Process for preparing epichlorohydrin through direct oxidation of chloropropene

By using nonionic surfactants and polyols in the epoxy chlorohydrin production process, the homogeneous mixing of chloropropylene and hydrogen peroxide is solved by using titanium silicon molecular sieve TS-1 catalyst, the low production efficiency and energy caused by solvent use are solved. The problem of high consumption has achieved efficient and environmentally friendly preparation of epoxypropane.

CN119059991AActive Publication Date: 2024-12-03DALIAN INSTITUTE OF CHEMICAL PHYSICS CHINESE ACADEMY OF SCIENCES
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202310643742.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-06-01
Publication Date
2024-12-03
Estimated Expiration
2043-06-01

Smart Images

  • Figure BDA0004262896110000061
    Figure BDA0004262896110000061
Patent Text Reader

Abstract

The invention discloses a process for preparing epichlorohydrin by direct oxidation of chloropropene, which at least comprises the following steps: introducing a homogeneous mixture containing chloropropene, hydrogen peroxide, polyol and a nonionic surfactant into a fixed bed reactor for reaction to obtain a product containing epichlorohydrin. Compared with a traditional method, the method has the advantages that few reaction byproducts are produced, a product after hydrogen peroxide reaction is water, the nonionic surfactant and the polyhydric alcohol are added, an organic phase and a water phase are promoted to be mixed into a homogeneous phase, the selectivity is improved, a large amount of solvent does not need to be added, the processes of solvent evaporation and recovery and the like are avoided, the process is energy-saving and environment-friendly, and the equipment process is simple; the method is high in yield and selectivity, suitable for industrial large-scale production, high in economic benefit, free of solvent evaporation and recovery, beneficial to industrial production amplification, low in equipment maintenance cost, low in system cost, small in environmental pollution, simple to operate, easy to repeat and capable of efficiently producing epoxy chloropropane.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to a process for preparing epichlorohydrin by direct oxidation of allyl chloride, which uses hydrogen peroxide as an oxygen source and titanium silicon molecular sieve TS-1 as a catalyst to catalyze the direct oxidation of allyl chloride to prepare epichlorohydrin, and belongs to the field of preparation and synthesis of epichlorohydrin. Background Art

[0002] Epichlorohydrin (ECH) is an important organic chemical raw material and an important intermediate in petrochemical industry. It is mainly used to produce epoxy resin, glycerin, epichlorohydrin rubber and other derivatives. It can also be used as a solvent, plasticizer, flame retardant and surfactant. The production process of epichlorohydrin (ECH) is mainly based on the propylene method. The glycerin method is second, but all the above methods have certain problems. The glycerin method production process has the advantages of mild reaction conditions, high selectivity and yield, and greatly reduced three wastes compared with the propylene method. However, with the continuous release of new production capacity of epichlorohydrin by glycerin method in China, the demand for glycerin has increased, resulting in a sharp increase in the cost of the glycerin method. The epichlorohydrin by glycerin method is in a high-cost and low-profit state, and even in a loss-making state in some stages. At the same time, with the increasing requirements for environmental protection and safety, the new environmentally friendly process of synthesizing epichlorohydrin by hydrogen peroxide method has received more and more attention.

[0003] The new process of preparing epichlorohydrin by direct oxidation with hydrogen peroxide is an emerging process and the most environmentally friendly production process for epichlorohydrin so far. The new green process will surely lead the future development of epichlorohydrin. However, in the current process, more solvents are usually used to dissolve the reaction raw material allyl chloride and the oxidant hydrogen peroxide to form a homogeneous phase. If the solvent is less, the two phases cannot be fully dissolved, which is not conducive to the mass transfer and heat transfer process, increases the occurrence of side reactions, and reduces the yield and selectivity of epichlorohydrin. However, the use of solvents, on the one hand, increases the cost of production, and on the other hand, requires a lot of energy to evaporate and recycle the solvent, which restricts the industrialization process of the process in many aspects. Summary of the invention

[0004] According to one aspect of the present application, a method for preparing epichlorohydrin is provided, the method comprising adding a nonionic surfactant and a polyol to a reaction system, making allyl chloride and hydrogen peroxide two phases form a homogeneous phase, and pumping it into a fixed bed reactor equipped with titanium silicon molecular sieve TS-1 by a metering pump to obtain the epichlorohydrin. The method promotes the mixing of the organic phase and the aqueous phase by adding a nonionic surfactant, does not require a large amount of solvent added in the traditional process, avoids a large amount of energy-consuming processes such as solvent evaporation and recovery, and has energy-saving and environmentally friendly processes, simple equipment and process, high yield and selectivity of epichlorohydrin, and is suitable for large-scale industrial production of epichlorohydrin. The solvent-free synthesis system used in the method has greater economic benefits, lower system cost, less environmental pollution, simple operation, easy to repeat, low equipment maintenance cost, and can efficiently produce epichlorohydrin.

