Fillet welding process and ship body
By combining the flat and vertical corner welding processes and performing Z-shaped swings during the welding process, the problem of difficulty in forming 8mm welding feet in the existing technology is solved, and efficient and stable welding effects are achieved, and welding speed and welding foot strength are improved.
Patent Information
- Application Number
- CN202411408820.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-10
- Publication Date
- 2024-12-03
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing fillet welding process is difficult to form 8mm height welding feet and cannot meet the strength requirements of the hull structure.
By combining the flat corner welding process and the vertical corner welding process, the welding gun performs specific arc starting, welding and arc extinguishing parameters on the robotic arm, the welding foot height is 8mm, and the Z-shaped oscillation is performed during the welding process. To improve welding uniformity.
The welding foot height is 8mm stable forming, which improves the welding speed and strength and reliability of the welding foot. The welding speed is more than 20% higher than manual welding, and the weld quality is stable, without pores, undercuts, inclusions, and cracks. etc.
Smart Images

Figure CN119057187A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of ships, and in particular to a fillet welding process and a hull. Background Art
[0002] In the current shipbuilding field, with the advancement of technology and the improvement of production efficiency, robot welding technology has become an indispensable part. Fillet welding process is a key link in hull structure welding, which is mainly divided into flat fillet welding process and vertical fillet welding process. However, in actual application, the flat fillet welding process can only form a maximum weld foot of 7.5mm in height, and it is difficult to form a weld foot of 8mm in height, resulting in the weld failing to meet the strength requirements of the hull structure.
[0003] Based on this, a fillet welding process and a hull are urgently needed to solve the above-mentioned problems. Summary of the invention
[0004] Based on the above, the purpose of the present invention is to provide a fillet welding process and a hull, which can achieve a T-joint with a welding leg height of 8 mm by using both a flat fillet welding process and a vertical fillet welding process, thereby ensuring stable weld quality, and increasing the welding speed by more than 20% compared with manual welding, thereby improving the weld leg strength and reliability.
[0005] To achieve the above object, the present invention adopts the following technical solutions:
[0006] On the one hand, a fillet welding process is provided, wherein a welding gun is arranged on a robot arm, and the welding gun adopts the fillet welding process to be applied to a T-joint with a welding leg height of 8 mm, wherein the fillet welding process includes a flat fillet welding process and a vertical fillet welding process, and the flat fillet welding process includes the following steps:
[0007] S11, the welding gun performs arc welding according to the first arc starting parameter;
[0008] S12, the welding gun performs standard welding according to the first welding parameters;
[0009] S13, the welding gun performs arc extinguishing welding according to the first arc extinguishing parameter, completing the first welding to form a first weld leg;
[0010] S14, the welding gun performs arc welding on the surface of the first welding leg according to the second arc starting parameters;
[0011] S15, the welding gun performs standard welding on the surface of the first welding leg according to the second welding parameters;
[0012] S16, the welding gun performs arc extinguishing welding on the surface of the first weld leg according to the second arc extinguishing parameter, and completes the second welding to form a second weld leg on the surface of the first weld leg, wherein the sum of the heights of the first weld leg and the second weld leg is 8 mm;
[0013] The vertical fillet welding process comprises the following steps:
[0014] S21, the welding gun performs arc starting welding according to the third arc starting parameter;
[0015] S22, the welding gun performs standard welding according to the third welding parameter;
[0016] S23, the welding gun performs arc extinguishing welding according to the third arc extinguishing parameter to form a third weld leg with a weld leg height of 8 mm.
[0017] As a preferred technical solution of a fillet welding process, in steps S11, S12 and S13, the welding gun is swung according to a first swung parameter;
[0018] In steps S14, S15 and S16, the welding gun is swung according to the second swung parameter;
[0019] In steps S21, S22 and S23, the welding gun is swung according to a third swung parameter.
[0020] As a preferred technical solution for fillet welding process, the first swing parameter includes the following parameters: the swing form is "Z-shaped", the swing frequency is 1.5 Hz, the swing amplitude is 4 mm, and the swing limit position dwell time is 0.1 s; and / or
[0021] The second swing parameters include the following parameters: the swing form is "Z-shaped", the swing frequency is 1.5 Hz, the swing amplitude is 2 mm, and the swing limit position dwell time is 0 s; and / or
[0022] The third swing parameter includes the following parameters: the swing form is "Z-shaped", the swing frequency is 1 Hz, the swing amplitude is 7 mm, and the swing limit position dwell time is 0.4 s.
