Liquid crystal light beam deflector and preparation method thereof

By using an orientation layer in the liquid crystal beam deflector to anchor the liquid crystal molecules, forming a gradient refractive index distribution, the high operating voltage and light scattering problems caused by the polymer network are solved, and the beam deflection and high transmittance under the condition of no external voltage are achieved .

CN119065171APending Publication Date: 2024-12-03HEFEI UNIV OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411452982.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-17
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

Due to the existence of the polymer network, existing liquid crystal beam deflectors have increased operating voltage and severe light scattering, which affects the performance of the device.

Method used

The first orientation layer and the second orientation layer are used as polymer brushes to anchor the direction of the liquid crystal molecules to form a gradient refractive index distribution, reducing the distribution of the polymer in the liquid crystal layer, thereby reducing the working voltage and light scattering.

Benefits of technology

Deflection of the light beam under no external voltage is achieved, reducing the working voltage and light scattering, and improving the transmittance and response speed of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119065171A_ABST
    Figure CN119065171A_ABST
Patent Text Reader

Abstract

The invention provides a liquid crystal light beam deflector and a preparation method thereof, and belongs to the technical field of optical devices, and the liquid crystal light beam deflector comprises a first substrate, a first orientation layer, a liquid crystal layer, a second orientation layer and a second substrate. Wherein the first orientation layer is arranged on the first substrate; the liquid crystal layer is arranged on the first orientation layer; the second orientation layer is arranged on the liquid crystal layer; the second substrate is arranged on the second orientation layer; when the voltage is not applied to the liquid crystal light beam deflector, the liquid crystal layer has a refractive index changing in a gradient mode in the first direction. The first direction is parallel to the surface of the liquid crystal layer. According to the liquid crystal light beam deflector and the preparation method thereof, the gradient refractive index distribution formed in the liquid crystal layer is fixed by utilizing the anchoring effect of the orientation layer, and a deflection effect can be applied to the light beam under the condition of no external voltage without arranging a complex modulation circuit on the substrate.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of optical devices, and in particular to a liquid crystal light beam deflector and a preparation method thereof. Background Art

[0002] Beam deflection technology refers to the technology of changing the direction of the light beam or adjusting the imaging visual axis. It has great application prospects in optical processing, laser scanning, optical communication, medical treatment and other aspects. At present, the mainstream beam deflection technology is mainly divided into mechanical and non-mechanical types. Mechanical beam deflection technology is mature, but it has problems such as large size, high energy consumption, and motion sensitivity; while non-mechanical beam deflection has many advantages such as low energy consumption, lightness and flexibility, and automatic control. Liquid crystal materials have the optical properties of uniaxial crystals. Using liquid crystal molecules as phase shifting materials can modulate the wavefront phase of the incident light. Liquid crystal materials have great application potential in the field of non-mechanical beam deflection due to their low cost, fast response and electrically adjustable properties.

[0003] Liquid crystal beam deflectors have many advantages such as low power consumption, high precision, light weight, and miniaturization. The basic principle of liquid crystal beam deflectors is to utilize the electro-optical effect and electrically controlled birefringence effect of liquid crystals, and to control the direction of the liquid crystal director by applying an external electric field to form a periodically arranged gradient refractive index distribution in the liquid crystal layer, and to phase modulate the incident linearly polarized light parallel to the extraordinary optical axis. The incident light obtains a sawtooth periodic phase delay, forming a blazed grating to achieve beam deflection.

[0004] When a voltage higher than the threshold is applied to the liquid crystal molecules, the orientation of the liquid crystal molecules will change, and the effective extraordinary refractive index (n e-eff , formula (1)) will also change; at this time, due to the change in the optical path difference, a phase difference will be generated after the light passes through the entire liquid crystal box ( Formula (2)), θ represents the angle between the long axis of the liquid crystal molecule and the liquid crystal director, n e is the extraordinary refractive index, n o is the ordinary refractive index, is the relative phase difference of the incident linear polarized light, D is the cell thickness, and λ is the incident wavelength.

[0005]

[0006]

[0007] When this phase difference distribution meets certain conditions (periodic blazed grating or non-periodic blazed grating principle), according to the principle of optical diffraction, most of the energy of the emitted extraordinary light will be distributed at a certain angle in the far field, thus achieving beam deflection modulation.

[0008] At present, fast response liquid crystal beam deflectors usually introduce polymers into the liquid crystal layer and use the anchoring effect of the polymer network on the liquid crystal molecules to make the liquid crystal layer have a gradient refractive index that meets the requirements to meet the specific phase distribution, thereby achieving the deflection of the incident light beam. However, the polymer network in the liquid crystal layer will also hinder the rotation of the liquid crystal molecules, causing the operating voltage of the liquid crystal beam deflector to increase; at the same time, the mismatch between the refractive index of the polymer network and the liquid crystal molecules will inevitably cause scattering, affecting the transmittance of the device.

[0009] Therefore, it is necessary to provide a liquid crystal beam deflector and a preparation method thereof to reduce the excessively high operating voltage and severe light scattering of the liquid crystal beam deflector, thereby solving the above technical problems. Summary of the invention

[0010] In view of the above problems existing in the prior art, the present invention provides a liquid crystal beam deflector and a preparation method thereof to improve the technical problems of excessively high operating voltage and severe light scattering caused by introducing a polymer network into the liquid crystal layer of the existing liquid crystal beam deflector.

[0011] To achieve the above-mentioned object and other related objects, the present invention provides a liquid crystal beam deflector in a first aspect, the liquid crystal beam deflector comprising a first substrate, a first alignment layer, a liquid crystal layer, a second alignment layer and a second substrate:

[0012] Among them, the first orientation layer is arranged on the first substrate; the liquid crystal layer is arranged on the first orientation layer; the second orientation layer is arranged on the liquid crystal layer; the second substrate is arranged on the second orientation layer; when the liquid crystal beam deflector is not supplied with voltage, the liquid crystal layer has a refractive index that changes gradiently in the first direction; the first direction is parallel to the surface of the liquid crystal layer.

