
[0042] The above-mentioned adsorbent is specifically as follows: a plurality of polymer main chains having hydrophilic groups are cross-linked to form a three-dimensional structure. Furthermore, when the adsorbent absorbs moisture from the air, both adsorption and absorption of water vapor are performed simultaneously.
[0043] Furthermore, regarding the above-mentioned adhesive, adhesives commonly used in the field of heat exchangers, such as fluororesins, acrylic resins, epoxy resins, and urethane resins, etc., can be used. In addition, in the present invention, the solvent is mainly composed of water, so it is preferred that the adhesive contains a group (hydrophilic group) that is easy to chemically react with the hydrophilic layer components of the adsorption component. In this way, not only can the dispersibility of the adhesive in water be improved, but also the effect of improving the hygroscopicity of the adsorbent layer is unexpectedly obtained as the close adhesion of the adsorption component is improved. Regarding the introduction amount of the hydrophilic group, the hydrophilic component containing the hydrophilic group is preferably 1 to 5 mass%, more preferably 1.3 to 1.8 mass%, relative to 100 mass% of the entire suspension.
[0044] The hydrophilic component containing the hydrophilic group is not particularly limited, but for example, it includes a low molecular organic compound or a high molecular compound containing a hydroxyl group, an amino group, an amide group, a carboxyl group or an alkali metal salt thereof, a sulfonic acid group or an alkali metal salt thereof or a derivative thereof, or a low molecular organic compound or a high molecular compound containing two or more ether bonds in one molecule. Specific examples of the hydrophilic component include: polyvinyl alcohol, starch, homopolymers or copolymers of acrylic acid, homopolymers or copolymers of methacrylic acid, homopolymers or copolymers of maleic anhydride (e.g., maleic anhydride-styrene copolymers), polyethylene sulfonic acid or its copolymers or their alkali metal salts, polyethylene glycol (also known as polyethylene oxide), polypropylene glycol, polyethylene-propylene glycol, polytetramethylene glycol and other polyalkylene glycols, glycerol, polyglycerol and other polyols or polymers thereof, water-soluble modified cellulose (e.g., hydroxyethyl cellulose, methyl cellulose, methyl hydroxypropyl cellulose, sodium carboxycellulose, cellulose nitrate carboxymethyl ether), etc. As the hydrophilic group, it is preferably at least one of a hydroxyl group, an amino group, a carboxyl group and a metal sulfonic acid group.
[0045] It should be noted that, as mentioned above, the solvent is composed of 470 parts by mass of water and 30 parts by mass of alcohol. However, the alcohol content of the above-mentioned solvent is only an example. In the present embodiment, the alcohol component in the solvent accounts for less than 20% by mass of the entire suspension. From the viewpoint of further exerting the effect of the present invention, it is preferably less than 10% by mass, and more preferably 3% to 5% by mass. It should be noted that the upper limit of the content of the alcohol component must be greater than 0% by mass, considering the influence of water as a solvent on the adsorbent, that is, it does not include the case of 0% by mass. In this way, in the suspension of the present invention, alcohol is not used as the main component, so it is similar to the hydrophilic layer coating with a water content of more than 95%, and the adhesion of the two is improved. As the type of alcohol, there is no particular limitation, and ethanol, isopropanol, butyl cellosolve (ethylene glycol monobutyl ether) and the like can be cited.
[0046] The type and content of the alcohol in the suspension of the present invention can be identified by FT-IR.
[0047] Furthermore, there is a difference in the linear thermal expansion coefficient between the adsorbent layer and the substrate sheet, thereby generating thermal stress, and shear stress acts on the bonding surface between the adsorbent layer and the substrate sheet. As a result, there is a risk that the above-mentioned adsorbent layer will peel off from the substrate sheet. In order to avoid such a risk, an elastomer can be added to the suspension. As elastomers that can be used, there is no particular limitation, and examples thereof include oxazoline compounds, vinyl ether compounds, epoxy compounds, oxetane compounds, polyol compounds, polyamide polyamine epoxy halogen adducts, hydroxyacrylamide compounds, oxazolone compounds, bisoxazolone compounds or polyoxazolone compounds, 2-oxotetrahydro-1,3-oxazolidine compounds, alkylene carbonate compounds, and the like.