[0023] As a preferred technical solution of a fillet welding process, the first swing parameter and the second swing parameter also include that the angle between the axis of the welding gun and the horizontal plane is 45°, and the axis of the welding gun is perpendicular to the weld; and / or
[0024] The third swing parameter also includes that the posture of the welding gun is push welding, the angle between the axis of the welding gun and the horizontal plane is 15°, and the axis of the welding gun is located on the bisector of the angle between the two welding plates.
[0025] As a preferred technical solution for a fillet welding process, the first arc starting parameters include the following parameters: arc starting current is 274A, arc starting voltage is 24V, arc starting wire feeding speed is 11000mm / min; and / or
[0026] The second arc starting parameters include the following parameters: arc starting current is 220A, arc starting voltage is 25.5V, arc starting wire feeding speed is 9000mm / min; and / or
[0027] The third arc starting parameters include the following parameters: arc starting current is 170A, arc starting voltage is 21V, and arc starting wire feeding speed is 5200mm / min.
[0028] As a preferred technical solution of a fillet welding process, the first welding parameters include the following parameters: welding current is 280A, welding voltage is 30V, welding speed is 5.5mm / s, wire feeding speed is 12500mm / min; and / or
[0029] The second welding parameters include the following parameters: welding current is 220A, welding voltage is 25.5V, welding speed is 8.5mm / s, wire feeding speed is 9000mm / min; and / or
[0030] The third welding parameters include the following parameters: welding current is 195A, welding voltage is 22.5V, welding speed is 2.6mm / s, and wire feeding speed is 7000mm / min.
[0031] As a preferred technical solution for a fillet welding process, the first arc extinguishing parameters include the following parameters: arc extinguishing current is 220A, arc extinguishing voltage is 23V, arc extinguishing wire feeding speed is 8000mm / min; and / or
[0032] The second arc extinction parameters include the following parameters: arc extinction current is 210A, arc extinction voltage is 23.2V, arc extinction wire feeding speed is 9000mm / min; and / or
[0033] The third arc extinguishing parameter includes the following parameters: arc extinguishing current is 160A, arc extinguishing voltage is 20V, and arc extinguishing wire feeding speed is 4500mm / min.
[0034] As a preferred technical solution for a fillet welding process, in the flat fillet welding process and the vertical fillet welding process, a shielding gas is sprayed on the welding part, the shielding gas is CO2, and the gas flow rate of the shielding gas is 15L / min-25L / min.
[0035] As an optimal technical solution for a fillet welding process, the start time of supplying the shielding gas is 1 second before arc starting welding, and the end time of supplying the shielding gas is 1.5 seconds after arc extinguishing welding.
[0036] On the other hand, a hull is provided, which is welded by the fillet welding process described in any of the above schemes.
[0037] The beneficial effects of the present invention are:
[0038] The present invention provides a fillet welding process and a hull. When welding a T-joint with a weld leg height of 8 mm, a welding gun can weld the weld by a flat fillet welding process. The welding gun performs arc welding according to a first arc starting parameter; then, the welding gun performs standard welding according to the first welding parameter; then, the welding gun performs arc extinguishing welding according to the first arc extinguishing parameter, and completes the first welding to form a first weld leg; then, the welding gun performs arc welding on the surface of the first weld leg according to a second arc starting parameter; then, the welding gun performs standard welding on the surface of the first weld leg according to the second welding parameter; finally, the welding gun performs arc extinguishing welding on the surface of the first weld leg according to the second arc extinguishing parameter, and completes the second welding to form a second weld leg on the surface of the first weld leg, and the sum of the heights of the first weld leg and the second weld leg is 8 mm. The flat fillet welding process can effectively meet the welding requirements of high weld legs by forming a T-joint with a weld leg height of 8 mm through two welding passes.
[0039] The welding gun can also weld the weld using a vertical fillet welding process, wherein the welding gun performs arc welding according to the third arc starting parameter; then, the welding gun performs standard welding according to the third welding parameter; finally, the welding gun performs arc extinguishing welding according to the third arc extinguishing parameter to form a third weld leg with a weld leg height of 8 mm. The vertical fillet welding process can form a T-joint with a weld leg height of 8 mm at one time.