[0013] In an example of the present invention, the first alignment layer and the second alignment layer are polymer brushes, and when no voltage is applied to the liquid crystal beam deflector, the first alignment layer and the second alignment layer anchor the director direction of the liquid crystal molecules in the liquid crystal layer.

[0014] In an example of the present invention, the gradient-varying refractive index distribution on the liquid crystal layer is periodically arranged in the first direction.

[0015] In an example of the present invention, the thickness of the first alignment layer and the second alignment layer is 20 nm to 500 nm.

[0016] In an example of the present invention, the thickness of the liquid crystal layer is 5 μm to 100 μm.

[0017] In a second aspect, the present invention provides a method for preparing a liquid crystal beam deflector, the method comprising:

[0018] providing a first substrate and a second substrate;

[0019] forming a first alignment layer on a surface of the first substrate, and forming a second alignment layer on a surface of the second substrate;

[0020] performing an alignment treatment on the first alignment layer and the second alignment layer;

[0021] The first substrate and the second substrate are arranged opposite to each other, and a liquid crystal layer is formed between the first alignment layer and the second alignment layer;

[0022] The liquid crystal layer is divided into a plurality of modulation areas, and the direction of the directing vector of the liquid crystal molecules in each of the modulation areas is gradiently adjusted along a first direction and photocured so that the liquid crystal layer has a refractive index that changes gradiently along the first direction when no voltage is applied; wherein the first direction is parallel to the surface of the liquid crystal layer.

[0023] In one example of the present invention, the direction of the director of the liquid crystal molecules in each of the modulation areas is adjusted along the first direction and photocured, including:

[0024] Acquire a voltage-phase relationship of the liquid crystal layer, divide the liquid crystal layer into a plurality of modulation areas along the first direction according to a preset phase difference and phase gradient, and acquire a plurality of adjustment voltages corresponding to phase gradient changes for the plurality of modulation areas;

[0025] According to the phase gradient variation trend, the corresponding adjustment voltage is applied to each of the modulation areas in the first direction in turn, and the director direction of the modulated liquid crystal molecules in the modulation area is solidified by light.

[0026] In an example of the present invention, the preparation method further includes a step of modulating the periodic refractive index gradient distribution of the liquid crystal layer, and the periodic refractive index gradient modulation step includes:

[0027] Dividing the liquid crystal layer into a plurality of periodic modulation regions along the first direction, and performing modulation with the same refractive index gradient distribution on each of the periodic modulation regions;

[0028] Among them, for each of the periodic modulation areas: the periodic modulation area is divided into a plurality of modulation areas along the first direction, and the direction of the pointing vector of the liquid crystal molecules in each of the modulation areas is gradient adjusted and photocured along the first direction, so that the periodic modulation area has a refractive index distribution that changes gradiently along the first direction when no voltage is applied.

[0029] In an example of the present invention, a first alignment layer is formed on a surface of the first substrate, and a second alignment layer is formed on a surface of the second substrate, including:

[0030] A photoinitiator, a liquid crystal alignment agent and a solvent are mixed and coated on the surfaces of the first substrate and the second substrate; the solvent on the first substrate and the second substrate is heated and dried to form a first alignment layer on the first substrate and a second alignment layer on the second substrate.

[0031] In one example of the present invention, the solvent is at least one of deionized water, dimethylacetamide, N-methylpyrrolidone and toluene; the liquid crystal alignment agent is at least one of polyvinyl alcohol, polyimide and polystyrene; and the photoinitiator has an absorption peak including the photocuring band.

[0032] In an example of the present invention, performing an alignment treatment on the first alignment layer and the second alignment layer includes: performing a friction treatment on the surfaces of the first alignment layer and the second alignment layer along the same direction.

[0033] In an example of the present invention, the first substrate and the second substrate are arranged opposite to each other, and a liquid crystal layer is formed between the first alignment layer and the second alignment layer, including:

[0034] The first substrate and the second substrate are arranged opposite to each other, and the first alignment layer and the second alignment layer are arranged opposite to each other; wherein the alignment directions of the first alignment layer and the second alignment layer arranged opposite to each other are opposite; and monomers and liquid crystals are filled between the first alignment layer and the second alignment layer to form a liquid crystal layer; wherein the monomers are acrylic acid ester liquid crystal monomers, and the liquid crystals are positive nematic phase liquid crystals.

[0035] The liquid crystal beam deflector and its preparation method of the present invention form an alignment layer on the surface of the first substrate and the second substrate, and use the light-induced anchoring effect of the alignment layer to solidify the direction of the director of the liquid crystal molecules after voltage modulation, so that the liquid crystal layer can have a refractive index with a gradient distribution along the first direction when no external voltage is applied, so as to achieve the deflection effect on the light beam without external voltage. As an active beam deflector, the liquid crystal beam deflector uses the anchoring effect of the polymer brush on the alignment layer to form a gradient refractive index in the liquid crystal layer, and does not need to set a complex modulation circuit on the substrate, and can apply a deflection effect on the light beam without external voltage; and the polymer in the liquid crystal beam deflector only exists near the first substrate and the second substrate, and is not distributed in the liquid crystal layer, which can effectively reduce the scattering caused by the multi-domain system and improve the transmittance of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0036] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings in the following description are only some embodiments of the present invention. For ordinary technicians in this field, other embodiments can be obtained based on these drawings without paying creative work.

