Equipment for producing multi-layer polycrystalline diamond compact and pressing regulation and control method thereof
By designing heating, pressure and cooling parts and intelligent control systems equipment in the production of multi-layer polycrystalline diamond composite sheets, the problems of material distribution and pressing parameter control are solved, efficient and accurate production processes are achieved, and product quality is improved. consistency.
Patent Information
- Application Number
- CN202411227192.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-03
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2044-09-03
AI Technical Summary
The existing multi-layer polycrystalline diamond composite sheet production technology is difficult to achieve uniform distribution and close integration of materials, resulting in unstable product performance, and traditional equipment cannot accurately control pressing parameters such as pressure, temperature and time, affecting product quality and consistency.
A device including a heating part, a pressure part, a cooling part and a control system is designed. The initial working parameters are set according to the physical characteristics and environmental parameters of the raw materials through the pressing control program, and the heating and cooling process is accurately controlled to ensure uniform pressure and temperature. Sex and stability.
Improves the accuracy of the pressing process and the effectiveness of the cooling process, ensures the quality and consistency of the multi-layer polycrystalline diamond composite sheet, is suitable for different production environments, reduces energy consumption and production costs, and is also extended to other composite materials. Suppress production.
Smart Images

Figure CN119058216A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of mechanical automation technology, and in particular to a device for producing a multi-layer polycrystalline diamond composite sheet and a pressing and regulating method thereof. Background Art
[0002] In modern industry, polycrystalline diamond (PCD) is widely used in cutting, drilling and grinding due to its excellent hardness, wear resistance and thermal stability. However, traditional single-layer PCD composites have limitations in certain applications, such as interlayer delamination under high temperature and high pressure conditions. In order to solve this problem, multi-layer polycrystalline diamond composites came into being. The multi-layer structure can effectively improve the overall performance of the composite sheet and enhance its stability and service life under extreme conditions.
[0003] However, the existing multi-layer PCD composite sheet production technology has many shortcomings. For example, it is difficult to achieve uniform distribution and close bonding of each layer of material during the pressing process, resulting in unstable performance of the final product. In addition, traditional pressing equipment also has limitations in regulation and control, and it is impossible to accurately control pressing parameters such as pressure, temperature and time, thus affecting the quality and consistency of the product.
[0004] Therefore, inventing an apparatus for producing multi-layer polycrystalline diamond composite sheets and a pressing and controlling method thereof can effectively solve the problems in the prior art and improve the production quality and consistency of multi-layer PCD composite sheets. Summary of the invention
[0005] In view of this, the present invention proposes an apparatus for producing a multilayer polycrystalline diamond composite sheet and a pressing and controlling method thereof, aiming to overcome the deficiencies in the prior art and improve the production quality and consistency of the multilayer polycrystalline diamond composite sheet.
[0006] The present invention provides a device for producing a multi-layer polycrystalline diamond composite sheet, comprising a heating part, a pressure part, a cooling part and a control system;
[0007] Wherein, the heating unit is configured to provide a temperature field for producing a multi-layer polycrystalline diamond compact;
[0008] The pressure portion is configured to apply pressure during heating;
[0009] The cooling unit is configured to cool the synthesis product after the synthesis process is completed;
[0010] The control system is connected to the heating part, the pressure part and the cooling part; the control system is provided with a pressing control program, and the pressing control program is configured to set the initial working parameters of the heating part, the pressure part and the cooling part according to the original property data of the raw materials and the product target parameters; the pressing control program is also configured to adjust the initial working parameters of the cooling part according to the environmental parameters.
[0011] Preferably, the suppression control program is configured as follows:
[0012] a1) obtaining an initial heating temperature according to the melting point of the raw material;
[0013] a2) obtaining an initial heating rate according to the initial heating temperature, the heating power, the specific heat capacity of the raw material, the initial temperature of the raw material, the total weight of the raw material and the target heating time;
[0014] a3) obtaining an initial applied pressure based on the initial compaction density of the raw material, the particle size, the purity of the raw material and the target compaction density, combined with the thermal expansion coefficient of the raw material during the heating process;
[0015] a4) obtaining an initial pressure application rate according to the initial heating temperature, the thermal expansion coefficient of the raw material, the bulk modulus of the raw material, the initial applied pressure, and the target applied pressure;
[0016] a5) obtaining an initial cooling rate according to the initial heating temperature, the target cooling temperature, the thermal conductivity of the raw material, the density of the raw material, the specific heat capacity of the raw material and the target cooling time.
[0017] Preferably, the initial heating temperature is obtained according to the melting point of the raw material using the following calculation formula:
[0018] T0=max(Tm,d,Tm,s)+ΔTm;
[0019] Wherein, T0 represents the initial heating temperature; Tm,d represents the melting point of diamond powder; Tm,s represents the melting point of cemented carbide substrate; ΔTm represents the safety temperature margin; max(Tm,d, Tm,s) represents taking the larger value of Tm,d and Tm,s.
[0020] Preferably, the initial heating rate is obtained using the following calculation formula according to the initial heating temperature, heating power, specific heat capacity of the raw material, initial temperature of the raw material, total weight of the raw material and target heating time:
[0021]
[0022]
[0023] Among them, Rh0 represents the initial heating rate; Rh1 represents the heating rate I; Rh2 represents the heating rate II; T0 represents the initial heating temperature; Ti represents the initial temperature of the raw material; th represents the target heating time; Q represents the heating power; m represents the total weight of the raw material; cp represents the weighted average specific heat capacity of the diamond powder and the cemented carbide substrate.
