Early strength type paving mortar and preparation method thereof
By adding crack-resistant fibers and modified epoxy resin to the mortar, combined with dopamine-modified aramid fibers and nano-modified rubber particles, the problem of insufficient compressive strength of the mortar is solved, and the mechanical properties and stability of the mortar are significantly improved. Ensure the safety of high-rise buildings.
Patent Information
- Application Number
- CN202411176488.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-26
- Publication Date
- 2024-12-03
AI Technical Summary
The existing mortar is insufficient when used in high-rise buildings, which has safety hazards and is difficult to meet huge strength requirements.
The preparation method of early strength paving mortar is adopted. By adding crack-resistant fibers and modified epoxy resin to the mortar, combined with dopamine-modified aramid fibers and nano-modified rubber particles, the mechanical strength and temperature resistance of the mortar are improved. , enhance the stability of the mortar.
It significantly improves the compressive strength and crack resistance of the mortar, reduces the crack phenomenon of the mortar under different temperature environments, improves the overall mechanical properties and stability, and ensures the safety of high-rise buildings.
Smart Images

Figure BDA0005010861350000081
Abstract
Description
Technical Field
[0001] The present application relates to the field of mortar, and in particular to an early-strength paving mortar and a preparation method thereof. Background Art
[0002] Mortar is a practical bonding material for bricklaying in construction. It is made of a certain proportion of sand and binding materials (cement, lime paste, clay, etc.) and water. It is also called mortar. It can be used for the masonry of bricks, stones, blocks, etc. and the installation of components. It can also be used for plastering of walls, floors, roofs, beams and columns to meet the requirements of protection and decorative lighting.
[0003] In construction projects, high requirements are placed on the mortar used for paving. Especially when building high-rise buildings, the mortar needs to have great strength, otherwise safety hazards are likely to occur, so there is room for improvement. Summary of the invention
[0004] In order to improve the compressive strength of mortar, the present application provides an early-strength paving mortar and a preparation method thereof.
[0005] The present application provides an early-strength paving mortar and a preparation method thereof using the following technical solutions: In the first aspect, the present application provides an early-strength paving mortar, which adopts the following technical solution: An early-strength paving mortar comprises the following components by mass: 80-100 parts of aggregate; 30-40 parts of anti-cracking fiber, 40-60 parts of modified epoxy resin, 150-210 parts of sand and gravel, 100-150 parts of cement, and 3-9 parts of water reducing agent.
[0006] By adopting the above technical solution, modified epoxy resin and anti-cracking fibers are filled in the mortar, which can effectively improve the mechanical strength of the paving mortar. At the same time, the anti-cracking fibers can improve the mortar's resistance to temperature changes, and it can also have good mechanical properties under different temperature environments, further improving the overall mechanical properties and stability of the paving mortar.
[0007] Preferably, the anti-cracking fiber comprises aramid fiber, dopamine and a graft coupling agent.
[0008] By adopting the above technical solution, aramid fiber is a new type of polymer fiber with good temperature resistance and excellent strength and toughness. It is added to the mortar as a reinforcing material to further improve the mechanical properties and stability of the mortar body. Dopamine is the adhesion component of mussel adhesion protein. Using dopamine to modify aramid fiber can further enhance the connection between aramid fiber and various components of paving mortar, making the paving mortar more stable and improving the overall mechanical properties of the paving mortar.
[0009] Preferably, the anti-cracking fiber is prepared by the following method: The aramid fiber is washed and dried for later use, a dopamine solution is prepared using hydrochloric acid, dopamine and deionized water, the dried aramid fiber is immersed in the prepared dopamine solution, stirred for 4-6 hours to obtain dopamine-modified aramid fiber, polyethyleneimine is added at a temperature of 30-34°C, stirred for 9-11 hours, the fiber is washed, and dried to obtain crack-resistant modified fiber.
[0010] Preferably, the concentration of dopamine in the dopamine solution is 10-13 g / 100 mL.
[0011] By adopting the above technical solution and controlling the concentration of dopamine within the above range, the stability of the crack-resistant fiber can be further improved.