[0040] The present invention sets a first arc starting parameter, a first welding parameter, a first arc extinction parameter, a second arc starting parameter, a second welding parameter and a second arc extinction parameter. The welding gun on the robot arm adopts the above-mentioned fillet welding process to form a T-joint with a weld foot height of 8 mm, thereby ensuring stable weld quality, and the welding speed is increased by more than 20% compared with manual welding. The weld foot is fully formed without defects such as pores, undercuts, inclusions and cracks, thereby improving the strength and reliability of the weld foot. BRIEF DESCRIPTION OF THE DRAWINGS
[0041] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments of the present invention. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the contents of the embodiments of the present invention and these drawings without paying any creative work.
[0042] Figure 1 It is a process flow chart of a flat fillet welding process provided by a specific embodiment of the present invention;
[0043] Figure 2 It is a process flow chart of a vertical fillet welding process provided by a specific embodiment of the present invention;
[0044] Figure 3It is a front view of a welding gun provided in a specific embodiment of the present invention using a flat fillet welding process;
[0045] Figure 4 It is a schematic diagram of the angle of the welding gun relative to the weld when the welding gun provided by the specific embodiment of the present invention adopts the flat fillet welding process;
[0046] Figure 5 It is a top view of a welding gun provided in a specific embodiment of the present invention using a vertical fillet welding process;
[0047] Figure 6 It is a schematic diagram of the angle of the welding gun relative to the weld when the welding gun provided by the specific embodiment of the present invention adopts the vertical fillet welding process.
[0048] The following are marked in the figure:
[0049] 1. Welding plate; 11. Welding seam; 2. Welding gun. DETAILED DESCRIPTION
[0050] The present invention will be further described in detail below in conjunction with the accompanying drawings and embodiments. It is to be understood that the specific embodiments described herein are only used to explain the present invention, rather than to limit the present invention. It should also be noted that, for ease of description, only parts related to the present invention, rather than all structures, are shown in the accompanying drawings.
[0051] In the description of the present invention, unless otherwise clearly specified and limited, the terms "connected", "connected", and "fixed" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0052] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0053] In the description of this embodiment, the terms "upper", "lower", "left", "right" and other directions or positional relationships are based on the directions or positional relationships shown in the drawings, and are only for the convenience of description and simplification of operation, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operate in a specific direction, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are only used to distinguish in the description and have no special meaning.
[0054] In the current shipbuilding field, with the advancement of technology and the improvement of production efficiency, robot welding technology has become an indispensable part. Fillet welding process is a key link in hull structure welding, which is mainly divided into flat fillet welding process and vertical fillet welding process. However, in actual application, the flat fillet welding process can only form a maximum weld foot of 7.5mm in height, and it is difficult to form a weld foot of 8mm in height, resulting in the weld failing to meet the strength requirements of the hull structure.
[0055] To solve the above problems, Figure 1-Figure 6 As shown, this embodiment provides a fillet welding process, the welding gun 2 is arranged on the robot arm, and the welding gun 2 adopts the fillet welding process to weld a T-shaped joint with a weld leg height of 8 mm. The flat fillet welding process includes the following steps:
[0056] S11, welding gun 2 performs arc welding according to the first arc starting parameter;
[0057] S12, welding gun 2 performs standard welding according to the first welding parameters;
[0058] S13, welding gun 2 performs arc extinguishing welding according to the first arc extinguishing parameter, completing the first welding to form a first weld leg;
[0059] S14, welding gun 2 performs arc welding on the first welding leg surface according to the second arc starting parameter;
[0060] S15, welding gun 2 performs standard welding on the first welding leg surface according to the second welding parameters;
[0061] S16, welding gun 2 performs arc extinguishing welding on the surface of the first weld leg according to the second arc extinguishing parameter, and completes the second welding to form a second weld leg on the surface of the first weld leg, and the sum of the heights of the first weld leg and the second weld leg is 8 mm;
[0062] The flat fillet welding process can effectively meet the welding requirements of high weld legs by forming a T-shaped joint with a weld leg height of 8 mm through two welding passes. In this embodiment, the height of the first weld leg is 5 mm, and the height of the second weld leg is 3 mm.