[0024] Preferably, the weighted average specific heat capacity of diamond powder and cemented carbide substrate is calculated as:
[0025]
[0026] Wherein, cp represents the weighted average specific heat capacity of diamond powder and cemented carbide substrate; mi is the mass of the i-th raw material; cp,i represents the specific heat capacity of the i-th raw material.
[0027] Preferably, the initial applied pressure is obtained using the following calculation formula based on the initial compaction density of the raw material, the particle size, the raw material purity and the target compaction density, combined with the thermal expansion coefficient of the raw material during the heating process:
[0028]
[0029] Where Pi represents the initial applied pressure; Di represents the initial compaction density of the raw material; Dt represents the target compaction density; CF represents the compaction factor determined based on particle size and purity; EV represents the effective volume after thermal expansion;
[0030] The calculation formula for the compaction factor CF based on particle size and purity is:
[0031]
[0032] Wherein, Ja represents the average particle size of diamond powder; Jmax represents the maximum particle size of diamond powder; Pp represents the purity of diamond powder;
[0033] The calculation formula for the effective volume EV after thermal expansion is:
[0034]
[0035] ΔT=T0-Ti;
[0036] Among them, V0,i represents the initial volume of the i-th material; βi represents the volume thermal expansion coefficient of the i-th material; T0 represents the initial heating temperature; Ti represents the initial temperature of the raw material; ΔT represents the temperature change.
[0037] Preferably, the initial pressure application rate is obtained using the following calculation formula according to the initial heating temperature, the thermal expansion coefficient of the raw material, the bulk modulus of the raw material, the initial applied pressure, and the target applied pressure:
[0038] ΔVd=Vd·βd·ΔT;
[0039] ΔVa=Va·βa·ΔT;
[0040]
[0041] Vt=Va+Vd;
[0042]
[0043] Wherein, Rp represents the initial pressure application rate; Kd represents the bulk modulus of diamond powder; βd represents the volume thermal expansion coefficient of diamond powder; Vd represents the initial volume of diamond powder; Ka represents the bulk modulus of cemented carbide substrate; βa represents the volume thermal expansion coefficient of cemented carbide substrate; Va represents the initial volume of cemented carbide substrate; Pd represents the additional pressure requirement of diamond powder; Pa represents the additional pressure requirement of cemented carbide substrate; ΔPd represents the pressure increment of diamond powder due to temperature change; ΔPa represents the pressure increment of cemented carbide substrate due to temperature change; Vt represents the total initial volume of diamond powder and cemented carbide substrate; Vd represents the initial volume of diamond powder; Va represents the initial volume of cemented carbide substrate; Δt represents the pressure application time; ΔVa represents the volume expansion of cemented carbide substrate; ΔVd represents the volume expansion of diamond powder; Pf represents the target applied pressure.
[0044] Preferably, the initial cooling rate is obtained using the following calculation formula according to the initial heating temperature, the target cooling temperature, the thermal conductivity of the raw material, the density of the raw material, the specific heat capacity of the raw material and the target cooling time:
[0045]
[0046] Ht=(md·cp,d+ma·cp,a)·Tx;
[0047] Wherein, Rc represents the initial cooling rate; Ht represents the total heat of diamond powder and cemented carbide substrate; Hf represents the heat corresponding to the final target temperature; Δtx represents the target cooling time; md represents the mass of diamond powder; ma represents the mass of cemented carbide substrate; cp,d represents the specific heat capacity of diamond powder; cp,a represents the specific heat capacity of cemented carbide substrate; Tx represents the temperature at the beginning of cooling.
[0048] Preferably, the initial operating parameters of the cooling unit are adjusted according to the environmental parameters using the following calculation formula:
[0049]
[0050] Among them, Ra represents the adjusted cooling rate; Rc represents the initial cooling rate; Ty represents the target cooling temperature; k represents the cooling rate empirical adjustment coefficient; Tamb represents the ambient temperature during the cooling process.
[0051] The present invention also provides a pressing and controlling method for producing a multilayer polycrystalline diamond composite sheet, comprising:
[0052] The initial heating temperature is obtained according to the melting point of the raw material;
[0053] obtaining an initial heating rate according to the initial heating temperature, the heating power, the specific heat capacity of the raw material, the initial temperature of the raw material, the total weight of the raw material, and the target heating time;
[0054] The initial applied pressure is obtained based on the initial compaction density of the raw material, the particle size, the purity of the raw material and the target compaction density, combined with the thermal expansion coefficient of the raw material during the heating process;
[0055] obtaining an initial pressure application rate according to an initial heating temperature, a thermal expansion coefficient of the raw material, a bulk modulus of the raw material, an initial applied pressure, and a target applied pressure;
[0056] Obtaining an initial cooling rate according to an initial heating temperature, a target cooling temperature, a thermal conductivity of the raw material, a density of the raw material, a specific heat capacity of the raw material, and a target cooling time;
[0057] The multi-layer polycrystalline diamond compact is produced by pressing according to the initial heating temperature, the initial heating rate, the initial applied pressure, the initial pressure application rate and the initial cooling rate.
