Method for producing steel lock body in rolling mode

The steel lock body is produced through rolling, which solves the problems of high cost, low efficiency and low material utilization in the production of traditional steel lock body, and reduces costs, shortens cycles and improves material utilization, avoids the pulling process The cracking problem achieves the purpose of reducing carbon, reducing emissions and increasing efficiency.

CN119056887APending Publication Date: 2024-12-03NANJING IRON & STEEL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310621902.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-30
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

In the production process of traditional steel locks, there are problems such as high raw material cost, low production efficiency, processing difficulties and low material utilization. In particular, the pulling process is prone to cracking, which seriously restricts the development of steel locks.

Method used

The steel lock body is produced by rolling. The specific process is steelmaking-rolling-shaping-segmented lock body blanks. It adopts the controlled rolling and cold-controlled process, and 18 rolling passages. The first 16 rolling mills adopt flat-over alternating. 17-18 are flat rolling mills, with easy-to-cut elements, such as Pb, Sn, Te, Bi, Ca, and the chemical composition is controlled at C≤0.50%, Si≤2.00%, Mn≤2.00%, P≤0.10%, S ≤0.40%.

Benefits of technology

It reduces raw material costs, shortens production cycles, improves material utilization, avoids annealing and pulling processes, solves the problem of prone to cracking of traditional steel lock body blank materials, and at the same time achieves carbon reduction, emission reduction and efficiency improvement.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a method for producing a steel lock body in a rolling mode, and relates to the technical field of steel production, 18-pass rolling is adopted in a whole rolling line, a controlled rolling and controlled cooling process is adopted in the rolling process, and the specific parameters are as follows: the initial rolling temperature is 1120-1180 DEG C, the final rolling temperature is 980-1040 DEG C, and the temperature on a cooling bed is 950-1000 DEG C; the steel comprises the following chemical components in percentage by mass: not more than 0.50% of C, not more than 2.00% of Si, not more than 2.00% of Mn, not more than 0.10% of P and not more than 0.40% of S. On one hand, zinc alloy, copper alloy and the like are replaced by steel, the material selection range of the lock body is expanded, and the cost of raw materials is reduced, and on the other hand, a traditional steel lock body blank is directly formed in a rolling mode, so that the annealing and drawing procedures in the traditional machining process can be reduced, the production period is shortened, and the manufacturing cost of each ton of blank is reduced by about 2000 yuan. The problems that a traditional steel lock body blank material is low in utilization rate, prone to cracking during drawing and the like can be solved, and meanwhile the purposes of carbon reduction, emission reduction and efficiency improvement are achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of steel production, and in particular to a method for producing a steel lock body by rolling. Background Art

[0002] Domestic lock body manufacturers are mainly concentrated in Wenzhou, Yongkang, Pujiang and Guangzhou. Finished locks are exported all over the world. The annual demand for materials is about 500,000 tons. The main materials are zinc alloy, copper, steel and cast iron. The core of lock body size design lies in the cross-sectional size control. The length of the lock body is divided according to the purpose. There are three common lock bodies, among which the gourd lock body is the most difficult to produce.

[0003] Traditional lock bodies are made of zinc alloy, copper and other materials, facing problems such as high raw material costs and low production efficiency. Traditional steel lock bodies also face processing problems. The production process of traditional steel lock body blanks is: steelmaking-rolling (round steel)-annealing-drawing-annealing-drawing-segmentation-lock body blanks. Due to its long production cycle, low manufacturing cost, low material utilization rate, large cross-sectional area changes, it is easy to cause drawing cracks, which seriously restricts the development of steel lock bodies. Summary of the invention

[0004] The present invention aims at the above technical problems, overcomes the shortcomings of the prior art, and provides a method for producing a steel lock body by rolling. The production process of the steel lock body blank is: steelmaking - rolling - shaping - segmentation - lock body blank. The whole rolling line adopts 18 rolling passes, and the rolling process adopts controlled rolling and controlled cooling technology. The specific parameters are as follows: starting rolling temperature 1120-1180℃, final rolling temperature 980-1040℃, upper cooling bed temperature 950-1000℃; The chemical composition and mass percentage are as follows: C≤0.50%, Si≤2.00%, Mn≤2.00%, P≤0.10%, S≤0.40%.

[0005] The technical solution further defined in the present invention is: In the above-mentioned method of producing a steel lock body by rolling, the first 16 rolling mills adopt horizontal-vertical alternation, and the 17th-18th rolling mills are horizontal rolling mills.

[0006] In the above-mentioned method of producing a steel lock body by rolling, the roughing and intermediate rolling area is the first 12 rolling mills.

[0007] The aforementioned method of producing a steel lock body by rolling adds free-cutting elements, and the free-cutting elements include at least one of Pb, Sn, Te, Bi, and Ca.

[0008] The aforementioned method of producing a steel lock body by rolling has the following chemical composition and mass percentage: C: 0.22%-0.50%, Si: 0.6%-2.00%, Mn: 1.12%-2.00%, P≤0.03%, S≤0.3%.

