Surface strengthening compounding process of profile steel roller

Through powder flame spraying and laser remelting technology, a coating with uniform thickness and excellent wear resistance is prepared, which solves the problem of insufficient paint uniformity and wear resistance in the surface treatment of steel rolls, extends service life and reduces production costs .

CN119061344APending Publication Date: 2024-12-03TAIER HEAVY INDUSTRY CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411197337.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-29
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

The existing surface treatment technology of steel rolling rolls has problems such as difficult to control the uniformity of the coating, high material hardness, difficulty in subsequent processing, insufficient wear resistance, etc., resulting in short service life of the roll and high production costs.

Method used

Powder flame spraying method was used to prepare WC-10Ni-5Cr coating with a thickness of 0.3-0.5 mm, and the bonding strength and wear resistance of the coating and the substrate were further improved through laser remelting technology.

Benefits of technology

The dense metallurgical combination of the coating is achieved, avoiding shedding, improving the material deposition rate and spraying efficiency, extending the service life of the roll, and reducing manufacturing costs.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a surface strengthening compound process for a profile steel roller, which combines powder flame spraying and laser remelting, and specifically comprises the following steps: step 1, cleaning the surface of the profile steel roller; 2, the surface of the profile steel roller is subjected to sand blasting roughening treatment; 3, a wear-resistant coating of 0.3-0.5 mm is prepared on the surface of the profile steel roller through a powder flame spraying method; and 4, the wear-resistant coating is subjected to laser remelting. According to the surface strengthening composite technology, the coating resistant layer which is excellent in abrasion resistance, large in thickness, uniform in thickness and good in combination is prepared on the surface of the profile steel roller through powder flame spraying and laser remelting, the service life of the profile steel roller is prolonged, and the manufacturing cost is also reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Background

[0001] The invention relates to a composite process for strengthening the surface of a section steel roller. Background Art

[0003] As a rolling tool for angle steel, H-shaped steel, channel steel and other steel materials, steel rollers have a wide variety of specifications and are generally made of semi-steel and other materials. After a period of use, the hole type of steel rollers will wear out. Taking the BD rollers of large steel billet mills as an example, the amount of steel passed on a single line is usually around 6,000 tons, and it is offline in about 3 days. A pair of new rollers usually reaches the scrap size after being used on the machine for about 7 times, and the total amount of steel passed is about 40,000 tons. The manufacturing cost of BD rollers is relatively high, and the cost of each pair of rollers is basically around 1 million. Under normal circumstances, a production line consumes more than 10 million yuan for BD rollers alone. Therefore, strengthening the surface of steel rollers plays a key role in ensuring normal production and reducing production costs.

[0004] Chinese patent "201310264744.X" discloses a laser alloying method for steel rolls, which is to prepare 0.3-0.5mm Ni60+45% WC alloy coating on the roll surface by laser alloying method; the process has the following problems: 1. The coating uniformity control is difficult; 2. The surface state is poor after laser alloying, and the material hardness is high, which makes the subsequent processing of the pass of the steel roll difficult; 3. The wear resistance of the material is insufficient. Chinese patent "2013100908572" discloses a supersonic spraying method for the pass of a steel roll made of semi-steel, which has the following problems: 1. The coating thickness is very thin 0.03-0.07mm, and the lifting effect is not obvious; 2. The supersonic spray coating is mechanically bonded, and the bonding strength is low, so the coating is easy to fall off; 3. There are gaps in the supersonic spray coating. Although the hole is sealed, it is difficult to ensure that the cooling water will not penetrate into the coating, causing the coating to fall off and fail. Chinese patent "2016108460515" discloses a laser remelting method for supersonic sprayed WC-12Co coating, which has the following disadvantages: 1. The thickness of the supersonic sprayed coating is very thin, 200-300μm, and the lifting effect is not obvious; 2. The coating material WC-12Co uses Co as the bonding phase, which is highly brittle. When the thickness of the sprayed layer exceeds 0.2mm, cracks are prone to occur, and the coating is prone to cracking during the remelting process. Summary of the invention

[0005] The problem to be solved by the present invention is to provide a surface strengthening composite process for steel section rollers, which prepares a coating layer with excellent wear resistance, thick thickness, uniform thickness and good bonding on the surface of the steel section roller through the composite of powder flame spraying and laser remelting, thereby extending the service life of the steel section roller and reducing the manufacturing cost.

[0006] The invention discloses a surface strengthening composite process for a section steel roller, which is a combination of powder flame spraying and laser remelting.

[0007] The present invention provides a surface strengthening composite process for a steel roll, which specifically comprises:

[0008] Step 1: Clean the surface of the steel roller;

[0009] Step 2: sandblasting the surface of the steel roller;

[0010] Step 3: Prepare a 0.3-0.5 mm wear-resistant coating on the surface of the steel roll by using a powder flame spraying method;

[0011] Step 4: Laser remelting of the wear-resistant coating.

[0012] Wherein, step 3: the composition and mass percentage of the wear-resistant coating are: WC: 80-85%, Ni: 10-12%, Cr: 5-8%.

[0013] Among them, step 4: the specific process of laser remelting is: power 6000W, spot size 20*3mm, speed 800-1200mm / min.