[0058] Compared with the prior art, the present invention has the following beneficial effects:
[0059] 1. Improved the accuracy of the pressing process. By comprehensively considering the physical properties of the raw materials (such as particle size, purity, thermal expansion coefficient, etc.), the initial applied pressure and pressure application rate can be set more accurately, thereby ensuring that the raw materials reach the expected compaction density during the heating process.
[0060] 2. The cooling process is optimized. By calculating the initial cooling rate and the adjusted cooling rate, the cooling speed can be controlled more effectively to avoid internal stress and cracks in the material caused by rapid temperature changes, thereby improving the quality of multilayer polycrystalline diamond composite sheets.
[0061] 3. By adjusting the environmental parameters, the present invention can adapt to different production environments and ensure the stability and repeatability of the pressing process under different temperature conditions, thereby improving production efficiency and product consistency.
[0062] 4. The pressing and regulating method of the present invention is not only applicable to the production of multilayer polycrystalline diamond composite sheets, but can also be extended to the pressing production of other composite materials, and has broad application prospects.
[0063] 5. By precisely controlling the heating and cooling processes, the present invention can reduce energy consumption, lower production costs, and reduce the impact on the environment.
[0064] In summary, the present invention provides an efficient, precise and environmentally friendly method for pressing and controlling a multi-layer polycrystalline diamond composite sheet, which can significantly improve product quality and production efficiency and has important industrial application value. BRIEF DESCRIPTION OF THE DRAWINGS
[0065] Various other advantages and benefits will become apparent to those of ordinary skill in the art by reading the detailed description of the preferred embodiments below. The accompanying drawings are only for the purpose of illustrating the preferred embodiments and are not to be considered as limiting the present invention. Moreover, the same reference symbols are used throughout the accompanying drawings to represent the same components. In the accompanying drawings:
[0066] Figure 1 It is a schematic diagram of the equipment for producing multi-layer polycrystalline diamond composite sheets of the present invention;
[0067] Figure 2 The present invention is a flow chart of the pressing and controlling method for producing a multi-layer polycrystalline diamond composite sheet. DETAILED DESCRIPTION
[0068] Exemplary embodiments of the present disclosure will be described in more detail below with reference to the accompanying drawings. Although exemplary embodiments of the present disclosure are shown in the accompanying drawings, it should be understood that the present disclosure can be implemented in various forms and should not be limited by the embodiments described herein. On the contrary, these embodiments are provided in order to enable a more thorough understanding of the present disclosure and to fully convey the scope of the present disclosure to those skilled in the art. It should be noted that, in the absence of conflict, the embodiments of the present invention and the features described in the embodiments can be combined with each other. The present invention will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.
[0069] See also Figure 1 , this embodiment provides an apparatus for producing a multilayer polycrystalline diamond compact, including a heating portion, a pressure portion, a cooling portion and a control system;
[0070] Wherein, the heating unit is configured to provide a temperature field for producing a multi-layer polycrystalline diamond compact;
[0071] The pressure portion is configured to apply pressure during heating;
[0072] The cooling unit is configured to cool the synthesis product after the synthesis process is completed;
[0073] The control system is connected to the heating part, the pressure part and the cooling part; the control system is provided with a pressing control program, and the pressing control program is configured to set the initial working parameters of the heating part, the pressure part and the cooling part according to the original property data of the raw materials and the product target parameters; the pressing control program is also configured to adjust the initial working parameters of the cooling part according to the environmental parameters.
[0074] It is understood that this embodiment introduces an advanced device that is specifically used to produce multi-layer polycrystalline diamond compacts. The device consists of several key parts, including a heating part, a pressure part, a cooling part, and a highly intelligent control system. These parts work together to ensure high-quality production of multi-layer polycrystalline diamond compacts.
[0075] Specifically, the main function of the heating unit is to provide the necessary temperature field for the multilayer polycrystalline diamond composite sheet during the production process. By precisely controlling the temperature, the heating unit ensures that the raw materials reach ideal reaction conditions during the synthesis process, thereby promoting the formation of high-quality composite sheets.
[0076] The function of the pressure unit is to apply appropriate pressure during the heating process. By applying uniform and controllable pressure, the pressure unit helps the raw materials to fuse better under high temperature and high pressure, thereby forming a multi-layer polycrystalline diamond composite sheet with a dense structure and superior performance.
[0077] The cooling unit is responsible for effectively cooling the composite product after the synthesis process is completed. Through a reasonable cooling procedure, the cooling unit can prevent cracks or other defects in the composite sheet during the cooling process, ensuring the quality of the final product.
[0078] The control system is the core of the entire equipment. It is closely connected with the heating, pressure and cooling parts to ensure that these parts can work in a coordinated manner. The control system is equipped with a software module called the pressing control program, which can set the initial working parameters of the heating, pressure and cooling parts according to the original property data of the raw materials and the target parameters of the products. This means that before production starts, the control system has already made precise parameter settings according to the characteristics of the raw materials and the requirements of the target products.
[0079] In addition, the pressing control program also has the function of dynamically adjusting the initial working parameters of the cooling unit according to environmental parameters. This means that during the production process, if environmental conditions change, the control system can adjust the cooling program in real time to ensure that the quality of the final product is not affected. This flexibility and adaptability is one of the key factors in ensuring the production quality of multi-layer polycrystalline diamond composite sheets.
[0080] In summary, the equipment provided in this embodiment realizes comprehensive control over the production process of multi-layer polycrystalline diamond composite sheets through its heating part, pressure part, cooling part and control system, thereby ensuring high quality and high consistency of the products.