[0048] <Adsorption parts>
[0049] The adsorption component of this embodiment is used in an adsorption heat exchanger, and the adsorption component has an adsorbent layer stacked on the surface of a substrate sheet. A suspension containing the adsorbent is applied to the surface of the substrate sheet of the adsorption component, and the suspension is dried to form an adsorbent layer containing the adsorbent on the surface of the substrate sheet, and the content of the alcohol component in the adsorption component is 1% by mass or less. It should be noted that the upper limit of the content of the alcohol component must be greater than 0% by mass, that is, 0% by mass is not included, considering the influence of water as a solvent on the adsorbent.
[0050] The type and content of the alcohol in the adsorption member of the present invention can be identified by FT-IR.
[0051] The substrate sheet of the adsorption component of the present embodiment can be surface treated. As surface treatment, it can be cited as: coating the surface of the substrate sheet with a corrosion-resistant coating, a hydrophilic coating, etc. After the substrate sheet is immersed in a suspension to form an adsorbent layer, the suspension adheres to the hydrophilic layer of the fin, but if it is a solvent containing an alcohol component, the adhesion between the hydrophilic layer of the substrate sheet and the adsorbent layer obtained from the suspension is reduced, but if the suspension contains a hydrophilic group, the adhesion between the hydrophilic layer of the substrate sheet and the adsorbent layer of the suspension is improved. In addition, due to the influence of the hydrophilic group of the suspension, water easily reacts with the adsorbent layer coated on the fin, and the hygroscopicity of the adsorbent layer is improved.
[0052] By treating the surface of the substrate sheet in this manner, effects other than flame retardancy can be expected. The adsorption member according to the embodiment of the present invention is formed by laminating a corrosion-resistant layer, a hydrophilic layer, and an adsorbent layer in this order on a substrate sheet.
[0053] <Humidity Control Device, Adsorption Heat Exchanger>
[0054] The adsorption member of this embodiment is applied to an adsorption heat exchanger of a humidity control device, and therefore, the humidity control device and the adsorption heat exchanger of the present invention are described in detail below with reference to the drawings. It should be noted that the adsorption member of this embodiment corresponds to a "fin" in the adsorption heat exchanger.
[0055] <Structure of humidity control device>
[0056] As shown in Fig. 1, in this embodiment, an adsorption heat exchanger (20) is provided in the humidity control device. The humidity control device is configured to be able to perform a dehumidification function of supplying dehumidified air to the room and a humidification function of supplying humidified air to the room.
[0057] The humidity control device includes a refrigerant circuit (10). The refrigerant circuit (10) is a closed circuit provided with a first adsorption component (11), a second adsorption component (12), a compressor (13), a four-way switching valve (14), and an electric expansion valve (15), and is filled with a refrigerant. The refrigerant circuit (10) performs a vapor compression refrigeration cycle by circulating the refrigerant. Moreover, the first adsorption component (11) and the second adsorption component (12) are both composed of the adsorption heat exchanger (20) involved in the present invention.
[0058] The discharge side of the compressor (13) is connected to the first port of the four-way switching valve (14), and the suction side is connected to the second port of the four-way switching valve (14). One end of the first adsorption component (11) is connected to the third port of the four-way switching valve (14). The other end of the first adsorption component (11) is connected to one end of the second adsorption component (12) via the electric expansion valve (15). The other end of the second adsorption component (12) is connected to the fourth port of the four-way switching valve (14).
[0059] The above-mentioned four-way switching valve (14) can be switched into two states, namely, a first state in which the first port is connected to the third port and the second port is connected to the fourth port (the state shown in Figure 1(A)), and a second state in which the first port is connected to the fourth port and the second port is connected to the third port (the state shown in Figure 1(B)).
[0060] <Structure of adsorption heat exchanger>
[0061] As described above, the first adsorption component (11) and the second adsorption component (12) are respectively constituted by an adsorption heat exchanger (20). Figure 2 , Figure 3 and Figure 4 The adsorption heat exchanger (20) will be described.