[0037] Figure 1 It is a schematic structural diagram of a liquid crystal light beam deflector in one embodiment of the present invention;

[0038] Figure 2 A physical diagram of a liquid crystal beam deflector in one embodiment of the present invention;

[0039] Figure 3 is a flow chart of a method for preparing a liquid crystal beam deflector in one embodiment of the present invention;

[0040] Figure 4 A schematic diagram of a preparation process of a liquid crystal beam deflector according to an embodiment of the present invention;

[0041] Figure 5 This is a flow chart of step S2 in one embodiment of the present invention;

[0042] Figure 6 This is a flow chart of step S5 in one embodiment of the present invention;

[0043] Figure 7 is a schematic diagram of a mask used in step S5 in one embodiment of the present invention;

[0044] Figure 8 Schematic diagram of the process of step-by-step adjustment and photocuring of the liquid crystal layer in step S5 in one embodiment of the present invention;

[0045] Fig. 9 The plan view (a) and cross-sectional view (b) of a polymer brush formed by the first alignment layer and the second alignment layer after photocuring in one embodiment of the present invention;

[0046] Fig.10 A schematic diagram of a test optical path for testing a light beam deflection effect of a liquid crystal light beam deflector in one embodiment of the present invention;

[0047] Fig.11 is a transmittance curve diagram of a liquid crystal beam deflector before and after light curing in one embodiment of the present invention;

[0048] Fig.12 A schematic diagram of the offset position of the incident light beam cursor center of the liquid crystal light beam deflector before and after the test light path is added in one embodiment of the present invention;

[0049] Fig.13FIG. 1 is a diagram showing the electrically adjustable effect of a liquid crystal beam deflector on an incident light beam in one embodiment of the present invention.

[0050] Component number description

[0051] 11. First substrate; 12. First alignment layer; 13. Liquid crystal layer; 14. Second alignment layer; 15. Second substrate. DETAILED DESCRIPTION

[0052] The following is an explanation of the embodiments of the present invention by specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention. It should be noted that the features in the following embodiments and the embodiments can be combined with each other without conflict. It should also be understood that the terms used in the embodiments of the present invention are intended to describe specific embodiments, rather than to limit the scope of protection of the present invention. The test methods for which specific conditions are not specified in the following examples are usually carried out under conventional conditions or according to the conditions recommended by the manufacturers.

[0053] When numerical ranges are given in the embodiments, it should be understood that unless otherwise specified in the present invention, both endpoints of each numerical range and any value between the two endpoints can be selected. Unless otherwise defined, all technical and scientific terms used in the present invention are familiar to those skilled in the art and the description of the present invention, and any method, device and material of the prior art similar or equivalent to the method, device and material in the embodiments of the present invention can also be used to implement the present invention.

[0054] It should be noted that the terms such as "upper", "lower", "left", "right", "middle" and "one" etc. used in this specification are only for the convenience of description and are not intended to limit the scope of implementation of the present invention. Changes or adjustments to their relative relationships, without substantially changing the technical content, should also be regarded as the scope of implementation of the present invention.

[0055] See also Figure 1 and Figure 2In one aspect, the present invention provides a liquid crystal beam deflector. The liquid crystal beam deflector comprises a first substrate 11, a first orientation layer 12, a liquid crystal layer 13, a second orientation layer 14 and a second substrate 15. The first orientation layer 12 is arranged on the first substrate 11, the liquid crystal layer 13 is arranged on the first orientation layer 12, the second orientation layer 14 is arranged on the liquid crystal layer 13, and the second substrate 15 is arranged on the second orientation layer 14. The first orientation layer 12 and the second orientation layer 14 cooperate to anchor and control the tilt angle of the liquid crystal molecules in the liquid crystal layer 13, so that when the liquid crystal beam deflector is not supplied with voltage, the liquid crystal layer 13 inside the liquid crystal beam deflector has a gradient refractive index in the first direction, and the gradient refractive index distribution is generated by the liquid crystal layer 13 under external electric field modulation and anchored by the polymer brushes on the first orientation layer 12 and the second orientation layer 14. The first direction can be any direction parallel to the surface of the liquid crystal layer 13. Since the liquid crystal layer 13 has a gradient refractive index along the first direction, a specific phase difference distribution is formed in the first direction. According to the principle of optical diffraction, the near-field phase of the control beam in the liquid crystal layer 13 is distributed in the form of a blazed grating, so that most of the energy of the extraordinary light of the incident light beam after phase difference modulation after passing through the liquid crystal layer 13 will be distributed in a certain spectral order in the far field (i.e., at a certain angle), thereby achieving a large-angle deflection of the main-order diffraction of the outgoing light beam.

[0056] Among them, the deflection angle (β) of the incident light after passing through the liquid crystal beam deflector satisfies the following relationship:

[0057]

[0058] N is the phase step bundle in the liquid crystal layer 13 (ie, the number of regions with the same refractive index), d is the distance between adjacent phase steps, m is the diffraction order, and λ is the wavelength of the incident light.

[0059] As an active beam deflector, the liquid crystal beam deflector has a beam deflection function when no external voltage is applied; when an external voltage is applied, the electric field force applied to the liquid crystal layer 13 opposes the anchoring effect provided by the first orientation layer 12 and the second orientation layer 14, so that the phase difference of the preset phase distribution of the liquid crystal layer 13 becomes smaller, and the beam deflection function is gradually lost. Therefore, the liquid crystal beam deflector can switch from deflection to non-deflection by applying an electric field.