[0012] Preferably, the modified epoxy resin comprises nano-modified rubber particles, epoxy resin and cage-type silsesquioxane.
[0013] By adopting the above technical solution, epoxy resin is also added to the mortar filler as a filler, which can synergize with aramid fiber to improve the temperature resistance of the paving mortar, and can also effectively reduce the cracking of the mortar in the future. Epoxy resin and modified rubber particles are used as fillers to improve the overall mechanical properties of the mortar and further reduce the occurrence of cracking on the mortar surface.
[0014] Preferably, the graft coupling agent includes γ-aminopropyltriethoxysilane and polyethyleneimine.
[0015] Preferably, the modified epoxy resin comprises nano-modified rubber particles, epoxy resin and cage-type silsesquioxane.
[0016] By adopting the above technical solution, the modified rubber particles, epoxy resin and cage-type double-plate siloxane are combined to obtain a modified epoxy resin material with improved compatibility, which can effectively improve the mechanical properties of the concrete after being added to the concrete.
[0017] The mass ratio of the nano-modified rubber particles, the epoxy resin and the cage-type silsesquioxane is 10:(4-8):1.
[0018] By adopting the above technical solution, the mass ratio of the modified rubber particles, the epoxy resin and the cage-type silsesquioxane is controlled within the above range, which can further improve the stability of the modified epoxy resin.
[0019] Preferably, the nano-modified rubber particles include nitrile nano-rubber, white carbon black and tannic acid.
[0020] By adopting the above technical scheme, white carbon black and rubber particles can synergistically improve the overall mechanical properties of nitrile nano rubber particles. After white carbon black is modified with tannic acid, the dispersion effect of white carbon black in rubber can be improved, and the compatibility between white carbon black and rubber particles is improved, further improving the stability of nano-modified rubber particles, thereby improving the mechanical properties of nitrile nano rubber particles.
[0021] Preferably, the nano-modified rubber particles are prepared by the following method: Mixing tannic acid and white carbon black, and feeding into an ethanol solution, stirring, washing and centrifuging to obtain white powder, and drying the white powder to obtain modified white carbon black; The natural rubber and the rubber are mixed and kneaded to obtain modified rubber, and the modified rubber is ground to obtain nano-modified rubber particles.
[0022] In a second aspect, the present application provides a method for preparing an early-strength paving mortar, which adopts the following technical solution: A preparation method for early-strength paving mortar comprises the following steps: mixing cement, sand and aggregate, adding anti-cracking fiber and modified epoxy resin, stirring for 30-40 minutes, adding a water reducing agent, and continuing to stir to obtain early-strength paving mortar.
[0023] In summary, the present application includes at least one of the following beneficial technical effects: 1. In this application, in addition to the basic components of the mortar, anti-cracking fibers and modified epoxy resins are also added. Under the synergistic effect of the anti-cracking fibers and the modified epoxy resins, the temperature resistance of the laying mortar can be improved together, and the overall compressive strength and crack resistance of the mortar can be improved. In the subsequent use of the mortar, the occurrence of cracks in the mortar can be effectively reduced, and the overall stability of the mortar can be improved.
[0024] 2. The aramid fiber is modified by dopamine, and phenol, imino group, etc. are introduced to improve the activity of the aramid fiber, thereby increasing the interface connection strength between the various components of the aramid fiber in the mortar system, thereby improving the overall mechanical strength of the mortar; 3. The addition of silica effectively improves the mechanical properties of nitrile nano-rubber particles. The addition of tannic acid can further improve the dispersion performance of silica and make the silica and nitrile nano-rubber particles cross-link to form a dense network structure to obtain modified epoxy resin. Adding it to the mortar system can improve the overall mechanical properties of the paving mortar. DETAILED DESCRIPTION
[0025] The present application discloses an early-strength paving mortar and a preparation method thereof. The present application is further described in detail below in conjunction with the embodiments: Example 1 Preparation of modified nano rubber particles: Weigh 13.88 g of silica for use, add 1.12 g of tannic acid to 40 ml of ethanol, mix to obtain a tannic acid solution, add the weighed silica and tannic acid solution to 200 ml of deionized water and mix thoroughly to obtain a mixture A, ultrasonicate the mixture A in a water bath sonicator at 45° C. for 30 min to obtain modified silica, dry the modified silica prepared above in an oven at 60° C. for 12 h to obtain dried modified silica, mix the modified silica prepared above with 80 g of nitrile nano-rubber particles, send them into an internal mixer for internal mixing to obtain modified rubber, and crush the modified rubber to obtain modified rubber particles.
