Robot welding method and ship

The robot welding method with precise parameters and swinging motions addresses weld depth and foot height issues, enhancing weld quality and speed in T-joints.

CN119057188AActive Publication Date: 2024-12-03SHANGHAI WAIGAOQIAO SHIP BUILDING CO LTD

Patent Information

Application Number
CN202411408823.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-10
Publication Date
2024-12-03
Estimated Expiration
2044-10-10

AI Technical Summary

Technical Problem

Robot welding technologies face challenges in setting proper parameters, leading to insufficient weld depth, pores, and inadequate weld foot height, which affect weld strength and safety, especially in T-joints, due to lack of adaptive capabilities and real-time feedback.

Method used

A robot welding method with specific parameters for arc starting, welding, and extinguishing, combined with swinging motions and shielding gas, is applied to achieve a 6mm weld foot height, ensuring stable weld quality and increased speed.

Benefits of technology

The method enhances weld strength, prevents pores, and achieves a 20% increase in welding speed by forming high-quality T-joints with consistent weld foot height, improving product reliability and efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119057188A_ABST
    Figure CN119057188A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of ships, and discloses a robot welding method and a ship. The robot welding method comprises the following steps that S1, a welding gun conducts arcing welding according to specific arcing parameters; s2, a welding gun conducts standard welding according to specific welding parameters; when flat fillet welding is adopted, the specific welding parameters comprise the following parameters that the welding current is 280 A, the welding voltage is 27 V, the welding speed is 7.5 mm / s, and the wire feeding speed is 12000 mm / min; when vertical fillet welding is adopted, the specific welding parameters comprise the following parameters that the welding current is 190 A, the welding voltage is 22 V, the welding speed is 4 mm / s, and the wire feeding speed is 6400 mm / min; s3, the welding gun conducts arc quenching welding according to the specific arc quenching parameters; in the step S1, the step S2 and the step S3, the welding gun swings according to specific swinging parameters so as to form a weld leg with the weld leg height of 6 mm.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of ships, and in particular to a robot welding method and a ship. Background Art

[0002] In modern manufacturing, robot welding technology has become an indispensable part with its high efficiency, stability and precision. The adjustment and control of the robot's welding parameters is still a crucial link. When the welding parameters are not set properly, a series of welding defects will occur, which will seriously affect the quality of the weld and the overall performance of the product. Specifically, if the welding parameters are poor, the first problem that may arise is that the weld depth is insufficient due to insufficient heat input or inaccurate welding parameter settings, thereby reducing the strength of the weld and increasing the risk of product failure. In addition, pores are also one of the common welding defects. They are formed when gas is trapped in the welding pool during the welding process, which weakens the density and strength of the weld and further increases the safety hazards of the product. In addition to the above defects, for T-joints with a weld foot height of 6mm, the weld foot height may not meet the structural requirements, reducing the welding strength.

[0003] Furthermore, robots do not have the same adaptive capabilities as welders. For example, they are unable to collect factors such as groove changes and provide real-time feedback control. The above factors make the robot-specific welding process extremely complicated.

[0004] Based on this, there is an urgent need for a robot welding method and a ship to solve the above-mentioned problems. Summary of the invention

[0005] Based on the above, the purpose of the present invention is to provide a robot welding method and a ship, wherein the robot performs standard welding with specific welding parameters, realizes a T-joint with a formed weld foot height of 6 mm, ensures stable weld quality, and increases the welding speed by more than 20% compared with manual welding.