[0063] The vertical fillet welding process includes the following steps:
[0064] S21, welding gun 2 performs arc starting welding according to the third arc starting parameter;
[0065] S22, welding gun 2 performs standard welding according to the third welding parameters;
[0066] S23, the welding gun 2 performs arc extinguishing welding according to the third arc extinguishing parameter to form a third weld leg with a weld leg height of 8 mm. This vertical fillet welding process can form a T-shaped joint with a weld leg height of 8 mm in one step.
[0067] The present invention ensures that the robot can stably reproduce the weld 11 with stable quality by setting the first arc starting parameter, the first welding parameter, the first arc extinction parameter, the second arc starting parameter, the second welding parameter and the second arc extinction parameter. The welding gun 2 on the robot arm adopts the above-mentioned fillet welding process to form a T-joint with a weld foot height of 8 mm, thereby ensuring the stable quality of the weld 11. The welding speed is increased by more than 20% compared with manual welding. The weld foot is fully formed without defects such as pores, undercuts, inclusions and cracks, thereby improving the strength and reliability of the weld foot.
[0068] Preferably, in step S11, step S12 and step S13, the welding gun 2 swings according to the first swing parameter; in step S14, step S15 and step S16, the welding gun 2 swings according to the second swing parameter; in step S21, step S22 and step S23, the welding gun 2 swings according to the third swing parameter. The welding gun 2 on the robot arm can swing during welding, and even if the groove changes, the welding gun 2 can cover the weld 11 when swinging, which can ensure the welding quality of the weld 11 and achieve the effect of correcting the deviation of the weld 11.
[0069] In this embodiment, the first swing parameter includes the following parameters: the swing form is "Z-shaped", the swing frequency is 1.5Hz, the swing amplitude is 4mm, and the swing limit position dwell time is 0.1s; and / or the second swing parameter includes the following parameters: the swing form is "Z-shaped", the swing frequency is 1.5Hz, the swing amplitude is 2mm, and the swing limit position dwell time is 0s; and / or the third swing parameter includes the following parameters: the swing form is "Z-shaped", the swing frequency is 1Hz, the swing amplitude is 7mm, and the swing limit position dwell time is 0.4s. The welding gun 2 on the robot arm performs regular lateral swings on the weld 11 by setting reasonable first swing parameters, second swing parameters and third swing parameters, so that the welding energy is more evenly distributed on the weld 11, thereby improving the uniformity of the weld 11. Swing welding can form a good fusion between the weld 11 and the welding plate 1, thereby improving the strength and stability of the welding.
[0070] More preferably, if Figure 3-Figure 6As shown, the first swing parameter and the second swing parameter also include that the angle between the axis of the welding gun 2 and the horizontal plane is 45°, and the axis of the welding gun 2 is perpendicular to the weld 11; and / or the third swing parameter also includes that the posture of the welding gun 2 is push welding, the angle between the axis of the welding gun 2 and the horizontal plane is 15°, and the axis of the welding gun 2 is located on the bisector of the angle between the two welding plates 1. The appropriate angle of the welding gun 2 helps to reduce defects such as undercut and slag inclusion generated during welding, improve the forming quality of the weld 11 and improve welding efficiency.
[0071] In this embodiment, the first arc starting parameter includes the following parameters: the arc starting current is 274A, the arc starting voltage is 24V, and the arc starting wire feeding speed is 11000mm / min; and / or the second arc starting parameter includes the following parameters: the arc starting current is 220A, the arc starting voltage is 25.5V, and the arc starting wire feeding speed is 9000mm / min; and / or the third arc starting parameter includes the following parameters: the arc starting current is 170A, the arc starting voltage is 21V, and the arc starting wire feeding speed is 5200mm / min. The welding gun 2 on the robot arm can ensure the smooth transition of the weld foot at the arc starting welding part, ensure the aesthetics of the arc starting part, and the weld foot at the arc starting part is fully formed, thereby improving the strength and reliability of the weld foot.
[0072] Further, the first welding parameters include the following parameters: welding current is 280A, welding voltage is 30V, welding speed is 5.5mm / s, wire feeding speed is 12500mm / min; and / or the second welding parameters include the following parameters: welding current is 220A, welding voltage is 25.5V, welding speed is 8.5mm / s, wire feeding speed is 9000mm / min; and / or the third welding parameters include the following parameters: welding current is 195A, welding voltage is 22.5V, welding speed is 2.6mm / s, wire feeding speed is 7000mm / min. The welding gun 2 on the robot arm can form a weld foot with a weld foot height of 8mm by setting reasonable first welding parameters, second welding parameters and third welding parameters, and the weld 11 has high quality and can smoothly transition with the arc welding part, so that the hardness of the heat-affected zone meets the requirements and prevents the weld 11 from cracking.