[0060] like Figure 1 and Fig. 9As shown, in some embodiments, the first alignment layer 12 initiates polymerization of a polymer brush on the surface of the first substrate 11, and similarly, the second alignment layer 14 is also a polymer brush that initiates polymerization on the surface of the second substrate 15. Since the polymer chains in the polymer brush are highly stretched, oriented, and have a high coverage rate. The first alignment layer 12 and the second alignment layer 14 located on both sides of the liquid crystal layer 13 can form a polymer brush under light initiation to anchor the direction of the director of the liquid crystal molecules. Therefore, the direction of the director generated by the liquid crystal molecules in the liquid crystal layer 13 under external electric field modulation can be solidified by the anchoring effect generated by the first alignment layer 12 and the second alignment layer 14 under light initiation. After the external electric field is removed, the first alignment layer 12 and the second alignment layer 14 can cooperate to anchor the direction of the director of the liquid crystal molecules in the liquid crystal layer 13, so that the liquid crystal layer 13 still has a phase distribution applied by the electric field modulation, that is, the liquid crystal layer 13 has a refractive index distribution that changes gradiently along the first direction when no voltage is applied.

[0061] In addition, the liquid crystal beam deflector limits the polymer brush formed by the first orientation layer 12 to the surface of the first substrate 11, and limits the polymer brush formed by the second orientation layer 14 to the surface of the second substrate 15, which can reduce the refraction at the polymer / liquid crystal interface in the device, thereby effectively reducing the scattering caused by the multi-domain system and improving the transmittance of the device. In addition, the polymer brushes are arranged on both sides of the liquid crystal layer 13, which can accelerate the free relaxation of liquid crystal molecules and effectively improve the response speed of the device, so that the response speed of the liquid crystal beam deflector reaches the sub-millisecond level.

[0062] like Figure 1 and Figure 2 As shown, in some embodiments, the liquid crystal layer 13 has a refractive index distribution with a periodic gradient change in the first direction, wherein the refractive index distribution with a gradient change on the liquid crystal layer 13 is arranged periodically in the first direction.

[0063] It should be noted that the first substrate 11 and the second substrate 15 can be made of any conductive light-transmitting material on the market. For example, in some embodiments, the first substrate 11 and the second substrate 15 can be made of indium tin oxide (ITO) glass. The first orientation layer 12 and the second orientation layer 14 include a photoinitiator and a liquid crystal orientation agent. The photoinitiator can be an organic substance that contains an absorption peak in the photocuring band. The liquid crystal orientation agent is at least one of polyvinyl alcohol, polyimide and polystyrene. The liquid crystal layer 13 includes liquid crystal and monomers, wherein the monomers are acrylic acid ester liquid crystal monomers, for example, 1,4-bis-[4-(3-acryloxypropoxy)benzoyloxy]-2-methylbenzene (RM257), 1,4-bis-[4-(6-acryloxyhexyloxy)benzoyloxy]-2-methylbenzene (RM82), 4-methoxyphenyl 4-(6-(acryloxy)hexyloxy)benzoate (RM105), 4-cyanophenyl 4'-(6-acryloxyhexyloxy)benzoate (RM23), isooctyl acrylate (EHA), 2-dodecyl acrylate (C12A), trimethylolpropane triacrylate (TMPTA). The liquid crystal may be a positive nematic phase liquid crystal. The polymer brushes on the first alignment layer 12 and the second alignment layer 14 are polymers formed by polymerization of the photoinitiator in the alignment layer and the monomers in the liquid crystal layer 13.

[0064] In addition, in some embodiments, the thickness of the first alignment layer 12 and the second alignment layer 14 is 20nm to 500nm, for example, the thickness of the first alignment layer 12 and the second alignment layer 14 can be 20nm, 30nm, 50nm, 70nm, 100nm, 150nm, 200nm, 250nm, 300nm, 350nm, 400nm, 450nm or 500nm. The thickness of the liquid crystal layer 13 is 5μm to 100μm, for example, the thickness of the liquid crystal layer 13 can be 5μm, 10μm, 15μm, 20μm, 25μm, 30μm, 35μm, 40μm, 45μm, 50μm, 55μm, 60μm, 65μm, 70μm, 75μm, 80μm, 85μm, 90μm or 100μm.

[0065] See also Figures 3 to 9 On the other hand, the present invention also provides a method for preparing a liquid crystal beam deflector. Figure 3 and Figure 4 As shown, the preparation method comprises the following steps:

[0066] S1, providing a first substrate 11 and a second substrate 15;

[0067] S2, forming a first alignment layer 12 on the surface of the first substrate 11, and forming a second alignment layer 14 on the surface of the second substrate 15;

[0068] S3, performing an alignment process on the first alignment layer 12 and the second alignment layer 14;

[0069] S4, placing the first substrate 11 and the second substrate 15 opposite to each other, and forming a liquid crystal layer 13 between the first alignment layer 12 and the second alignment layer 14; wherein the alignment directions of the first alignment layer 13 and the second alignment layer 14 opposite to each other are opposite;

[0070] S5. Divide the liquid crystal layer 13 into a plurality of modulation areas, and gradiently adjust and photo-cure the direction of the pointing vector of the liquid crystal molecules in each of the modulation areas along a first direction, so that the liquid crystal layer 13 has a refractive index that gradiently changes along the first direction when no voltage is applied; wherein the first direction is parallel to the surface of the liquid crystal layer 13.

[0071] In step S1, substrates of conductive transparent materials are provided as the first substrate 11 and the second substrate 15. For example, the first substrate 11 and the second substrate 15 are made of indium tin oxide (ITO) glass. In addition, in some embodiments, step S1 also includes performing hydrophilic treatment on the surfaces of the first substrate 11 and the second substrate 15 to enhance the surface hydrophilicity of the first substrate 11 and the second substrate 15. The surface treatment method for the first substrate 11 and the second substrate 15 can be one or more of ultraviolet ozone treatment, reactive ion etching, and coating with a surfactant.

