Semiconductor cleaning step

By first depositing a carbon layer in the semiconductor cavity to cover the residual layer, and then performing plasma cleaning, the damage problem of the cavity cleaning step on the heater is solved, the process efficiency and automation are improved, and the service life of the heater is extended.

CN119061355APending Publication Date: 2024-12-03UNITED SEMICONDUCTOR (XIAMEN) CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310642023.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-06-01
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

In semiconductor manufacturing processes, the cavity cleaning step will cause damage to the heater, affecting its surface uniformity and life, and traditional methods require additional vacuum and vacuum breaking steps to reduce process efficiency.

Method used

Before the gas plasma cleaning step, deposit a layer of carbon on the bottom and side walls of the cavity and the heater surface to cover the residual layer, and perform plasma cleaning in the same cavity to remove the carbon layer and residual layer to avoid direct Bombardment heater.

Benefits of technology

It effectively protects the heater surface, extends its life, and performs cleaning steps in the same cavity, reducing the vacuum extraction and vacuum breaking time, and improving process efficiency and automation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119061355A_ABST
    Figure CN119061355A_ABST
Patent Text Reader

Abstract

A semiconductor cleaning step includes providing a cavity including a bottom surface and a sidewall, the cavity including a heater on the bottom surface, performing a first deposition step to leave a residual layer on the sidewall of the cavity, performing a carbon deposition step to form at least a carbon layer on a surface of the heater, and performing a second deposition step to leave a carbon layer on the surface of the heater. And performing a plasma cleaning step to simultaneously remove the residual layer on the side wall of the cavity and the carbon layer on the bottom surface.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the semiconductor field, and in particular to a cleaning method for a cavity of a semiconductor machine, which helps to reduce damage to a heater during the cleaning process. Background Art

[0002] The deposition step is one of the commonly used steps in the semiconductor manufacturing process, including physical vapor deposition (PVD) and chemical vapor deposition (CVD) and other manufacturing processes. The target object (such as a substrate) is placed in a cavity, and then various materials are deposited on the target object to form a material layer. The deposition step can form various stacked material layers on the substrate, and is one of the main methods for forming a stacked structure in the current semiconductor manufacturing process.

[0003] During the deposition step in the current semiconductor manufacturing process, the target object needs to be placed in a chamber. After the deposition step is completed, since there may be a residual layer attached inside the chamber, in order to prevent these residual layers from affecting the next deposition step, the chamber usually needs to be cleaned to ensure the quality of the subsequent manufacturing process.

[0004] However, the chamber cleaning step is also one of the necessary manufacturing processes for semiconductors. Excessive cleaning steps may prolong the overall manufacturing process time or more easily cause damage to components inside the chamber. Therefore, improving the efficiency of semiconductor manufacturing processes is also one of the research directions in this field. Summary of the invention

[0005] The present invention provides a semiconductor cleaning step, comprising providing a chamber, the chamber comprising a bottom surface and a side wall, the chamber comprising a heater located on the bottom surface, performing a first deposition step to leave a residual layer on the side wall of the chamber, performing a carbon deposition step to form a carbon layer at least on the surface of the heater, and performing a plasma cleaning step to simultaneously remove the residual layer on the side wall of the chamber and the carbon layer on the bottom surface.

[0006] In the existing steps, after the deposition step of the cavity is completed, gas plasma cleaning is performed to clean the inside of the cavity to remove the residual material layer remaining on the side wall of the cavity. However, during this cleaning step, the heater at the bottom of the cavity will also be partially damaged, thereby affecting the uniformity of the heater surface. The present invention is characterized in that before the gas plasma cleaning step is performed, an additional carbon layer is deposited to cover the heater at the bottom of the cavity and the side wall of the cavity, and then the inside of the cavity is cleaned with gas plasma, so as to avoid gas plasma from damaging the heater in the cavity. In addition, the deposition of the carbon layer and the cleaning step of the present invention are carried out in the same cavity, which omits the time for evacuating and breaking the vacuum, and helps to improve the overall production process efficiency and automation. BRIEF DESCRIPTION OF THE DRAWINGS

[0007] Figures 1 to 4 It is a schematic cross-sectional structure diagram of the semiconductor cleaning step of the present invention.