[0005] At least the following steps are included:

[0006] Passing a homogeneous mixture containing allyl chloride, hydrogen peroxide, polyol and nonionic surfactant into a fixed bed reactor for reaction to obtain a product containing epichlorohydrin;

[0007] The fixed bed reactor is filled with a catalyst containing titanium silicon molecular sieve TS-1;

[0008] Nonionic surfactants and polyols are added to the reaction system to make the oil-water phases of allyl chloride and hydrogen peroxide form a homogeneous phase, which is then pumped into a fixed bed reactor filled with titanium silicalite TS-1 through a metering pump.

[0009] The polyol is selected from at least one of ethylene glycol, diethylene glycol, triethylene glycol, tetraethylene glycol, 1,2-propylene glycol, 1,3-propylene glycol, 1,4-butylene glycol, 1,6-hexanediol, polyethylene glycol 200, polyethylene glycol 400, polyethylene glycol 600, polyethylene glycol 800, 1,4-cyclohexanediol, 1,4-cyclohexanedimethanol, terephthalate, glycerol, trimethylolpropane, pentaerythritol, xylitol or sorbitol;

[0010] The nonionic surfactant is selected from at least one of alkyl glucoside (APG), fatty acid glyceride, fatty acid sorbitan (Span), polysorbate (Tween), polyoxyethylene fatty alcohol ether (Brij) and nonylphenol polyoxyethylene ether (NP);

[0011] The reaction temperature is 20 to 90°C;

[0012] Optionally, the reaction temperature is independently selected from any value of 20°C, 25°C, 30°C, 35°C, 40°C, 45°C, 50°C, 55°C, 60°C, 65°C, 70°C, 75°C, 80°C, 85°C, 90°C or any value therebetween.

[0013] The feed mass space velocity of the reaction is 0.5 to 10 h -1 .

[0014] Optionally, the feed mass space velocity of the reaction is independently selected from 0.5h -1 , 1h -1 , 1.5h -1 , 2h -1 , 2.5h -1 , 3h -1 , 3.5h -1 , 4h -1 , 4.5h -1 , 5h -1 , 5.5h -1 , 6h -1 , 6.5h -1 , 7h -1 , 7.5h -1 , 8h -1 , 8.5h -1 , 9h -1 , 9.5h -1 or 10h -1 Any value in between or any value in between.

[0015] The molar ratio of the propylene chloride to the polyol is 5 to 10:1.

[0016] Optionally, the molar ratio of allyl chloride to polyol is independently selected from any of 5:1, 6:1, 7:1, 8:1, 9:1 or 10:1 or any value therebetween.

[0017] Optionally, the molar ratio of allyl chloride to polyol is 6 to 10:1;

[0018] Optionally, the molar ratio of allyl chloride to polyol is 8 to 10:1.

[0019] The molar ratio of allyl chloride to hydrogen peroxide is 1-10:1.

[0020] Optionally, the molar ratio of allyl chloride to hydrogen peroxide is independently selected from any value of 1:1, 2:1, 3:1, 4:1, 5:1, 6:1, 7:1, 8:1, 9:1 or 10:1 or any value therebetween.

[0021] Optionally, the molar ratio of allyl chloride to hydrogen peroxide is 3 to 10:1;

[0022] Optionally, the molar ratio of allyl chloride to hydrogen peroxide is 5 to 10:1.

[0023] The molar ratio of the hydrogen peroxide to the non-ionic surfactant is 1 to 50:1.

[0024] Optionally, the molar ratio of hydrogen peroxide to the nonionic surfactant is independently selected from any value of 1:1, 2:1, 3:1, 5:1, 10:1, 15:1, 20:1, 30:1, 40:1 or 50:1 or any value therebetween.

[0025] Optionally, the molar ratio of the hydrogen peroxide to the non-ionic surfactant is 10 to 50:1;

[0026] Optionally, the molar ratio of the hydrogen peroxide to the non-ionic surfactant is 30 to 50:1.