[0062] The adsorption heat exchanger (20) includes two subunits (subunits) (21) and (22) (refer to Figure 2 Each subunit (21), (22) includes a so-called cross-fin type fin and tube heat exchanger, i.e., a heat exchanger body (25), and an adsorbent layer (30) formed on the surface of the heat exchanger body (25) (see Figure 4 The two subunits (21) and (22) of the adsorption heat exchanger (20) are arranged to overlap each other, the first subunit (21) is located on the upstream side of the air flow passing through the adsorption heat exchanger (20), and the second subunit (22) is located on the downstream side of the air flow.
[0063] The heat exchanger body (25) includes a heat transfer tube component, i.e., a circular heat transfer tube (27) and a plurality of fins (26). Each fin (26) is an aluminum component in the shape of a rectangular plate. Each fin (26) is arranged in parallel in a state facing each other and arranged in a row at a certain interval. The heat transfer tube (27) is formed into a shape in which a straight tube portion (28) and a U-shaped tube portion (29) alternately snake left and right. The straight tube portion (28) of the heat transfer tube (27) is arranged to pass through each of the arranged fins (26). The straight tube portion (28) of the heat transfer tube (27) is joined to the fin (26), and the outer peripheral surface of the straight tube portion (28) is tightly joined to the fin (26).
[0064] like Figure 4 As shown, the adsorbent layer (30) is covered on both sides of the fin (26). The thickness ta of the adsorbent layer (30) is about 0.25 mm. Preferably, the thickness ta of the adsorbent layer (30) is greater than 0.1 mm and less than 0.35 mm (0.1 mm ≤ ta ≤ 0.35 mm). It should be noted that the adsorbent layer (30) is not only formed on the surface of the fin (26), but also formed on the surface of the portion of the heat transfer tube (27) not covered by the fin (26) (U-shaped tube portion (29), etc.). However, the thickness of the adsorbent layer (30) formed on the portion other than the fin (26) may also exceed the range of greater than 0.1 mm and less than 0.35 mm.
[0065] The adsorbent layer (30) contains an adsorbent (31) formed of a hygroscopic organic polymer material. The adsorbent (31) is, for example, in the form of particles having an average particle size of about 50 μm. In the adsorbent (31), a plurality of polymer main chains having hydrophilic polar groups (hydrophilic groups) in the molecules are cross-linked with each other, and the plurality of cross-linked polymer main chains form a three-dimensional structure.
[0066] The adsorbent (31) swells due to capturing water vapor (i.e., absorbing moisture). The mechanism of action of the adsorbent (31) swelling due to absorbing moisture is speculated as follows. That is, when the adsorbent (31) absorbs moisture, water vapor is adsorbed around the hydrophilic polar groups, and the force generated by the reaction of the hydrophilic polar groups with the water vapor acts on the polymer main chain, resulting in deformation of the polymer main chain. Then, the water vapor enters the gaps between the deformed polymer main chains through capillary force, and the entry of the water vapor causes the three-dimensional structure formed by multiple polymer main chains to expand, resulting in an increase in the volume of the adsorbent (31).
[0067] In this way, the adsorbent (31) provided in the adsorbent layer (30) of the present embodiment produces two phenomena: the phenomenon that water vapor is adsorbed by the adsorbent (31) and the phenomenon that water vapor is absorbed by the adsorbent (31). That is, the adsorbent (31) adsorbs and absorbs water vapor. Moreover, the water vapor captured by the adsorbent (31) not only enters the surface of the three-dimensional structure formed by a plurality of cross-linked polymer main chains, but also enters the interior of the structure. Therefore, compared with zeolite and the like that only adsorbs water vapor on the surface, the adsorbent (31) captures a large amount of water vapor.
[0068] The adsorbent (31) shrinks due to the release of water vapor (i.e., dehumidification). That is, when the adsorbent (31) dehumidifies, the amount of water captured in the gaps between the polymer main chains gradually decreases, and the shape of the three-dimensional structure formed by the multiple polymer main chains gradually recovers, so the volume of the adsorbent (31) decreases.