[0026] Preparation of modified epoxy resin: Weigh 21.33 g of polyphenol oxide resin and 5.34 g of cage-type silsesquioxane (CAS No.: 1204591-17-2), mix the two and add them into 500 ml of dimethyl sulfoxide (CAS No.: 67-68-5) and stir for 2 hours. After dissolving evenly, under nitrogen protection, heat to 150 ° C and maintain for 3 hours, then cool to 30 ° C to obtain a white solid. The white solid is crushed and sent to an internal mixer with 53.33 g of the modified rubber prepared above for internal mixing. After internal mixing, it is crushed and ground to obtain modified resin particles.
[0027] Preparation of crack-resistant aramid fibers: Weigh 42.35 g of aramid fiber, add acetone until the acetone covers the fiber surface, stir for 30 minutes, send it into an ultrasonic cleaner, wash it 3 times at 40 kHz, each time for 45 minutes, then wash the aramid fiber with deionized water, send it into an oven, and dry it at 45 ° C for 12 hours to obtain the pre-treated aramid fiber; use 1 mol / L hydrochloric acid and distilled water (the mass ratio of hydrochloric acid to distilled water is 1:1) and dopamine (CAS No.: 51-61-6) to prepare a dopamine solution, use Tris buffer solution to adjust the pH value of the dopamine solution to 8.5, and obtain a dopamine solution with a dopamine concentration of 10 g / 100 mL. The aramid fiber was added to 120 ml of the prepared dopamine solution, stirred at 30°C for 7 hours, and washed with deionized water to obtain dopamine grafted aramid fiber; γ-aminopropyltriethoxysilane (CAS No.: 919-30-2) and polyethyleneimine (CAS No.: 9002-98-6) were mixed in a mass ratio of 1:1 to obtain a grafted coupling agent, 2.65 g of the grafted coupling agent was mixed with 120 ml of deionized water to obtain a coupling agent mixed solution, the dopamine grafted aramid fiber was added to the coupling agent mixed solution, stirred at 50°C for 3 hours, then washed with deionized water, and dried in an oven at 50°C for 6 hours to obtain crack-resistant aramid fiber.
[0028] Preparation of early strength paving mortar: After mixing 100g of cement, 150g of sand and gravel and 80g of aggregate, add 30g of the above-prepared anti-cracking fiber and 40g of modified epoxy resin particles, stir for 30min, add 3g of water reducer and continue to stir for 1h to obtain early strength paving mortar; Among them, the water reducer is a naphthalene-based water reducer.
[0029] Example 2 Preparation of modified nano rubber: Weigh 13.76 g of silica for use, add 1.24 g of tannic acid to 40 ml of ethanol, mix to obtain a tannic acid solution, add the weighed silica and tannic acid solution to 200 ml of deionized water and mix thoroughly to obtain a mixture A, ultrasonicate the mixture A in a water bath sonicator at 45° C. for 30 min to obtain modified silica, dry the modified silica prepared above in an oven at 60° C. for 12 h to obtain dried modified silica, mix the modified silica prepared above with 80 g of nitrile nano-rubber particles, send them into an internal mixer for internal mixing to obtain modified rubber, and crush the modified rubber to obtain modified rubber particles.
