Naphthylamine ionic liquid as well as preparation method and application thereof
Naphthylamine ionic liquid is prepared through the structural design of ionic liquid and acid-base neutralization reaction, which solves the problem of insufficient tribological properties and anti-oxidation properties of ester oil at high temperatures, and realizes high-temperature anti-wear and anti-oxidation of ester oils Improved performance, suitable for high-performance lubricating additives.
Patent Information
- Application Number
- CN202411250361.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-06
- Publication Date
- 2024-12-03
AI Technical Summary
Traditional mineral-based lubricating oil cannot meet the tribological properties and oxidation resistance requirements of mechanical parts under high temperature, extreme pressure and extremely high speed conditions. Ester oils lack tribological properties and load-bearing capacity at high temperatures, and are easy to be lubricated with other lubricants. Competing adsorption of additives makes it difficult to meet the harsh conditions of industrial applications.
Using the structural design of ionic liquid, naphthylamine-based ionic liquid is prepared through acid-base neutralization reaction. As an additive for ester oil, octylated phenyl-α-naphthylamine and di-(2) are synthesized at room temperature by ion bond modification method. The composition of -ethylhexyl)phosphate or didecyl dithiophosphate forms a novel structured naphthamine ionic liquid for improving the tribological and antioxidant properties of ester oils.
It significantly reduces the wear of steel balls, improves the tribological properties and oxidation resistance of ester oils, enhances its application performance under high temperature conditions, shows excellent anti-wear and oxidation resistance, and is suitable for high-performance lubricating additives .
Smart Images

Figure FT_1 
Figure FT_2 
Figure FT_3
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of lubricating additives and relates to an ionic liquid, in particular to a naphthylamine ionic liquid and a preparation method thereof. The ionic liquid is mainly used as an additive for ester oils. Background Art
[0002] With the accelerated development of modern industry, many mechanical parts need to work under harsh conditions such as high temperature, extreme pressure, and high speed, and mechanical equipment will experience severe wear during operation. In order to reduce the friction and wear of mechanical parts and ensure their safety, the base oil and lubricant additives used in mechanical parts must have excellent tribological properties under harsh working conditions. Traditional mineral-based lubricants can no longer meet the requirements in terms of high and low temperature performance, lubrication performance, biodegradability, and low evaporation loss. In addition, under high temperature and heavy load conditions, the load is almost entirely borne by the lubricating film or friction film generated by the interaction between the lubricant / additive and the friction surface, which puts higher requirements on the service performance of lubricating materials under harsh conditions.
[0003] Pentaerythritol ester oil (PE) has excellent thermal stability and lubrication performance, and is widely used in lubrication fields such as engine oil, compressor oil and aviation oil. However, the tribological properties and load-bearing capacity of ester oil at high temperature are not outstanding, the polarity is high, and it is easy to compete with other lubricating additives for adsorption. Moreover, under high temperature conditions, pure ester oil cannot better meet the requirements of tribological properties and antioxidant properties. Lubricating additives are used to give special properties to base oils, which can improve the overall performance of lubricating oils to withstand various harsh working conditions. Ionic liquids refer to ionic compounds composed of organic cations and organic / inorganic anions that are liquid near room temperature. Its chemical stability and high thermal stability meet the requirements of lubricating additives. At the same time, ionic liquids have unique properties and functions such as extremely low saturated vapor pressure, high thermal stability, strong structural designability, and strong solubility. Based on the designability of its structure, functional functional groups can be introduced into the anion and cation structures, thereby designing and synthesizing ionic liquids with special functions, which are suitable for different service conditions.
[0004] The present invention draws on the unique organic molecular anion and cation structure of ionic liquids, adopts an ionic bond modification method, and prepares two naphthylamine ionic liquids through a simple acid-base neutralization reaction at room temperature. The ionic liquid not only eliminates the transient high friction of ester oils during the friction process, but also effectively reduces the wear of steel balls. It can also significantly improve the oxidation stability of ester oils and promote the application of ester oils under high temperature conditions. Summary of the invention
[0005] The present invention aims to provide a naphthylamine ionic liquid and a preparation method thereof, which are mainly used as additives for ester oils. The present invention starts with the structural design of the ionic liquid and prepares an ionic liquid with a novel structure and good high-temperature performance, which not only improves the tribological properties of the ester oil, but also significantly improves the antioxidant capacity of the ester oil, and is expected to be widely used as an ester oil additive in the lubrication engineering and industrial fields.