[0081] In some preferred embodiments of the present application, the suppression control program is configured as follows:
[0082] a1) obtaining an initial heating temperature according to the melting point of the raw material;
[0083] a2) obtaining an initial heating rate according to the initial heating temperature, the heating power, the specific heat capacity of the raw material, the initial temperature of the raw material, the total weight of the raw material and the target heating time;
[0084] a3) obtaining an initial applied pressure based on the initial compaction density of the raw material, the particle size, the purity of the raw material and the target compaction density, combined with the thermal expansion coefficient of the raw material during the heating process;
[0085] a4) obtaining an initial pressure application rate according to the initial heating temperature, the thermal expansion coefficient of the raw material, the bulk modulus of the raw material, the initial applied pressure, and the target applied pressure;
[0086] a5) obtaining an initial cooling rate according to the initial heating temperature, the target cooling temperature, the thermal conductivity of the raw material, the density of the raw material, the specific heat capacity of the raw material and the target cooling time.
[0087] It can be understood that the suppression control program of this embodiment is designed and configured to perform the following steps:
[0088] a1) First, determine an initial heating temperature based on the melting point of the raw material. This melting point is the temperature at which the raw material changes from solid to liquid, and is an important reference factor for selecting the initial heating temperature.
[0089] a2) Next, an initial heating rate is calculated using parameters such as initial heating temperature, heating power, specific heat capacity of the raw material, initial temperature of the raw material, total weight of the raw material, and target heating time. This heating rate determines the rate at which the temperature of the raw material rises during the heating process to ensure that the raw material can be heated to the desired temperature evenly and effectively.
[0090] a3) Then, an initial applied pressure is calculated based on the initial compaction density of the raw material, the particle size, the purity of the raw material and the target compaction density, combined with the thermal expansion coefficient of the raw material during the heating process. This applied pressure is to maintain the shape and density of the raw material during the heating process and prevent the raw material from uneven expansion or deformation during the heating process.
[0091] a4) Further, an initial pressure application rate is calculated based on the initial heating temperature, the thermal expansion coefficient of the raw material, the bulk modulus of the raw material, the initial applied pressure, and the target applied pressure. The pressure application rate determines the speed of change of the applied pressure during the heating process to ensure that the raw material can expand uniformly during the heating process and reach the target compaction density.
[0092] a5) Finally, an initial cooling rate is calculated based on the initial heating temperature, the target cooling temperature, the thermal conductivity of the raw material, the density of the raw material, the specific heat capacity of the raw material, and the target cooling time. This cooling rate determines the speed at which the raw material cools to the target temperature after heating is completed, so as to ensure that the raw material will not produce cracks or other defects due to too fast temperature changes during the cooling process.
[0093] Through the above steps, the pressing control program can accurately control the temperature and pressure changes of the raw materials during the heating and cooling process, thereby ensuring the quality and performance of the final product.
[0094] In some preferred embodiments of the present application, the initial heating temperature is obtained according to the melting point of the raw material using the following calculation formula:
[0095] T0=max(Tm,d,Tm,s)+ΔTm;
[0096] Wherein, T0 represents the initial heating temperature; Tm,d represents the melting point of diamond powder; Tm,s represents the melting point of cemented carbide substrate; ΔTm represents the safety temperature margin; max(Tm,d, Tm,s) represents taking the larger value of Tm,d and Tm,s.
[0097] It can be understood that the present embodiment determines the initial heating temperature through a specific calculation formula. Specifically, the initial heating temperature is calculated based on the melting point of the raw material. In the formula, T0 represents the initial heating temperature, and Tm,d represents the melting point of the diamond powder. Tm,s represents the melting point of the cemented carbide substrate. ΔTm represents the safety temperature margin, which is used to ensure that the material will not be damaged due to excessive temperature during the heating process. max(Tm,d, Tm,s) means taking the larger value of Tm,d and Tm,s to ensure that the initial heating temperature is at least higher than the one with the higher melting point of the two raw materials.
[0098] In this way, it can be ensured that during the heating process, both the diamond powder and the cemented carbide substrate can be heated within a safe temperature range, thereby avoiding material damage caused by excessive temperature. This calculation method is not only simple and easy to implement, but also can effectively ensure the safety and reliability of the heating process.
[0099] In some preferred embodiments of the present application, the initial heating rate is obtained according to the initial heating temperature, heating power, specific heat capacity of the raw material, initial temperature of the raw material, total weight of the raw material and target heating time using the following calculation formula:
[0100]
[0101] Among them, Rh0 represents the initial heating rate; Rh1 represents the heating rate I; Rh2 represents the heating rate II; T0 represents the initial heating temperature; Ti represents the initial temperature of the raw material; th represents the target heating time; Q represents the heating power; m represents the total weight of the raw material; cp represents the weighted average specific heat capacity of the diamond powder and the cemented carbide substrate.
[0102] It is understood that the advantage of this embodiment is that the heating process can be accurately controlled, thereby ensuring that the raw material reaches a uniform temperature distribution during the heating process. By optimizing the initial heating rate, the thermal stress concentration caused by excessive temperature gradient can be effectively avoided, thereby reducing the cracks and deformation that may occur in the raw material during the heating process. In addition, by accurately calculating the heating power and heating time, the production efficiency can be significantly improved, the production cycle can be shortened, and energy consumption can be reduced.