[0030] Preparation of modified epoxy resin: Weigh 33.69 g of polyphenol oxide resin and 4.21 g of cage-type silsesquioxane (CAS No.: 1204591-17-2), mix the two and add them into 500 ml of dimethyl sulfoxide (CAS No.: 67-68-5) and stir for 2 hours. After dissolving evenly, under nitrogen protection, heat to 150 ° C and maintain for 3 hours, then cool to 30 ° C to obtain a white solid. The white solid is crushed and sent to an internal mixer with 42.1 g of the modified rubber prepared above for internal mixing. After internal mixing, it is crushed and ground to obtain modified resin particles.
[0031] Preparation of crack-resistant aramid fibers: Weigh 42.63 g of aramid fiber, add acetone until the acetone covers the fiber surface, stir for 30 minutes, send it into an ultrasonic cleaner, wash it 3 times at 40 kHz, each time for 45 minutes, then wash the aramid fiber with deionized water, send it into an oven, and dry it at 45 ° C for 12 hours to obtain the pre-treated aramid fiber; use 1 mol / L hydrochloric acid and distilled water (the mass ratio of hydrochloric acid to distilled water is 1:1) and dopamine (CAS No.: 51-61-6) to prepare a dopamine solution, use Tris buffer solution to adjust the pH value of the dopamine solution to 8.5, and obtain a dopamine solution with a dopamine concentration of 13 g / 100 ml. The aramid fiber was added to 120 ml of the prepared dopamine solution, stirred at 30°C for 7 hours, and washed with deionized water to obtain dopamine grafted aramid fiber; γ-aminopropyltriethoxysilane (CAS No.: 919-30-2) and polyethyleneimine (CAS No.: 9002-98-6) were mixed in a mass ratio of 1:1 to obtain a grafted coupling agent, 2.37 g of the grafted coupling agent was mixed with 120 ml of deionized water to obtain a coupling agent mixed solution, the dopamine grafted aramid fiber was added to the coupling agent mixed solution, stirred at 50°C for 3 hours, then washed with deionized water, and dried in an oven at 50°C for 6 hours to obtain crack-resistant aramid fiber.
[0032] Preparation of early strength paving mortar: After mixing 150g of cement, 270g of sand and gravel and 120g of aggregate, add 40g of the above-prepared anti-cracking fiber and 60g of modified epoxy resin particles, stir for 40min, add 9g of water reducer and continue to stir for 1h to obtain early-strength paving mortar; Among them, the water reducer is a naphthalene-based water reducer.
[0033] Example 3 Preparation of modified nano rubber: Weigh 13.51 g of silica for use, add 1.49 g of tannic acid to 40 ml of ethanol, mix to obtain a tannic acid solution, add the weighed silica and tannic acid solution to 200 ml of deionized water and mix thoroughly to obtain a mixture A, ultrasonicate the mixture A in a water bath sonicator at 45° C. for 30 min to obtain modified silica, dry the modified silica prepared above in an oven at 60° C. for 12 h to obtain dried modified silica, mix the modified silica prepared above with 80 g of nitrile nano-rubber particles, send them into an internal mixer for internal mixing to obtain modified rubber, and crush the modified rubber to obtain modified rubber particles.
[0034] Preparation of modified epoxy resin: Weigh 28.24 g of polyphenol oxide resin and 4.71 g of cage-type silsesquioxane (CAS No.: 1204591-17-2), mix the two and add them into 500 ml of dimethyl sulfoxide (CAS No.: 67-68-5) and stir for 2 hours. After dissolving evenly, under nitrogen protection, heat to 150 ° C and maintain for 3 hours, then cool to 30 ° C to obtain a white solid. The white solid is crushed and sent to an internal mixer with 47.05 g of the modified rubber prepared above for internal mixing. After internal mixing, it is crushed and ground to obtain modified resin particles.