[0006] 1. Naphthylamine ionic liquids and their preparation The preparation method of the naphthylamine ionic liquid of the present invention comprises dissolving octylated phenyl-α-naphthylamine (OPANA) in an ethanol solvent, and then slowly dropping di(2-ethylhexyl) phosphate (DEHP) or didecyl dithiophosphate (C 10 -DDP), stirred at 60-70°C for 12-15h, rotary evaporated to remove the ethanol solvent, and vacuum dried to obtain the naphthylamine ionic liquid [OPANA][DEHP] or [OPANA][C 10 -DDP]. The molar ratio of octylated phenyl-α-naphthylamine to di(2-ethylhexyl)phosphate or didecyl dithiophosphate is 1:1.
[0007] The prepared naphthylamine ionic liquid has the following structural formula: In the formula, R 1 =iC 8 H 17 , R 2 =iC 8 H 17 , R 3 =nC 10 H 21 .
[0008] The naphthylamine ionic liquid of the present invention can be used as an additive for ester oil. The naphthylamine ionic liquid of the present invention exhibits excellent anti-wear performance as an ester oil lubricating additive, and can be used as a high-performance lubricating anti-wear additive in the field of lubrication engineering. The naphthylamine ionic liquid of the present invention exhibits more excellent antioxidant performance as an ester oil lubricating additive, and can be used as a high-performance antioxidant in the field of lubrication engineering.
[0009] Beneficial effects of the present invention: 1. The naphthylamine ionic liquid of the present invention has a novel structure, a simple preparation method and excellent thermal stability; 2. The naphthylamine ionic liquid in the present invention is used as a lubricating additive for ester oil, which not only eliminates transient high friction during the friction process, but also effectively reduces the wear of ester oil at high temperature. As an additive, it has excellent anti-wear ability in ester oil; 3. The naphthylamine ionic liquid in the present invention not only has excellent thermal stability, but also can significantly enhance the antioxidant capacity of ester oil as an additive, thereby promoting the application of ester oil under high temperature conditions. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] Figure 1 For [OPANA][DEHP] and [OPANA][C 10 -DDP] NMR spectrum.
[0011] Figure 2 Friction curves of different lubricants.
[0012] Figure 3 is the wear spot diameter of different lubricants.
[0013] Figure 4 is the initial oxidation temperature of different lubricants. DETAILED DESCRIPTION
[0014] The present invention is further explained below with reference to specific embodiments.
[0015] Example 1 First, 6.62 g of octylated phenyl-α-naphthylamine (OPANA) was placed in a round-bottom flask containing 100 ml of ethanol solvent. After OPANA was dissolved, an equal molar amount of DEHP (6.45 g) was slowly added to the round-bottom flask, stirred at 60°C for 15 h, and the ethanol solvent was removed by rotary evaporation. [OPANA][DEHP] was obtained by vacuum drying at 70°C for 24 h. The NMR spectrum of [OPANA][DEHP] is shown in Figure 1 .
[0016] [OPANA][DEHP]: 1 H NMR (chloroform-d, 600 MHz)δ 0.63-0.98 (m, 21 H,CH 3 ), 1.05-1.47 (m, 22 H, CH 2 ), 1.50-1.87 (m, 4 H, CH 2 ), 3.70-4.00 (m, 4 H,CH 2 ),7.00-7.10(s, 2 H, CH),7.25-7.29(s, 3 H, CH),7.31-7.39(s, 2 H, CH),7.42-7.63(s, 4 H, CH),7.81-7.89(s, 1 H, CH),7.89-8.01(s, 1 H, CH).
[0017] Preparation of pentaerythritol ester oil: Pentaerythritol (648 g), n-octanoic acid (144 g), 2-ethylhexanoic acid (1009 g), heptanoic acid (1562 g) and solid acid catalyst (34 g) were added to a three-necked flask for esterification reaction; a thermometer and a glass stopper were inserted on both sides of the three-bubble flask, and the middle was connected to the water separator and condenser tube in turn. Petroleum ether was added to the water separator as a water carrier to promote the separation of water in the reaction. The esterification reaction was carried out at 220°C and 450 r / min for 12 h. The acid value of the reaction system was tested to obtain an ester oil with an esterification rate of 95.80%. The remaining fatty acids in the reaction system were removed by vacuum distillation to obtain pentaerythritol ester oil, which was recorded as PE.