[0072] like Figures 4 to 5 As shown, in some embodiments, step S2 includes the following steps:

[0073] S21, mixing a photoinitiator, a liquid crystal alignment agent and a solvent and coating the mixture on the surfaces of the first substrate 11 and the second substrate 15;

[0074] It should be noted that in step S21, the photoinitiator, the liquid crystal alignment agent and the solvent can be mixed evenly according to the conventional mass ratio of the polymer layer prepared in the art and coated on the conductive surfaces of the first substrate 11 and the second substrate 15, and the specific mass ratio range of the photoinitiator, the liquid crystal alignment agent and the solvent is not limited in the present invention. For example, in one example, in step S21, the photoinitiator, the liquid crystal alignment agent and the solvent can be mixed evenly according to the mass ratio of 3.5:100:1700, and the mixed solution can be spin-coated on the conductive surfaces of the first substrate 11 and the second substrate 15.

[0075] The solvent is at least one of deionized water, dimethylacetamide, N-methylpyrrolidone and toluene; the liquid crystal alignment agent is at least one of polyvinyl alcohol (PVA), polyimide (PI) and polystyrene (PS); the photoinitiator has an absorption peak including a photocuring band, for example, in some embodiments, the absorption peak of the photoinitiator includes an ultraviolet band with a wavelength of 365nm, and the photoinitiator can be one or more of 2-hydroxy-4'-(2-hydroxyethoxy)-2-methylpropiophenone (i.e., I2959), diphenyl (2,4,6-trimethylbenzoyl) phosphine oxide (i.e., TPO), and phenyl bis (2,4,6-trimethylbenzoyl) phosphine oxide (i.e., 819).

[0076] S22 , heating and drying the solvent on the first substrate 11 and the second substrate 15 to form a first alignment layer 12 on the first substrate 11 and a second alignment layer 14 on the second substrate 15 .

[0077] In step S22, the first substrate 11 and the second substrate 15 are placed on a heating platform, and the first substrate 11 and the second substrate 15 are heated at a temperature higher than the boiling point of the solvent to dry the first substrate 11 and the second substrate 15 so that the solvent in the coating layer on the first substrate 11 and the second substrate 15 is completely volatilized, thereby forming a first orientation layer 12 encapsulating the photoinitiator on the first substrate 11 and a second orientation layer 14 encapsulating the photoinitiator on the second substrate 15.

[0078] In step S3 , the surfaces of the first alignment layer 12 and the second alignment layer 14 are rubbed along the same direction using nylon cloth, and the rubbing direction is the orientation direction of the polymer brushes on the first alignment layer 12 and the second alignment layer 14 .

[0079] like Figure 4As shown, in some embodiments, in step S4, the first substrate 11 and the second substrate 15 are first arranged opposite to each other, the first alignment layer 12 and the second alignment layer 14 are oriented opposite to each other, and the orientation directions of the first alignment layer 12 and the second alignment layer 14 arranged opposite to each other are opposite, that is, the friction directions of the surfaces of the first alignment layer 12 and the second alignment layer 14 opposite to each other are opposite; specifically, the first substrate 11 and the second substrate 15 are adhered to each other, and spacers are arranged at the edges of the gap between the first substrate 11 and the second substrate 15. Or the spacer controls the spacing, so that a liquid crystal box with a photoinitiating layer coated on the inner surface is formed between the first substrate 11 and the second substrate 15, and the thickness of the liquid crystal box is controlled to be 5μm to 100μm, for example, the thickness of the liquid crystal box can be 5μm, 10μm, 15μm, 20μm, 25μm, 30μm, 35μm, 40μm, 45μm, 50μm, 55μm, 60μm, 65μm, 70μm, 75μm, 80μm, 85μm, 90μm or 100μm. Among them, the adhesive for adhering the first substrate 11 and the second substrate 15 is an epoxy resin glue.

[0080] Then, the monomer and liquid crystal are filled in the liquid crystal box between the first substrate 11 and the second substrate 15, and the filling port is sealed so that the monomer and the liquid crystal form a liquid crystal layer 13 between the first orientation layer 12 and the second orientation layer 14. The monomer is an acrylic ester liquid crystal monomer, for example, it can be one of 1,4-bis-[4-(3-acryloxypropoxy)benzoyloxy]-2-methylbenzene (RM257), 1,4-bis-[4-(6-acryloxyhexyloxy)benzoyloxy]-2-methylbenzene (RM82), 4-methoxyphenyl 4-(6-(acryloxy)hexyloxy)benzoate (RM105), 4-cyanophenyl 4'-(6-acryloxyhexyloxy)benzoate (RM23), isooctyl acrylate (EHA), 2-dodecyl acrylate (C12A), and trimethylolpropane triacrylate (TMPTA). The liquid crystal can be a positive nematic liquid crystal.

[0081] like Figure 6 and Figure 8 As shown, in some embodiments, step S5 includes the following steps:

[0082] S51, obtaining a voltage-phase relationship of the liquid crystal layer 13, dividing the liquid crystal layer 13 into a plurality of modulation areas along the first direction according to a preset phase difference and phase gradient, and obtaining a plurality of adjustment voltages corresponding to phase gradient changes for the plurality of modulation areas;

[0083] In step S51, a test optical path is constructed by conventional experimental means to measure the voltage-phase relationship of the liquid crystal layer 13, that is, the direction of the pointing vector of the liquid crystal molecules in the liquid crystal layer 13 under different voltages. In addition, since the liquid crystal layer 13 is fixed by oppositely oriented polymer brushes, its refractive index of the effective extraordinary light of the incident light (that is, the polarization of light parallel to the arrangement direction of the liquid crystal molecules) can be adjusted by changing the externally applied voltage. Therefore, step S51 can be based on the voltage-phase correspondence of the liquid crystal layer 13, and according to the design requirements of the periodic gradient refractive index distribution (that is, gradient phase distribution) of the liquid crystal layer 13 in the first direction, obtain the phase difference and phase gradient of the liquid crystal layer 13 corresponding to the design requirements; then, based on the preset phase difference and phase gradient, divide the liquid crystal layer 13 into a plurality of modulation areas along the first direction, and obtain a plurality of adjustment voltages that can cause the liquid crystal layer 13 to produce a gradient phase change for the plurality of modulation areas, such as a plurality of adjustment voltages from high to low being V 1 、V 2 ,…,V n .