[0035] Preparation of crack-resistant aramid fibers: Weigh 42.5 g of aramid fiber, add acetone until the acetone covers the fiber surface, stir for 30 min, send it into an ultrasonic cleaner, wash it 3 times at 40 kHz, each time for 45 min, then wash the aramid fiber with deionized water, send it into an oven, dry it at 45 ° C for 12 h, and obtain the pre-treated aramid fiber; use 1 mol / L hydrochloric acid and distilled water (the mass ratio of hydrochloric acid to distilled water is 1:1) and dopamine (CAS No.: 51-61-6) to prepare a dopamine solution, use Tris buffer solution to adjust the pH value of the dopamine solution to 8.5, and obtain a dopamine solution with a dopamine concentration of 12 g / 100 ml. The aramid fiber was added to 120 ml of the prepared dopamine solution, stirred at 30°C for 7 hours, and washed with deionized water to obtain dopamine grafted aramid fiber; γ-aminopropyltriethoxysilane (CAS No.: 919-30-2) and polyethyleneimine (CAS No.: 9002-98-6) were mixed in a mass ratio of 1:1 to obtain a grafted coupling agent, 2.5 g of the grafted coupling agent was mixed with 120 ml of deionized water to obtain a coupling agent mixed solution, the dopamine grafted aramid fiber was added to the coupling agent mixed solution, stirred at 50°C for 3 hours, then washed with deionized water, and dried in an oven at 50°C for 6 hours to obtain crack-resistant aramid fiber.
[0036] Preparation of early strength paving mortar: After mixing 130g of cement, 210g of sand and gravel with 100g of aggregate, add 35g of the above-prepared anti-cracking fiber and 50g of modified epoxy resin particles, stir for 35min, add 6g of water reducer and continue to stir for 1h to obtain early strength paving mortar; Among them, the water reducer is a naphthalene-based water reducer.
[0037] Example 4 Example 4 is based on Example 3. The only difference between Example 4 and Example 3 is that in Example 4, when preparing the modified nano rubber, the added amount of tannic acid is 0.85 g and the added amount of white carbon black is 14.15 g.
[0038] Example 5 Example 5 is based on Example 3. The only difference between Example 5 and Example 3 is that in Example 5, when preparing the modified nano rubber, the added amount of tannic acid is 1.84 g and the added amount of white carbon black is 13.16 g.
[0039] Example 6 Example 6 is based on Example 3. The only difference between Example 6 and Example 3 is that in Example 6, when preparing the modified epoxy resin, the modified nano rubber particles used are 61.54 g, the polyphenol oxide resin is 12.31 g, and the cage-type silsesquioxane is 6.15 g.
[0040] Example 7 Example 7 is based on Example 3. The only difference between Example 7 and Example 3 is that in Example 7, when preparing the modified epoxy resin, the modified nano rubber particles used are 34.78 g, the polyphenol oxide resin is 41.74 g, and the cage-type silsesquioxane is 3.48 g.
[0041] Example 9 Example 9 is based on Example 3. The only difference between Example 9 and Example 3 is that in Example 9, when preparing the modified nano rubber particles, no modification is performed by tannic acid.
[0042] Example 10 Example 10 is based on Example 3. The only difference between Example 10 and Example 3 is that when preparing the modified epoxy resin in Example 10, no cage-type silsesquioxane is added, 50g of nitrile nano-rubber particles are added, and 30g of polyphenol oxide resin is added.
[0043] Embodiment 11 Example 11 is based on Example 3. The only difference between Example 11 and Example 3 is that in Example 11, when preparing the coupling agent mixture, the graft coupling agent is replaced with an equal amount of γ-aminopropyltriethoxysilane.
[0044] Example 12 Example 12 is based on Example 3. The only difference between Example 12 and Example 3 is that in Example 12, when preparing the coupling agent mixture, the grafting coupling agent is replaced by an equal amount of polyethyleneimine.
[0045] Comparative Example 1 Comparative Example 1 is based on Example 3, and the difference between Comparative Example 1 and Example 3 is that in Comparative Example 1, the anti-cracking fiber is replaced by ordinary aramid fiber.
[0046] Comparative Example 2 Comparative Example 2 is based on Example 3. The difference between Comparative Example 2 and Example 3 is that in Comparative Example 2, when preparing the crack-resistant aramid fiber, dopamine is not used to treat the aramid fiber.
[0047] Comparative Example 3 Comparative Example 3 and Example 3 are used as a benchmark. The difference between Comparative Example 3 and Example 3 is that in Comparative Example 3, when preparing the crack-resistant aramid fiber, the graft coupling agent is not used to treat the aramid fiber.