[0103] In some preferred embodiments of the present application, the weighted average specific heat capacity of diamond powder and cemented carbide substrate is calculated as follows:
[0104]
[0105] Wherein, cp represents the weighted average specific heat capacity of diamond powder and cemented carbide substrate; mi is the mass of the i-th raw material; cp,i represents the specific heat capacity of the i-th raw material.
[0106] It can be understood that the advantage of this embodiment is that by accurately calculating the weighted average specific heat capacity of the diamond powder and the cemented carbide substrate, the thermal management during the pressing process can be optimized. During the pressing process, temperature control is crucial to ensure the quality of the coating. If the temperature is too high, it may cause thermal damage to the diamond and even cause deformation of the cemented carbide substrate; while if the temperature is too low, the diamond powder may not be fully activated, affecting the adhesion and uniformity of the coating. Therefore, by accurately calculating the weighted average specific heat capacity of the diamond powder and the cemented carbide substrate, it can be ensured that the best thermal equilibrium state is achieved during the pressing process. This thermal equilibrium state helps to maintain a constant temperature during the pressing process, thereby avoiding the occurrence of the above-mentioned problems.
[0107] In some preferred embodiments of the present application, the initial applied pressure is obtained by using the following calculation formula according to the initial compaction density of the raw material, the particle size, the purity of the raw material and the target compaction density, combined with the thermal expansion coefficient of the raw material during the heating process:
[0108]
[0109] Where Pi represents the initial applied pressure; Di represents the initial compaction density of the raw material; Dt represents the target compaction density; CF represents the compaction factor determined based on particle size and purity; EV represents the effective volume after thermal expansion;
[0110] The calculation formula for the compaction factor CF based on particle size and purity is:
[0111]
[0112] Wherein, Ja represents the average particle size of diamond powder; Jmax represents the maximum particle size of diamond powder; Pp represents the purity of diamond powder;
[0113] The calculation formula for the effective volume EV after thermal expansion is:
[0114]
[0115] ΔT=T0-Ti;
[0116] Among them, V0,i represents the initial volume of the i-th material; βi represents the volume thermal expansion coefficient of the i-th material; T0 represents the initial heating temperature; Ti represents the initial temperature of the raw material; ΔT represents the temperature change.
[0117] It can be understood that the advantage of this embodiment is that it can ensure that the thermal expansion of the raw materials during the heating process is reasonably controlled by accurately calculating the initial applied pressure, so as to achieve the target compaction density. This calculation method not only improves production efficiency, but also reduces material waste and energy consumption.
[0118] In some preferred embodiments of the present application, the initial pressure application rate is obtained according to the initial heating temperature, the thermal expansion coefficient of the raw material, the bulk modulus of the raw material, the initial applied pressure, and the target applied pressure using the following calculation formula:
[0119] ΔVd=Vd·βd·ΔT;
[0120] ΔVa=Va·βa·ΔT;
[0121]
[0122] Vt=Va+Vd;
[0123]
[0124] Wherein, Rp represents the initial pressure application rate; Kd represents the bulk modulus of diamond powder; βd represents the volume thermal expansion coefficient of diamond powder; Vd represents the initial volume of diamond powder; Ka represents the bulk modulus of cemented carbide substrate; βa represents the volume thermal expansion coefficient of cemented carbide substrate; Va represents the initial volume of cemented carbide substrate; Pd represents the additional pressure requirement of diamond powder; Pa represents the additional pressure requirement of cemented carbide substrate; ΔPd represents the pressure increment of diamond powder due to temperature change; ΔPa represents the pressure increment of cemented carbide substrate due to temperature change; Vt represents the total initial volume of diamond powder and cemented carbide substrate; Vd represents the initial volume of diamond powder; Va represents the initial volume of cemented carbide substrate; Δt represents the pressure application time; ΔVa represents the volume expansion of cemented carbide substrate; ΔVd represents the volume expansion of diamond powder; Pf represents the target applied pressure.
[0125] It can be understood that the advantage of this embodiment is that it can ensure that the thermal expansion and volume change of the diamond powder and the cemented carbide substrate during the synthesis process are fully considered by accurately calculating the initial pressure application rate. In this way, material damage or synthesis failure caused by improper pressure application can be effectively avoided, thereby improving the yield and quality of synthetic diamonds.
[0126] In actual operation, the setting of the initial heating temperature is crucial to the entire synthesis process. The increase in temperature will cause the volume expansion of diamond powder and cemented carbide substrate, which will affect the effect of applied pressure. Through the above calculation formula, the initial applied pressure required at different temperatures can be determined in advance to ensure that the applied pressure is always in the optimal state during the entire heating process.
[0127] In addition, the bulk modulus and volume thermal expansion coefficient of the raw material are important parameters that affect the application of pressure. The bulk modulus reflects the material's ability to resist volume changes, while the volume thermal expansion coefficient describes the volume expansion characteristics of the material under temperature changes. By accurately measuring and calculating these parameters, the volume change of the material during the heating process can be more accurately predicted, thereby optimizing the pressure application strategy.