[0084] S52, applying the corresponding adjustment voltage to each modulation area in the first direction in turn according to the phase gradient change trend, and curing the director direction of the liquid crystal molecules in the modulation area after modulation by light. Fig. 9 As shown, after curing, polymer brushes that anchor the direction of the directors of the liquid crystal molecules in the liquid crystal layer 13 are formed on the first alignment layer 12 and the second alignment layer 14, so that the liquid crystal layer 13 retains the electrically modulated gradient refractive index distribution when no power is supplied.

[0085] like Figure 6 As shown, step S52 specifically includes the following steps:

[0086] S521, designing a mask corresponding to a plurality of modulation regions divided in the first direction of the liquid crystal layer 13;

[0087] like Figure 7 As shown, the effective area size of the mask pattern matches the size of the liquid crystal layer 13, and the mask includes a light-transmitting area and an opaque mask area. The light-transmitting area and the mask area are arranged along the first direction, and the width of the light-transmitting area is equal to the width of a modulation area in the first direction. In one example, when it is necessary to modulate a gradient refractive index distribution of one period on the liquid crystal layer 13, only one group of light-transmitting areas and mask areas are arranged on the mask. In another example, when it is necessary to modulate a gradient refractive index distribution of multiple periods on the liquid crystal layer 13, multiple groups of light-transmitting areas and mask areas are arranged along the first direction on the mask, and the sum of the widths of the light-transmitting areas and the mask areas is the width of a gradient refractive index distribution area of ​​one period in the liquid crystal layer 13 in the first direction.

[0088] S522, such as Figure 4 As shown, a modulated light path is constructed, and a liquid crystal beam deflector and a mask are placed on the modulated light path, so that the mask overlaps with the liquid crystal layer 13 of the liquid crystal beam deflector, and the light in the curing band can cover the mask and the liquid crystal layer 13, and the curing band light generated by the modulated light path can pass through the light-transmitting area on the mask to irradiate the liquid crystal layer 13. In one example, the wavelength of the light source used in the modulated light path is 365nm, and the light intensity is 0-30W / cm 2 .

[0089] S523, using a step-by-step photocuring method or a continuous photocuring method, electrically adjusting and photocuring the direction of the director of each modulation area in turn. Wherein, when using step-by-step curing, the sample is photocured under several fixed voltage and displacement conditions, at which time the phase plane of the liquid crystal layer 13 is distributed in a step-like manner, and the phase difference between every two adjacent steps is equal. When using continuous curing, the sample is photocured under continuously changing voltage and displacement, at which time the phase plane of the liquid crystal layer 13 is close to an ideal inclined plane.

[0090] like Figure 4 and Figure 8 As shown, in one example, in step S523, the light source of the modulated light path is turned on, and the curing band light generated by the modulated light path can be irradiated to the first modulated area of ​​the liquid crystal layer 13 through the light-transmitting area on the mask; the adjustment voltages (V 1 、V 2 ,…,V n ), and after each voltage adjustment effect is cured, the mask is moved along the first direction by a light-transmitting area width through a precision translation stage, so that the next modulation area that needs phase modulation is exposed to the light of the curing band, thereby applying a corresponding voltage to the next modulation area that needs phase modulation to adjust the direction of the director of the liquid crystal molecules in the area, and at the same time, the phase distribution adjusted in the modulation area is cured by light. After traversing all modulation areas, a liquid crystal beam deflector with a gradient refractive index distribution without voltage can be obtained.

[0091] In addition, in some embodiments, the preparation method further includes periodically modulating the gradient refractive index of the liquid crystal layer 13 so that the liquid crystal layer 13 has a periodically arranged refractive index gradient distribution in the first direction, and the periodic refractive index gradient modulation step includes:

[0092] Divide the liquid crystal layer 13 into a plurality of periodic modulation regions along the first direction, and modulate each periodic modulation region with the same refractive index gradient distribution, that is, perform a modulation process as in step S5 on each periodic modulation region;

[0093] Specifically, the modulation process for each periodic modulation area includes: dividing the periodic modulation area into a plurality of modulation areas along the first direction, and obtaining a plurality of adjustment voltages corresponding to the phase gradient change for the plurality of modulation areas; applying the corresponding adjustment voltage to each modulation area in the first direction in turn according to the phase gradient change trend, and using light to solidify the direction of the director of the liquid crystal molecules in the modulation area after modulation, so that the periodic modulation area has a refractive index distribution with a gradient change along the first direction when no voltage is applied. The liquid crystal layer 13 has the same refractive index gradient distribution in each periodic modulation area after modulation, and thus has a periodically arranged refractive index gradient distribution in the first direction.

[0094] For example, in one example, when the preparation method modulates the periodic gradient refractive index distribution on the liquid crystal layer 13, Figure 7 and Figure 8 As shown, in step S51, a mask plate having multiple groups of light-transmitting areas and mask areas is used, and the mask plate arranges multiple groups of light-transmitting areas and mask areas along a first direction, and the sum of the widths of the light-transmitting areas and the mask areas is the width of a single-period gradient refractive index distribution area in the first direction; and continuing to the subsequent step S52, a liquid crystal layer 13 with a periodic gradient refractive index distribution can be obtained.

[0095] The technical scheme of the present invention is described in detail below through specific examples. Unless otherwise specified, the raw materials and reagents used in the following examples are commercially available or can be prepared by conventional methods in the art.

[0096] Example

[0097] S1. Take indium tin oxide glass with a thickness of 0.55 mm as the first substrate 11 and the second substrate 15, and perform reactive ion etching treatment on the surfaces of the first substrate 11 and the second substrate 15 (reaction atmosphere: O2, power: 25 W, time: 20 s). The surface energy of the first substrate 11 and the second substrate 15 after surface treatment is 72.3 mN / m.