[0008] Main component symbols

[0009] 10: Cavity

[0010] 10A: Bottom

[0011] 10B: Sidewall

[0012] 12: Heater

[0013] 14: Residual layer (material layer)

[0014] 16: Carbon layer

[0015] A: Area

[0016] B: Area

[0017] C: Region

[0018] P1: First deposition step

[0019] P2: Carbon deposition step

[0020] P3: Plasma cleaning step

[0021] T1: Thickness

[0022] T2: Thickness

[0023] T3:Thickness

[0024] T4:Thickness

[0025] W:Whip DETAILED DESCRIPTION

[0026] In order to enable a person skilled in the art to further understand the present invention, the preferred embodiments of the present invention are listed below, and the components and intended effects of the present invention are described in detail with reference to the accompanying drawings.

[0027] For the convenience of explanation, the drawings of the present invention are only for illustration to make it easier to understand the present invention, and the detailed proportions can be adjusted according to the design requirements. The upper and lower relationships of the relative elements in the drawings described in the text should be understood by those skilled in the art to refer to the relative positions of the objects, so they can be flipped to present the same components, which should all fall within the scope of the disclosure of this specification, and will be explained here first.

[0028] Please refer to Figures 1 to 4 , Figures 1 to 4 A schematic cross-sectional structure diagram of the semiconductor cleaning step of the present invention is shown. First, Figure 1 As shown, a chamber 10 is provided, for example, a chamber in a semiconductor machine used for a deposition step in a semiconductor manufacturing process, the chamber 10 includes a bottom surface 10A and a side wall 10B, and includes a heater 12 located on the bottom surface 10A of the chamber 10. The function of the heater 12 is to heat a target placed on the heater 12 during the deposition step, for example, when a wafer W is placed on the heater 12, the wafer W can be heated. Whether the target is to be heated while the deposition step is being performed or the target is to be heated after the deposition step is completed, the heater 12 may be used.

[0029] Generally speaking, the heater 12 is in the shape of a plate with a flat surface. After the wafer W is placed on the heater 12, a first deposition step P1 is performed to deposit a material layer 14 onto the wafer W in the chamber 10. The material layer 14 here may be a material layer of a specific material, such as one of the layers of material formed on the wafer W in the semiconductor manufacturing process, such as a metal material or an insulating layer, etc., but the present invention is not limited thereto. It is worth noting that, since the particles of the material layer will fill the entire space in the chamber 10 during the deposition step, in addition to the residual material layer 14 formed on the top of the wafer W, other places in the chamber 10, such as the heater 12, the bottom surface 10A and the side wall 10B that are not covered by the wafer W may also be formed with a material layer 14. Here, the other material layers 14 formed outside the surface of the wafer W are defined as residual layers 14, wherein the material layer 14 and the residual layer 14 are composed of the same material. In addition, since the deposition step is mainly performed on the bottom surface 10A of the cavity 10, and the side wall 10B is not the main deposition target, the thickness T1 of the material layer 14 (or the residual layer 14) at the bottom surface 10A is greater than the thickness T2 at the side wall 10B. In addition, the portion of the material layer 14 close to the bottom surface of the cavity 10 will be deposited thicker, that is, the thickness of the material layer 14 in area A will be thinner than the thickness of the material layer 14 in area B.

[0030] like Figure 2 As shown, after the chip W is moved out of the cavity 10, the heater 12, the bottom surface 10A and the side wall 10B not covered by the chip W all contain a residual layer 14. This part of the residual layer 14 will be removed in a subsequent cleaning step to prevent the residual layer 14 from contaminating the cavity 10 and affecting other subsequent deposition manufacturing processes.

[0031] In the current technology, gas plasma is usually used to bombard the inside of the chamber 10 (hereinafter referred to as the plasma cleaning step) to remove the residual layer 14 in the chamber 10. However, since a portion of the region C of the heater 12 is covered by the wafer W in the previous step, no residual layer 14 is formed on the surface of the region C. Therefore, during the plasma cleaning step, the plasma gas will not only remove the residual layer 14 remaining on the bottom surface 10A and the side wall 10B of the chamber 10 or the surface of the heater 12, but will also bombard the surface of the region C, and may cause partial damage to the surface of the region C. Long-term accumulation will cause the surface of the heater 12 to have an uneven profile, and may make the heating effect uneven. If the heater is to be replaced, it will also cause a loss of money and time due to the high cost of the heater and the need to shut down the machine during the replacement.