[0006] To achieve the above object, the present invention adopts the following technical solutions:

[0007] On the one hand, a robot welding method is provided, wherein a welding gun is arranged on a robot arm, and the welding gun is applied to a T-joint with a welding leg height of 6 mm using the robot welding method, and the robot welding method comprises the following steps:

[0008] S1. The welding gun starts arc welding according to specific arc starting parameters;

[0009] S2, welding gun performs standard welding according to specific welding parameters;

[0010] When flat fillet welding is used, the specific welding parameters include the following parameters: welding current is 280A, welding voltage is 27V, welding speed is 7.5mm / s, and wire feeding speed is 12000mm / min;

[0011] When vertical fillet welding is adopted, the specific welding parameters include the following parameters: welding current is 190A, welding voltage is 22V, welding speed is 4mm / s, and wire feeding speed is 6400mm / min;

[0012] S3, the welding gun performs arc extinguishing welding according to specific arc extinguishing parameters;

[0013] In step S1, step S2 and step S3, the welding gun is swung according to specific swung parameters to form a weld foot with a weld foot height of 6 mm.

[0014] As a preferred technical solution of a robot welding method, when flat fillet welding is adopted, the specific swing parameters include the following parameters: the swing form is "Z-shaped", the swing frequency is 1.5 Hz, the swing amplitude is 2 mm, and the swing limit position dwell time is 0;

[0015] When vertical fillet welding is adopted, the specific swing parameters include the following parameters: the swing form is "Z-shaped", the swing frequency is 1 Hz, the swing amplitude is 5 mm, and the swing limit position dwell time is 0.4 s.

[0016] As a preferred technical solution of a robot welding method, when flat fillet welding is adopted, the specific swing parameter also includes that the angle between the axis of the welding gun and the horizontal plane is 45°, and the axis of the welding gun is perpendicular to the weld;

[0017] When vertical fillet welding is adopted, the specific swing parameters also include that the posture of the welding gun is push welding, the angle between the axis of the welding gun and the horizontal plane is 15°, and the axis of the welding gun is located on the bisector of the angle between the two welding plates.

[0018] As a preferred technical solution of a robot welding method, in step S1, when flat fillet welding is adopted, the specific arc starting parameters include the following parameters: arc starting current is 274A, arc starting voltage is 25V, arc starting wire feeding speed is 11000mm / min;

[0019] When vertical fillet welding is adopted, the specific arc starting parameters include the following parameters: arc starting current is 170A, arc starting voltage is 22V, and arc starting wire feeding speed is 5200mm / min.

[0020] As a preferred technical solution of a robot welding method, in steps S1, S2 and S3, a shielding gas is sprayed on the welding part, and the gas flow rate of the shielding gas is 15L / min-25L / min.

[0021] As a preferred technical solution of a robot welding method, the start time of supplying the shielding gas is 1 second before arc starting welding, and the end time of supplying the shielding gas is 1.5 seconds after arc extinguishing welding.

[0022] As a preferred technical solution of a robot welding method, the protective gas is CO 2 .

[0023] As a preferred technical solution of a robot welding method, in step S3, when flat fillet welding is adopted, the specific arc extinction parameters include the following parameters: arc extinction current is 220A, arc extinction voltage is 23V, arc extinction wire feeding speed is 8000mm / min;

[0024] When vertical fillet welding is adopted, the specific arc extinguishing parameters include the following parameters: arc extinguishing current is 160A, arc extinguishing voltage is 20V, and arc extinguishing wire feeding speed is 4500mm / min.

[0025] As a preferred technical solution for a robot welding method, the weld gap between the two welding plates is 0-2 mm.

[0026] On the other hand, a ship is provided, wherein the ship is welded by the robot welding method described in any of the above schemes.

[0027] The beneficial effects of the present invention are:

[0028] The invention provides a robot welding method and a ship. When welding a T-joint with a weld leg height of 6 mm, a welding gun on a robot arm performs arc starting welding according to specific arc starting parameters; then, the welding gun performs standard welding according to the specific welding parameters; when flat fillet welding is adopted, the specific welding parameters include the following parameters: welding current is 280A, welding voltage is 27V, welding speed is 7.5mm / s, and wire feeding speed is 12000mm / min; when vertical fillet welding is adopted, the specific welding parameters include the following parameters: welding current is 190A, welding voltage is 22V, welding speed is 4mm / s, and wire feeding speed is 6400mm / min; finally, the welding gun performs arc extinguishing welding according to the specific arc extinguishing parameters. Arc welding is performed according to the above-mentioned specific welding parameters, and the robot arm performs standard welding according to the above-mentioned specific welding parameters to ensure that the heat input meets the requirements, ensure the weld depth, improve the weld strength, prevent the formation of pores in the weld foot, and form a weld foot with a height of 6mm. The weld quality is high and can smoothly transition with the arc welding part, so that the hardness of the heat-affected zone meets the requirements and prevents weld cracking.