[0128] In some preferred embodiments of the present application, the initial cooling rate is obtained according to the initial heating temperature, the target cooling temperature, the thermal conductivity of the raw material, the density of the raw material, the specific heat capacity of the raw material and the target cooling time using the following calculation formula:
[0129]
[0130] Ht=(md·cp,d+ma·cp,a)·Tx;
[0131] Wherein, Rc represents the initial cooling rate; Ht represents the total heat of diamond powder and cemented carbide substrate; Hf represents the heat corresponding to the final target temperature; Δtx represents the target cooling time; md represents the mass of diamond powder; ma represents the mass of cemented carbide substrate; cp,d represents the specific heat capacity of diamond powder; cp,a represents the specific heat capacity of cemented carbide substrate; Tx represents the temperature at the beginning of cooling.
[0132] It can be understood that the advantage of this embodiment is that it can ensure that the diamond powder and the cemented carbide substrate reach the best thermal matching state during the cooling process by accurately calculating the initial cooling rate. This thermal matching state is crucial to ensure the bonding strength between the diamond powder and the cemented carbide substrate. By optimizing the cooling rate, thermal stress can be effectively reduced, and cracks or peeling of the coating during the cooling process can be avoided, thereby improving the overall quality and service life of the coating.
[0133] In practical applications, by adjusting the initial heating temperature and the target cooling time, the cooling rate can be flexibly controlled to adapt to the specific needs of different diamond powders. For example, in some cases, a faster cooling rate may be required to shorten the production cycle, while in other cases, a slower cooling rate may be required to ensure the uniformity and stability of the coating.
[0134] In addition, this embodiment also considers the effect of the thermal conductivity and density of the raw material on the cooling process. Materials with higher thermal conductivity can conduct heat faster, which helps to achieve a more uniform cooling effect. The density of the raw material affects the heat capacity of the material during the cooling process, which in turn affects the calculation of the cooling rate. By comprehensively considering these factors, the cooling process can be controlled more accurately to ensure that the performance of the diamond powder is optimal.
[0135] In summary, this embodiment not only improves the quality and reliability of diamond powder by accurately calculating the initial cooling rate, but also provides greater flexibility and controllability for the production process of diamond powder. This makes diamond powder have a wider application prospect in various industrial applications, especially in areas requiring high wear resistance and high hardness, such as cutting tools, drill bits and wear-resistant parts.
[0136] In some preferred embodiments of the present application, the initial operating parameters of the cooling unit are adjusted according to the environmental parameters using the following calculation formula:
[0137]
[0138] Among them, Ra represents the adjusted cooling rate; Rc represents the initial cooling rate; Ty represents the target cooling temperature; k represents the cooling rate empirical adjustment coefficient; Tamb represents the ambient temperature during the cooling process.
[0139] It is understandable that the advantage of this embodiment is that the cooling parameters can be flexibly adjusted according to the actual environmental conditions, so as to ensure the efficiency and stability of the cooling process. By introducing the ambient temperature Tamb and the target cooling temperature Ty, the system can monitor and adapt to external changes in real time, avoiding the poor cooling effect caused by environmental fluctuations. In addition, the introduction of the empirical adjustment coefficient k makes the adjustment of the cooling rate more accurate and personalized, so as to meet the needs of different application scenarios. Among them, the setting of the empirical adjustment coefficient k can be optimized based on a large amount of experimental data and historical records. In practical applications, the setting of the k value usually needs to consider factors such as the type of cooling medium, the performance of the cooling equipment, and the characteristics of the object to be cooled. For example, in a coolant cooling system, the k value may be adjusted according to the thermal conductivity and fluidity of the coolant. In an air cooling system, the k value may be related to the speed and air volume of the fan.
[0140] See also Figure 2 This embodiment also provides a pressing and controlling method for producing a multi-layer polycrystalline diamond composite sheet, comprising:
[0141] The initial heating temperature is obtained according to the melting point of the raw material;
[0142] obtaining an initial heating rate according to the initial heating temperature, the heating power, the specific heat capacity of the raw material, the initial temperature of the raw material, the total weight of the raw material, and the target heating time;
[0143] The initial applied pressure is obtained based on the initial compaction density of the raw material, the particle size, the purity of the raw material and the target compaction density, combined with the thermal expansion coefficient of the raw material during the heating process;
[0144] obtaining an initial pressure application rate according to an initial heating temperature, a thermal expansion coefficient of the raw material, a bulk modulus of the raw material, an initial applied pressure, and a target applied pressure;
[0145] Obtaining an initial cooling rate according to an initial heating temperature, a target cooling temperature, a thermal conductivity of the raw material, a density of the raw material, a specific heat capacity of the raw material, and a target cooling time;
[0146] The multi-layer polycrystalline diamond compact is produced by pressing according to the initial heating temperature, the initial heating rate, the initial applied pressure, the initial pressure application rate and the initial cooling rate.
[0147] It is understood that the advantage of this embodiment is that the key parameters in the production process can be accurately controlled, thereby ensuring the quality and performance of the multilayer polycrystalline diamond composite sheet. By optimizing the initial heating temperature, the problem of overheating or uneven heating of the raw material during the heating process can be avoided, thereby ensuring the uniformity of the raw material. The calculation of the initial heating rate ensures the stability of the heating process and avoids the internal stress concentration of the raw material caused by too fast temperature change.
[0148] The determination of the initial applied pressure takes into account the initial compaction density, particle size, purity and target compaction density of the raw materials, which helps to achieve uniform distribution and tight bonding of the raw materials during the pressing process. At the same time, combined with the thermal expansion coefficient of the raw materials during the heating process, it can effectively prevent internal stress caused by temperature changes and ensure the stability of the pressing process.