[0032] Therefore, in order to solve the above problems, the present invention provides an improved cavity cleaning method. Figure 3 As shown, before the plasma cleaning step is performed, a carbon deposition step P2 is performed to deposit an additional carbon layer 16 covering the bottom surface 10A, the side wall 10B of the chamber 10 and the surface of the heater 12. Since the residual layer 14 has been formed first, the carbon layer 16 will cover the residual layer 14. Similarly, since the deposition step is mainly performed on the bottom surface 10A of the chamber 10, and the side wall 10B is not the main deposition target, the thickness T3 of the carbon layer 16 on the bottom surface 10A will be greater than the thickness T4 on the side wall 10B. Then, as shown in FIG. Figure 4 As shown, a plasma cleaning step P3 is performed to remove the carbon layer 16 and the residual layer 14 remaining in the chamber 10. The plasma cleaning step P3 is, for example, nitrogen plasma and oxygen plasma, but the present invention is not limited thereto. It is worth noting that since the area C is already covered by the carbon layer 16, when the plasma cleaning step P3 is performed, the gas plasma is not easy to directly bombard the surface of the heater 12, thereby protecting the surface of the heater 12 and extending the life of the heater 12.

[0033] The reason why the residual layer 14 is covered with the carbon layer 16 in the present invention instead of other material layers (such as silicon nitride, silicon oxide, etc.) is that the carbon material has a higher stability and is therefore not easy to react with other material layers to form undesirable compounds. In addition, the carbon material is relatively easy to be removed by gas plasma, so the applicant has found that when the carbon layer 16 covers the residual layer 14, the rate at which the residual layer 14 is removed by gas plasma is further increased, that is, the cleaning effect of the cavity can be improved.

[0034] In addition, in some other embodiments, after the wafer W is removed from the cavity 10, a blank wafer (not shown) may be reloaded into the cavity 10 and cover the area C, and then the plasma cleaning step P3 is performed to remove the residual layer 14 in the cavity 10. At this time, the area C can also be protected by the blank wafer and will not be corroded by the gas plasma. However, the method of forming the carbon layer 16 in the first embodiment of the present invention replaces the method of covering the area C with a blank wafer, which has several advantages in comparison. First, the blank wafer is usually a silicon wafer, and when the silicon wafer is bombarded by the gas plasma, some particles will also be generated and scattered into the cavity, which may cause partial contamination in the cavity, while the carbon layer of the present invention is less likely to contaminate the cavity 10. The second advantage is that the method of the present invention does not require the loading or removal of a blank wafer, that is, the plasma cleaning step P3 of the present invention is performed in the same cavity, which can reduce the time of vacuuming and breaking the vacuum of the cavity and is conducive to the automation of the manufacturing process, while also reducing the possibility of contamination caused by contact with the outside air. The third advantage is that the formation of the carbon layer 16 helps to increase the rate of removing the residual layer 14.

[0035] In summary, the present invention provides a semiconductor cleaning step, including providing a chamber 10, the chamber 10 including a bottom surface 10A and a side wall 10B, the chamber 10 including a heater 12 located on the bottom surface 10A, performing a first deposition step P1 to leave a residual layer 14 on the side wall 10B of the chamber 10, performing a carbon deposition step P2 to form a carbon layer 16 at least on the surface of the heater 12, and performing a plasma cleaning step P3 to simultaneously remove the residual layer 14 on the side wall 10B of the chamber 10 and the carbon layer 16 on the bottom surface 10A.

[0036] In some embodiments of the present invention, when the carbon layer 16 is formed, the carbon layer 16 further covers the residual layer 14 on the sidewall 10B of the cavity 10 .

[0037] In some embodiments of the present invention, when the plasma cleaning step P3 is performed, the residual layer 14 and the carbon layer 16 on the sidewall 10B of the chamber 10 and the carbon layer 16 on the bottom surface 10A are removed simultaneously.

[0038] In some embodiments of the present invention, performing the first deposition step P1 further includes: placing a chip W on the surface of the heater, performing the first deposition step P1, and moving the chip W out of the chamber 10.

[0039] In some embodiments of the present invention, after the first deposition step P1 , a residual layer 14 is formed on the sidewall 10B of the cavity 10 , while a portion of the surface (region C) of the heater does not form the residual layer 14 .

[0040] In some embodiments of the present invention, the plasma cleaning step P3 includes bombarding the carbon layer 16 and the residual layer 14 with nitrogen ions in an oxygen environment to remove the carbon layer 16 and the residual layer 14 .

[0041] In some embodiments of the present invention, the carbon layer 16 does not include silicon nitride or silicon oxide.

[0042] In some embodiments of the present invention, after the plasma cleaning step P3, a second deposition step (ie, another deposition step performed in the subsequent steps) is further performed.

[0043] In some embodiments of the present invention, the second deposition step includes placing another wafer on the surface of the heater, and depositing another material layer on the other wafer.