[0069] - Operation of the humidity control device -
[0070] Here, the operation of the humidity control device is described. The humidity control device performs dehumidification operation and humidification operation. The humidity control device repeatedly alternates between the first operation and the second operation at a predetermined time interval (for example, every 3 minutes) in both the dehumidification operation and the humidification operation.
[0071] In the dehumidification operation, the humidity control device sucks in outdoor air (OA) as the first air and indoor air (RA) as the second air. In the humidification operation, the humidity control device sucks in indoor air (RA) as the first air and outdoor air (OA) as the second air.
[0072] <First Action>
[0073] First, the first action is described. In the first action, the second air is sent to the first adsorption component (11), and the first air is sent to the second adsorption component (12). When performing the first action, the four-way switching valve (14) in the refrigerant circuit (10) is set to the first state. Once the compressor (13) is running, the refrigerant circulates in the refrigerant circuit (10) to cool. At this time, in the refrigerant circuit (10), the first adsorption component (11) works as a condenser, and the second adsorption component (12) works as an evaporator.
[0074] Specifically, the refrigerant discharged from the compressor (13) releases heat and condenses in the first adsorption component (11). The refrigerant condensed in the first adsorption component (11) is decompressed when passing through the electric expansion valve (15), and then absorbs heat and evaporates in the second adsorption component (12). The refrigerant evaporated in the second adsorption component (12) is sucked into the compressor (13), compressed, and then discharged from the compressor (13).
[0075] In the first adsorption component (11) formed of the adsorption heat exchanger (20), the adsorbent layer (30) on the surface of the fin (26) is heated by the refrigerant in the heat transfer tube (27) to dehumidify, and water vapor is released from the adsorbent layer (30) and given to the second air. In addition, in the second adsorption component (12) also formed of the adsorption heat exchanger (20), the adsorbent layer (30) on the surface of the fin (26) absorbs moisture from the first air, and the heat generated at this time is absorbed by the refrigerant in the heat transfer tube (27).
[0076] In the dehumidification operation, the first air dehumidified by the second adsorption element (12) is supplied to the room, and the water vapor released from the first adsorption element (11) is discharged to the outside together with the second air. On the other hand, in the humidification operation, the second air humidified by the first adsorption element (11) is supplied to the room, and the first air whose water vapor is absorbed by the second adsorption element is discharged to the outside.
[0077] <Second Action>
[0078] Next, the second action is described. In the second action, the first air is sent to the first adsorption component (11), and the second air is sent to the second adsorption component (12). When performing the second action, the four-way switching valve (14) in the refrigerant circuit (10) is set to the second state. Once the compressor (13) is running, the refrigerant circulates in the refrigerant circuit (10) to perform a refrigeration cycle. At this time, in the refrigerant circuit (10), the second adsorption component (12) works as a condenser and the first adsorption component (11) works as an evaporator.
[0079] Specifically, the refrigerant discharged from the compressor (13) releases heat and condenses in the second adsorption component (12). The refrigerant condensed in the second adsorption component (12) is decompressed when passing through the electric expansion valve (15), and then absorbs heat and evaporates in the first adsorption component (11). The refrigerant evaporated in the first adsorption component (11) is sucked into the compressor (13), compressed, and then discharged from the compressor (13).
[0080] In the second adsorption component (12) formed by the adsorption heat exchanger (20), the adsorbent layer (30) on the surface of the fin (26) is heated by the refrigerant in the heat transfer tube (27) to dehumidify, and the water vapor released from the adsorbent layer (30) is given to the second air. In the first adsorption component (11) also formed by the adsorption heat exchanger (20), the adsorbent layer (30) on the surface of the fin (26) absorbs moisture from the first air, and the heat generated at this time is absorbed by the refrigerant in the heat transfer tube (27).
[0081] In the dehumidification operation, the first air dehumidified by the first adsorption element (11) is supplied to the room, and the water vapor released from the second adsorption element (12) is discharged to the outside together with the second air. On the other hand, in the humidification operation, the second air humidified by the second adsorption element (12) is supplied to the room, and the first air whose water vapor has been absorbed by the first adsorption element (11) is discharged to the outside.