[0027] The mass concentration of the hydrogen peroxide is 10-70%.

[0028] Optionally, the mass concentration of the hydrogen peroxide is independently selected from any value of 10%, 15%, 20%, 25%, 30%, 35%, 40%, 45%, 50%, 55%, 60%, 65%, 70% or any value therebetween.

[0029] The titanium silicate molecular sieve TS-1 is a titanium-doped silicon-based zeolite molecular sieve.

[0030] The titanium silicate molecular sieve TS-1 has an MFI type topological structure.

[0031] The alkyl glucoside (APG) is selected from at least one of APG0810, APG0810-1214, APG0814, C12-18 alkyl glucoside, C20 alkyl glucoside and lauryl alkyl glucoside;

[0032] The fatty acid glyceride is selected from at least one of glyceryl trioleate (olein), glyceryl tripalmitate (palmitin) and glyceryl tristearate (stearin);

[0033] The fatty acid sorbitan (Span) is at least one selected from Span 20 (sorbitan laurate), Span 40 (sorbitan palmitate), Span 60 (sorbitan stearate), Span 65 (sorbitan tristearate), Span 80 (sorbitan oleate) and Span 85 (sorbitan trioleate);

[0034] The polysorbate (Tween) is selected from at least one of Tween 20 (polysorbate 20), Tween 40 (polysorbate 40), Tween 60 (polysorbate 60), Tween 65 (polysorbate 65), Tween 80 (polysorbate 80) and Tween 85 (polysorbate 85);

[0035] The polyoxyethylene fatty alcohol ether (Brij) is selected from at least one of Brij15, Brij20, Brij30 or Brij35;

[0036] The nonylphenol polyoxyethylene ether (NP) is selected from at least one of NP-5, NP-7, NP-9 and NP-10.

[0037] The beneficial effects of this application include:

[0038] (1) The present application provides a method for preparing epichlorohydrin. Compared with the traditional method, the preparation process of the present invention uses titanium silicon molecular sieve TS-1 as a catalyst and hydrogen peroxide as an oxygen source. In a fixed bed reactor, allyl chloride is directly oxidized to epichlorohydrin. There are fewer reaction by-products. The product after the hydrogen peroxide reaction is water, which has little pollution to the environment and is green and environmentally friendly.

[0039] (2) The preparation method of epichlorohydrin provided in the present application promotes the mixing of the organic phase and the aqueous phase into a homogeneous phase by adding a non-ionic surfactant and a polyol, thereby improving the selectivity of the reaction. It does not require the large amount of solvent added in the traditional process. The reaction liquid after the reaction is clear and transparent, avoiding a large amount of energy-consuming processes such as solvent evaporation and recovery.

[0040] (3) The preparation method of epichlorohydrin provided in the present application is energy-saving and environmentally friendly, has simple equipment and process, high yield and selectivity of epichlorohydrin, and is suitable for large-scale industrial production.

[0041] (4) The preparation method of epichlorohydrin provided in the present application does not require the traditional energy-intensive solvent evaporation and recovery process, is conducive to industrial production scale-up, has low equipment maintenance cost, low system cost, low environmental pollution, simple operation, easy to repeat, and can efficiently produce epichlorohydrin. DETAILED DESCRIPTION

[0042] The present application is described in detail below with reference to embodiments, but the present application is not limited to these embodiments.

[0043] Unless otherwise specified, the raw materials in the examples of this application were purchased through commercial channels.

[0044] The analysis method in the examples of this application is as follows:

[0045] The selectivity of epoxy chloropropylene and the utilization rate of hydrogen peroxide during the reaction were detected using a gas chromatograph model 7890A produced by Agilent Technologies.

[0046] The epichlorohydrin selectivity and hydrogen peroxide utilization rate are detected by gas chromatography.

[0047] The detection of the hydrogen peroxide conversion rate adopts the cerium sulfate titration method, using o-phenanthroline ferrous iron as an indicator, and the titration end point is that the light red solution changes to a transparent light blue.

[0048] Example 1

[0049] Use a metering pump at an air velocity of 3.0h -1 A mixed solution of allyl chloride, 30% mass concentration of hydrogen peroxide, NP-10 and polyethylene glycol 200 was pumped into a fixed bed reactor equipped with titanium silicalite TS-1 catalyst at a molar ratio of allyl chloride: hydrogen peroxide: non-ionic surfactant of 50:5:1:6, and the temperature was raised to 45°C. After the reaction, a small amount of reaction liquid was taken for gas chromatography analysis and cerium sulfate titration of hydrogen peroxide. The results showed that the conversion rate of hydrogen peroxide was 98.2%, the utilization rate of hydrogen peroxide was 97%, and the selectivity of epichlorohydrin was 98.6%.