[0098] S2. Mix the photoinitiator, liquid crystal alignment agent and deionized water in a mass ratio of 3.5:100:1700 in a light-proof environment.

[0099] The mixed solution is spin-coated onto the hydrophilic treated surfaces of the first substrate 11 and the second substrate 15; the first substrate 11 and the second substrate 15 are heated at a temperature higher than the boiling point of the solvent, and the solvent on the first substrate 11 and the second substrate 15 is dried, so that the liquid crystal alignment agent on the first substrate 11 and the second substrate 15 is dried to form a film and covers the photoinitiator, thereby forming a first alignment layer 12 on the first substrate 11 and a second alignment layer 14 on the second substrate 15. The liquid crystal alignment agent is PVA, and the molecular weight of PVA is 9000 to 10000; the photoinitiator is I2959; and the solvent is deionized water. The thickness of the first alignment layer 12 and the second alignment layer 14 is 187nm.

[0100] S3 , using nylon cloth to rub the first alignment layer 12 on the first substrate 11 and the second alignment layer 14 on the second substrate 15 in the same direction, and marking the rubbing direction as the alignment direction of the first alignment layer 12 and the second alignment layer 14 .

[0101] S4, spraying spacers with an outer diameter of 7 μm on the surface of the first substrate 11 or the second substrate 15, and then placing the first substrate 11 and the second substrate 15 in opposite directions, and bonding the first substrate 11 and the second substrate 15 in opposite directions together using epoxy curing adhesive, so that a liquid crystal box is formed between the first substrate 11 and the second substrate 15, and the thickness of the liquid crystal box is 7.2 μm; then pouring a mixture of monomers and liquid crystals into the liquid crystal box, and sealing the crystal pouring port, so that the monomers and liquid crystals form a liquid crystal layer 13 between the first orientation layer 12 and the second orientation layer 14. Among them, the monomer is RM257, the liquid crystal is positive nematic phase liquid crystal E7 (Merk), and the mass ratio of liquid crystal to monomer is 9:1.

[0102] S5. First, a test optical path is constructed, and the voltage-phase correspondence of the liquid crystal layer 13 is obtained by testing the test optical path. Fig.10 As shown, the constructed test optical path includes He-Ne laser (632.8nm), attenuation plate, polarizer, sample, analyzer and CCD in sequence according to the light incident direction. The polarization direction of the polarizer is orthogonal to the polarization direction of the analyzer, and the orientation direction of the sample is 45° to the polarizer. According to the pre-designed phase difference and phase gradient, the liquid crystal layer 13 is divided into 8 periodic regions along the first direction, and 9 modulation regions are divided along the first direction in each periodic region. The width of each periodic region in the first direction is 225μm, the total phase difference of each periodic region is 4π, the phase gradient between adjacent modulation regions is 0.44π, and the size of each modulation region in the first direction is 25μm; at the same time, based on the voltage-phase correspondence and the total phase difference and phase gradient in each period, 9 adjustment voltages corresponding to the 9 modulation regions of a single period are obtained.

[0103] Secondly, based on the eight periodic regions divided along the first direction on the liquid crystal layer 13 and the nine modulation regions in each periodic region, a mask corresponding to the partition is designed. Figure 7 As shown, the designed mask shape coincides with the liquid crystal layer 13, and the mask includes 8 groups of periodically arranged light-transmitting areas and mask areas in the first direction, and the width of one group of light-transmitting areas and mask areas is 225 μm, the width of the light-transmitting area is 25 μm, and the width of the mask area is 200 μm.

[0104] Then, a modulated optical path is constructed, and the wavelength of the light source used in the modulated optical path is 365nm. The liquid crystal beam deflector and the mask are placed on the modulated optical path, the uncured liquid crystal beam deflector is placed on the sample holder, and an external power supply is connected, and the timing and amplitude of the sample applied voltage are controlled by LabVIEW software; the mask is set on a motion controller (Newport ESP300) and placed in front of the liquid crystal beam deflector, the mask overlaps with the liquid crystal layer 13 of the liquid crystal beam deflector, and the light in the curing band can cover the mask and the liquid crystal layer 13, and the curing band light generated by the modulated optical path can pass through the light-transmitting area on the mask to irradiate the liquid crystal layer 13.

[0105] Finally, a voltage V is applied to the liquid crystal beam deflector. 1 With a light intensity of 350mW / cm 2 After the transparent area is irradiated with 365nm purple light, the first modulation area on each periodic area of ​​the liquid crystal layer 13 is solidified and anchored after irradiation for 1 minute. After the solidification is completed, the motion controller is turned on to move the mask plate 25μm along the first direction, and the second modulation area of ​​each periodic area of ​​the liquid crystal layer 13 is exposed to the transparent area, and a voltage V is applied to the liquid crystal beam deflector. 2 (V 2 <V 1 ), continue light curing for 1 minute to anchor the solidification of the tilt angle of the liquid crystal molecules in the second modulation area; then repeat the above operation in the order of adjusting voltage from high to low until the phase modulation and curing of a periodic area are completed, thereby obtaining a liquid crystal layer 13 with a periodic gradient refractive index change in the first direction. A test light path is set up to test the transmittance and deflection function of the liquid crystal beam deflector in the above embodiment to verify the efficacy of the present invention.

[0106] like Fig.10 As shown, the constructed test optical path includes a He-Ne laser (632.8nm), an attenuation plate, a polarizer, a liquid crystal beam deflector, a lens, an analyzer and a CCD in sequence according to the light incident direction. The polarization direction of the polarizer is parallel to the first direction of the liquid crystal beam deflector, and the polarization direction of the polarizer is orthogonal to the polarization direction of the analyzer.