[0149] The calculation of the initial pressure application rate ensures uniform pressure transfer during the pressing process, avoiding cracks or defects caused by too rapid pressure changes. The determination of the initial cooling rate takes into account the thermal conductivity, density, specific heat capacity of the raw materials and the target cooling time, which helps to control the temperature gradient during the cooling process and prevent thermal stress and cracks caused by too rapid cooling.
[0150] In summary, this embodiment achieves fine regulation of the pressing process of the multi-layer polycrystalline diamond composite sheet by accurately controlling key parameters in the production process, thereby improving the quality and performance of the product.
[0151] Those skilled in the art will appreciate that the embodiments of the present application may be provided as methods, systems or computer program products. Therefore, the present application may adopt the form of a complete hardware embodiment, a complete software embodiment, or an embodiment in combination with software and hardware. Moreover, the present application may adopt the form of a computer program product implemented on one or more computer-usable storage media (including but not limited to disk storage, CD-ROM, optical storage, etc.) containing computer-usable program codes.
[0152] The present application is described with reference to flowcharts and / or block diagrams of methods, devices (systems) and computer program products according to embodiments of the present application. It should be understood that each process and / or box in the flowchart and / or block diagram, as well as the combination of processes and / or boxes in the flowchart and / or block diagram, can be implemented by computer program instructions. These computer program instructions can be provided to a processor of a general-purpose computer, a special-purpose computer, an embedded processor or other programmable data processing device to generate a machine, so that the instructions executed by the processor of the computer or other programmable data processing device generate instructions for implementing the processes in the flowchart and / or block diagram. Figure 1 A process or multiple processes and / or boxes Figure 1 A device that provides the functions specified in a block or multiple blocks.
[0153] These computer program instructions may also be stored in a computer readable memory capable of directing a computer or other programmable data processing device to operate in a specific manner, so that the instructions stored in the computer readable memory produce an article of manufacture including an instruction device, which implements the process Figure 1 A process or multiple processes and / or boxes Figure 1 A function specified in one or more boxes.
[0154] These computer program instructions can also be loaded onto a computer or other programmable data processing device so that a series of operating steps are executed on the computer or other programmable device to produce a computer-implemented process, thereby providing instructions for implementing the process in the computer or other programmable device. Figure 1 A process or multiple processes and / or boxes Figure 1 The steps for the functions specified in one or more boxes.
[0155] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the above embodiments, ordinary technicians in the relevant field should understand that the specific implementation methods of the present invention can still be modified or replaced by equivalents. Any modification or equivalent replacement that does not depart from the spirit and scope of the present invention should be covered within the scope of protection of the claims of the present invention.
Claims
1. An apparatus for producing a multilayer polycrystalline diamond composite sheet, characterized in that: It includes a heating part, a pressure part, a cooling part and a control system; Wherein, the heating unit is configured to provide a temperature field for producing a multi-layer polycrystalline diamond compact; The pressure portion is configured to apply pressure during heating; The cooling unit is configured to cool the synthesis product after the synthesis process is completed; The control system is connected to the heating part, the pressure part and the cooling part; the control system is provided with a pressing control program, and the pressing control program is configured to set the initial working parameters of the heating part, the pressure part and the cooling part according to the original property data of the raw materials and the product target parameters; the pressing control program is also configured to adjust the initial working parameters of the cooling part according to the environmental parameters.
2. The device for producing a multilayer polycrystalline diamond compact according to claim 1, characterized in that: The suppression control program is configured to: a1) obtaining an initial heating temperature according to the melting point of the raw material; a2) obtaining an initial heating rate according to the initial heating temperature, the heating power, the specific heat capacity of the raw material, the initial temperature of the raw material, the total weight of the raw material and the target heating time; a3) obtaining an initial applied pressure based on the initial compaction density of the raw material, the particle size, the purity of the raw material and the target compaction density, combined with the thermal expansion coefficient of the raw material during the heating process; a4) obtaining an initial pressure application rate according to the initial heating temperature, the thermal expansion coefficient of the raw material, the bulk modulus of the raw material, the initial applied pressure, and the target applied pressure; a5) obtaining an initial cooling rate according to the initial heating temperature, the target cooling temperature, the thermal conductivity of the raw material, the density of the raw material, the specific heat capacity of the raw material and the target cooling time.
3. The device for producing a multilayer polycrystalline diamond compact according to claim 2, characterized in that: The initial heating temperature is obtained based on the melting point of the raw materials using the following calculation formula: T0=max(Tm,d,Tm,s)+ΔTm; Wherein, T0 represents the initial heating temperature; Tm,d represents the melting point of diamond powder; Tm,s represents the melting point of cemented carbide substrate; ΔTm represents the safety temperature margin; max(Tm,d, Tm,s) represents taking the larger value of Tm,d and Tm,s.
4. The device for producing a multilayer polycrystalline diamond compact according to claim 3, characterized in that: The initial heating rate is obtained using the following calculation formula based on the initial heating temperature, heating power, specific heat capacity of the raw material, initial temperature of the raw material, total weight of the raw material, and target heating time: Among them, Rh0 represents the initial heating rate; Rh1 represents the heating rate I; Rh2 represents the heating rate II; T0 represents the initial heating temperature; Ti represents the initial temperature of the raw material; th represents the target heating time; Q represents the heating power; m represents the total weight of the raw material; cp represents the weighted average specific heat capacity of the diamond powder and the cemented carbide substrate.