[0073] In this embodiment, the first arc extinction parameter includes the following parameters: the arc extinction current is 220A, the arc extinction voltage is 23V, and the arc extinction wire feeding speed is 8000mm / min; and / or the second arc extinction parameter includes the following parameters: the arc extinction current is 210A, the arc extinction voltage is 23.2V, and the arc extinction wire feeding speed is 9000mm / min; and / or the third arc extinction parameter includes the following parameters: the arc extinction current is 160A, the arc extinction voltage is 20V, and the arc extinction wire feeding speed is 4500mm / min. The welding gun 2 on the robot arm sets reasonable first arc extinction parameters, second arc extinction parameters, and third arc extinction parameters, so that the arc is stable during the arc extinction process, ensuring that the arc pit of the arc extinction welding part is filled, and preventing defects such as looseness, cracks, pores or slag inclusions from occurring in the arc extinction welding part.
[0074] Preferably, in the flat fillet welding process and the vertical fillet welding process, a shielding gas is sprayed on the welding part, the shielding gas is CO2, and the gas flow rate of the shielding gas is 15L / min-25L / min. By spraying the shielding gas, the weld 11 area can be isolated from oxygen and moisture in the air, thereby preventing oxidation and corrosion of the high-temperature metal. This can not only maintain the metal composition and performance of the weld 11, but also reduce the generation of welding defects such as pores and cracks, and improve the corrosion resistance and durability of the weld 11. The shielding gas can also play a certain protective role on the welding gun 2, reduce equipment damage caused by high temperature and oxidation, and extend the service life of the equipment.
[0075] Further preferably, the shielding gas supply starts 1 second before arc welding, which can ensure that the air in the nozzle is exhausted, and the welding part is within the protection range of the shielding gas at the beginning of welding, reducing the impact of air on welding quality; the shielding gas supply ends 1.5 seconds after arc welding, and the shielding gas can cool and protect the welding point after welding stops. This embodiment improves the quality of the welding part while ensuring welding efficiency.
[0076] In this embodiment, the gap of the weld 11 between the two welding plates 1 is 0-2mm, and the thickness of the welding plate 1 is 3mm-16mm. Before welding, the area to be welded should be cleaned to ensure that there is no impurities such as oil, moisture, rust, etc. The welding wire in this embodiment uses a flux-cored wire with a diameter of 1.2mm.
[0077] This embodiment also provides a hull, which is welded and formed by the above-mentioned fillet welding process, the weld 11 is formed to be qualified, the weld leg height is 8mm-9mm and meets the requirements, and the weld leg has no defects such as pores, undercuts, inclusions, cracks, etc. The robot adopts the above-mentioned fillet welding process, which not only significantly improves the forming quality, but also increases the speed by more than 20% compared with the traditional welding method.
[0078] Note that the above are only preferred embodiments of the present invention and the technical principles used. Those skilled in the art will understand that the present invention is not limited to the specific embodiments described herein, and that various obvious changes, readjustments and substitutions can be made by those skilled in the art without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in more detail through the above embodiments, the present invention is not limited to the above embodiments, and may include more other equivalent embodiments without departing from the concept of the present invention, and the scope of the present invention is determined by the scope of the appended claims.
Claims
1. A fillet welding process, characterized in that: A welding gun (2) is arranged on a mechanical arm, and the welding gun (2) adopts the fillet welding process to be applied to a T-joint with a welding leg height of 8 mm, the fillet welding process comprising a flat fillet welding process and a vertical fillet welding process, and the flat fillet welding process comprises the following steps: S11, the welding gun (2) performs arc welding according to the first arc starting parameter; S12, the welding gun (2) performs standard welding according to the first welding parameters; S13, the welding gun (2) performs arc extinguishing welding according to the first arc extinguishing parameter, completing the first welding pass to form a first weld leg; S14, the welding gun (2) performs arc welding on the surface of the first welding leg according to the second arc starting parameters; S15, the welding gun (2) performs standard welding on the surface of the first welding leg according to second welding parameters; S16, the welding gun (2) performs arc extinguishing welding on the surface of the first weld leg according to the second arc extinguishing parameter, and completes the second welding to form a second weld leg on the surface of the first weld leg, wherein the sum of the heights of the first weld leg and the second weld leg is 8 mm; The vertical fillet welding process comprises the following steps: S21, the welding gun (2) performs arc welding according to the third arc starting parameter; S22, the welding gun (2) performs standard welding according to the third welding parameters; S23, the welding gun (2) performs arc extinguishing welding according to the third arc extinguishing parameter to form a third weld leg with a weld leg height of 8 mm.