[0107] The transmittance of the liquid crystal beam deflector before and after step-by-step curing modulation was tested using a violet-visible spectrophotometer. The test results are as follows: Fig.11 As shown, the liquid crystal beam deflector still has a high transmittance after step-curing phase modulation.

[0108] use Fig.10 The test optical path constructed tests the deflection effect of the liquid crystal beam deflector on the incident light. The test results are as follows: Fig.12 As shown, the liquid crystal beam deflector realizes the deflection function of the incident light, and when the deflection angle is 0.16°, the diffraction efficiency is as high as 80.3%.

[0109] use Fig.10 The test light path constructed was used to test the liquid crystal beam deflector for the electrically adjustable function of the deflection effect. The test results are as follows: Fig.13 As shown, the liquid crystal beam deflector does not have the deflection function for the incident light in the power-on state, and has the deflection function for the incident light in the power-off state.

[0110] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.

Claims

1. A liquid crystal beam deflector, characterized in that: include: a first substrate; A first alignment layer, which is disposed on the first substrate; a liquid crystal layer disposed on the first alignment layer; a second alignment layer, which is disposed on the liquid crystal layer; a second substrate, disposed on the second alignment layer; Wherein, when no voltage is applied to the liquid crystal beam deflector, the liquid crystal layer has a refractive index that changes in a gradient in a first direction; the first direction is parallel to the surface of the liquid crystal layer.

2. The liquid crystal beam deflector according to claim 1, characterized in that: The first alignment layer and the second alignment layer are polymer brushes. When no voltage is applied to the liquid crystal beam deflector, the first alignment layer and the second alignment layer anchor the director directions of the liquid crystal molecules in the liquid crystal layer.

3. The liquid crystal beam deflector according to claim 1, characterized in that: The gradient-varying refractive index distribution on the liquid crystal layer is periodically arranged in the first direction.

4. The liquid crystal beam deflector according to claim 1, characterized in that: The thickness of the first alignment layer and the second alignment layer is 20 nm to 500 nm; the thickness of the liquid crystal layer is 5 μm to 100 μm.

5. A method for preparing a liquid crystal beam deflector, characterized in that: include: providing a first substrate and a second substrate; forming a first alignment layer on a surface of the first substrate, and forming a second alignment layer on a surface of the second substrate; performing an alignment treatment on the first alignment layer and the second alignment layer; The first substrate and the second substrate are arranged opposite to each other, and a liquid crystal layer is formed between the first alignment layer and the second alignment layer; wherein the first alignment layer and the second alignment layer arranged opposite to each other have opposite alignment directions; The liquid crystal layer is divided into a plurality of modulation areas, and the direction of the directing vector of the liquid crystal molecules in each of the modulation areas is gradiently adjusted along a first direction and photocured so that the liquid crystal layer has a refractive index that changes gradiently along the first direction when no voltage is applied; wherein the first direction is parallel to the surface of the liquid crystal layer.

6. The preparation method according to claim 5, characterized in that: Gradiently adjusting and photocuring the direction of the director of the liquid crystal molecules in each of the modulation regions along a first direction, comprising: Acquire a voltage-phase relationship of the liquid crystal layer, divide the liquid crystal layer into a plurality of modulation areas along the first direction according to a preset phase difference and phase gradient, and acquire a plurality of adjustment voltages corresponding to phase gradient changes for the plurality of modulation areas; According to the phase gradient variation trend, the corresponding adjustment voltage is applied to each of the modulation areas in the first direction in turn, and the director direction of the modulated liquid crystal molecules in the modulation area is solidified by light.

7. The preparation method according to claim 5, characterized in that: The method further includes a step of modulating the liquid crystal layer to have a periodic refractive index gradient distribution, wherein the periodic refractive index gradient modulation step includes: Dividing the liquid crystal layer into a plurality of periodic modulation regions along the first direction, and performing modulation with the same refractive index gradient distribution on each of the periodic modulation regions; Among them, for each of the periodic modulation areas: the periodic modulation area is divided into a plurality of modulation areas along the first direction, and the direction of the pointing vector of the liquid crystal molecules in each of the modulation areas is gradient adjusted and photocured along the first direction, so that the periodic modulation area has a refractive index distribution that changes gradiently along the first direction when no voltage is applied.

8. The preparation method according to claim 5, characterized in that: Forming a first alignment layer on a surface of the first substrate and forming a second alignment layer on a surface of the second substrate, comprising: A photoinitiator, a liquid crystal alignment agent and a solvent are mixed and coated on the surfaces of the first substrate and the second substrate; wherein the solvent is at least one of deionized water, dimethylacetamide, N-methylpyrrolidone and toluene; the liquid crystal alignment agent is at least one of polyvinyl alcohol, polyimide and polystyrene; and the photoinitiator has an absorption peak including the photocuring band; The solvent on the first substrate and the second substrate is heated and dried to form a first alignment layer on the first substrate and a second alignment layer on the second substrate.

9. The preparation method according to claim 5, characterized in that: Performing an alignment process on the first alignment layer and the second alignment layer, comprising: The surfaces of the first alignment layer and the second alignment layer are rubbed in the same direction.

10. The preparation method according to claim 5, characterized in that: The first substrate and the second substrate are arranged opposite to each other, and a liquid crystal layer is formed between the first alignment layer and the second alignment layer, comprising: The first substrate and the second substrate are arranged opposite to each other, so that the first alignment layer and the second alignment layer are arranged opposite to each other; wherein the first alignment layer and the second alignment layer arranged opposite to each other have opposite alignment directions; A monomer and a liquid crystal are filled between the first alignment layer and the second alignment layer to form a liquid crystal layer; wherein the monomer is an acrylic ester liquid crystal monomer, and the liquid crystal is a positive nematic phase liquid crystal.