[0014] The beneficial effects of the surface strengthening composite process of the steel roller of the present invention are as follows: 1. After the coating obtained by powder flame spraying is laser remelted, the coating and the substrate are densely metallurgically bonded to avoid the risk of coating peeling; 2. Compared with supersonic spraying, powder flame spraying has a higher material deposition rate and higher spraying efficiency, and is particularly suitable for preparing thick coatings (>0.3mm), which meets the requirements of energy saving and material saving; at the same time, the coating after spraying is smooth and evenly distributed, and the coating is smoother after laser remelting, and no subsequent processing is required; 3. The WC content in the coating exceeds 80%, and the wear resistance is excellent, which strengthens the surface of the steel roller and prolongs its service life; 4. The coating contains Ni with good plasticity and toughness, which is not easy to crack, so it is easier to prepare a thick coating (thickness reaches 0.3-0.5mm), and the coating is not easy to crack during the remelting process. Therefore, the surface strengthening composite process of the present invention can obtain a coating with good wear resistance, thick thickness, not easy to fall off, and smooth on the surface of the steel roller, thereby prolonging the service life of the steel roller. At the same time, the surface strengthening composite process of the present invention is not limited to strengthening the surface of a steel roller, but can also be applied to other parts that require surface strengthening. DETAILED DESCRIPTION

[0015] Example 1

[0016] The invention discloses a surface strengthening composite process for a section steel roller, which is a combination of powder flame spraying and laser remelting.

[0017] Example 2

[0018] The present invention provides a surface strengthening composite process for a steel roll, which specifically comprises:

[0019] Step 1: Clean the surface of the steel roller;

[0020] Step 2: sandblasting the surface of the steel roller;

[0021] Step 3: Prepare a 0.3-0.5 mm wear-resistant coating on the surface of the steel roll by using a powder flame spraying method;

[0022] Step 4: Laser remelting of the wear-resistant coating.

[0023] Among them, step 2 is to perform sandblasting and roughening treatment on the surface of the steel roller, which can improve the bonding strength between the coating and the substrate, thereby preventing the coating from falling off; step 3 powder flame spraying has a higher material deposition rate and higher spraying efficiency than supersonic spraying, and is particularly suitable for preparing thick coatings (>0.3mm), which meets the requirements of energy saving and material saving; step 4 laser remelting further improves the bonding strength between the powder flame spraying coating and the substrate, and improves the performance of the coating.

[0024] Example 3

[0025] The surface strengthening composite process of a steel roller of the present invention: Step 3: The composition and mass percentage of the wear-resistant coating are: WC: 80-85%, Ni: 10-12%, Cr: 5-8%.

[0026] The wear-resistant coating material WC-10Ni5Cr of the present invention contains Ni with good plasticity and toughness, so that a thick coating can be prepared more easily and is not prone to cracking during the remelting process; at the same time, WC increases the hardness of the coating and improves the wear resistance.

[0027] Example 4

[0028] The present invention discloses a surface strengthening composite process for a steel roller: Step 4: The specific process of laser remelting is: power 6000W, rectangular spot 20*3mm, speed 800-1200mm / min.

[0029] Laser remelting remelts the coating surface and the steel roller surface to form a metallurgical bond, which improves the bonding strength between the coating and the substrate and avoids the risk of coating peeling; at the same time, the coating structure performance is enhanced and the wear resistance is improved.

[0030] Example 5

[0031] The present invention discloses a surface strengthening composite process for a steel roller: Step 1: using a mixed solution of acetone and anhydrous ethanol to ultrasonically clean the surface.

[0032] Example 6

[0033] The present invention discloses a surface strengthening composite process for a steel roller: Step 2: a sandblasting machine uses white corundum to roughen the surface, and the particle size of the white corundum is 100 meshes.

[0034] The beneficial effects of the surface strengthening composite process of the steel roller of the present invention are as follows: 1. After the coating obtained by powder flame spraying is laser remelted, the coating and the substrate are densely metallurgically bonded to avoid the risk of coating peeling; 2. Compared with supersonic spraying, powder flame spraying has a higher material deposition rate and higher spraying efficiency, and is particularly suitable for preparing thick coatings (>0.3mm), which meets the requirements of energy saving and material saving; at the same time, the coating after spraying is smooth and evenly distributed, and the coating is smoother after laser remelting, and no subsequent processing is required; 3. The WC content in the coating exceeds 80%, and the wear resistance is excellent, which strengthens the surface of the steel roller and prolongs its service life; 4. The coating contains Ni with good plasticity and toughness, which is not easy to crack, so it is easier to prepare a thick coating (thickness reaches 0.3-0.5mm), and the coating is not easy to crack during the remelting process. Therefore, the surface strengthening composite process of the present invention can obtain a coating with good wear resistance, thick thickness, not easy to fall off, and smooth on the surface of the steel roller, thereby prolonging the service life of the steel roller and reducing the manufacturing cost. At the same time, the surface strengthening composite process of the present invention is not limited to strengthening the surface of a steel roller, but can also be applied to other parts that require surface strengthening.

Claims

1. A surface strengthening composite process for steel rolls. Its characteristics are: It is a combination of powder flame spraying and laser remelting.

2. The surface strengthening composite process according to claim 1, wherein: Step 1: Clean the surface of the steel roller; Step 2: sandblasting the surface of the steel roller; Step 3: Prepare a 0.3-0.5 mm wear-resistant coating on the surface of the steel roll by using a powder flame spraying method; Step 4: Laser remelting of the wear-resistant coating.

3. The surface strengthening composite process according to claim 2, Its characteristics are: In step 3: the composition and mass percentage of the wear-resistant coating are: WC: 80-85%, Ni: 10-12%, Cr: 5-8%.

4. The surface strengthening composite process according to claim 2 is characterized in that: in step 4: the specific process of laser remelting is: power 6000W, spot size 20*3mm, speed 800-1200mm / min.

Citation Information

Patent Citations

  • Processing process of composite cold roll

    CN102758166A

  • Method for preparing tungsten carbide coating on surface of roller for lithium battery production

    CN113699478A

  • Flame-spraying / welding powdered alloy for high-performance heat continuous rolling mill outlet roller / cylinder

    CN1733962A

  • WC-ni wear-resistant coating on 316l stainless steel surface and preparation method therefor

    WO2024077654A1