[0044] In some embodiments of the present invention, after the plasma cleaning step P3 , the residual layer 14 on the sidewall 10B of the cavity 10 has been completely removed.

[0045] In some embodiments of the present invention, the first deposition step P1 , the carbon deposition step P2 , and the plasma cleaning step P3 are all performed in the chamber 10 .

[0046] In some embodiments of the present invention, during the process from the carbon deposition step P2 to the plasma cleaning step P3, the chamber 10 is maintained in a vacuum state, and a vacuum breaking step is not performed.

[0047] In some embodiments of the present invention, the thickness of the carbon layer 16 on the surface of the heater 12 is equal to the thickness of the residual layer 14 on the sidewall 10B of the chamber 10. Figure 3 As shown, the thickness T3 of the carbon layer 16 on the bottom surface 10A is approximately equal to twice the thickness T4 of the residual layer 14 on the sidewall 10B. In this way, when the carbon layer 16 on the bottom surface 10A is removed, the residual layer 14 can also be removed at the same time.

[0048] In the existing steps, after the deposition step of the cavity is completed, gas plasma cleaning is performed to clean the inside of the cavity to remove the residual material layer remaining on the side wall of the cavity. However, during this cleaning step, the heater at the bottom of the cavity will also be partially damaged, thereby affecting the uniformity of the heater surface. The present invention is characterized in that before the gas plasma cleaning step is performed, an additional carbon layer is deposited to cover the heater at the bottom of the cavity and the side wall of the cavity, and then the inside of the cavity is cleaned with gas plasma, so as to avoid gas plasma from damaging the heater in the cavity. In addition, the deposition of the carbon layer and the cleaning step of the present invention are carried out in the same cavity, which omits the time for evacuating and breaking the vacuum, and helps to improve the overall production process efficiency and automation.

[0049] The above descriptions are only preferred embodiments of the present invention. All equivalent changes and modifications made according to the claims of the present invention should fall within the scope of the present invention.

Claims

1. A semiconductor cleaning step, comprising: Providing a cavity, the cavity comprising a bottom surface and a side wall, the cavity comprising a heater located on the bottom surface; performing a first deposition step to leave a residual layer on the sidewall of the cavity; performing a carbon deposition step to form a carbon layer on at least a surface of the heater; as well as A plasma cleaning step is performed to simultaneously remove the residual layer on the sidewall of the cavity and the carbon layer on the bottom surface. 2 . The semiconductor cleaning step as claimed in claim 1 , wherein when the carbon layer is formed, the carbon layer also covers the residual layer on the sidewall of the cavity.

3. The semiconductor cleaning step as claimed in claim 2, wherein when the plasma cleaning step is performed, the residual layer and the carbon layer on the sidewall of the chamber, and the carbon layer on the bottom surface are removed simultaneously.

4. The semiconductor cleaning step as claimed in claim 1, wherein performing the first deposition step further comprises: placing a wafer on the surface of the heater; performing the first deposition step; and The wafer is moved out of the chamber. 5 . The semiconductor cleaning step as claimed in claim 4 , wherein after the first deposition step, the residual layer is formed on the sidewall of the chamber, while the residual layer is not formed on a portion of the surface of the heater. 6 . The semiconductor cleaning step as claimed in claim 1 , wherein the plasma cleaning step comprises bombarding the carbon layer and the residual layer with nitrogen ions in an oxygen environment to remove the carbon layer and the residual layer.

7. The semiconductor cleaning process as claimed in claim 1, wherein the carbon layer does not contain silicon nitride or silicon oxide.

8. The semiconductor cleaning process as claimed in claim 1, further comprising performing a second deposition step after the plasma cleaning step.

9. The semiconductor cleaning step of claim 8, wherein the second deposition step comprises: placing another wafer onto the surface of the heater; and A material layer is deposited on the other wafer. 10 . The semiconductor cleaning step of claim 8 , wherein after the plasma cleaning step, the residual layer on the sidewall of the cavity has been completely removed. 11 . The semiconductor cleaning step as claimed in claim 1 , wherein the first deposition step, the carbon deposition step and the plasma cleaning step are all performed in the chamber. 12 . The semiconductor cleaning step as claimed in claim 11 , wherein during the process from the carbon deposition step to the completion of the plasma cleaning step, the chamber is maintained in a vacuum state and no vacuum breaking step is performed.

13. The semiconductor cleaning step as claimed in claim 1, wherein a thickness of the carbon layer on the surface of the heater is equal to twice a thickness of the residual layer on the side of the heater.