[0048] Comparative Example 4 Comparative Example 4 is based on Example 3. The difference between Comparative Example 4 and Example 3 is that in Comparative Example 4, the modified epoxy resin particles are replaced with ordinary epoxy resin particles.
[0049] Performance testing The paving mortars prepared in Examples 1-12 and Comparative Examples 1-4 were sampled and subjected to the following performance tests: (1) Compressive strength performance test Based on the "JGJ / T70-2009 Standard for Test Methods for Basic Properties of Building Mortar", the compressive strength test was carried out on the samples. Each sample was tested three times, the average value was taken, and the test results were filled in Table 1.
[0050] (2) Temperature change performance test The prepared sample was cast to obtain a 50cm*20cm*20cm mortar block, and the mortar block was placed in a temperature change box. The temperature change range in the temperature change box was controlled at -10-40℃. The temperature cycle was carried out, and the temperature was maintained for 2h each time for 7d. The surface condition of the sample was recorded. Each sample was tested 3 times, the average value was taken, and the results were recorded in Table 1.
[0051] Table 1 Test results of compressive strength and temperature change performance of paving mortar Data analysis shows that after 3d compressive strength test, the compressive strength of Examples 1-3 is above 35MPa, indicating that the paving mortar prepared in the present application has good compressive strength performance; as shown in Table 1, after 7d temperature change test, the number of cracks on the surface of Examples 1-3 is less than 5, and the average crack length is less than 8mm, indicating that the paving mortar prepared in the present application has good temperature change resistance.
[0052] It can be seen from Table 1 that the compressive strength and temperature variation resistance of Example 4 and Example 5 are both reduced. This may be because when the content of tannic acid decreases, it is difficult to cross-link white carbon black and the modified nano-rubber particles. At the same time, the dispersion performance of white carbon black in the system is reduced, causing white carbon black to agglomerate, and the mechanical properties of the modified nano-rubber particles are reduced, affecting the stability of the mortar system. Therefore, the compressive strength is reduced. At the same time, when the tannic acid in the system decreases, the temperature variation resistance of the entire mortar system is also affected. When the content of tannic acid is too much, the stability of the system will also decrease. Therefore, the compressive strength and temperature variation resistance of Example 4 and Example 5 are both reduced.
[0053] The compressive strength and temperature variation resistance of Examples 6 and 7 are both reduced. This may be because when the content of phenoloxy resin is too much, the modification effect of cage-type silsesquioxane on the phenoloxy resin is reduced, thereby reducing the compatibility of the phenoloxy resin in the system, so the composition effect of the resin network is reduced, and the stability of the system is reduced. When the content of phenoloxy resin is too small, the content of cage-type silsesquioxane is too much, which increases the number of movable segments of the phenoloxy resin, and the network load of the phenoloxy resin reaches the limit and loses its effect. The stability of the system is reduced. Therefore, the compressive strength of Examples 6 and 7 is reduced, and the temperature variation resistance is also reduced.
[0054] The compressive strength and temperature variation resistance of Example 8 and Example 9 are both decreased. This may be because when the dopamine content is reduced, the surface modification effect on the aramid fiber is reduced, the interaction effect between dopamine and polyethyleneimine is also reduced, the roughness of the fiber surface is reduced, and the stability in the system is reduced, which reduces the improvement of the mechanical properties of the aramid fiber. When the dopamine content is too much, too much dopamine will be accumulated on the surface of the aramid fiber, making the coating on the surface of the aramid fiber too thick and falling off, reducing the stability of the aramid fiber. Therefore, the compressive strength and temperature variation resistance of Example 10 and Example 11 are both reduced.
[0055] In Comparative Example 1, the crack-resistant aramid fiber is replaced with ordinary aramid fiber. The compressive performance and temperature variation resistance of Comparative Example 1 are both reduced. This is because the aramid fiber is not modified by dopamine and graft coupling agent, and the roughness of the aramid fiber surface is reduced, which makes the stability of the aramid fiber in the mortar system reduced, and at the same time reduces the mechanical strength of the aramid fiber itself. Therefore, the compressive strength of Comparative Example 1 is reduced, and the temperature variation resistance of the unmodified aramid fiber is also reduced.