5. The device for producing a multilayer polycrystalline diamond compact according to claim 4, characterized in that: The weighted average specific heat capacity of diamond powder and cemented carbide substrate is calculated as follows: Wherein, cp represents the weighted average specific heat capacity of diamond powder and cemented carbide substrate; mi is the mass of the i-th raw material; cp,i represents the specific heat capacity of the i-th raw material.
6. The device for producing a multilayer polycrystalline diamond compact according to claim 2, characterized in that: The initial applied pressure is obtained using the following calculation formula based on the initial compaction density of the raw material, the particle size, the raw material purity and the target compaction density, combined with the thermal expansion coefficient of the raw material during heating: Where Pi represents the initial applied pressure; Di represents the initial compaction density of the raw material; Dt represents the target compaction density; CF represents the compaction factor determined based on particle size and purity; EV represents the effective volume after thermal expansion; The calculation formula for the compaction factor CF based on particle size and purity is: Wherein, Ja represents the average particle size of diamond powder; Jmax represents the maximum particle size of diamond powder; Pp represents the purity of diamond powder; The calculation formula for the effective volume EV after thermal expansion is: ΔT=T0-Ti; Among them, V0,i represents the initial volume of the i-th material; βi represents the volume thermal expansion coefficient of the i-th material; T0 represents the initial heating temperature; Ti represents the initial temperature of the raw material; ΔT represents the temperature change.
7. The device for producing a multilayer polycrystalline diamond compact according to claim 6, characterized in that: The initial pressure application rate is obtained using the following calculation formula based on the initial heating temperature, the thermal expansion coefficient of the raw material, the bulk modulus of the raw material, the initial applied pressure, and the target applied pressure: ΔVd=Vd·βd·ΔT; ΔVa=Va·βa·ΔT; Vt=Va+Vd; Wherein, Rp represents the initial pressure application rate; Kd represents the bulk modulus of diamond powder; βd represents the volume thermal expansion coefficient of diamond powder; Vd represents the initial volume of diamond powder; Ka represents the bulk modulus of cemented carbide substrate; βa represents the volume thermal expansion coefficient of cemented carbide substrate; Va represents the initial volume of cemented carbide substrate; Pd represents the additional pressure requirement of diamond powder; Pa represents the additional pressure requirement of cemented carbide substrate; ΔPd represents the pressure increment of diamond powder due to temperature change; ΔPa represents the pressure increment of cemented carbide substrate due to temperature change; Vt represents the total initial volume of diamond powder and cemented carbide substrate; Vd represents the initial volume of diamond powder; Va represents the initial volume of cemented carbide substrate; Δt represents the pressure application time; ΔVa represents the volume expansion of cemented carbide substrate; ΔVd represents the volume expansion of diamond powder; Pf represents the target applied pressure.
8. The device for producing a multi-layer polycrystalline diamond compact according to claim 2, characterized in that: The initial cooling rate is obtained using the following calculation formula based on the initial heating temperature, the target cooling temperature, the thermal conductivity of the raw material, the density of the raw material, the specific heat capacity of the raw material, and the target cooling time: Ht=(md·cp,d+ma·cp,a)·Tx; Wherein, Rc represents the initial cooling rate; Ht represents the total heat of diamond powder and cemented carbide substrate; Hf represents the heat corresponding to the final target temperature; Δtx represents the target cooling time; md represents the mass of diamond powder; ma represents the mass of cemented carbide substrate; cp,d represents the specific heat capacity of diamond powder; cp,a represents the specific heat capacity of cemented carbide substrate; Tx represents the temperature at the beginning of cooling.
9. The device for producing a multilayer polycrystalline diamond compact according to claim 2, characterized in that: The initial operating parameters of the cooling unit are adjusted according to the environmental parameters using the following calculation formula: Among them, Ra represents the adjusted cooling rate; Rc represents the initial cooling rate; Ty represents the target cooling temperature; k represents the cooling rate empirical adjustment coefficient; Tamb represents the ambient temperature during the cooling process.
10. A method for pressing and controlling a multilayer polycrystalline diamond composite sheet, characterized in that: include: The initial heating temperature is obtained according to the melting point of the raw material; obtaining an initial heating rate according to the initial heating temperature, the heating power, the specific heat capacity of the raw material, the initial temperature of the raw material, the total weight of the raw material, and the target heating time; The initial applied pressure is obtained based on the initial compaction density of the raw material, the particle size, the purity of the raw material and the target compaction density, combined with the thermal expansion coefficient of the raw material during the heating process; obtaining an initial pressure application rate according to an initial heating temperature, a thermal expansion coefficient of the raw material, a bulk modulus of the raw material, an initial applied pressure, and a target applied pressure; Obtaining an initial cooling rate according to an initial heating temperature, a target cooling temperature, a thermal conductivity of the raw material, a density of the raw material, a specific heat capacity of the raw material, and a target cooling time; The multi-layer polycrystalline diamond compact is produced by pressing according to the initial heating temperature, the initial heating rate, the initial applied pressure, the initial pressure application rate and the initial cooling rate.
Citation Information
Patent Citations
Preparation method of polycrystalline diamond
CN104014282A
Preparation method of polycrystalline diamond compact and polycrystalline diamond compact
CN106694887A
Diamond compact and preparation method thereof
CN111420616A
Synthetic apparatus for producing for diamond
CN204911432U
Method and device for synthesizing diamond crystal
JP1998005572A