[0050] Example 2

[0051] Use a metering pump at an air velocity of 3.0h -1 A mixed solution of allyl chloride, 30% mass concentration of hydrogen peroxide, Tween 20, and ethylene glycol was pumped into a fixed bed reactor equipped with titanium silicon molecular sieve TS-1 catalyst according to the molar ratio of allyl chloride: hydrogen peroxide: non-ionic surfactant of 100:10:1:23, and the temperature was raised to 70° C. After the reaction, a small amount of the reaction liquid was taken for gas chromatography analysis and cerium sulfate titration of hydrogen peroxide. The results showed that the conversion rate of hydrogen peroxide was 98.5%, the utilization rate of hydrogen peroxide was 98%, and the selectivity of epichlorohydrin was 99.2%.

[0052] Embodiments 3 to 11

[0053] The specific ingredient types, materials and reaction conditions are shown in Table 1 below. Other operations during the synthesis process are the same as in Example 1.

[0054] Table 1 Raw material composition, ratio, reaction conditions and reaction results of Examples 3 to 11

[0055]

[0056] The test results of epichlorohydrin in other examples were similar to those described above, and products containing epichlorohydrin were obtained.

[0057] Example 12

[0058] Use a metering pump at an air velocity of 3.0h -1 A mixed solution of allyl chloride, 30% mass concentration of hydrogen peroxide, NP-7, and polyethylene glycol 200 was pumped into a fixed bed reactor equipped with titanium silicon molecular sieve TS-1 catalyst at a molar ratio of allyl chloride: hydrogen peroxide: non-ionic surfactant: polyol of 50:5:1:5, and the temperature was raised to 50° C. After the reaction, a small amount of the reaction liquid was taken for gas chromatography analysis and cerium sulfate titration of hydrogen peroxide. The results showed that the conversion rate of hydrogen peroxide was 98.3%, the utilization rate of hydrogen peroxide was 97%, and the selectivity of epichlorohydrin was 97.5%.

[0059] Comparative Example 1

[0060] The same reaction conditions as in Example 12 were used, but no surfactant was added. The specific operation was as follows: a metering pump was used at a space velocity of 3.0 h -1 A mixed solution of allyl chloride and 30% mass concentration of hydrogen peroxide was pumped into a fixed bed reactor equipped with titanium silicon molecular sieve TS-1 catalyst at a molar ratio of allyl chloride: hydrogen peroxide of 50:5, and the temperature was raised to 50°C. After the addition, it was water-oil two-phase, and after stirring, it was a turbid liquid. The temperature was raised to 50°C, and the reaction time was 1 hour. After the reaction was completed, a small amount of the reaction liquid was taken for gas chromatography analysis and cerium sulfate titration of hydrogen peroxide. The results showed that the conversion rate of hydrogen peroxide was 77.2%, the utilization rate of hydrogen peroxide was 65%, and the selectivity of epichlorohydrin was 91.8%.

[0061] Example 13

[0062] Use a metering pump at an air velocity of 10.0h -1 A mixed solution of allyl chloride, 50% mass concentration of hydrogen peroxide, Brij35, and ethylene glycol was pumped into a fixed bed reactor equipped with titanium silicon molecular sieve TS-1 catalyst according to a molar ratio of allyl chloride: hydrogen peroxide: non-ionic surfactant: polyol of 10:3:1:1, and the temperature was raised to 60°C. The reaction time was 3 hours. After the reaction was completed, a small amount of the reaction liquid was taken for gas chromatography analysis and cerium sulfate titration of hydrogen peroxide. The results showed that the conversion rate of hydrogen peroxide was 97.8%, the utilization rate of hydrogen peroxide was 98%, and the selectivity of epichlorohydrin was 97.3%.