[0056] In Comparative Example 2, when preparing the crack-resistant aramid fiber, the graft coupling agent was not used to treat the aramid fiber. It was difficult to form a carbon layer on the surface of the aramid fiber, the degradation of the aramid fiber was accelerated, and the heat resistance was reduced. Therefore, the stability of the aramid fiber was greatly reduced, and the compressive strength and temperature change resistance were reduced.
[0057] In Comparative Example 3, when preparing crack-resistant aramid fibers, dopamine was not used to modify the aramid fibers, which made it difficult for the surface of the aramid fibers to become rough, the specific surface area was reduced, the surface polarity was difficult to increase, the interface properties of the aramid fibers were difficult to improve, and the stability in the mortar system was reduced, so the compressive strength and temperature change resistance were reduced.
[0058] In Comparative Example 4, the modified epoxy resin particles are replaced with ordinary epoxy resin particles. The unmodified epoxy resin particles are brittle and the impact resistance is difficult to improve. Therefore, the compressive strength in Comparative Example 4 is difficult to improve, and the temperature change resistance is also reduced.
[0059] This specific embodiment is only an explanation of the present application, and it is not a limitation of the present application. Through the above description, relevant staff can make various changes and modifications without deviating from the technical idea of the present application. The technical scope of the present application is not limited to the content in the specification, and its technical scope must be determined according to the scope of the claims.
Claims
1. An early-strength paving mortar, characterized in that: The composition includes the following components by mass: Aggregate 800-1000 parts; 30-40 parts of anti-crack fiber Modified epoxy resin 40-60 parts 150-210 parts of sand and gravel 100-150 parts of cement 3-9 parts of water reducing agent.
2. The early-strength paving mortar according to claim 1, characterized in that: The anti-cracking fiber comprises aramid fiber, dopamine and a graft coupling agent.
3. The early-strength paving mortar according to claim 1, characterized in that: The anti-cracking fiber is prepared by the following method: The aramid fiber is washed and dried for later use, a dopamine solution is prepared using hydrochloric acid, dopamine and deionized water, the dried aramid fiber is immersed in the prepared dopamine solution, stirred for 4-6 hours to obtain dopamine-modified aramid fiber, polyethyleneimine is added at a temperature of 30-34°C, stirred for 9-11 hours, the fiber is washed, and dried to obtain crack-resistant modified fiber.
4. The early-strength paving mortar according to claim 3, characterized in that: The concentration of dopamine in the dopamine solution is 10-13 g / 100 mL.
5. The early-strength paving mortar according to claim 4, characterized in that: The graft coupling agent includes gamma-aminopropyltriethoxysilane and polyethyleneimine.
6. The early-strength paving mortar according to claim 1, characterized in that: The modified epoxy resin comprises nano-modified rubber particles, epoxy resin and cage-type silsesquioxane.
7. The early-strength paving mortar according to claim 6, characterized in that: The mass ratio of the nano-modified rubber particles, the epoxy resin and the cage-type silsesquioxane is 10:(4-8):
1.
8. The early-strength paving mortar according to claim 6, characterized in that: The nano-modified rubber particles include natural rubber, white carbon black and tannic acid.
9. The early-strength paving mortar according to claim 8, characterized in that: The nano-modified rubber particles are prepared by the following method: Mixing tannic acid and white carbon black, and feeding into an ethanol solution, stirring, washing and centrifuging to obtain white powder, and drying the white powder to obtain modified white carbon black; The natural rubber and the rubber are mixed and kneaded to obtain modified rubber, and the modified rubber is ground to obtain nano-modified rubber particles.
10. A method for preparing the early-strength paving mortar according to claim 1, characterized in that: The steps include: After mixing cement, sand and aggregate, add anti-cracking fiber and modified epoxy resin, stir for 30-40 minutes, add water reducer, and continue stirring to obtain early-strength paving mortar.