[0018] Pentaerythritol (purity ≥ 98%) was purchased from Yunnan Yuntianhua Co., Ltd.; solid acid catalyst (HND-260) was purchased from Jiangyin Nanda Synthetic Chemical Co., Ltd.; fatty acids including 2-ethylhexanoic acid (purity ≥ 98%), octanoic acid (purity ≥ 98%), and heptanoic acid (purity ≥ 98%) were purchased from Shanghai McLean Biochemical Co., Ltd.
[0019] 0.5 g of [OPANA][DEHP] was added to 49.5 g of PE and after dissolution, an ester oil containing 1.0% by mass of naphthylamine ionic liquid was obtained, which was recorded as PE+1.0% [OPANA][DEHP].
[0020] Example 2 First, 6.62 g of octylated phenyl-α-naphthylamine (OPANA) was placed in a round-bottom flask containing 100 ml of ethanol solvent. After OPANA was dissolved, an equal molar amount of DEHP (6.45 g) was slowly added dropwise into the round-bottom flask. The mixture was stirred at 70°C for 12 h, and the ethanol solvent was removed by rotary evaporation. The ionic liquid was dried in vacuum at 70°C for 24 h to obtain [OPANA][DEHP].
[0021] Example 3 The preparation process of [OPANA][DEHP] and PE is the same as that in Example 1.
[0022] 1.0 g of [OPANA][DEHP] was added to 49.0 g of PE and after dissolution, an ester oil containing 2.0% by mass of naphthylamine ionic liquid was obtained, which was recorded as PE+2.0% [OPANA][DEHP].
[0023] Example 4 The preparation process of [OPANA][DEHP] and PE is the same as that in Example 1.
[0024] 1.5 g of [OPANA][DEHP] was added to 48.5 g of PE and dissolved to obtain an ester oil containing 3.0% by mass of naphthylamine ionic liquid, recorded as PE+3.0% [OPANA][DEHP].
[0025] Example 5 Place 6.62 g of octylated phenyl-α-naphthylamine (OPANA) in a round-bottom flask containing 100 ml of ethanol solvent. After OPANA is dissolved, slowly drop an equal mole of C 10 -DDP (8.20 g) was stirred at 60 °C for 15 h, the ethanol solvent was removed by rotary evaporation, and vacuum dried at 70 °C for 24 h to obtain [OPANA][C 10 -DDP]. [OPANA][C 10 -DDP] NMR spectrum is as follows Figure 1 .
[0026] [OPANA][C 10 -DDP]: 1 H NMR (chloroform-d, 600 MHz) δ 0.63-0.98 (m, 15 H,CH 3 ), 1.10-1.50 (m, 34 H, CH 2 ), 1.55-1.90 (m, 6 H, CH 2 ), 4.00-4.35 (m, 4 H,CH 2 ),7.00-7.10(s, 2 H, CH),7.25-7.30(s, 4 H, CH),7.33-7.40(s, 2 H, CH),7.40-7.60(s, 3 H, CH),7.80-7.89(s,1 H, CH),7.89-8.01(s, 1 H, CH) The preparation process of PE is consistent with that in Example 1.
[0027] Take 0.5 g [OPANA][C 10 -DDP] was added to 49.5 g PE and dissolved to obtain an ester oil containing 1.0% by mass of naphthylamine ionic liquid, recorded as PE+1.0% [OPANA][C 10 -DDP].
[0028] Example 6 Place 6.62 g of octylated phenyl-α-naphthylamine (OPANA) in a round-bottom flask containing 100 ml of ethanol solvent. After OPANA is dissolved, slowly drop an equal mole of C10 -DDP (8.20 g) was stirred at 70 °C for 12 h, the ethanol solvent was removed by rotary evaporation, and the ionic liquid was obtained by vacuum drying at 70 °C for 24 h, which was recorded as [OPANA][C 10 -DDP].
[0029] Example 7 [OPANA][C 10 The preparation process of -DDP] is consistent with that of Example 5, and the preparation process of PE is consistent with that of Example 1.
[0030] Take 1.0 g [OPANA][C 10 -DDP] was added to 49.0 g PE and dissolved to obtain an ester oil containing 2.0% by mass of naphthylamine ionic liquid, recorded as PE+2.0% [OPANA][C 10 -DDP].
[0031] Example 8 [OPANA][C 10 The preparation process of -DDP] is consistent with that of Example 5, and the preparation process of PE is consistent with that of Example 1.
[0032] Take 1.5 g [OPANA][C 10 -DDP] was added to 48.5 g PE and dissolved to obtain an ester oil containing 3.0% by mass of naphthylamine ionic liquid, recorded as PE+3.0% [OPANA][C 10 -DDP].