[0029] In the above welding process, the welding gun swings according to specific swing parameters to form a weld foot with a weld foot height of 6 mm. The welding gun on the robot arm can swing during welding. Even if the groove changes, the welding gun can cover the weld when swinging, which can ensure the welding quality of the weld and achieve the effect of weld correction. The welding gun on the robot arm can form a T-joint with a weld foot height of 6 mm using the above robot welding method, ensuring stable weld quality, and the welding speed is more than 20% higher than manual welding. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments of the present invention. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the contents of the embodiments of the present invention and these drawings without paying any creative work.

[0031] Figure 1 is a process flow chart of a robot welding method provided by a specific embodiment of the present invention;

[0032] Figure 2 It is a front view of a welding gun provided in a specific embodiment of the present invention using flat fillet welding;

[0033] Figure 3 It is a schematic diagram of the angle of the welding gun provided in a specific embodiment of the present invention using a flat fillet welding gun relative to the weld;

[0034] Figure 4 It is a top view of a welding gun provided by a specific embodiment of the present invention using vertical fillet welding;

[0035] Figure 5 It is a schematic diagram of the angle of the welding gun relative to the weld when the welding gun provided by the specific embodiment of the present invention adopts vertical fillet welding.

[0036] The following are marked in the figure:

[0037] 1. Welding plate; 11. Welding seam; 2. Welding gun. DETAILED DESCRIPTION

[0038] The present invention will be further described in detail below in conjunction with the accompanying drawings and embodiments. It is to be understood that the specific embodiments described herein are only used to explain the present invention, rather than to limit the present invention. It should also be noted that, for ease of description, only parts related to the present invention, rather than all structures, are shown in the accompanying drawings.

[0039] In the description of the present invention, unless otherwise clearly specified and limited, the terms "connected", "connected", and "fixed" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0040] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.

[0041] In the description of this embodiment, the terms "upper", "lower", "left", "right" and other directions or positional relationships are based on the directions or positional relationships shown in the drawings, and are only for the convenience of description and simplification of operation, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operate in a specific direction, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are only used to distinguish in the description and have no special meaning.

[0042] In modern manufacturing, robot welding technology has become an indispensable part with its high efficiency, stability and precision. The adjustment and control of the robot's welding parameters is still a crucial link. When the welding parameters are not set properly, a series of welding defects will occur, which will seriously affect the quality of the weld and the overall performance of the product. Specifically, if the welding parameters are poor, the first problem that may arise is that the weld is not completely through. This is due to insufficient heat input or inaccurate welding parameter settings, which leads to insufficient weld depth, thereby reducing the strength of the weld and increasing the risk of product failure. In addition, pores are also one of the common welding defects. They are formed when gas is trapped in the welding pool during the welding process, which weakens the density and strength of the weld, further increasing the safety risks of the product. In addition to the above defects, for T-joints with a weld foot height of 6mm, the weld foot height may not meet the structural requirements, reducing the welding strength.