[0082] -Method for manufacturing adsorption heat exchanger-
[0083] Next, please refer to the detailed description of the manufacturing method of the above-mentioned adsorption heat exchanger (20) Figure 5 In the manufacture of the adsorption heat exchanger (20), a preparation step, a coating step and a drying step are performed. The coating step and the drying step are repeated and performed alternately.
[0084] First, the preparation step is a step of preparing a suspension (32) mixed with an adsorbent (31). As described above, the composition of the suspension (32) is as follows: 100 parts by mass of the adsorbent (31), 30 parts by mass of the binder (33), 470 parts by mass of water, and 30 parts by mass of alcohol.
[0085] The preparation process is as follows: a powdered adsorbent, which is mostly in the form of particles, i.e., a plurality of granular adsorbents (31) and a binder (33) are mixed in a solvent (34) to prepare a raw material liquid, i.e., a suspension (32). The adsorbent (31), the binder (33) and the solvent (34) in the suspension are fully stirred to fully disperse the adsorbent (31) and the binder (33) in the solvent (34).
[0086] The coating step is a dipping step of dipping the heat exchanger body (25) in the suspension (32). That is, the coating step is: dipping the heat exchanger body (25) composed of a common tube-fin type heat exchanger in the suspension (32) to coat the surface of the heat exchanger body (25) with the suspension (32). It should be noted that in the coating step, in order to make the suspension (32) spread over every corner of the heat exchanger body (25), the heat exchanger body (25) can be repeatedly immersed in and drawn out of the suspension (32), or the heat exchanger body (25) in the suspension (32) can be shaken. By doing so, the suspension (32) can fully enter the narrow space between the fins (26), so that the suspension (32) is firmly and evenly attached to the entire surface of the heat exchanger body (25).
[0087] It is noteworthy that the suspension (32) in the above-mentioned coating process contains the above-mentioned adsorbent (31) in a shrunken state. The shrunken state of the adsorbent (31) mentioned here means that the adsorbent (31) has only absorbed the water constituting the aqueous resin (hydrophilic resin) (35), and the particle size in the raw material powder state is basically maintained.
[0088] The drying step is a step of drying the heat exchanger body (25) after the immersion step (i.e., the heat exchanger body (25) in a state where the suspension (32) is applied to the surface). In the drying step, the solvent (34) (alcohol and water) contained in the suspension (32) attached to the heat exchanger body (25) evaporates, and the granular adsorbent (31) and the adhesive (33) remain on the surface of the heat exchanger body (25). The granular adsorbent (31) is bonded to the surface of the heat exchanger body (25) or other adsorbents (31) adjacent to the granular adsorbent (31) through the adhesive (33).
[0089] A relatively thin adsorbent layer (30) is formed on the surface of the heat exchanger body (25) after the drying process. In the manufacturing method of this embodiment, in order to increase the thickness of the adsorbent layer (30) formed on the surface of the heat exchanger body (25), the impregnation process and the drying process are repeated several to dozens of times. Then, when the final drying process is completed, the adsorption heat exchanger (20) is completed. On the completed adsorption heat exchanger (20), an adsorbent layer (30) with a thickness of about 0.25 mm is formed on the surface of the heat exchanger body (25).
[0090] Here, the phenomena of the adsorbent (31) and the binder (33) in the above-mentioned coating step and drying step will be described with reference to schematic diagrams.
[0091] First, as shown in FIG6(A), when the suspension (32) is coated on a substrate, i.e., a heat exchanger body (25), the adsorbent (31) and the adhesive (33) are mixed in a solvent (34) in which the alcohol component is less than 20% by mass of the entire suspension (32), and the adsorbent (31) can be evenly distributed.
[0092] Then, as shown in FIG6(B), when entering the drying process, the water and alcohol components as the solvent evaporate; as shown in FIG6(C), at the end of the drying process, the adsorbent (31) is evenly distributed on the surface of the heat exchanger body (25), and an adsorbent layer (30) is formed in which the adsorbent (31) is covered by the adhesive (33). The arrangement state of the adsorbent (31) in the adsorbent layer (30) after the drying process maintains a uniform arrangement state that is substantially the same as the arrangement state in the suspension (32) state.