[0033] Comparative Example 1 The preparation process of PE is consistent with that in Example 1.
[0034] 0.5 g of zinc dialkyl dithiophosphate (ZDDP RF2202) was added to 49.5 g of PE, and after dissolution, an ester oil containing 1.0% ZDDP by mass was obtained, which was recorded as PE+1.0% ZDDP.
[0035] Comparative Example 2 The preparation process of PE is consistent with that of Example 1.
[0036] 1.0 g of zinc dialkyl dithiophosphate (ZDDP RF2202) was added to 49.0 g of PE, and after dissolution, an ester oil containing 2.0% ZDDP by mass was obtained, which was recorded as PE+2.0% ZDDP.
[0037] Comparative Example 3 The preparation process of PE is consistent with that in Example 1.
[0038] 1.5 g of zinc dialkyl dithiophosphate (ZDDP RF2202) was added to 48.5 g of PE, and after dissolution, an ester oil containing 3.0% ZDDP by mass was obtained, which was recorded as PE+3.0% ZDDP.
[0039] Tribological performance test of the ionic liquid ester oil high temperature lubricating additive prepared in the examples and comparative examples: The tribological properties of the ionic liquid of the present invention as an ester oil additive were investigated on a Jinan Shunmao MRS-1J four-ball friction and wear tester, and a comparative test was conducted with ZDDP. The upper and lower test balls used in this experiment were made of GCr15 bearing steel with a diameter of 12.7 mm, a surface roughness of 0.025 μm, and a hardness of 60-63 HRC. The tribological test was carried out at 150°C, 392 N, and 1200 r / min for 1 hour. The friction test results are shown in Table 1. The friction coefficient curve is shown in Figure 2 As shown, the wear spot diameter is Figure 3 shown.
[0040] Depend on Figure 2 It can be seen that ester oils have transient high friction under high temperature conditions. This is because the base oil cannot form a stable friction film during the friction process. 10 -DDP] can form a friction film on the metal surface to stabilize the friction coefficient after adding ester oil. The wear spot diameter of the steel ball can be seen from Table 1. Compared with ZDDP in the comparative example, the naphthylamine ionic liquid of the present invention as an ester oil lubricating additive exhibits more excellent anti-wear performance and can be used as a high-performance lubricating and anti-wear additive in the field of lubrication engineering.
[0041] According to the test standard ASTM D 6186-08, the initial oxidation temperature of the lubricant was tested by a high pressure differential scanning calorimeter (NETZSCH DSC 204HP) by a programmed temperature method, with a heating rate of 10°C / min, an oxygen flow rate of 100mL / min, and a test temperature of room temperature to 310°C. Figure 4 It can be obtained that the initial oxidation temperature of ester oil is 206.10℃; the initial oxidation temperature of PE+1%ZDDP is 238.30℃, the initial oxidation temperature of PE+1%[OPANA][DEHP] is 267.0℃, and the initial oxidation temperature of PE+1%[OPANA][C 10 -DDP] has an initial oxidation temperature of 267.30° C. Compared with ZDDP in the comparative example, the naphthylamine ionic liquid of the present invention exhibits more excellent antioxidant properties as an ester oil lubricating additive and can be used as a high-performance antioxidant in the field of lubrication engineering.
[0042] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.
Claims
1. A naphthylamine ionic liquid having the structural formula: Where, R1=i-C8H 17 , R2=i-C8H 17 , R3=nC 10 H 21 .
2. A method for preparing a naphthylamine ionic liquid as claimed in claim 1, characterized in that: Octylated phenyl-α-naphthylamine was dissolved in ethanol solvent, and then di(2-ethylhexyl) phosphate or didecyl dithiophosphate was slowly added dropwise, stirred at 60-70°C for 12-15h, the ethanol solvent was removed by rotary evaporation, and the naphthylamine ionic liquid [OPANA][DEHP] or [OPANA][C 10 -DDP].
3. The method for preparing the naphthylamine ionic liquid according to claim 2, wherein: The molar ratio of octylated phenyl-α-naphthylamine to di(2-ethylhexyl)phosphate or didecyl dithiophosphate is 1:
1.
4. Use of the naphthylamine ionic liquid as claimed in claim 1 as an additive for ester oil.
Citation Information
Patent Citations
Ester compound, preparation method and application thereof, and antioxidant composition
CN114478289A
Hydrocarbon oil additive and lubricating oil composition containing the same
JP1993140556A