[0043] To solve the above problems, Figure 1-Figure 5As shown, this embodiment provides a robot welding method, the welding gun 2 is arranged on the robot arm, and the welding gun 2 is applied to a T-joint with a welding leg height of 6 mm using the robot welding method. The robot welding method includes the following steps:

[0044] S1, welding gun 2 performs arc welding according to specific arc starting parameters;

[0045] S2, welding gun 2 performs standard welding according to specific welding parameters;

[0046] When flat fillet welding is adopted, the specific welding parameters include the following parameters: welding current is 280A, welding voltage is 27V, welding speed is 7.5mm / s, and wire feeding speed is 12000mm / min; when vertical fillet welding is adopted, the specific welding parameters include the following parameters: welding current is 190A, welding voltage is 22V, welding speed is 4mm / s, and wire feeding speed is 6400mm / min; arc welding is performed according to the above-mentioned specific welding parameters, and the robot arm performs standard welding according to the above-mentioned specific welding parameters so that the heat input meets the requirements, ensures the depth of weld 11, improves the strength of weld 11, prevents the formation of pores at the weld foot, forms a weld foot with a height of 6mm, and the weld 11 is of high quality and can smoothly transition with the arc welding part, so that the hardness of the heat-affected zone meets the requirements, and prevents the weld 11 from cracking.

[0047] S3, welding gun 2 performs arc extinguishing welding according to specific arc extinguishing parameters;

[0048] In step S1, step S2 and step S3, the welding gun 2 swings according to specific swing parameters to form a weld foot with a weld foot height of 6 mm; the welding gun 2 on the robot arm can swing during welding, and even if the groove changes, the welding gun 2 can cover the weld 11 when swinging, which can ensure the welding quality of the weld 11 and achieve the effect of correcting the deviation of the weld 11. The welding gun 2 on the robot arm of this embodiment can form a T-joint with a weld foot height of 6 mm using the above-mentioned robot welding method, ensure the stable quality of the weld 11, and the welding speed is increased by more than 20% compared with manual welding.

[0049] Preferably, in step S1, when flat fillet welding is adopted, the specific arc starting parameters include the following parameters: arc starting current is 274A, arc starting voltage is 25V, arc starting wire feeding speed is 11000mm / min; when vertical fillet welding is adopted, the specific arc starting parameters include the following parameters: arc starting current is 170A, arc starting voltage is 22V, arc starting wire feeding speed is 5200mm / min; arc starting welding is performed according to the above-mentioned specific arc starting parameters, which can ensure a smooth transition of the weld foot at the arc starting welding part, ensure the aesthetics of the arc starting part, and the weld foot at the arc starting part is fully formed, thereby improving the strength and reliability of the weld foot.

[0050] Preferably, in step S2, when flat fillet welding is adopted, the specific welding parameters include the following parameters: welding current is 280A, welding voltage is 27V, welding speed is 7.5mm / s, and wire feeding speed is 12000mm / min; when vertical fillet welding is adopted, the specific welding parameters include the following parameters: welding current is 190A, welding voltage is 22V, welding speed is 4mm / s, and wire feeding speed is 6400mm / min. The robot arm performs standard welding according to the above-mentioned specific welding parameters, and can form a weld foot with a weld foot height of 6mm, and the weld 11 is of high quality, and can smoothly transition with the arc welding part, so that the hardness of the heat-affected zone meets the requirements, and the weld 11 is prevented from cracking.

[0051] Furthermore, when flat fillet welding is adopted, the specific swing parameters include the following parameters: the swing form is "Z-shaped", the swing frequency is 1.5Hz, the swing amplitude is 2mm, and the swing limit position dwell time is 0; when vertical fillet welding is adopted, the specific swing parameters include the following parameters: the swing form is "Z-shaped", the swing frequency is 1Hz, the swing amplitude is 5mm, and the swing limit position dwell time is 0.4s. The above-mentioned specific swing parameters are adopted for swing welding, and regular lateral swings are performed on the weld 11, so that the welding energy is more evenly distributed on the weld 11, thereby improving the uniformity of the weld 11. Swing welding can form a good fusion between the weld 11 and the welding plate 1, thereby improving the strength and stability of the welding.