2. The fillet welding process according to claim 1, characterized in that: In steps S11, S12 and S13, the welding gun (2) is swung according to a first swung parameter; In steps S14, S15 and S16, the welding gun (2) is swung according to a second swung parameter; In steps S21, S22 and S23, the welding gun (2) is swung according to a third swung parameter.
3. The fillet welding process according to claim 2, characterized in that: The first swing parameters include the following parameters: the swing form is "Z-shaped", the swing frequency is 1.5 Hz, the swing amplitude is 4 mm, and the swing limit position dwell time is 0.1 s; and / or The second swing parameters include the following parameters: the swing form is "Z-shaped", the swing frequency is 1.5Hz, the swing amplitude is 2mm, and the swing limit position dwell time is 0s; and / or The third swing parameter includes the following parameters: the swing form is "Z-shaped", the swing frequency is 1 Hz, the swing amplitude is 7 mm, and the swing limit position residence time is 0.4 s.
4. The fillet welding process according to claim 2, characterized in that: The first swing parameter and the second swing parameter also include that the angle between the axis of the welding gun (2) and the horizontal plane is 45°, and the axis of the welding gun (2) is perpendicular to the weld (11); and / or The third swing parameter also includes that the posture of the welding gun (2) is push welding, the angle between the axis of the welding gun (2) and the horizontal plane is 15°, and the axis of the welding gun (2) is located on the bisector of the angle between the two welding plates (1).
5. The fillet welding process according to claim 1, characterized in that: The first arc starting parameters include the following parameters: arc starting current is 274A, arc starting voltage is 24V, arc starting wire feeding speed is 11000mm / min; and / or The second arc starting parameters include the following parameters: arc starting current is 220A, arc starting voltage is 25.5V, arc starting wire feeding speed is 9000mm / min; and / or The third arc starting parameters include the following parameters: arc starting current is 170A, arc starting voltage is 21V, and arc starting wire feeding speed is 5200mm / min.
6. The fillet welding process according to claim 1, characterized in that: The first welding parameters include the following parameters: welding current is 280A, welding voltage is 30V, welding speed is 5.5mm / s, wire feeding speed is 12500mm / min; and / or The second welding parameters include the following parameters: welding current is 220A, welding voltage is 25.5V, welding speed is 8.5mm / s, wire feeding speed is 9000mm / min; and / or The third welding parameters include the following parameters: welding current is 195A, welding voltage is 22.5V, welding speed is 2.6mm / s, and wire feeding speed is 7000mm / min.
7. The fillet welding process according to claim 1, characterized in that: The first arc extinguishing parameters include the following parameters: arc extinguishing current is 220A, arc extinguishing voltage is 23V, arc extinguishing wire feeding speed is 8000mm / min; and / or The second arc extinction parameters include the following parameters: arc extinction current is 210A, arc extinction voltage is 23.2V, arc extinction wire feeding speed is 9000mm / min; and / or The third arc extinguishing parameter includes the following parameters: arc extinguishing current is 160A, arc extinguishing voltage is 20V, and arc extinguishing wire feeding speed is 4500mm / min.
8. The fillet welding process according to claim 1, characterized in that: In the flat fillet welding process and the vertical fillet welding process, a shielding gas is sprayed on the welding part. The shielding gas is CO2, and the gas flow rate of the shielding gas is 15L / min-25L / min.
9. The fillet welding process according to claim 8, characterized in that: The supply of the shielding gas starts 1 second before arc-starting welding, and ends 1.5 seconds after arc-extinguishing welding.
10. A hull, characterized in that: The hull is welded by the fillet welding process as described in any one of claims 1 to 9.
Citation Information
Patent Citations
Robot welding process for ship curved surface structure
CN114147317A
Method for achieving joint-free welding seam of space complex component through double-robot collaborative welding
CN114273749A
Control method for lap welding of bead joint
JP1999077305A