[0009] The beneficial effects of the present invention are as follows: on the one hand, the present invention adopts steel to replace zinc alloy, copper alloy, etc., to expand the material selection range of the lock body and reduce the cost of raw materials; on the other hand, the traditional steel lock body blank is directly formed by rolling, which can not only reduce the annealing and drawing steps in the traditional processing process and shorten the production cycle, and reduce the manufacturing cost of each ton of blank by about 2,000 yuan, but also solve the problems of low material utilization rate and easy cracking of traditional steel lock body blanks during drawing, while achieving the purpose of carbon reduction, emission reduction and efficiency improvement. Implementation Example

[0010] This embodiment provides a method for producing a steel lock body by rolling, wherein the composition range is: C: 0.06wt.%, Si: 0.03wt.%, Mn: 1.10wt.%, P: 0.045wt.%, S: 0.32wt.%. The entire rolling line adopts 18 rolling passes, the first 16 rolling mills adopt horizontal-vertical alternation, the 17th-18th rolling mills are horizontal rolling mills, of which the roughing and medium rolling area is the first 12 rolling mills, and the rolling process adopts a controlled rolling and controlled cooling process, and the specific parameters are as follows: (1) the starting rolling temperature is 1136°C; (2) the final rolling temperature is 990°C; (3) the upper cooling bed temperature is 960°C. Example

[0011] This embodiment provides a method for producing a steel lock body by rolling, with a composition range of C: 0.14wt.%, Si: 0.10wt.%, Mn: 1.16wt.%, P: 0.075wt.%, S: 0.30wt.%. The entire rolling line adopts 18 passes of rolling, the first 16 rolling mills adopt horizontal-vertical alternation, the 17th and 18th rolling mills are horizontal rolling mills, of which the roughing and medium rolling area is the first 12 rolling mills, and the rolling process adopts a controlled rolling and controlled cooling process, with the following specific parameters: (1) starting rolling temperature 1145℃; (2) final rolling temperature 999℃; (3) upper cooling bed temperature 970℃. Example

[0012] This embodiment provides a method for producing a steel lock body by rolling, wherein the composition range is: C: 0.28wt.%, Si: 0.24wt.%, Mn: 0.88wt.%, P: 0.028wt.%, S: 0.12wt.%. The entire rolling line adopts 18 rolling passes, the first 16 rolling mills adopt horizontal-vertical alternation, the 17th-18th rolling mills are horizontal rolling mills, of which the roughing and medium rolling area is the first 12 rolling mills, and the rolling process adopts a controlled rolling and controlled cooling process, and the specific parameters are as follows: (1) the starting rolling temperature is 1160℃; (2) the final rolling temperature is 1010℃; (3) the upper cooling bed temperature is 988℃. Example

[0013] This embodiment provides a method for producing a steel lock body by rolling, wherein the composition range is: C: 0.40wt.%, Si: 0.30wt.%, Mn: 1.32wt.%, P: 0.03wt.%, S: 0.03wt.%. The entire rolling line adopts 18 rolling passes, the first 16 rolling mills adopt horizontal-vertical alternation, the 17th-18th rolling mills are horizontal rolling mills, of which the roughing and medium rolling area is the first 12 rolling mills, and the rolling process adopts a controlled rolling and controlled cooling process, and the specific parameters are as follows: (1) the starting rolling temperature is 1130℃; (2) the final rolling temperature is 985℃; (3) the upper cooling bed temperature is 954℃. Example

[0014] This embodiment provides a method for producing a steel lock body by rolling, with a composition range of C: 0.48wt.%, Si: 1.84wt.%, Mn: 1.87wt.%, P: 0.02wt.%, S: 0.005wt.%. The entire rolling line adopts 18 passes of rolling, the first 16 rolling mills adopt horizontal-vertical alternation, the 17th and 18th rolling mills are horizontal rolling mills, of which the roughing and medium rolling area is the first 12 rolling mills, and the rolling process adopts a controlled rolling and controlled cooling process, with the following specific parameters: (1) starting rolling temperature 1165℃; (2) final rolling temperature 1025℃; (3) upper cooling bed temperature 998℃.

[0015] In addition to the above embodiments, the present invention may also have other implementation modes. Any technical solution formed by equivalent replacement or equivalent transformation falls within the protection scope required by the present invention.

Claims

1. A method for producing a steel lock body by rolling, characterized in that: The production process of steel lock body blank is: steelmaking - rolling - shaping - segmentation - lock body blank. The whole rolling line adopts 18 rolling passes, and the rolling process adopts controlled rolling and controlled cooling technology. The specific parameters are as follows: starting rolling temperature 1120-1180℃, final rolling temperature 980-1040℃, upper cooling bed temperature 950-1000℃; The chemical composition and mass percentage are as follows: C≤0.50%, Si≤2.00%, Mn≤2.00%, P≤0.10%, S≤0.40%.

2. The method for producing a steel lock body by rolling according to claim 1, characterized in that: The first 16 rolling mills adopt horizontal-vertical alternation, and the 17th and 18th rolling mills are horizontal rolling mills.

3. The method for producing a steel lock body by rolling according to claim 2, characterized in that: The roughing and intermediate rolling area is the first 12 rolling mills.

4. The method for producing a steel lock body by rolling according to claim 1, characterized in that: Free-cutting elements are added, and the free-cutting elements include at least one of Pb, Sn, Te, Bi, and Ca.

5. The method for producing a steel lock body by rolling according to claim 1, characterized in that: The chemical composition and mass percentage are as follows: C: 0.22%-0.50%, Si: 0.6%-2.00%, Mn: 1.12%-2.00%, P≤0.03%, S≤0.3%.