[0052] In this embodiment, Figure 2 and Figure 3 As shown, when flat fillet welding is used, the specific swing parameters also include that the angle between the axis of the welding gun 2 and the horizontal plane is 45°, and the axis of the welding gun 2 is perpendicular to the weld 11; Figure 4 and Figure 5 As shown, when vertical fillet welding is adopted, the specific swing parameters also include that the posture of the welding gun 2 is push welding, the angle between the axis of the welding gun 2 and the horizontal plane is 15°, and the axis of the welding gun 2 is located on the angle bisector of the angle between the two welding plates 1, wherein the two welding plates 1 are vertical, and the angle between the axis of the welding gun 2 and the two welding plates 1 is 45°. The appropriate angle of the welding gun 2 helps to reduce defects such as undercut and slag inclusion generated during welding, improve the quality of the weld 11 and improve welding efficiency.

[0053] Furthermore, in step S3, when flat fillet welding is adopted, the specific arc extinction parameters include the following parameters: arc extinction current is 220A, arc extinction voltage is 23V, arc extinction wire feeding speed is 8000mm / min; when vertical fillet welding is adopted, the specific arc extinction parameters include the following parameters: arc extinction current is 160A, arc extinction voltage is 20V, arc extinction wire feeding speed is 4500mm / min. Arc extinction welding is performed according to the above-mentioned specific arc extinction parameters, and the arc is stable during the arc extinction process, ensuring that the arc pit of the arc extinction welding part is filled, and preventing defects such as looseness, cracks, pores or slag inclusions from occurring in the arc extinction welding part.

[0054] Preferably, in step S1, step S2 and step S3, the welding part is sprayed with shielding gas, and the gas flow rate of shielding gas is 15L / min-25L / min. By spraying shielding gas, the weld 11 area can be isolated from oxygen and moisture in the air, thereby preventing oxidation and corrosion of high-temperature metal. This can not only maintain the metal composition and performance of the weld 11, but also reduce the generation of welding defects such as pores and cracks, and improve the corrosion resistance and durability of the weld 11. The shielding gas can also play a certain protective role on the welding gun 2, reduce equipment damage caused by high temperature and oxidation, and extend the service life of the equipment. In this embodiment, the shielding gas is CO2.

[0055] Further preferably, the shielding gas supply starts 1 second before arc welding, which can ensure that the air in the nozzle is exhausted, and the welding part is within the protection range of the shielding gas at the beginning of welding, reducing the impact of air on welding quality; the shielding gas supply ends 1.5 seconds after arc welding, and the shielding gas can cool and protect the welding point after welding stops. This embodiment improves the quality of the welding part while ensuring welding efficiency.

[0056] In this embodiment, the gap of the weld 11 between the two welding plates 1 is 0-2mm, and the thickness of the welding plate 1 is 3mm-16mm. Before welding, the area to be welded should be cleaned to ensure that there is no impurities such as oil, moisture, rust, etc. The welding wire in this embodiment uses a flux-cored wire with a diameter of 1.2mm.

[0057] This embodiment also provides a ship, which is welded by the above-mentioned robot welding method, the weld 11 is formed to be qualified, the weld foot height is 6mm-7mm, which meets the requirements, and the weld foot has no defects such as pores, undercuts, inclusions, cracks, etc. The robot adopts the above-mentioned robot welding method, which not only significantly improves the forming quality, but also increases the speed by more than 20% compared with the traditional welding method.

[0058] Note that the above are only preferred embodiments of the present invention and the technical principles used. Those skilled in the art will understand that the present invention is not limited to the specific embodiments described herein, and that various obvious changes, readjustments and substitutions can be made by those skilled in the art without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in more detail through the above embodiments, the present invention is not limited to the above embodiments, and may include more other equivalent embodiments without departing from the concept of the present invention, and the scope of the present invention is determined by the scope of the appended claims.