[0063] Comparative Example 2

[0064] The same reaction conditions as in Example 13 were used, but no nonionic surfactant and polyol were added to the reaction. Methanol was added to the organic phase. The specific operation was as follows: a metering pump was used at a space velocity of 10.0 h -1 A mixed solution of allyl chloride, 50% mass concentration of hydrogen peroxide and methanol was pumped into a fixed bed reactor equipped with titanium silicon molecular sieve TS-1 catalyst at a molar ratio of allyl chloride: hydrogen peroxide: methanol of 10:3:50, and the temperature was raised to 60°C. The reaction time was 3 hours. After the reaction was completed, a small amount of the reaction liquid was taken for gas chromatography analysis and cerium sulfate titration of hydrogen peroxide. The results showed that the conversion rate of hydrogen peroxide was 89.1%, the utilization rate of hydrogen peroxide was 93%, and the selectivity of epichlorohydrin was 93.7%.

[0065] The above are only a few embodiments of the present application and do not constitute any form of limitation to the present application. Although the present application is disclosed as above with preferred embodiments, it is not intended to limit the present application. Any technician familiar with the profession, without departing from the scope of the technical solution of the present application, using the technical content disclosed above to make slight changes or modifications are equivalent to equivalent implementation cases and fall within the scope of the technical solution.

Claims

1. A process for preparing epichlorohydrin by direct oxidation of allyl chloride, characterized in that: At least the following steps are included: Passing a homogeneous mixture containing allyl chloride, hydrogen peroxide, polyol and nonionic surfactant into a fixed bed reactor for reaction to obtain a product containing epichlorohydrin; The fixed bed reactor is filled with a catalyst containing titanium silicon molecular sieve TS-1; The polyol is selected from at least one of ethylene glycol, diethylene glycol, triethylene glycol, tetraethylene glycol, 1,2-propylene glycol, 1,3-propylene glycol, 1,4-butylene glycol, 1,6-hexanediol, polyethylene glycol 200, polyethylene glycol 400, polyethylene glycol 600, polyethylene glycol 800, 1,4-cyclohexanediol, 1,4-cyclohexanedimethanol, terephthalate, glycerol, trimethylolpropane, pentaerythritol, xylitol or sorbitol; The nonionic surfactant is selected from at least one of alkyl glucoside, fatty acid glyceride, fatty acid sorbitan, polysorbate, polyoxyethylene fatty alcohol ether or nonylphenol polyoxyethylene ether.

2. The method according to claim 1, characterized in that The reaction temperature is 20-90°C.

3. The method according to claim 1, characterized in that The feed mass space velocity of the reaction is 0.5 to 10 h -1 .

4. The method according to claim 1, characterized in that: The molar ratio of allyl chloride to polyol is 5 to 10:1; The molar ratio of allyl chloride to hydrogen peroxide is 1 to 10:1; The molar ratio of the hydrogen peroxide to the non-ionic surfactant is 1 to 50:

1.

5. The method according to claim 1, characterized in that The molar ratio of allyl chloride to polyol is 6 to 10:1; The molar ratio of allyl chloride to hydrogen peroxide is 3 to 10:1; The molar ratio of the hydrogen peroxide to the non-ionic surfactant is 10-50:

1.

6. The method according to claim 1, characterized in that The molar ratio of allyl chloride to polyol is 8 to 10:1; The molar ratio of allyl chloride to hydrogen peroxide is 5 to 10:1; The molar ratio of the hydrogen peroxide to the non-ionic surfactant is 30-50:

1.

7. The method according to claim 1, characterized in that The mass concentration of the hydrogen peroxide is 10-70%.

8. The method according to claim 1, characterized in that The alkyl glucoside is selected from at least one of APG0810, APG0810-1214, APG0814, C12-18 alkyl glucoside, C20 alkyl glucoside or lauryl alkyl glucoside; The fatty acid glyceride is selected from at least one of glyceryl trioleate, glyceryl tripalmitate or glyceryl tristearate; The fatty acid sorbitan is selected from at least one of Span 20, Span 40, Span 60, Span 65, Span 80 and Span 85; The polysorbate is selected from at least one of Tween 20, Tween 40, Tween 60, Tween 65, Tween 80 or Tween 85; The polyoxyethylene fatty alcohol ether is selected from at least one of Brij15, Brij20, Brij30 or Brij35; The nonylphenol polyoxyethylene ether is selected from at least one of NP-5, NP-7, NP-9 and NP-10.

Citation Information

Patent Citations

  • Method for preparing epoxy chloropropane

    CN102464632A

  • Method for preparing epoxy chloropropane

    CN111574481A

  • Epichlorohydrin producing method

    RU2628801C1

  • Process for the manufacture of epichlorohydrin

    US20140256968A1