[0093] Next, the suspension (32) is repeatedly applied. That is, as shown in FIG6(D), the suspension (32) is applied to the adsorbent layer (30) after the drying process. At this time, as shown in FIG6(E), the dried adsorbent (31) is again wetted with alcohol and water as solvents.
[0094] Then, a drying step is performed, and the coating step and the drying step are repeated multiple times. As a result, an adsorbent layer (30) having an extremely good dispersion of the adsorbent (31) is formed on the surface of the heat exchanger body (25).
[0095] The adsorbent (31) in the adsorbent layer (30) is uniformly mixed in the entire adsorbent layer (30). That is, the uniformity mentioned here refers to the dispersion state of the adsorbent after mixing the adsorbent in the solvent in the horizontal direction, and in the vertical (adsorbent thickness) direction, it refers to the thickness of the adsorbent layer accumulated after repeated coating.
[0096] -Effects of Implementation Methods-
[0097] The suspension of this embodiment contains an alcohol component as a solvent accounting for 20% or less of the total suspension, so that an adsorption component having an alcohol content of 1% or less can be manufactured. Since the alcohol content in the adsorption component is low, explosion-proof measures are not required, thereby suppressing equipment cost consumption.
[0098] It should be noted that, generally speaking, when the alcohol component accounts for 20 mass % or more and less than 30 mass % of the entire suspension, combustion will be initiated (but combustion will not continue); when it is 30 mass % or more, combustion will continue.
[0099] Since the adsorption member of the present embodiment has a low alcohol component content, no explosion-proof measures are required.
[0100] Furthermore, according to the suspension of this embodiment, a group (hydrophilic group) that easily reacts chemically with the components of the hydrophilic layer of the fin is mixed in the binder, so the wettability of the hydrophilic layer of the fin with the suspension is improved. It should be noted that regarding the wetting ability, the wetting ability is excellent when the contact angle is less than 10°.
[0101] -Industrial Applicability-
[0102] In summary, the present invention is very helpful for an adsorption heat exchanger having an adsorbent layer formed on the surface of the heat exchanger body.
[0103] Explanation of symbols
[0104] 20 Adsorption heat exchanger
[0105] 25Heat exchanger body
[0106] 26 fins
[0107] 27Heat transfer tube (heat transfer tube component)
[0108] 30 adsorbent layers
[0109] 31 Adsorbent
[0110] 32 Suspension
[0111] 33 Adhesives
[0112] 34Solvents
[0113] 35 water-based resin (hydrophilic resin).
Claims
1. An adsorption component for an adsorption heat exchanger, characterized in that: An adsorbent layer is laminated on the surface of the base sheet of the adsorption member, and the content of the alcohol component in the adsorbent layer is 1% by mass or less.
2. The adsorption component according to claim 1, characterized in that: The substrate sheet is surface treated.
3. The adsorption component according to claim 2, characterized in that: The surface treatment comprises sequentially laminating a corrosion-resistant layer and a hydrophilic layer on the substrate sheet.
4. A suspension for forming an adsorbent layer of an adsorption component in an adsorption heat exchanger, characterized in that: The suspension is obtained by mixing an adsorbent, a binder and a solvent, wherein the alcohol component in the solvent accounts for 20% by mass or less of the entire suspension.
5. The suspension according to claim 4, characterized in that The suspension is applied to a substrate sheet to obtain an adsorption member.
6. The suspension according to claim 4 or 5, characterized in that The binder contains a hydrophilic group.
7. The suspension according to claim 6, characterized in that The hydrophilic group is at least one of a hydroxyl group, an amino group, a carboxyl group and a metal sulfonic acid group.
8. The suspension according to claim 4, characterized in that Further, an elastomer is added. 9 . A heat exchanger using the adsorption member according to claim 1 , or the adsorption member having an adsorbent layer formed of the suspension according to claim 4 . 10 . A humidity control device comprising the heat exchanger according to claim 9 .