Claims

1. A robot welding method, characterized in that: A welding gun (2) is arranged on a robot arm, and the welding gun (2) is applied to a T-joint with a welding leg height of 6 mm using the robot welding method. The robot welding method comprises the following steps: S1, welding gun (2) performs arc welding according to specific arc starting parameters; S2, welding gun (2) performs standard welding according to specific welding parameters; When flat fillet welding is used, the specific welding parameters include the following parameters: welding current is 280A, welding voltage is 27V, welding speed is 7.5mm / s, and wire feeding speed is 12000mm / min; When vertical fillet welding is adopted, the specific welding parameters include the following parameters: welding current is 190A, welding voltage is 22V, welding speed is 4mm / s, and wire feeding speed is 6400mm / min; S3, the welding gun (2) performs arc extinguishing welding according to specific arc extinguishing parameters; In step S1, step S2 and step S3, the welding gun (2) is swung according to specific swung parameters to form a weld foot with a weld foot height of 6 mm.

2. The robot welding method according to claim 1, characterized in that: When flat fillet welding is used, the specific swing parameters include the following parameters: the swing form is "Z-shaped", the swing frequency is 1.5 Hz, the swing amplitude is 2 mm, and the swing limit position dwell time is 0; When vertical fillet welding is adopted, the specific swing parameters include the following parameters: the swing form is "Z-shaped", the swing frequency is 1 Hz, the swing amplitude is 5 mm, and the swing limit position dwell time is 0.4 s.

3. The robot welding method according to claim 2, characterized in that: When flat fillet welding is used, the specific swing parameters also include that the angle between the axis of the welding gun (2) and the horizontal plane is 45°, and the axis of the welding gun (2) is perpendicular to the weld (11); When vertical fillet welding is adopted, the specific swing parameters also include that the posture of the welding gun (2) is push welding, the angle between the axis of the welding gun (2) and the horizontal plane is 15°, and the axis of the welding gun (2) is located on the bisector of the angle between the two welding plates (1).

4. The robot welding method according to claim 1, characterized in that: In step S1, when flat fillet welding is adopted, the specific arc starting parameters include the following parameters: arc starting current is 274A, arc starting voltage is 25V, and arc starting wire feeding speed is 11000mm / min; When vertical fillet welding is adopted, the specific arc starting parameters include the following parameters: arc starting current is 170A, arc starting voltage is 22V, and arc starting wire feeding speed is 5200mm / min.

5. The robot welding method according to claim 1, characterized in that: In step S1, step S2 and step S3, the welding position is sprayed with a shielding gas, and the flow rate of the shielding gas is 15L / min-25L / min.

6. The robot welding method according to claim 5, characterized in that: The supply of the shielding gas starts 1 second before arc-starting welding, and ends 1.5 seconds after arc-extinguishing welding.

7. The robot welding method according to claim 5, characterized in that: The protective gas is CO2.

8. The robot welding method according to claim 1, characterized in that: In step S3, when flat fillet welding is used, the specific arc extinguishing parameters include the following parameters: arc extinguishing current is 220A, arc extinguishing voltage is 23V, and arc extinguishing wire feeding speed is 8000mm / min; When vertical fillet welding is adopted, the specific arc extinguishing parameters include the following parameters: arc extinguishing current is 160A, arc extinguishing voltage is 20V, and arc extinguishing wire feeding speed is 4500mm / min.

9. The robot welding method according to claim 1, characterized in that: The gap of the weld (11) between the two welding plates (1) is 0-2 mm.

10. A ship, characterized in that: The ship is welded by the robot welding method as described in any one of claims 1 to 9.

Citation Information

Patent Citations

  • Fillet weld automatically-tracking and automatically-adjusting device and intelligent welding robot thereof

    CN105935829A

  • Continuous automatic manufacturing process for T-shaped steel purlin supporting sheet

    CN110757102A

  • Laser-MIG composite double-gun synchronous symmetric welding method for titanium alloy T-shaped joint of medium plate

    CN114669880A

  • Welding method of oil tanker wall pier

    CN118404169A

  • Control method for lap welding of bead joint

    JP1999077305A

Cited By

  • Method for welding lower wrap angle of vertical T-shaped connector through welding robot

    CN119772322A